Corrosion resistant expansion joint for flue
By using an inner arc-shaped telescopic tube and a Ni-Cr-Mo based 625 alloy coating, combined with an airtight protective cover, the problems of ash accumulation and acidic condensate corrosion in the flue expansion joint were solved, thus improving the equipment's corrosion resistance and economy.
Patent Information
- Application Number
- CN202522750842.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-25
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-12-25
AI Technical Summary
Existing flue expansion joints are prone to ash accumulation and acidic condensate corrosion in high-temperature flue gas environments, and their corrosion resistance is insufficient, resulting in shortened equipment lifespan and high costs.
The design incorporates an inner arc-shaped telescopic tube combined with a Ni-Cr-Mo-based 625 alloy coating and an airtight protective cover. The inner arc-shaped telescopic tube eliminates dead zones for dust and liquid accumulation, the outer insulation layer maintains the wall temperature, and the Ni-Cr-Mo-based 625 alloy layer provides chemical corrosion protection.
It effectively prevents corrosion, extends equipment life, reduces costs, improves chemical corrosion resistance, and is highly economical.
Smart Images

Figure CN224956466U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the technical field of thermal pipeline compensation equipment, specifically to a corrosion-resistant expansion joint used in flue systems in industries such as power, metallurgy, and chemical engineering. Background Technology
[0002] Industrial flue gas systems often transport high-temperature flue gas containing corrosive components such as sulfur oxides and nitrogen oxides. Currently, most expansion joints used in flues are made of ordinary austenitic stainless steel (such as 304). Their traditional U-shaped or V-shaped corrugated structure has inherent defects. When the flue gas temperature is below the acid dew point, acidic liquid condenses on the wall surface, causing severe low-temperature corrosion of the metal components. Simultaneously, dust particles accumulate in the grooves of the corrugated pipe, combining with the condensed acid to form corrosive slurry, further accelerating the corrosion process. Furthermore, conventional stainless steel lacks sufficient corrosion resistance in complex acid-alkali alternating environments, while using higher-grade corrosion-resistant alloys (such as Hastelloy) would lead to a sharp increase in cost and poor economic efficiency.
[0003] Therefore, it is crucial to develop a new type of expansion joint that effectively solves the corrosion problem and is cost-effective. Utility Model Content
[0004] The technical problem to be solved by this utility model is to address the issues of easy ash accumulation, acidic condensate corrosion, and chemical corrosion in existing flue expansion joints, and to provide a corrosion-resistant expansion joint for flues.
[0005] This utility model provides a corrosion-resistant expansion joint for flues, which also features a streamlined anti-ash accumulation structure and anti-condensation design. The corrosion-resistant expansion joint for flues includes two flange interfaces (1). The two flange interfaces (1) are connected by a telescopic pipe (2). The sidewall of the telescopic pipe (2) has an inner arc shape with an arc of 120°-180°.
[0006] Furthermore, the telescopic tube (2) is made of a metal substrate.
[0007] Furthermore, the inner surface of the telescopic tube (2) is coated with a corrosion-resistant alloy layer (3).
[0008] Furthermore, an insulation layer (4) is wrapped around the outside of the telescopic tube (2).
[0009] Furthermore, the corrosion-resistant alloy layer (3) is a Ni-Cr-Mo based 625 alloy coating.
[0010] Furthermore, the thickness of the corrosion-resistant alloy layer (3) is 0.3-0.5 mm.
[0011] Furthermore, the surface of the corrosion-resistant alloy layer (3) is mechanically polished.
[0012] Furthermore, an airtight protective cover (5) is provided on the outside of the insulation layer (4).
[0013] The beneficial effects of this utility model are: 1. The telescopic tube is inner arc-shaped, which can eliminate the accumulation of liquid medium inside the expansion joint, eliminate dead corners for ash and liquid accumulation, and prevent corrosive media from accumulating, thereby effectively reducing corrosion. 2. Eliminate the source of corrosion: The external insulation + airtight cover design effectively maintains the wall temperature and prevents the flue gas temperature from dropping below the dew point, fundamentally eliminating the generation of acidic condensate and solving the core problem of low-temperature corrosion. 3. Improve chemical corrosion resistance: The corrosion-resistant alloy layer (such as 625 alloy) on the inner surface provides a barrier protection for the base material, which can resist the chemical corrosion of various acids and chloride ions in complex flue gas environments, and its service life is far longer than that of ordinary stainless steel. 4. High reliability and economy: The base material of the corrosion-resistant expansion joint for flue gas of this utility model is made of low-cost steel (such as Q235B), and the inner side is composited with high-performance materials. The structural and material anti-corrosion effects work synergistically, which significantly improves the corrosion resistance life while effectively controlling the manufacturing cost, resulting in extremely high comprehensive economic benefits. Attached Figure Description
[0014] Figure 1 This is a schematic diagram of the axial cross-sectional structure of this utility model.
[0015] Explanation of the labels in the diagram:
[0016] 1. Flange interface; 2. Expansion pipe; 3. Corrosion-resistant alloy layer; 4. Insulation layer; 5. Airtight protective cover. Detailed Implementation
[0017] The technical solution of the gas-liquid distribution and guiding device in the embodiments of this utility model will be clearly and completely described below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a full understanding of this utility model. However, this utility model can also be implemented in other ways different from those described herein. Those skilled in the art can make similar extensions without departing from the spirit of this utility model. Therefore, this utility model is not limited to the specific embodiments disclosed below.
[0018] Example 1:
[0019] The applicant describes a flue gas duct internal arc-shaped corrosion-resistant expansion joint implemented at the production site, comprising two flange interfaces 1, with a telescopic pipe 2 connected between the two flange interfaces 1, such as... Figure 1As shown, the sidewall profile of the telescopic pipe 2 is an inner arc shape, meaning that the arc-shaped portion of the sidewall bulges inward towards the inside of the pipe. The inner wall profile of the telescopic pipe 2 is continuous and smooth, ensuring that the inner surface is free of any flat pits where dust or liquid can accumulate. The preferred curvature of the aforementioned inner arc is 120°-180°. In this embodiment, the curvature of the telescopic pipe is 150°.
[0020] The telescopic tube 2 is made of a metal substrate. In this embodiment, the metal substrate is made of Q235B material. A dense Ni-Cr-Mo based 625 alloy coating is prepared on the inner surface of the telescopic tube 2 by a high-velocity oxygen fuel spraying (HVOF) process, forming a corrosion-resistant alloy layer 3 with a thickness of about 0.3-0.5 mm. This alloy layer is then mechanically polished to achieve a smooth surface.
[0021] On the outside of the expansion tube 2, a layer of ceramic fiber insulation cotton is tightly wrapped as the insulation layer 4. Finally, an airtight protective cover 5 made of 304 stainless steel sheet is used to completely seal and wrap the entire insulation layer 4. All seams are continuously welded to ensure its airtightness and effectively isolate external cold air.
[0022] After the corrosion-resistant expansion joint is installed in the flue, when high-temperature corrosive flue gas passes through, the wall temperature of the expansion pipe 2 is maintained due to the airtight protective cover 5 and the insulation layer 4, preventing condensation. Even in extreme cases of fluctuating operating conditions, the smooth inner arc-shaped surface and the corrosion-resistant alloy layer 3 provide double protection, ensuring the long-term safe operation of the equipment.
[0023] The expansion joint manufactured by the applicant according to this embodiment has shown excellent results after more than three years of practical application. It can achieve sufficient expansion compensation capacity while effectively slowing down the corrosion process.
[0024] The above embodiments are only used to illustrate the technical solution of this utility model and are not intended to limit it. Any simple modifications, substitutions, and alterations based on the essence of this utility model should be covered within the scope of protection of the claims of this utility model.
Claims
1. A corrosion-resistant expansion joint for flues, comprising two flange interfaces (1), characterized in that: A telescopic pipe (2) is connected between two flange interfaces (1). The sidewall of the telescopic pipe (2) has an inner arc shape with an arc of 120°-180°.
2. The flue corrosion-resistant expansion joint as described in claim 1, characterized in that: The telescopic tube (2) is made of metal substrate.
3. The flue corrosion-resistant expansion joint as described in claim 1, characterized in that: The inner surface of the telescopic tube (2) is coated with a corrosion-resistant alloy layer (3).
4. The flue corrosion-resistant expansion joint as described in claim 1, characterized in that: An insulation layer (4) is wrapped around the outside of the telescopic tube (2).
5. The flue corrosion-resistant expansion joint as described in claim 3, characterized in that: The corrosion-resistant alloy layer (3) is a Ni-Cr-Mo based 625 alloy coating.
6. The flue corrosion-resistant expansion joint as described in claim 5, characterized in that: The thickness of the corrosion-resistant alloy layer (3) is 0.3-0.5 mm.
7. The flue corrosion-resistant expansion joint as described in claim 5, characterized in that: The surface of the corrosion-resistant alloy layer (3) is mechanically polished.
8. The flue corrosion-resistant expansion joint as described in claim 4, characterized in that: An airtight protective cover (5) is provided on the outside of the insulation layer (4).