Die core of battery cooling pipe die

By dividing the battery cooling tube mold core into straight core and bending core, and using different metal materials and connecting ring designs, the problem of high core molding is solved, efficient processing and maintenance is achieved, and the use is extended life.

CN222115762UActive Publication Date: 2024-12-06ANHUI NINGGUGO ZHONGDING MOLD MFG CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420087217.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-15
Publication Date
2024-12-06
Estimated Expiration
2034-01-15

AI Technical Summary

Technical Problem

During the processing of battery cooling tube molds, the mold core is difficult to form and the yield is low. Since the material needs to be consistent at different stages, the cost of use is high and the service life is affected.

Method used

Design a battery cooling tube mold core, divided into straight core and curved core, adopt different metal materials, and is connected to the lock block through lock grooves, and the connection ring is spaced to allow independent production and maintenance, reducing material costs and processing time.

Benefits of technology

The separation and production of die cores is realized, saving production time, reducing material costs, improving service life, and simplifying maintenance and replacement through regional segmented design, improving processing efficiency and yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222115762U_ABST
    Figure CN222115762U_ABST
Patent Text Reader

Abstract

The utility model provides a battery cooling pipe mould core, which relates to the technical field of mould cores, and comprises a mould body, a mould core and fixing knots, the mould core comprises a straight core and a bent core, the end parts of the straight core and the bent core are connected to form the mould core, a groove is arranged on the mould body, and two ends of the mould core are arranged in the groove through the fixing knots to form a mould clamping cavity. The die core can be separated into the straight part core and the bent part core, the straight part core and the bent part core can operate in two independent manufacturing modes, the manufacturing time of the whole die core is saved, and the efficiency is improved; according to the utility model, the straight core and the bent core can be made of different materials, so that the cost of the materials used in different areas is reduced; the connection position of the straight core and the bent core is separated by the connecting ring, the straight core and the bent core can be separated by damaging the connection position when the mold core is damaged, the damaged part can be replaced, and resources are saved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of mold cores, in particular to a battery cooling tube mold core. Background Art

[0002] In the use of batteries, most batteries use liquid cooling to adjust the temperature inside the battery. The coolant inside will use rubber cooling tubes to circulate the coolant. Rubber cooling tube products are slender, generally more than 600mm in length, and the degree of bending and compaction is irregular. The mold core is difficult to form, the deformation is large, the yield rate is low, and it is more complicated in machining. Generally, 718 material is selected and the overall layout is processed. The mold of the rubber cooling tube will use a core to make the middle of the rubber tube hollow. The material used in the core at different stages is the same, so the toughness and stiffness required for the metal at different stages are different, but the material of the entire core cannot be changed, which increases the cost of use and affects the service life. Utility Model Content

[0003] The technical problem to be solved by the utility model is to provide a battery cooling tube mold core to reduce the processing cost of the mold core, while reducing the processing flow of the mold core and improving the service life.

[0004] Based on the technical problems existing in the background technology, the utility model proposes a battery cooling tube mold core, including a mold body, a mold core, and a fixed section. The mold core includes a straight core and a curved core. The ends of the straight core and the curved core are connected to form the mold core. A groove is opened on the mold body. Both ends of the mold core are installed in the groove through a fixed section to form a mold clamping cavity.

[0005] Preferably, both ends of the straight core and the curved core are provided with mutually matching locking grooves and locking blocks, and the locking blocks of the curved core are matched and fixed to the locking grooves of the straight core.

[0006] Preferably, the connecting end between the curved core and the straight core is provided with an R angle.

[0007] Preferably, a connecting ring is sleeved on the locking block, and both ends of the connecting ring are provided with R angles.

[0008] Preferably, the straight core is made of SKD61 or HRC49-53 metal material.

[0009] Preferably, the bending core is made of ASD3-VIP, HRC43-45 metal material.

[0010] Preferably, the cross-section of the locking block is stepped, and the length of the locking groove is greater than the length of the locking block.

[0011] Preferably, the outer ring radius of the connecting ring is larger than the radius of the straight core or the curved core.

[0012] Preferably, the inner ring radius of the connecting ring is equal to the radius of the locking block.

[0013] Compared with the prior art, the battery cooling tube mold core proposed by the utility model adopts the above technical solution and achieves the following technical effects:

[0014] The utility model can separate the mold core into a straight core and a curved core. The straight core and the curved core can be operated through two independent production methods, which saves the time of the entire mold core production and improves efficiency. In the utility model, the materials of the straight core and the curved core can be different, so as to reduce the cost of materials used in different areas. In the utility model, the connection between the straight core and the curved core is separated by a connecting ring. Damage to the mold core can separate the straight core from the curved core by damaging the connection, and the damaged part can be replaced, saving resources. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 This is a schematic diagram of the mold core and mold installation structure of the utility model;

[0016] Figure 2 This is a schematic diagram of the mold core structure of the utility model;

[0017] Figure 3 It is a schematic cross-sectional view of the mold core of the utility model;

[0018] Figure 4 It is an enlarged view of area a of the present utility model.

[0019] In the figure: 1. mold body; 2. mold core; 3. fixed section; 21. straight core; 22. curved core; 11. groove; 4. locking groove; 5. locking block; 6. R angle; 7. connecting ring. DETAILED DESCRIPTION

[0020] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0021] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0022] Example

[0023] Please refer to Figure 1-Figure 4 The utility model proposes a battery cooling tube mold core 2 and a processing method, including a mold body 1, a mold core 2, and a fixed section 3. The mold core 2 includes a straight core 21 and a curved core 22. The ends of the straight core 21 and the curved core 22 are connected to form the mold core 2. A groove 11 is opened on the mold body 1. Both ends of the mold core 2 are installed in the groove 11 through the fixed section 3 to form a mold clamping cavity. In the utility model, the core 2 is composed of a variety of materials to meet the material requirements of different segments of the core 2. A material with relatively high hardness is used in the straight area, and a material with relatively high toughness is used in the curved part. After the entire core 2 is segmented, material savings can be made. At the same time, in terms of efficiency, the straight part needs to be manufactured after the curved part is manufactured to complete the manufacture of a complete core 2, which will affect the start time of the manufacture of the next core 2. Therefore, through separate production and composition, the manufacturing time of some areas of the core 2 can be effectively shortened. The more segments there are, the shorter the manufacturing time of a core 2, thereby saving time. In terms of maintenance and replacement, due to the regionalized segmentation, the damaged part of the core 2 can be replaced, effectively saving the undamaged area and saving costs.

[0024] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4 The ends of the straight core 21 and the curved core 22 are provided with mutually matching locking grooves 4 and locking blocks 5, and the locking blocks 5 of the curved core 22 are matched and fixed to the locking grooves 4 of the straight core 21. The ends of the straight core 21 and the curved core 22 are fixedly connected by welding, or fixed by threaded installation. In the utility model, the locking blocks 5 and the locking grooves 4 are inserted for positioning, and then the welding is performed, and then the entire mold core 2 is manufactured by grinding and filing.

[0025] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4, the connecting end of the curved core 22 and the straight core 21 is provided with an R angle 6. When the R angle 6 at the ends of the curved core 22 and the straight core 21 are welded and fixed, the welding point will not protrude too much from the surface, and the connected surface after welding will also become an inclined angle, so that the force can be decomposed when subjected to force, making the connection area more secure. A connecting ring 7 is sleeved on the locking block 5, and R angles 6 are provided at both ends of the connecting ring 7. The R angle 6 on the connecting ring 7 has the same function, and the connecting ring 7 can not only play a connecting role, but also can destroy the connecting ring 7 when the mold core 2 is damaged to separate the straight core 21 from the curved core 22, and can be reconnected and used after repair, thereby reducing costs.

[0026] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4 The straight core 21 is made of SKD61 or HRC49-53 metal material.

[0027] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4 The bending core 22 is made of ASD3-VIP, HRC43~45 metal material.

[0028] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4 The cross section of the locking block 5 is stepped, and the length of the locking groove 4 is greater than the length of the locking block 5. The stepped shape of the locking block 5 can play a guiding role during the installation process and play a fixing role of the entire device.

[0029] Please refer to Figure 1-Figure 4 A method for processing a battery cooling tube mold core comprises the following steps:

[0030] Step 1: The straight core 21 and the curved core 22 are respectively manufactured by filing, lathe, and electric pulse; the straight core 21 and the curved core 22 can be manufactured by various methods such as stamping and filing, and the main method is that they can be manufactured independently of each other, further shortening the manufacturing time of a mold core 2.

[0031] Step 2: filing and milling the two ends of the straight core 21 into a tubular locking block 5 and a locking groove 4 matching the locking block 5;

[0032] Step 3: Install the locking block 5 corresponding to the locking groove 4, and put the connecting ring 7 on the locking block 5;

[0033] Step 4: The end of the connecting ring 7 is welded to the end of the straight core 21 or the curved core 22, and the welding point is located on the R angle 6;

[0034] Step 5: File and mill the welding part between the connecting ring 7 and the straight core 21 or the curved core 22 to make the straight core 21 or the curved core 22 at the welding part have the same diameter. The cooling pipe made of the straight core 21 and the curved core 22 will form a cavity with the same diameter.

[0035] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4 The outer ring radius of the connecting ring 7 in step 4 is greater than the radius of the straight core 21 or the curved core 22. The radius of the connecting ring 7 is greater than or equal to the radius of the straight core 21, which can prevent the cooling pipe from being discontinuous due to the small radius. The radius of the connecting ring 7 can be reduced by filing.

[0036] In a specific embodiment, refer to Figure 2 , Figure 3 , Figure 4 , the inner ring radius of the connecting ring 7 is equal to the radius of the locking block 5.

[0037] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes within the technical scope disclosed by the present invention according to the technical scheme and the utility model concept of the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A battery cooling tube mold core, characterized in that: The mold body (1) comprises a mold core (2) and a fixing section (3). The mold core (2) comprises a straight core (21) and a curved core (22). The ends of the straight core (21) and the curved core (22) are connected to form the mold core (2). A groove (11) is provided on the mold body (1). The two ends of the mold core (2) are installed in the groove (11) through the fixing section (3) to form a mold clamping cavity.

2. The battery cooling tube mold core according to claim 1, characterized in that: Both ends of the straight core (21) and the curved core (22) are provided with mutually matching locking grooves (4) and locking blocks (5), and the locking blocks (5) of the curved core (22) are matched and fixed to the corresponding locking grooves (4) of the straight core (21).

3. The battery cooling tube mold core according to claim 1, characterized in that: The connection end between the curved core (22) and the straight core (21) is provided with an R angle (6).

4. The battery cooling tube mold core according to claim 2, characterized in that: The locking block (5) is sleeved with a connecting ring (7), and both ends of the connecting ring (7) are provided with R corners (6).

5. The battery cooling tube mold core according to claim 1, characterized in that: The straight core (21) is made of SKD61 or HRC49-53 metal material.

6. The battery cooling tube mold core according to claim 1, characterized in that: The bending core (22) is made of ASD3-VIP, HRC43-45 metal material.

7. The battery cooling tube mold core according to claim 2, characterized in that: The cross section of the locking block (5) is stepped, and the length of the locking groove (4) is greater than the length of the locking block (5).

8. The battery cooling tube mold core according to claim 4, characterized in that: The outer ring radius of the connecting ring (7) is greater than the radius of the straight core (21) or the curved core (22).

9. The battery cooling tube mold core according to claim 4, characterized in that: The inner ring radius of the connecting ring (7) is equal to the radius of the locking block (5).

Citation Information

Cited By

  • Battery cooling pipe mold core and processing method

    CN117921910A