Antibacterial glass structure
Through the combination of frame structure and elastic parts, combined with nano-anti-bacterial film and color-tool film, the problems of antibacterial glass processing complexity and coating peeling are solved, and efficient heat insulation, sound insulation and impact resistance are achieved, simplified the processing process and Reduced costs.
Patent Information
- Application Number
- CN202420696661.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-07
- Publication Date
- 2025-01-14
- Estimated Expiration
- 2034-04-07
AI Technical Summary
The processing process of existing antibacterial glass is cumbersome, time-consuming and difficult, with many coatings and complex drying processes, which can easily lead to the fall of the external coating and affect the aesthetics and functionality.
Using frame structure and elastic parts, the number of coatings is reduced through laminated glass and hollow glass design, stainless steel sheets and POM plastic materials are used to combine nano-anti-bacterial film to achieve thermal insulation, sound insulation and impact resistance, and through color-to-color film Adjust the light.
The processing process is simplified, the cost is reduced, the explosion resistance, sound insulation and heat insulation are improved, the antibacterial function is ensured while avoiding the outer coating falling off, and the wear resistance and aesthetics of the glass are enhanced.
Smart Images

Figure CN222346465U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of glass, in particular to an antibacterial glass structure. Background Art
[0002] Antibacterial glass refers to a glass plate with a layer of nano-antibacterial film evenly coated on the surface. The film layer has extremely high uniformity and hardness, which is the highest level of coated glass. It is a new type of ecological functional material and a deep-processed glass with bactericidal and antibacterial functions. Unlike traditional self-cleaning glass, nano-antibacterial glass does not require the use of ultraviolet rays for disinfection, and realizes the functions of antibacterial, antibacterial and sterilization around the clock under normal conditions.
[0003] 202220127145.8 A nano-coated glass with antibacterial function, comprising a glass substrate, a vacuum zone is arranged inside the glass substrate, and a heavy metal ion layer is arranged on the surface of the glass substrate through a protective layer. The utility model sets a vacuum zone inside the glass substrate by setting an anti-pull screen, a lamination layer, a vacuum zone and an etching layer, which can achieve the effect of sound insulation and heat insulation. Under the action of the heavy metal ion layer, the glass can have a bactericidal property. The heat insulation layer and the lamination layer can make the glass substrate have good heat resistance and impact resistance. It has a simple structure and has the advantages of antibacterial sterilization and anti-glare. It solves the problem that glass is easily stained and sometimes inconvenient to clean, resulting in a large number of bacteria easily generated on the glass, which may cause infection to the user and thus affect the user's health.
[0004] This technical solution increases the heat insulation, sterilization, impact resistance, anti-glare, wear resistance and other properties of glass through various coatings. Although the antibacterial glass has many functions, it is very difficult to process. It is necessary to use spraying, brushing, soaking and other processes to make the solvent settle on the surface of the glass plate to form a coating. During the processing, it is necessary to process the internal coating first, and then wait for the internal coating to dry before starting the external coating processing, and then wait for the external coating to dry. The more coatings, the more time it takes, and the dried internal coating needs to be polished, otherwise the external coating is difficult to adhere and easy to fall off, and it is necessary to avoid the internal coating from being exposed to the outside for a long time, and avoid external impurities such as oil and dust from adhering to the surface of the internal coating, resulting in impurities between the external coating and the internal coating after coating, which not only affects the appearance but also easily causes the external coating to fall off, and it is necessary to avoid excessive drying of the internal coating, because after the internal coating is over-dried, the internal coating lacks active polar groups, which makes the external coating and the internal coating lack the binding force from chemical bonds, thereby reducing the interlayer adhesion and causing it to fall off. In summary, it can be seen that this technical solution is very cumbersome, time-consuming and difficult in the processing process. Utility Model Content
[0005] Based on this, the purpose of the present invention is to provide an antibacterial glass structure to solve the technical problems mentioned in the above background technology.
[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: an antibacterial glass structure, comprising a frame, an elastic member connected to the upper part of the frame, a first glass plate and a second glass plate are respectively arranged on one side of the frame, and a first adhesive layer is arranged on one side of the first glass plate and the second glass plate, a third glass plate and a fourth glass plate are respectively arranged on the other side of the frame, and a second adhesive layer is arranged between the third glass plate and the fourth glass plate.
[0007] By adopting the above technical solution, laminated glass is formed between the first glass plate and the second glass plate through the first adhesive layer, and laminated glass is also formed between the third glass plate and the fourth glass plate through the second adhesive layer. It has good explosion resistance to prevent the glass from flying around and injuring people or equipment after breaking, and the structure of the laminated glass can achieve good sound insulation effect. At the same time, the hollow space between the second glass plate and the fourth glass plate forms a hollow glass, which increases the effect of heat insulation and sound insulation. Since the structure of the hollow glass has a certain sound insulation effect, the cost can be reduced by reducing the thickness of the third glass plate and the fourth glass plate. At the same time, the hollow space between the two laminated glasses is ensured by the cooperation of the frame and the elastic member, and the elastic member has good elasticity and is M-shaped, so it can shrink and absorb energy when the antibacterial glass is impacted, thereby achieving a buffering effect.
[0008] Furthermore, four frames are provided, and the frames are formed by bending stainless steel sheets.
[0009] By adopting the above technical solution, when processing the antibacterial glass, the stainless steel sheet is first bent into the style shown in the figure, and then the two sides of the bent stainless steel sheet are chamfered, and the chamfer angle is forty-five degrees to complete the processing of the frame, and the four frames are spliced into a rectangle and fixed into a whole by rivets, welding and other processes.
[0010] Furthermore, the elastic member is made of POM plastic.
[0011] By adopting the above technical solution, the POM material has good elasticity, fatigue resistance, environmental resistance and wear resistance, and the elastic parts made of POM plastic can play a buffering and impact-resistant effect.
[0012] Furthermore, the elastic member is in an "M" shape.
[0013] By adopting the above technical solution, the elastic member has good elasticity and is in an M shape, so it can shrink and absorb energy when the antibacterial glass is impacted, thereby achieving a buffering effect.
[0014] Furthermore, the thickness of the first glass plate and the second glass plate is greater than the thickness of the third glass plate and the fourth glass plate.
[0015] By adopting the above technical solution, since the structure of the hollow glass has a certain sound insulation effect, the cost can be reduced by reducing the thickness of the third glass plate and the fourth glass plate.
[0016] Furthermore, there is a hollow space between the second glass plate and the fourth glass plate.
[0017] By adopting the above technical solution, the hollow space between the second glass plate and the fourth glass plate forms a hollow glass, which increases the effect of heat insulation and sound insulation and effectively reduces noise and heat conduction.
[0018] Furthermore, the other side of the first glass plate is coated with a first nano-antibacterial film, and the other side of the third glass plate is coated with a second nano-antibacterial film.
[0019] By adopting the above technical solution, the product has bactericidal and antibacterial functions, realizing the antibacterial, antibacterial and bactericidal functions around the clock under normal conditions.
[0020] Furthermore, a color adjustment film is provided between the first glass plate and the second glass plate via a first adhesive layer.
[0021] By adopting the above technical solution, during the use of the antibacterial glass, the color-adjusting film is energized to make the antibacterial glass transparent or atomized, thereby avoiding dazzling due to excessive external light.
[0022] In summary, the utility model mainly has the following beneficial effects:
[0023] The utility model is provided with a frame, a first glass plate, a first adhesive layer, a second glass plate, an elastic member, a third glass plate, a second adhesive layer and a fourth glass plate. Firstly, the first glass plate and the second glass plate are provided with a laminated glass through the first adhesive layer, and the third glass plate and the fourth glass plate are provided with a laminated glass through the second adhesive layer. The utility model has good explosion resistance to prevent the glass from flying to the surrounding area and injuring people or equipment after being broken. The structure of the laminated glass can achieve good sound insulation effect. At the same time, the hollow space between the second glass plate and the fourth glass plate forms a hollow glass, which increases the effects of heat insulation and sound insulation. Since the structure of the hollow glass has a certain sound insulation effect, the cost is reduced by reducing the thickness of the third glass plate and the fourth glass plate. At the same time, the hollow space between the two laminated glasses is ensured by the cooperation of the frame and the elastic member. The elastic member has good elasticity and is in an M shape. Therefore, it can shrink and absorb energy when the antibacterial glass is impacted, thereby achieving a buffering effect. The coating is used less and there is no internal and external coating, which is convenient to process. At the same time, the utility model has the effects of heat insulation, sound insulation and impact resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a structural schematic diagram of the utility model;
[0025] Figure 2 It is a schematic diagram of the cross-sectional structure of the utility model;
[0026] Figure 3 For the utility model Figure 2 A magnified view of the structure at A;
[0027] Figure 4 It is a schematic diagram of the frame explosion structure of the utility model.
[0028] In the figure: 1, frame; 2, first glass plate; 3, first adhesive layer; 4, second glass plate; 5, color adjustment film; 6, first nano-antibacterial film; 7, elastic member; 8, third glass plate; 9, second adhesive layer; 10, fourth glass plate; 11, second nano-antibacterial film. DETAILED DESCRIPTION
[0029] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. The embodiments described below with reference to the drawings are exemplary and are only used to explain the utility model, and cannot be understood as limiting the utility model.
[0030] The following describes an embodiment of the utility model based on its overall structure.
[0031] Embodiment 1:
[0032] An antimicrobial glass structure, such as Figure 1-Figure 4 As shown, it includes a frame 1, and the frame 1 is provided with four. The frame 1 is formed by bending a stainless steel sheet, which is easy to process and low in cost; an elastic member 7 is connected to the upper part of the frame 1, and the elastic member 7 is made of POM plastic. The elastic member 7 is in an "M" shape and can shrink and absorb energy when the antibacterial glass is impacted, thereby playing a buffering effect; a first glass plate 2 and a second glass plate 4 are respectively provided on one side of the frame 1, and a first adhesive layer 3 is provided on one side of the first glass plate 2 and the second glass plate 4, and a third glass plate 8 and a fourth glass plate 9 are respectively provided on the other side of the frame 1. A second adhesive layer 9 is arranged between the glass plate 10, the third glass plate 8 and the fourth glass plate 10 to form a laminated glass, which has good explosion resistance to prevent the glass from flying around and injuring people or equipment after shattering, and the structure of the laminated glass can achieve good sound insulation effect; the thickness of the first glass plate 2 and the second glass plate 4 is greater than that of the third glass plate 8 and the fourth glass plate 10, and the cost is reduced by reducing the thickness of the third glass plate 8 and the fourth glass plate 10; the second glass plate 4 and the fourth glass plate 10 are hollow, which increases the effect of heat insulation and sound insulation.
[0033] See also Figure 1-Figure 3 In the above embodiment, the other side of the first glass plate 2 is coated with a first nano-antibacterial film 6, and the other side of the third glass plate 8 is coated with a second nano-antibacterial film 11, which has bactericidal and antibacterial functions, realizing the all-weather antibacterial, antibacterial and bactericidal functions under normal conditions.
[0034] Embodiment 2:
[0035] On the basis of the above-mentioned embodiment 1, although by setting the frame 1, the first glass plate 2, the first adhesive layer 3, the second glass plate 4, the elastic member 7, the third glass plate 8, the second adhesive layer 9 and the fourth glass plate 10, the coating is used less and there is no internal and external coating for convenient processing, and at the same time it has the effects of heat insulation, sound insulation and impact resistance; but when the external light is strong, especially in summer, it is easy to be dazzling; now by setting the color adjustment film 5, the antibacterial glass can be made light-transmitting or atomized to avoid dazzling caused by excessive external light.
[0036] See also Figure 2 and Figure 3 In the above embodiment, a tinting film 5 is provided between the first glass plate 2 and the second glass plate 4 through the first adhesive layer 3, so that the antibacterial glass is light-transmissive or atomized to avoid dazzling due to excessive external light.
[0037] The implementation principle of the utility model is: first, when processing the antibacterial glass, the stainless steel sheet is bent into Figure 3 In the middle style, both sides of the bent stainless steel sheet are then chamfered, and the chamfering angle is 45 degrees to complete the processing of the frame 1, and then the elastic member 7 is inserted into the frame 1 and the side of the elastic member 7 is fixed to the frame 1 by an adhesive, and then the staff coats the first nano antibacterial film 6 on the side of the first glass plate 2, and coats the second nano antibacterial film 11 on the side of the third glass plate 8, and then the remaining structures are bonded and fixed by the first adhesive layer 3 and the second adhesive layer 9, so that the first glass plate 2, the color adjustment film 5 and the second glass plate 4 are fixed together, and the third glass plate 8 and the fourth glass plate 10 are fixed together, and then the first glass plate 2, the second glass plate 4, the third glass plate 8 and the fourth glass plate 10 are all placed in the frame 1, and then the four frames 1 are spliced into a rectangle and the four frames 1 are fixed into a whole by rivets, welding and other processes;
[0038] During the use of the antibacterial glass, the tinting film 5 is energized to make the antibacterial glass translucent or atomized to avoid dazzling due to excessive external light. At the same time, the first glass plate 2 and the second glass plate 4 are laminated by the first adhesive layer 3, and the third glass plate 8 and the fourth glass plate 10 are laminated by the second adhesive layer 9. The antibacterial glass has good explosion resistance to prevent the glass from flying around and injuring people or equipment after breaking. The structure of the laminated glass can achieve good sound insulation. At the same time, the hollow space between the second glass plate 4 and the fourth glass plate 10 forms a hollow glass to increase the effect of heat insulation and sound insulation. Since the structure of the hollow glass has a certain sound insulation effect, the cost can be reduced by reducing the thickness of the third glass plate 8 and the fourth glass plate 10. At the same time, the frame 1 cooperates with the elastic member 7 to ensure the hollow space between the two laminated glasses. The elastic member 7 has good elasticity and is in an M shape. Therefore, it can shrink and absorb energy when the antibacterial glass is impacted, thereby achieving a buffering effect.
[0039] Although an embodiment of the utility model has been shown and described, this specific embodiment is only an explanation of the utility model and is not a limitation of the utility model. The specific features, structures, materials or characteristics described may be combined in a suitable manner in any one or more embodiments or examples. After reading this specification, those skilled in the art may make modifications, substitutions and variations to the embodiments without creative contribution as needed without departing from the principles and purpose of the utility model. However, as long as they are within the scope of the claims of the utility model, they are protected by patent law.
Claims
1. An antibacterial glass structure, comprising a frame (1), characterized in that: An elastic member (7) is connected to the upper part of the frame (1), a first glass plate (2) and a second glass plate (4) are respectively arranged on one side of the frame (1), and a first adhesive layer (3) is arranged on one side of the first glass plate (2) and the second glass plate (4), and a third glass plate (8) and a fourth glass plate (10) are respectively arranged on the other side of the frame (1), and a second adhesive layer (9) is arranged between the third glass plate (8) and the fourth glass plate (10).
2. The antibacterial glass structure according to claim 1, characterized in that: Four frames (1) are provided, and the frames (1) are formed by bending stainless steel thin plates.
3. The antibacterial glass structure according to claim 1, characterized in that: The elastic member (7) is made of POM plastic.
4. The antibacterial glass structure according to claim 2, characterized in that: The elastic member (7) is in an "M" shape.
5. The antibacterial glass structure according to claim 1, characterized in that: The thickness of the first glass plate (2) and the second glass plate (4) is greater than the thickness of the third glass plate (8) and the fourth glass plate (10).
6. The antibacterial glass structure according to claim 5, characterized in that: There is a hollow space between the second glass plate (4) and the fourth glass plate (10).
7. The antibacterial glass structure according to claim 1, characterized in that: The other side of the first glass plate (2) is coated with a first nano-antibacterial film (6), and the other side of the third glass plate (8) is coated with a second nano-antibacterial film (11).
8. The antibacterial glass structure according to claim 7, characterized in that: A color adjustment film (5) is provided between the first glass plate (2) and the second glass plate (4) via a first adhesive layer (3).