Manufacturing an air inlet lip with reduced thickness zones
By mechanically machining reduced thickness zones on sheet metal and using hydroforming, the method efficiently produces lightweight air inlet lips for aeronautical engine nacelles with preserved mechanical integrity.
Patent Information
- Application Number
- FR2020010783
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-21
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-10-21
AI Technical Summary
Existing methods for manufacturing air inlet lips for aeronautical engine nacelles are cumbersome and inefficient, particularly in reducing thickness in specific zones, leading to a high overall mass without preserving mechanical integrity.
A method involving mechanical machining of reduced thickness zones on a sheet metal plate before shaping, followed by hydroforming to create an air inlet lip with localized thinning, ensuring mechanical properties are maintained.
The method results in an air inlet lip with reduced overall mass and maintained mechanical properties, achieved through precise and simplified manufacturing processes.
Smart Images

Figure 00000012_0000 
Figure 00000013_0000 
Figure 00000013_0001
Abstract
Description
Title of the invention: Manufacture of an air intake lip with reduced thickness zones Technical field
[0001] The present invention relates to the manufacture of air intake lips for aircraft engine nacelles. Prior art
[0002] Aircraft engine nacelles comprise an air intake cowl extended at the front by a lip having in section the shape of a U open towards the rear. The air intake lip has in particular the function of ensuring the aerodynamic flow of air, on the one hand, towards the fan duct and, on the other hand, towards the outside of the nacelle.
[0003] The air inlet lips are manufactured in one piece or from several individual annular sectors assembled together subsequently.
[0004] Air inlet lips or annular sectors are manufactured individually by forming sheets and more specifically by centrifugal turning (also called "spin forming"). The manufacture of an air inlet lip or an annular sector of an air inlet lip typically comprises the shaping of a sheet metal part so as to obtain a part having the shape of an air inlet lip or an annular sector.
[0005] In order to reduce the overall mass of the air inlet lip, the thickness of the sheet metal is reduced in one or more areas on the inner side of the air inlet lip. These areas of reduced thickness are produced by chemical or mechanical machining after shaping the part. Chemical machining is a long and difficult process since it requires masking the parts of the part that must not be thinned, dipping the part in a chemical etching bath and finally cleaning and drying the part.
[0006] However, there is a need to obtain an air inlet lip having a reduced overall mass without the aforementioned drawbacks. Statement of the invention
[0007] To this end, the invention proposes a method of manufacturing an air inlet lip comprising:
[0008] - the supply of a sheet metal plate,
[0009] - cutting the sheet metal plate so as to form a ring,
[0010] - mechanical machining of one or more zones of reduced thickness in the ring, each zone of reduced thickness being produced on a face of the ring corresponding to the internal surface of a final air inlet lip,
[0011] - shaping the ring so as to obtain an air inlet lip having a U-shaped section and comprising on its internal surface one or more zones of reduced thickness.
[0012] Thus, the method of the invention considerably simplifies the machining of the zone(s) of reduced thickness in the air inlet lip. Indeed, in accordance with the method of the invention, the zone(s) of reduced thickness are produced from the start of the process of manufacturing the lip on the flat sheet. This allows the implementation of precise, simple and rapid mechanical machining and ultimately to obtain an air inlet lip with a reduced overall mass.
[0013] According to a particular characteristic of the method of the invention, the zone(s) of reduced thickness have a thickness corresponding to at most 90% of the thickness of the sheet metal plate.
[0014] According to another particular characteristic of the method of the invention, the latter further comprises, after cutting the sheet metal plate and before shaping the ring:
[0015] - the formation of a truncated cone from the ring,
[0016] - preforming an air inlet lip blank from the truncated cone,
[0017] - the placement of the blank opposite a three-dimensional forming surface of a die of a hydroforming tool, the shaping of the air inlet lip being carried out by hydroforming the blank on the three-dimensional surface of the die.
[0018] According to another particular characteristic of the method of the invention, the latter further comprises, after shaping the ring, the production of one or more openings in the wall of the air inlet lip.
[0019] The invention also relates to a method for manufacturing an annular air inlet lip sector comprising:
[0020] - the supply of a sheet metal plate,
[0021] - cutting the sheet metal plate so as to form a portion of a ring,
[0022] - mechanical machining of one or more zones of reduced thickness in the portion ring, each zone of reduced thickness being produced on one face of the ring portion corresponding to the internal surface of an annular sector of the final air inlet lip,
[0023] - shaping the ring portion so as to obtain a lip sector air inlet having a U-shaped section and comprising on its internal surface one or more zones of reduced thickness.
[0024] According to a particular characteristic of the method of the invention, the zone(s) of reduced thickness have a thickness corresponding to at most 90% of the thickness of the sheet metal plate.
[0025] According to another particular characteristic of the method of the invention, the latter further comprises, after cutting the sheet metal plate and before shaping the ring portion:
[0026] - the formation of a portion of a truncated cone from the portion of a ring,
[0027] - preforming a blank of annular sector from the ring portion,
[0028] - the placement of the blank opposite a three-dimensional forming surface of a die of a hydroforming tool, the shaping of the air inlet lip sector being carried out by hydroforming the blank on the three-dimensional surface of the die.
[0029] According to another particular characteristic of the method of the invention, the latter further comprises, after shaping the ring portion, the production of one or more openings in the wall of the annular air inlet lip sector.
[0030] The invention also relates to a method for manufacturing an air inlet lip comprising the production of annular air inlet lip sectors according to the invention and the assembly of said sectors so as to obtain an air inlet lip sector having a U-shape in section and comprising on its internal surface one or more zones of reduced thickness. Brief description of the drawings
[0031] [Fig-1] [Fig.l] is a flowchart showing the steps of a fa process construction of an air inlet lip according to an embodiment of the invention,
[0032] [Fig.2] [Fig.2] is a schematic view of a sheet metal plate,
[0033] [Fig.3] [Fig.3] is a schematic of a ring obtained after cutting the sheet metal plate of [Fig.2],
[0034] [Fig.4] [Fig.4] is a schematic view of the ring of [Fig.3] after machining an area of reduced thickness,
[0035] [Fig.5] [Fig.5] is a sectional view of the ring of [Fig.4],
[0036] [Fig.6] [Fig.6] is a schematic perspective view of a truncated cone obtained from the ring of [Fig.5],
[0037] [Fig.7] [Fig.7] is a schematic perspective view of an air inlet lip blank obtained from the truncated cone of [Fig.6],
[0038] [Fig.8] [Fig.8] is a schematic perspective view showing the placement of the blank of [Fig.7] in a hydroforming tool,
[0039] [Fig.9] [Fig.9] is a schematic sectional view of the hydroforming tool of [Fig.8] when closed and in operation,
[0040] [Fig. 10] [Fig. 10] is a schematic perspective view showing the air inlet lip obtained after hydroforming the blank of [Fig.7] in the tooling hydroforming of Figures 8 and 9 and cutting openings in the lip,
[0041] [Fig. 11] [Fig. 11] is a flowchart showing the steps of a method of manufacturing an annular sector of an air inlet lip in accordance with one embodiment of the invention,
[0042] [Fig. 12] [Fig. 12] is a schematic view of a sheet metal plate,
[0043] [Fig. 13] [Fig. 13] is a schematic of a portion of a ring obtained after cutting of the sheet metal plate of [Fig. 12],
[0044] [Fig. 14] [Fig. 14] is a schematic view of the ring portion of [Fig. 13] after machining an area of reduced thickness,
[0045] [Fig. 15] [Fig. 15] is a sectional view of the ring portion of [Fig. 14],
[0046] [Fig. 16] [Fig. 16] is a schematic perspective view of a portion of a trunk of cone obtained from the ring of [Fig. 15],
[0047] [Fig. 17] [Fig. 17] is a schematic perspective view of a blank of an annular air inlet lip sector obtained from the truncated cone portion of [Fig. 16],
[0048] [Fig. 18] [Fig. 18] is a schematic perspective view showing the placement of the blank of [Fig. 17] in a hydroforming tool,
[0049] [Fig. 19] [Fig. 19] is a schematic sectional view of the hydroforming tool of [Fig. 18] when closed and in operation,
[0050] [Fig.20] [Fig.20] is a schematic perspective view showing the annular sector of the air inlet lip obtained after hydroforming the blank of [Fig.17] in the hydroforming tool of figures 18 and 19. Description of the embodiments
[0051] The invention applies generally to the production of air inlet lips or annular sectors for air inlet lips for aircraft engine nacelles.
[0052] [Fig. 1] describes the steps of a method of manufacturing an air inlet lip according to the invention.
[0053] As illustrated in [Fig. 2], the method begins by providing a sheet metal plate 10, for example made of aluminum alloy (step S1). The sheet metal 10 may be an integral plate or obtained by assembling several plates fixed together by welding in order to obtain large sheet metal plates from smaller unit sheet metal plates.
[0054] The sheet metal plate 10 is then cut to form a ring 20 illustrated in [Fig.3] (step S2).
[0055] At this stage and in accordance with the invention, the ring 20 is machined to form one or more zones of reduced thickness therein (step S3). More precisely, in the example described here as illustrated in Figures 4 and 5, a zone of reduced thickness 21 is machined on the face 20a of the ring 20 intended to form the internal face of the final air inlet lip. The remaining parts 22, 23 and 24 of the ring 20 located outside the zone of reduced thickness have a thickness corresponding to the initial sheet thickness of the ring 20.
[0056] The zone(s) of reduced thickness extend over specific portions of the ring. The location of each portion is chosen in particular according to the mechanical properties of the final lip. In other words, the zone(s) of reduced thickness are preferably machined on portions of the ring which will then constitute parts of the air inlet lip which are subject to little mechanical stress. It is thus possible to reduce the thickness of the sheet metal locally over specific portions without altering the mechanical strength properties expected for the lip.
[0057] After machining, the reduced thickness zone 21 has a thickness EP2[ less than the thicknesses EP22, EP23 and EP24 respectively of the remaining parts 22, 23 and 24 as illustrated in [Fig.5].
[0058] The thickness EP2[ of the reduced thickness zone 21 corresponds at most to 90% of the initial thickness of the sheet of the ring 20. By way of example, the initial thickness of the sheet constituting the ring 20 and corresponding to the thickness of the remaining parts 22, 23 and 24 is 2 mm while the thickness of the reduced thickness zone 21 is 1.6 mm.
[0059] A truncated cone 30 illustrated in [Fig. 6] is then formed from the ring 20 by the known technique of sheet metal rolling (step S4). The truncated cone has on its internal surface 30a a zone of reduced thickness 31 corresponding to the zone of reduced thickness 21 of the ring 20 and parts 32, 33 and 34 corresponding respectively to the remaining parts 22, 23 and 24 of the ring 20.
[0060] Once formed, the truncated cone 30 is preformed, for example by embossing and / or stamping, into an air inlet lip blank 40 having a general shape close to that of the final lip, i.e. already having a U-shape in section as shown in [Fig. 7] (step S5). The lip blank 40 comprises on its internal surface 40a a zone of reduced thickness 41 corresponding to the zone of reduced thickness 31 of the truncated cone 30 and parts 42, 43 and 44 corresponding respectively to the parts 32, 33 and 34 of the truncated cone 30.
[0061] The final shaping of an air inlet lip is then carried out by hydroforming or internal high-pressure forming (step S6). More precisely and as illustrated in [Fig. 8], the blank 40 is placed in a mold 51, also called a die, of a hydroforming tool 50, the die 51 comprising a three-dimensional surface 510 corresponding to the shape of the lip preform to be obtained. The tool 51 is then hermetically sealed by a cover 52 as illustrated in [Fig.9]. The cover 52 has an opening 520 through which a fluid 53 is introduced under high pressure. The high pressure P of the fluid 53 exerted on the blank 40 forces it to take the shape of the three-dimensional surface 510 of the die 51.
[0062] Once the hydroforming is completed, an air inlet lip 60 is obtained in a single piece having a shape of revolution having a U-shape in section. The air inlet lip is then demolded as shown in [Fig. 10]. The air inlet lip 60 has on its internal surface 60a a zone of reduced thickness 61 corresponding to the zone of reduced thickness 41 of the lip blank and more specifically to the zone of reduced thickness 21 initially produced in the ring 20.
[0063] In the example described here, the reduced thickness zone 61 extends on the side of the internal face 60a of the lip 60 over a determined portion at the level of the external wall 65, the lip 60 comprising an internal wall 68 extending the external wall 65 inside the lip 60. The external wall 65 comprises parts 62, 63 and 64 having a thickness greater than the thickness of the reduced thickness zone 61, the parts 62, 63 and 64 corresponding respectively to the remaining parts 22, 23 and 24 of the ring 20. The parts 62, 63 and 64 therefore have the same thickness as the remaining parts 22, 23 and 24.
[0064] The part 62 corresponding essentially to the internal wall 65 and the part 64 are intended to be fixed on the nacelle of an aeronautical engine. They therefore constitute parts of the air intake lip which are intended to be mechanically stressed and must therefore have mechanical resistance properties. It is therefore not desirable to reduce the thickness of the sheet metal in these parts. The part 63 is intended to be used for fixing an added part (for example a hatch). Since this part must have mechanical resistance properties to ensure that the attachment of the added part is maintained, it is also not desirable to reduce the sheet metal thickness.
[0065] On the other hand, the reduced thickness zone 61 extends over a portion of the external wall 65 of the lip 60 which has only an aerodynamic function, namely ensuring the aerodynamic flow of air towards the outside of the nacelle. The thickness of this portion of the lip 60 can, consequently, be reduced without harming the overall mechanical properties of the air inlet lip.
[0066] This results in an air inlet lip which has a reduced overall mass thanks to the presence of the zone of reduced thickness while having the required holding and mechanical resistance properties in operation.
[0067] In the example described here, openings are further made in the external wall 65 of the lip 60. More precisely, a first portion 661 is cut out on the wall external 65 in order to create a first opening 66 at the level of the part 63. An added part (not shown in [Fig. 10]), for example a hatch, can then be fixed on the edge 662 of the opening 66 which here has a thickness EP23 sufficient to ensure its fixing and its maintenance.
[0068] A second portion 671 is also cut out of the external wall 65 in order to produce a second opening 67 at the level of the reduced thickness zone 61. The opening 67 is not intended to support an added part. It can therefore be produced in the reduced thickness zone 61 without altering the overall mechanical properties of the lip 60.
[0069] [Fig. 11] describes the steps of a method of manufacturing an annular sector of an air inlet lip according to the invention.
[0070] As illustrated in [Fig. 12], the method begins by providing a sheet metal plate 100, for example made of aluminum alloy (step S10). The sheet metal 100 may be an integral plate or obtained by assembling several plates fixed together by welding in order to obtain large sheet metal plates from smaller unit sheet metal plates.
[0071] The sheet metal plate 100 is then cut to form a portion of ring 120 illustrated in [Fig.13] (step SU).
[0072] At this stage and in accordance with the invention, the ring portion 120 is machined to form one or more zones of reduced thickness therein (step S13). More specifically, in the example described here as illustrated in FIGS. 14 and 15, a zone of reduced thickness 121 is machined on the face 120a of the ring portion 120 intended to form the internal face of the final air inlet lip. The remaining parts 122 and 124 of the ring portion 120 located outside the zone of reduced thickness have a thickness corresponding to the initial sheet metal thickness of the ring portion 120.
[0073] The zone(s) of reduced thickness extend over specific areas of the ring portion. The location of each zone is chosen in particular according to the mechanical properties of the final lip. In other words, the zone(s) of reduced thickness are preferably machined on areas of the ring portion which will then constitute parts of the air inlet lip which are subject to little mechanical stress. It is thus possible to reduce the thickness of the sheet metal locally over specific areas without altering the mechanical strength properties expected for the lip.
[0074] After machining, the reduced thickness zone 121 has a thickness Epm less than the thicknesses EPi22 and EPi24 respectively of the remaining parts 122 and 124 as illustrated in [Fig. 15].
[0075] The thickness Epl21 of the reduced thickness zone 121 corresponds at most to 90% of the initial thickness of the sheet of the ring portion 120. By way of example, the thickness initial thickness of the sheet constituting the ring portion 120 and corresponding to the thickness of the remaining parts 122 and 124 is 2 mm while the thickness of the reduced thickness zone 121 is 1.6 mm.
[0076] A truncated cone portion 130 illustrated in [Fig. 16] is then formed from the ring portion 120 by the known technique of sheet metal rolling (step S14). The truncated cone portion has on its inner surface 130a a reduced thickness zone 131 corresponding to the reduced thickness zone 121 of the ring 120 and portions 132 and 134 corresponding respectively to the remaining portions 122 and 124 of the ring portion 120.
[0077] Once formed, the truncated cone portion 130 is preformed, for example by embossing and / or stamping, into a blank of an annular air inlet lip sector 140 having a general shape close to that of the final lip, i.e. already having a U-shape in section as shown in [Fig. 17] (step S15). The annular sector blank 140 comprises on its internal surface 140a a zone of reduced thickness 141 corresponding to the zone of reduced thickness 131 of the truncated cone portion 130 and parts 142 and 144 corresponding respectively to the parts 132 and 134 of the truncated cone portion 130.
[0078] The final shaping of an annular air inlet lip sector is then carried out by hydroforming or internal high-pressure forming (step S16). More precisely and as illustrated in [Fig. 18], the blank 140 is placed in a mold 151, also called a die, of a hydroforming tool 150, the die 151 comprising a three-dimensional surface 1510 corresponding to the shape of the lip preform to be obtained. The tool 151 is then hermetically closed by a cover 152 as illustrated in [Fig. 19]. The cover 152 comprises an opening 1520 through which a fluid 153 is introduced under high pressure. The high pressure P of the fluid 153 exerted on the blank 140 forces it to take the shape of the three-dimensional surface 1510 of the die 151.
[0079] Once the hydroforming is completed, an annular air inlet lip sector 160 is obtained in a single piece having a shape of revolution having a U-shape in section. The annular air inlet lip sector is then demolded as shown in [Fig. 20]. The annular sector 160 has on its internal surface 160a a zone of reduced thickness 161 corresponding to the zone of reduced thickness 141 of the annular sector blank and more specifically to the zone of reduced thickness 121 initially produced in the ring portion 120.
[0080] In the example described here, the zone of reduced thickness 161 extends on the side of the internal face 160a of the annular sector 160 over a determined portion at the level of the external wall 165, the annular sector 160 comprising an internal wall 166 extending the external wall 165 inside the annular sector 160. The external wall 165 comprises parts 162 and 164 having a thickness greater than the thickness of the reduced thickness zone 161, the parts 162 and 164 corresponding respectively to the remaining parts 122 and 124 of the ring portion 20. The parts 162 and 164 therefore have the same thickness as the remaining parts 122 and 124.
[0081] The part 162 corresponding essentially to the internal wall 165 and the part 164 are intended to be fixed on the nacelle of an aeronautical engine. They therefore constitute parts of an air intake lip which are intended to be mechanically stressed and must therefore have mechanical resistance properties. It is therefore not desirable to reduce the thickness of the sheet metal in these parts.
[0082] On the other hand, the reduced thickness zone 161 extends over a portion of the external wall 165 of the annular sector 160 which has only an aerodynamic function, namely ensuring the aerodynamic flow of air towards the outside of the nacelle. The thickness of this portion of the annular sector 160 can, consequently, be reduced without harming the overall mechanical properties of the air inlet lip.
[0083] This results in an annular air inlet lip sector which has a reduced overall mass thanks to the presence of the zone of reduced thickness while having the required holding and mechanical resistance properties in operation.
[0084] An air inlet lip can be obtained by assembling together several annular sectors like the one described above.
[0085] One or more openings may further be made in the annular air inlet lip sector. As explained above, if the opening is not intended to fix and hold an insert, it may be made in the area of reduced thickness. Otherwise, the opening is made in an area of the annular sector having sufficient thickness to ensure the fixing and holding of the insert.
Claims
Claims
1. A method of manufacturing an air intake lip comprising: - providing a sheet metal plate (10), - cutting the sheet metal plate so as to form a ring (20), - mechanically machining one or more reduced thickness zones (21) in the ring (20), each reduced thickness zone being produced on a face (20a) of the ring corresponding to the internal surface of a final air intake lip, - shaping the ring so as to obtain an air intake lip (60) having a U-shaped section and comprising on its internal surface (60a) one or more reduced thickness zones (61), characterized in that the method further comprises, after cutting the sheet metal plate (10) and before shaping the ring (20): - forming a truncated cone (30) from the ring, - preforming a blank air inlet lip (40) from the truncated cone,- placing the blank (40) opposite a three-dimensional forming surface (510) of a die (51) of a hydroforming tool (50), the shaping of the air inlet lip being carried out by hydroforming the blank on the three-dimensional surface of the die.,
2. Method according to claim 1, in which the zone(s) of reduced thickness (61) have a thickness (Ep2i) corresponding to at most 90% of the thickness (EP22, EP23, EP24) of the sheet metal plate.
3. A method according to claim 1 or 2, further comprising, after shaping the ring (20), making one or more openings in the wall (65) of the air inlet lip.
4. A method of manufacturing an annular air inlet lip sector comprising: - providing a sheet metal plate (100), - cutting the sheet metal plate so as to form a ring portion (120), - mechanically machining one or more reduced thickness zones (121) in the ring portion (120), each reduced thickness zone being produced on a face (120a) of the ring portion corresponding to the internal surface of a final annular air inlet lip sector, - shaping the ring portion so as to obtain a air inlet lip sector (160) having a U-shape in section and comprising on its internal surface (160a) one or more zones of reduced thickness (161), characterized in that the method further comprises, after cutting the sheet metal plate (100) and before shaping the ring portion (120): - forming a truncated cone portion (130) from the ring portion, - preforming an annular sector blank (140) from the ring portion, - placing the blank (140) opposite a three-dimensional forming surface (1510) of a die (151) of a hydroforming tool (150), the shaping of the air inlet lip sector (160) being carried out by hydroforming the blank on the three-dimensional surface of the die.
5. Method according to claim 4, in which the zone(s) of reduced thickness (161) have a thickness (EPi2i) corresponding to at most 90% of the thickness (EP[22, EPi24) of the sheet metal plate.
6. A method according to claim 4 or 5, further comprising, after shaping the ring portion (120), making one or more openings in the wall (165) of the annular air inlet lip sector (160).
7. A method of manufacturing an air inlet lip comprising producing annular air inlet lip sectors (160) according to any one of claims 4 to 6 and assembling said sectors so as to obtain an air inlet lip sector having a U-shape in section and comprising on its internal surface one or more zones of reduced thickness (161).