SiC MOSFET device with SJ structure
The SiC MOSFET device with an SJ structure addresses the trade-off between breakdown voltage and on-resistance by using graded doping and shield regions, enhancing performance and power density.
Patent Information
- Application Number
- CN202323439509.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-15
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2033-12-15
AI Technical Summary
Existing SiC MOSFET devices face a trade-off between high breakdown voltage and low on-resistance, leading to increased on-resistance and switching losses, which limits their application and power density.
A SiC MOSFET device with a super junction (SJ) structure, featuring alternately arranged column structures of opposite conductivity types with graded impurity doping concentrations, and shield regions to reduce on-resistance and switching losses.
The SJ structure significantly reduces on-resistance and switching losses, improving the figure of merit (FOM) and voltage resistance, breaking the traditional silicon limit on on-resistance and breakdown voltage relationship.
Smart Images

Figure CN222126535U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of semiconductors, and in particular relates to a SiC MOSFET device with an SJ structure. Background Art
[0002] In the prior art, the basic structure of SiC MOSFET devices is as follows: Figure 1 As shown, it includes an epitaxial region (N-epi) 101, a shield region (P+shield) 102, a base region (P-base) 103, a source region (N+) 104, a gate oxide layer (GOX) 105, a gate polysilicon (Gate Poly) 106, an isolation dielectric layer (Oxide) 107 and a metal layer (Metal) 108.
[0003] SiC MOSFET devices with this structure use a thick low-doped epitaxial layer epi to ensure that the device has sufficient breakdown voltage. The thicker the low-doped epitaxial layer N-epi is, the greater the withstand voltage rating of the SiC MOSFET device is. However, the on-resistance of the SiC MOSFET device increases with the 2.4-2.6 power of the breakdown voltage. Therefore, the thicker the low-doped epitaxial layer N-epi is, the more the on-resistance increases sharply, resulting in a reduction in the current rating of the SiC MOSFET device.
[0004] In order to reduce the on-resistance (Rsdon), the silicon wafer area must be increased. A larger chip area is needed to reduce the on-resistance, and some high-current applications require a larger package size, which increases the cost. The increase in Crss capacitance leads to increased switching losses, and the system power density is difficult to improve, which greatly limits the application of SiC MOSFET devices. Utility Model Content
[0005] The utility model aims to solve the technical problem that the existing SiC MOSFET devices cannot reduce the on-resistance (Rsdon) at a low cost, and aims to provide a SiC MOSFET device with an SJ structure, so as to reduce the minimum specific resistance Rsp (Rdson*Area) and further optimize the switching loss of the SiC MOSFET device, so that the SiC MOSFET device has better FOM performance.
[0006] The SiC MOSFET device comprises an epitaxial layer, on which are arranged column structures of a first conductivity type and column structures of a second conductivity type alternately and at intervals.
[0007] Furthermore, there is a column structure of the first conductivity type between two adjacent column structures of the second conductivity type, and there is a column structure of the second conductivity type between two adjacent column structures of the first conductivity type.
[0008] Furthermore,
[0009] The first impurity doping concentration in the first conductive type column structure gradually increases from top to bottom,
[0010] The second impurity doping concentration in the second conductive type column structure gradually decreases from top to bottom;
[0011] or,
[0012] The first impurity doping concentration in the first conductive type column structure gradually decreases from top to bottom,
[0013] The second impurity doping concentration in the second conductive type column structure gradually increases from top to bottom.
[0014] Furthermore,
[0015] The first conductive type pillar structure has a first pillar upper section, a first pillar middle section and a first pillar lower section;
[0016] The second conductive type pillar structure has a second pillar upper section, a second pillar middle section and a second pillar lower section.
[0017] Furthermore,
[0018] The doping concentration of the upper section of the first column is greater than the doping concentration of the middle section of the first column and greater than the doping concentration of the lower section of the first column;
[0019] The doping concentration of the upper section of the second column is less than the doping concentration of the middle section of the second column, which is less than the doping concentration of the lower section of the second column.
[0020] Furthermore,
[0021] The doping concentration of the upper section of the first column is less than the doping concentration of the middle section of the first column and less than the doping concentration of the lower section of the first column;
[0022] The doping concentration of the upper section of the second column is greater than the doping concentration of the middle section of the second column and greater than the doping concentration of the lower section of the second column.
[0023] Furthermore,
[0024] The first conductivity type is N type, and the second conductivity type is P type;
[0025] or,
[0026] The first conductivity type is P type, and the second conductivity type is N type.
[0027] Furthermore,
[0028] The SiC MOSFET device further comprises:
[0029] at least two spaced-apart L-shaped shielding regions located in the epitaxial layer and directly above the pillar structures of the first conductivity type;
[0030] At least two base regions, each located above the corresponding shielding region;
[0031] At least two source regions are correspondingly located between the shielding region and the base region.
[0032] Furthermore,
[0033] The SiC MOSFET device further comprises:
[0034] A gate oxide layer, located on the upper surface of the epitaxial layer;
[0035] Gate polysilicon, located in the middle of the upper surface of the gate oxide layer;
[0036] An isolation dielectric layer is wrapped around the upper surface of the gate polysilicon.
[0037] Furthermore,
[0038] The SiC MOSFET device further comprises:
[0039] A metal layer is located above the isolation dielectric layer.
[0040] Furthermore,
[0041] The first conductive type pillar structure and the second conductive type pillar structure have the same thickness.
[0042] Furthermore,
[0043] A JEF region is provided between the two base regions.
[0044] Furthermore,
[0045] The base region is a channel.
[0046] Furthermore,
[0047] The length of the channel: the length of the JEFT region is 10:2 to 10:4, preferably 10:3.
[0048] The positive and progressive effects of the utility model are:
[0049] The utility model adds an SJ structure to the SiC MOSFET device, that is, alternately arranges pillar structures of opposite conductivity types in the epitaxial layer. This design can significantly reduce the on-resistance (Rdson) and simultaneously reduce Qg, thereby reducing FOM (Rdson*Qg), thereby improving the performance of the SiC MOSFET device. BRIEF DESCRIPTION OF THE DRAWINGS
[0050] The disclosure of the present invention will become more apparent with reference to the accompanying drawings. It should be understood that these drawings are only for illustrative purposes and are not intended to limit the scope of protection of the present invention. In the drawings:
[0051] Figure 1 A schematic cross-sectional view of a SiC MOSFET device in the prior art;
[0052] Figure 2 A cross-sectional schematic diagram of the utility model;
[0053] Figure 3 The utility model is a process flow chart. DETAILED DESCRIPTION
[0054] The following is an explanation of the implementation of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific implementations, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0055] It should be noted that the following embodiments and features therein may be combined with each other if there is no conflict.
[0056] Reference Figure 2 The utility model provides a SiC MOSFET device with an SJ structure. The SiC MOSFET device has an epitaxial layer, and the epitaxial layer has a first conductive type column structure and a second conductive type column structure that are alternately arranged at intervals.
[0057] That is, there is a first conductive type column structure between two adjacent second conductive type column structures, and there is a second conductive type column structure between two adjacent first conductive type column structures. The first conductive type column structure and the second conductive type column structure have the same thickness.
[0058] Wherein, when the first conductivity type is N type, the second conductivity type is P type. When the first conductivity type is P type, the second conductivity type is N type.
[0059] Among them, the first impurity doping concentration in the column structure of the first conductive type gradually increases from top to bottom, and the second impurity doping concentration in the column structure of the second conductive type gradually decreases from top to bottom; or, the first impurity doping concentration in the column structure of the first conductive type gradually decreases from top to bottom, and the second impurity doping concentration in the column structure of the second conductive type gradually increases from top to bottom.
[0060] In one example, the epitaxial layer is of N type, and the column structure inserted into the epitaxial layer is a P type column. The P type column has several sections, and the N type column also has several sections.
[0061] Specifically, the first conductive type column structure has a first column upper section, a first column middle section and a first column lower section, and the second conductive type column structure correspondingly has a second column upper section, a second column middle section and a second column lower section.
[0062] In one example, the doping concentration of the upper section of the first column is greater than the doping concentration of the middle section of the first column and greater than the doping concentration of the lower section of the first column, and the doping concentration of the upper section of the second column is less than the doping concentration of the middle section of the second column and less than the doping concentration of the lower section of the second column. In another example, the doping concentration of the upper section of the first column is less than the doping concentration of the middle section of the first column and less than the doping concentration of the lower section of the first column; the doping concentration of the upper section of the second column is greater than the doping concentration of the middle section of the second column and greater than the doping concentration of the lower section of the second column.
[0063] In one example, the first conductivity type is P-type and the second conductivity type is N-type, and the column structure is a P-type column 201 and an N-type column 202 accordingly.
[0064] The doping concentration of the P-type impurities in each section of the P-type column 201 is uniform, and the doping concentration in each section decreases from top to bottom. Correspondingly, the doping concentration of the N-type impurities in each section of the N-type column 202 is also uniform, and the doping concentration in each section increases from top to bottom.
[0065] Specifically, taking a SiC MOSFET device with a withstand voltage of 6000V as an example, both the P-type column and the N-type column have three sections, and the P-type column 2011 is composed of a P-column upper section 2013, a P-column middle section 2012, and a P-column lower section 2011 from top to bottom. The N-type column 202 is composed of an N-column upper section 2023, an N-column middle section 2022, and an N-column lower section 2021 from top to bottom. More specifically, the doping concentration of the P-column upper section 2013 is 2.0E+16 / cm 3 The doping concentration of the middle section of the P column 2012 is 1.0E+16 / cm 3 The doping concentration of the lower section of the P column 2011 is 1.0E+15 / cm 3 The doping concentration of the upper part of the N column 2013 is 1.0E+15 / cm 3 The doping concentration of the middle section 2012 of the N column is 1.0E+16 / cm3 The doping concentration of the lower section of the N column 2011 is 2.0E+16 / cm 3 .
[0066] This doping concentration setting results in very small depletion charge balance deviation, good voltage blocking capability retention, good device avalanche capability and unit consistency, and lower switching loss.
[0067] In an example, the SiC MOSFET device further includes at least two shield regions (P+shield) 203 , at least two base regions (P-base) 204 , and at least two source regions (N+) 205 .
[0068] The shielding region (P+shield) 203 is located in the epitaxial layer (N-epi) 211 and directly above the P-type pillar 201 structure. The base region (P-base) 204 is located above the shielding region (P+shield) 203. The source region (N+) 205 is located between the shielding region (P+shield) 203 and the base region (P-base) 204.
[0069] In one example, the SiC MOSFET device further includes a gate oxide dielectric layer (GOX) 206 , a gate polysilicon (GatePoly) 207 and an isolation dielectric layer (Oxide) 208 .
[0070] The gate oxide dielectric layer (GOX) 206 is located on the upper surface of the epitaxial layer (N-epi) 211. The gate polysilicon (GatePoly) 207 is located in the middle of the upper surface of the gate oxide dielectric layer (GOX) 206. The isolation dielectric layer (Oxide) 208 is wrapped around the upper surface of the gate polysilicon (GatePoly) 207.
[0071] In one example, the SiC MOSFET device further includes a metal layer (Metal) 209 , and the metal layer (Metal) 209 is located above the isolation dielectric layer (Oxide) 208 .
[0072] In one example, a JEFT region 210 is provided between two shield regions (P+shield) 203 above adjacent P-type pillars 201, and a base region (P-base) 204 between the JEFT region 210 and the source region (N+) becomes a channel after forming an inversion layer. Preferably, the length A of the channel: the length B of the JEFT region is 10:2 to 10:4, preferably 10:3, the length A of the channel is preferably 1um, and the length B of the JEFT region is preferably 0.3um.
[0073] Working principle: In this super junction structure, the N-type column 202 for vertical conduction is sandwiched between the two P-type columns 201. In the horizontal direction, PN junctions are formed on both sides of the N-type column 202 and the P-type column 201, and the base region (P-base) 204 forms an inversion layer to generate a channel, which connects the source region (N+) 205 and the JFET region 209 and then connects with the N-type column 202.
[0074] When the SiC MOSFET device is turned off, the P-type column 201 and the N-type column 202 form a reverse biased PN junction, and depletion layers are formed on both sides of the PN junction to establish a horizontal lateral electric field, which is a rectangular electric field. As the depletion layer increases, the lateral horizontal electric field also increases. As the external reverse bias voltage increases, the width of the depletion layer in the N-type column 202 and the P-type column 201 continues to increase until the vertical conductive N region and the entire P-type column are completely depleted and all become depletion layers. The lateral rectangular electric field of the depletion layer reaches a very high amplitude and has a very high breakdown voltage. Compared with the SiC MOSFET device without SJ structure in the prior art, this undoubtedly improves the degree of voltage resistance of the device. Since the N-type column and the P-type column are completely depleted, even if the doping concentration in the column area is extremely high, it will not affect the voltage resistance of the device. The high-concentration doped column can reduce the on-resistance (Rdson), breaking the "silicon limit" in which the on-resistance of traditional power devices is limited by the breakdown voltage, so that the on-resistance and the breakdown voltage reach an approximately linear relationship. On the other hand, the non-uniformly doped pillar region can enable the device to more quickly extract free charges from the pillar region when it is turned off, thereby reducing switching losses and significantly improving device performance.
[0075] Reference Figure 3 The following steps can be used to manufacture a SiC MOSFET device with an SJ structure according to the present invention:
[0076] Step S1 : using a multi-epitaxial process to manufacture a P-type pillar (P pillar) 201 and an N-type pillar (N pillar) 202 , and then growing an epitaxial layer (N-Epi) 211 on the P-type pillar (P pillar) and the N-type pillar (N pillar).
[0077] Step S2, implant and diffuse the shielding region (P+shield) 203 and the base region (P-base) 204 on the epitaxial layer (N-Epi) 211. The Al implantation concentration of the diffusion shielding region (P+shield) 203 is 1.0E+19 / cm 3 The AL implant concentration of the base region (P-base) 204 is 1E+17 / cm 3 .
[0078] Step S3, implanting and diffusing the source region (N+) 205 between the shield region (P+shield) 203 and the base region (P-base) 204. The implantation concentration of the source region (N+) 205N is 1.0E+19 / cm 3 .
[0079] Step S4, growing and etching back a gate oxide layer (GOX) 206 on the P+ shield region 203, the base region (P-base) 204 and the source region (N+) 205. The thickness of the gate oxide layer (GOX) 206 is 500 Å.
[0080] Step S5, growing and etching back gate polysilicon (Gate Poly) 207 on the gate oxide layer (GOX).
[0081] Step S6 , growing an isolation dielectric layer (Oxide) 208 on the gate polysilicon (Gate Poly) 207 .
[0082] Step S7 , growing a metal layer (Metal) 209 on top of the growing isolation dielectric layer (Oxide) 208 .
[0083] The utility model is described in detail above in conjunction with the embodiments of the drawings. A person skilled in the art can make various variations of the utility model according to the above description. Therefore, some details in the embodiments should not constitute a limitation of the utility model, and the utility model shall be protected within the scope defined by the attached claims.
Claims
1. A SiC MOSFET device with an SJ structure, characterized in that: The SiC MOSFET device comprises an epitaxial layer, on which are arranged column structures of a first conductivity type and column structures of a second conductivity type alternately and at intervals.
2. The SiC MOSFET device with SJ structure according to claim 1, characterized in that: There is a first conductive type column structure between two adjacent second conductive type column structures, and there is a second conductive type column structure between two adjacent first conductive type column structures.
3. The SiC MOSFET device with SJ structure according to claim 1, characterized in that: The first conductive type pillar structure has a first pillar upper section, a first pillar middle section and a first pillar lower section; The second conductive type pillar structure has a second pillar upper section, a second pillar middle section and a second pillar lower section.
4. The SiC MOSFET device with SJ structure according to claim 1, characterized in that: The first conductivity type is N type, and the second conductivity type is P type; or, The first conductivity type is P type, and the second conductivity type is N type.
5. The SiC MOSFET device with SJ structure according to claim 4, characterized in that: The SiC MOSFET device further comprises: at least two spaced-apart L-shaped shielding regions located in the epitaxial layer and directly above the pillar structures of the first conductivity type; At least two base regions, each located above the corresponding shielding region; At least two source regions are correspondingly located between the shielding region and the base region.
6. The SiC MOSFET device with SJ structure according to claim 5, characterized in that: The SiC MOSFET device further comprises: A gate oxide layer, located on the upper surface of the epitaxial layer; Gate polysilicon, located in the middle of the upper surface of the gate oxide layer; An isolation dielectric layer is wrapped around the upper surface of the gate polysilicon.
7. The SiC MOSFET device with SJ structure according to claim 6, characterized in that: The SiC MOSFET device further comprises: The metal layer is located above the isolation dielectric layer.
8. The SiC MOSFET device with SJ structure according to claim 1, characterized in that: The first conductive type pillar structure and the second conductive type pillar structure have the same thickness.
9. The SiC MOSFET device with SJ structure according to claim 5, characterized in that: A JEF region is provided between the two base regions.
10. The SiC MOSFET device with SJ structure according to claim 9, characterized in that: The base region is a channel.
11. The SiC MOSFET device with SJ structure according to claim 10, characterized in that: The length of the channel: the length of the JEFT region is 10:2~10:
4.