Electronic structure, method for manufacturing electronic structure, and method for manufacturing electronic device

The method addresses the challenge of transferring functional parts by using sacrificial layers and a covering layer to facilitate easy peeling and transfer, enhancing process efficiency and accuracy.

JP2024139226APending Publication Date: 2024-10-09OKI ELECTRIC INDUSTRY CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023050073
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09

AI Technical Summary

Technical Problem

Conventional methods for transferring functional parts from a substrate to a transfer substrate involve peeling off the support layer, which can lead to broken pieces adhering to the transfer substrate, causing poor bonding and complicating the transfer process.

Method used

A method involving a laminated substrate with sacrificial layers and a covering layer is used to facilitate the transfer of functional parts by removing the sacrificial layers, ensuring the functional part is held with a weak adhesive force, allowing easy peeling and transfer while maintaining positional accuracy.

Benefits of technology

The method enables efficient and accurate transfer of functional parts by minimizing adhesion issues and simplifying the process, improving production efficiency and reducing the need for additional cleaning steps.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024139226000001_ABST
    Figure 2024139226000001_ABST
Patent Text Reader

Abstract

To facilitate processes involving transfer of a functional unit.SOLUTION: A method for manufacturing an electronic structure (1) includes the steps of: forming a second sacrificial layer (13) extending from a substrate (10) to a functional unit (12) by using a laminated substrate having the substrate (10), a first sacrificial layer (11) formed on the substrate (10), and a functional section (12) formed on the first sacrificial layer (11); forming a covering layer (14) extending from the substrate (10) to the second sacrificial layer (13); and removing the first sacrificial layer (11) and the second sacrificial layer (13).SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to electronic structures, methods of making electronic structures, and methods of making electronic devices. [Background technology]

[0002] There is known a technique in which a functional part is formed on a substrate via a support layer, and the functional part is peeled off from the substrate and transferred to another substrate (also called a transfer substrate) (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2009-152387 A (see Abstract) Summary of the Invention [Problem to be solved by the invention]

[0004] In the above-mentioned conventional technology, the support layer is peeled off from the substrate together with the functional part and transferred to the transfer substrate. Therefore, the support layer needs to be removed during the transfer process or a subsequent process. In addition, since a part of the support layer breaks during the peeling, the broken pieces may adhere to the transfer substrate, causing defects such as poor bonding. Therefore, there is a demand for facilitating the process including the transfer of the functional part.

[0005] The present disclosure aims to facilitate processes involving the transfer of features. [Means for solving the problem]

[0006] The method for manufacturing an electronic component of the present disclosure uses a laminated substrate having a substrate, a first sacrificial layer formed on the substrate, and a functional portion formed on the first sacrificial layer, and includes the steps of forming a second sacrificial layer extending from the substrate to the functional portion, forming a covering layer extending from the substrate to the second sacrificial layer, and removing the first sacrificial layer and the second sacrificial layer.

[0007] The electronic structure of the present disclosure has a substrate, a functional portion formed on the substrate, and a covering layer formed on the substrate so as to surround the functional portion, with a gap being formed between the functional portion and the covering layer.

[0008] The method for manufacturing an electronic device disclosed herein includes the steps of forming a first sacrificial layer on a substrate, forming a functional unit on the first sacrificial layer, forming a second sacrificial layer extending from the substrate to the functional unit, forming a covering layer extending from the substrate to the second sacrificial layer, removing the first sacrificial layer and the second sacrificial layer to bring the substrate and the functional unit into contact, peeling the functional unit from the substrate, and transferring the functional unit to a substrate other than the substrate. Effect of the Invention

[0009] According to the present disclosure, since the first sacrificial layer and the second sacrificial layer are removed and the functional part is held on the substrate, the functional part can be easily peeled off from the substrate and transferred to another substrate, which makes it possible to facilitate the process including the transfer of the functional part. [Brief description of the drawings]

[0010] [Figure 1] 3 is a flowchart showing a method for manufacturing the electronic structure according to the first embodiment. [Diagram 2] 4A is a cross-sectional view showing a step of forming a first sacrificial layer and a functional portion on a substrate, and FIG. 4B is a cross-sectional view showing a step of forming a second sacrificial layer in a manufacturing method for an electronic component according to the first embodiment. [Diagram 3] 4A is a cross-sectional view showing a step of roughening the surface of a second sacrificial layer, and FIG. 4B is a cross-sectional view showing a step of patterning the second sacrificial layer, in the method for manufacturing the electronic component according to the first embodiment. [Figure 4] 4A and 4B are a cross-sectional view and a plan view showing a step of forming a support layer (covering layer) in a manufacturing method for an electronic component according to the first embodiment. [Diagram 5]5A and 5B are a cross-sectional view and a bottom view showing a step of removing a first sacrificial layer and a second sacrificial layer in the method for manufacturing the electronic component according to the first embodiment. [Figure 6] 1A is a cross-sectional view and FIG. 1B is a plan view showing an electronic structure and a transfer tool according to a first embodiment. [Figure 7] 4A and 4B are cross-sectional views showing a stepwise process of peeling off the functional part of the electronic structure of the first embodiment from a substrate. [Figure 8] 4A and 4B are cross-sectional views showing step-by-step processes for transferring the functional portion of the electronic structure of the first embodiment onto a transfer substrate. [Figure 9] 4A and 4B are a cross-sectional view and a plan view showing a process of forming wiring and the like on a functional section transferred from the electronic structural body of the first embodiment to a transfer substrate. [Figure 10] 4 is a cross-sectional view showing another configuration example of the electronic structure according to the first embodiment. FIG. [Figure 11] 13A and 13B are a cross-sectional view and a plan view showing a state in which a first sacrificial layer, a functional unit, a second sacrificial layer, and a retaining layer are formed on a substrate in a manufacturing method for an electronic component according to a modified example. [Figure 12] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a first sacrificial layer and a second sacrificial layer in a manufacturing method for an electronic component according to a modified example. [Figure 13] 10 is a flowchart showing a method for manufacturing an electronic structural member according to a second embodiment. [Figure 14] FIG. 11 is a cross-sectional view (A) showing a step of forming a first sacrificial layer and a functional part on a substrate in a manufacturing method for an electronic component of embodiment 2, a cross-sectional view (B) showing a step of forming a second sacrificial layer, and a cross-sectional view (C) showing a step of patterning the second sacrificial layer. [Figure 15] 13A is a cross-sectional view showing a step of forming a retention layer, and FIG. 13B is a cross-sectional view showing a step of removing a first sacrificial layer and a second sacrificial layer in a manufacturing method for an electronic component according to a second embodiment. [Figure 16] 11 is a flowchart showing a method for manufacturing an electronic structure according to a third embodiment. [Figure 17]FIG. 11 is a cross-sectional view (A) showing a step of forming a third sacrificial layer and a first sacrificial layer on a substrate in a manufacturing method for an electronic component of embodiment 3; FIG. 11 is a cross-sectional view (B) showing a step of forming a functional unit on the first sacrificial layer; and FIG. 11 is a cross-sectional view (C) showing a step of forming a second sacrificial layer. [Figure 18] 13A is a cross-sectional view showing a step of roughening the surface of a second sacrificial layer, and FIG. 13B is a cross-sectional view showing a step of patterning the second sacrificial layer, in a manufacturing method for an electronic component according to a third embodiment. [Figure 19] 13A is a cross-sectional view showing a step of forming a retention layer, and FIG. 13B is a cross-sectional view showing a step of removing a first sacrificial layer in a manufacturing method for an electronic component according to a third embodiment. [Figure 20] 13A and 13B are a cross-sectional view and a plan view showing a step of roughening the surface of a third sacrificial layer in a manufacturing method for an electronic component according to a third embodiment. [Figure 21] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a second sacrificial layer in a manufacturing method for an electronic component according to a third embodiment. [Figure 22] 11A and 11B are cross-sectional views showing a step-by-step process of peeling off a functional unit of an electronic structure according to a third embodiment from a substrate. [Figure 23] 13A and 13B are cross-sectional views showing a stepwise process of transferring a functional unit of an electronic structure according to a third embodiment onto a transfer substrate. [Figure 24] 13A and 13B are a cross-sectional view and a plan view showing a state in which a first sacrificial layer, a functional unit, a second sacrificial layer, and a retaining layer are formed on a substrate in a manufacturing method for an electronic component according to a fourth embodiment. [Diagram 25] 1A and 1B are a cross-sectional view and a plan view showing an electronic structural body according to a fourth embodiment. [Figure 26] 13A and 13B are cross-sectional views showing a stepwise process of peeling off a functional portion of an electronic structure according to a fourth embodiment from a substrate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An electronic structure and a method for manufacturing the same according to an embodiment will now be described with reference to the drawings. The electronic structure is used in the manufacturing process of an electronic device.

[0012] The electronic device is, for example, a photoelectric conversion device having a photoelectric conversion element (light emitting element, light receiving element) such as an LED (light emitting diode), etc. The photoelectric conversion device is used in a photoelectric conversion module such as an LED display or an image sensor.

[0013] The electronic device may be a piezoelectric device, which is used in a piezoelectric module such as a piezoelectric sensor, an actuator, an ultrasonic sensor, an ultrasonic generator, a pressure transducer, etc. The electronic device may be a switch element, a power device, etc.

[0014] First Embodiment <Method of manufacturing electronic structures> Fig. 1 is a flowchart showing a method for manufacturing an electronic structure according to embodiment 1. Fig. 2(A) is a cross-sectional view showing a step of forming a first sacrificial layer 11 and a functional portion 12 on a substrate 10. Fig. 2(B) is a cross-sectional view showing a step of forming a second sacrificial layer 13.

[0015] In step S101 (FIG. 1), a first sacrificial layer 11 is formed on a substrate 10, and a functional portion 12 is formed on the first sacrificial layer 11, as shown in FIG. 2(A).

[0016] The substrate 10 is a semiconductor substrate or an insulating substrate. When the functional portion 12 described below is a semiconductor layer that serves as a light-emitting element, the substrate 10 is desirably a GaAs substrate (wafer) suitable for forming a semiconductor layer.

[0017] The first sacrificial layer 11 is formed on the surface of the substrate 10. When the functional section 12 is epitaxially grown on the first sacrificial layer 11, the first sacrificial layer 11 is preferably an AlGaAs layer having a lattice constant close to that of the functional section 12 and a large etching selectivity. The thickness of the first sacrificial layer 11 is, for example, 10 nm or more and 1 μm or less.

[0018] The functional portion 12 is, for example, a semiconductor layer or an epitaxial layer, and is also called a functional thin film.

[0019] The functional portion 12 is, for example, a GaP / AlInGaP heterojunction semiconductor film. The functional portion 12 may also be GaAs, InGaP, GaN, AlGaN, InGaN. The functional portion 12 may also be a crystal layer having piezoelectric properties.

[0020] As described above, the functional section 12 is formed on the first sacrificial layer 11 by epitaxial growth. However, the functional section 12 may be epitaxially grown on a substrate other than the substrate 10, and then peeled off from the substrate and transferred onto the first sacrificial layer 11. In this case, the first sacrificial layer 11 may be formed of an inorganic film such as Al2O3 or SiO2 formed by CVD (chemical vapor deposition), or an organic film such as a photosensitive resist. The substrate 10 may be, for example, a Si substrate.

[0021] The bottom surface of the functional section 12, that is, the surface on the substrate 10 side, is a smooth surface with a surface roughness (maximum height Ry) of 10 nm or less.

[0022] In step S102 (FIG. 1), as shown in FIG. 2(B), the first sacrificial layer 11 and the functional section 12 are patterned by etching or the like to form a separation groove 61 that exposes the surface of the substrate 10. The substrate 10, the first sacrificial layer 11, and the functional section 12 are collectively referred to as a laminated substrate.

[0023] In step S103 (FIG. 1), as shown in FIG. 2(B), a second sacrificial layer 13 is formed extending from the surface of the substrate 10 to the functional portion 12. The second sacrificial layer 13 is, for example, an inorganic film such as Al2O3 or SiO2, or an organic film such as a photosensitive resist. The thickness of the second sacrificial layer 13 is, for example, 100 nm.

[0024] If the materials of the first sacrificial layer 11 and the second sacrificial layer 13 are selected so that they can be removed with the same etching solution, the first sacrificial layer 11 and the second sacrificial layer 13 can be removed simultaneously in step S107 described below.

[0025] The second sacrificial layer 13 is formed so as to extend from the surface of the substrate 10 exposed by the separation grooves 61 to the surface of the functional section 12 (that is, the surface opposite to the substrate 10).

[0026] Fig. 3(A) is a cross-sectional view showing a step of roughening the surface of the second sacrificial layer 13. Fig. 3(B) is a cross-sectional view showing a step of patterning the second sacrificial layer 13.

[0027] In step S104 (FIG. 1), as shown in FIG. 3A, the surface 13e of the second sacrificial layer 13 is roughened. The roughening is a process for increasing the surface roughness, and is performed by, for example, a plasma process such as ashing.

[0028] Furthermore, the method is not limited to plasma treatment, and particles may be attached to the surface 13e of the second sacrificial layer 13. For example, when a metal material is vacuum-deposited, the metal material is granulated by self-organization and attached to the surface 13e of the second sacrificial layer 13, thereby roughening the surface. Regardless of which roughening method is used, in addition to the surface 13e of the second sacrificial layer 13, the side surface of the second sacrificial layer 13 is also roughened.

[0029] The surface roughness of the surface 13e of the second sacrificial layer 13 after roughening is rougher than the surface roughness of the bottom surface (i.e., the surface on the substrate 10 side) of the functional portion 12. As an example, the surface roughness (maximum height Ry) of the surface 13e of the second sacrificial layer 13 is rougher than 10 nm.

[0030] In step S105 (FIG. 1), as shown in FIG. 3(B), the second sacrificial layer 13 is patterned to form an opening 62. The opening 62 is formed so that an etching solution can easily reach the first sacrificial layer 11 in a process (step S107) of removing the sacrificial layers 11 and 13, which will be described later.

[0031] 4(A) and (B) are a cross-sectional view and a plan view showing a step of forming the retention layer 14. Note that Fig. 4(A) corresponds to a cross-sectional view taken along line 4A-4A shown in Fig. 4(B).

[0032] In step S106 (FIG. 1), as shown in FIG. 4(A), a retention layer 14 is formed as a covering layer extending from the surface of the substrate 10 to the second sacrificial layer 13. The material of the retention layer 14 is preferably a material that is not eroded by an etching solution in the step (step S107) of removing the first sacrificial layer 11 and the second sacrificial layer 13 described below, and an organic resist is used as an example.

[0033] A surface 14e of the retention layer 14 that contacts the surface 13e of the second sacrificial layer 13 is roughened in the same manner as the surface 13e of the second sacrificial layer 13. The surface roughness of the surface 14e of the retention layer 14 is, for example, rougher than the surface roughness of the bottom surface (i.e., the surface on the substrate 10 side) of the functional portion 12. As an example, the surface roughness (maximum height Ry) of the surface 14e of the retention layer 14 is rougher than 10 nm.

[0034] As shown in FIG. 4(A), the retention layer 14 has a top portion 14a formed on the surface of the second sacrificial layer 13, a base portion 14b formed on the surface of the substrate 10, and a column portion 14c extending between the top portion 14a and the base portion 14b.

[0035] Moreover, it is preferable to pattern the retention layer 14 as shown in Fig. 4(B). Here, an X direction and a Y direction that are perpendicular to each other are defined along the surface of the substrate 10. The planar shape of the functional section 12 is a rectangle having two sides extending in the X direction and two sides extending in the Y direction.

[0036] The retention layer 14 has a first extension portion 141 that straddles the functional portion 12 in the X direction and a second extension portion 142 that straddles the functional portion 12 in the Y direction in top view. The first extension portion 141 and the second extension portion 142 intersect at the center of the surface of the functional portion 12.

[0037] Since the retention layer 14 is patterned in this manner, openings 63 are formed at positions corresponding to the four corners of the functional portion 12. Note that the openings 62 of the second sacrificial layer 13 formed in step S105 above are formed at positions corresponding to the openings 63.

[0038] 5(A) and (B) are a cross-sectional view and a plan view showing a step of removing the first sacrificial layer 11 and the second sacrificial layer 13. Note that Fig. 5(A) corresponds to a cross-sectional view taken along line 5A-5A shown in Fig. 5(B).

[0039] In step S107 (FIG. 1), the first sacrificial layer 11 and the second sacrificial layer 13 are removed by wet etching, as shown in FIG. 5(A). As an etching solution, for example, a mixture of phosphoric acid and hydrogen peroxide can be used.

[0040] By removing the first sacrificial layer 11 and the second sacrificial layer 13, the functional portion 12 floats in the etching solution. At this time, since the functional portion 12 is surrounded by the retention layer 14, the positional displacement of the functional portion 12 is suppressed.

[0041] In particular, since the retention layer 14 is arranged to straddle the functional unit 12 in the X and Y directions, misalignment of the functional unit 12 in a plane parallel to the surface of the substrate 10 is prevented, and the position of the functional unit 12 in a direction perpendicular to the surface of the substrate 10 is also regulated.

[0042] In addition, the removal of the sacrificial layer means that most of the sacrificial layer is removed, and a small portion may remain. For example, a small portion of the first sacrificial layer 11 may remain on the substrate 10 (see FIG. 10 described later).

[0043] When the substrate 10 is removed from the etching solution, the functional part 12 adheres to and is held on the surface of the substrate 10 by its own weight. The adhesive force between the functional part 12 and the surface of the substrate 10 is due to its own weight and is weak. In addition, a gap A is formed between the functional part 12 and the holding layer 14.

[0044] The gap W between the side surface of the functional part 12 and the retention layer 14 corresponds to the thickness of the second sacrificial layer 13. The thinner the second sacrificial layer 13, the smaller the gap W can be, and the more the positional deviation of the functional part 12 while it is floating in the etching solution can be suppressed. In other words, the positional accuracy of the functional part 12 on the substrate 10 can be improved.

[0045] The thickness of the second sacrificial layer 13 is set to 100 nm here, but is not limited to 100 nm. Since the positional accuracy of the functional section 12 on the transfer substrate 20 (FIG. 8(A)) described later is required to be on the order of 1 μm, it is desirable that the thickness of the second sacrificial layer 13 be 1 μm or less.

[0046] In step S107, the first sacrificial layer 11 and the second sacrificial layer 13 are simultaneously removed, but either one may be removed first. In this case, the materials of the first sacrificial layer 11 and the second sacrificial layer 13 are selected so that they can be removed by different etchants.

[0047] For example, when the first sacrificial layer 11 is removed before the second sacrificial layer 13, the second sacrificial layer 13 holds the functional part 12 at a position away from the substrate 10 while the first sacrificial layer 11 is being removed. This makes it possible to prevent the peripheral part of the functional part 12 from sagging, and allows the etching solution to fully penetrate the entire first sacrificial layer 11. This makes it possible to remove the first sacrificial layer 11 efficiently without leaving any etching residue.

[0048] 5(A), an electronic structure 1 is obtained which has a substrate 10, a functional section 12, and a retaining layer 14, with a gap A provided between the functional section 12 and the retaining layer 14. Steps S101 to S107 correspond to the manufacturing process of the electronic structure 1.

[0049] The electronic device 2 is manufactured by these steps S101 to S107 and steps S108 to S110 which will be described below.

[0050] Fig. 6(A) is a cross-sectional view showing the electronic structure 1 and the transfer tool 17. Fig. 6(B) is a bottom view showing the transfer tool 17.

[0051] In step S108 (FIG. 1), the functional section 12 and the holding layer 14 are peeled off from the substrate 10 of the electronic structure 1. A transfer tool 17 shown in FIG. 6(A) is used for the peeling. The transfer tool 17 has a holding body 18 and a support substrate 19 that supports the holding body 18.

[0052] The holder 18 is preferably adhesive (tacky) and elastic, and is an organic structure in this embodiment. For example, the holder 18 can be formed of an elastomer or a thick-film resist on the surface of the support substrate 19 made of a hard material.

[0053] The holder 18 has a first contact portion 18a in contact with the surface of the functional portion 12 and a second contact portion 18b in contact with the surface (i.e., the surface of the top portion 14a) of the holder layer 14. The first contact portion 18a is located at a position protruding toward the electronic structure 1 side more than the second contact portion 18b.

[0054] When the retention layer 14 extends in a cross shape in the X and Y directions (see FIG. 5(B)), the first contact portions 18a are arranged in two rows and two columns in the X and Y directions. The second contact portions 18b are formed as grooves extending in a cross shape similar to the retention layer 14.

[0055] 7(A) and (B) are cross-sectional views showing a stepwise process of peeling off the functional section 12 and the support layer 14 from the substrate 10. FIG.

[0056] 7(A), contact portions 18a and 18b of a holder 18 of a transfer tool 17 are pressed against the functional unit 12 and the holder layer 14. The holder layer 14 is deformed by being pressed from above by the holder 18, and comes into contact with the surface of the functional unit 12. However, since a surface 14e of the holder layer 14 on the functional unit 12 side is roughened, the adhesive force between the holder layer 14 and the functional unit 12 is extremely weak.

[0057] 7(B), the transfer tool 17 is moved in a direction away from the substrate 10. Since the adhesive force between the holder 18 of the transfer tool 17 and the functional unit 12 is stronger than the adhesive force between the functional unit 12 and the surface of the substrate 10, the functional unit 12 is peeled off from the substrate 10 together with the retaining layer 14.

[0058] 8(A) and (B) are cross-sectional views showing a stepwise process of transferring the functional section 12 and the retaining layer 14 to a substrate (called a transfer substrate) 20 different from the substrate 10. The transfer substrate 20 has a smooth surface in the mounting area of ​​the functional section 12, and the surface roughness (maximum height Ry) of the smooth surface is 10 nm or less. The transfer substrate 20 is also called a second substrate.

[0059] In step S109 (FIG. 1), the transfer tool 17 is moved above the transfer substrate 20, and the functional part 12 held by the transfer tool 17 is pressed against the surface of the transfer substrate 20, as shown in FIG. 8(A).

[0060] Since the bottom surface of the functional part 12 and the surface of the transfer substrate 20 are both smooth surfaces with a surface roughness of 10 nm or less, by applying a specified pressure and heat, the bottom surface of the functional part 12 and the surface of the transfer substrate 20 are bonded together by intermolecular forces, i.e., strong bonding forces.

[0061] Thereafter, as shown in FIG. 8(B), the transfer tool 17 is moved in a direction away from the transfer substrate 20.

[0062] The bonding strength between the bottom surface of the functional part 12 and the surface of the transfer substrate 20 is stronger than the adhesive strength between the retainer 18 of the transfer tool 17 and the functional part 12 and the retaining layer 14. In addition, since the surface 14e of the retaining layer 14 facing the functional part 12 is roughened, the adhesive strength between the retaining layer 14 and the functional part 12 is very weak.

[0063] Therefore, the functional portion 12 remains bonded to the transfer substrate 20, and the retention layer 14 is separated from the transfer substrate 20 together with the transfer tool 17. Since only the functional portion 12 remains on the transfer substrate 20, it is not necessary to remove unnecessary members from the transfer substrate 20.

[0064] 9(A) and (B) are a cross-sectional view and a plan view showing a process of forming wiring and the like in the functional unit 12 transferred to the transfer substrate 20. Note that Fig. 9(A) corresponds to a cross-sectional view taken along line 9A-9A shown in Fig. 9(B).

[0065] 9A and 9B, in step S110 (FIG. 1), wiring and the like are formed in the functional section 12. The functional section 12 is formed into, for example, an LED by forming a mesa structure by patterning and forming wiring and the like.

[0066] For example, by a semiconductor process, wiring layers 23 and 24 are formed so as to connect the anode layer 12a and the cathode layer 12b of the functional section 12 to the wirings 21 and 22 on the transfer substrate 20. The process is not limited to the semiconductor process, and for example, wire bonding or a printing process may be used.

[0067] This completes the electronic device 2. When a voltage is applied from the drive circuit to the wiring layers 23 and 24 via the wirings 21 and 22, light is emitted from the functional unit 12 which is an LED.

[0068] <effect> 5(A), the electronic structure 1 of the first embodiment is manufactured by forming a first sacrificial layer 11, a functional section 12, a second sacrificial layer 13, and a retaining layer 14 on a substrate 10, and then removing the first sacrificial layer 11 and the second sacrificial layer 13. Therefore, the functional section 12 is attached to and retained on the surface of the substrate 10 by a weak force.

[0069] 7B, the functional section 12 can be easily peeled off from the substrate 10 and transferred to the transfer substrate 20. This makes it possible to facilitate the process including the transfer of the functional section 12.

[0070] 8(B), since the retention layer 14 is removed while remaining attached to the transfer tool 17 after the functional portion 12 is transferred to the transfer substrate 20, there is no need to perform a step of removing the retention layer 14 from the transfer substrate 20. Therefore, the transfer substrate 20 can be a printed circuit board, a flexible circuit board, or the like, on which electronic components or the like are mounted in advance.

[0071] 5(A), since the retaining layer 14 extends from the substrate 10 to the second sacrificial layer 13, the retaining layer 14 can suppress misalignment of the functional unit 12 in the step of removing the first sacrificial layer 11 and the second sacrificial layer 13. Therefore, the positional accuracy of the functional unit 12 on the substrate 10 can be improved.

[0072] 3(A), by roughening the surface 13e of the second sacrificial layer 13, the surface 14e of the retention layer 14 formed on the second sacrificial layer 13 on the functional unit 12 side is also roughened. This makes it possible to weaken the adhesive force between the functional unit 12 and the retention layer 14, and makes it possible to easily separate the retention layer 14 from the functional unit 12 in the step shown in FIG. 8(B).

[0073] <Advantages of the First Embodiment> As described above, the manufacturing method for the electronic structure 1 of embodiment 1 uses a laminated substrate having a substrate 10, a first sacrificial layer 11 provided on the substrate 10, and a functional section 12 formed on the first sacrificial layer 11, and includes the steps of forming a second sacrificial layer 13 extending from the substrate 10 to the functional section 12, forming a retention layer (covering layer) 14 extending from the substrate 10 to the second sacrificial layer 13, and removing the first sacrificial layer 11 and the second sacrificial layer 13.

[0074] In this electronic structure 1, the functional unit 12 is held in a state of being attached to the substrate 10 by weak adhesive force, so that the functional unit 12 can be easily peeled off from the substrate 10 and transferred to the transfer substrate 20. This makes it possible to facilitate the process including the transfer of the functional unit 12.

[0075] Furthermore, in the process of removing the first sacrificial layer 11 and the second sacrificial layer 13, the retention layer 14 acts to suppress misalignment of the functional unit 12. Therefore, the positional accuracy of the functional unit 12 on the substrate 10 can be improved.

[0076] Furthermore, by making the surface roughness of the surface 14e of the retention layer 14 facing the functional part 12 rougher than the surface roughness of the bottom surface of the functional part 12 (i.e., the surface facing the substrate 10), the retention layer 14 can be easily separated from the functional part 12 after the functional part 12 is transferred to the transfer substrate 20.

[0077] Furthermore, since the first sacrificial layer 11 and the second sacrificial layer 13 are removed with the same etching material, the first sacrificial layer 11 and the second sacrificial layer 13 can be removed in a single process (step S107), thereby further improving production efficiency.

[0078] Fig. 10 is a diagram showing another configuration example of the electronic structure 1. The electronic structure 1 shown in Fig. 10 is manufactured by the same manufacturing method as in the first embodiment, but a part of the first sacrificial layer 11 (referred to as a remaining portion 11a) is left in step S107 (Fig. 1).

[0079] In this configuration example, the substrate 10 and the functional unit 12 are bonded via the remaining portion 11a, which is highly effective in suppressing misalignment of the functional unit 12 on the substrate 10. Furthermore, if the area of ​​the remaining portion 11a of the first sacrificial layer 11 is made small, the functional unit 12 can be easily peeled off from the substrate 10 in the peeling process of step S108 (FIG. 1).

[0080] However, a cleaning step for removing the remaining portion 11a from the bottom surface of the substrate 10 is required before the transfer step (FIG. 8(A)) for transferring the functional portion 12 to the transfer substrate 20.

[0081] Variations. Next, a modified example of the first embodiment will be described. In the modified example, a functional unit 30 including a plurality of elements and a wiring layer is used instead of the functional section 12 of the first embodiment. The functional unit 30 is formed on another growth substrate, for example, peeled off from the growth substrate, and transferred to the substrate 10.

[0082] 11(A) and (B) are a cross-sectional view and a plan view showing the state in which a first sacrificial layer 11, a functional unit 30, a second sacrificial layer 13 and a retention layer 14 are formed on a substrate 10 in a manufacturing method of an electronic structure 1A that is a modified example of embodiment 1.

[0083] A functional unit 30 serving as a functional portion has a base layer 31, a functional layer 32, a first wiring layer 33, a second wiring layer 34, and an encapsulation layer 35 covering these.

[0084] The base layer 31 is disposed on the first sacrificial layer 11 and is made of an insulator such as SiO2. The base layer 31 has through holes (through holes) 31a, 31b that reach the first sacrificial layer 11. The bottom surface of the base layer 31, i.e., the surface on the substrate 10 side, is a smooth surface with a surface roughness (maximum height Ry) of 10 nm or less.

[0085] The functional layer 32 is, for example, a semiconductor layer and an epitaxial layer. The functional layer 32 includes an anode layer 32a and a cathode layer 32b. The functional layer 32 is also called a functional thin film.

[0086] The wiring layers 33 and 34 are formed of, for example, gold (Au) or an alloy thereof. The first wiring layer 33 extends from the anode layer 32a of the functional layer 32 to the through-hole 31a of the base layer 31. The first wiring layer 33 is exposed on the lower surface of the base layer 31 through the through-hole 31a to form an electrode pad 33a. The surface roughness of the electrode pad 33a is, for example, 10 nm.

[0087] The second wiring layer 34 extends from the cathode layer 32b of the functional layer 32 to the through-hole 31b of the base layer 31. The second wiring layer 34 is exposed on the lower surface of the base layer 31 through the through-hole 31b to form an electrode pad 34a. The surface roughness of the electrode pad 34a is, for example, 10 nm.

[0088] The encapsulation layer 35 is formed so as to cover the base layer 31, the functional layer 32, and the wiring layers 33 and 34, and is made of an insulator such as SiO2. When the functional layer 32 is a semiconductor element such as an LED, the encapsulation layer 35 is made of a material that transmits light.

[0089] An element having a predetermined function (e.g., a light emitting function) is configured by the functional layer 32, the first wiring layer 33, and the second wiring layer 34. As shown in Fig. 12(B) described later, a plurality of elements having different functions are provided in the functional unit 30. Here, three sets of elements (functional layer 32 and wiring layers 33, 34) that emit red, green, and blue light are provided in the functional unit 30.

[0090] The functional unit 30 is provided on a first sacrificial layer 11. In addition, a second sacrificial layer 13 is provided on the functional unit 30, and a retention layer 14 is provided on the second sacrificial layer 13. The substrate 10, the first sacrificial layer 11, and the functional unit 30 are collectively referred to as a laminated substrate.

[0091] The first sacrificial layer 11 and the second sacrificial layer 13 are, for example, an inorganic film or an organic film. More specifically, the first sacrificial layer 11 and the second sacrificial layer 13 are formed of a material that can be removed by an etching solution that does not corrode the base layer 31 and the encapsulation layer 35 of the functional unit 30.

[0092] The support layer 14 is formed of, for example, an organic resist. As described in the first embodiment, the support layer 14 has a top portion 14a, a base portion 14b, and a column portion 14c.

[0093] As described in the first embodiment, the surface 13e of the second sacrificial layer 13 is roughened, and the surface 14e of the retention layer 14 in contact therewith is also roughened.

[0094] In this embodiment, the surface 13e of the second sacrificial layer 13 is roughened to roughen the surface 14e of the retaining layer 14, but the surface 14e of the retaining layer 14 may be roughened by other methods. For example, if the surface of the capsule layer 35 of the functional unit 30 is roughened, the surface 13e of the second sacrificial layer 13 is roughened accordingly, and the surface 14e of the retaining layer 14 can be roughened.

[0095] 12(A) and (B) are a cross-sectional view and a plan view showing a step of removing the first sacrificial layer 11 and the second sacrificial layer 13. Note that Fig. 12(A) corresponds to a cross-sectional view taken along line 12A-12A shown in Fig. 12(B).

[0096] The first sacrificial layer 11 and the second sacrificial layer 13 are removed by wet etching, similar to step S107 in the first embodiment. As the etchant, a material that does not corrode the base layer 31 and the encapsulation layer 35 of the functional unit 30 is selected.

[0097] The first sacrificial layer 11 and the second sacrificial layer 13 may be removed in the same step, or the first sacrificial layer 11 may be removed first.

[0098] Although the functional unit 30 floats in the etching solution, the retaining layer 14 suppresses the displacement of the functional unit 30. Note that, electrode pads 33a, 34a, which are part of the wiring layers 33, 34, are exposed on the bottom surface of the functional unit 30 and come into contact with the etching solution, so the wiring layers 33, 34 are formed of a material (such as the above-mentioned gold) that is not corroded by the etching solution.

[0099] After the first sacrificial layer 11 and the second sacrificial layer 13 are removed, the functional unit 30 is attached and held by weak adhesion to the surface of the substrate 10. In addition, a gap A is formed between the functional unit 30 and the holding layer 14. This forms the electronic structure 1A.

[0100] The functional unit 30 of the electronic structure 1A is peeled off from the substrate 10 by the transfer tool 17 and transferred to the transfer substrate 20 in the same manner as described with reference to FIGS. 6(A) to 8(B).

[0101] Since the functional unit 30 is attached to the surface of the substrate 10 with a weak adhesive force, the functional unit 30 can be easily peeled off from the substrate 10.

[0102] In order to ensure the accuracy of alignment between the electrode pads 33a, 34a on the bottom surface of the functional unit 30 and the wiring 21, 22 on the transfer substrate 20 (Figure 9 (B)), it is desirable that the thickness of the second sacrificial layer 13 be at least half the short-side width of each of the electrode pads 33a, 34a.

[0103] In this modification, the functional unit 30 having a plurality of elements, wirings, and the like can be easily peeled off from the substrate 10 and transferred to the transfer substrate 20. Therefore, the process including the transfer of the functional unit 30 can be facilitated.

[0104] Furthermore, in the process of removing the first sacrificial layer 11 and the second sacrificial layer 13, the retention layer 14 suppresses misalignment of the functional unit 30, so that the positional accuracy of the functional unit 30 on the substrate 10 can be improved.

[0105] Embodiment 2 Fig. 13 is a flowchart showing a method for manufacturing an electronic structural body 1B according to embodiment 2. Embodiment 2 differs from embodiment 1 in that surface roughening (step S104 in Fig. 1) is not performed.

[0106] Fig. 14(A) is a cross-sectional view showing a process of forming a first sacrificial layer 11 and a functional section 12 on a substrate 10. Fig. 14(B) is a cross-sectional view showing a process of patterning the first sacrificial layer 11 and the functional section 12 to form a second sacrificial layer 13. Fig. 14(C) shows a process of patterning the second sacrificial layer 13.

[0107] In step S101 (FIG. 13), a first sacrificial layer 11 is formed on a substrate 10, and a functional portion 12 is formed on the first sacrificial layer 11, as shown in FIG. 14(A).

[0108] In step S102 (FIG. 13), as shown in FIG. 14(B), the first sacrificial layer 11 and the functional unit 12 are patterned by etching or the like to form a separation groove 61 that exposes the surface of the substrate 10. The substrate 10, the first sacrificial layer 11, and the functional unit 12 are collectively referred to as a laminated substrate.

[0109] In step S103 (FIG. 13), as shown in FIG. 14(B), a second sacrificial layer 13 is formed, extending from the surface of the substrate 10 to the functional section 12.

[0110] In the first embodiment, the surface of the second sacrificial layer 13 is roughened in step S104, but in the second embodiment, the surface is not roughened.

[0111] In step S105 (FIG. 13), the second sacrificial layer 13 is patterned to form an opening 62, as shown in FIG. 14(C).

[0112] Fig. 15(A) is a cross-sectional view showing a step of forming the retention layer 14. Fig. 15(B) is a cross-sectional view showing a step of removing the first sacrificial layer 11 and the second sacrificial layer 13.

[0113] In step S106 (FIG. 13), as shown in FIG. 15(A), a retention layer 14 is formed extending from the surface of the substrate 10 to the second sacrificial layer 13. Since the surface of the second sacrificial layer 13 is not roughened, the surface of the retention layer 14 that comes into contact with the second sacrificial layer 13 is also not roughened.

[0114] In step S107 (FIG. 13), as shown in FIG. 15(B), the first sacrificial layer 11 and the second sacrificial layer 13 are removed by etching. By removing the sacrificial layers 11 and 13, the functional unit 12 is attached and held on the surface of the substrate 10 by weak adhesion. In addition, a gap A is formed between the functional unit 12 and the holding layer 14. As a result, the electronic structure 1B is obtained.

[0115] The functional portion 12 of the electronic structure 1B is peeled off from the substrate 10 by a transfer tool 17 and transferred to a transfer substrate 20 in the same manner as that described with reference to FIGS. 6(A) to 8(B).

[0116] As described above, the functional section 12 is attached to the surface of the substrate 10 with weak adhesive force, so that in the step of peeling the functional section 12 from the substrate 10, the functional section 12 can be easily peeled off from the substrate 10.

[0117] In the second embodiment, the surface of the retention layer 14 facing the functional section 12 is not roughened. However, if the material of the retention layer 14 is selected so that the adhesive strength between the retention layer 14 and the functional section 12 is sufficiently smaller than the bonding strength between the functional section 12 and the surface of the transfer substrate 20, the retention layer 14 can be peeled off from the transfer substrate 20 while leaving the functional section 12 on the transfer substrate 20.

[0118] Embodiment 3 Next, a third embodiment will be described. Fig. 16 is a flow chart showing a manufacturing method of an electronic structure 1C of the third embodiment. Fig. 17(A) is a cross-sectional view showing a step of forming a third sacrificial layer 15 and a first sacrificial layer 11 on a substrate 10. Fig. 17(B) is a cross-sectional view showing a step of forming a functional unit 30 on the first sacrificial layer 11. Fig. 17(C) is a cross-sectional view showing a step of forming a second sacrificial layer 13.

[0119] In step S201 (FIG. 16), a third sacrificial layer 15 serving as a third sacrificial layer is formed on a substrate 10, and a first sacrificial layer 11 is formed on the third sacrificial layer 15, as shown in FIG. 17(A).

[0120] The third sacrificial layer 15 is, for example, an inorganic film or an organic film. The first sacrificial layer 11 is, for example, an inorganic film or an organic film. More specifically, the first sacrificial layer 11 is formed of a material that can be removed by an etching solution that does not corrode the third sacrificial layer 15 and the second sacrificial layer 13 described later.

[0121] In step S202 (FIG. 16), as shown in FIG. 17(A), the third sacrificial layer 15 and the first sacrificial layer 11 are patterned by dry etching or the like to form separation grooves 61 that expose the surface of the substrate 10.

[0122] In step S203 (FIG. 16), as shown in FIG. 17(B), a functional unit 30 is formed on the first sacrificial layer 11. As described in the modification of the first embodiment, the functional unit 30 is a complex including a plurality of elements and a wiring layer. The functional unit 30 is formed, for example, on another growth substrate, peeled off from the growth substrate, and transferred to the substrate 10.

[0123] The functional unit 30 has a base layer 31, a functional layer 32, a first wiring layer 33, a second wiring layer 34, and an encapsulation layer 35 that covers them. These are similar to those in the modified example of the first embodiment (FIGS. 11(A) to 12(B)), so a description thereof will be omitted. The substrate 10, the third sacrificial layer 15, the first sacrificial layer 11, and the functional unit 30 are collectively referred to as a laminated substrate.

[0124] In step S204 (FIG. 16), as shown in FIG. 17(C), a second sacrificial layer 13 is formed extending from the surface of the substrate 10 to the functional unit 30. The second sacrificial layer 13 is, for example, an inorganic film such as Al2O3 or SiO2. The thickness of the second sacrificial layer 13 is, for example, 100 nm.

[0125] Fig. 18(A) is a cross-sectional view showing a step of roughening the surface of second sacrificial layer 13. Fig. 18(B) is a cross-sectional view showing a step of patterning second sacrificial layer 13.

[0126] In step S205 (FIG. 16), as shown in FIG. 18(A), the surface 13e of the second sacrificial layer 13 is roughened. As a method for roughening the surface, a plasma treatment such as ashing may be performed, or particles of metal or the like may be attached.

[0127] In step S206 (FIG. 16), the second sacrificial layer 13 is patterned to form an opening 62, as shown in FIG. 18(B).

[0128] Fig. 19(A) is a cross-sectional view showing a step of forming the retention layer 14. Fig. 19(B) is a cross-sectional view showing a step of removing the first sacrificial layer 11.

[0129] In step S207 (FIG. 16), as shown in FIG. 19(A), a retention layer 14 is formed as a covering layer extending from the surface of the substrate 10 to the second sacrificial layer 13. The retention layer 14 is formed of a material that is not corroded by an etching solution in a step of removing the first sacrificial layer 11 (step S208) described below, such as an organic resist. A surface 14e of the retention layer 14 that contacts the surface 13e of the second sacrificial layer 13 is roughened in the same manner as the surface 13e of the second sacrificial layer 13.

[0130] 19(A), the retention layer 14 has a top portion 14a formed on the surface of the second sacrificial layer 13, a base portion 14b formed on the surface of the substrate 10, and a column portion 14c extending between the top portion 14a and the base portion 14b. In addition, the retention layer 14 is desirably patterned into the planar shape shown in FIG. 4(B) of the first embodiment, for example.

[0131] In step S208 (FIG. 16), the first sacrificial layer 11 is removed by wet etching, as shown in FIG. 19(B). As an etching solution, diluted hydrochloric acid or the like can be used.

[0132] Since the first sacrificial layer 11 is removed but the second sacrificial layer 13 is not removed, the functional unit 30 is held by the holding layer 14 via the second sacrificial layer 13. Therefore, a gap C is formed between the third sacrificial layer 15 on the substrate 10 and the functional unit 30.

[0133] 20(A) and (B) are a cross-sectional view and a plan view showing a step of roughening the surface of the third sacrificial layer 15. Note that Fig. 20(A) corresponds to a cross-sectional view taken along line segment 20A-20A shown in Fig. 20(B).

[0134] In step S209 (FIG. 16), as shown in FIGS. 20(A) and 20(B), the surface of the third sacrificial layer 15 is roughened. Although the surface of the third sacrificial layer 15 is within a narrow gap C, it is possible to roughen the surface by ashing or other plasma treatment. In addition, when the third sacrificial layer 15 is made of metal, the surface of the third sacrificial layer 15 can also be roughened by heating.

[0135] In the case of plasma treatment, it is desirable to use a material (eg, an inert gas) that does not roughen the bottom surface of the functional unit 30 (including the electrode pads 33a and 34a).

[0136] The surface roughening is performed so that the surface roughness of the third sacrificial layer 15 is rougher than the bottom surface of the base layer 31 of the functional unit 30. As an example, the surface roughening is performed so that the surface roughness (maximum height Ry) of the third sacrificial layer 15 is rougher than 10 nm.

[0137] Figures 21(A) and (B) are a cross-sectional view and a plan view showing a step of removing the second sacrificial layer 13. Note that Figure 21(A) corresponds to a cross-sectional view taken along line 21A-21A shown in Figure 21(B). Also, in Figure 21(B), the retention layer 14 is indicated by a dashed line.

[0138] In step S210 (FIG. 16), the second sacrificial layer 13 is removed by wet etching, as shown in FIG. 21(B). Phosphoric acid or the like can be used as an etching solution.

[0139] As the second sacrificial layer 13 is removed, the functional unit 30 floats in the etching solution, but since the retention layer 14 is provided to surround the functional unit 30 (Figure 21 (B)), displacement of the functional unit 30 is suppressed.

[0140] When the substrate 10 is removed from the etching solution, the functional unit 30 is held on the surface of the third sacrificial layer 15 by its own weight. Since the surface of the third sacrificial layer 15 is roughened, the adhesive force between the third sacrificial layer 15 and the functional unit 30 is extremely weak. In addition, a gap A is formed between the functional unit 30 and the holding layer 14.

[0141] 21(B), an electronic structure 1C is obtained which has the substrate 10, the functional unit 30, and the support layer 14, with a gap A provided between the functional unit 30 and the support layer 14. Steps S201 to S210 correspond to the manufacturing process of the electronic structure 1C.

[0142] Through these steps S201 to S210 and steps S211 to S213 described below, the electronic device 2C is obtained.

[0143] 22(A) and (B) are cross-sectional views showing a stepwise process of peeling the functional unit 30 and the support layer 14 from the substrate 10. FIG.

[0144] In step S211 (FIG. 16), the functional unit 30 and the support layer 14 are peeled off from the substrate 10 of the electronic structure 1C. For the peeling, a transfer tool 17 shown in FIG. 22(A) is used. The configuration of the transfer tool 17 is as described in the first embodiment.

[0145] 22(A), the retainer 18 of the transfer tool 17 is pressed against the functional unit 30 and the retainer layer 14. The retainer layer 14 is deformed by being pressed from above by the retainer 18, and comes into contact with the surface of the functional unit 30. However, since the surface 14e of the retainer layer 14 facing the functional unit 30 is roughened, the adhesive force between the retainer layer 14 and the functional unit 30 is extremely weak.

[0146] 22(B), the transfer tool 17 is moved in a direction away from the substrate 10. The adhesive force between the holder 18 of the transfer tool 17 and the functional unit 30 is stronger than the adhesive force between the functional unit 30 and the third sacrificial layer 15. Therefore, the functional unit 30 is peeled off from the substrate 10 together with the holder layer 14.

[0147] In FIG. 22B, the support layer 14 breaks when the functional unit 30 is peeled off, and the base portion 14b remains on the substrate 10. However, the support layer 14 may be separated completely from the substrate 10.

[0148] 23(A) and (B) are cross-sectional views showing a stepwise process of transferring the functional unit 30 to a transfer substrate 40 which is separate from the substrate 10. The transfer substrate 40 has a similar structure to the transfer substrate 20 described in the first embodiment, but has wirings 41 and 42 formed thereon in advance.

[0149] In step S212 (FIG. 16), the transfer tool 17 is moved above the transfer substrate 20, and the functional unit 30 held by the transfer tool 17 is pressed against the transfer substrate 20, as shown in FIG. 23(A).

[0150] The bottom surface of the functional unit 30 and the surface of the transfer substrate 20 are smooth surfaces with a surface roughness (maximum height Ry) of 10 nm or less. Therefore, by applying a predetermined pressure and heat, the bottom surface of the functional unit 30 and the surface of the transfer substrate 20 are bonded to each other by intermolecular forces, i.e., strong bonding forces.

[0151] If the extension direction of the wirings 41, 42 on the transfer substrate 40 is the Y direction, the functional unit 30 is transferred to the transfer substrate 40 so that the three elements (the functional layer 32 and the wiring layers 33, 34) are aligned in the Y direction.

[0152] In the above-mentioned process of removing the second sacrificial layer 13 (step S210), the retention layer 14 suppresses misalignment of the functional unit 30, thereby minimizing the misalignment between the electrode pads 33a, 34a of the functional unit 30 and the wirings 41, 42 of the transfer substrate 40.

[0153] Thereafter, as shown in FIG. 23(B), the transfer tool 17 is moved in a direction away from the transfer substrate 20.

[0154] The bonding strength between the bottom surface of the functional unit 30 and the surface of the transfer substrate 20 is stronger than the adhesive strength between the holder 18 of the transfer tool 17 and the functional unit 30 and the retaining layer 14. In addition, since the surface 14e of the retaining layer 14 facing the functional unit 30 is roughened, the adhesive strength between the retaining layer 14 and the functional unit 30 is weak.

[0155] Therefore, the functional unit 30 remains bonded onto the transfer substrate 20 , and the retention layer 14 together with the transfer tool 17 is separated from the transfer substrate 20 .

[0156] This provides an electronic device 2C in which the functional unit 30 is arranged on the transfer substrate 20. By applying a voltage to the wiring layers 33 and 34 via the wirings 41 and 42 from a drive circuit (not shown), red, green and blue light is emitted from the three elements of the functional unit 30.

[0157] As described above, in the third embodiment, after removing the first sacrificial layer 11, the surface of the third sacrificial layer 15 on the substrate 10 is roughened. When the second sacrificial layer 13 is removed, the functional unit 30 is held by the roughened surface of the third sacrificial layer 15, and therefore the adhesive force between the functional unit 30 and the third sacrificial layer 15 is weak. Therefore, in the peeling step, the functional unit 30 can be easily peeled off from the third sacrificial layer 15.

[0158] Although an example using the functional unit 30 has been described here, the functional portion 12 described in the first embodiment may be used instead of the functional unit 30. Also, as described in the second embodiment of the first embodiment, the second sacrificial layer 13 does not need to be roughened.

[0159] Embodiment 4 Next, a fourth embodiment will be described. Figures 24(A) and (B) are a cross-sectional view and a plan view showing a state in which a first sacrificial layer 11, a functional unit 30, a second sacrificial layer 13, and a retention layer 14 are formed on a substrate 10 in a manufacturing method of an electronic structure 1D according to the fourth embodiment.

[0160] In the fourth embodiment, instead of the retaining layer 14 of the first embodiment, a plurality of retaining layers 51 are used as covering layers arranged along the outer periphery of the functional unit 30. Here, as shown in Fig. 24(B), four retaining layers 51 are arranged on the four sides of the functional unit 30, respectively.

[0161] In other words, the retention layers 51 are disposed at positions sandwiching the functional unit 30 from both sides in the X direction and both sides in the Y direction. Note that the retention layers 51 are not limited to being disposed on the four sides of the functional unit 30, and may be disposed, for example, at the four corners. Each retention layer 51 is formed, for example, from an organic resist.

[0162] It is desirable that the retaining layer 51 does not reach the central region of the functional unit 30 in top view. In this way, in the peeling step of the functional unit 30 ( FIG. 26(A) ), the retaining body 18 of the transfer tool 17 can be brought into contact only with the functional unit 30 without contacting the retaining layer 51.

[0163] 24(A), each support layer 51 has a top 51a located on the surface of the second sacrificial layer 13, a base 51b formed on the substrate 10, and a column 51c extending between the top 51a and the base 51b. A corner 51d between the top 51a and the column 51c follows the curved shape of the corner 30a of the capsule layer 35 of the functional unit 30 and has a similar curved shape.

[0164] 24(B), the shortest distance Dx between the tops 51a of the two retention layers 51 facing each other in the X direction is shorter than the X-direction width of the functional unit 30. Similarly, the shortest distance Dy between the tops 51a of the retention layers 51 facing each other in the Y direction is shorter than the Y-direction width of the functional unit 30.

[0165] 25(A) and (B) are a cross-sectional view and a plan view showing a process of removing the first sacrificial layer 11 and the second sacrificial layer 13 by wet etching. Note that Fig. 25(A) corresponds to a cross-sectional view taken along line 25A-25A shown in Fig. 25(B).

[0166] In the process of removing the first sacrificial layer 11 and the second sacrificial layer 13, the functional unit 30 floats in the etching solution. However, as shown in Fig. 25(A), since the functional unit 30 is surrounded by a plurality of retaining layers 51, the positional deviation of the functional unit 30 in a plane parallel to the surface of the substrate 10 is suppressed, and the positional deviation of the functional unit 30 in a direction perpendicular to the surface of the substrate 10 is also restricted.

[0167] By removing the first sacrificial layer 11 and the second sacrificial layer 13, the functional unit 30 is held in a state of being attached to the surface of the substrate 10 by weak adhesion. In addition, a gap A is formed between the functional unit 30 and the holding layer 51. In this way, the electronic structure 1D is obtained.

[0168] 26(A) and (B) are cross-sectional views showing step-by-step processes for peeling the functional unit 30 of the electronic structure 1D from the substrate 10. The transfer tool 17 described in the first embodiment is used for peeling the functional unit 30.

[0169] The holder 18 of the transfer tool 17 is pressed against the upper surface of the functional unit 30. Since the top 51a of the holder layer 51 does not reach the central region of the functional unit 30, the holder 18 can be brought into contact only with the functional unit 30 without contacting the holder layer 51.

[0170] As shown in FIG. 26(A), when the transfer tool 17 is moved in a direction away from the substrate 10, the functional unit 30 is peeled off from the substrate 10.

[0171] As shown in Figure 26 (B), when the transfer tool 17 is further moved in a direction away from the substrate 10, the curved surface 35a of the corner of the capsule layer 35 of the functional unit 30 abuts against the top 51a of the retention layer 51, pushing the retention layer 51 outward.

[0172] The retaining layer 51 is formed of an organic resist and has a certain degree of elasticity and flexibility, and therefore can be elastically deformed by being biased by the functional unit 30. Therefore, the functional unit 30 can be separated from the substrate 10 without breaking the retaining layer 51.

[0173] The transfer of the functional unit 30 onto the transfer substrate 40 is as described with reference to Figures 23(A) and (B) in the third embodiment. However, since the retention layer 51 is not attached to the transfer tool 17, the functional unit 30 can be easily transferred onto the transfer substrate 20.

[0174] In the fourth embodiment, since the retention layer 51 does not remain on the transfer tool 17, the transfer tool 17 can be reused.

[0175] Although an example in which four support layers 51 are arranged around the functional unit 30 has been described here, the number of support layers 51 is not limited to four and may be two or more. For example, support layers 51 may be provided on three sides of the functional unit 30.

[0176] Moreover, the functional section 12 of the first embodiment may be used instead of the functional unit 30. The third sacrificial layer 15 described in the third embodiment may be provided. The substrate 10, the third sacrificial layer 15, the first sacrificial layer 11, and the functional unit 30 (or the functional section 12) are collectively referred to as a laminated substrate.

[0177] As described above, in the fourth embodiment, since a plurality of retaining layers (covering layers) 51 arranged at a distance from each other are used, it is possible to prevent the functional unit 30 from being displaced when the sacrificial layers 11 and 13 are removed, and it is possible to make the transfer tool 17 contact only the functional unit 30, facilitating the process including the transfer. Furthermore, since no retaining layer 51 remains on the transfer tool 17, it becomes possible to reuse the transfer tool 17.

[0178] Note that the functional section 12 described in the first embodiment may be used instead of the functional unit 30. Also, as described in the second embodiment, the second sacrificial layer 13 does not need to be roughened. Also, as described in the third embodiment, the third sacrificial layer 15 may be provided and its surface may be roughened.

[0179] Although the preferred embodiments have been specifically described above, the present disclosure is not limited to the above-described embodiments, and various improvements and modifications can be made.

[0180] The present disclosure can be applied to manufacturing methods of electronic devices such as piezoelectric devices, photoelectric conversion devices, switching elements, and power devices.

[0181] Various aspects of the present disclosure are summarized below as appendices. (Appendix 1) A step of forming a second sacrificial layer extending from the substrate to the functional portion by using a laminated substrate having a substrate, a first sacrificial layer formed on the substrate, and a functional portion formed on the first sacrificial layer; forming a cover layer extending from the substrate to the second sacrificial layer; removing the first sacrificial layer and the second sacrificial layer; A method for producing an electronic structure having the above structure. (Appendix 2) Prior to the step of forming the second sacrificial layer, forming the first sacrificial layer on the substrate; forming the functional portion on the first sacrificial layer; A method for producing the electronic structure described in appendix 1, comprising: (Appendix 3) In the step of removing the first sacrificial layer and the second sacrificial layer, 3. A method for producing an electronic structure according to claim 1 or 2. (Appendix 4) The surface roughness of the surface of the covering layer on the functional part side is made rougher than the surface roughness of the surface of the functional part on the substrate side. 4. A method for producing an electronic structure according to any one of claims 1 to 3. (Appendix 5) the laminate substrate has a third sacrificial layer between the substrate and the first sacrificial layer; The step of removing the first sacrificial layer and the second sacrificial layer includes: removing the first sacrificial layer; making a surface roughness of the third sacrificial layer on a side opposite to the substrate rougher than a surface roughness of the functional portion on the substrate side; and removing the second sacrificial layer. 5. A method for producing an electronic structure according to any one of claims 1 to 4. (Appendix 6) In the step of removing the second sacrificial layer, the functional portion is brought into contact with the third sacrificial layer. 6. A method for producing an electronic structure according to claim 5, (Appendix 7) In the step of removing the first sacrificial layer and the second sacrificial layer, The first sacrificial layer and the second sacrificial layer are removed using the same etching material. 5. A method for producing an electronic structure according to any one of claims 1 to 4. (Appendix 8) In the step of removing the first sacrificial layer and the second sacrificial layer, The first sacrificial layer is removed using a predetermined etching material, and then the other of the second sacrificial layers is removed using an etching material different from the first etching material. 5. A method for producing an electronic structure according to any one of claims 1 to 4. (Appendix 9) In the step of forming the coating layer, A plurality of coating layers are formed along the outer periphery of the functional portion. 9. A method for producing an electronic structure according to any one of claims 1 to 8. (Appendix 10) A substrate; A functional portion formed on the substrate; a covering layer formed on the substrate so as to surround the functional portion; having A gap is formed between the functional portion and the covering layer. electronic structure. (Appendix 11) The surface roughness of the surface of the covering layer on the side of the functional part is greater than the surface roughness of the surface of the functional part on the side of the covering layer. 11. The electronic structure of claim 10. (Appendix 12) A sacrificial layer is provided between the substrate and the functional portion, The surface roughness of the sacrificial layer on the side opposite to the substrate is greater than the surface roughness of the functional portion on the side facing the substrate. 12. The electronic structure according to claim 10 or 11, (Appendix 13) A plurality of the coating layers are formed along the outer periphery of the functional portion. 13. The electronic structure according to any one of claims 10 to 12, (Appendix 14) A step of forming a covering layer extending from the substrate to the second sacrificial layer using a laminate substrate having a substrate, a first sacrificial layer formed on the substrate, and a functional portion formed on the first sacrificial layer; removing the first sacrificial layer and the second sacrificial layer to bring the substrate and the functional portion into contact with each other; peeling the functional portion from the substrate; transferring the functional portion onto a substrate different from the substrate; A method for manufacturing an electronic device comprising the steps of: (Appendix 15) In the step of peeling the functional portion from the substrate, The covering layer is peeled off from the substrate together with the functional portion. A method for producing the electronic device described in Appendix 14. (Appendix 16) In the step of peeling the functional portion from the substrate, The functional portion is peeled off from the substrate while the covering layer is being deformed. A method for producing the electronic device described in Appendix 14. [Explanation of symbols]

[0182] 1,1A,1B,1C,1D electronic structure, 2,2C electronic device, 10 substrate (first substrate), 11 first sacrificial layer, 12 functional portion, 13 second sacrificial layer, 13e surface, 14 retaining layer (covering layer), 14e surface, 15 third sacrificial layer (sacrificial layer, third sacrificial layer), 17 transfer tool, 18 retainer, 19 support, 20,40 transfer substrate (second substrate), 30 functional unit (functional portion), 31 base layer, 32 functional portion, 33 first wiring layer, 33a,34a electrode pad, 34 second wiring layer, 35 encapsulation layer (cover layer), 51 retaining layer (covering layer).

Claims

1. A step of forming a second sacrificial layer extending from the substrate to the functional portion by using a laminated substrate having a substrate, a first sacrificial layer formed on the substrate, and a functional portion formed on the first sacrificial layer; forming a cover layer extending from the substrate to the second sacrificial layer; removing the first sacrificial layer and the second sacrificial layer; A method for producing an electronic structure having the above structure.

2. Prior to the step of forming the second sacrificial layer, forming the first sacrificial layer on the substrate; forming the functional portion on the first sacrificial layer; The method of claim 1 comprising the steps of:

3. In the step of removing the first sacrificial layer and the second sacrificial layer, the functional portion and the substrate are brought into contact with each other.

3. The method for producing an electronic component according to claim 1 or 2.

4. The surface roughness of the surface of the covering layer on the functional part side is made rougher than the surface roughness of the surface of the functional part on the substrate side.

3. The method for producing an electronic component according to claim 1 or 2.

5. the laminate substrate has a third sacrificial layer between the substrate and the first sacrificial layer; The step of removing the first sacrificial layer and the second sacrificial layer includes: removing the first sacrificial layer; making a surface roughness of the third sacrificial layer on a side opposite to the substrate rougher than a surface roughness of the functional portion on the substrate side; and removing the second sacrificial layer.

3. The method for producing an electronic component according to claim 1 or 2.

6. In the step of removing the second sacrificial layer, the functional portion is brought into contact with the third sacrificial layer. The method for producing an electronic component according to claim 4 .

7. In the step of removing the first sacrificial layer and the second sacrificial layer, The first sacrificial layer and the second sacrificial layer are removed using the same etching material.

3. The method for producing an electronic component according to claim 1 or 2.

8. In the step of removing the first sacrificial layer and the second sacrificial layer, The first sacrificial layer is removed by using a predetermined etching material, and then the other of the second sacrificial layers is removed by using an etching material different from the first etching material.

3. The method for producing an electronic component according to claim 1 or 2.

9. In the step of forming the coating layer, A plurality of coating layers are formed along the outer periphery of the functional portion.

3. The method for producing an electronic component according to claim 1 or 2.

10. A substrate; A functional portion formed on the substrate; a covering layer formed on the substrate so as to surround the functional portion; having A gap is formed between the functional portion and the covering layer. electronic structure.

11. The surface roughness of the covering layer on the functional part side is greater than the surface roughness of the functional part on the substrate side.

11. The electronic structure of claim 10.

12. A sacrificial layer is provided between the substrate and the functional portion, The surface roughness of the sacrificial layer on the side opposite to the substrate is greater than the surface roughness of the functional portion on the side facing the substrate.

12. An electronic structure according to claim 10 or 11.

13. A plurality of the coating layers are formed along the outer periphery of the functional portion.

12. An electronic structure according to claim 10 or 11.

14. A step of forming a second sacrificial layer extending from the substrate to the functional portion by using a laminated substrate having a substrate, a first sacrificial layer formed on the substrate, and a functional portion formed on the first sacrificial layer; forming a cover layer extending from the substrate to the second sacrificial layer; removing the first sacrificial layer and the second sacrificial layer to bring the substrate and the functional portion into contact with each other; peeling the functional portion from the substrate; transferring the functional portion onto a substrate different from the substrate; A method for manufacturing an electronic device comprising the steps of:

15. In the step of peeling the functional portion from the substrate, The covering layer is peeled off from the substrate together with the functional portion. The method for producing an electronic device according to claim 14 .

16. In the step of peeling the functional portion from the substrate, The functional portion is peeled off from the substrate while the covering layer is being deformed. The method for producing an electronic device according to claim 14 .

Citation Information

Patent Citations

  • Acoustic sensor and method for manufacturing the same

    JP2011234227A

  • Semiconductor device, and manufacturing method thereof

    JP2016022550A

  • Method for manufacturing semiconductor element

    JP2019149528A

  • Semiconductor substrate, semiconductor substrate manufacturing method, and semiconductor element manufacturing method

    JP2021077909A

  • Method of manufacturing electronic device, electronic device substrate for transfer, and display device

    JP2009152387A