Guanidinium based ionic porous organic polymer
Patent Information
- Application Number
- IN202441080497
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-10-23
- Publication Date
- 2026-10-23
- Estimated Expiration
- 2044-10-23
Abstract
Description
FIELD OF INVENTION:The present invention relates to a novel Guanidinium based ionic porous organic polymer of formula (I) the process for preparation thereof. The present invention provides Guanidinium based ionic porous organic polymer of formula (I) that may optionally be doped with copper and can act both as an adsorbent and a heterogeneous catalyst in chemical reactions. Further, the process of the present invention provides a mechanochemical process for preparation of Guanidinium based ionic porous organic polymer of formula (I) which is simple and requires less time as compared to the conventional solvothermal process. BACKGROUND OF THE INVENTION:Porous organic polymers are emerging class of polymers noted for their porous nature, high chemical and thermal stability, and functional tunability. Ionic porous organic polymers gained paramount importance as materials capable of both ion exchange and adsorption.Guanidium based ionic porous organic polymer are disclosed in the prior arts. An article titled "Guanidinium-Based Ionic Covalent Organic Porous Polymer as Natamycin Delivery Agents for Anti-Candida albicans" by Xia Liu et.al published in Chemistry Select, Volume 6, Issue 40 in 2021 discloses a biodegradable ionic covalent organic porous polymers (ICOP) with dynamic double selenium bond (Se-Se) as carriers for the antifungal drug-natamycin (NAT). An article titled "Guanidinium-Based Ionic Covalent Organic Framework for Rapid and Selective Removal of Toxic Cr(VI) Oxoanions from Water" by Santa Jansone-Popova et.al published in Environmental Science & TechnologyVol 53 / Issue 2 in 2018 discloses the organic polymer preferably BT-DGCl for removal of toxic Cr(VI) oxoanions from aqueous solutions by ion-exchange mechanism. Guanidinium-Based Ionic Covalent Organic polymers though are known in the art, there are certain disadvantages and limitations such as the said Guanidinium-Based Ionic Covalent Organic polymers require certain pH to operate, are not versatile in their activity, few have heavy metals embedded which make them costly and the use of such heavy metals limit their activity due to toxic nature of the heavy metals. In view of the above disadvantages, the present inventors envisaged that there is a scope in the art to provide guanidinium-based ionic porous organic polymer devoid of any heavy metals and can possess both adsorbent and catalytic activity. Further, the present inventors observed that though solvothermal processes are known in the art, the process is complicated requires excessive use of solvent, high temperature, long hours of reaction time which makes the process economically and industrially not viable. In light of the above, the present inventors felt that the need in the art may be overcome by providing a multipurpose guanidinium-based ionic porous organic polymer and an improved process for synthesis thereof. This remains the objective of the invention. OBJECTIVES OF THE INVENTION:The primary objective of the present invention is to provide a multipurpose guanidinium-based ionic porous organic polymer and to the process for preparation thereof which is cost effective and industrially feasible. SUMMARY OF THE INVENTION:In accordance with the above, the present invention provides guanidinium-based ionic porous organic polymer of Formula (I), comprising; Formula IIn an aspect, the Guanidinium-based porous polymer of the present invention comprises 4,4',4'' [1,3,5-triazine-2,4,6- triyltris(oxy)tris]3-methoxybenzaldehyde [TBM] and triaminoguanidinium hydrochloride [TGDM] in 1:1 ratio. In an aspect, the guanidinium-based ionic porous organic polymer of Formula (I) is crystalline in nature and is characterized by PXRD with characteristic peaks at 10, 13, 23, 28, 31, 39 degrees ±2θ.In another aspect, the elemental analysis of guanidinium-based ionic porous organic polymer of Formula (I) showed the presence of 58% C, 15% N, 21% O, and 6% Cl in the framework.The thermal stability of guanidinium-based ionic porous organic polymer of Formula (I) was analyzed using thermogravimetric analysis (TGA) and was observed to be stable up to 300°C. In yet another aspect, the guanidinium-based ionic porous organic polymer of Formula (I) has a BET surface area of 30-40 m2 / gThe guanidinium-based ionic porous organic polymer of Formula (I) is porous in nature, has high chemical and thermal stability, and functional tenability. The Guanidinium based ionic porous organic polymers are particularly significant due to their capabilities in ion exchange and adsorption.In yet another aspect, the present invention provides a mechanochemical process for synthesis of guanidinium-based ionic porous organic polymer of Formula (I) comprising;(i) Mixing 4,4',4'' [1,3,5-triazine-2,4,6-Triyltris(oxy)tris]3-methoxybenzaldehyde (TMB) and triaminoguanidinium hydrochloride (TGDM) in equimolar mixture and heating; (ii) Adding acetic acid as catalyst to the above heated mix and grinding uniformly until completion of polymerization; and(iii) Washing several times to ensure the removal of unreacted monomeric units and drying to obtain the desired product. The process is depicted below: In an aspect, the preparation of guanidinium-based ionic porous organic polymer of Formula (I) by mechanochemical method was completed in 40-50minutes. In yet another aspect, the present inventions provide a guanidinium-based ionic porous organic polymer of Formula (I) doped with copper. In an aspect, the guanidinium-based ionic porous organic polymer of Formula (I) doped with copper is prepared by a process comprising; (i) Dropping aqueous solution of copper salt over a thin layer of uniformly spreaded polymer; (ii) Evaporating the resulting suspension of step (i) to dryness, washing and drying until the desired loading of the copper metal is achieved. In another aspect, the copper metal is loaded on to the polymer in an amount ranging between 50- 100mg. In yet another aspect, the present invention relates to the carbonization process of synthesis of copper doped porous carbon material [Cu- PCM] derived from guanidinium based porous organic polymer [gn-ipop-cl] as the precursor. The process comprises heating of the polymer at a temperature ranging between 350-450°C for about 4 hours at a heating rate of 5°C / minute under nitrogen atmosphere.The copper doped porous carbon material [Cu- PCM] is crystalline nature evident from SEM and elemental analysis. Further, the copper doped porous carbon material is characterized by PXRD with characteristic peaks at 36,43,50,74 ±2θ. The FE SEM images [Figure 8c and 8d] obtained shows the highly porous network morphology of the carbonized material.In another aspect, the copper doped porous carbon material [Cu- PCM] exhibits the BET surface area of 1560 m2 / g. In yet another aspect, the guanidinium-based ionic porous organic polymer of Formula (I) optionally doped with copper exhibits both adsorbent activity as well as may be used as a catalyst. DETAILED DESCRIPTION OF DRAWINGSFigure 1 illustrates [a] FT-IR spectra for TGDM, TMB, gn-ipop-cl and [b] CPMAS 13C NMR spectra of gn-ipop-cl Figure 2 illustrates pXRD pattern of [a] gn-ipop-cl(ST), [b] gn-ipop-cl(MC); TGA profile of [c] gn-ipop-cl(ST), [d] gn-ipop-cl(MC); BET surface area for [e] gn-ipop-cl(ST), [f] gn-ipop-cl(MC)Figure 3 illustrates field emission scanning electron microscopy (FE SEM) images of [a,b] gn-ipop-cl(ST) and [c,d] gn-ipop-cl(MC)Figure 4 illustrates [a] UV-Vis spectra of KMnO4 demonstrating the fast uptake of permanganate in presence of gn-ipop-cl, [b] First order fitting for KMnO4 adsorption, [c] Isotherm for adsorption of KMnO4 and [d] Freundlich fitting for adsorption isotherm. Figure 5 illustrates photographs of permanganate solution and polymer adsorbent before and after adsorption of permanganateFigure 6 illustrates UV-Visible spectra and Uptake capacity observed for [a,b] Methyl orange[1004 mg / g], [c,d] Crystal violet[400 mg / g], [e,f] Rhodamine B[127 mg / g], [g,h] Eriochrome black T[115 mg / g] obtained using gn-ipop-cl as adsorbent.Figure 7 illustrates [a] UV-Visible of adsorption of iodine [b] Uptake capacity calculated for adsorption of iodine.Figure 8 illustrates schematic representation of synthesis of copper dopped porous carbon material [Cu-PCM] derived from guanidinium based porous organic polymer [gn-ipop-cl] as the precursorFigure 9 illustrates [a] PXRD pattern of Cu-PCM [b] BET surface area analysis of Cu-PCM [c] and [d] FE SEM images of Cu-PCMFigure 10 illustrates [a] Effect of catalyst loading on % conversion, [b] Effect of temperature on % conversion, [c] Effect of reaction time on % conversion and [d] Effect of concentration of substrate on % conversionDETAILED DESCRIPTION OF THE INVENTION:Unless specified otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art, to which this invention belongs. Although any methods and materials similar or equivalent to those described herein can be used in the practice or testing of the invention, the preferred methods and materials are described. To describe the invention, certain terms are defined herein specifically as follows.Unless stated to the contrary, any of the words "including," "includes," "comprising," and "comprises" mean "including without limitation" and shall not be construed to limit any general statement that it follows to the specific or similar items or matters immediately following it. The term "consists essentially of" means excluding other materials that contribute to function.Embodiments of the invention are not mutually exclusive, but may be implemented in various combinations. The described embodiments of the invention and the disclosed examples are given for the purpose of illustration rather than limitation of the invention as set forth in the appended claims.The term "gn-ipop-cl" as used herein in the entire specification means and relates to Guanidinium based ionic porous organic polymer of formula (I). The term "Cu-gn-ipop-cl" as used herein in the entire specification means and relates to Guanidinium based ionic porous organic polymer of formula (I) doped with copper. The term "Cu-PCM" as used herein in the entire specification means and relates to copper doped porous carbon material.Abbreviations: TMB: 4,4',4'' [1,3,5-triazine-2,4,6-Triyltris(oxy)tris]3-methoxybenzaldehyde TGDM: triaminoguanidinium hydrochloride gn-ipop-cl: Guanidinium based ionic porous organic polymerPorous organic polymers are emerging class of polymers used for their porous nature, high chemical and thermal stability, and functional tunability. The present inventors have developed a novel Guanidinium based ionic porous organic polymers that is versatile in its activity exhibiting as an adsorbent and as an effective catalyst in chemical reactions. Further, Guanidinium based ionic porous organic polymers are synthesized in the art by solvothermal process, however, the process makes extensive use of the solvents, requires high temperature and long hours of reaction time making the process economically and industrially not feasible. The present invention provides a mechanochemical process which ameliorates the disadvantages of the solvothermal process. The mechanochemical process used in the present invention is relatively simple, efficient, fast and feasible method for the synthesis of porous organic polymers as it follows a green synthetic pathway which does not require any harsh experimental conditions, high energy consumption and the use of toxic organic solvents.In an embodiment, the present invention relates to a novel guanidinium-based ionic porous organic polymer of Formula (I), comprising; Formula IIn an embodiment, the ratio of TBM:TGDM in the guanidinium-based ionic porous organic polymer of Formula (I) is 1:1.In an embodiment, the guanidinium-based ionic porous organic polymer of Formula (I) is crystalline in nature and is characterized by PXRD with characteristic peaks at 10, 13, 23, 28, 31, 39 ±2theta. [Fig 2a]In another embodiment, the elemental analysis of guanidinium-based ionic porous organic polymer of Formula (I) showed the presence of 58% C, 15% N, 21% O, and 6% Cl in the framework.The FT-IR spectra of TGDM showed the characteristic vibration of amine group around 3200 cm-1[Fig 1a]. TMB shows a strong carbonyl stretching around 1700 cm-1 [Fig 1a]. The strong absorption at 1500-1400 cm-1 for gn-ipop-cl [Fig 1a] suggests the formation of imine linkage through schiff base condensation. The absence of carbonyl and amine peaks in the spectra of gn-ipop-cl further confirms the complete conversion of the monomers. The solid state 13C NMR spectra of gn-ipop-cl also confirms the formation of imine linkage [Fig 1b]. The peaks observed around 140-150 ppm corresponds to imine carbon. The absence of any peak in the region of 190-200 ppm further confirms the complete condensation of monomers [Fig 1b].The thermal stability of guanidinium-based ionic porous organic polymer of Formula (I) was analyzed using thermogravimetric analysis (TGA) and was observed to be stable up to 300°C (Fig 2c-2d). In yet another embodiment, the guanidinium-based ionic porous organic polymer of Formula (I) has a BET surface area of 30 to 40m2 / g.The guanidinium-based ionic porous organic polymer of Formula (I) is porous in nature, has high chemical and thermal stability, and functional tenability. The Guanidinium based ionic porous organic polymers are particularly significant due to their capabilities in ion exchange and adsorption.In yet another aspect, the present invention discloses mechanochemical process for synthesis of guanidinium-based ionic porous organic polymer of Formula (I) comprising;(i) Imine Condensation of 4,4',4'' [1,3,5-triazine-2,4,6-Triyltris(oxy)tris]3-methoxybenzaldehyde (TMB) and triaminoguanidinium hydrochloride (TGDM) by mixing in equimolar quantity and heating; (ii) Adding acetic acid as catalyst to the above heated mix and grinding uniformly until completion of polymerization; and(iii) Washing several times to ensure the removal of unreacted monomeric units and drying to obtain the desired product. The process is depicted below: According to the process described above, an equimolar mixture of TMB and TGDM were taken, dry powder was slightly heated, acetic acid catalyst was added and uniformly grinded about one hour to complete the polymerization. The collected yellow powder was then subjected to multiple washing to ensure the removal of unreacted monomeric units. In an embodiment, the preparation of guanidinium-based ionic porous organic polymer of Formula (I) by mechanochemical method was completed in about one hour. In an embodiment, the guanidinium-based ionic porous organic polymer of Formula (I) exhibited adsorbent activity and effectively was used for adsorption of undesired ions, water pollutants like organic dyes, iodine etc. In an embodiment, the present invention discloses the adsorption of permanganate ions from aqueous solution using the guanidinium-based ionic porous organic polymer of Formula (I). The polymer showed a fast adsorption kinetics with a removal efficiency of 100%. It was evident from the absorbance spectra as the absorbance decreases to zero after 20 minutes of contact. The adsorption follows pseudo first order kinetics as evident from the kinetic studies [illustrated in [Fig 4b]. The uptake capacity of the polymer was found to be about 9.4 g / g [Fig 4c] which was exceptionally high compared to the existing literature reports where the maximum uptake is lower than 5.3g / g. The adsorption model also complied with Freundlich model suggesting the multilayer adsorption [Fig 4d]. The temperature dependence of adsorption of permanganate over gn-ipop-cl was also evaluated. It was observed that there was a decrease in the adsorption performance upon increasing the temperature from 25° to 35°C which would be attributed to the physical nature of adsorption.The guanidinium-based ionic porous organic polymer of Formula (I) could be used to remove several other hazardous pollutants like organic dyes, iodine etc. as depicted in figs 6a-h and Fig 7a-b. In yet another embodiment, the present inventions provide a guanidinium-based ionic porous organic polymer of Formula (I) doped with copper. In an aspect, the guanidinium-based ionic porous organic polymer of Formula (I) doped with copper is prepared by a process comprising; (i) Dropping aqueous solution of copper salt over a thin layer of uniformly spreaded polymer; (ii) Evaporating the resulting suspension of step (i) to dryness, washing and drying until the desired loading of the copper metal is achieved. In yet another embodiment, the present invention relates to the carbonization process of synthesis of copper doped porous carbon material [Cu- PCM] derived from guanidinium based porous organic polymer [gn-ipop-cl] as the precursor. The process comprises heating of the polymer at a temperature ranging between 350-450°C for about 4 hours at a heating rate of 5°C / minute under nitrogen atmosphere.The copper doped porous carbon material [Cu- PCM] is crystalline nature evident from SEM and elemental analysis. Further, the copper doped porous carbon material is characterized by PXRD with characteristic peaks at 36, 43, 50, 74±2theta. The FE SEM images [Figure 8c and 8d] obtained shows the highly porous network morphology of the carbonized material.In another embodiment, the copper doped porous carbon material [Cu- PCM] exhibits the BET surface area of 1560 m2 / g. In another aspect, the copper metal is loaded on to the polymer in an mount ranging between 50- 100mg. In another embodiment, the copper doped porous carbon material [Cu- PCM] acts as a heterogenous catalyst for chemical reactions. In an embodiment, the benzene hydroxylation was carried out using copper doped porous carbon material [Cu- PCM] as heterogenous catalyst. Cu-PCM showed high catalytic efficiency with a maximum conversion of 86 % with a selectivity of 30.31 % phenol and 69.68% dihydroxy benzene as the products as shown belwo in table 1. The obtained products were confirmed via gas chromatography as well as liquid chromatography coupled with mass spectrometry analysis. The catalyst was recyclable up to 3 cycles. Moreover the catalytic process operates under milder conditions making the process more economical and environmentally benign.In yet another embodiment, the present invention discloses the use of guanidinium-based ionic porous organic polymer of Formula (I) as an effective adsorbent of ions, pollutants and hazardous pollutants like organic dyes, iodine etc. and in ion-exchange reactions. In another embodiment, the present invention discloses the copper doped porous carbon material [Cu- PCM] derived by carbonization of copper doped guanidinium-based ionic porous organic polymer of Formula (I) as heterogenous catalyst. In another embodiment, the present invention discloses a method for adsorption of ions, pollutants and hazardous pollutants like organic dyes, iodine etc. in ion-exchange reactions comprising adding an effective amount the guanidinium-based ionic porous organic polymer of Formula (I) to the sample thereof. In yet another embodiment, the present invention discloses a method for efficient chemical reactions comprising adding in effective amount the heterogeneous catalyst copper doped porous carbon material [Cu-PCM] derived by carbonization of copper doped guanidinium-based ionic porous organic polymer of Formula (I).In an embodiment, the Guanidinium based porous organic polymer of the present invention was employed to develop porous carbon materials (PCM), PCM derived from Guanidinium based porous organic polymer which possess large surface areas, high pore volume, and good electrical conductivity. The Guanidinium-based porous organic polymer serves as a multipurpose material, functioning as both an effective adsorbent for hazardous pollutants and a heterogeneous catalyst for chemical reactions.In an embodiment, the present invention provides a green synthesis method comprising the mechanochemical method for synthesis of Guanidinium based porous organic polymer which is economical and industrially feasible over the conventional solvothermal process. The following examples, which include preferred embodiments, is intended to illustrate the practice of this invention. It is being understood that the particulars shown are by way of example and for purpose of illustrative discussion of preferred embodiments of the invention.EXAMPLES:EXAMPLE 1A] Preparation of triaminoguanidinium hydrochloride(TGDM)Monomer TGDM [Scheme 1a] was synthesized by reacting guanidinium hydrochloride and hydrazine hydrate using 1,4-dioxane as the solvent under reflux condition for 2 hours. The obtained solid product was collected by filtration, washed with 1,4-dioxane and dried. Yield and Purity % yield = [Observed weight / Theoretical weight]*100Yield obtained = 97 % yield.The product obtained in step A was characterized by 1H NMR [Fig S1] and FT-IR spectroscopy [Fig 1a]. All the proton signals of the product were confirmed in the 1H NMR spectrum. The FT-IR spectra of TGDM shows characteristic vibrational bands around 3350 and 3180 cm-1 corresponding to NH2 stretching and vibrational bands around 1690 cm-1 corresponding to imine stretching respectively [Fig 1a].B] Preparation of4,4,4 [1,3,5-triazine-2,4,6-triyltris(oxy)tris]3-methoxybenzaldehyde[TMB].Monomer TMB [Scheme 1b] was synthesized by reacting cyanuric chloride and vanillin [7.5 mmoles] using sodium hydroxide as base and acetone / water as solvent. The reaction was carried out at 0 to 5°C for 6 hours. The resultant product was collected through filtration, washed with distilled water and dried. The yield value is 95%.C] Synthesis of guanidinium based ionic porous organic Polymer of formula I by mechano chemical process. Guanidinium based ionic porous organic polymer was synthesized by an imine condensation reaction between triaminoguanidinium hydrochloride[TGDM] and 4,4,4 [1,3,5-triazine-2,4,6-triyltris(oxy)tris]3-methoxybenzaldehyde[TMB]. An equimolar mixture of TMB and TGDM prepared above was taken, dry powder was slightly heated, 0.2 mL of 6 M acetic acid catalyst was added and uniformly grinded for 45 minutes to complete the polymerization. The collected yellow powder was then subjected to multiple washing to ensure the removal of unreacted monomeric units if any. The yield value is 96.7 %Characterization of guanidinium based ionic porous organic Polymer of formula I.The product was characterized by 1HNMR and FT-IR spectroscopy [Fig 1a]. The 1H NMR spectrum confirmed all the proton peaks associated with the product. The FT-IR spectra of the compound shows carbonyl stretching band at 1700 cm-1. The vibrational band around 1570 cm-1 corresponds to triazine ring. The characteristic stretching vibration of C-O was observed around 1145 cm-1. The absence of hydroxyl stretching and C-Cl stretching further confirms the complete conversion of the starting materials. The FT-IR spectra of TGDM shows the characteristic vibration of amine group around 3200 cm-1[Fig 1a]. TMB shows a strong carbonyl stretching around 1700 cm-1 [Fig 1a]. The strong absorption at 1500-1400 cm-1 for gn-ipop-cl [Fig 1a] suggests the formation of imine linkage through schiff base condensation. The absence of carbonyl and amine peaks in the spectra of gn-ipop-cl further confirms the complete conversion of the monomers. The solid state 13C NMR spectra of gn-ipop-cl also confirms the formation of imine linkage [Fig 1b]. The peaks observed around 140-150 ppm corresponds to imine carbon. The absence of any peak in the region of 190-200 ppm further confirms the complete condensation of monomers [Fig 1b].Scheme 1. Synthetic scheme for the Guanidinium based ionic porous organic polymer gn-ipop-cl Figure 1. [a] FT-IR spectra for TGDM, TMB, gn-ipop-cl and [b] CPMAS 13C NMR spectra of gn-ipop-cl The powder x-ray diffraction pattern of gn-ipop-cl(MC) [MC representing mechanochemically synthesized polymer] exhibitted several intense peaks at 2θ 20 to 40 indicating the crystallinity of the sample. Whereas gn-ipop-cl(ST) [ST representing solvothermally synthesized polymer] showed a broad diffraction peak suggestive of the amorphous nature of the polymer [Fig 2a and 2b]. The thermal stability of the sample was analysed using thermogravimetric analysis (TGA) and found to be stable upto 300°C [Fig 2c, 2d]. Figure 2. pXRD pattern of [a] gn-ipop-cl(ST), [b] gn-ipop-cl(MC); TGA profile of [c] gn-ipop-cl(ST), [d] gn-ipop-cl(MC); BET surface area for [e] gn-ipop-cl(ST), [f] gn-ipop-cl(MC)The nitrogen sorption analysis performed at 77 K indicated a Brunauer-Emmett-Teller (BET) surface area of 30 m2 / g [Fig 2e, 2f]. This is nearly identical for both mechanochemical as well as solvothermal method. Furthermore the morphological characterization of the polymer was performed using field emission scanning electron microscopy (FE SEM). The obtained results indicated that the synthetic method indeed has a great influence on the morphology of the polymer as the solvothermal and mechanochemical synthesis resulted in entirely different morphology of the material [Fig 3]. The elemental analysis of gn-ipop-cl showed the presence of 58% C, 15 % N, 21% O and 6% Cl atoms in the framework. The superior quality with respect to the physicochemical properties and the environmental beningity of synthesis prompted us to select gn-ipop-cl(MC) as an adsorbent material and has been further explored for permanganate adsorption studies. Figure 3. Field emission scanning electron microscopy (FE SEM) images of [a,b] gn-ipop-cl(ST) and [c,d] gn-ipop-cl(MC) Example 2: Comparative process for preparation of guanidinium based porous organic polymer of formula (I) by solvothermal process .An equimolar mixture of TMB and TGDM were taken in a schlenk tube along with 8 mL of solvent [water and 1,4-dioxane in the ratio of 1:3]. The mixture was then sonicated for one hour to disperse the monomers completely, followed by the addition of 0.2 mL of 6 M acetic acid which serves as the catalyst for the polymerization. The reaction mixture was then heated at 120°C for 3 days. The resulting yellow powder was filtered and washed multiple times using water, 1,4-dioxane, and acetone and dried in an air oven overnight. The yield value from the above reaction is 92.5 %EXAMPLE 3Permanganate uptake studiesThe guanidinium based porous organic polymer for adsorptive removal of permanganate ions as the cationic charge in the framework attracts the anionic pollutant several folds compared to a neutral molecule and could increase the adsorption capacity. Biocompatible guanidinium moiety enhances its applicability in treating real water samples. We have employed gn-ipop-cl for the removal of permanganate ions from aqueous solution. The adsorption of permanganate ions from aqueous solution by gn-ipop-cl was monitored by UV-Vis spectra. A 1 mM aqueous solution of potassium permanganate was used for the preliminary studies. The UV-Vis spectra of each solution were recorded after ten times dilution of the original aliquots. The decrease in absorbance value of permanganate with time [Fig 4a] clearly indicated the removal of permanganate ions from water. The polymer showed a fast adsorption kinetics with a removal efficiency of 100% . It is evident from the absorbance spectra as the absorbance decreases to zero after 20 minutes of contact.Figure 4 . [a] UV-Vis spectra of KMnO4 demonstrating the fast uptake of permanganate in presence of gn-ipop-cl, [b] First order fitting for KMnO4 adsorption, [c] Isotherm for adsorption of KMnO4 and [d] Freundlich fitting for adsorption isotherm. The adsorption follows pseudo first order kinetics as evident from the kinetic studies [illustrated in [Fig 4b]. The uptake capacity of the polymer was found to be 9.4 g / g [Fig 4c] which is exceptionally high compared to the existing literature reports where the maximum uptake is lower than 2 g / g.[7] The adsorption model fits well with Freundlich model suggestive of multilayer adsorption [Fig 4d]. The temperature dependence of adsorption of permanganate over gn-ipop-cl was also evaluated. It was observed that there is a decrease in the adsorption performance upon increasing the temperature from 25° to 35 °C.. This might be attributed to the physical nature of adsorption. Thus we report that the material exhibits exceptionaly high uptake for permanganate ions from water (Fig 5). The exceptionally high uptake of permanganate ions can be attributed the strong adsorptive interaction due to electrostatic interaction which might be the reason for formation of multilayers. Figure 5. Photographs of permanganate solution and polymer adsorbent before and after adsorption of permanganateThe gn-ipop-cl(MC) and gn-ipop-cl(ST) showed identical activity in the studies for removal of permanganate ions. Hence, we also report that mechanochemically synthesized guanidine based ionic porous organic polymer is easier to synthesize, faster process, showed superior properties compared to its solvothermal analogue and retained similar activity. Figure 6. UV-Visible spectra and Uptake capacity observed for [a,b] Methyl orange[1004 mg / g], [c,d] Crystal violet[400 mg / g], [e,f] Rhodamine B[127 mg / g], [g,h] Eriochrome black T[115 mg / g] obtained using gn-ipop-cl as adsorbentFigure 7. [a] UV-Visible of adsorption of iodine [b] Uptake capacity calculated for adsorption of iodineEXAMPLE 4Adsorption of other hazardous pollutantsAdditionally it could also remove several other hazardous pollutants like organic dyes, iodine etc.EXAMPLE 5Synthesis of porous carbon material from Guanidinium based porous organic polymer5.1. Synthesis of copper dopped polymer [Cu-gn-ipop-cl]Cu2+ ions were introduced into the polymer framework through a post synthetic modification strategy, insipient wetness impregnation [Figure 8]. In this method, aqueous solution of cupric nitrate was dropped over a thin layer of uniformly spreaded polymer. The resulting suspension was evaporated to dryness at room temperature, washed with distilled water and dried at 60°C for overnight in an air oven. The process was repeated thrice to obtain desired metal loading into the polymer. Cu-gn-ipop-cl was then employed for high temperature thermal processing to obtain Cu2+ doped porous carbon material (Cu-PCM).5.2. Synthesis of copper dopped porous carbon material [Cu-PCM] (Fig. 8)Figure 8 : schematic representation of synthesis of copper dopped porous carbon material [Cu-PCM] derived from guanidinium based porous organic polymer [gn-ipop-cl] as the precursorCu-PCM was synthesized from Cu-gn-ipop-cl by the carbonization method at high temperature. The high temperature thermal processing involves the heating of the the polymer in a tubular furnace at 400°C for 4 hours at a heating rate of 5°C / minute under nitrogen atmosphere.The resulting carbon material was characterized using powder X-ray diffraction, N2 sorpton analyss, Field emission scanning electron microscopy and elemental analysis. High crystallinity of the sample is evident from the PXRD pattern [Figure 8a]. The thermal processing of polymer was performed at 400 °C, which causes the decomposition of cupric nitrate to CuO. This is evident from the PXRD pattern as well. The PXRD pattern shows intense peaks around 2θ 42, 50 and 74 which is matched with the PXRD pattern of CuO reported. A slight elevation in the region of 2θ 20 to 30 which is mostly masked by high intensity CuO peaks represents amorphous carbon phase
[55] . The nitrogen sorption analysis performed at 77 K [Figure 8b] indicated a Brunauer-Emmett-Teller (BET) surface area of 1560 m2 / g which is considerably high suggestive of highly porous nature of the catalyst. This was further confirmed in the FE SEM images. The FE SEM images [Figure 8c and 8d] obtained shows the highly porous network morphology of the carbonized material. The elemental analysis confirmed the presence of Cu2+ in the frameworkFigure 9 : [a] PXRD pattern of Cu-PCM [b] BET surface area analyss of Cu-PCM [c] and [d] FE SEM images of Cu-PCMFigure 10 : [a] Effect of catalyst loading on % conversion, [b] Effect of temperature on % conversion, [c] Effect of reaction time on % conversion and [d] Effect of concentration of substrate on % conversionSl no. Product Retention time % selectivity1 phenol 5.057 30.312 dihydroxybenzene 8.907 10.923 dihydroxybenzene 9.509 58.76Table 1 : illustration of % selectivity of productsResults: Cu-PCM showed high catalytic efficiency with a maximum conversion of 86 % with a selectivity of 30.31 % phenol and 69.68% dihydroxy benzene as the products. The obtained products were confirmed via gas chromatography as well as liquid chromatography coupled with mass spectrometry analysis. The catalyst was recyclable upto 3 cycles. Moreover the catalytic process operates under milder conditions making the process more economical and environmentally benign.
Claims
1. Guanidinium-based ionic porous organic polymer of Formula (I), comprising; 4,4',4" [1,3,5-triazine- 2,4,6- triyltris(oxy)tris]3-methoxybenzaldehyde [TMB] and triaminoguanidinium hydrochloride[TGDM] in 1;1 ratio characterized by Powder x-ray diffraction pattern with characteristic peaks at 10,13,23,28,31,39 ±2θ.
2. The Guanidinium-based porous polymer as claimed in claim 1, wherein said organic polymer is stable up to 300°C.
3. The Guanidinium-based porous polymer as claimed in claim 1, wherein the said organic polymer has a BET surface area of 30-40 m2 / g.
4. A mechanochemical process for synthesis of guanidinium-based ionic porous organic polymer of Formula (I) as claimed in claim 1 comprising; a) Mixing 4,4',4" [1,3,5-triazine-2,4,6-Triyltris(oxy)tris]3- methoxybenzaldehyde (TMB) and triaminoguanidinium hydrochloride (TGDM) in equimolar mixture and heating; b) Adding acetic acid as catalyst to the above heated mix and grinding uniformly until completion of polymerization; and c) Washing several times to ensure the removal of unreacted monomeric units and drying to obtain the desired product.
5. The guanidinium-based ionic porous organic polymer of Formula (I) as claimed in any one of the claims 1 to 4, wherein the guanidinium-based ionic porous organic polymer is doped with copper.
6. The guanidinium-based ionic porous organic polymer as claimed in claim 5, prepared by the process comprising; a) dropping aqueous solution of copper salt over a thin layer of uniformly spreaded polymer; b) evaporating the resulting suspension of step (i) to dryness, washing and drying until the desired loading of the copper metal is achieved.
7. The guanidinium-based ionic porous organic polymer as claimed in claim 6, wherein the copper is loaded in an amount ranging between 50- 100mg per. 150 to 300 mg.wt of the polymer.
8. A copper doped porous carbon material [Cu- PCM] characterized by PXRD with characteristic peaks at 36, 43, 50, 74±2theta.
9. The copper doped porous carbon material [Cu- PCM] as claimed in claim 8, with the BET surface area of 1560m2 / g.
10. A copper doped porous carbon material [Cu- PCM] prepared by carbonization of the copper doped polymer claimed in claim 7 at a temperature ranging between 350-450°C at a heating rate of 5°C / minute under nitrogen atmosphere.
11. Use of guanidinium-based ionic porous organic polymer as claimed in any one of the preceding claims 1-10 as an adsorbent and as a heterogeneous catalyst.
12. A method of adsorbing the ions and other pollutants comprising adding an effective amount of the guanidinium-based ionic porous organic polymer as claimed in any one of the preceding claims 1-10.
13. A method of performing the chemical reaction with high selectivity comprising adding an effective amount of the guanidinium-based ionic porous organic polymer as a heterogeneous catalyst as claimed in any one of the preceding claims 1-10.