Method for deposition of depth-varying refractive index film

By varying material concentrations in optical device films using controlled power levels or gas flow rates, the method addresses discontinuous refractive index profiles, enhancing light transmission and reflectance in optical devices.

JP2024133461AActive Publication Date: 2024-10-02APPLIED MATERIALS INC
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2024089203
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2020-07-22
Filing Date
2024-05-31
Publication Date
2024-10-02
Estimated Expiration
2041-07-08

AI Technical Summary

Technical Problem

Conventional optical device films exhibit discontinuous refractive index profiles due to multiple layers, leading to optical aberrations and reduced light transmission and reflectance.

Method used

A method for forming optical device films with a continuous refractive index profile by varying the concentration of materials such as TiO2 and SiO2 across zones, controlled through power levels or gas flow rates in PVD or CVD processes.

Benefits of technology

The method allows for continuous adjustment of refractive index, reducing optical aberrations and improving light transmission and reflectance in optical devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024133461000001_ABST
    Figure 2024133461000001_ABST
Patent Text Reader

Abstract

To provide an optical device film and an improved method of forming an optical device film.SOLUTION: Embodiments of the present disclosure relate to optical device films and methods of forming optical device films. Specifically, embodiments described herein provide an optical device film having a constant oxygen concentration, a first concentration profile of the first material, and a second concentration profile of the second material. The first material, described and referenced to herein, has a first refractive index of about 2.0 or greater and the second material has a second refractive index less than 2.0.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE

[0001] Embodiments of the present disclosure relate to optical device films and methods of forming optical device films. [Background technology]

[0002]

[0002] Optical devices such as waveguides, planar optical devices, metasurfaces, color filters, and anti-reflective coatings are designed to exhibit the properties of high refractive index and low absorption loss. Metal-oxide-containing materials, such as titanium dioxide (TiO2), have high refractive index and low absorption loss, which allows for efficient large-scale manufacturing of optical devices.

[0003]

[0003] Graded index optical film is used to control light interacting with a surface or within the film. In conventional optical film, it is difficult to continuously tune the refractive index over a large range by changing the deposition conditions of a single material, and it is necessary to use multiple materials to approximate a continuous profile with a step profile.

[0004]

[0004] Conventional optical device films typically include multiple distinct layers of materials with different refractive index characteristics, such as step index waveguides. For example, an optical device film may be formed with a TiO2 layer deposited on the surface of an optical device substrate, with a silicon dioxide (SiO2) layer formed above the TiO2 layer. Here, the TiO2 layer has a refractive index of about 2.4 (n=2.4) and the SiO2 layer has a refractive index of about 1.5 (n=1.5). The difference in refractive index between the TiO2 layer and the SiO2 layer is approximately 0.9, which represents an abrupt change for light passing between the layers. This abrupt change can be characterized as a discontinuous step between the optical materials, which reduces desired optical device properties, such as optical reflectance and optical transmittance, for light passing between the different layers. Conventional optical device films often include multiple distinct layers of two or more materials to reduce the change in refractive index between the layers and improve the desired optical properties between the layers. However, the refractive index of these conventional optical device films is discontinuous, and optical aberrations may exist in such conventional optical device films.

[0005]

[0005] Therefore, there is a need in the art for improved optical device films and methods of forming optical device films. Summary of the Invention

[0006] In one embodiment, an optical device film is provided. The optical device film includes a thickness divided into a series of zones from a first surface corresponding to 0% of the thickness to a second surface corresponding to 100% of the thickness. Each zone in the series of zones has a zone thickness. The optical device film has an oxygen concentration or a nitrogen concentration in each zone in the series of zones. The optical device film also includes a first material having a first refractive index greater than or equal to about 2.0 and a second material having a second refractive index less than about 2.0. The first material has a first concentration profile throughout the series of zones. The second material has a second concentration profile throughout the series of zones. The second concentration profile is different from the first concentration profile.

[0007] In another embodiment, a method is provided. The method includes disposing an optical device substrate on a substrate support. The substrate support is disposed within a chamber. The chamber includes a first target and a second target disposed within the chamber. The first target includes a first material and the second target includes a second material. An optical device film is deposited on the optical device substrate by depositing the first material with a first concentration profile and depositing the second material with a second concentration profile. Depositing the first material includes providing a first power level to the first target. The first concentration profile of the first material is controlled by at least one of increasing or decreasing the first power level provided to the first target. Depositing the second material includes providing a second power level to the second target. The second concentration profile of the second material is controlled by at least one of increasing or decreasing the second power level provided to the second target.

[0008] In another embodiment, a method is provided. The method includes disposing an optical device substrate on a substrate support. The substrate support is disposed within a chamber. The chamber includes a first target and a gas source. The first target includes a first material. The gas source is operable to flow a precursor gas including a second material. An optical device film is deposited on the optical device substrate by depositing the first material with a first concentration profile and depositing the second material with a second concentration profile. Depositing the first material includes providing a first power level to the first target. The first concentration profile of the first material is controlled by at least one of increasing or decreasing the first power level provided to the first target. Depositing the second material includes providing a precursor gas at a flow rate. The second concentration profile of the second material is controlled by at least one of increasing or decreasing the flow rate of the precursor.

[0009] In yet another embodiment, a method is provided that includes placing an optical device substrate in a chamber, flowing a first gas containing a first material into the chamber at a first flow rate, and flowing a second gas containing a second material into the chamber at a second flow rate. A first concentration profile of the first material in the deposited optical device film is controlled by at least one of increasing or decreasing the first flow rate during the flowing of the first gas. A second concentration profile of the second material in the deposited optical device film is controlled by at least one of increasing or decreasing the second flow rate during the flowing of the second gas.

[0010]

[0010] In order that the features of the present disclosure described above may be understood in detail, a more detailed description of the present disclosure briefly summarized above may be obtained by reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings show only exemplary embodiments, and therefore should not be considered as limiting the scope of the present disclosure, which may admit of other equally effective embodiments. [Brief description of the drawings]

[0011] [Figure 1] 1 is a schematic cross-sectional view of an optical device film according to an embodiment described herein. [Figure 2A-2B]

[0012] 1 is a schematic cross-sectional view of an optical device formed from an optical device film. [Diagram 3]

[0013] 1 is a schematic cross-sectional view of a physical vapor deposition (PVD) chamber according to an embodiment described herein. [Figure 4]

[0014] 1 is a schematic cross-sectional view of a chemical vapor deposition (CVD) chamber according to an embodiment described herein. [Diagram 5]

[0015] FIG. 2 is a flow diagram of a method for manufacturing an optical device film according to embodiments described herein. [Figure 6] FIG. 2 is a flow diagram of a method for manufacturing an optical device film according to embodiments described herein. [Figure 7] FIG. 2 is a flow diagram of a method for manufacturing an optical device film according to embodiments described herein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012]

[0016] For ease of understanding, the same reference numerals have been used, where possible, to designate identical elements that are common to several figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further description.

[0013]

[0017] SUMMARY OF THE DISCLOSURE Embodiments of the present disclosure relate to optical device films and methods of forming optical device films. In particular, embodiments described herein provide an optical device film having an oxygen or nitrogen concentration, a first concentration profile of a first material, and a second concentration profile of a second material. The optical device film includes a first material at a first concentration and a second material at a second concentration throughout the thickness of the film. The first material described and referenced herein has a first refractive index of about 2.0 or greater. The second material described and referenced herein has a second refractive index of less than 2.0. The first material includes, but is not limited to, oxides or nitrides of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb). The second material includes, but is not limited to, oxides or nitrides of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg).

[0014]

[0018] 1 is a schematic cross-sectional view of an optical device film 100. The optical device film 100 is disposed on an optical device substrate 101 according to embodiments described herein. The optical device substrate 101 is any suitable optical device substrate on which an optical device may be formed. In one embodiment, the optical device substrate 101 is a silicon (Si)-containing optical device substrate. In one embodiment, the optical device substrate 101 is a silicon oxide-based glass or a metal oxide-based glass. In one embodiment, the optical device substrate 101 includes, but is not limited to, silicon (Si), silicon nitride (SiN), silicon dioxide (SiO2), fused silica, quartz, silicon carbide (SiC), germanium (Ge), silicon germanium (SiGe), indium phosphide (InP), gallium arsenide (GaAs), gallium oxide (GaO), diamond, lithium niobate (LiNbO3), gallium nitride (GaN), sapphire, tantalum oxide (Ta2O5), titanium dioxide (TiO2), or combinations thereof. The optical device substrate 102 may include an optically transparent perovskite material. In another embodiment, the optical device substrate 101 is a layered optical device substrate, such as, for example, a thin glass bonded to a silicon carrier. A layered optical device substrate may be a substrate on which an optical device stack (e.g., patterned optical device films for gratings, waveguides, optoelectronics, monolithically integrated CMOS-optical devices, heterogeneously integrated CMOS-optical devices) is disposed. In yet another embodiment, the optical device substrate 101 is a laminated substrate including multiple layers of bonding glass.

[0015]

[0019] The optical device film 100 has a first surface 102, a second surface 110, and a thickness 106. The thickness 106 of the optical device film 100 is divided into zones 105 measured from the first surface 102 corresponding to 0% of the thickness 106 to the second surface 110 corresponding to 100% of the thickness 106. In one embodiment, which can be combined with other embodiments described herein, the thickness 106 has a constant or substantially constant oxygen or nitrogen concentration throughout the range of the zones 105 of the optical device film 100. In one embodiment, the difference in oxygen or nitrogen concentration between each zone 104 within the range of the zones 105 is 10% (e.g., ±5%) atomic percentage. In one embodiment, the oxygen concentration of the optical device film 100 of the first material of TiO2 and the second material of SiO2 is about 66.67 atomic percent ±10%. Each zone 104 has a zone thickness of about 0.001% to about 50% of the thickness 106. Each zone 104 includes a first material at a first concentration and a second material at a second concentration. The first material described and referenced herein has a first refractive index of about 2.0 or greater. The second material described and referenced herein has a second refractive index of less than 2.0. The first material and the second material may be metal-containing or semiconductor materials. For example, the first material may include, but is not limited to, oxides or nitrides of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb). For example, the second material may include, but is not limited to, oxides or nitrides of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg).

[0016]

[0020] Incorporating successively different concentrations of the first and second materials during deposition allows for modification of the optical properties, i.e., refractive index, of the optical device film 100. In one embodiment, each zone 104 has a zone thickness of about 0.001% to about 50% of the thickness 106. The first concentration of the first material through the range of the zone 105 of the thickness 106 has a first concentration profile, and the second concentration of the second material through the range of the zone 105 of the thickness 106 has a second concentration profile. In one embodiment, the first concentration has a maximum concentration in a first zone 108 of the range of the zone 105 adjacent the first surface 102 and a minimum concentration in a final zone 109 of the range of the zone 105 adjacent the second surface 110. The second concentration has a minimum concentration in the first zone 108 and a maximum concentration in the final zone 109 of the range of the zone 105. In an embodiment where the oxygen concentration (e.g., of a TiO2 first material and a SiO2 second material) is about 66.67 atomic percent ±10%, the minimum concentration is about 0 atomic percent and the maximum concentration is about 33.3 atomic percent. In an embodiment, the first concentration of each zone 104 deposited immediately above the preceding zone is less than or equal to the first concentration of the preceding zone and the second concentration of each zone 104 deposited immediately above the preceding zone is greater than or equal to the second concentration of the preceding zone.

[0017]

[0021] In another embodiment, the first concentration has a minimum concentration in the initial zone 108 and a maximum concentration in the final zone 109. The second concentration has a maximum concentration in the initial zone 108 and a minimum concentration in the final zone 109. In an embodiment, the first concentration of each zone 104 deposited immediately above a preceding zone is greater than or equal to the first concentration of the preceding zone, and the second concentration of each zone 104 deposited immediately above a preceding zone is less than or equal to the second concentration of the preceding zone.

[0018]

[0022] In another embodiment, the first and second concentration profiles have sinusoidal profiles. In one embodiment where the first and second concentration profiles have sinusoidal profiles, the first concentration has a maximum concentration in the initial zone 108 that decreases to a minimum concentration at the midpoint of the range of the zone 105 and increases to a maximum concentration at the final zone 109. The second concentration has a minimum concentration in the initial zone 108 that increases to a maximum concentration at the midpoint of the range of the zone 105 and decreases to a minimum concentration at the final zone 109. In another embodiment where the first and second concentration profiles have sinusoidal profiles, the first concentration has a minimum concentration in the initial zone 108 that increases to a maximum concentration at the midpoint of the range of the zone 105 and decreases to a minimum concentration at the final zone 109. The second concentration has a maximum concentration in the initial zone 108 that decreases to a minimum concentration at the midpoint of the range of the zone 105 and increases to a maximum concentration at the final zone 109.

[0019]

[0023] In yet another embodiment, the first concentration profile of the first material and the second concentration profile of the second material of the optical device film 100 are controlled by the embodiments of the methods 500, 600, 700 to obtain any desired profile. In the embodiment of the method 500 of forming the optical device film 100 described herein, the first concentration and the second concentration can be controlled by at least one of increasing or decreasing a first power level provided to a first target of the first material or increasing or decreasing a second power level provided to a second target of the second material. In the embodiment of the method 600 of forming the optical device film 100 described herein, the first concentration and the second concentration can be controlled by at least one of increasing or decreasing a first power level provided to a first target of the first material and increasing or decreasing a flow rate of a precursor gas including the second material. In the embodiments of the method 700 for forming the optical device film 100 described herein, the first concentration and the second concentration can be controlled by at least one of increasing or decreasing a first flow rate of a first gas containing the first material and increasing or decreasing a second flow rate of a second gas containing the second material. Thus, the optical device film 100 having oxygen or nitrogen concentrations can include any desired profile of the first and second materials.

[0020]

[0024] The optical device film 100 of the methods 500, 600, 700 described herein formed from a first material and a second material may include one or more of an oxide or nitride of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb), and one or more of an oxide or nitride of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg).

[0021]

[0025] 2A and 2B are schematic cross-sectional views of optical devices 200a, 200b formed from the optical device film 100. The optical devices 200a, 200b include optical device structures 202a, 202b disposed on an optical device substrate 101. The optical device structures 202a, 202b include submicron critical dimensions, e.g., nano-sized dimensions, corresponding to the widths 203 of the optical device structures 202a, 202b. The optical device structure 202a can be a binary structure in which the top surface 224 of the optical device structure 202a is parallel to the surface 102 of the optical device substrate 101. The first sidewall 225 and the second sidewall 226 are parallel to the third sidewall 227 and the fourth sidewall 228. The sidewalls 225, 226, 227, and 228 are oriented in a direction perpendicular to the major axis of the optical device substrate 101. The optical device structure 202b may be an angled structure having sidewalls 225, 226, 227, and 228 that are angled relative to the surface 102 of the optical device substrate 101. The optical devices 200a, 200b are formed from an optical device film 100 having a first concentration profile of a first material, a second concentration profile of a second material, and a concentration of oxygen or nitrogen throughout the thickness 106 of the optical device film 100.

[0022]

[0026] 3 is a schematic cross-sectional view of a PVD chamber 300. The PVD chamber 300 may be used for the methods 500 and 600 described herein. It should be understood that the PVD chamber 300 described below is an exemplary PVD chamber, and that other PVD chambers, including PVD chambers from other manufacturers, may be used or modified to accomplish aspects of the present disclosure.

[0023]

[0027] The PVD chamber 300 includes multiple cathodes 302, 303 with corresponding multiple targets (at least one first target 304 and at least one second target 306) mounted (e.g., via a chamber body adapter 308) to a chamber body 310. The first target 304 includes at least one first material as described herein, and the second target 306 includes at least one second material as described herein. Each cathode (e.g., the first target 304 and the second target 306) may be coupled to a DC power source 312 or an RF power source 314, and a matching network 316.

[0024]

[0028] The PVD chamber 300 is configured to include a substrate support 332 having a support surface 334 for supporting the optical device substrate 101. The PVD chamber 300 includes an opening 350 (e.g., a slit valve) through which an end effector (not shown) passes to place the optical device substrate 101 onto lift pins (not shown) for lowering the optical device substrate 101 onto the support surface 334.

[0025]

[0029] The PVD chamber 300 includes a sputter gas source 361 operable to supply a sputter gas, such as argon (Ar), to the processing space 305. A gas flow controller 362 is disposed between the sputter gas source 361 and the processing space 305 to control the flow of the sputter gas from the sputter gas source 361 to the processing space 305. The PVD chamber 300 includes a reactive gas source 363 operable to supply a reactive gas, such as an oxygen-containing gas or a nitrogen-containing gas, to the processing space 305. A gas flow controller 364 is disposed between the reactive gas source 363 and the processing space 305 to control the flow of the reactive gas from the reactive gas source 363 to the processing space 305. The PVD chamber 300 may include a precursor gas source 370 operable to supply a precursor gas to the processing space 305. A gas flow controller 371 is disposed between the precursor gas source 370 and the processing space 305 to control the flow of the precursor gas from the precursor gas source 370 to the processing space 305.

[0026]

[0030] In the embodiment shown in FIG. 3, the substrate support 332 includes an RF bias power supply 338 coupled to a bias electrode 340 disposed within the substrate support 332 via a matching network 342. The substrate support 332 includes a mechanism (not shown) for holding the optical device substrate 101 on a support surface 334 of the substrate support 332, such as an electrostatic chuck, a vacuum chuck, a substrate holding clamp, or the like. The substrate support 332 includes a cooling conduit 365 disposed within the substrate support 332 that controllably cools the substrate support 332 and the optical device substrate 101 positioned thereon to a predetermined temperature, for example, between about −20° C. and 300° C. The cooling conduit 365 is coupled to a cooling fluid source 368 that provides a cooling fluid (not shown). The substrate support 332 also includes a heater 367 embedded therein. A heater 367, such as a resistive element, disposed within the substrate support 332 is coupled to an optional heater power supply 366 to controllably heat the substrate support 332 and the optical device substrate 101 positioned thereon to a predetermined temperature, for example between approximately -20°C and 300°C.

[0027]

[0031] Although FIG. 3 shows one first target 304 and one second target 306, the PVD chamber 300 may include one or more first targets 304 and / or one or more second targets 306. For example, three to five targets selected from at least one of the first targets 304 or the second targets 306 may be included in the PVD chamber 300. Each first target 304 is operable to deposit a different material. For example, three to five second targets 306 may be included in the PVD chamber 400. Each optical material target 306 is operable to deposit a different material. In an embodiment having one or more first targets 304 and one or more second targets 306, each first target 304 is operable to deposit a different first material and / or each second target 306 is operable to deposit a different second material.

[0028]

[0032] 4 is a schematic cross-sectional view of a CVD chamber 400 that may be used in the method 700 described herein. It should be understood that the CVD chamber 400 described herein is an exemplary CVD chamber, and that other CVD chambers, including CVD chambers from other manufacturers, may be used or modified to accomplish aspects of the present disclosure.

[0029]

[0033] The CVD chamber 400 has a chamber body 402 that includes a processing space 404 in which a substrate support 406 is disposed to support the optical device substrate 101 thereon. The substrate support 406 includes heating / cooling conduits 410 and a mechanism for holding the optical device substrate 101 on a support surface 407 of the substrate support 406, such as an electrostatic chuck, a vacuum chuck, a substrate holding clamp, or the like. The substrate support 406 is coupled and movably positioned within the processing space 404 by a stem 408 that is coupled to a lift system (not shown) that moves the substrate support 406 between a raised processing position and a lowered position that facilitates transfer of the optical device substrate 101 to and from the CVD chamber 400 through an opening 412.

[0030]

[0034] The CVD chamber 400 includes a flow controller 418A disposed between the first gas source 416A and the chamber body 402 for controlling a first flow rate of a first process gas of a first material from the first gas source 416A to the showerhead 414. The CVD chamber 400 includes a flow controller 418B disposed between the second gas source 416B and the chamber body 402 for controlling a second flow rate of a second process gas of a second material from the second gas source 416B to the showerhead 414. The showerhead 414 is connected to an RF power supply 422 by an RF feed 424 for generating a plasma in the processing space 404 from the first process gas and / or the second process gas. The RF power supply 422 provides RF energy to the showerhead 414 to facilitate the generation of plasma between the showerhead 414 and the substrate support 406. A vacuum pump 420 is coupled to the chamber body 402 for controlling the pressure in the processing space 404. A controller 428 is coupled to the CVD chamber 400 and configured to control aspects of the chamber 400 during processing.

[0031]

[0035] 4 shows a first gas source 416A and a second gas source 416B, the CVD chamber 400 may include one or more first gas sources 416A and / or one or more second gas sources 416B. For example, 3-5 gas sources selected from at least one of the first gas source 416A or the second gas source 416B may be included in the CVD chamber 400. In an embodiment having one or more first gas sources 416A and one or more second gas sources 416B, each first gas source 416A is operable to deposit a different first material and / or each second gas source 416B is operable to deposit a different second material.

[0032]

[0036] Figure 5 is a flow diagram of a method 500 for forming an optical device film 100, which may be utilized for subsequent processing to form devices 200a, 200b. For ease of explanation, Figure 5 will be described with reference to the PVD chamber 300 of Figure 3. However, it should be noted that PVD chambers other than the PVD chamber 300 of Figure 3 may be utilized in conjunction with method 500.

[0033]

[0037] In operation 501, the optical device substrate 101 is placed on a substrate support in a PVD chamber 300. In operation 502, a first zone 108 of the zone 105 of the optical device film 100 is deposited. A first target 304 having a first material is set to a first power level and a second target 306 having a second material is set to a second power level. In one embodiment, the first material of the first target 304 and / or the second material of the second target 306 comprises an oxygen-containing material or a nitrogen-containing material. The first material described and referenced herein has a first refractive index of about 2.0 or greater. The second material described and referenced herein has a second refractive index of less than 2.0. The first material includes, but is not limited to, oxides or nitrides of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb). The second material includes, but is not limited to, oxides or nitrides of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg). In another embodiment, an oxygen-containing gas or a nitrogen-containing gas is supplied to the process space 305. In an embodiment, the deposited first material and the second material react with the oxygen-containing gas or the nitrogen-containing gas to form the first zone 108 of the optical device film 100. In another embodiment, the optical device substrate 101 is maintained at a predetermined temperature between -20°C and 300°C.

[0034]

[0038] In one embodiment, the first concentration of the first material has a maximum concentration in the first zone 108 of the range of zones 105 by applying a first power level to the first target 304 at an upper limit of the first power level. An upper limit of the first power level corresponding to the highest power level is provided to the first target 304 during the method 500. In an embodiment, the second concentration of the second material has a minimum concentration in the first zone 108 by applying no second power level or applying a second power level to the second target 306 at a lower limit of the second power level. A lower limit of the second power level corresponding to a lowest power level is provided to the second target 306 during the method 500. In another embodiment, the first concentration of the first material has a minimum concentration in the first zone 108 of the range of zones 105 by applying no first power level or applying a first power level to the first target 304 at a lower limit of the first power level. A lower limit of the first power level corresponding to a lowest power level is provided to the first target 304 during the method 500. In an embodiment, the second concentration of the second material has a maximum concentration in the first zone 108 by applying a second power level to the second target 306 at an upper limit of the second power level. An upper limit of the second power level corresponding to a highest power level is provided to the second target 306 during the method 500. In yet another embodiment, the first concentration and the second concentration may be controlled by at least one of setting the first power level provided to the first target 304 of the first material and setting the second power provided to the second target 306 of the second material to different power levels between the upper and lower limits of the first power level and the second power level.

[0035]

[0039] In operation 503, subsequent zones of the optical device film 100 are deposited until the final zone 109 of the extent of the zone 105 is deposited. Deposition of the subsequent zones includes at least one of setting a first power level provided to the first target 304 of the first material and setting a second power level provided to the second target 306 of the second material to different power levels to form the optical device film 100. The optical device film 100 includes an oxygen concentration or a nitrogen concentration, a first concentration profile of the first material, and a second concentration profile of the second material. In an embodiment, which can be combined with other embodiments described herein, the thickness 106 has a constant or substantially constant oxygen or nitrogen concentration throughout the extent of the zone 105 of the optical device film 100.

[0036]

[0040] Figure 6 is a flow diagram of a method 600 for forming an optical device film 100, which may be utilized for subsequent processing to form devices 200a, 200b. For ease of explanation, Figure 6 will be described with reference to the PVD chamber 300 of Figure 3. However, it should be noted that PVD chambers other than the PVD chamber 300 of Figure 3 may be utilized in conjunction with method 600.

[0037]

[0041] In operation 601, the optical device substrate 101 is placed on a substrate support in the PVD chamber 300. In operation 602, a first zone 108 of the zone 105 of the optical device substrate 101 is deposited. A first target 304 having a first material is set at a first power level and a precursor gas including a second material is provided at a precursor flow rate. In one embodiment, the first material of the first target 304 and / or the precursor gas of the second material includes an oxygen-containing material or a nitrogen-containing material. The first material described and referenced herein has a first refractive index of about 2.0 or greater. The second material described and referenced herein has a second refractive index of less than 2.0. The first material includes, but is not limited to, oxides or nitrides of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb). The second material includes, but is not limited to, oxides or nitrides of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg). In another embodiment, an oxygen-containing gas is supplied to the processing space 305. In another embodiment, an oxygen-containing gas or a nitrogen-containing gas is supplied to the processing space 305. In an embodiment, the deposited first material and the second material react with the oxygen-containing gas or the nitrogen-containing gas to form the first zone 108 of the optical device film 100. In another embodiment, the optical device substrate 101 is maintained at a predetermined temperature between about -20°C and 300°C.

[0038]

[0042] In one embodiment, the first concentration of the first material has a maximum concentration in the first zone 108 of the range of zones 105 by applying a first power level to the first target 304 at an upper limit of the first power level. An upper limit of the first power level corresponding to the highest power level is provided to the first target 304 during the method 600. In an embodiment, the second concentration of the second material has a minimum concentration in the first zone 108 by not flowing a precursor gas or by flowing a precursor gas at a minimum flow rate during the method 600. In another embodiment, the first concentration of the first material has a minimum concentration in the first zone 108 of the range of zones 105 by not applying a first power level or by applying a first power level to the first target 304 at a lower limit of the first power level. A lower limit of the first power level corresponding to the lowest power level is provided to the first target 304 during the method 600. In an embodiment, the second concentration of the second material has a maximum concentration in the first zone 108 during method 600 by flowing the precursor gas at a maximum flow rate during method 500. In yet another embodiment, the first concentration and the second concentration may be controlled during method 600 by varying at least one of a first power level delivered to the first target 304 of the first material and varying a flow rate of the precursor gas.

[0039]

[0043] In operation 603, subsequent zones of the optical device film 100 are deposited until a final zone 109 of the extent of zone 105 is deposited. Deposition of the subsequent zones includes increasing or decreasing a first power level provided to a first target of a first material and / or increasing or decreasing a flow rate of a precursor gas including a second material to form an optical device film 100 having an oxygen or nitrogen concentration, a first concentration profile of the first material, and a second concentration profile of the second material. In an embodiment, which may be combined with other embodiments described herein, the thickness 106 has a constant or substantially constant oxygen or nitrogen concentration throughout the extent of zone 105 of the optical device film 100.

[0040]

[0044] Figure 7 is a flow diagram of a method 700 for forming an optical device film 100, which may be used for subsequent processing to form devices 200a, 200b. For ease of explanation, Figure 7 will be described with reference to the CVD chamber 400 of Figure 4. However, it should be noted that CVD chambers other than the CVD chamber 400 of Figure 4 may be used in conjunction with method 700.

[0041]

[0045] In operation 701, the optical device substrate 101 is placed on a substrate support in the CVD chamber 400. In operation 702, a first zone 108 of the zone 105 of the optical device substrate 101 is deposited. The first gas has a first gas flow rate and the second gas has a second gas flow rate. The first material of the first gas described and referenced herein has a first refractive index of about 2.0 or greater. The second material of the second gas described and referenced herein has a second refractive index of less than 2.0. In one embodiment, the precursor gas of the first material and / or the second material of the first target 304 includes an oxygen-containing material or a nitrogen-containing material. In one embodiment, the optical device substrate 101 is maintained at a predetermined temperature between about -20°C and 300°C.

[0042]

[0046] In one embodiment, the first concentration of the first material has a maximum concentration in the first zone 108 of the range of zones 105 by flowing the first gas at a maximum flow rate during the method 700. In an embodiment, the second concentration of the second material has a minimum concentration in the first zone 108 by not flowing the second gas or by flowing the second gas at a minimum flow rate during the method 700. In another embodiment, the first concentration of the first material has a minimum concentration in the first zone 108 of the range of zones 105 by not flowing the first gas or by flowing the first gas at a minimum flow rate during the method 700. In an embodiment, the second concentration of the second material has a maximum concentration in the first zone 108 by flowing the second gas at a maximum flow rate during the method 700. In yet another embodiment, the first concentration and the second concentration can be controlled by at least one of varying the first gas flow rate and varying the second gas flow rate during the method 700.

[0043]

[0047] In operation 703, subsequent zones of the optical device film 100 are deposited until a final zone 109 of the extent of zone 105 is deposited. Deposition of the subsequent zones includes at least one of increasing or decreasing a first flow rate of a first gas containing a first material and increasing or decreasing a second flow rate of a precursor gas containing a second material to form an optical device film 100 having an oxygen concentration or nitrogen concentration, a first concentration profile of the first material, and a second concentration profile of the second material. In an embodiment, which can be combined with other embodiments described herein, the thickness 106 has a constant or substantially constant oxygen or nitrogen concentration throughout the extent of zone 105 of the optical device film 100.

[0044]

[0048] In summary, an optical device film having an oxygen or nitrogen concentration, a first concentration profile of a first material, and a second concentration profile of a second material, and a method for forming the optical device film are described herein. By incorporating different concentrations of the first and second materials successively during deposition, the optical properties of the optical device film, i.e., the refractive index, can be modified. In one embodiment, the method includes controlling the first and second concentration profiles by at least one of increasing or decreasing a first power level provided to a first target of the first material, or increasing or decreasing a second power level provided to a second target of the second material. In another embodiment, the method includes controlling the first and second concentration profiles by at least one of increasing or decreasing a first power level provided to a first target of the first material, and increasing or decreasing a flow rate of a precursor gas including the second material. In yet another embodiment, the method includes controlling the first and second concentration profiles by at least one of increasing or decreasing a first flow rate of a first gas including the first material and increasing or decreasing a second flow rate of a second gas including the second material.

[0045]

[0049] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, the scope of which is determined by the claims that follow.

Claims

1. An optical device film, a thickness, the thickness being divided into a series of zones from a first surface substantially corresponding to 0% of the thickness to a second surface substantially corresponding to 100% of the thickness, each zone in the series of zones having a zone thickness; an oxygen or nitrogen concentration for each zone of the series of zones of the optical device film, the oxygen or nitrogen concentration being maintained throughout all of the zones of the series of zones; a first material having a first refractive index of about 2.0 or greater, the first material having a first concentration profile across the series of zones; a second material having a second refractive index less than 2.0, the second material having a second concentration profile across the series of zones, the second concentration profile being different from the first concentration profile; An optical device film comprising:

2. The optical device film of claim 1 , wherein the zone thickness is from about 0.001% to about 50% of the thickness.

3. 10. The optical device film of claim 1, wherein the first material comprises an oxide or nitride of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb).

4. 2. The optical device film of claim 1, wherein the second material comprises an oxide or nitride of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg).

5. 2. The optical device film of claim 1, wherein the oxygen concentration is about 66.67 atomic percent, ±10%.

6. a first zone of the series of zones adjacent the first surface, a maximum concentration of the first material; and a minimum concentration of 0 atomic percent of said second material; and the final zone in the series of zones adjacent the second surface comprises: a minimum concentration of 0 atomic percent of the first material; a maximum concentration of the second material; and The optical device film of claim 1 .

7. a first concentration of each zone located immediately above a preceding zone in the first concentration profile is less than or equal to the first concentration of the preceding zone; and a second concentration of each zone located immediately above the preceding zone in the second concentration profile is equal to or greater than the second concentration of the preceding zone; The optical device film of claim 6.

8. the first concentration profile has the maximum concentration at the first zone of the series of zones, the first concentration profile has the minimum concentration at a midpoint of the series of zones, the first concentration profile has the maximum concentration at the last zone of the series of zones, and the second concentration profile has the minimum concentration at the first zone of the series of zones, the second concentration profile has the maximum concentration at the midpoint of the series of zones, and the second concentration profile has the minimum concentration at the last zone of the series of zones. The optical device film of claim 6.

9. a first zone of the series of zones adjacent the first surface, a maximum concentration of the second material; and a minimum concentration of 0 atomic percent of said first material; and the final zone in the series of zones adjacent the second surface comprises: a minimum concentration of 0 atomic percent of said second material; a maximum concentration of the first material; and The optical device film of claim 1 .

10. a first concentration of each zone located immediately above a preceding zone in the first concentration profile is equal to or greater than the first concentration of the preceding zone; and a second concentration of each zone located immediately above the preceding zone in the second concentration profile is less than or equal to the second concentration of the preceding zone; 10. The optical device film of claim 9.

11. the first concentration profile has the minimum concentration at the first zone of the series of zones, the first concentration profile has the maximum concentration at a midpoint of the series of zones, the first concentration profile has the minimum concentration at the last zone of the series of zones, and the second concentration profile has the maximum concentration at the first zone of the series of zones, the second concentration profile has the minimum concentration at the midpoint of the series of zones, and the second concentration profile has the maximum concentration at the last zone of the series of zones.

10. The optical device film of claim 9.

12. The optical device film of claim 1 having a plurality of optical device structures disposed therein.

13. The optical device film of claim 12 , wherein the plurality of optical device structures are tilted relative to the first surface of the optical device film.

14. 13. The optical device film of claim 12, wherein the difference in the oxygen concentration or the nitrogen concentration between each zone in the series of zones is an atomic percentage of 10%.

15. 1. A method comprising:

2. Disposing an optical device substrate on a substrate support, the substrate support being disposed within a chamber, the chamber comprising: a first target disposed within the chamber, the first target including a first material; and a second target disposed within the chamber, the second target comprising a second material; disposing an optical device substrate; depositing an optical device film onto the optical device substrate; depositing the first material having a first concentration profile, the depositing of the first material comprising providing a first power level to the first target, the first concentration profile of the first material being controlled by at least one of increasing or decreasing the first power level provided to the first target, and a first concentration of the first material being greatest in a first zone of a series of zones of the optical device film; depositing the second material having a second concentration profile, the depositing of the second material comprising providing a second power level to the second target, the second concentration profile of the second material being controlled by at least one of increasing or decreasing the second power level provided to the second target, and a second concentration of the second material being minimum in a first zone of the series of zones of the optical device film; and Maintaining oxygen or nitrogen concentrations throughout said series of zones. depositing an optical device film, A method comprising:

16. 16. The method of claim 15, wherein the first material comprises an oxide or nitride of titanium (Ti), tantalum (Ta), zirconium (Zr), indium (In), or niobium (Nb).

17. 16. The method of claim 15, wherein the second material comprises an oxide or nitride of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg).

18. 1. A method comprising:

2. Disposing an optical device substrate on a substrate support, the substrate support being disposed within a chamber, the chamber comprising: a first target disposed within the chamber, the first target including a first material; and a gas source operable to flow a precursor gas comprising the second material; disposing an optical device substrate; depositing an optical device film onto the optical device substrate; depositing the first material having a first concentration profile, the depositing of the first material comprising providing a first power level to the first target, the first concentration profile of the first material being controlled by at least one of increasing or decreasing the first power level provided to the first target, and a first concentration of the first material being greatest in a first zone of a series of zones of the optical device film; depositing the second material having a second concentration profile, the depositing of the second material comprising providing a precursor gas at a flow rate, the second concentration profile of the second material being controlled by at least one of increasing or decreasing a flow rate of the precursor gas, and a second concentration of the second material being minimum in a first zone of the series of zones of the optical device film; and Maintaining oxygen or nitrogen concentrations throughout said series of zones. depositing an optical device film, A method comprising:

19. 20. The method of claim 18, wherein the second material comprises an oxide or nitride of silicon (Si), aluminum (Al), hafnium (Hf), scandium (Sc), tin (Sn), yttrium (Y), praseodymium (Pr), or magnesium (Mg).

20. 1. A method comprising: placing an optical device substrate within a chamber; flowing a first gas including a first material into the chamber at a first flow rate, wherein a first concentration profile of the first material in a deposited optical device film is controlled by at least one of increasing or decreasing the first flow rate during the flowing of the first gas, and a first concentration of the first gas is greatest in a first zone of a series of zones in the optical device film; flowing a second gas comprising a second material into the chamber at a second flow rate, wherein a second concentration profile of the second material in the deposited optical device film is controlled by at least one of increasing or decreasing the second flow rate during the flowing of the second gas, and a second concentration of the second gas is minimum in a first zone of the series of zones in the optical device film; maintaining an oxygen concentration or a nitrogen concentration throughout said series of zones; A method comprising:

Citation Information

Patent Citations

  • Method for depositing film on substrate, and article obtained by the method

    JP2001192823A

  • Thin-film-forming method

    JP2006022389A

  • Optical wavelength plate and manufacturing method of same

    JP2008164680A

  • Method of manufacturing multilayer film

    JP2012092410A

  • Nd filter and optical device

    JP2013015827A