Rivet high-conductivity glue curing structure of full-welding-free battery test circuit
By using fully-free welding technology and highly conductive glue curing structure in the battery test circuit, the problem of poor welding offset of long strip SMT components is solved, and the stable connection and efficient production of battery electrodes are achieved, reducing costs and simplifying operate.
Patent Information
- Application Number
- CN202420072951.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-11
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-01-11
AI Technical Summary
During the circuit board manufacturing process, during the reflow soldering of long strip SMT components, the solder paste melting deviation is poor due to the hot air heating method, resulting in high soldering defect rate, especially components with long lengths and only one side of the solder joint is located on one side Welding quality is difficult to guarantee.
The rivet high-conductivity glue curing structure using a fully-free welding battery test circuit is adopted. By setting up a U-shaped connector on the substrate and injecting high-conductivity glue, the stable connection of the battery electrode is achieved, avoiding poor contact during welding.
It reduces production costs, improves production efficiency, ensures stable connection of battery electrodes, avoids degradation of battery performance due to poor contact, and simplifies battery installation and disassembly operations.
Smart Images

Figure CN222128405U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of rechargeable batteries, in particular to a rivet high-conductivity glue curing structure of a completely welding-free battery test circuit. Background Art
[0002] During the circuit board manufacturing process, the soldering of surface mount technology (SMT) components is a routine operation. The traditional SMT component soldering process includes printing solder paste on the circuit board, placing the SMT components on the pads, and then soldering the components at high temperature through the reflow soldering process. However, for long SMT components (greater than 7 mm) with long lengths and solder joints only on one side, the solder paste is very likely to deviate after melting due to the hot air heating method during the reflow soldering process. Even if the wind speed during reflow soldering is reduced to 25%, the defect rate is still as high as about 10%. Utility Model Content
[0003] The utility model aims to solve at least one of the technical problems existing in the prior art. To this end, the utility model proposes a rivet high-conductivity glue curing structure of a completely welding-free battery test circuit, which adopts welding-free technology, reduces production costs, and improves production efficiency. The use of high-conductivity glue ensures the stable connection of the battery electrodes and avoids the degradation of battery performance due to poor contact. Finally, the design of the structure fully considers the installation and disassembly of the battery, making the operation easier.
[0004] The rivet high-conductivity glue curing structure of the fully welding-free battery test circuit according to the first aspect of the embodiment of the utility model is used to connect the electrodes of the battery, and is characterized in that it includes: a substrate, and a charging circuit and a working circuit arranged on the substrate, the substrate is provided with at least one through hole, a connector with a U-shaped cross-section and an open end is embedded in the through hole, wherein the open end of one of the connectors is in the same direction as the bottom surface of the substrate, and the open end of the other connector is in the same direction as the top surface of the substrate, and the open end of the connector is provided with a flange, and the flange is fixedly mounted on the substrate by surface mounting;
[0005] The connector is provided with a receiving cavity for receiving the electrode of the battery, and the receiving cavity is provided with conductive glue by injection, and the conductive glue is respectively solidified and connected with the inner wall of the receiving cavity and the electrode of the battery.
[0006] The rivet high-conductivity glue curing structure of the completely welding-free battery test circuit according to the embodiment of the utility model has at least the following beneficial effects: the rivet high-conductivity glue curing structure of the completely welding-free battery test circuit, the core components of which include a substrate, a charging circuit, a working circuit, and a connector, etc. Its unique design and exquisite craftsmanship give the battery higher performance and safety.
[0007] As the foundation of the entire circuit, the substrate bears the important task of carrying other components. On the substrate, there are charging circuits and working circuits, which are responsible for charging and managing the battery respectively. In addition, there is at least one through hole on the substrate, which is where the connector is embedded.
[0008] The connector is a special component with a U-shaped cross-section and an open end. The two connectors are in the same direction as the bottom and top of the substrate, respectively, to facilitate the connection and removal of the battery. The open end of the connector is provided with a flange, which is fixed to the substrate by surface mounting, enhancing the stability of the connection. A receiving cavity is provided inside the connector to accommodate the battery electrodes. Conductive glue is provided in the receiving cavity by injection. This glue has high conductivity and high strength, which can ensure a firm connection between the battery electrode and the inner wall of the receiving cavity. At the same time, the conductive glue is also solidified and connected to the battery electrode, further improving the performance and safety of the battery.
[0009] The rivet high-conductivity glue-cured structure of the fully welding-free battery test circuit has many advantages. First, the structure adopts welding-free technology, which reduces production costs and improves production efficiency. Secondly, the use of highly conductive glue ensures the stable connection of the battery electrodes and avoids the degradation of battery performance due to poor contact. Finally, the design of the structure fully considers the installation and removal of the battery, making the operation easier.
[0010] According to some embodiments of the present invention, the connector is configured as a cylinder with a U-shaped cross-section, one end of the connector is provided with a circular opening, and the edge of the opening is provided with an annular flange.
[0011] According to some embodiments of the utility model, the flange is fixedly mounted on the substrate by surface mounting with glue.
[0012] According to some embodiments of the utility model, an output pole is mounted on the connector whose opening end is in the same direction as the upper surface of the substrate by curing conductive glue.
[0013] According to some embodiments of the present invention, a power transmission head is provided at one end of the output pole away from the substrate.
[0014] Additional aspects and advantages of the present invention will be given in part in the following description, and in part will become apparent from the following description, or will be learned through the practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:
[0016] Figure 1 This is a schematic diagram of the state of the embodiment of the utility model when the battery is connected;
[0017] Figure 2 It is a schematic diagram of the internal structure of an embodiment of the utility model.
[0018] 110, substrate; 120, through hole; 130, connector; 131, flange; 132, accommodating cavity. DETAILED DESCRIPTION
[0019] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0020] In the description of the present invention, it should be understood that descriptions involving orientation, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0021] In the description of the present utility model, "several" means one or more, "more" means more than two, "greater than", "less than", "exceed" etc. are understood to exclude the number itself, and "above", "below", "within" etc. are understood to include the number itself. If there is a description of "first" or "second", it is only used for the purpose of distinguishing the technical features, and cannot be understood as indicating or implying the relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0022] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.
[0023] Reference Figure 1-2According to the first aspect of the present invention, the rivet high-conductivity glue curing structure of the fully welding-free battery test circuit is used to connect the electrodes of the battery, and is characterized in that it includes: a substrate 110, and a charging circuit and a working circuit arranged on the substrate 110, the substrate 110 is provided with at least one through hole 120, and a connector 130 with a U-shaped cross-section and an open end is embedded in the through hole 120, wherein the open end of one of the connectors 130 is in the same direction as the bottom surface of the substrate 110, and the open end of the other connector 130 is in the same direction as the top surface of the substrate 110, and the open end of the connector 130 is provided with a flange 131, and the flange 131 is fixedly mounted on the substrate 110 by surface mounting;
[0024] The connector 130 is provided with a receiving cavity 132 for receiving the electrode of the battery. The receiving cavity 132 is provided with conductive glue by injection. The conductive glue is respectively solidified and connected with the inner wall of the receiving cavity 132 and the electrode of the battery.
[0025] The rivet high-conductivity glue curing structure of the completely welding-free battery test circuit according to the embodiment of the utility model has at least the following beneficial effects: the rivet high-conductivity glue curing structure of the completely welding-free battery test circuit, the core components of which include a substrate 110, a charging circuit, a working circuit and a connector 130, etc., and its unique design and exquisite craftsmanship give the battery higher performance and safety.
[0026] As the foundation of the entire circuit, the substrate 110 bears the important task of carrying other components. On the substrate 110, there are designed charging circuits and working circuits, which are responsible for charging and managing the battery respectively. In addition, at least one through hole 120 is opened on the substrate 110, which is the location where the connector 130 is embedded.
[0027] The connector 130 is a special component with a U-shaped cross-section and an open end. The two connectors 130 are respectively in the same direction as the bottom and top of the substrate 110, which facilitates the connection and removal of the battery. The open end of the connector 130 is provided with a flange 131, which is fixed to the substrate 110 by surface mounting, thereby enhancing the stability of the connection. A receiving cavity 132 is provided inside the connector 130 for accommodating the battery electrodes. Conductive glue is provided in the receiving cavity 132 by injection. This glue has high conductivity and high strength, and can ensure a firm connection between the battery electrodes and the inner wall of the receiving cavity 132. At the same time, the conductive glue is also solidified and connected to the battery electrodes, further improving the performance and safety of the battery.
[0028] The rivet high-conductivity glue-cured structure of the fully welding-free battery test circuit has many advantages. First, the structure adopts welding-free technology, which reduces production costs and improves production efficiency. Secondly, the use of highly conductive glue ensures the stable connection of the battery electrodes and avoids the degradation of battery performance due to poor contact. Finally, the design of the structure fully considers the installation and removal of the battery, making the operation easier.
[0029] Further, according to some embodiments of the present invention, the connector 130 is configured to be a cylinder with a U-shaped cross section, one end of the connector 130 is provided with a circular opening, and the edge of the opening is provided with an annular flange 131. The connector 130 has a unique design, and its cross section is U-shaped, similar to a cylinder. This design enables the connector 130 to have high functional stability and reliability, and can exert good performance in various application scenarios.
[0030] A circular opening is provided at one end of the connector 130. This opening design not only makes the connector 130 more convenient to use, but also can meet the connection requirements in different occasions. An annular flange 131 is provided at the edge of the circular opening. The flange 131 is provided to enhance the durability and safety of the connector 130.
[0031] Further, according to some embodiments of the present invention, the flange 131 is fixedly mounted on the substrate 110 by surface mounting with glue.
[0032] In some embodiments of the present invention, the flange 131 is fixedly mounted on the substrate 110 by means of glue surface mounting. This installation method has the advantages of simple operation and high efficiency, and can ensure a firm connection between the flange 131 and the substrate 110, thereby improving the stability and durability of the entire structure.
[0033] First, glue is applied to the corresponding position of the surface of the substrate 110, and then the flange 131 is placed on the surface of the substrate 110 on which the glue is applied. By adjusting the position of the flange 131, the contact area between the flange 131 and the surface of the substrate 110 is maximized, thereby improving the bonding effect. After the flange 131 is in full contact with the surface of the substrate 110, light pressure is applied to form a good connection between the glue and the substrate 110. Finally, the glue is allowed to cure, so that the flange 131 is firmly fixed to the substrate 110.
[0034] This glue mounting and fixing method is not only applicable to the structure of the substrate 110 and the flange 131 mentioned in the utility model, but can also be applied to the assembly of components of other similar structures. By selecting suitable glue and reasonable mounting process, a fast, stable and durable assembly effect can be achieved.
[0035] In summary, the glue mounting and fixing method of the flange 131 provided by the utility model has the advantages of simple operation and firm connection, and provides an efficient and reliable solution for the assembly of various substrates 110 and flange 131 structures. In practical applications, the appropriate glue type and mounting process can be selected according to specific needs to ensure the stability and service life of the structure.
[0036] Further, according to some embodiments of the present invention, an output pole is mounted on the connector 130 with the opening end in the same direction as the upper surface of the substrate 110 by curing conductive glue.
[0037] In certain embodiments of the utility model, an output pole is mounted on the connector 130 whose open end is in the same direction as the upper side of the substrate 110 by curing with conductive glue. This design aims to achieve efficient, stable and reliable electrical connection. The output pole is cured and installed with conductive glue to ensure the stability and reliability of the connection. The conductive glue has good electrical conductivity and bonding strength, and can form a tight connection between the connector 130 and the output pole to prevent problems such as excessive contact resistance and loose connection. In addition, the conductive glue also has good heat resistance and corrosion resistance, which helps to extend the service life of the connector 130.
[0038] Furthermore, according to some embodiments of the present invention, a power transmission head is provided at one end of the output pole away from the substrate 110 .
[0039] One end of the output pole is connected to the substrate 110, and the other end is provided with an efficient power transmission head. The power transmission head is a key component of the output pole, which is responsible for achieving efficient transmission of electric energy. In the design of the utility model, the power transmission head adopts advanced materials and processes to ensure minimum power loss. In addition, the design of the power transmission head also takes into account the stability and reliability of the electrical connection, so that the device can maintain stable performance during long-term operation.
[0040] The present embodiment is described in detail above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiment. Various changes can be made within the knowledge scope of ordinary technicians in the technical field without departing from the present purpose.
Claims
1. The rivet high-conductivity glue curing structure of the fully welding-free battery test circuit is used to connect the battery electrodes, characterized in that: include: A substrate (110), and a charging circuit and a working circuit arranged on the substrate (110), wherein the substrate (110) is provided with at least one through hole (120), and a connector (130) having a U-shaped cross section and an open end is embedded in the through hole (120), wherein the open end of one of the connectors (130) is in the same direction as the bottom surface of the substrate (110), and the open end of the other connector (130) is in the same direction as the top surface of the substrate (110), and the open end of the connector (130) is provided with a flange (131), and the flange (131) is fixedly mounted on the substrate (110) by surface mounting; The connector (130) is provided with a receiving cavity (132) for receiving an electrode of a battery, and conductive glue is injected into the receiving cavity (132), and the conductive glue is respectively solidified and connected to the inner wall of the receiving cavity (132) and the electrode of the battery.
2. The rivet high-conductivity glue curing structure of the fully welding-free battery test circuit according to claim 1 is characterized in that: The connector (130) is configured to be a cylindrical shape with a U-shaped cross section, one end of the connector (130) is provided with a circular opening, and the edge of the opening is provided with an annular flange (131).
3. The rivet high-conductivity glue curing structure of the fully welding-free battery test circuit according to claim 2 is characterized in that: The flange (131) is fixedly mounted on the substrate (110) by means of glue surface mounting.
4. The rivet high-conductivity glue curing structure of the fully welding-free battery test circuit according to claim 1 is characterized in that: An output pole is mounted on the connector (130) whose opening end is in the same direction as the upper surface of the substrate (110) by curing conductive glue.
5. The rivet high-conductivity glue curing structure of the fully welding-free battery test circuit according to claim 4 is characterized in that: A power transmission head is arranged at one end of the output pole away from the substrate (110).