Processes for manufacturing carbon-coated particles from recovered carbon and other particles

By coating rC particles with carbon using energy sources and hydrocarbon deposition, the method enhances their rubber reinforcement properties, addressing the limitations of rC and achieving performance comparable to virgin carbon black.

FR3148241A1Pending Publication Date: 2024-11-01CABOT CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2024004420
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-26
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

Recovered carbon (rC) particles exhibit poor rubber reinforcement properties due to low surface activity, large aggregates, and compact structure, making them unsuitable as a substitute for carbon black in rubber applications.

Method used

A method of coating rC particles with carbon using energy sources like hot gas, microwave energy, induction energy, direct current, or solar radiation, and introducing a hydrocarbon source to form carbon deposits, enhancing their surface activity and structural properties.

Benefits of technology

The carbon-coated rC particles demonstrate improved tensile modulus, hysteresis, tear strength, and fatigue life, comparable to virgin carbon black, while reducing carbon emissions and greenhouse gas intensity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000047_0000
    Figure 00000047_0000
  • Figure 00000047_0001
    Figure 00000047_0001
Patent Text Reader

Abstract

The invention relates to methods for forming carbon-coated particles. The methods for forming coated particles involve exposing the particles to an energy source, which is at least one of the following: hot gas, microwave energy, induction energy, direct current passing through the particles, electromagnetic radiation, or solar radiation, so as to form heated particles. They also involve supplying a hydrocarbon source, in the form of a gas or vapor, to the chamber, such that the hydrocarbon source pyrolyzes, at least partially, within the chamber to form carbon deposits, thereby coating the heated base particles with the carbon deposits and forming the carbon-coated particles. The invention further relates to coated particles produced by one of the methods of the present invention. The invention also relates to the advantages obtained through the methods.
Need to check novelty before this filing date? Find Prior Art

Description

Title of Invention: Methods of manufacturing carbon-coated particles from recovered carbon and other particles

[0001] The present invention relates to methods for coating various particles with a carbon coating, such as carbon coating of reclaimed carbon and other carbon particles and other types of particles. The present invention further relates to carbon-coated carbon particles and other carbon-coated particles, as well as articles containing the same.

[0002] There is increasing demand and effort in the field of recycling materials in order to prevent materials from being disposed of in landfills and avoid further depletion of natural resources.

[0003] Thus, the use of recovered carbon (rC) from used tires (or other sources) as a substitute for carbon black (CB) in rubber reinforcement applications may be a promising strategy. However, recovered carbon suffers from poor rubber reinforcement, such as low tensile modulus, low tear strength, and / or low fatigue life, compared to CB with the same surface area and structure as measured by OAN. One hypothesis was that one of the main causes of poor rubber reinforcement by rC was its low surface activity.Other possible causes of poor rubber reinforcement include a high percentage of large, hard-to-disperse aggregates of recovered particles present in the rubber as defects in the form of large, undispersed particles, which would significantly reduce the tensile strength, tear resistance, and fatigue life of the rubber. However, another possible cause of poor reinforcement of recovered carbon is its compact structure, which is very different from the more extensive fractal structure of carbon black that allows for high rubber reinforcement. Besides recovered carbon, other materials from recycling or other materials may have the same or similar problems as recovered carbon.

[0004] Accordingly, there is a need in the industry to develop processes that can utilize rC particles and other similar particles that are unsuitable as such for use as filler in rubber reinforcement and other applications so as to make them a suitable replacement or partial replacement for virgin carbon black. For example, coating reclaimed carbon particles with a fresh carbon surface similar to carbon black is expected to improve its activity of surface. Although some techniques may have been attempted to coat carbon particles with carbon, there is a demand in the industry to provide other particle coating processes such as rC, which do not rely on carbon black reactors or similar techniques. SUMMARY OF THE PRESENT INVENTION

[0005] A feature of the present invention is to provide methods for coating recovered carbon with a carbon layer.

[0006] An additional feature of the present invention is to provide methods for coating particles, other than reclaimed carbon, with a layer of carbon, such as particles that are non-ASTM reinforcement grade particles.

[0007] Another feature of the present invention is to provide methods for making recovered carbon a more viable material for use as a reinforcing material in applications such as rubber.

[0008] Another additional feature of the present invention is to provide methods for modifying one or more properties of the recovered carbon or other particles so as to make it a more viable material for use as a reinforcing grade filler.

[0009] Further, a feature of the present invention is to provide methods for treating reclaimed carbon and / or other carbon particles and / or non-ASTM reinforcing grade particles and non-carbon-containing particles, such that the particles can impart comparable rubber reinforcing properties, such as, but not limited to, acceptable tensile modulus, hysteresis (as measured by tan delta), tear strength and / or fatigue life compared to virgin carbon black.

[0010] Another feature of the present invention is to provide methods for treating reclaimed carbon and / or other carbon particles and / or other non-ASTM reinforcing grade particles and non-carbon-containing particles, such that the particles can impart superior rubber reinforcing properties, such as, but not limited to, acceptable tensile modulus, hysteresis (as measured by tan delta), tear strength and / or fatigue life compared to the untreated starting material.

[0011] An additional feature of the present invention is to provide carbon-coated reclaimed carbon and / or carbon-coated particles having one or more different properties compared to non-carbon-coated reclaimed carbon (e.g., reclaimed carbon or ground reclaimed carbon).

[0012] An additional feature of the present invention is to provide methods for manufacturing carbon-coated recovered carbon and / or particles carbon coated with reduced or zero generation of carbon dioxide emissions.

[0013] An additional feature of the present invention is to provide methods for manufacturing carbon-coated recovered carbon and / or carbon-coated particles having low greenhouse gas intensity and / or high amounts of recycled content.

[0014] To achieve these and other advantages, and in accordance with the objectives of the present invention, as embodied and broadly described herein, the present invention, in part, relates to methods for forming carbon-coated base particles, e.g., carbon-coated carbon particles. More particularly, one method relates to methods for forming carbon-coated base particles, the method comprising introducing base particles into a chamber and exposing the base particles to an energy source that is at least one of a hot gas, microwave energy, induction energy, a direct current passing through said base particles, electromagnetic radiation, or solar radiation, so as to form heated base particles. The method comprises introducing a hydrocarbon source that comprises or is a gas or vapor into the chamber.The hydrocarbon source pyrolyzes, at least in part, in the chamber to form carbon deposits, and thereby coat the heated base particles with the carbon deposits and form the carbon-coated base particles. Examples of base particles that are used in the process may be or include reclaimed carbon particles or other carbon particles that are non-ASTM reinforcement grade particles.

[0015] The present invention further relates to the use of the above method with particles which, for example, have lower amounts of carbon in the particle compared to the recovered carbon.

[0016] The present invention further relates, in part, to a method for forming carbon-coated precipitated silica particles. The method may include introducing precipitated silica particles into a chamber and exposing the precipitated silica particles to microwave energy or other forms of energy as detailed herein, to form heated precipitated silica particles. The method further includes introducing into the chamber a hydrocarbon source that comprises or is a gas or vapor. The hydrocarbon source pyrolyzes, at least in part, in the chamber to form carbon deposits, and thereby coat the heated precipitated silica particles with the carbon deposits and form the carbon-coated precipitated silica particles.

[0017] Further, the present invention relates, in part, to carbon-coated particles and carbon-coated particles formed by the methods of the present invention.

[0018] The present invention further relates to products and / or articles, such as, but not limited to, tires, tire parts and / or elastomeric composites formed, at least in part, from the coated particles of the present invention.

[0019] It is to be understood that the above general description and the following detailed description are given by way of example only and are intended to provide further explanation of the present invention as claimed.

[0020] The accompanying drawings, which are incorporated in and constitute a part of this application, illustrate various features of the present invention and, together with the description, serve to explain the principles of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] [Fig.l] is a simplified cross-sectional view of an example of a system with a chamber suitable for use in a method of the present invention.

[0022] [Fig.2] is a simplified cross-sectional view of another example of a two-chamber system suitable for use in a method of the present invention.

[0023] The figures are not to scale and are provided as simplified views and do not necessarily represent all possible embodiments or components that may be present. DETAILED DESCRIPTION OF THE PRESENT INVENTION

[0024] The present invention relates to methods for coating various types of particles with carbon, carbon-coated particles obtained thereby, and the concomitant production of hydrogen. The particles that are coated may be carbon particles. The particles that are coated may be carbon-containing particles. The particles that are coated may be particles not of ASTM reinforcement grade. The carbon particles that may be coated include reclaimed carbon. The particles that are coated may be non-carbon-containing particles such as silica particles, preferably precipitated silica particles.

[0025] A method of the present invention relates to the formation of carbon-coated base particles. This method includes, comprises, consists essentially of, or consists of introducing base particles into a chamber and exposing the base particles to an energy source which is at least one of microwave energy, induction energy, direct current passing through said base particles, electromagnetic radiation, or solar radiation, so as to form heated base particles. The method comprises introducing a hydrocarbon source which includes, comprises, consists essentially of, or consists into a gas or vapor in the chamber. The hydrocarbon source pyrolyzes, at least in part, in the chamber to form carbon deposits, and thereby coats the heated base particles with the carbon deposits to form the carbon-coated base particles. The base particles may comprise, consist essentially of, consist of, include, or be a) reclaimed carbon particles and / or b) other carbon particles that are non-ASTM reinforcement grade particles. The temperature of the heated base particles may be at least 800°C, at least 900°C, at least 1000°C, at least 1100°C, at least 1200°C, at least 1300°C, at least 1400°C, or at least 1500°C, for example, 900 to 1200°C or 1300 to 1600°C.

[0026] The base particles that are introduced into a chamber may be different types of carbon particles. Furthermore, as described later, instead of carbon particles, the particles may be particles that contain or do not contain carbon. In the context of the present invention, a carbon particle is a particle that is primarily composed of carbon. The carbon particle generally has carbon as a major component (e.g., carbon is present at least 75%, at least 80%, at least 85%, at least 90%, at least 95%, at least 98%, at least 99%, e.g., 75% to 95% or 75% to 100% by weight relative to the total weight of the particle). Examples of carbon particles include, but are not limited to, recovered carbon (rC) particles.The rC can optionally be disaggregated (i.e., disaggregated recovered carbon) or disaggregated rC that is disaggregated from recovered carbon aggregates (i.e., recovered aggregates).

[0027] rC, such as rC aggregates, are commercially available. Generally, rC aggregates are derived from the pyrolysis of tires and / or other rubber or plastic materials that contained filler materials or reinforcing materials, such as carbon black. rC is composed primarily of carbon black that has been used to reinforce rubber or plastic. The source tire and other rubber or other source material contain components that can be pyrolyzed, such as the rubber components, and due to the high temperatures described herein for the methods of the present invention, at least a portion of these components are pyrolyzed to produce pyrolysis carbon. The pyrolysis carbon is processed to remove at least one macroscopic contaminant such as fabric or wire and produce recovered carbon (rC).The rC may optionally be milled to reduce the average particle size by jet milling or as described in WO2023122582. .

[0028] Carbon particles that are non-ASTM reinforcement grade particles are carbon particles that would not meet one of the ASTM 100, 200, or 300 series carbon black fillers, or would not meet any of the ASTM 500, 600, or 700 series carbon black fillers. Examples of such a carbon particle may be carbon black, but also include, but are not limited to, solid hydrothermal carbon (HTC), silicon-treated carbon black, silica-coated carbon black, graphene, reduced graphene oxide, single-walled carbon nanotubes, multi-walled carbon, carbon nanostructures, carbon black-coated particles, and biochar. In addition, the reclaimed carbon particles mentioned above would also not meet this ASTM standard.

[0029] Instead of carbon particles, other types of particles that have a certain carbon content (e.g., from 0% to 75% by weight or from 10% by weight to 60% by weight or from 10% by weight to 50% by weight or from 10% by weight to 40% by weight relative to the total weight of the particle) may be used. For example, the particles may be graphene oxide, lignin, or nanocrystalline cellulose. Other examples of carbon-containing particles include particles of biological origin. Specific examples of particles of biological origin include, but are not limited to, polysaccharides or modified polysaccharides.

[0030] Instead of carbon particles, particles that have low or no carbon content (e.g., less than 10% by weight carbon) may be used. For example, the particles may be precipitated silica, rice hull silica, clays, nanoclays, diatomaceous earth, metal oxides, or metal carbonates.

[0031] Optionally, and to contribute to more efficient heating of the base particles and further allow for more uniform or efficient coating of the base particles, the base particles may have one or more of the following particle size parameters: A: Volume weighted average aggregate size less than 2 microns (e.g. less than 1.75 micron, less than 1.5 micron, less than 1 micron, less than 0.9 micron, less than 0.8 micron, less than 0.7 micron, less than 0.6 micron, e.g. 0.5 micron to 1.9 micron, 0.5 micron to 1.7 micron, 0.5 micron to 1.5 micron, 0.5 micron to 1.25 micron, 0.5 micron to 1 micron, 0.5 micron to 0.8 micron, 0.6 micron to 1.9 micron, 0.7 micron to 1.9 micron, 0.8 micron to 1.9 micron, 0.9 micron to 1.9 micron, 1 micron to 1.9 micron); B: D10 aggregate size less than 400 nm (e.g., less than 375 nm, less than 350 nm, less than 325 nm, less than 300 nm, less than 275 nm, less than 250 nm, less than 225 nm, less than 200 nm, less than 175 nm, less than 150 nm, e.g., 140 nm to 390 nm, 150 nm to 390 nm, 160 nm to 390 nm, 175 nm to 390 nm, 180 nm to 390 nm, 190 nm to 390 nm, 200 nm to 390 nm, 210 nm to 390 nm, 220 nm to 390 nm, 230 nm to 390 nm, 240 nm to 390 nm, 250 nm to 390 nm, 260 nm to 390 nm, 275 nm to 390 nm, 280 nm to 390 nm, 300 nm to 390 nm, 310 nm to 390 nm, 320 nm to 390 nm, 330 nm to 390 nm, 340 nm to 390 nm, 350 nm to 390 nm, 360 nm to 390 nm, 380 nm to 390 nm, 400 nm to 400 nm, 410 nm to 410 nm, 420 nm to 420 nm, 430 nm to 430 nm, 440 n nm to 390 nm, from 170 nm to 390 nm, from 180 nm to 390 nm, from 190 nm to 390 nm, from 200 nm to 390 nm, from 140 nm to 380 nm, from 140 nm to 350 nm, from 140 nm to 300 nm, from 140 nm to 250 nm, from 140 nm to 200 nm); C: D25 aggregate size less than 1 micron (e.g., less than 0.9 micron, less than 0.8 micron, less than 0.7 micron, less than 0.6 micron, less than 0.5 micron, less than 0.4 micron, less than 0.3 micron, less than 0.25 micron, less than 0.2 micron, e.g., 0.2 micron to 0.9 micron, 0.3 micron to 0.9 micron, 0.4 micron to 0.9 micron, 0.5 micron to 0.9 micron, 0.2 micron to 0.8 micron, 0.2 micron to 0.5 micron, 0.2 micron to 0.4 micron); D: D50 aggregate size less than 4 microns (e.g., less than 3.5 microns, less than 3 microns, less than 2.5 microns, less than 2 microns, less than 1.5 microns, less than 1 micron, less than 0.75 microns, less than 0.5 microns, less than 0.4 microns, less than 0.35 microns, e.g., 0.35 microns to 3.9 microns, 0.4 microns to 3.9 microns, 0.5 microns to 3.9 microns, 0.6 microns to 3.9 microns, 0.7 microns to 3.9 microns, 0.8 microns to 3.9 microns, 0.35 microns to 3.5 microns, 0.35 microns to 3 microns, 0.35 microns to 2.5 microns, from 0.35 micron to 2 microns, from 0.35 micron to 1.5 micron, from 0.35 micron to 1 micron, from 0.35 to 0.9 micron); E: D75 aggregate size less than 4.5 microns (e.g. less than 4 microns, less than 3.5 microns, less than 3 microns, less than 2.75 microns, less than 2.5 microns, less than 2.25 microns, less than 2 microns, less than 1.75 microns, less than 1.5 microns, less than 1.25 microns, less than 1 micron, e.g. 1 micron to 4 microns, 1 micron to 3.5 microns, 1 micron to 3 microns, 1 micron to 2.5 microns, 1 micron to 2 microns, 1 micron to 1.5 microns, 1.1 microns to 4 microns, 1.2 microns to 3.5 microns, 1.3 microns to 3 microns); F: D90 aggregate size less than 5 microns (e.g. less than 4.5 microns, less than 4 microns, less than 3.5 microns, less than 3 microns, less than 2.75 microns, less than 2.5 microns, less than 2.25 microns, less than 2 microns, e.g. 2 microns to 4.5 microns, 2 microns to 4.25 microns, 2 microns to 4 microns, 2 microns to 3.5 microns, 2 microns to 3 microns, 2.25 microns to 4 microns, 2.5 microns to 4 microns, 2.75 microns to 4 microns); G: Heterogeneity Index (HI) (defined as the ratio of the volume-weighted average aggregate size to the number-weighted average aggregate size) less than 20 (e.g., less than 15, less than 10, less than 9, less than 8, less than 7, less than 6, less than 5, less than 4, e.g., 4 to 15, 4 to 10, 4 to 9, 4 to 7, 4 to 6, 5 to 15, 6 to 15, 7 to 15, 8 to 12); H: % by mass > 1 micron or less than 60% (e.g. less than 55%, less than 50%, less than 45%, less than 40%, less than 40%, less than 35%, less to 30%, less than 25%, less than 20%, less than 15%, less than 10%, for example from 10% to 55%, from 10% to 50%, from 10% to 45%, from 10% to 40%, from 10% to 35%, from 10% to 30%, from 10% to 25%, from 15% to 45%, from 20% to 45%, from 25% to 45%, from 30% to 45%). The basic particles may have any or all of the above aggregate size parameters. Any combination of A to H is possible (e.g., one or more of A to H, at least two of A to H, at least three of A to H, at least four of A to H, at least five of A to H, at least six of A to H, at least seven or all of A to H).

[0032] A disaggregated rC relative to rC aggregates may have one or more of average aggregate size, D10 aggregate size, D25 aggregate size, D50 aggregate size, D75 aggregate size, D90 aggregate size, HI and / or mass % > 1 micron, reduced by 10%, reduced by 20%, reduced by 50%, reduced by 75% or more.

[0033] The rC may contain fractions of non-carbon material. For example, the rC may contain from 1 wt% to at least 20 wt% (based on the total weight of the rC) of non-carbon material or components, such as, but not limited to, silica particles and / or ZnO and the like.

[0034] With respect to the chamber, the chamber may be of any suitable shape and size and made of a material that allows energy from an energy source to contact the base particles to obtain heated base particles and cause the hydrocarbon source to pyrolyze. For example, the chamber may be a fluidized bed reactor, an ablative pyrolysis reactor, a vacuum pyrolysis reactor, a falling type fixed bed reactor, or a solar pyrolyzer.

[0035] With respect to the energy sources to which the base particles are exposed so as to obtain heated base particles, these energy sources include, but are not limited to, exposure to a hot gas, resistive heating, microwave energy, induction energy, direct current passing through base particles, electromagnetic radiation, or solar radiation. Heating of the particles may be carried out by means of dielectric heating or induction heating. For methods relying on the passage of an electric current through the base particles, it is preferable that the base particles exhibit electrical conductivity.

[0036] Microwave energy can be obtained from any type of microwave generator. For example, the microwave generator may be a magnetron that includes a vacuum-sealed chamber with a heated filament and a magnetic field. When the filament is heated, it emits electrons that are accelerated by the magnetic field, creating a stream of electrons that travels to an anode. As electrons pass through a resonant cavity, they oscillate and produce a high-frequency electromagnetic field, which is then directed out of the cavity by an antenna. Other types of microwave generators include klystrons, traveling wave tubes, semiconductor devices, and the like. The microwave generator may be located inside the chamber or adjacent to the chamber. Commercial examples include, but are not limited to, MUEGGE microwave generators, CEM microwave generators, such as the CEM LABWAVE and AIRWAVE models, THERMEX THERMATRON microwave generators, and the like.

[0037] The microwave generator may produce electromagnetic radiation with frequencies of at least 0.5 GHz, for example from 0.5 GHz to 300 GHz or more.

[0038] The microwave generator may operate at power levels ranging from 300 watts to at least 4 MW, for example from 1 kW to 1 MW, from 10 kW to 500 kW, from 100 kW to 400 kW or from 200 kW to 300 kW.

[0039] Induction energy may be provided by an induction heater. Induction heating is a non-contact method of heating a material using a strong magnetic field that induces an alternating current in the material, which excites the atoms of the material and heats it. Induction heaters incorporate a coil powered directly by a power supply. Also called an inductor, the coil is used to transfer energy from a power unit to the material. Inductors vary in complexity from a simple coiled solenoid comprising a plurality of turns of copper tubing wrapped around a mandrel, to a precision item machined from solid copper, brazed and soldered together.Commercial examples of such induction heating devices include, but are not limited to, AMBRELL's EASYHEAT and EKOHEAT induction heating systems, INDUCTOHEAT's INDUCTOFORGE induction heating systems, ENRX's HEATLINE induction heating devices, and the like.

[0040] The induction heating device, for example, may operate at a frequency of at least 5 kHz, for example from 5 kHz to 500 kHz or more. The induction heating device may operate at an induction heating energy level of at least 50 MJ / kg, for example from 50 MJ / kg to 250 MJ / kg or more (kg being the amount of particles treated in the chamber).

[0041] A direct current may pass through the base particles from a direct current power source to heat the base particles. The direct current power source may include batteries, power supplies, electrochemical cells, renewable energy systems, and the like.

[0042] The DC power source, for example, may have a voltage of at least 1 V to 400 V or more. For example, the voltage of the DC power source may range from 10 V to 300 V, from 50 V to 200 V, or from 100 V to 150 V.

[0043] Electromagnetic radiation includes waves of the electromagnetic field, such as radio waves, infrared, microwaves, visible light, ultraviolet, X-rays, induction heating, and gamma rays. Examples of microwave generators and induction heating generators are described above. Other devices that generate electromagnetic radiation include infrared heaters, lasers, radio frequency heaters, and the like.

[0044] The frequency and power required for electromagnetic radiation generators depend on the type of electromagnetic radiation being generated. For example, the frequency range of infrared heaters may be from 1 pm to 100 pm, and the power levels may range from 1 W to 100 kW. The frequency range of radio frequency heaters may be from 1 kHz to 100 MHz, and the power levels may range from 1 W to 100 kW. The frequency of laser systems may be from 1 Hz to 100 tHz, and the power levels may range from 1 mW to 100 kW.

[0045] Solar radiation may be used to heat particles such as base particles. The present invention may use solar radiation concentrators that increase the intensity of the solar radiation to heat the base particles. The solar radiation concentrators may include solar thermal collectors, solar furnaces, solar ovens, solar dryers, and the like. These devices use parabolic troughs, parabolic collectors, collector towers, mirrors, lenses, reflectors, and the like to amplify and concentrate the heat from the solar radiation onto the base particles.

[0046] The energy source used may optionally be produced from renewable energy generation, such as renewable electricity (e.g., solar-generated, wind-generated, and the like).

[0047] With respect to the hydrocarbon source, as indicated, the hydrocarbon source includes, comprises, consists essentially of, consists of, or is a gas or vapor, which is introduced into the chamber. The hydrocarbon source can be considered a carbon source which can be pyrolyzed to form carbon deposits.

[0048] The hydrocarbon source may comprise or include or be natural gas.

[0049] Other examples of the hydrocarbon source include, but are not limited to, propane. The hydrocarbon source may comprise or include or be a vapor bio-oil, recycled oil, sustainable oil; a by-product of biofuel or biochemical production, or an oil derived from tires, for example from tire pyrolysis, an oil from plastic pyrolysis or recycling, or an oil from hydrothermal liquefaction or paper processing.

[0050] Other specific examples of hydrocarbon source include the following: • Glycerin from biodiesel production. • Other hydrocarbon by-products from biofuel production, e.g., distillers corn oil. • The vaporizable fraction of hydrocarbons resulting from hydrothermal liquefaction • Crude tall oil, the vaporizable component of tall oil pitch, turpentine, a resin or tall oil fats. • Used cooking oil. • Biomethane or renewable natural gas produced from the decomposition of sludge, wastewater, agricultural waste or landfill material. • Oil derived from lignin. • Vegetable oils, edible or inedible (e.g. jatropha oil). • Pyrolysis oil for tires from the pyrolysis of tires or rubber articles made from natural rubber. • Hydrocarbon derived from algae or other uncultivated plants. • Hydrocarbon derived from or produced by cyanobacteria. • Hydrocarbon derived from black liquor from the manufacturing process of paper. • Vaporizable oil derived from animal waxes or fats, for example lanolin, lard or tallow. Oil produced by pyrolysis, thermal decomposition, or rendering of animal processing by-products, such as turkey carcasses. Recycled oil or vaporizable hydrocarbons can be: • Vaporizable component of used engine oil. • Hydrocarbon oil or gas from the pyrolysis of plastic waste. • Hydrocarbon oil or gas from the pyrolysis of solid waste municipal. • Oil or hydrocarbon gas from the pyrolysis of end-of-life or used tires.

[0051] The hydrocarbon source may be from a single source or a mixture of at least two sources.

[0052] The hydrocarbon source may be introduced into the chamber as a single introduction or multiple introductions. For example, the hydrocarbon source may be introduced (e.g., injected) into the chamber through one or more feed jets or lines. The multiple feed lines may be located or distributed around the chamber such that the hydrocarbon source is uniformly distributed throughout the chamber, which may lead to better distribution of carbon deposits on the base particles resulting from pyrolysis of the hydrocarbon.

[0053] The amount of the hydrocarbon source may be an amount based on the amount of coated particles and / or the desired coating thickness and may depend on the carbon content and pyrolysis behavior of the hydrocarbon source. For example, the amount of hydrocarbon source may be 0.01 kg or more per 1 kg of particles, or 0.1 kg or more per 1 kg of particles, or at least 0.15 kg per 1 kg of particles. Other amounts below or above these ranges may also be used. The hydrocarbon source or the gas or vapor containing the hydrocarbon source may be a gas or vapor. The amount of hydrocarbon source including the gas or vapor may be any amount.The amount of hydrocarbon source in the gas or vapor may be, for example, at least 25% by volume, or at least 50% by volume, or at least 75% by volume, or at least 80% by volume, or at least 90% by volume, or at least 95% by volume, or at least 99% by volume.

[0054] The amount of hydrocarbon source that pyrolyzes is preferably 100% or about 100% by volume. Amounts less than 100% by volume are possible (e.g., 50% to 99% or 75% to 99%, or 85% to 99% or other amounts by volume based on the total volume of hydrocarbon source present). If amounts of the hydrocarbon source are not pyrolyzed, these unused amounts may optionally be recycled and used in subsequent batches to form carbon-coated particles.

[0055] According to one option, the hydrocarbon may be heated in addition to or instead of heating the base particles. The hydrocarbon may be heated to a temperature of at least 800°C, at least 900°C, at least 1000°C, at least 1100°C, at least 1200°C, at least 1300°C, at least 1400°C, or at least 1500°C, for example 900 to 1200°C or 1300 to 1600°C.

[0056] According to one option, an oxidizing atmosphere may be present in the chamber for at least a portion of the residence time that the base particles spend in the chamber. The oxidizing atmosphere may be at least achieved by introducing water into the chamber. Preferably, the oxidizing atmosphere is present in the early or initial stages of the residence time of the base particles in the chamber (e.g., present during the first half, or first third, or first quarter of the residence time). Preferably, oxygen is not introduced into the chamber during pyrolysis of the hydrocarbon source, thereby delaying or preventing the generation of carbon dioxide and carbon monoxide. Preferably, carbon dioxide and carbon monoxide are not introduced into the chamber during pyrolysis, thereby reducing or eliminating carbon dioxide and / or carbon monoxide in the gas stream discharged from the chamber after pyrolysis.

[0057] According to another option, the methods of the present invention may comprise carrying out steam oxidation of the base particles in the chamber. The steam oxidation may occur at any time during the residence time in the chamber. Preferably, this option is present in the early or initial stages of the residence time of the base particles in the chamber (e.g., present during the first half, or first third, or first quarter of the residence time).

[0058] Alternatively, the methods of the present invention may further comprise heating the carbon-coated particles, in a second step (subsequent step), either in the same chamber or in a different chamber, in a neutral atmosphere or a reducing atmosphere. Thus, once the base particles are coated with carbon by a method of the present invention, this additional step may occur.The supplemental heating may be achieved with the same or a different energy source than that used in the coating step or may be a completely different energy source, such as, but not limited to, a rotary kiln, a furnace, a carbon black reactor (e.g., a multi-stage carbon black reactor or a furnace carbon black reactor), or a modified carbon black reactor (e.g., a carbon black reactor that does not include any injection ports for a carbon black-forming feedstock). The heating chamber may be one or more thermally insulated chambers. The rotary kiln may be a directly heated rotary kiln or an indirectly heated rotary kiln. The rotary kiln may be a Feeco rotary kiln.

[0059] The heating in this optional second step may be a temperature of at least 300°C, or at least 500°C, or at least 800°C. The heating, if used, may depend on the function of the heater. If the heating is used to promote or further promote pyrolysis, higher heating temperatures may be more desirable (at least 500°C or at least 800°C). If the heating is used to promote or further promote the removal of volatiles, lower heating temperatures may be sufficient (e.g., at least 300°C). This optional heating may benefit from the fact that non-carbonaceous substances may be vaporized or otherwise removed, or at least some of these types of substances. The residence time for this optional second step may be at least 10 seconds or at least 10 minutes or at least 1 to 2 hours.

[0060] Optionally, an unreacting carrier gas or a non-reactive carrier gas may be present with the hydrocarbon source as a mixture or co-introduced into the chamber, or introduced before and / or after the introduction of the hydrocarbon source. Examples of such gases include, but are not limited to, nitrogen, argon, helium, or any combination thereof. The amount of this optional gas may be up to 20:80 (hydrocarbon:non-reactive gas volume ratio). Amounts lower or higher than this ratio are possible.

[0061] As indicated, the hydrocarbon gas may be introduced into the chamber at at least two locations in the chamber. And, according to one option, the optional non-reactive carrier gas may be introduced into the chamber either separately or with the hydrocarbon gas at at least two or more locations in the chamber.

[0062] With respect to introducing or feeding the base particles into the chamber, the base particles may be introduced into the chamber in batches, continuously, or semi-continuously. For example, the base particles may be placed on a tray that is then introduced into the chamber. Or, as an option, the base particles may be introduced into the chamber using a conveyor or other mechanical device that moves or introduces particles from one location to another.

[0063] The feed rate of the base particles into the chamber may be any feed rate and may depend on the size of the chamber and the energy source. Examples of suitable feed rates may be at least 100 kg / h or at least 250 kg / h, or at least 500 kg / h, or at least 750 kg / h, or at least 1000 kg / h, or at least 2000 kg / h, or at least 3000 kg / h, or at least 4000 kg / h, or at least 5000 kg / h of particles. The base particles may be positioned or located on a fixed bed within the chamber or may be placed on a movable tray or platform or conveyor for introduction into the chamber.

[0064] According to one option, the base particles may be on a moving bed which passes through the chamber.

[0065] In the methods of the present invention, when the hydrocarbon source pyrolyzes and the carbon deposits form, the carbon deposits may completely cover the base particles. Alternatively, the carbon may be deposited almost completely on the base particles such that at least 75%, or at least 80%, or at least 90%, or at least 95%, or at least 98%, or at least 99% of the exposed external surface of the base particles is coated by carbon deposits.

[0066] The resulting carbon-coated base particles may have a ratio of Raman D band area to Raman G band area (Id / I / g) of 0.5 to 2.45, for example 1 to 2.45 or 1.5 to 2.45. The Raman measurements are based on Gruber et al., "Raman Studies of Heat-Treated Carbon Blacks," Carbon Vol. 32 (7), pp. 1377-1382, 1994. The Raman spectrum of carbon includes two major "resonance" bands at about 1340 cm1 and 1580 cm1, referred to as the "D" and "G" bands, respectively. The D band is generally considered to be assigned to disordered sp2 carbon and the G band to graphitic or "ordered" sp2 carbon. Thus, a decrease in the D / G band ratio (also called ID / IG) corresponds to a more ordered crystal structure.

[0067] With respect to the coating on the base particles, the coating may have uniformly or substantially uniformly the same thickness around the outer surface of the base particles. For example, the thickness around the outer surface of the base particles (on average) may vary by less than 20%, less than 15%, less than 10%, less than 5% in terms of thickness around the outer surface of the base particles. This determination may be based on analysis of, for example, 5% or 2% or 1% by weight of the coated base particles in the batch.

[0068] The carbon deposit coating may have an average thickness of about 0.5 nanometers (nm) to about 500 nm or more, or about 0.75 nm to 500 nm or more, or about 1 nm to 500 nm or more, hence 0.5 nm to 450 nm, 0.5 nm to 400 nm, 0.5 nm to 350 nm, 0.5 nm to 300 nm, 1 nm to 250 nm, 1 nm to 200 nm, 1 nm to 150 nm, 1 nm to 125 nm, 1 nm to 100 nm, 1 nm to 75 nm, 1 nm to 50 nm, 1 nm to 25 nm, from 1 nm to 20 nm, from 1 nm to 15 nm, from 1 nm to 10 nm, from 1 nm to 7.5 nm, from 1 nm to 5 nm, from 1 nm to 2.5 nm, from 0.5 nm to 1 nm, from 0.5 nm to 5 nm, from 10 nm to 500 nm, from 50 nm to 500 nm, from 100 nm to 500 nm, from 250 nm to 500 nm, from 1 nm to 500 nm, from 7.5 nm to 50 nm, from 10 nm to 50 nm, from 1.25 nm to 5 nm, from 1.5 nm to 5 nm, from 2 nm to 5 nm, from 2.5 nm to 5 nm, from 3 nm to 5 nm, or any range based on any two values ​​described herein.The average thickness may be based for example on the analysis of, for example, 5% or 2% or 1% by weight of the carbon coated particles in the batch.

[0069] Alternatively, the methods of the present invention may result in the carbon deposits at least partially covering the base particles rather than coating 100% of the base particles. With partial coating, for example, 25-75% or 50-95% of the outer surface of the base particles (on average) are coated with carbon deposits.

[0070] The residence time of the base particles in the chamber is generally sufficient time for carbon deposits to form and coat the base particles. The residence time may depend on the amount of base particles heated, the type of energy source, the power or frequency of the energy source, the hydrocarbon source, and the heating temperature. The base particles, for example, may have a residence time in the chamber ranging from 1 second to 3 hours or more.The residence time can be from 1 second to 2.75 hours, from 1 second to 2.5 hours, from 1 second to 2.25 hours, from 1 second to 2 hours, from 1 second to 1.75 hours, from 1 second to 1.5 hours, from 1 second to 1h25, from 1 second to 1 hour, from 1 second to 45 minutes, from 1 second to 30 minutes, from 1 second to 15 minutes, from 1 second to 10 minutes, from 1 second to 5 minutes, from 1 second to 60 seconds, from 1 second to 30 seconds, from 5 seconds to 2 hours, from 5 seconds to 1 hour, from 5 seconds to 30 minutes, from 5 seconds to 15 minutes, from 5 seconds to 3 hours, from 30 seconds to 3 hours, from 1 minute to 3 hours, from 5 minutes to 3 hours, from 30 minutes to 3 hours, etc.

[0071] According to one option, the methods of the present invention can be carried out in the absence of any catalyst.

[0072] Alternatively, the methods of the present invention may be conducted in the absence of oxygen or an introduced oxygen-containing gas (e.g., a gas in which oxygen is more than 10% or more than 15% or more than 20% by volume based on the total volume of the gas).

[0073] Alternatively, the methods of the present invention may produce no or substantially no carbon dioxide or carbon monoxide (e.g., the amount of carbon dioxide and / or carbon monoxide generated is less than 0.5 kg of total CO2 and CO per kg of carbon-coated particles). In addition, the decomposition of the hydrocarbon results in the production of hydrogen gas. This hydrogen gas is thus produced with no or substantially no carbon dioxide, the carbon from the hydrocarbon being deposited as a solid on the base particles.For example, the gas exhausted from the chamber may contain at most 0.5 kg of combined carbon dioxide and carbon monoxide / kg of carbon-coated particles, for example at most 0.2 kg of carbon dioxide and carbon monoxide / kg of carbon-coated particles or at most 0.1 kg of carbon dioxide and carbon monoxide / kg of carbon-coated particles. The resulting hydrogen gas may be separated from other gases exhausted from the chamber by any technique known to those skilled in the art, for example, pressure swing absorption, hydrogen-permeable ceramic membranes, etc.

[0074] The gas vented from the chamber may contain at least 50% by volume hydrogen. In embodiments in which oxygen-containing gases, steam, or other carrier gases are not introduced into the chamber or are introduced only in limited amounts, the gas vented from the chamber may be at least 60% by volume, at least 70% by volume, at least 80% by volume, or at least 90% by volume hydrogen, e.g., 60% by volume to 90% by volume, 70% by volume to 95% by volume, or 80% by volume to 99% by volume. The resulting hydrogen may be used as a fuel source. In some embodiments, the gas vented from the chamber may be used as a fuel source without further purification processes.

[0075] The base particles that are heated by the energy source in the chamber are heated, for example, to a temperature of at least 800°C, or at least 900°C, or at least 1200°C, or at least 1500°C, for example from 800°C to 1600°C or from 800°C to 1400°C, or from 800°C to 1300°C, or from 800°C to 1200°C, or from 800°C to 1100°C, or from 800°C to 1000°C, or from 800°C to 900°C, or from 900°C to 1500°C, or from 1000°C to 1500°C, or from 1100°C to 1500 °C, or from 1200 °C to 1400 °C, or from 1200 °C to 1500 °C, or from 850 °C to 1500 °C, or from 875 °C to 1500 °C, or from 950 °C to 1500 °C, or from 1050 °C to 1500 °C, or from 1150 °C to 1500 °C, or from 1250 °C to 1500 °C, or from 1350 °C to 1500 °C, or from 800 °C to 1450 °C, or from 850 °C to 1450 °C, or temperatures above 1500 C, or any temperature range using any limits of any combination of ranges.

[0076] Reference to the temperature relating to the heating of the particles herein and throughout the description (for the other step(s)) is a temperature that is calculated based on thermodynamic calculations (without including possible heat losses through the chamber or reactor wall) of the materials introduced into the reactor. Alternatively, the chamber may have more than one zone where the heating occurs. When more than one zone is present for the heating chamber, one or more of the other zones may be used as additional heat treatment zones (i.e., have zone temperatures of at least 300°C or at least 500°C or at least 800°C) or may be used as quenching zones and / or for other purposes.If more than one zone is used to achieve zone temperatures of at least 300°C or at least 500°C or at least 800°C, each of these zones may have the same or similar or different heating temperatures. The residence times for each of these zones, if used, may be the same, similar or different. The temperatures and / or residence times of each of these zones, if used, may be at most 1%, at most 5%, at most 10%, at most 20%, at most . 30%, to at most 40%, to at most 50%, to at most 75% of each other or may differ by at least any of the percentages mentioned herein.

[0077] If the room has more than one heating zone, the energy source used in each zone may be the same or different.

[0078] According to one option, the chamber may comprise at least a first chamber and a second chamber. In such a configuration, in the first chamber, the base particles are exposed to at least one of the energy sources (e.g., microwave energy or induction energy) such that the base particles reach an average surface temperature of at least 800°C, at least 900°C, at least 1000°C, at least 1100°C, at least 1200°C, at least 1300°C, at least 1400°C, at least 1500°C, or at least 1600°C (e.g., 800°C to 1600°C or 800°C to 1500°C, or 1000°C to 1300°C) in the absence of any hydrocarbon source to obtain heated base particles. Then the heated base particles are transported to the second chamber where the introduction of the hydrocarbon source is carried out (and one of the other optional features of the hydrocarbon source).

[0079] In the second chamber, additional heating of the base particles may or may not occur. Due to the high temperature to which the particles may be heated, this high temperature may be sufficient that no additional heating is required in the second chamber, and the temperature causes pyrolysis of the hydrocarbon source in the second chamber. Although not required, as an option, the base particles in the second chamber may be subjected to additional heating by another energy source or the same energy source as in the first chamber. The type of energy source may be the same or different from the energy source used in the first chamber.

[0080] When another heating source is used in the second chamber, the heating source may maintain the heated base particles at an average surface temperature of at least 800°C, at least 900°C, at least 1000°C, at least 1100°C, at least 1200°C, at least 1300°C, at least 1400°C, at least 1500°C or at least 1750°C or at least 2000°C (e.g., 800°C to 2200°C or 800°C to 2000°C, or 1000°C to 1800°C). Alternatively, the heated base particles are on a moving bed in the second chamber.

[0081] According to one option, at least one catalyst may be used during the process of the present invention. For example, the catalyst may be a metal catalyst or an inorganic catalyst. According to another option, recycled iron or limestone may be used and applied to at least a portion of the surface of the base particles before exposing them to said energy source. The catalyst, in the processes of the present invention, is preferably covered by the carbon deposits that coat the base particles and, therefore, are not exposed or visible on the surface of the coated base particles. The amount of catalyst may be consistent with amounts used for conventional or ordinary waste contamination processes. The catalyst may be, but is not limited to, potassium, sodium, magnesium, calcium, aluminum, nickel, iron or a catalyst-based material with one or more of these metals or any combination thereof. It may be advantageous to deliberately add a known pyrolysis catalyst, such as, for example, iron, at a content of up to 10% by weight (other amounts may be used).

[0082] When two or more chambers are used, optionally, the base particles, if not already disintegrated, may be disintegrated, at least in part, in the first chamber.

[0083] When two or more chambers are used, the chambers, for example the first chamber compared to the second chamber, may be of different sizes in terms of volume. For example, the first chamber may be at least 25% smaller in volume or at least 50% smaller in volume compared to the volume of the second chamber (for example, from 25% to 75% smaller in volume compared to the volume of the second chamber).

[0084] By applying some of the major aspects of the methods of the present invention to particles other than carbon particles, the present invention can provide methods for coating non-carbonaceous particles, such as silica, preferably precipitated silica particles, with carbon.

[0085] For example, the present invention further relates to a method for forming carbon-coated precipitated silica particles. The method comprises introducing precipitated silica particles into a chamber and exposing the precipitated silica particles to one of the energy sources described herein, such as microwave energy or induction energy, to form heated precipitated silica particles. The method further comprises introducing into the chamber a hydrocarbon source that comprises or is a gas or vapor. The hydrocarbon source pyrolyzes, at least in part, in the chamber to form carbon deposits, thereby coating the heated precipitated silica particles with the carbon deposits and forming the carbon-coated precipitated silica particles.

[0086] The various details and examples and operating parameters and other aspects of the methods described above with reference to carbonaceous base particles as the particle being coated also apply herein to this part of the present invention.

[0087] Through the present invention, it has been discovered that the size of the base particles can affect the ability to obtain a carbon-coated particle. The coated particles, although in particulate form, may be in the form of larger aggregates (particularly from commercial sources that supply the particles). Thus, one aspect of the present invention may involve taking steps to reduce the size of the particles that are to be coated, so that their size results in a carbon-coated particle.

[0088] Alternatively, disintegration may occur in the same chamber and by the same heating of the particles which results in pyrolysis of the hydrocarbon source.

[0089] With respect to the process steps of disaggregating a particle (such as an rC aggregate), the methods described in US Patent Application No. 63 / 493,812 filed on April 3, 2023 may be used presently prior to the steps of coating the particles. In summary, the method for at least partially disaggregating particles, such as carbon particles, e.g., rC aggregates, comprises, consists essentially of, consists of, or includes introducing the particles, such as rC aggregates (e.g., the starting rC aggregates) into a heating chamber having one or more zones. In this method, the heating chamber has at least one zone that has a zone temperature of at least 800°C or at least 900°C.The starting particles, such as rC aggregates, are in the at least one zone that has the zone temperature for a residence time sufficient to result in the disaggregation of at least a portion of the particles, such as rC aggregates. Thus, the method provides disaggregated particles such as disaggregated rC aggregates (i.e., aggregates with small aggregate sizes or aggregates that have a smaller aggregate size compared to the starting aggregate size of the starting rC aggregates). Other steps before and / or after the disaggregation may occur.

[0090] The aggregate size distribution can be measured using TEM images of the particles according to ASTM D3849. Approximately 20 mg of the particles are added to 13 ml of chloroform in a beaker and then sonicated in an ice bath for 10 min at 50% amplitude using Misonix XL2020 with a sonication probe with a half-inch tip. The sonicated dispersion is then diluted with additional chloroform to approximately 100 to 120 ppm and then sonicated with the probe for an additional three minutes. A drop of this dispersion was placed on a 200 mesh carbon-coated TEM grid and allowed to dry in a desiccator. TEM images were acquired using a JEOL JEM-1200 transmission electron microscope (TEM) with an electron accelerating voltage of 80 kV using an image resolution of 1.6 nm / pixel and a field of view of at least 5 pm x 5 pm. The images can then be analyzed according to ASTM D3849 method using automated programs based on the NIH ImageJ macro language and Microsoft Excel Visual Basic for Applications (VBA). The projected area equivalent diameter Dcircle of a recovered carbon aggregate was used as a metric for aggregate size. At least 2000 aggregates were analyzed to obtain number-weighted and volume-weighted aggregate size distributions of recovered carbon samples.

[0091] It is believed that the presence of rC aggregates larger than 1 micron contributes greatly to its poor rubber reinforcing properties when used as a partial or total substitute for virgin carbon black. Aggregates larger than 1 micron may represent a large portion of the total RC aggregates by mass. Therefore, it is believed that a substantial percentage of the starting rC aggregates or other similarly sized aggregates, if used "as is," do not impart positive rubber reinforcing properties or are in fact detrimental to achieving positive rubber reinforcing properties.

[0092] Furthermore, it is believed that starting aggregates larger than 1 micron (e.g., 1.1 microns to 10 microns or larger) significantly reduce fatigue life and abrasion resistance when used in compositions such as elastomeric products. For example, elastomeric products made using starting rC aggregates may contain 5 to 10 times more large undispersed particles than typical carbon black-containing elastomeric composites that contain virgin carbon black in place of starting rC aggregates.

[0093] Large undispersed rC particles or other particles may be significant factors leading to reduced fatigue life, for example in a tire sidewall formulation containing rC (e.g., up to 60% reduction in fatigue life using the DeMattia fatigue test) compared to a sidewall formulation containing virgin carbon black.

[0094] The figures are provided to present aspects of the present invention in a simplified schematic manner.

[0095] [Fig. 1] shows a general cross-sectional view of a configuration for one embodiment of the present invention. The overall system or device 10 may include at least one chamber 14 in which heating of the particles (e.g., carbon particles 18) occurs. The particles are introduced via an inlet or trap 20 and once the process is complete, the carbon-coated particles may either similarly exit through the inlet 20 or exit through an outlet or trap 22. The particles may be on a bed or other support surface 24. This may be a fixed or moving bed. The hydrocarbon gas or vapor may be introduced into the chamber 14 via a tube or injector or feed 12. Multiple feeds may be present and distributed uniformly in the chamber, if any. An energy source 16 is located in the chamber 14 or adjacent to the chamber 14. The location of the energy source (or a portion thereof) may be below or above or around the particles 18.

[0096] Once the carbon-coated particles are formed, the carbon-coated particles exit through the chamber outlet so that the carbon-coated particles can be recovered. The carbon-coated particles may be cooled for the recovery step, for example, by one or more quenching steps, which may occur in one or more quenching zones. The carbon-coated particles may be recovered in a manner identical or similar to that used to recover virgin carbon black from carbon black reactors.

[0097] [Fig. 2] shows a simplified cross-sectional view of another embodiment of an overall system or configuration 30 of the present invention in which two chambers are used. The first chamber 42 may initially receive the particles 48 (e.g., carbon particles or other particles) and heating may occur in the first chamber in the absence of a hydrocarbon source. The heating may be carried out under an oxygen atmosphere, an inert atmosphere, or under vacuum. Heating the particles in the first chamber may either provide heated particles that will be hot enough that when contacted with a hydrocarbon source (in the second chamber 34, the hydrocarbon source introduced via the tube or feed 32 is pyrolyzed) and coat the particles 37, and / or the heating may be used to disintegrate the particles 48.Heating of the first chamber may be accomplished with any energy source 44 as described herein or other types of energy sources (e.g., an oven, a dryer, and the like). The location of the energy source (or a portion thereof) may be below or above or around the particles 48. Once heating is accomplished in the first chamber 42, the heated particles may be transferred 46 by any conventional means (e.g., tray, conveyor belt, container, feeder) to an inlet or trap 38 in the second or main chamber 34, where the heated particles 37 may be subjected to the hydrocarbon-containing gas or vapor that may be introduced into the chamber 34 via a tube or injector or feeder 32. Once the particles are coated, the particles may either exit in the same manner through the inlet 38 or exit via an outlet or trap 50.The particles may be on a bed or other support surface 35. This may be a fixed or moving bed. Multiple power supplies may be present and distributed evenly throughout the chamber, if desired. An energy source 36 may optionally be located in the chamber 34 or adjacent to the chamber 34. The additional energy source 36 . may be used to maintain the particles at a desired temperature and / or may be used to remove volatile substances from the particles. The location of the energy source (or part thereof) may be below or above or around the particles 37.

[0098] Alternatively, the base particles may be coated in a two-step process. For example, particles 18 exiting chamber 14 may be directed to an additional chamber similar to chamber 14 or chamber 34 to be coated with additional carbon. The additional chamber may be maintained at a higher or lower temperature than chamber 14. Alternatively or additionally, particles 38 exiting chamber 14 may be directed to an additional chamber similar to chamber 14 or chamber 34 to be coated with additional carbon. The additional chamber may be maintained at a higher or lower temperature than chamber 34. The use of a higher or lower temperature may influence one or more of the carbon deposition kinetics and the proportion of disordered and graphitic carbon as described by ID / IG.Without being bound by any particular theory, it is believed that higher temperatures are correlated with lower ID / IG ratios and therefore, higher proportions of graphitic carbon and / or larger graphitic crystallite sizes.

[0099] Alternatively, the starting base particles, before the starting base particles are introduced into the chamber, may be subjected to one or more size reduction processes such as mechanical grinding. Mechanical grinding may reduce the size of any agglomerates to form the starting carbon particles or other particles. However, mechanical grinding will not reduce the aggregate size of particles such as rC. Generally, the mill may be configured to pulverize, grind, and / or fragment the starting carbon particles or other particles into smaller agglomerates. The mill may include a hammer mill, a ball mill, a jet mill, a steam mill, and / or some other grinding, pulverizing, or milling machine.The grinding steps and / or techniques as well as the parameters of the starting particles and the ground particles as described in International Publication (PCT) No. WO2023122582 filed on December 20, 2022, can be used presently for the purposes of the present invention.

[0100] The grinder may be directly connected to the inlet of the chamber. For example, rC or other particles may be introduced into the grinder and the grinder directly introduces the ground rC or other particles into the chamber. Alternatively, the grinder may be separate from the chamber, in which the particles, such as rC, are ground first and then transported to the inlet of the chamber.

[0101] Once the carbon-coated particles are formed, the method of the present invention may include the quenching step.

[0102] Alternatively, the outlet of the chamber may lead to an inlet of a quenching chamber or quenching zone. The quenching chamber may spray a quenching fluid, such as water, onto the carbon-coated particles. In general, quenching serves to cool the starting base particles. Optionally, quenching may be multi-stage or occur at multiple points within the quenching chamber. Pressure spraying, gas atomized spraying, or other quenching techniques may be used. With respect to complete quenching of the carbon-coated particles or other particles, any conventional means for quenching the carbon-coated particles or other particles downstream of the chamber may be used and is known to those skilled in the art.For example, a quenching fluid may be injected, which may be water or other fluids suitable for cooling the carbon-coated particles or other particles.

[0103] After quenching, the cooled carbon-coated particles or other particles pass downstream to any conventional cooling and separation means by which the carbon-coated particles are recovered. Any conventional means for recovering the coated particles may be used, and such means may include, but are not limited to, a precipitator, cyclone separator, bag filter, or other means known to those skilled in the art. Once the carbon-coated particles are recovered, they may optionally be subjected to a granulation step, similar to virgin carbon black.

[0104] To granulate the carbon-coated particles in a mixer, a spray nozzle may wet the carbon-coated particles or other particles with a binding agent, such as water, toluene, mineral oil, or the like. The mixer mixes the binder and the carbon-coated particles into a substantially homogeneous mixture that agglomerates (or clumps) into granules of carbon-coated particles. The granules may then be dried to a particular moisture content, e.g., less than 1% by weight. By reducing the moisture content of the granules, the method of the present invention may prevent the introduction of unwanted moisture into the rubber mixture that can contribute to gas emissions (or outgassing) that are emitted when the granules are heated in a rubber mixer and / or a plastic masterbatch mixer.These gas emissions can carry toxic components, such as polycyclic aromatic hydrocarbons, into the air of a manufacturing facility when residual moisture in the agglomerates evaporates under heat.

[0105] The carbon-coated particles of the present invention may be used as a substitute for or combined with carbon black or other reinforcing agents as a component in elastomer or rubber products. The carbon-coated particles may be used as a reinforcing agent or filler in materials, such as rubber products, e.g., tire components.

[0106] The carbon-coated particles of the present invention may be incorporated into rubber articles, used, for example, for tire tread, particularly in tread for passenger car, light vehicle, truck and bus, off-road ("OTR"), aircraft tires and the like; an undertread; a thin wire coating; sidewalls; a toe rubber for retreaded tires; and other uses in tires.

[0107] In other applications, the carbon-coated particles of the present invention may be used in industrial rubber articles, such as engine mounts, hydraulic mounts, bearings, seismic isolators, tank tracks, tank tracks or treads, mining conveyors, hoses, gaskets, seals, blades, weather stripping, bumpers or anti-vibration parts and the like.

[0108] The carbon-coated particles of the present invention may be added instead of or in addition to first reinforcing agents for tire components and / or other industrial end uses of rubber. The carbon-coated particles of the present invention may be combined with natural and / or synthetic rubber in a suitable dry or wet mixing process based on an internal batch mixer, a continuous mixer or a roller mill.

[0109] The performance of the carbon-coated particles of the present invention as a reinforcing agent for rubber compounds may be evaluated by determining, for example, the performance of a rubber composition using the carbon-coated particles of the present invention relative to the performance of a comparative rubber composition that is similar in all respects except for the use of carbon-coated particles of the present invention. In other approaches, the values ​​obtained for the compositions prepared according to the present invention may be compared to values ​​known in the art associated with the desired parameters in a given application.

[0110] Coating with rC carbon or other particles using the processes described herein can improve the performance of rubber compounds prepared with the carbon-coated material compared to the bare base particle. For example, coating with rC carbon can improve reinforcing properties such as tensile modulus, hysteresis (measured by tan delta), tear strength, and / or fatigue life. The performance of rubber compounds prepared with coated rC may be comparable to the performance of rubber compounds prepared with virgin carbon black. Alternatively or additionally, the performance of rubber compounds prepared with coated RC may be comparable to the performance of rubber compounds prepared with uncoated rC. In any of these embodiments, performance may be determined by one or more of tensile modulus at 100% strain, tensile modulus at 300% strain, elongation at break, tan delta (60°C), tear strength (ASTM D624, Matrix B), and / or fatigue life (ASTM D4482).For each of these properties, performance can be improved by at least 5%, at least 10%, at least 15%, or at least 20%, for example, 5 to 25%, 10 to 20%, 5 to 15%, or 15 to 30%. Tensile modulus and elongation at break are measured according to ASTM D412 (Test Method A, Type C) at 23°C, 50% relative humidity, and a cross-sectional speed of 500 mm / min. Tan delta 60° is determined using a dynamic strain sweep between 0.01% and 60% at 10 Hz and 60°C. Tan dmax (sometimes referred to as tan delta) is considered the maximum value of tan d in this strain range. Fatigue life is measured according to ASTM D4482.

[0111] Unless otherwise indicated, all proportions of materials expressed herein as percentages are by weight.

[0112] The present invention comprises the following aspects / embodiments / features in any order and / or in any combination: 1 - The present invention comprises a method for forming carbon-coated base particles, for example carbon-coated carbon particles, said method comprising introducing base particles into a chamber and subjecting the base particles to an energy source which is at least one of a hot gas, microwave energy, induction energy, a direct current passing through said base particles, electromagnetic radiation or solar radiation, so as to form heated base particles, and supplying a hydrocarbon source which comprises a gas or a vapor into said chamber, wherein the hydrocarbon source pyrolyzes, at least in part, in said chamber to form carbon deposits,and thereby coating said heated base particles with said carbon deposits and forming said carbon-coated base particles, the base particles optionally comprising recovered carbon particles. 2 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles comprise particles of carbon or particles which have a carbon content of at least 10% or at least 75%. 3 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles comprise solid hydrothermal carbon (HTC), carbon particles that are non-ASTM reinforcement grade particles, silicon-treated carbon black, silica-coated carbon black, graphene, reduced graphene oxide, single-walled carbon nanotubes, multi-walled carbon nanotubes, carbon nanostructures, carbon black-coated particles, biochar, and any combination thereof. 4 - A method according to any of the preceding or following embodiments / features / aspects, wherein the base particles comprise graphene oxide, lignin or nanocrystalline cellulose, particles of biological origin, polysaccharides, modified polysaccharides, or any combination thereof. 5 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the recovered carbon particles comprise disaggregated and / or ground recovered carbon particles. 6 - A method according to any of the preceding or following embodiments / features / aspects, wherein the base particles comprise precipitated silica, rice husk silica, clays, nanoclays, diatomaceous earth, metal oxides, metal carbonates, or any combination thereof. 7 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are exposed to microwave energy. 8 - A method according to any one of the preceding or following embodiments / features / aspects, wherein said microwave energy is at least 0.5 GHz, for example from 0.5 GHz to 10 GHz. 9 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are exposed to induction energy. 10 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the induction energy is provided by an induction heating device operating at a frequency of at least 5 kHz. 11 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the induction energy is provided by an induction heating device operating at a frequency of 5 kHz to 500 kHz. 12 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the induction heater operates at an induction heating power of at least 50 MJ / kg. 13 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the induction heater operates at an induction heating power of 50 MJ / kg to 250 MJ / kg. 14 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the chamber comprises a fluidized bed reactor, an ablative pyrolysis reactor, a vacuum pyrolysis reactor, a falling type fixed bed reactor or a solar pyrolyzer. 15 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the microwave energy or induction energy is produced from renewable electricity. 16 - Method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are particles of biological origin. 17 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the hydrocarbon source comprises natural gas. 18 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the hydrocarbon source is natural gas. 19 - A method according to any one of the preceding or following embodiments / features / aspects, the method being carried out in the absence of a catalyst. 20 - A method according to any one of the preceding or following embodiments / features / aspects, the method being carried out in the absence of introduced oxygen. 21 - A method according to any one of the preceding or following embodiments / features / aspects, the method producing at most 0.5 kg of carbon dioxide and carbon monoxide / kg of carbon-coated particles, e.g., no carbon dioxide or carbon monoxide. 22 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are heated to a temperature of at least 800°C. 23 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are heated to a temperature of at least 900°C. 24 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are heated to a temperature of at least 1000°C. 25 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are heated to a temperature of at least 1500°C. 26 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the hydrocarbon source comprises a vapor of bio-oil, recycled oil, sustainable oil; a by-product of biofuel or biochemical production, or an oil derived from tires, for example from tire pyrolysis, an oil from plastic pyrolysis or recycling, or an oil from hydrothermal liquefaction or paper conversion. 27 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are on a fixed bed within the chamber. 28 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are on a moving bed which passes through the chamber. 29 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the carbon deposits uniformly cover the base particles. 30 - Method according to any one of the preceding or following embodiments / features / aspects, wherein the carbon deposits at least partially cover the base particles. 31.- A method according to any one of the preceding or following embodiments / features / aspects, wherein the carbon-coated base particles of the product have a coating having an average thickness of 0.5 to 500 nanometers. 32 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles have a residence time in said chamber of 1 second to 3 hours. 33 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles have a residence time in said chamber of 5 seconds to 2 hours. 34 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the chamber comprises at least a first chamber and a second chamber, wherein, in the first chamber, the base particles are exposed to microwave energy or induction energy such that the base particles reach an average surface temperature of at least 800°C in the absence of any hydrocarbon source to obtain heated base particles, and then transporting said heated base particles to the second chamber where said feeding of the hydrocarbon source occurs. 35 - A method according to any one of the preceding or following embodiments / features / aspects, wherein, in the second chamber, the second chamber comprises a heating source which maintains the heated base particles at a surface temperature of at least 800°C. 36 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the heated base particles are on a moving bed in the second chamber. 37 - A method according to any one of the preceding or following embodiments / features / aspects, wherein recycled iron or limestone is applied to at least a portion of the surface of the base particles before being exposed to said energy source. 38. A method according to any one of the preceding or following embodiments / features / aspects, wherein the base particles are disaggregated, at least in part, in said first chamber. 39 - A method according to any one of the preceding or following embodiments / features / aspects, wherein an oxidizing atmosphere is present in said chamber during at least part of said method. 40 - A method according to any one of the preceding or following embodiments / features / aspects, wherein an oxidizing atmosphere is present in said chamber during at least a part of said method which is at least achieved by the introduction of water into the chamber. 41 - A method according to any one of the preceding or following embodiments / features / aspects, further comprises carrying out steam oxidation of the base particles in said chamber. 42 - A method according to any one of the preceding or following embodiments / features / aspects, further comprising heating said carbon-coated particles in a second step, either in the same chamber or in a different chamber, in a neutral atmosphere or a reducing atmosphere. 43 - A method according to any one of the preceding or following embodiments / features / aspects, wherein a non-reactive carrier gas is present with the hydrocarbon source. 44 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the hydrocarbon gas is introduced into the chamber at at least two locations in the chamber. 45 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the unreacted carrier gas is introduced into the chamber either separately or with said hydrocarbon gas at at least two locations in the chamber. 46 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the first chamber has a volume at least 25% smaller than the volume of the second chamber. 47 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the first chamber has a volume at least 50% smaller than the volume of the second chamber. 48 - A method according to any one of the preceding or following embodiments / features / aspects, further comprising introducing the carbon-coated base particles into a further chamber and exposing the base particles to an energy source which is at least one of a hot gas, microwave energy, induction energy, direct current passing through said base particles, electromagnetic radiation or solar radiation, so as to form heated carbon-coated base particles, and supplying a hydrocarbon source which comprises a gas or vapor into said further chamber, wherein the hydrocarbon source pyrolyzes, at least in part, in said further chamber to form carbon deposits, and thereby coating said heated carbon-coated base particles with further carbon deposits. 49 - The present invention further relates to a method for forming carbon-coated precipitated silica particles, said method comprising: introducing precipitated silica particles into a chamber and exposing the precipitated silica particles to microwave energy or induction energy to form heated precipitated silica particles, and supplying a hydrocarbon source which comprises a gas or vapor into said chamber, wherein the hydrocarbon source pyrolyzes, at least in part, in said chamber to form carbon deposits, and thereby coating said heated precipitated silica particles with said carbon deposits and forming said carbon-coated precipitated silica particles. 50 - The present invention further relates to coated carbon particles or other particles formed by any method according to any of the preceding or following embodiments / features / aspects. 51 - The present invention further relates to a process for producing hydrogen, comprising carrying out the process according to any one of the preceding embodiments / features / aspects, wherein the pyrolysis of the hydrocarbon source results in the production of a gaseous stream comprising hydrogen. 52 - A method according to any one of the preceding or following embodiments / features / aspects, further comprises separating hydrogen from the remaining portion of the gas stream to obtain a purified hydrogen stream. 53 - A method according to any one of the preceding or following embodiments / features / aspects, further comprising guiding the remaining portion of the gas stream towards the hydrocarbon source. 54 - A method according to any one of the preceding or following embodiments / features / aspects, wherein the gas stream comprises at least 60% by volume of hydrogen, for example 80 to 99% by volume of hydrogen. 55 - The present invention further relates to carbon coated particles each comprising a base particle and carbon deposits disposed around the outer surface of the base particle, the carbon coated particles having a ratio of the areas of the Raman D band (1340 cm1) and the Raman G band (1590 cm 1 ) of 0.5 to 2.45, for example 1 to 2.45 or 1.5 to 2.45. 56 - Carbon coated particles according to any of the preceding or following embodiments / features / aspects, wherein the base particles comprise carbon particles or particles which have a carbon content of at least 10% by weight or at least 75% by weight. 57 - Carbon coated particles according to any one of the preceding or following embodiments / features / aspects, wherein the base particles comprise reclaimed carbon particles. 58 - Carbon coated particles according to any of the preceding or following embodiments / features / aspects, wherein the base particles comprise carbon particles that are non-ASTM reinforcement grade particles, solid hydrothermal carbon (HTC), silicon-treated carbon black, silica-coated carbon black, graphene, reduced graphene oxide, single-walled carbon nanotubes, multi-walled carbon nanotubes, carbon nanostructures, carbon black-coated particles, biochar, and any combination thereof. 59 - Carbon-coated particles according to any of the preceding or following embodiments / features / aspects, the base particles comprising graphene oxide, lignin, nanocrystalline cellulose, bio-derived particles, polysaccharides, modified polysaccharides, or any combination thereof. 60 - Carbon coated particles according to any of the preceding or following embodiments / features / aspects, wherein the recovered carbon particles comprise disaggregated and / or ground recovered carbon particles. 61 - Carbon-coated particles according to any of the preceding or following embodiments / features / aspects, wherein the base particles comprise precipitated silica, rice hull silica, clays, nanoclays, diatomaceous earth, metal oxides, metal carbonates, or any combination thereof. 62 - Carbon coated particles according to any one of the preceding or following embodiments / features / aspects, wherein the carbon deposit coating has an average thickness of 0.5 nm to 500 nm. 63 - A rubber article incorporating the carbon-coated particles according to any one of the preceding or following embodiments / features / aspects. 64 - A rubber article according to any one of the preceding or following embodiments / features / aspects, wherein the rubber article is a tire component selected from the group consisting of a tire tread, a sub-tread, a thin wire covering, a sidewall and a toe rubber, an engine mount, a hydraulic mount, a support apparatus, a seismic isolator, a tank track, a tank tread, a mining conveyor, a hose, a gasket, a seal, a blade, a weatherstripping article, a bumper, or an anti-vibration part. 65 - The present invention further relates to an elastomeric composite comprising the carbon-coated particles of any one of the preceding or following embodiments / features / aspects, wherein the base particle is reclaimed carbon, the elastomeric composite having at least one mechanical property selected from tensile modulus at 100% strain, tensile modulus at 300% strain, elongation at break, tan delta at 60 C, tear strength and fatigue life with an amplitude at least 5% greater than that of an elastomeric composite having the same composition but with reclaimed carbon instead of carbon-coated particles. EXAMPLES

[0113] Example 1 - Recovered carbon (CBP Cyprus Ltd) was introduced into a tube furnace at a rate of 360 g / h and treated with a residence time of approximately 1 hour at the temperature specified in Table 1 below. The tube had a diameter of 6 inches (15 cm) and a heated section of 60 inches (152 cm) in length and rotated at a speed of 1.8 rpm. Gas was introduced into the tube at a rate of 25 scfh (708 1 / h) (nitrogen) or 21 scfh (595 1 / h) (methane), with an additional 6 scfh (170 1 / h) of nitrogen used continuously to purge the system inlets and outlets. Samples were collected after one hour of steady-state operation, meaning that the flow of rC into and out of the furnace was constant, the temperature was stable and the desired gas (nitrogen or methane) had circulated through the tube for at least 90 minutes. [Tables 1] Furnace temperature (°C) Primary gas flow Ash (%) If in ash (%) If in particles (%) % increase in C* Id / Ig (area ratio) Untreated 15.52 14.99 2.33 - 2.63 + 0.12 1000 Nitrogen 15.53 14.91 2.32 0.5 2.52 + 0.13 900 Methane 14.31 14.77 2.11 11.6 2.39 + 0.11 1000 Methane 9.89 18.94 1.87 32.5 1.86 + 0.17 1100 Methane 7.27 23.2 1.69 51.4 1.51+0.06 *% increase in carbon calculated based on constant silicon

[0114] Elemental analysis was determined by first determining the mass percent carbon using the calcination method specified in ASTM D1506, assuming that all non-ash content was carbon. Inorganic elements were quantified by scanning electron microscopy / energy dispersive X-ray spectroscopy (SEM / EDS) of a thick layer of ash stamped onto a SEM punch with carbon tape. Regions measuring 560 microns x 420 microns were scanned with an EDS detector until a total of 50,000,000 X-ray counts had been recorded.

[0115] The results demonstrate that carbon was deposited on the surface of the rC particles. The decrease in ash also suggests that the ZnO in the rC was reduced, and then the metallic zinc (boiling point 907 °C) was evaporated. Assuming little or no loss of silicon during deposition, the increase in Si concentration in the ash suggests a reduced amount of ash, while the reduced proportion of Si in the rC suggests that the addition of new carbon to the rC increases with processing temperature. In addition, the decrease in ID / Ig indicates that the crystallinity of the deposited carbon increases with processing temperature.

[0116] Example 2 - Recovered carbon (e.g., from CBP Cyprus Ltd) is coated with carbon in a pilot-scale fluidized bed reaction system substantially similar to that described in connection with [Fig. 2] of US 10087330. The ideal fluidization velocity of recovered carbon is evaluated with room temperature air in a laboratory scale fluidization device. The initial charge of recovered carbon feedstock is loaded into the fluidized bed so that it rests above the bottom plate. The bed is then sealed and a stream of nitrogen is passed through the recovered carbon, entering through the bottom plenum, passing through the bottom plate and then the recovered carbon, and finally exiting through the top of the fluidized bed reactor. Electrical heaters were activated to bring the bed temperature to 1000°C. The nitrogen flow is then stopped and a stream of natural gas having a superficial velocity approximately equal to the ideal fluidization velocity is activated and the test is started.Samples are regularly taken from the bed using a dip tube and measured to monitor the progress of carbon black deposition. At the end of the desired test duration, the natural gas flow is stopped, along with the electric heaters, and nitrogen is again sent to the fluidized bed while it cools to room temperature. The final bed product is then collected from the bottom of the fluidized bed reactor. This product is expected to contain carbon deposited on the surface and a reduced amount of zinc compared to the starting product.

[0117] Example 3 - Particulate silica (e.g., precipitated silica) is coated with carbon in a pilot-scale fluidized bed reaction system having a configuration similar to that described with reference to [Fig. 2] of US 10087330. The ideal fluidization rate of the particulate silica is evaluated with air at room temperature in a laboratory-scale fluidization device. The initial charge of particulate silica starting material is loaded into the fluidized bed so that it rests above the bottom plate. The bed is then sealed and a stream of nitrogen is passed through the particulate silica, entering through the bottom plenum, passing through the bottom plate and then the particulate silica, and finally exiting through the top of the fluidized bed reactor. Electrical heaters were activated to bring the bed temperature to 1250 °C. The nitrogen flow is then stopped and a stream of natural gas with a superficial velocity approximately equal to the ideal fluidization velocity is activated and the test is started. Samples are regularly taken from the bed using a dip tube and measured to monitor the progress of carbon black deposition. At the end of the desired test duration, the flow of natural gas is stopped, along with the electric heaters, and the nitrogen is again sent to the fluidized bed while it cools to room temperature. The final bed product is then collected at the bottom of the fluidized bed reactor. Carbon is expected to be deposited on the surface of this product.

[0118] Example 4. Elastomeric composites with a particle loading of 50 phr are prepared with each of the five particles of Example 1, the amount of particles and hardeners indicated in Table 2, and Kralex SBR 1502 styrene-butadiene rubber (Synthos). All compositions are mixed in a 439 ml Brabender Prep mixer with two two-stage cam rotors, as described in Table 3. The compounds are sheeted on a 2-roll mill operating at 50 °C and about 22 rpm, followed by six passes with a nip of about 5 mm, with a rest time before the next mixing step (or curing, after the last step) of at least 3 hours. Curing is carried out in a heated press (150 °C, 2,500 Ibs) for 30 minutes.Compounds prepared with carbon-coated rC are expected to exhibit superior mechanical performance (e.g., at least a 5% improvement in one or more of tensile modulus at 100% strain, tensile modulus at 300% strain, elongation at break, tan delta (60 °C), tear strength, and fatigue life) compared to compounds prepared with rC that has not been carbon-coated. [Tables 2] Component phr 6PPDa 3 TMQb 1.5 Zinc oxidec 3 Stearic acid0 2 Wax beadsd 1 BBTSe 1.5 Sulfur0 1.5 a) N-(l,3-Dimethylbutyl)-N'-phenyl-p-phenylenediamine, 6PPD (Western Reserve Chemical) b) Poly(l,2-dihydro-2,2,4-trimethyl-quinoline), DQ antioxidant granules (Akrochem Corporation) c) Akrochem Corporation d) ACR0WAXmt 5031 (Akrochem Corporation) e) N-tert-Butyl-2-benzothiazole-sulfenamide (Akrochem Corporation) [Tables3] Stage 1 Fill Factor, % 70 Rotor Speed, RPM 80 Starting Temperature, °C 85 Time (s) Description 0 Add polymer 60-120 Gradually add filler - Reduce speed to 60°C if temperature approaches 160°C 180 Scrape / sweep, add pre-mixed particles (ZnO, Stearic Acid, Wax, 6PPD, TMQ) 240 Scrape / sweep, adjust RPM to maintain temperature <= 160°C. 300 Drain Stage 2 Fill Factor, % 68 Rotor Speed, RPM 60 Starting Temperature, °C 52 Time (s) Description 0 Add Stage 1 batch and hardeners 30 Scrape / sweep 90 Drain - Adjust rotor speed not to exceed 115°C

[0119] The present invention may comprise any combination of these different features or different embodiments above and / or below, as described herein in sentences and / or paragraphs. Any combination of the features described herein is considered part of the present invention and no limitation is intended with respect to the combinable features.

[0120] Where a quantity, concentration or other value or parameter is given as a range, preferred range or list of values upper and lower preferred values, this is to be understood as specifically indicating all ranges formed from any pair of any upper preferred range limit or value and any lower preferred range limit or value, regardless of whether the ranges are described separately or not. Where a range of numerical values ​​is referred to herein, unless otherwise indicated, the range is intended to include its endpoints, as well as all integers and fractions within the range. It is not intended that the scope of the invention be limited to the specific values ​​stated when defining a range.

[0121] Other embodiments of the present invention will become apparent to those skilled in the art from reading this specification and practicing the present invention described herein. It is to be understood that this specification and the examples are to be considered as given by way of example only, the true scope and spirit of the invention being indicated by the following claims and their equivalents.

Claims

Claims

1. A method for forming carbon-coated base particles, said method comprising introducing base particles into a chamber and subjecting the base particles to an energy source which is at least one of a hot gas, microwave energy, induction energy, a direct current passing through said base particles, electromagnetic radiation or solar radiation, so as to form heated base particles, and supplying a hydrocarbon source which comprises a gas or vapor into said chamber, wherein the hydrocarbon source pyrolyzes, at least in part, in said chamber to form carbon deposits, and thereby coating said heated base particles with said carbon deposits and forming said carbon-coated base particles, the base particles optionally comprising reclaimed carbon particles.

2. The method of claim 1, wherein the base particles comprise carbon particles or particles that have a carbon content of at least 10% or at least 75%.

3. The method of claim 1 or 2, wherein the base particles comprise carbon particles that are non-ASTM reinforcement grade particles, solid hydrothermal carbon (HTC), silicon-treated carbon black, silica-coated carbon black, graphene, reduced graphene oxide, single-walled carbon nanotubes, multi-walled carbon nanotubes, carbon nanostructures, carbon black-coated particles, biochar, and any combination thereof.

4. A method according to any one of claims 1 to 3, wherein the base particles comprise graphene oxide, lignin or nanocrystalline cellulose, particles of biological origin, polysaccharides, modified polysaccharides, or any combination thereof.

5. A method according to any one of claims 1 to 4, wherein the recovered carbon particles comprise disaggregated and / or ground recovered carbon particles.

6. A method according to any one of claims 1 to 5, wherein the base particles comprise precipitated silica,

7.

8.

9.

10.

11.

12.

13.

14.

15.

16.

17.

18.

19.

20. rice hull silica, clays, nanoclays, diatomaceous earth, metal oxides, metal carbonates, or any combination thereof. A method according to any one of claims 1 to 6, wherein the base particles are exposed to microwave energy. The method of claim 7, wherein said microwave energy is at least 0.5 GHz, for example 0.5 GHz to 10 GHz. A method according to any one of claims 1 to 6, wherein the base particles are exposed to induction energy. The method of claim 9, wherein the induction energy is provided by an induction heating device operating at a frequency of at least 5 kHz. A method according to claim 9 or 10, wherein the induction energy is provided by an induction heater operating at a frequency of 5 kHz to 500 kHz. A method according to any one of claims 9 to 11, wherein the induction heating device operates at an induction heating power of at least 50 MJ / kg. A method according to any one of claims 9 to 12, wherein the induction heating device operates at an induction heating power of 50 MJ / kg to 250 MJ / kg. A method according to any one of claims 1 to 13, wherein the chamber comprises a fluidized bed reactor, an ablative pyrolysis reactor, a vacuum pyrolysis reactor, a falling type fixed bed reactor or a solar pyrolyzer. A method according to any one of claims 1 to 14, wherein the microwave energy or induction energy is generated from renewable electricity. A method according to any one of claims 1 to 15, wherein the base particles are particles of biological origin. A method according to any one of claims 1 to 16, wherein the hydrocarbon source comprises natural gas. A method according to any one of claims 1 to 17, wherein the hydrocarbon source is natural gas. A process according to any one of claims 1 to 18, the process being carried out in the absence of a catalyst. A method according to any one of claims 1 to 19, wherein the method is carried out in the absence of introduced oxygen.

21. A method according to any one of claims 1 to 20, wherein the method produces at most 0.5 kg of carbon dioxide and carbon monoxide / kg of carbon-coated particles.

22. A method according to any one of claims 1 to 21, wherein the base particles are heated to a temperature of at least 800°C.

23. A method according to any one of claims 1 to 22, wherein the base particles are heated to a temperature of at least 900°C.

24. A method according to any one of claims 1 to 23, wherein the base particles are heated to a temperature of at least 1000°C.

25. A method according to any one of claims 1 to 24, wherein the base particles are heated to a temperature of at least 1500°C.

26. A method according to any one of claims 1 to 25, wherein the hydrocarbon source comprises a vapor of bio-oil, recycled oil, sustainable oil; a by-product of biofuel or biochemical production, or an oil derived from tires, for example from tire pyrolysis, an oil from plastic pyrolysis or recycling, or an oil from hydrothermal liquefaction or paper conversion.

27. ​​A method according to any one of claims 1 to 26, wherein the base particles are on a fixed bed within the chamber.

28. A method according to any one of claims 1 to 27, wherein the base particles are on a moving bed which passes through the chamber.

29. A method according to any one of claims 1 to 28, wherein the carbon deposits uniformly cover the base particles.

30. A method according to any one of claims 1 to 29, wherein the carbon deposits at least partially cover the base particles.

31. A method according to any one of claims 1 to 30, wherein the carbon coated particles of the product have a coating having an average thickness of 0.5 to 500 nanometers.

32. A method according to any one of claims 1 to 31, wherein the base particles have a residence time in said chamber of 1 second to 3 hours.

33. A method according to any one of claims 1 to 32, wherein the base particles have a residence time in said chamber ranging from 5 seconds to 2 hours.

34. A method according to any one of claims 1 to 33, wherein the chamber comprises at least a first chamber and a second chamber, wherein in the first chamber the base particles are exposed to microwave energy or induction energy such that the base particles reach an average surface temperature of at least 800°C in the absence of any hydrocarbon source to obtain heated base particles, and then transporting said heated base particles to the second chamber where said feeding of the hydrocarbon source occurs.

35. The method of claim 34, wherein in the second chamber, the second chamber includes a heating source that maintains the heated base particles at a surface temperature of at least 800°C.

36. A method according to claim 34 or 35, wherein the heated base particles are on a moving bed in the second chamber.

37. A method according to any one of claims 34 to 36, wherein the base particles are disaggregated, at least in part, in said first chamber.

38. A method according to any one of claims 34 to 37, wherein the first chamber has a volume at least 25% smaller than the volume of the second chamber.

39. A method according to any one of claims 34 to 38, wherein the first chamber has a volume at least 50% smaller than the volume of the second chamber.

40. A method according to any one of claims 1 to 39, wherein recycled iron or limestone is applied to at least a portion of the surface of the base particles before being exposed to said energy source.

41. A method according to any one of claims 1 to 40, wherein an oxidizing atmosphere is present in said chamber during at least part of said method.

42. A method according to any one of claims 1 to 41, wherein an oxidizing atmosphere is present in said chamber during at least a portion of said method which is at least achieved by the introduction of water into the chamber.

43. A method according to any one of claims 1 to 42, further comprising carrying out steam oxidation of the base particles in said chamber.

44. A method according to any one of claims 1 to 43, further comprising heating said carbon-coated particles in a second step, either in the same chamber or in a different chamber, in a neutral atmosphere or a reducing atmosphere.

45. A method according to any one of claims 1 to 44, wherein a non-reactive carrier gas is present with the hydrocarbon source.

46. The method of claim 45, wherein the non-reactive carrier gas is introduced into the chamber either separately or with said hydrocarbon gas at at least two locations in the chamber.

47. A method according to any one of claims 1 to 46, wherein the hydrocarbon gas is introduced into the chamber at at least two locations in the chamber.

48. A method according to any one of claims 1 to 47, further comprising introducing the carbon-coated base particles into a further chamber and exposing the base particles to an energy source which is at least one of a hot gas, microwave energy, induction energy, a direct current passing through said base particles, electromagnetic radiation or solar radiation, so as to form heated carbon-coated base particles, and supplying a hydrocarbon source which comprises a gas or vapor into said further chamber, wherein the hydrocarbon source pyrolyzes, at least in part, in said further chamber to form carbon deposits, and thereby coating said heated carbon-coated base particles with further carbon deposits.

49. A method of forming carbon-coated precipitated silica particles, said method comprising: introducing precipitated silica particles into a chamber and exposing the precipitated silica particles to microwave energy or induction energy to form heated precipitated silica particles, and supplying a hydrocarbon source that comprises a gas or vapor into said chamber, wherein the hydrocarbon source pyrolyzes, at least in part, in said chamber to form carbon deposits, and thereby coating said heated precipitated silica particles with said carbon deposits and forming said carbon-coated precipitated silica particles.

50. A method of producing hydrogen, comprising carrying out the method according to any one of the preceding claims, wherein the pyrolysis of the hydrocarbon source results in the production of a gaseous stream comprising hydrogen.

51. The method of claim 50, further comprising separating hydrogen from the remaining portion of the gas stream to obtain a purified hydrogen stream.

52. The method of claim 51, further comprising guiding the remaining portion of the gas stream toward the hydrocarbon source.

53. A method according to any one of claims 50 to 52, wherein the gas stream comprises at least 60% by volume of hydrogen, for example 80 to 99% by volume of hydrogen.

54. Carbon coated particles each comprising a base particle and carbon deposits disposed around the outer surface of the base particle, the carbon coated particles having a ratio of the areas of the Raman D band (1340 cm1) and the Raman G band (1590 cm1) of 0.5 to 2.45, for example 1 to 2.45 or 1.5 to 2.

45.

55. Carbon-coated particles according to claim 54, wherein the base particles comprise carbon particles or particles which have a carbon content of at least 10% by weight or at least 75% by weight.

56. Carbon coated particles according to claim 54 or 55, wherein the base particles comprise reclaimed carbon particles.

57. Carbon coated particles according to any one of claims 54 to 56, wherein the base particles include carbon particles that are non-ASTM reinforcement grade particles, solid hydrothermal carbon (HTC), silicon-treated carbon black, silica-coated carbon black, graphene, reduced graphene oxide, single-walled carbon nanotubes, multi-walled carbon nanotubes, carbon nanostructures, carbon black-coated particles, biochar, and any combination thereof.

58. Carbon-coated particles according to any one of claims 54 to 57, wherein the base particles comprise graphene oxide, lignin or nanocrystalline cellulose, particles of biological origin, polysaccharides, modified polysaccharides, or any combination thereof.

59. Carbon coated particles according to any one of claims 54 to 58, wherein the recovered carbon particles comprise disaggregated and / or ground recovered carbon particles.

60. Carbon-coated particles according to any one of claims 54 to 59, wherein the base particles comprise precipitated silica, rice hull silica, clays, nanoclays, diatomaceous earth, metal oxides, metal carbonates, or any combination thereof.

61. Carbon coated particles according to any one of claims 54 to 60, wherein the carbon deposit coating has an average thickness of 0.5 nm to 500 nm.

62. A rubber article incorporating the carbon-coated particles of any one of claims 54 to 61.

63. The rubber article of claim 62, wherein the rubber article is a tire component selected from the group consisting of a tire tread, a sub-tread, a thin wire covering, a sidewall and toe rubber, an engine mount, a hydraulic mount, a support apparatus, a seismic isolator, a tank track, a tank tread, a mining conveyor, a hose, a gasket, a seal, a blade, a weather stripping article, a bumper or an anti-vibration part.

64. An elastomeric composite comprising the carbon-coated particles of any one of claims 54 to 61, wherein the base particle is reclaimed carbon, the elastomeric composite having at least one mechanical property selected from tensile modulus at 100% strain, tensile modulus at 300% strain, elongation at break, tan delta at 60 C, tear strength and fatigue life with an amplitude at least 5% greater than that of an elastomeric composite having the same composition but with reclaimed carbon instead of carbon-coated particles.