Gap machining tool for battery corner
By setting insulating film components in the corner area of the lithium-ion battery to build gaps, the lithium-ion battery is solved, extending the battery life and improving safety.
Patent Information
- Application Number
- CN202323637316.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2033-12-29
AI Technical Summary
The corner area of lithium-ion batteries is prone to lithium extraction problems after long-term circulation, which affects the service life and may cause safety hazards.
Set up insulating film components at the corners of the lithium-ion battery to build gaps, provide space to store electrolyte, improve interface wetting, and reduce the impact of lithium evolution problems.
Through the gap setting, the battery life is extended, ensuring that the battery works normally in the later stage of the cycle, and avoiding battery performance degradation and safety risks caused by lithium-ion.
Smart Images

Figure CN222126637U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of batteries, in particular to a gap processing tool for battery corners. Background Art
[0002] Lithium-ion batteries are widely used in various digital products and mobile devices due to their advantages such as high energy density, low self-discharge, wide operating temperature range and no environmental pollution.
[0003] The battery cell of a lithium-ion battery includes a first separator, an anode sheet, a second separator, and a cathode sheet. The battery cell in which the pole sheets and separators are stacked in sequence, wound into shape, and hot-pressed to shape is also called a roll core. The roll core is immersed in the electrolyte. During the cyclic charge and discharge process, the electrolyte will be gradually consumed on the one hand, and the pole sheet will continue to expand on the other hand. Therefore, after long-term circulation, the roll core will have abnormal conditions such as lithium deposition, which will affect the service life and may even cause safety problems.
[0004] Taking the square wound lithium-ion battery as an example, the core has multiple straight areas and multiple corner areas arranged alternately in the winding direction. After winding, the straight areas form the straight part of the core, and the corner areas form the corners of the core. Due to the differences in gaps, stresses, etc. between the straight parts and the corners, the lithium plating problem is particularly serious at the corners. Utility Model Content
[0005] To this end, the technical problem to be solved by the utility model is to overcome the problem of lithium plating in the corner area of the existing square lithium battery which affects its service life, and to provide a gap processing tool for the corner of the battery. By arranging an insulating film component at the corner of the winding core to construct a gap, space is provided to store electrolyte, improve interface wettability, reduce the impact of the lithium plating problem on the corner of the winding core, and extend the battery life.
[0006] The utility model provides a gap processing tool for battery corners, which is used to construct gaps at the first corner part and the second corner part of the winding core respectively; the gap processing tool for the battery corners includes a first insulating film component, a second insulating film component, a third insulating film component and a fourth insulating film component, the first insulating film component has a first rolling-in portion for rolling up the first corner part and a first handle portion connected to the first rolling-in portion, the second insulating film component has a second rolling-in portion for rolling up the first corner part and a second handle portion connected to the second rolling-in portion, wherein the first rolling-in portion and the second rolling-in portion are arranged opposite to and spaced apart along a first direction, and the first direction is the axial direction of the winding core; the third insulating film component has a third rolling-in portion for rolling up the second corner part and a third handle portion connected to the third rolling-in portion, and the fourth insulating film component has a fourth rolling-in portion for rolling up the second corner part and a fourth handle portion connected to the fourth rolling-in portion, wherein the third rolling-in portion and the fourth rolling-in portion are arranged opposite to and spaced apart along the first direction.
[0007] In one embodiment of the present invention, in the first direction, the length of the first rolling-in portion, the length of the second rolling-in portion, the length of the third rolling-in portion and the length of the fourth rolling-in portion are all configured to be 30%-49% of the length of the winding core.
[0008] In an embodiment of the present invention, the first insulating film component, the second insulating film component, the third insulating film component and the fourth insulating film component are all integrally formed structures.
[0009] In one embodiment of the present invention, in the first direction, the length of the first insulating film component, the length of the second insulating film component, the length of the third insulating film component and the length of the fourth insulating film component are all configured to be 50%-100% of the length of the winding core.
[0010] In one embodiment of the present invention, the thickness of the first rolling-in portion, the thickness of the second rolling-in portion, the thickness of the third rolling-in portion and the thickness of the fourth rolling-in portion are all 0.1 mm-5 mm.
[0011] In one embodiment of the present invention, the first insulating film component, the second insulating film component, the third insulating film component and the fourth insulating film component are all arranged between the first isolation film and the anode sheet of the winding core, or between the anode sheet and the second isolation film of the winding core, or between the second isolation film and the cathode sheet of the winding core, or between the cathode sheet and the first isolation film.
[0012] In one embodiment of the present invention, when the first insulating film component and the second insulating film component are both located between the Nth corner and the N+1th corner of the first corner portion, the widths of the first insulating film component and the second insulating film component are both configured to be 95% of the arc length of the N+1th corner, wherein N≥1, and N is an integer; when the third insulating film component and the fourth insulating film component are both located between the Mth corner and the M+1th corner of the second corner portion, the widths of the third insulating film component and the fourth insulating film component are both configured to be 95% of the arc length of the M+1th corner, wherein M≥1, and M is an integer.
[0013] In one embodiment of the present invention, the center line of the first insulating film part in the width direction, the center line of the second insulating film part in the width direction, the center line of the third insulating film part in the width direction and the center line of the fourth insulating film part in the width direction are all configured to be in the same plane as the axis of the winding core, and the plane is parallel to the straight part of the winding core.
[0014] In one embodiment of the utility model, a plurality of the first insulating film component, the second insulating film component, the third insulating film component and the fourth insulating film component are each provided; the spacing between any two adjacent first insulating film components, the spacing between any two adjacent second insulating film components, the spacing between any two adjacent third insulating film components and the spacing between any two adjacent fourth insulating film components are configured as n×D, wherein D is the sum of the thicknesses of a cathode sheet, an anode sheet, a first isolation film and a second isolation film; n≥1, and n is an integer.
[0015] In one embodiment of the present invention, the first insulating film member, the second insulating film member, the third insulating film member and the fourth insulating film member are organic insulating films or inorganic insulating films.
[0016] The above technical solution of the utility model has the following advantages compared with the prior art:
[0017] The gap processing tooling for the battery corners described in the utility model, during the production process of the core, sets the first rolling part of the first insulating film component and the second rolling part of the second insulating film component at the first corner of the corresponding core to construct a gap, and sets the third rolling part of the third insulating film component and the fourth rolling part of the fourth insulating film component at the second corner of the corresponding core to construct a gap. By setting the gap, there is enough space at the corresponding corner to store electrolyte and ensure the normal operation of the core in the later stage of the cycle, which can improve the interface wettability, reduce the impact of lithium plating on the corner of the core, and extend the service life of the battery. At the same time, since the first rolling part and the second rolling part are arranged relative to each other and spaced along the first direction, and the third rolling part and the fourth rolling part are arranged relative to each other and spaced along the first direction, it can ensure the successful construction of the gap and avoid the gap size difference caused by the overlapping of the rolling parts, and the problem of difficulty in taking out due to the friction between the overlapping rolling parts. In addition, since the first handle portion of the first insulating film component and the second handle portion of the second insulating film component are both retained outside the winding core, and the third handle portion of the third insulating film component and the fourth handle portion of the fourth insulating film component are both retained outside the winding core, it is possible to quickly remove the corresponding insulating film component from the winding core through the corresponding handle portion after the winding core is formed, thereby improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to make the content of the utility model easier to understand, the utility model is further described in detail according to the specific embodiments of the utility model in combination with the accompanying drawings, wherein:
[0019] Figure 1 It is a schematic diagram of the structure of the winding core;
[0020] Figure 2 This is a schematic structural diagram of the first insulating film component in a preferred embodiment of the utility model;
[0021] Figure 3 This is one of the first perspective structural schematic diagrams of the gap processing tooling in the preferred embodiment of the utility model;
[0022] Figure 4 It is a second perspective structural schematic diagram of the gap processing tooling in the preferred embodiment of the utility model;
[0023] Figure 5 Schematic diagram of the gap structure of the winding core;
[0024] Figure 6 This is a schematic diagram of the size structure of the first insulating film component in the preferred embodiment of the utility model;
[0025] Figure 7 This is one of the schematic diagrams of the location of the first insulating film component in the preferred embodiment of the utility model;
[0026] Figure 8 This is the second schematic diagram of the location of the first insulating film component in the preferred embodiment of the utility model;
[0027] Fig. 9 This is the third schematic diagram of the location of the first insulating film component in the preferred embodiment of the utility model;
[0028] Fig.10 This is the fourth schematic diagram of the location of the first insulating film component in the preferred embodiment of the utility model;
[0029] Fig.11 This is the second first-view structural schematic diagram of the gap processing tooling in the preferred embodiment of the utility model;
[0030] Fig.12 This is the third first-view structural schematic diagram of the gap processing tooling in the preferred embodiment of the utility model.
[0031] Explanation of the reference numerals in the specification: D1, first direction; 10, winding core; 11, first corner portion; 12, second corner portion; 13, gap; 141, first isolation film; 142, anode sheet; 143, second isolation film; 144, cathode sheet; 20, first insulating film component; 21, first rolling-in portion; 22, first handle portion; 30, second insulating film component; 31, second rolling-in portion; 32, second handle portion; 40, third insulating film component; 41, third rolling-in portion; 42, third handle portion; 50, fourth insulating film component; 51, fourth rolling-in portion; 52, fourth handle portion. DETAILED DESCRIPTION
[0032] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.
[0033] Reference Figure 1 As shown, the winding core 10 includes a first corner portion 11 , a second corner portion 12 , and a straight portion connecting the first corner portion 11 and the second corner portion 12 .
[0034] Reference Figure 2 , Figure 3 , Figure 4 and Figure 5As shown, the utility model discloses a gap processing tool for battery corners, which is used to construct a gap 13 at a first corner portion 11 and a second corner portion 12 of a winding core 10. The gap processing tool for battery corners includes a first insulating film component 20, a second insulating film component 30, a third insulating film component 40 and a fourth insulating film component 50. The first insulating film component 20 has a first rolling-in portion 21 for rolling up the first corner portion 11 and a first handle portion 22 connected to the first rolling-in portion 21, the second insulating film component 30 has a second rolling-in portion 31 for rolling up the first corner portion 11 and a second handle portion 32 connected to the second rolling-in portion 31, wherein the first rolling-in portion 21 and the second rolling-in portion 31 are opposite to and spaced apart along a first direction D1, and the first direction D1 is the axial direction of the winding core 10; the third insulating film component 40 has a third rolling-in portion 41 for rolling up the second corner portion 12 and a third handle portion 42 connected to the third rolling-in portion 41, the fourth insulating film component 50 has a fourth rolling-in portion 51 for rolling up the second corner portion 12 and a fourth handle portion 52 connected to the fourth rolling-in portion 51, wherein the third rolling-in portion 41 and the fourth rolling-in portion 51 are opposite to and spaced apart along the first direction D1.
[0035] The gap processing tooling for the battery corner described in the utility model, during the production process of the core 10, sets the first rolling-in portion 21 of the first insulating film component 20 and the second rolling-in portion 31 of the second insulating film component 30 at the first corner portion 11 of the corresponding core 10 to construct the gap 13, and sets the third rolling-in portion 41 of the third insulating film component 40 and the fourth rolling-in portion 51 of the fourth insulating film component 50 at the second corner portion 12 of the corresponding core 10 to construct the gap 13. By setting the gap 13, there can be enough space at the corresponding corner portion to store electrolyte and ensure the normal operation of the battery cell in the later stage of the cycle, which can improve the interface wettability, reduce the influence of lithium plating on the corner portion of the core 10, and extend the service life of the battery. At the same time, since the first rolling-in portion 21 and the second rolling-in portion 31 are arranged oppositely and spaced along the first direction D1, and the third rolling-in portion 41 and the fourth rolling-in portion 51 are arranged oppositely and spaced along the first direction D1, it is possible to ensure the successful construction of the gap 13, and avoid the size difference of the gap 13 caused by the overlapping of the rolling-in portions, and the problem of difficulty in taking out due to the friction between the overlapping rolling-in portions. In addition, since the first handle portion 22 of the first insulating film component 20 and the second handle portion 32 of the second insulating film component 30 are both left outside the winding core 10, and the third handle portion 42 of the third insulating film component 40 and the fourth handle portion 52 of the fourth insulating film component 50 are both left outside the winding core 10, it is convenient to quickly take out the corresponding insulating film component from the winding core 10 through the corresponding handle portion after the winding core 10 is formed, so as to improve production efficiency.
[0036] Reference Figure 2 and Figure 6As shown, in the battery corner gap processing tooling of the utility model, in some embodiments, in the first direction D1, the length of the first rolling portion 21, the length of the second rolling portion 31, the length of the third rolling portion 41 and the length of the fourth rolling portion 51 are all L 11 , the length of the winding core 10 is recorded as L 20 Among them, the length of the rolled-in part is L 11 The length L of the winding core 10 is configured 20 The specific length L of the rolling part can be selected according to actual needs. 11 , such as the length L of the winding core 10 20 30%, 35%, 40%, 45%, 49%, etc. By 11 Further definition, under the premise that the first winding-in portion 21 and the second winding-in portion 31 can be arranged relative to and spaced apart, and the third winding-in portion 41 and the fourth winding-in portion 51 can be arranged relative to and spaced apart, after the core 10 is wound, the staff or the device can easily remove the insulating film component from the core 10 through the handle portion, which can not only ensure the processing efficiency, but also avoid damage to the core when taking out the winding-in portion due to the excessive winding length.
[0037] Reference Figure 2 As shown, in the gap processing tooling for the battery corner described in the utility model, in some embodiments, the first insulating film component 20, the second insulating film component 30, the third insulating film component 40 and the fourth insulating film component 50 are all integrally formed structures. The insulating film component of the integrally formed structure can effectively ensure its own structural strength and avoid the situation where the insulating film component is disconnected during the removal process and remains in the winding core 10. It should be noted that in some other embodiments, the connection between the corresponding handle part and the rolling part can also be achieved by bonding, clamping, etc., and it is not limited to integral molding, as long as the rolling part can be taken out of the winding core 10 through the handle part.
[0038] Reference Figure 2 and Figure 6 As shown, in the battery corner gap processing tooling of the utility model, in some embodiments, in the first direction D1, the length of the first insulating film component 20, the length of the second insulating film component 30, the length of the third insulating film component 40 and the length of the fourth insulating film component 50 are all recorded as L 10 . The length L of the insulating film part 10 The length L of the winding core 10 is configured 20 The length L of the corresponding insulating film component can be set according to actual needs. 10 , such as 50%, 60%, 80%, 100%, etc. By 11It is further defined that, under the premise of ensuring successful construction of the gap 13, the handle portion remaining outside the core 10 has a certain length, so that subsequent staff or equipment can easily remove the insulating film component from the core 10 through the handle portion to ensure processing efficiency.
[0039] Reference Figure 2 As shown, in the gap processing tooling for the battery corners described in the utility model, in some embodiments, the thickness of the first rolling part 21, the thickness of the second rolling part 31, the thickness of the third rolling part 41 and the thickness of the fourth rolling part 51 are all recorded as D. The thickness D of the rolling part is set to 0.1mm-5mm. By further limiting and ensuring the size of the gap 13 formed by the thickness D of the rolling part, the setting requirements of the gap 13 of different needs are met, so as to increase the storage capacity of the electrolyte at the position of the gap 13 through gaps 13 of different sizes, thereby improving the interface wettability and ensuring that the corresponding corner part has sufficient electrolyte in the later stage of the cycle, thereby extending the service life of the battery. According to actual needs, sizes such as 0.1mm, 0.2mm, 0.3mm, 1mm, 3mm, 5mm, etc. can be selected.
[0040] In some embodiments, the gap processing tool for the battery corner described in the utility model can select the specific setting positions of the first insulating film component 20, the second insulating film component 30, the third insulating film component 40 and the fourth insulating film component 50. In the prior art, the winding core 10 generally includes a first isolation film 141, an anode sheet 142, a second isolation film 143 and a cathode sheet 144 stacked in sequence. Based on this, referring to Figure 7 As shown, the first insulating film member 20, the second insulating film member 30, the third insulating film member 40 and the fourth insulating film member 50 can be arranged between the first separator 141 and the anode sheet 142 of the winding core 10. Figure 8 As shown, the first insulating film member 20, the second insulating film member 30, the third insulating film member 40 and the fourth insulating film member 50 can be arranged between the anode sheet 142 and the second separator 143 of the winding core 10. Fig. 9 As shown, the first insulating film member 20, the second insulating film member 30, the third insulating film member 40 and the fourth insulating film member 50 can be arranged between the second isolation film 143 and the cathode sheet 144 of the winding core 10. Fig.10As shown, the first insulating film component 20, the second insulating film component 30, the third insulating film component 40 and the fourth insulating film component 50 can be arranged between the cathode sheet 144 and the first separator 141. By arranging the first insulating film component 20, the second insulating film component 30, the third insulating film component 40 and the fourth insulating film component 50 at different positions of the winding core 10, the requirements of different winding cores 10 for gaps 13 at different positions can be met, so that the storage amount of the electrolyte at the position of the gap 13 is increased through the gaps 13 at different positions, thereby improving the interface wettability and ensuring that the corresponding corner portion has sufficient electrolyte in the later stage of the cycle, thereby extending the service life of the battery.
[0041] Reference Figure 2 and Figure 6 As shown, in some embodiments of the gap processing tooling for battery corners described in the utility model, when the first insulating film component 20 and the second insulating film component 30 are both located between the Nth corner and the N+1th corner of the first corner portion 11, the widths of the first insulating film component 20 and the second insulating film component 30 are both configured to be 95% of the arc length of the N+1th corner, wherein N≥1, and N is an integer; when the third insulating film component 40 and the fourth insulating film component 50 are both located between the Mth corner and the M+1th corner of the second corner portion 12, the widths of the third insulating film component 40 and the fourth insulating film component 50 are both configured to be 95% of the arc length of the M+1th corner, wherein M≥1, and M is an integer. Taking the first insulating film component 20 as an example, the width of the first insulating film component 20 is denoted as L 12 , let the arc length of the N+1th corner of the first corner portion 11 be L 21 , then L 12 =0.95×L 21 By further limiting the widths of the first insulating film component 20, the second insulating film component 30, the third insulating film component 40 and the fourth insulating film component 50, the position of the gap 13 can be constructed more flexibly, thereby improving the interface wettability and ensuring that the corresponding corner has sufficient electrolyte in the later stage of the cycle, thereby extending the service life of the battery.
[0042] Reference Figure 6 As shown, in the gap processing tooling for battery corners described in the present invention, in some embodiments, the center line of the first insulating film component 20 in the width direction, the center line of the second insulating film component 30 in the width direction, the center line of the third insulating film component 40 in the width direction, and the center line of the fourth insulating film component 50 in the width direction are all configured to be in the same plane as the axis of the core 10, and the plane is parallel to the straight portion of the core 10.
[0043] Reference Fig.11 and Fig.12As shown, in some embodiments, the gap processing tooling of the battery corner described in the utility model is provided with multiple first insulating film components 20, second insulating film components 30, third insulating film components 40 and fourth insulating film components 50, so as to construct gaps 13 at multiple locations of the first corner portion 11 and the second corner portion 12, so as to increase the storage capacity of the electrolyte at the position of the gap 13, thereby improving the interface wettability and ensuring that the corresponding corner portion has sufficient electrolyte in the later stage of the cycle, thereby extending the service life of the battery. Specifically, the spacing between any two adjacent first insulating film components 20, the spacing between any two adjacent second insulating film components 30, the spacing between any two adjacent third insulating film components 40 and the spacing between any two adjacent fourth insulating film components 50 are configured as n×D, wherein D is the sum of the thickness of a cathode sheet 144, an anode sheet 142, a first isolation film 141 and a second isolation film 143; n≥1, n is an integer. The value of n can be selected according to different needs, for example, 1, 2, 3, 4, etc.
[0044] In some embodiments of the gap processing tool for battery corners described in the utility model, the first insulating film component 20, the second insulating film component 30, the third insulating film component 40 and the fourth insulating film component 50 are organic insulating films or inorganic insulating films. Specifically, organic insulating films such as polyethylene film, polytetrafluoroethylene film, polyimide film, polyvinylidene fluoride, etc. can be selected according to actual needs, or inorganic insulating films such as silicon oxide, silicon nitride, aluminum oxide, aluminum nitride, etc. can be selected to meet different insulation requirements.
[0045] The gap processing tooling for the battery corner described in the utility model, during the production process of the core 10, sets the first rolling-in portion 21 of the first insulating film component 20 and the second rolling-in portion 31 of the second insulating film component 30 at the first corner portion 11 of the corresponding core 10 to construct the gap 13, and sets the third rolling-in portion 41 of the third insulating film component 40 and the fourth rolling-in portion 51 of the fourth insulating film component 50 at the second corner portion 12 of the corresponding core 10 to construct the gap 13. By setting the gap 13, there can be enough space at the corresponding corner portion to store electrolyte and ensure the normal operation of the battery cell in the later stage of the cycle, which can improve the interface wettability, reduce the influence of lithium plating on the corner portion of the core 10, and extend the service life of the battery. At the same time, since the first rolling part 21 and the second rolling part 31 are arranged oppositely and spaced along the first direction D1, and the third rolling part 41 and the fourth rolling part 51 are arranged oppositely and spaced along the first direction D1, it is possible to ensure the successful construction of the gap 13, and avoid the size difference of the gap 13 caused by the overlapping of the rolling parts, and the problem of difficulty in taking out due to the friction between the overlapping rolling parts. In addition, since the first handle part 22 of the first insulating film part 20 and the second handle part 32 of the second insulating film part 30 are both left outside the core 10, the third handle part 42 of the third insulating film part 40 and the fourth handle part 52 of the fourth insulating film part 50 are both left outside the core 10, it is convenient to quickly take out the corresponding insulating film part from the core 10 through the corresponding handle part after the core 10 is formed, so as to improve production efficiency. On this basis, by further limiting the length and thickness of the rolling part, the length of the entire insulating film part, and the setting position of the insulating film part, it is effectively ensured that the gap 13 can meet the performance requirements of different cores 10.
[0046] Obviously, the above embodiments are merely examples for the purpose of clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived from these are still within the scope of protection of the invention of the utility model.
Claims
1. A battery corner gap processing tool, used for constructing a gap (13) at a first corner (11) and a second corner (12) of a winding core (10), characterized in that: The gap processing tool for the battery corner comprises a first insulating film component (20), a second insulating film component (30), a third insulating film component (40) and a fourth insulating film component (50), wherein the first insulating film component (20) has a first rolling-in portion (21) for rolling up the first corner portion (11) and a first handle portion (22) connected to the first rolling-in portion (21), and the second insulating film component (30) has a second rolling-in portion (31) for rolling up the first corner portion (11) and a second handle portion (32) connected to the second rolling-in portion (31), wherein the first rolling-in portion (21) and the second rolling-in portion (32) are 1) are arranged opposite to and spaced apart along a first direction (D1), wherein the first direction (D1) is the axial direction of the winding core (10); the third insulating film component (40) has a third rolling-in portion (41) for rolling up the second corner portion (12) and a third handle portion (42) connected to the third rolling-in portion (41); the fourth insulating film component (50) has a fourth rolling-in portion (51) for rolling up the second corner portion (12) and a fourth handle portion (52) connected to the fourth rolling-in portion (51), wherein the third rolling-in portion (41) and the fourth rolling-in portion (51) are arranged opposite to and spaced apart along the first direction (D1).
2. The battery corner gap processing tool according to claim 1, characterized in that: In the first direction (D1), the length of the first rolling-in portion (21), the length of the second rolling-in portion (31), the length of the third rolling-in portion (41) and the length of the fourth rolling-in portion (51) are all configured to be 30%-49% of the length of the winding core (10).
3. The battery corner gap processing tool according to claim 1, characterized in that: The first insulating film component (20), the second insulating film component (30), the third insulating film component (40) and the fourth insulating film component (50) are all integrally formed structures.
4. The battery corner gap processing tool according to claim 1, characterized in that: In the first direction (D1), the length of the first insulating film component (20), the length of the second insulating film component (30), the length of the third insulating film component (40) and the length of the fourth insulating film component (50) are all configured to be 50%-100% of the length of the winding core (10).
5. The battery corner gap processing tool according to claim 1, characterized in that: The thickness of the first rolling-in portion (21), the thickness of the second rolling-in portion (31), the thickness of the third rolling-in portion (41) and the thickness of the fourth rolling-in portion (51) are all in the range of 0.1 mm to 5 mm.
6. The battery corner gap processing tool according to any one of claims 1 to 5, characterized in that: The first insulating film component (20), the second insulating film component (30), the third insulating film component (40) and the fourth insulating film component (50) are all arranged between the first isolation film (141) and the anode sheet (142) of the winding core (10), or between the anode sheet (142) and the second isolation film (143) of the winding core (10), or between the second isolation film (143) and the cathode sheet (144) of the winding core (10), or between the cathode sheet (144) and the first isolation film (141).
7. The battery corner gap processing tool according to claim 6, characterized in that: When the first insulating film component (20) and the second insulating film component (30) are both located between the Nth corner and the N+1th corner of the first corner portion (11), the widths of the first insulating film component (20) and the second insulating film component (30) are both configured to be 95% of the arc length of the N+1th corner, wherein N≥1, and N is an integer; when the third insulating film component (40) and the fourth insulating film component (50) are both located between the Mth corner and the M+1th corner of the second corner portion (12), the widths of the third insulating film component (40) and the widths of the fourth insulating film component (50) are both configured to be 95% of the arc length of the M+1th corner, wherein M≥1, and M is an integer.
8. The battery corner gap processing tool according to claim 6, characterized in that: The center line of the first insulating film component (20) in the width direction, the center line of the second insulating film component (30) in the width direction, the center line of the third insulating film component (40) in the width direction, and the center line of the fourth insulating film component (50) in the width direction are all configured to be in the same plane as the axis of the winding core (10), and the plane is parallel to the straight part of the winding core (10).
9. The battery corner gap processing tool according to claim 6, characterized in that: The first insulating film component (20), the second insulating film component (30), the third insulating film component (40) and the fourth insulating film component (50) are each provided in plurality; the spacing between any two adjacent first insulating film components (20), the spacing between any two adjacent second insulating film components (30), the spacing between any two adjacent third insulating film components (40) and the spacing between any two adjacent fourth insulating film components (50) are configured as n×D, wherein D is the sum of the thicknesses of a cathode sheet (144), an anode sheet (142), a first isolation film (141) and a second isolation film (143); and n≥1, where n is an integer.
10. The battery corner gap processing tool according to claim 1, characterized in that: The first insulating film member (20), the second insulating film member (30), the third insulating film member (40) and the fourth insulating film member (50) are organic insulating films or inorganic insulating films.