CCMFPC of soft gold electroplating process
The CCM_FPC with a soft gold electroplating process addresses nickel corrosion issues by using a thick gold layer as a barrier, ensuring stable wire bonding and enhancing the reliability of high-pixel camera modules in mobile phones.
Patent Information
- Application Number
- CN202420464603.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-11
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-03-11
AI Technical Summary
Existing FPC boards face nickel corrosion during chemical nickel-palladium-gold surface treatment, which affects the reliability and stability of high-pixel camera modules in mobile phones.
A CCM_FPC with a soft gold electroplating process that includes a bonding layer, ground layer, data transfer layer, and BTB layer, featuring electroplated leads and ground areas to prevent nickel corrosion, and uses a thick gold layer as a barrier, enhancing stability and reliability.
The soft gold electroplating process prevents nickel corrosion, ensures stable wire bonding, and provides a delicate gold surface with high lattice density, improving the reliability and quality of camera modules in mobile phones.
Smart Images

Figure CN222108215U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of FPC, in particular to a CCM_FPC with a soft gold electroplating process. Background Art
[0002] FPC board, also called flexible circuit board, is a highly reliable and excellent flexible printed circuit board made of polyimide or polyester film as the base material.
[0003] As the income and consumption level of mobile phone users increase, end consumers pay more and more attention to the camera function of mobile phones. The camera capability of smart phones has gradually become the main selling point of mobile phones and the driving force for consumers to change their phones. Major mobile phone manufacturers are committed to creating the ultimate photography experience for users, improving the shooting quality by increasing the number of cameras, and multi-camera solutions are constantly penetrating. In addition to the trend of increasing the "quantity" of mobile phone cameras, another obvious development trend is the improvement in "quality". High-pixel cameras are packaged using the Wire bonding process, and the mainstream surface treatment of FPC corresponding to Wire bonding is chemical nickel-palladium-gold, but nickel corrosion will occur during the treatment process.
[0004] To this end, we propose a CCM_FPC with electroplating soft gold process. Utility Model Content
[0005] The purpose of the utility model is to provide a CCM_FPC with a soft gold electroplating process to solve the problems raised in the above background technology.
[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a CCM_FPC with a soft gold electroplating process, comprising a bonding layer, a ground layer, a data transfer layer and a BTB layer, wherein the bonding layer, the ground layer, the data transfer layer and the BTB layer are arranged in sequence from bottom to top, the bonding layer comprises a bonding pad area, a first ground area, a first via and a first electroplated lead, the bonding pad area is located at the top of the FPC, the first ground area is distributed around the device pad and the signal line in the bonding pad area, the first via is arranged at the connection between the bonding layer line and the ground layer line, the data transfer layer line and the BTB layer line, and the first electroplated lead is electrically connected to one end of the bonding layer and BTB layer electroplated circuits.
[0007] Optionally, the ground layer includes a ground line, a grid area and a second via hole, the ground line is laid between the bonding layer line and the data transfer layer line, the grid area is located in the middle of the ground line, and the second via hole is arranged at the connection between the ground layer line and the bonding layer line, the data transfer layer line and the BTB layer line.
[0008] Optionally, a 45-degree grid ground line with a line width of 0.1 MM and a line spacing of 0.3 MM is laid in the grid area.
[0009] Optionally, the data transmission layer line includes a second ground line area, an impedance signal line and a third via hole, the second ground line area is distributed around the data transmission line and the impedance signal line laid in the data transmission layer, the impedance signal line is laid between several data transmission lines, and the third via hole is arranged at the connection between the data transmission layer line and the ground layer line, the bonding layer line and the BTB layer line.
[0010] Optionally, the differential impedance of the impedance signal line is 100 ohms.
[0011] Optionally, the BTB layer includes a third ground area, a BTB pad, a fourth via hole and a second electroplated lead, the third ground area is arranged around the BTB pad and the BTB layer signal line, the BTB pad is arranged at the bottom of the FPC, the fourth via hole is arranged at the connection between the BTB layer line and the bonding layer line, the ground layer line and the data transfer layer line, and the other end of the second electroplated lead is electrically connected to the bonding layer and the BTB layer electroplated line.
[0012] Optionally, the BTB pad is soldered to the BTB device by reflow soldering.
[0013] Compared with the prior art, the beneficial effects of the utility model are:
[0014] The CCM_FPC of the soft gold electroplating process is provided with a first electroplating lead and a second electroplating lead. The first electroplating lead and the second electroplating lead play a drainage role. The first electroplating lead connects the independent pads of the bonding layer circuit and the BTB layer circuit to the electroplated ground wire, and then the second electroplating lead of the BTB layer is connected to the copper foil at the edge of the board. The clip of the surface treatment electroplating gold hanger is clamped on the copper foil at the edge of the board and connected to the anode of the gold plating tank to realize the electroplating gold process and thick gold electroplating. The lattice density between the electroplated gold molecules is high, the gold surface is delicate, the wire bonding gold line is more stable, and the reliability is high. The traditional palladium layer is changed as a barrier layer, and the middle electroplated thick gold layer is used as a barrier layer to prevent nickel corrosion.
[0015] The CCM_FPC with the soft gold electroplating process prevents nickel corrosion by using the middle gold layer as a barrier layer. When wirebonding the gold wire, the gold wire and pure gold fuse quickly and efficiently. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a schematic diagram of the structure of the bonding layer of a CCM_FPC using a soft gold electroplating process according to the utility model;
[0017] Figure 2 This is a schematic diagram of the structure of the ground layer of a CCM_FPC using a soft gold electroplating process according to the utility model;
[0018] Figure 3 This is a schematic diagram of the structure of the data transmission layer of a CCM_FPC using a soft gold electroplating process according to the utility model;
[0019] Figure 4 This is a schematic structural diagram of the BTB layer of a CCM_FPC using a soft gold electroplating process according to the utility model.
[0020] In the figure: 1, bonding layer; 11, bonding pad area; 12, first ground area; 13, first via hole; 14, first electroplated lead; 2, ground layer; 21, ground line; 22, grid area; 23, second via hole; 3, data transfer layer; 31, second ground area; 32, impedance signal line; 33, third via hole; 4, BTB layer; 41, third ground area; 42, BTB pad; 43, fourth via hole; 44, second electroplated lead. DETAILED DESCRIPTION
[0021] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0022] See also Figures 1 to 4The utility model provides a CCM_FPC with a soft gold electroplating process, comprising a bonding layer 1, a ground layer 2, a data transfer layer 3 and a BTB layer 4, wherein the bonding layer 1, the ground layer 2, the data transfer layer 3 and the BTB layer 4 are arranged in sequence from bottom to top, the bonding layer 1 comprises a bonding pad area 11, a first ground area 12, a first via 13 and a first electroplating lead 14, the bonding pad area 11 is located at the top of the FPC, the first ground area 12 is distributed around the device pad and the signal line of the bonding pad area 11, shielding the influence of external electromagnetic waves on the internal circuit and the electromagnetic waves generated inside from radiating outward, the first via 13 is arranged at the connection between the bonding layer 1 line and the ground layer 2 line, the data transfer layer 3 line and the BTB layer 4 line, and the first electroplating lead 14 is electrically connected to one end of the bonding layer 1 and the BTB layer 4 electroplating line.
[0023] The ground layer 2 includes a ground line 21, a grid area 22 and a second via 23. The ground line 21 is laid between the bonding layer 1 line and the data transmission layer 3 line to shield the mutual interference between the electromagnetic waves generated by the bonding layer 1 line when it is working and the electromagnetic waves generated by the data transmission layer 3 line when it is working. The grid area 22 is located in the middle of the ground line 21, and the second via 23 is set at the connection between the ground layer 2 line and the bonding layer 1 line, the data transmission layer 3 line and the BTB layer 4 line.
[0024] The grid area 22 is provided with a 45-degree grid ground line with a line width of 0.1 MM and a line spacing of 0.3 MM, so that the bending area is softer and more resistant to bending.
[0025] The data transmission layer 3 line includes a second ground line area 31, an impedance signal line 32 and a third via 33. The second ground line area 31 is distributed around the data transmission line and the impedance signal line 32 laid on the data transmission layer 3 to shield the influence of external electromagnetic waves on the internal circuit and the electromagnetic waves generated internally from radiating outward. The impedance signal line 32 is laid between several data transmission lines, and the third via 33 is set at the line connection between the data transmission layer 3 line and the ground layer 2 line, the bonding layer 1 line and the BTB layer 4 line.
[0026] The differential impedance of the impedance signal line 32 is 100 ohms, which reduces the signal attenuation when the signal is transmitted at high speed.
[0027] The BTB layer 4 includes a third ground area 41, a BTB pad 42, a fourth via 43 and a second electroplated lead 44. The third ground area 41 is arranged around the BTB pad 42 and the signal line of the BTB layer 4 to shield the influence of external electromagnetic waves on the internal circuit and the electromagnetic waves generated internally from radiating outward. The BTB pad 42 is arranged at the bottom of the FPC, the fourth via 43 is arranged at the connection between the BTB layer 4 line and the bonding layer 1 line, the ground layer 2 line and the data transfer layer 3 line, and the other end of the second electroplated lead 44 is electrically connected to the bonding layer 1 and the BTB layer 4 electroplated line.
[0028] The BTB pad 42 is soldered to the BTB device by reflow soldering.
[0029] Working principle:
[0030] The first electroplating lead 14 and the second electroplating lead 44 play a drainage role. The first electroplating lead 14 connects the independent pads of the bonding layer 1 circuit and the BTB layer 4 circuit to the electroplated ground wire, and then the second electroplating lead 44 of the BTB layer 4 is connected to the copper foil at the edge of the board. The clip of the surface treatment electroplating gold hanger is clamped on the copper foil at the edge of the board to connect to the anode of the gold plating tank to realize the electroplating gold process and thick gold electroplating. The lattice density between the electroplated gold molecules is high, the gold surface is delicate, the wire bonding gold line is more stable, and the reliability is high. The traditional palladium layer is changed as a barrier layer, and the middle electroplated thick gold layer is used as a barrier layer to prevent nickel corrosion.
[0031] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to these embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A CCM_FPC with a soft gold electroplating process, comprising a bonding layer (1), a ground layer (2), a data transmission layer (3) and a BTB layer (4), It is characterized in that The bonding layer (1), the ground layer (2), the data transfer layer (3) and the BTB layer (4) are arranged in sequence from bottom to top; the bonding layer (1) comprises a bonding pad area (11), a first ground area (12), a first conductive via (13) and a first electroplated lead (14); the bonding pad area (11) is located on the top of the FPC; the first ground area (12) is distributed around the device pad and the signal line of the bonding pad area (11); the first conductive via (13) is arranged at the connection between the bonding layer (1) line and the ground layer (2) line, the data transfer layer (3) line and the BTB layer (4) line; the first electroplated lead (14) is electrically connected to one end of the bonding layer (1) and the BTB layer (4) electroplated lines.
2. A CCM_FPC with a soft gold electroplating process according to claim 1, It is characterized in that The ground layer (2) comprises a ground line (21), a grid area (22) and a second conductive hole (23); the ground line (21) is laid between the bonding layer (1) line and the data transfer layer (3) line; the grid area (22) is located in the middle of the ground line (21); and the second conductive hole (23) is arranged at the connection between the ground layer (2) line and the bonding layer (1) line, the data transfer layer (3) line and the BTB layer (4) line.
3. A CCM_FPC with a soft gold electroplating process according to claim 2, It is characterized in that The grid area (22) is provided with a grid ground line with a line width of 0.1 mm and a line spacing of 0.3 mm, forming a 45-degree inclined grid.
4. The CCM_FPC of the soft gold electroplating process according to claim 2, It is characterized in that The data transmission layer (3) line comprises a second ground line area (31), an impedance signal line (32) and a third conductive via (33); the second ground line area (31) is distributed around the data transmission line and the impedance signal line (32) laid on the data transmission layer (3); the impedance signal line (32) is laid between a plurality of data transmission lines; and the third conductive via (33) is arranged at a line connection between the data transmission layer (3) line and the ground line layer (2) line, the bonding layer (1) line and the BTB layer (4) line.
5. The CCM_FPC of the soft gold electroplating process according to claim 4, It is characterized in that The differential impedance of the impedance signal line (32) is 100 ohms.
6. The CCM_FPC of the soft gold electroplating process according to claim 4, It is characterized in that The BTB layer (4) comprises a third ground line area (41), a BTB pad (42), a fourth conductive via (43) and a second electroplated lead (44); the third ground line area (41) is arranged around the BTB pad (42) and the signal line of the BTB layer (4); the BTB pad (42) is arranged at the bottom of the FPC; the fourth conductive via (43) is arranged at the connection between the BTB layer (4) line and the bonding layer (1) line, the ground layer (2) line and the data transmission layer (3) line; and the other end of the second electroplated lead (44) is electrically connected to the bonding layer (1) and the BTB layer (4) electroplated line.
7. The CCM_FPC of the soft gold electroplating process according to claim 6, It is characterized in that The BTB pad (42) is soldered to the BTB device through reflow soldering.