Ruthenium liner and cap for back-end-of-line applications
Patent Information
- Application Number
- JP2024088936
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-07-22
- Filing Date
- 2024-05-31
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-07-23
Smart Images

Figure 2024133059000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE Embodiments of the present disclosure generally relate to methods for forming interconnects in electronic devices. In particular, embodiments of the present disclosure relate to methods and electronic devices that use ruthenium-containing bilayers for liner and capping. [Background technology]
[0002] Semiconductor circuit elements have been miniaturized to the point where feature sizes of 20 nm and below are being manufactured on a commercial scale. As the size of the critical dimensions continues to decrease, new challenges arise for process steps such as filling the gaps between circuit elements. As the width between elements continues to decrease, the gaps between elements often become taller and narrower, making it more difficult to fill the gaps and more difficult to make robust contacts.
[0003] From the 20nm node to the 3nm node, cobalt (Co) liner and Co capping have been the primary materials to improve copper (Cu) gapfill and reliability. For nodes beyond 3nm, gapfill on cobalt liner shows some limitations.
[0004] Copper reflow on ruthenium (Ru) liners has shown potential scalability to small features, however there are reliability issues with the use of Ru, for example copper corrosion of interconnects has been observed resulting in reduced device lifetime. Summary of the Invention [Problem to be solved by the invention]
[0005] Therefore, there is a need for improved methods for forming interconnects in electronic devices. [Means for solving the problem]
[0006] One or more embodiments of the present disclosure are directed to an electronic device. A first conductive line extends along a first direction. A dielectric material is formed on a substrate surface on the first conductive line. The dielectric material has a top surface with a surface structure formed on the surface of the dielectric material. The surface structure has sidewalls and a via bottom. The via bottom includes a top surface of the first conductive line. A barrier layer is formed on the top surface and sidewalls of the dielectric material. A liner is formed on the barrier layer. The liner has a liner bottom surface spaced a distance from the top surface of the first conductive line. A conductive filler is within the surface structure. The conductive filler forms a second conductive line extending along a second direction and contacts the first conductive line.
[0007] A further embodiment of the present disclosure relates to a method of forming an electronic device. A passivation layer is formed in a via portion of a surface structure formed in a dielectric material. The passivation layer is formed on a surface of a first conductive material and is separated from the dielectric material by a barrier layer formed on the sidewalls, the bottom of the trench portion of the surface structure, and on a top of the dielectric material. The first conductive material extends along a first direction. A liner is formed on the barrier layer. The liner has a liner bottom surface that contacts the passivation layer in the via portion. The passivation layer is removed to leave the bottom surface of the liner spaced a distance from a top surface of the first conductive line. The surface structure is filled with a conductive fill to form a via in the via portion and a second conductive line in the trench portion. The second conductive line extends along a second direction. The via contacts the first conductive line in the via portion. A cap layer is formed on the conductive fill.
[0008] In order that the above-listed features of the present disclosure may be understood in detail, a more particular description of the present disclosure briefly summarized above may be made by reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings illustrate only typical embodiments of the present disclosure and therefore should not be considered as limiting its scope, since the present disclosure may admit of other equally effective embodiments. The embodiments described herein are illustrated by way of example, and not by way of limitation, in the figures of the accompanying drawings, in which like reference numerals denote like elements. [Brief description of the drawings]
[0009] [Figure 1] 1 is a partial cross-sectional view of an electronic device formed in accordance with one or more embodiments of the present disclosure. [Diagram 2] 1 is a partial cross-sectional view of an electronic device formed in accordance with one or more embodiments of the present disclosure. [Figure 3A] 1 is a partial cross-sectional view of an electronic device formed in accordance with one or more embodiments of the present disclosure. [Figure 3B] FIG. 3B is an enlarged view of region 3 in FIG. 3A. [Figure 4A] 1 is a partial cross-sectional view of an electronic device formed in accordance with one or more embodiments of the present disclosure. [Figure 4B] FIG. 4B is an enlarged view of region 3 in FIG. 4A. [Figure 5A] 1 is a partial cross-sectional view of an electronic device formed in accordance with one or more embodiments of the present disclosure. [Figure 5B] FIG. 5B is an enlarged view of region 3 in FIG. 5A. [Figure 6A] 1 is a partial cross-sectional view of an electronic device formed in accordance with one or more embodiments of the present disclosure. [Figure 6B] FIG. 6B is an enlarged view of region 6 of FIG. 6A. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Before describing certain example embodiments of the present disclosure, it is to be understood that the present disclosure is not limited to the details of construction or process steps set forth in the following description as being capable of other embodiments and of being practiced and carried out in various ways.
[0011] As used herein and in the appended claims, the term "substrate" refers to a surface or a portion of a surface on which a process acts. Those skilled in the art will also understand that a reference to a substrate can also refer to only a portion of the substrate, unless the context clearly indicates otherwise. Additionally, a reference to depositing on a substrate can refer to both a bare substrate and a substrate on which one or more films or features have been deposited or formed.
[0012] "Substrate" as used herein refers to any substrate or surface of material formed on a substrate on which film processing is performed during a manufacturing process. For example, substrate surfaces on which processing can be performed include materials such as silicon, silicon oxide, strained silicon, silicon-on-insulator (SOI), carbon-doped silicon oxide, amorphous silicon, doped silicon, germanium, gallium arsenide, glass, sapphire, and any other materials such as metals, metal nitrides, metal alloys, and other conductive materials, depending on the application. Substrates include, but are not limited to, semiconductor wafers. The substrate can be exposed to a pretreatment process to polish, etch, reduce, oxidize, hydroxylate, anneal, UV cure, e-beam cure, and / or bake the substrate surface. In addition to performing film processing directly on the surface of the substrate itself, the present disclosure also allows any of the disclosed film processing steps to be performed on an underlayer formed on the substrate, as disclosed in more detail below, and the term "substrate surface" is intended to include such underlayers as the context indicates. Thus, for example, when a film / layer or partial film / layer is deposited on a substrate surface, the exposed surface of the newly deposited film / layer becomes the substrate surface.
[0013] Ruthenium (Ru) as a liner could not previously be used for the N3 (3 nm node) due to at least reliability, line resistance Rs, copper corrosion, chemical mechanical planarization (CMP) and other integration issues. Some embodiments use ruthenium, optionally with Ru (doped Ru, bottomless Ru) liner and / or Ru (doped Ru) capping, in the N2 node to mitigate process integration issues. Some embodiments use bottomless ruthenium liners to prevent copper corrosion and reduce via resistance. The bottomless liner of some embodiments is deposited by selectively depositing ruthenium on a dielectric surface on a copper surface.
[0014] One or more embodiments of the present disclosure enable the replacement of cobalt with ruthenium as a liner and capping layer in advanced node applications. Some embodiments solve the reliability issues that limit the application of ruthenium from larger node devices. Some embodiments of the present disclosure enable ruthenium as a liner for gap-fill scalability, enable ruthenium as a capping layer for reliability, reduce via contact resistance (Rc), and / or provide an overall integrated scheme to prevent or slow copper corrosion.
[0015] Some embodiments of the ruthenium liner or doped ruthenium liner extend physical vapor deposition (PVD) copper reflow as a gap-fill solution for advanced nodes. Some embodiments provide ruthenium or doped ruthenium capping to improve device reliability. Some embodiments incorporate a surfactant-assisted ruthenium process to achieve a device with no ruthenium at the bottom of the structure, preventing corrosion and improving via resistance.
[0016] 1-6B illustrate an electronic device 100 during different stages of a method according to one or more embodiments of the present disclosure. The various fill patterns used in the figures are intended to facilitate distinguishing components and should not be construed as referring to any particular material.
[0017] With reference to FIG. 1, a first conductive line 120 is formed on a substrate 110 and extends along a first direction. The first direction may also be referred to as the X-axis direction. For example, the first conductive line 120 of some embodiments has a length along the X-axis direction, a width along the Y-axis direction, and a thickness measured along the Z-axis direction. The figure shows an XZ plane, with the Y-axis extending perpendicular to the page of the figure. The use of the X-axis, Y-axis, and Z-axis should not be construed to imply any particular orientation with respect to gravity.
[0018] In the illustrated embodiment, various spacer layers 112, 114, 116, 118 are shown. These various spacer layers are optional, and in some embodiments, any or all of the layers are omitted. The use of the term "spacer layer" is not intended to imply any particular function or purpose for the illustrated layers. The spacer layers 112, 114, 116, 118 can be any suitable material having any suitable purpose. For example, the spacer layers can include a dielectric, a diffusion barrier, an adhesion promoter, or any other layer known to one of ordinary skill in the art. In some embodiments, the spacer layer 114 includes a dielectric material and the spacer layers 112, 116 include a barrier or liner material to prevent direct contact between the first conductive line 120 and the substrate 110.
[0019] In some embodiments, forming the first conductive line 120 includes filling the trench with a layer of conductive material. In one or more embodiments, a base layer (not shown) is first deposited on the interior sidewalls and bottom of the trench, and then a conductive layer is deposited on the base layer (e.g., spacer layer 112). In one or more embodiments, the base layer includes a conductive seed layer (not shown) deposited on a conductive barrier layer (not shown). The seed layer can include copper (Cu), and the conductive barrier layer can include a metal such as aluminum (Al), titanium (Ti), tantalum (Ta), tantalum nitride (TaN), etc. The conductive barrier layer can be used to prevent diffusion of a conductive material, such as copper or cobalt, from the seed layer to the first insulating layer 104. In addition, the conductive barrier layer can be used to provide adhesion to the seed layer (e.g., copper).
[0020] The first conductive line 120 may be formed by any suitable process known to those skilled in the art. For example, in some embodiments, the first conductive line 120 is formed by one or more of an electroplating process, selective deposition, electrolysis, chemical vapor deposition (CVD), physical vapor deposition (PVD), molecular beam epitaxy (MBE), atomic layer deposition (ALD), spin-on techniques, or other deposition techniques known to those skilled in the art of microelectronic device manufacturing.
[0021] The first conductive line 120 can be any suitable conductive material known to one of ordinary skill in the art. In one or more embodiments, the first conductive line 120 includes a metal, such as copper (Cu), ruthenium (Ru), nickel (Ni), cobalt (Co), molybdenum (Mo), rhodium (Rh), iridium (Ir), niobium (Nb), nickel silicon (NiSi), a ternary compound (e.g., LaRu2As2), or any combination thereof.
[0022] The first conductive lines 120 can have any suitable thickness (measured along the z-axis of FIG. 1). In some embodiments, the first conductive lines 120 have a thickness in the range of 15 nm to 1000 nm, or in the range of 20 nm to 200 nm. In one non-limiting example, the width of the first conductive lines 120 (measured along the y-axis of FIG. 1, which extends perpendicular to the plane of the page) is in the range of 5 nm to 500 nm. In one non-limiting example, the spacing (pitch) between adjacent first conductive lines 120 is in the range of 2 nm to 500 nm, or in the range of 50 nm to 50 nm.
[0023] Dielectric material 130 is formed at the substrate surface (on top of first conductive lines 122) on first conductive lines 120. As used in this manner, the substrate surface is the exposed surface of the material on which dielectric material 130 is formed. For example, first conductive lines 120 in some embodiments are formed on the surface of substrate 110, forming a new substrate surface on which dielectric material 130 is formed.
[0024] In some embodiments, the dielectric material 130 has a top surface 132 with a surface structure 140. The surface structure 140 is formed on the top surface 132 of the dielectric material 130. In some embodiments, the surface structure 140 includes a sidewall 141, a via portion 142, and a trench portion 146. The via portion 142 of some embodiments includes a via bottom 143 and a via sidewall 144 opposite the sidewall 141. In some embodiments, the via bottom 143 includes the top surface 122 of the first conductive line 120.
[0025] Trench portion 146 in some embodiments includes a trench bottom 147 that connects via sidewall 144 with sidewall 141 to form a step-like structure, as shown. In some embodiments, surface structure 140 includes a uniformly shaped via or trench without a step-like structure.
[0026] The dielectric material 130 can be any material suitable for insulating adjacent devices and preventing leakage. In one or more embodiments, the dielectric material 130 is an oxide layer, e.g., silicon dioxide, or any other electrically insulating layer as determined by the electronic device design. In one or more embodiments, the dielectric material 130 comprises an interlayer dielectric (ILD). In one or more embodiments, the dielectric material 130 is a low-k dielectric, including, but not limited to, materials such as silicon dioxide, silicon oxide, carbon-doped oxides ("CDO"), e.g., carbon-doped silicon dioxide, porous silicon dioxide (SiO2), silicon nitride (SiN), or any combination thereof. The term "silicon oxide" may be used to describe the dielectric material 130, although one of ordinary skill in the art will recognize that the present disclosure is not limited to a particular stoichiometry. For example, the terms "silicon oxide" and "silicon dioxide" may both be used to describe materials having silicon atoms and oxygen atoms in any suitable stoichiometric ratio. The same is true for other materials listed in this disclosure, such as silicon nitride, silicon oxynitride, aluminum oxide, zirconium oxide, and the like.
[0027] In one or more embodiments, the dielectric material 130 comprises a dielectric material having a dielectric constant value of less than 5. In one or more embodiments, the dielectric material 130 comprises a dielectric material having a dielectric constant value of about 2 to about 4. In at least some embodiments, the dielectric material 130 comprises an oxide, a carbon doped oxide, black diamond, porous silicon dioxide, a carbide, an oxycarbide, a nitride, an oxynitride, an oxycarbonitride, a polymer, a phosphosilicate glass, a fluorosilicic acid (SiOF) glass, an organosilicate glass (SiOCH), a fluorosilicic acid glass (FSG), a porous low-k, or any combination thereof, other electrically insulating layers as determined by the electronic device design, or any combination thereof. In at least some embodiments, the dielectric material 130 can comprise a photosensitive material such as polyimide, an epoxy, benzocyclobutene (BCB), and a WPR series material, or a spin-on glass.
[0028] In one or more embodiments, the dielectric material 130 is a low-k interlayer dielectric to separate one metal line from another metal line on the substrate 110. In one or more embodiments, the thickness of the dielectric material 130 is in the approximate range of about 10 nanometers (nm) to about 2 microns (μm).
[0029] In one or more embodiments, the dielectric material 130 is deposited or formed using one of a number of deposition techniques, such as, but not limited to, plasma enhanced chemical vapor deposition ("PECVD"), physical vapor deposition ("PVD"), molecular beam epitaxy ("MBE"), metalorganic chemical vapor deposition ("MOCVD"), atomic layer deposition ("ALD"), spin-on, or other insulating deposition techniques known to those skilled in the art of microelectronic device manufacturing.
[0030] In some embodiments, the surface structures 140 are formed by any suitable technique known to those skilled in the art. In some embodiments, the dielectric material 130 is patterned and etched using a hard mask to form the surface structures 140 using one or more patterning and etching techniques known to those skilled in the art of microelectronic device manufacturing.
[0031] A barrier layer 150 is formed on the top surface 132 of the dielectric layer 130 and the sidewalls 141 of the surface structure 140. In some embodiments, the barrier layer 150 is formed on the via sidewalls 144 and trench bottom 147 in addition to the sidewalls 141 and top surface 132 of the dielectric material 130 as shown in Figure 1. In some embodiments, the barrier layer 150 is formed conformally to the sidewalls 141, top surface 132, via sidewalls 144, and trench bottom 147.
[0032] Barrier layer 150 may include any suitable material known to one of ordinary skill in the art formed by any suitable technique known to one of ordinary skill in the art. In one or more embodiments, barrier layer 150 includes one or more of titanium nitride (TiN), tantalum nitride (TaN), etc. In some embodiments, the barrier layer is deposited by atomic layer deposition.
[0033] In some embodiments, the barrier layer 150 is selectively deposited on the dielectric material 130 on the first conductive line 120. For example, as shown, the barrier layer 150 is formed in contact with the dielectric material 130 but does not nucleate or experiences a relatively long nucleation delay on the first conductive line 120.
[0034] Referring to FIG. 2, a passivation layer 160 is formed on the exposed top surface 122 of the first conductive line 120 through the surface structure 140. The passivation layer 160 can be any suitable material known to one of ordinary skill in the art and can be deposited by any suitable technique. In some embodiments, the passivation layer 160 is selectively deposited on the first conductive line 120 above the barrier layer 150. The passivation layer 160 can be any material that protects the first conductive line 120 from the subsequent formation of the liner 170. The passivation layer 160 in some embodiments has a thickness in the range of 5 Å to 1000 Å, or in the range of 1 nm to 50 nm.
[0035] Stated another way, in some embodiments, the passivation layer 160 is formed in the via portion 142 of the surface structure 140 formed in the dielectric material 130. The passivation layer 160 is formed on the surface of the first conductive material 120 and is separated from the dielectric material 130 by a barrier layer 150 formed on the sidewalls 141, the via sidewalls 144 and bottom of the trench portion 146 of the surface structure 140, and the top surface 132 of the dielectric material 130.
[0036] 3A and 3B, a liner 170 is formed on the barrier layer 150. The liner 170 in some embodiments is conformally formed on the barrier layer 150. In some embodiments, the liner 170 is selectively formed on the barrier layer 150 over the passivation layer 160. Although the figures show the liner 170 in contact with the passivation layer 160, one of ordinary skill in the art will recognize that the liner 170 does not nucleate on the passivation layer 160 and that the contact between the liner 170 and the passivation layer 160 is physical and not chemical.
[0037] With the passivation layer 160 on the first conductive line 120, a liner 170 is formed with a bottom liner surface 172 spaced a distance from the top surface 122 of the first conductive line 120. The distance between the top surface 122 of the first conductive line 120 and the bottom liner surface 172 of the liner 170 is defined by the thickness of the passivation layer 160.
[0038] 3B, the liner 170 of some embodiments includes a first liner layer and a second liner layer. The first liner layer has a first bottom liner surface 172a and the second liner layer has a second bottom liner surface 172b, each of the bottom liner surfaces spaced a distance from the top surface 122 of the first conductive line 120.
[0039] In some embodiments, liner 170 includes a ruthenium layer 174 in contact with barrier layer 150 and a cobalt layer 177 on the opposite side of ruthenium layer 174 from barrier layer 150. Stated differently, in some embodiments, liner 170 includes a ruthenium layer 174 in direct contact with barrier layer 150 and a cobalt layer 177 in contact with ruthenium layer 174, separated from barrier layer 150 by ruthenium layer 174.
[0040] In some embodiments, the liner 170 has a total thickness (i.e., the sum of the thicknesses of all layers) in the range of 5 Å to 50 Å. The thickness of the liner 170 is measured along the sidewall 141, the via sidewall 144, and the trench bottom 147 of the surface structure 140. In some embodiments, the ruthenium layer 174 has a thickness in the range of 2.5 Å to 25 Å, or in the range of 5 Å to 20 Å, or in the range of 10 Å to 15 Å. In some embodiments, the cobalt layer 177 has a thickness in the range of 2.5 Å to 25 Å, or in the range of 5 Å to 20 Å, or in the range of 10 Å to 15 Å. In some embodiments, the ruthenium layer 174 and the cobalt layer 177 have approximately the same thickness. In some embodiments, the ruthenium layer 174 and the cobalt layer 177 have a thickness ratio in the range of 0.95:1 to 1:0.95. In some embodiments, the thickness ratio of ruthenium:cobalt is about 1:1. In some embodiments, each of the ruthenium and cobalt layers is about 10 Å thick.
[0041] In some embodiments, the liner 170 includes a dual layer of ruthenium and cobalt, with the ruthenium in contact with the barrier layer 150. The ruthenium can be ruthenium metal or doped ruthenium. Suitable dopants include, but are not limited to, oxygen, nitrogen, boron, carbon, copper, tungsten, molybdenum, aluminum, or manganese.
[0042] The liner 170 may be deposited by any suitable technique known to one of ordinary skill in the art, in some embodiments, the liner 170 or individual layers of the liner are deposited by atomic layer deposition.
[0043] In some embodiments, after the formation of the liner 170, the passivation layer 160 is removed, as shown in FIGS. 4A and 4B. Removal of the passivation layer 160 leaves a gap 180 such that the liner bottom surface 172 is spaced a distance from the top surface 122 of the first conductive line 120. The distance or thickness of the gap 180 is substantially the same (i.e., within ±10%) as the thickness of the passivation layer 160. The passivation layer 160 can be removed by any suitable technique depending on the material used. In some embodiments, the passivation layer 160 is removed by a selective etching process that does not significantly affect other surface materials.
[0044] 4B , in some embodiments, removing passivation layer 160 exposes first liner bottom surface 172a and second liner bottom surface 172b in gap 180. Stated another way, in some embodiments, liner 170 does not contact first conductive line 120 such that gap 180 exists between top surface 122 of first conductive line 120 and a bottom edge of liner 170.
[0045] 5A and 5B, after removing the passivation layer 160, a conductive filler 185 is deposited in the surface structure 140. The conductive filler 185 forms a second conductive line 181 extending along a second direction. The conductive filler 185 (second conductive line 181) directly contacts the first conductive line 120 at the via bottom 143 of the via portion 142 of the surface structure 140.
[0046] The conductive fill 185 may be any suitable material and may be deposited by any suitable technique known to one of ordinary skill in the art. In some embodiments, the conductive fill 185 forming the second conductive line 181 comprises copper or consists essentially of copper. When used in this manner, the term "consists essentially of" means that the film comprises 95%, 98%, 99%, or 99.5% or more of the recited material.
[0047] The conductive fill 185 may be formed by any suitable technique known to one of ordinary skill in the art. In some embodiments, the conductive fill 185 is deposited by physical vapor deposition. In one or more embodiments, the second conductive material 220 comprises a metal film or a metal-containing film. Metal films suitable for the conductive fill 185 include, but are not limited to, films comprising one or more of cobalt (Co), molybdenum (Mo), tungsten (W), tantalum (Ta), titanium (Ti), ruthenium (Ru), rhodium (Rh), copper (Cu), iron (Fe), manganese (Mn), vanadium (V), niobium (Nb), hafnium (Hf), zirconium (Zr), yttrium (Y), aluminum (Al), tin (Sn), chromium (Cr), lanthanum (La), or any combination thereof. In some embodiments, the conductive fill 185 forming the second conductive line comprises copper (Cu).
[0048] In one or more embodiments, the conductive filling 185 is deposited using one of a number of deposition techniques, such as, but not limited to, ALD, CVD, PVD, MBE, MOCVD, spin-on, or other liner deposition techniques known to those skilled in the art of microelectronic device manufacturing.
[0049] 6A and 6B, in some embodiments, a cap layer 190 is formed on the conductive filling 185 forming the second conductive line 181. FIG. 6B shows an expanded view of region 6 of FIG. 6A. In some embodiments, the cap layer 190 formed on the top surface 182 of the second conductive line 181 includes a first capping layer and a second capping layer. In some embodiments, the cap layer 190 includes a ruthenium layer 192 in contact with the conductive filling 185 forming the second conductive line 181 and a cobalt layer 194 on the side of the ruthenium layer 192 opposite the conductive filling 185 that is the second conductive line 181.
[0050] Stated another way, in some embodiments, the capping layer 190 includes a ruthenium layer 192 in direct contact with the second conductive line 181 and a cobalt layer 194 in contact with the ruthenium layer 192 and separated from the second conductive line 181 by the ruthenium layer 192.
[0051] In some embodiments, capping layer 190 has a total thickness (i.e., the sum of the thicknesses of all layers) in the range of 5 Å to 50 Å. In some embodiments, ruthenium layer 192 has a thickness in the range of 2.5 Å to 25 Å, or in the range of 5 Å to 20 Å, or in the range of 10 Å to 15 Å. In some embodiments, cobalt layer 194 has a thickness in the range of 2.5 Å to 25 Å, or in the range of 5 Å to 20 Å, or in the range of 10 Å to 15 Å. In some embodiments, ruthenium layer 192 and cobalt layer 194 have approximately the same thickness. In some embodiments, ruthenium layer 192 and cobalt layer 194 have a thickness ratio in the range of 0.95:1 to 1:0.95. In some embodiments, the thickness ratio of ruthenium:cobalt is about 1:1. In some embodiments, each of the ruthenium layer and the cobalt layer is about 10 Å thick.
[0052] The capping layer 190 may be deposited by any suitable technique known to one of ordinary skill in the art. In some embodiments, the capping layer 190 or an individual layer is deposited by atomic layer deposition. In some embodiments, the capping layer 190 is selectively formed on the top surface 182 of the second conductive line 181.
[0053] In some embodiments, the use of a selective binary cap layer and a ruthenium liner increased the electromigration failure time (at the 50% level) by more than 2.5 times. Having Ru first, then Co in the cap layer increased the 50% failure rate by more than 2 times over Co first, then Ru. Using a binary liner in addition to a binary cap layer further increased the failure time.
[0054] Throughout this specification, references to "one embodiment," "a particular embodiment," "one or more embodiments," or "an embodiment" mean that a particular feature, structure, material, or characteristic described in connection with an embodiment is included in at least one embodiment of the disclosure. Thus, the appearances of phrases such as "in one or more embodiments," "in a particular embodiment," "in one embodiment," or "in an embodiment" in various places throughout this specification are not necessarily all referring to the same embodiment of the disclosure. Furthermore, particular features, structures, materials, or characteristics may be combined in any suitable manner in one or more embodiments.
[0055] Although the disclosure herein has been described with reference to specific embodiments, those skilled in the art will recognize that the described embodiments are merely illustrative of the principles and applications of the disclosure. It will be apparent to those skilled in the art that various modifications and variations can be made to the disclosed method and apparatus without departing from the spirit and scope of the disclosure. Thus, the disclosure is intended to include modifications and variations that come within the scope of the appended claims and their equivalents.
Claims
1. a first conductive line extending along a first direction; a dielectric material formed on a substrate surface on the first conductive line, the surface structure having a top surface formed on the surface of the dielectric material, the surface structure having a sidewall and a via bottom, the via bottom including a top surface of the first conductive line; a barrier layer formed on the top surface and the sidewalls of the dielectric material; a liner formed on the barrier layer, the liner having a bottom surface spaced a distance from the top surface of the first conductive line; a conductive filler within the surface structure, the conductive filler forming a second conductive line extending along a second direction and contacting the first conductive line; An electronic device comprising:
2. The electronic device of claim 1 , wherein the liner comprises a ruthenium layer in contact with the barrier layer and a cobalt layer on an opposite side of the ruthenium layer from the barrier layer.
3. The electronic device of claim 2 , wherein the liner has a total thickness in the range of 5 Å to 50 Å.
4. The electronic device of claim 2, wherein the ruthenium layer has a thickness in the range of 2.5 Å to 25 Å and the cobalt layer has a thickness in the range of 2.5 Å to 25 Å.
5. The electronic device of claim 2 , wherein the ruthenium layer and the cobalt layer have a thickness ratio in the range of 0.95:1 to 1:0.
95.
6. The electronic device of claim 2 , wherein the surface structure in the dielectric material includes a trench portion and a via portion, the trench portion having a trench bottom and the via portion having the via bottom.
7. The electronic device of claim 6 , wherein the barrier layer is formed at the bottom of the trench.
8. The electronic device of claim 7 , wherein the barrier layer is a conformal layer.
9. The electronic device of claim 8 , wherein the second conductive line directly contacts the first conductive line at the via bottom of the via portion of the surface structure.
10. The electronic device of claim 2 , wherein the liner does not contact the first conductive line such that a gap exists between the top surface of the first conductive line and a bottom edge of the liner.
11. 3. The electronic device of claim 2, wherein the electromigration failure time (at a 50% level) is greater than 2.5 times the electromigration failure time of a comparable electronic device not having said liner comprising ruthenium and cobalt layers.
12. The electronic device of claim 2 , wherein the conductive filling comprises copper.
13. 13. The electronic device of claim 12, further comprising a capping layer on the conductive filling, the capping layer comprising a ruthenium layer in contact with the conductive filling and a cobalt layer on an opposite side of the ruthenium layer from the conductive filling.
14. forming a passivation layer in a via portion of a surface structure formed in a dielectric material, the passivation layer being formed on a surface of a first conductive material and separated from the dielectric material by a barrier layer formed on sidewalls, a bottom of a trench portion of the surface structure, and on a top of the dielectric material, the first conductive material extending along a first direction; forming a liner on the barrier layer, the liner having a bottom surface in contact with the passivation layer in the via portion; removing the passivation layer to leave the bottom surface of the liner spaced a distance from a top surface of the first conductive line; filling the surface structure with a conductive filler to form a via in the via portion and a second conductive line in the trench portion, the second conductive line extending along a second direction and the via contacting the first conductive line in the via portion; forming a cap layer over the conductive filling; A method for forming an electronic device comprising:
15. The method of claim 14 , wherein the liner comprises a ruthenium layer in contact with the barrier layer and a cobalt layer on an opposite side of the ruthenium layer from the barrier layer.
16. The method of claim 15, wherein the ruthenium layer has a thickness in the range of 2.5 Å to 25 Å and the cobalt layer has a thickness in the range of 2.5 Å to 25 Å.
17. The method of claim 15, wherein the ruthenium layer and the cobalt layer have a thickness ratio in the range of 0.95:1 to 1:0.
95.
18. The method of claim 15 further comprising forming a cap layer over the conductive filling.
19. 20. The method of claim 18, wherein the cap layer comprises a ruthenium layer in contact with the conductive filling and a cobalt layer on an opposite side of the ruthenium layer from the conductive filling.
20. 20. The method of claim 19, wherein the ruthenium layer of the capping layer has a thickness in the range of 2.5 Å to 25 Å and the cobalt layer of the capping layer has a thickness in the range of 2.5 Å to 25 Å.
Citation Information
Patent Citations
Connection structure between wires and method of forming the same
JP2003249547A
Doped selective metal cap improves copper electromigration with ruthenium liner.
JP2019531604A
Enhanced cobalt agglomeration resistance and gap-filling action by ruthenium doping
JP2020506540A
Method of forming barrier free contact for metal interconnects
US20200144107A1