Liquid discharge head manufacturing method, nozzle substrate manufacturing method and liquid discharge head
The use of metal-assisted chemical etching to form nozzles with specific taper angles in liquid ejection heads addresses the challenges of turbulent ink flow and air bubble accumulation, resulting in improved print quality and efficiency.
Patent Information
- Application Number
- JP2023051084
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
AI Technical Summary
Conventional methods struggle to form ideal conical and vertical nozzles in liquid ejection heads, particularly with single crystal silicon, leading to turbulent ink flow, ink stagnation, and air bubble accumulation, which affects print quality.
A manufacturing method using metal-assisted chemical etching (MACE) to form nozzles with a tapered hole portion having a taper angle of 4° to 20° and a cylindrical hole portion, utilizing a semiconductor substrate like P-type single crystal silicon, to create a nozzle substrate with precise nozzle structures.
The method enables the production of nozzles with excellent ejection performance, reducing ink turbulence, air bubble discharge, and improving print quality by stabilizing ink flow and reducing the need for cleaning, while enhancing power efficiency.
Smart Images

Figure 2024140089000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a liquid ejection head, a method for manufacturing a nozzle substrate, and a liquid ejection head. [Background technology]
[0002] In recent years, inkjet printers have been attracting attention not only for printing purposes, but also as devices capable of applying liquefied materials to any location. Inkjet printers are equipped with a liquid ejection head that ejects liquid. A known liquid ejection head is one that ejects liquid filled in a pressure chamber from a nozzle by vibrating a vibration plate that forms the wall of the pressure chamber with a piezoelectric element. Liquid ejection heads that use piezoelectric materials as their power source are not limited to the type of liquid compared to heads that use heat as their power source, and are therefore expected to be used in a wide range of industrial applications.
[0003] Liquid ejection heads are often manufactured by applying MEMS technology. MEMS technology is an abbreviation for Micro Electro Mechanical Systems. A liquid ejection head has a nozzle and is provided with a nozzle substrate made of, for example, a silicon substrate. The nozzle substrate requires very high precision for nozzle processing. In Non-Patent Document 1, a nozzle is formed by forming a two-stage vertical hole using photolithography technology and Si-Deep-RIE. Si-Deep-RIE is a deep dry etching method for silicon.
[0004] In the nozzle composed of two vertical holes described in Non-Patent Document 1, the diameter of the first vertical hole is larger than that of the second vertical hole. This results in a large step between the first and second vertical holes. This step causes turbulence and stagnation of the ink flow. As a result, air bubbles may remain near the step. If air bubbles accumulate, problems with print quality such as missing dots may occur. A method of expelling air bubbles by pushing out a large amount of ink is considered. However, since the step causes stagnation of the ink flow, it is difficult to expel air bubbles even if a large amount of ink is pushed out.
[0005] Considering such problems, ideally, the nozzle should have a tapered hole whose diameter decreases from the ink inlet side to the ink ejection side, and a vertical hole connected to the tapered hole, as described in Non-Patent Document 2. Patent Document 1 describes the formation of a nozzle including a conical portion and a cylindrical portion by combining anisotropic etching and dry etching of a single crystal silicon material. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent Publication No. 2022-025115 [Non-patent literature]
[0007] [Non-Patent Document 1] IEEE Trans.MEMS00 Proceedings, pp. 793-798 [Non-Patent Document 2] Tadashi Shiozaki (ed.); Fundamentals and Latest Applications of Piezoelectric Materials <Popular Edition> (CMC Publishing), Figure 4 on page 170 Summary of the Invention [Problem to be solved by the invention]
[0008] However, it is very difficult to form an ideal conical hole by anisotropic etching. In particular, single crystal silicon is a brittle material and difficult to process. For this reason, it is difficult to obtain a nozzle that combines a conical hole and a vertical hole by the conventional method. Therefore, it is difficult to obtain a nozzle that can obtain optimal discharge characteristics by the conventional method, and therefore it is difficult to manufacture a liquid discharge head with excellent discharge performance. [Means for solving the problem]
[0009] A manufacturing method for a liquid ejection head according to a preferred embodiment of the present invention is a manufacturing method for a liquid ejection head including a pressure chamber substrate including a pressure chamber, and a nozzle substrate including a nozzle communicating with the pressure chamber and formed of a semiconductor substrate, characterized in that the manufacturing method for a liquid ejection head includes a first step of forming the nozzle by performing metal-assisted chemical etching in a state in which a metal film is formed on the nozzle substrate in a first portion of a first surface, which is the surface of the nozzle substrate facing the pressure chamber substrate, corresponding to the nozzle, and in which the metal film is not formed on the nozzle substrate in a second portion of the first surface not corresponding to the nozzle.
[0010] A manufacturing method for a nozzle substrate according to a preferred embodiment of the present invention is a manufacturing method for a nozzle substrate formed of a semiconductor substrate, including a nozzle, and includes a first step of forming the nozzle by performing metal-assisted chemical etching in a state in which a metal film is formed on the nozzle substrate in a first portion of a first surface of the nozzle substrate corresponding to the nozzle, and in a second portion of the first surface not corresponding to the nozzle, the metal film is not formed on the nozzle substrate.
[0011] A liquid ejection head according to a preferred embodiment of the present invention is a liquid ejection head including a pressure chamber substrate including a pressure chamber, and a nozzle substrate including a nozzle communicating with the pressure chamber, wherein the nozzle substrate is a p-type semiconductor substrate, and the nozzle includes a tapered hole portion having a taper angle of 4° or more and 20° or less. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a schematic diagram illustrating a configuration of a liquid ejection device according to a first embodiment. [Diagram 2] FIG. 2 is an exploded perspective view of the liquid ejection head shown in FIG. [Diagram 3] FIG. 3 is a cross-sectional view taken along line aa in FIG. [Figure 4] FIG. 4 is a plan view of the nozzle substrate shown in FIG. [Diagram 5] 5 is an enlarged cross-sectional view of a nozzle hole of the nozzle substrate shown in FIG. [Figure 6] 4 is a diagram showing a flow of a method for manufacturing the nozzle substrate shown in FIG. [Figure 7] 7 is a diagram for explaining the resist layer formation step to the second metal-assisted chemical etching step in FIG. 6. FIG. [Figure 8] 7A to 7C are diagrams for explaining the resist layer and metal film removing step to the polishing step in FIG. 6. [Figure 9] FIG. 1 is a diagram for explaining metal-assisted chemical etching. [Figure 10] FIG. 7 is a diagram for explaining the first metal-assisted chemical etching step of FIG. 6. [Figure 11] 1 is a graph showing the relationship between molar concentration volume ratio and taper angle. [Figure 12] FIG. 11 is a view for explaining a first step of the second embodiment. [Figure 13] 13A to 13C are diagrams for explaining the steps from the oxide film forming step to the resist layer patterning step in FIG. 12. [Figure 14] 13 is a diagram for explaining the oxide film etching step to the second metal-assisted chemical etching step in FIG. 12. FIG. [Figure 15] 13A to 13C are diagrams illustrating a flow of a manufacturing method of a nozzle substrate according to a third embodiment. [Figure 16] 16A to 16C are diagrams for explaining the steps from the protective film etching step to the metal film forming step in FIG. 15. [Figure 17] 16A to 16C are views for explaining the resist layer removal step to the second metal-assisted chemical etching step in FIG. 15. [Figure 18] FIG. 2 is a cross-sectional view showing a jig used in the first metal-assisted chemical etching step. [Figure 19] FIG. 2 is a diagram for explaining a first metal-assisted chemical etching step. [Figure 20] FIG. 2 is a diagram for explaining a first metal-assisted chemical etching step. [Figure 21] FIG. 13 is a diagram for explaining a second metal-assisted chemical etching step. [Figure 22] 5A to 5C are diagrams illustrating the flow of a liquid ejection head manufacturing method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] 1. First embodiment 1-1. Overall configuration of liquid ejection device 1 FIG. 1 is a configuration diagram illustrating a liquid ejection device 1 according to a first embodiment. In the following, for convenience of explanation, an X-axis, a Y-axis, and a Z-axis that are perpendicular to each other will be appropriately used. Moreover, one direction along the X-axis will be referred to as the X1 direction, and the direction opposite to the X1 direction will be referred to as the X2 direction. Similarly, one direction along the Y-axis will be referred to as the Y1 direction, and the direction opposite to the Y1 direction will be referred to as the Y2 direction. One direction along the Z-axis will be referred to as the Z1 direction, and the direction opposite to the Z1 direction will be referred to as the Z2 direction.
[0014] In addition, "element α and element β are in communication" includes cases where element α and element β are in direct communication with each other, as well as cases where element α and element β are in indirect communication with each other via another element. "Element β on element A" is not limited to a configuration where element α and element β are in direct contact with each other, but also includes a configuration where element A and element β are not in direct contact with each other.
[0015] The liquid ejection device 1 is an inkjet printing device that ejects ink, which is an example of a liquid, onto a medium 12. The medium 12 is typically printing paper, but any printing target made of any material, such as a resin film or fabric, can be used as the medium 12. As illustrated in Fig. 1, a container 14 that stores ink is installed in the liquid ejection device 1. For example, a cartridge that can be attached to and detached from the liquid ejection device 1, a bag-shaped ink pack made of a flexible film, or an ink tank that can be refilled with ink can be used as the container 14.
[0016] The liquid ejection device 1 includes a control unit 20, a transport mechanism 22, a moving mechanism 24, and a liquid ejection head 3. The control unit 20 includes one or more processing circuits, such as a CPU (Central Processing Unit) or an FPGA (Field Programmable Gate Array), and one or more storage circuits, such as a semiconductor memory, and performs overall control of each element of the liquid ejection device 1. The transport mechanism 22 transports the medium 12 in a direction along the Y axis under the control of the control unit 20.
[0017] The movement mechanism 24 reciprocates the liquid ejection head 3 along the X axis under the control of the control unit 20. The X axis intersects with the Y axis along the direction in which the medium 12 is transported. The movement mechanism 24 in the first embodiment includes a substantially box-shaped transport body 242 that houses the liquid ejection head 3, and a transport belt 244 to which the transport body 242 is fixed. Note that a configuration in which a plurality of liquid ejection heads 3 are mounted on the transport body 242, or a configuration in which the container 14 is mounted on the transport body 242 together with the liquid ejection head 3, may also be employed.
[0018] The liquid ejection heads 3 eject ink supplied from a container 14 from multiple nozzles onto the medium 12 under the control of a control unit 20. An image is formed on the surface of the medium 12 by each liquid ejection head 3 ejecting ink onto the medium 12 in parallel with the transportation of the medium 12 by the transportation mechanism 22 and the repeated reciprocating motion of the transportation body 242.
[0019] 1-2. Overall configuration of liquid ejection head 3 Fig. 2 is an exploded perspective view of the liquid ejection head 3 shown in Fig. 1. Fig. 3 is a cross-sectional view taken along line aa in Fig. 2. The cross section shown in Fig. 3 is a cross section parallel to the XZ plane. The Z axis is an axis along the direction in which ink is ejected by the liquid ejection head 3. Also, a view from the Z1 direction or the Z2 direction is referred to as a "planar view."
[0020] As illustrated in FIG. 2, the liquid ejection head 3 includes a plurality of nozzles N arranged along the Y axis. The plurality of nozzles N are divided into a first row La and a second row Lb arranged in parallel with each other at intervals along the X axis. Each of the first row La and the second row Lb is a collection of a plurality of nozzles N arranged linearly along the Y axis. The liquid ejection head 3 has a structure in which elements related to each nozzle N of the first row La and elements related to each nozzle N of the second row Lb are arranged substantially symmetrically with respect to a plane. The nozzles N belonging to the first row La are arranged in a line with a density of, for example, 300 dpi. Similarly, the nozzles N belonging to the second row Lb are arranged in a line with a density of, for example, 300 dpi. The nozzles N belonging to the second row Lb are arranged with a shift of, for example, 600 dpi with respect to the nozzles N belonging to the first row La. In the following description, the elements corresponding to the first row La will be described with emphasis, and the description of the elements corresponding to the second row Lb will be omitted as appropriate.
[0021] As illustrated in FIGS. 2 and 3, the liquid ejection head 3 includes a flow path structure 30, a plurality of piezoelectric elements , a sealing substrate 35, a housing portion , and a wiring substrate .
[0022] The flow path structure 30 is a structure in which a flow path is formed for supplying ink to each of the multiple nozzles N. The flow path structure 30 is composed of a communication plate 31, a pressure chamber substrate 32, a vibration plate 33, a nozzle substrate 37, and a vibration absorber .
[0023] Each member constituting the flow path structure 30 is a long plate-like member along the Y axis. A pressure chamber substrate 32 and a housing part 36 are provided on a surface of the communication plate 31 in the Z2 direction. A nozzle substrate 37 and a vibration absorber 38 are provided on a surface of the communication plate 31 in the Z1 direction. The members are fixed together by, for example, an adhesive.
[0024] The nozzle substrate 37 is a plate-like member in which a plurality of nozzles N are formed. Each of the plurality of nozzles N is a circular through-hole that ejects ink.
[0025] The communication plate 31 is formed with a plurality of throttle portions 312, a plurality of communication channels 314, a communication space Ra, and a common channel Rb. Each of the throttle portions 312 and the communication channels 314 extends in the Z1 direction and is a through hole formed for each nozzle N. The communication channel 314 overlaps the nozzle N in a plan view. The communication space Ra is an opening formed in an elongated shape along the Y axis. The communication space Ra extends along the Y axis. The common channel Rb communicates with the communication space Ra and overlaps with the communication space Ra in a plan view. The common channel Rb extends along the Y axis. The common channel Rb communicates with the plurality of throttle portions 312. In addition, the communication space Ra communicates the common channel Rb with an external channel of the liquid ejection head 3 via a space Rc described later.
[0026] A plurality of pressure chambers C1 are formed in the pressure chamber substrate 32. The pressure chamber C1 is a space located between the communication plate 31 and the vibration plate 33 and formed by the wall surface 320 of the pressure chamber substrate 32. The pressure chamber C1 is formed for each nozzle N. The pressure chamber C1 is an elongated space extending in the X1 direction. The plurality of pressure chambers C1 are arranged along the Y axis. One end of the pressure chamber C1 in the X1 direction is connected to the nozzle N via a communication flow path 314. The other end of the pressure chamber C1 in the X1 direction is connected to a throttle portion 312. The throttle portion 312 has a smaller cross-sectional area than the pressure chamber C1. The pressure chamber C1, the nozzle N, the communication flow path 314, and the throttle portion 312 form an individual flow path 300 for each nozzle N. By providing the communication flow passage 314 and the throttle portion 312 in the Z1 direction for the pressure chamber C1, it is possible to arrange the nozzles at a high density, and the liquid ejection head 3 can be made smaller and more dense.
[0027] The communication plate 31 and the pressure chamber substrate 32 are manufactured by processing a single crystal substrate of silicon (Si).
[0028] An elastically deformable vibration plate 33 is disposed above the pressure chamber C1. The vibration plate 33 is laminated on the pressure chamber substrate 32 and contacts the surface of the pressure chamber substrate 32 opposite to the communicating plate 31. The vibration plate 33 is a plate-like member formed in a long rectangular shape along the Y axis in a plan view. The thickness direction of the vibration plate 33 is parallel to the Z1 direction. The pressure chamber C1 communicates with the communicating flow path 314 and the throttle portion 312. Therefore, the pressure chamber C1 communicates with the nozzle N via the communicating flow path 314, and communicates with the communicating space Ra via the throttle portion 312. Note that, for ease of explanation, the pressure chamber substrate 32 and the vibration plate 33 are illustrated in FIG. 2 as separate substrates, but in reality, they are laminated on a single silicon substrate.
[0029] A piezoelectric element 34 is formed for each pressure chamber C1 on the surface of the vibration plate 33 opposite to the pressure chamber C1. The piezoelectric element 34 is an elongated passive element along the X-axis in a plan view. The piezoelectric element 34 is an example of an energy generating element that generates energy for ejecting ink when a drive signal is applied to it. Although a piezoelectric element that generates mechanical energy is described here as the energy generating element, an electrothermal conversion element that generates thermal energy may also be used as long as it is a system that has the vibration plate 33. The piezoelectric element 34 is also a driving element that is driven when a drive signal is applied to it.
[0030] The housing 36 is a case for storing ink to be supplied to the multiple pressure chambers C1, and is formed by, for example, injection molding of a resin material. A space Rc and a supply port 361 are formed in the housing 36. The supply port 361 is a conduit through which ink is supplied from the container 14, and communicates with the space Rc. The space Rc in the housing 36 and the communication space Ra in the communication plate 31 communicate with each other. The communication space Ra, the common flow path Rb, and the space Rc described above form a common space R that is shared by the multiple nozzles N. The common space R functions as a liquid storage chamber that stores ink to be supplied to the multiple pressure chambers C1. The ink stored in the common space R branches off to each throttle section 312 and is supplied to and filled in parallel with the multiple pressure chambers C1.
[0031] The vibration absorber 38 is a flexible film that constitutes the wall surface of the communication space Ra, and absorbs pressure fluctuations of the ink in the common space R. The vibration absorber 38 is, for example, a laminate of an ink-resistant resin film, a SUS (stainless steel) member that holds the resin film and has spring properties, and a fixed plate that protects the resin film and the SUS member. By providing the vibration absorber 38, the natural frequency of the individual flow path 300 that runs from the nozzle N through the pressure chamber C1 to the throttle section 312 is stabilized regardless of the nozzle N that is driven.
[0032] The sealing substrate 35 is a structure that protects the multiple piezoelectric elements 34 and reinforces the mechanical strength of the pressure chamber substrate 32 and the vibration plate 33, and is fixed to the surface of the vibration plate 33 with, for example, an adhesive. The multiple piezoelectric elements 34 are housed inside a recess formed on the surface of the sealing substrate 35 facing the vibration plate 33. A wiring board 40 is bonded to the surface of the vibration plate 33. The wiring board 40 is a mounting component on which multiple wiring lines are formed for electrically connecting the control unit 20 and the liquid ejection head 3. For example, a TCP (Tape Carrier Package) or an FPC (Flexible Printed Circuit) is used as the wiring board 40. A drive signal and a reference voltage for driving the piezoelectric elements 34 are supplied to each piezoelectric element 34 from the wiring board 40.
[0033] In the liquid ejection head 3, when the piezoelectric element 34 contracts due to energization, the vibration plate 33 is bent and deflected in a direction that reduces the volume of the pressure chamber C1, and the pressure inside the pressure chamber C1 rises, causing an ink droplet to be ejected from the nozzle N. At this time, pressure also propagates from the pressure chamber C1 toward the throttle portion 312, and ink also flows into the common flow path Rb through the throttle portion 312. After the ink is ejected, the piezoelectric element 34 returns to its original position. At this time, the ink in the common flow path Rb from the nozzle N also vibrates. Then, at the same time that the meniscus of the nozzle N returns to its original state, ink is supplied from the throttle portion 312. Through the above series of operations, ink is ejected from the nozzle N.
[0034] 1-3.Nozzle board 37 Fig. 4 is a plan view of the nozzle substrate 37 shown in Fig. 3. Fig. 5 is an enlarged view of a portion of the nozzle substrate 37 shown in Fig. 4. The nozzle substrate 37 shown in Figs. 4 and 5 is made of a semiconductor substrate such as a P-type single crystal silicon substrate with a crystal orientation of 100. The nozzle substrate 37 has a first surface 301 and a second surface 302. The first surface 301 is the surface on the pressure chamber substrate 32 side. The second surface 302 is the surface opposite to the first surface 301.
[0035] The nozzle substrate 37 includes a plurality of nozzles N. As described above, the nozzles N are spaced apart from one another and arranged along the Y axis. Each nozzle N is a hole extending in the Z1 direction. The Z2 direction of the nozzle N is the ink inflow side, and the Z1 direction of the nozzle N is the ink outflow side.
[0036] The nozzle N has a tapered hole portion N1 and a cylindrical hole portion N2. The tapered hole portion N1 and the cylindrical hole portion N2 are connected to each other. The planar shape of each of the tapered hole portion N1 and the cylindrical hole portion N2 is circular.
[0037] The tapered hole portion N1 is provided on the ink inflow side of the cylindrical hole portion N2. The tapered hole portion N1 tapers from the ink inflow side toward the ink outflow side. The opening area of the tapered hole portion N1 narrows from the ink inflow side toward the ink outflow side. Therefore, the width D1 of the tapered hole portion N1 gradually decreases toward the cylindrical hole portion N2. The width D1 is a diameter.
[0038] The taper angle θ of the tapered hole N1 is equal to or greater than 4° and equal to or less than 20°. The taper angle θ is the angle between a normal A0 of the first surface 301 and an inner wall surface 303 that forms the tapered hole N1.
[0039] If the taper angle θ is smaller than the lower limit, the flow resistance may become too large, and the ink speed may decrease. If the taper angle θ is larger than the upper limit, the meniscus may become unstable. As a result, air bubbles may be entrained, and the ink ejection direction may become unstable. Therefore, there is a risk that the print quality may be affected, and strict management may be required. In contrast, by providing the tapered hole portion N1 with a taper angle θ within the above range, it is possible to provide a nozzle substrate 37 with excellent ejection performance. Therefore, it is possible to provide a liquid ejection head 3 with excellent print quality. However, for the above reasons, it is preferable that the taper angle of the tapered hole portion N1 is 4° or more and 20° or less, but this is not necessarily required.
[0040] Furthermore, since the nozzle substrate 37 is a P-type single crystal silicon substrate, it is easy to form the tapered hole portion N1 having the taper angle θ within the above range.
[0041] The opening area of the cylindrical hole N2 is constant. Therefore, the width D2 of the cylindrical hole N2 is constant. The width D2 is the diameter. The width W2 of the cylindrical hole N2 and the width W1 of the end of the tapered hole N1 on the ink outflow side are equal. Therefore, there is no large step at the connection between the cylindrical hole N2 and the tapered hole N1. This makes it easy to avoid ink turbulence and stagnation of the ink flow. This makes it possible to reduce the risk of problems with print quality, such as missing dots.
[0042] The cylindrical hole N2 is essential for determining the ink ejection direction and stabilizing the ejection of the ink. The width W2 of the cylindrical hole N2 is not particularly limited, but is preferably 5 μm or more and 50 μm or less. If it is larger than 50 μm, there is a risk that air bubbles may easily get mixed in.
[0043] A liquid ejection head 3 equipped with a nozzle substrate 37 having such nozzles N is extremely excellent in terms of air bubble expulsion properties, and can print with almost no need for cleaning. Furthermore, a liquid ejection head 3 equipped with such nozzle substrate 37 is excellent in power efficiency, and can utilize that power to the maximum. Therefore, a liquid ejection head 3 with extremely high performance can be provided.
[0044] 1-4. Method for forming nozzle N FIG. 6 is a diagram showing the flow of a method for forming the nozzle N shown in FIG. 3. The liquid ejection head manufacturing method includes a method for manufacturing the nozzle substrate 37. The manufacturing method for the nozzle substrate 37 includes a method for forming the nozzle N. As shown in FIG. 6, the method for forming the nozzle N includes a first step S1. In the first step S1, metal-assisted chemical etching is used, which will be described later. Metal-assisted chemical etching is abbreviated as MACE, which is an acronym for Metal-Assisted Chemical Etching. By using metal-assisted chemical etching, it is possible to realize a nozzle N with a configuration that is difficult to process using conventional methods.
[0045] As shown in FIG. 6, the first step S1 includes a resist layer forming step S10, a resist layer patterning step S11, a metal film forming step S12, a first metal-assisted chemical etching step S13, a second metal-assisted chemical etching step S14, a removal step S15, and a polishing step S16.
[0046] Fig. 7 is a diagram for explaining the resist layer forming step S10 to the second metal-assisted chemical etching step S14 in Fig. 6. First, a nozzle substrate 37 is prepared, which is a semiconductor substrate such as a P-type single crystal silicon substrate having a crystal orientation of 100. The nozzle substrate 37 includes a first surface 301 and a second surface 302.
[0047] Fig. 7(a) is a diagram for explaining the resist layer forming step S10. As shown in Fig. 7(a), in the resist layer forming step S10, a resist layer 43 is formed on the outer surface of the nozzle substrate 37. Thus, the resist layer 43 is formed on the first surface 301 and the second surface 302. The resist is applied onto the outer surface of the nozzle substrate 37, and the resist layer 43 is formed by utilizing centrifugal force. The thickness of the resist layer 43 is not particularly limited, but is, for example, 1 µm or more and 3 µm or less.
[0048] Fig. 7(b) is a diagram for explaining the resist layer patterning step S11. As shown in Fig. 7(b), in the resist layer patterning step S11, the resist layer 43 is patterned by removing a part of the resist layer 43.
[0049] The first surface 301 of the nozzle substrate 37 includes a first portion 3011 and a second portion 3012. The first portion 3011 is a portion corresponding to the nozzle N. The second portion 3012 is a portion not corresponding to the nozzle N. The first portion 3011 is a portion from which the resist is removed for metal-assisted chemical etching, which will be described later. The second portion 3012 is a portion that is not removed and is protected in order to protect the substrate from the chemical solution of the metal-assisted chemical etching. In the resist layer patterning step S11, an opening is made in the first portion 3011 to expose the semiconductor substrate surface. Meanwhile, the resist layer 43 is patterned so as not to open in the second portion 3012.
[0050] FIG. 7(c) is a diagram for explaining the metal film forming step S12. As shown in FIG. 7(c), in the metal film forming step S12, a metal film 44 is formed on the first surface 301 of the nozzle substrate 37. In this embodiment, the metal film 44 is formed on the first surface 301 by electroless plating (substitution plating) using the resist layer 43 as a mask. The metal film 44 is formed on the first portion 3011, but not on the second portion 3012. This is because the difference in ionization tendency between the semiconductor material and the plating metal is utilized, and atoms on the semiconductor substrate surface dissolve in the first portion 3011 of the semiconductor substrate surface, receive the electrons, and the metal film 44 precipitates and becomes a metal film. On the other hand, the metal film 44 is not formed on the second portion 3012 covered with the resin film. Therefore, the metal film 44 overlaps the first portion 3011, but does not overlap the second portion 3012 in a plan view. The metal film 44 includes a plurality of portions 441. Each portion 441 contacts the first portion 3011 of the first surface 301 and corresponds to a nozzle N.
[0051] By using electroless plating, the number of pre-processes performed before the metal film forming process S12 can be reduced. Specifically, the pre-process only requires forming a resist layer 43 used as a mask in electroless plating. Since the number of pre-processes can be reduced, the formation time of the nozzle substrate 37 can be shortened.
[0052] Metal film 44 may also include, for example, platinum, gold, silver, ruthenium, palladium, molybdenum, chromium, copper, tantalum, titanium, or oxides of iridium, ruthenium, or the like.
[0053] Fig. 7(d) is a diagram for explaining the first metal-assisted chemical etching step S13. As shown in Fig. 7(d), in the first metal-assisted chemical etching step S13, a tapered hole portion N1 is formed by removing a part of the nozzle substrate 37 by the first metal-assisted chemical etching as the metal-assisted chemical etching. For example, metal-assisted chemical etching using a solution containing hydrogen fluoride and an oxidizing agent is optimal.
[0054] In metal-assisted chemical etching, the semiconductor material portion directly below the metal film 44 of the nozzle substrate 37 is oxidized by the catalytic action of the material of the metal film 44, the oxide of the nozzle substrate 37 is etched by the hydrogen fluoride solution, and the metal film 44 and the nozzle substrate 37 are repeatedly adsorbed by the Coulomb force. By repeating these processes, it is possible to form a hole in the Z1 direction. Furthermore, in this embodiment, by adjusting the ratio of hydrogen fluoride and oxidizing agent contained in the solution, it is possible to form a hole in the Z1 direction while having a taper angle θ. As a result, a tapered hole portion N1 having a taper angle θ can be formed.
[0055] 7(e) is a diagram for explaining the second metal-assisted chemical etching step S14. As shown in FIG. 7(e), in the second metal-assisted chemical etching step S14, a cylindrical hole portion N2 is formed by removing a part of the nozzle substrate 37 by second metal-assisted chemical etching. In this step as well, as in the previous step, it is optimal to use a solution containing, for example, hydrogen fluoride and an oxidizing agent.
[0056] In the second metal-assisted chemical etching process S14, as in the first metal-assisted chemical etching process S13, the oxidation of the nozzle substrate 37 by the catalytic action of the material of the metal film 44, the etching of the oxide of the nozzle substrate 37 by the solution, and the adsorption of the metal film 44 and the nozzle substrate 37 by Coulomb force are repeated. By repeating these processes, a hole is formed in the Z1 direction. In this embodiment, the ratio of hydrogen fluoride and the oxidizing agent contained in the solution is adjusted to form a cylindrical hole portion N2 with a constant width D1.
[0057] The first metal-assisted chemical etching step S13 and the second metal-assisted chemical etching step S14 are performed consecutively. Therefore, the tapered hole portion N1 and the cylindrical hole portion N2 are formed consecutively. After the first metal-assisted chemical etching step S13 is started and a predetermined time has elapsed and the first metal-assisted chemical etching is performed on the nozzle substrate 37 to a predetermined depth, the ratio of hydrogen fluoride and oxidizing agent contained in the solution is adjusted. By adjusting the ratio, the second metal-assisted chemical etching step S14 is started.
[0058] The times for the first metal-assisted chemical etching and the second metal-assisted chemical etching are determined in advance. Metal-assisted chemical etching is performed under the same conditions as the first metal-assisted chemical etching step S13 and the second metal-assisted chemical etching step S14 to obtain an etching rate. Then, the etching time required to dig to a predetermined depth is calculated. Based on this etching time, the times for the first metal-assisted chemical etching and the second metal-assisted chemical etching are determined.
[0059] 8 is a diagram for explaining the removal step S15 to the polishing step S16 in FIG. 6. As shown in FIG. 8(a), in the removal step S15, the resist layer 43 and the metal film 44 are removed. The metal film 44 is removed, for example, by immersing it in a dissolving solution. In this step, the nozzle substrate 37 does not have a through hole. Therefore, no opening is formed on the second surface 302 of the nozzle substrate 37.
[0060] 8(b), in the polishing process S16, the second surface 302 of the nozzle substrate 37 is polished to remove a portion of the nozzle substrate 37. As a result, a nozzle N including a tapered hole portion N1 and a cylindrical hole portion N2 is formed. Furthermore, the polishing process S16 can make the nozzle substrate 37 have a desired thickness.
[0061] By including the polishing step S16, even if a portion of the metal film 44 remains in the previous step without being removed, the remaining portion of the metal film 44 can be removed. This prevents the remaining portion of the metal film 44 from remaining as a foreign object in the cylindrical hole portion N2. This improves the yield and quality of the nozzle N.
[0062] The polishing step S16 may be omitted. In this case, the nozzle N, which is a hole penetrating the nozzle substrate 37, is formed in the removing step S15.
[0063] FIG. 9 is a diagram for explaining metal-assisted chemical etching. As shown in FIG. 9(a), the metal film 44 has a plurality of through holes H. Each through hole H penetrates the metal film 44 in the Z1 direction. The through holes H may be formed by any method. The opening area of the through holes H is not particularly limited, and may be sufficient as long as the solution can pass through. The thickness of the metal film 44 is preferably 8 nm or more and 40 nm or less, and more preferably 15 nm or more and 25 nm or less. In the MACE process, the metal film 44 moves toward the inside of the semiconductor substrate, so it is subjected to tensile stress. Since it is necessary to withstand this stress, the thicker the film, the higher the strength, and the film will not break during the MACE process, and the etching shape will not be deformed, and a stable etching shape can be realized. On the other hand, if the thickness is 40 nm or more, it becomes difficult to form the through holes H, and there is a risk that etching after oxidation of the semiconductor substrate directly below the metal film 44 will not be performed.
[0064] As shown in FIG. 9(a), the oxidizing agent contained in the solution reacts with the metal film 44, and the nozzle substrate 37 is oxidized by the catalytic action of the material of the metal film 44. As a result, an oxide of the nozzle substrate 37 is formed. As shown by the arrows in FIG. 9(b), the solution moves through the through-holes H of the metal film 44. The solution penetrates between the nozzle substrate 37 and the metal film 44 from the through-holes H. The oxide of the nozzle substrate 37 is dissolved by the hydrogen fluoride contained in the solution that penetrates. As shown in FIG. 9(c), the metal film 44 is adsorbed to the nozzle substrate 37 by the Coulomb force between the metal film 44 and the nozzle substrate 37. The states shown in FIG. 9(a), (b), and (c) are repeated to form holes in the Z1 direction.
[0065] As described above, the manufacturing method of the nozzle substrate 37 includes a first step S1 of forming the nozzle N by metal-assisted chemical etching. In the first step S1, the metal film 44 is formed on a first portion 3011 corresponding to the nozzle N of the first surface 301 of the nozzle substrate 37, and the metal-assisted chemical etching is performed in a state in which the metal film 44 is not formed on a second portion 3012 of the first surface 301 that does not correspond to the nozzle N.
[0066] By using metal-assisted chemical etching, fine processing is possible, and the nozzle N can be formed with high precision. In addition, dry etching requires processing one by one, and the processing time for one sheet may be enormous, but metal-assisted chemical etching allows batch processing in which a large number of sheets can be processed in one etching tank, so the processing time is significantly reduced. In addition, it is difficult to control the aspect ratio of the nozzle N with anisotropic wet etching along the crystal orientation, but metal-assisted chemical etching makes it easy to form a nozzle N with a desired aspect ratio. Therefore, by using metal-assisted chemical etching, the nozzle N can be formed with high precision. Therefore, the nozzle N with the desired shape can be realized. Specifically, as described above, the nozzle N including the tapered hole portion N1 and the cylindrical hole portion N2 can be realized. Therefore, the nozzle substrate 37 with excellent ejection performance can be obtained. Therefore, the liquid ejection head 3 with excellent printing quality can be provided.
[0067] The nozzle substrate 37 formed by this method has an extremely high air bubble discharge performance, and can significantly reduce excess ink consumption for air bubble discharge. On the other hand, the flow path resistance is reduced and the ink speed is increased, which improves the accuracy of the ink landing position, making it easy to realize high-definition images.
[0068] As described above, the first step S1 includes a resist layer forming step S10, a resist layer patterning step S11, and a metal film forming step S12. In the resist layer forming step S10, a resist layer 43 is formed on the first surface 301 of the nozzle substrate 37. In the resist layer patterning step S11, after forming the resist layer 43, the resist layer 43 is patterned so as to open in the first portion 3011 and not to open in the second portion 3012. In the metal film forming step S12, after patterning the resist layer 43, a metal film 44 is formed on the first surface 301.
[0069] By using the patterned resist layer 43, it is easy to form the metal film 44 corresponding to the first portion 3011. That is, the metal film 44 can be easily formed at a desired location. Furthermore, when the metal film 44 is formed by electroless plating as in this embodiment, the patterned resist layer 43 can be suitably used as a mask.
[0070] In addition, in the first step S1, it is preferable to perform metal-assisted chemical etching using a solution containing hydrogen fluoride and an oxidizing agent. By using hydrogen fluoride, it is easy to remove oxides from the nozzle substrate 37 by etching. By using an oxidizing agent, it is possible to react with the metal film 44 and oxidize the nozzle substrate 37. Therefore, the metal-assisted chemical etching can be performed efficiently.
[0071] The oxidizing agent is not particularly limited, but examples thereof include hydrogen peroxide (H2O2), nitric acid (HNO3), potassium persulfate (KHSO5), potassium permanganate (KMnO4), and the like. In particular, in this embodiment, the nozzle substrate 37 is a silicon substrate. In this case, for efficient formation of an oxide on the nozzle substrate 37, it is preferable that the oxidizing agent is hydrogen peroxide. Note that the type of solution is not limited to one containing hydrogen fluoride and an oxidizing agent.
[0072] As described above, the metal film 44 includes, for example, platinum, gold, silver, ruthenium, platinum, palladium, molybdenum, chromium, copper, tantalum, titanium, or iridium. Of these, the metal film 44 is preferably made of gold. This is because gold is particularly excellent in catalytic reactions and can be easily removed by etching or other processes. Furthermore, when the oxidizing agent contained in the solution is hydrogen peroxide, not only can the catalytic reaction of gold be favorably exhibited, but the solution does not turn into a solid powder even when it dries, and the yield is not reduced due to particle scattering, making it suitable for precision processing.
[0073] FIG. 10 is a diagram for explaining the first metal-assisted chemical etching step S13 in FIG. 6. The oxidizing agent generates holes H0 due to the catalytic action of the metal film 44. The holes H0 oxidize the nozzle substrate 37 directly below the metal film 44, but some of them diffuse inside the nozzle substrate 37 and reach the surface of the nozzle substrate 37, oxidizing that part of the nozzle substrate 37, and are etched by hydrogen fluoride. The amount of etching increases closer to the metal film 44 and decreases farther away. As described above, the taper angle θ of the tapered hole portion N1 of the nozzle N can be adjusted by the ratio of hydrogen fluoride and oxidizing agent contained in the solution. Since the taper angle θ can be adjusted by the ratio, it is easy to form the tapered hole portion N1 having the desired taper angle θ. In other words, it is easy to control the taper angle θ with high precision and to increase the yield.
[0074] When the concentration of the oxidizing agent is increased, the taper angle θ increases. This is because the oxidizing agent contained in the solution reacts with the metal film 44 to generate excess holes H0. As shown by the arrow A1 in FIG. 10, the holes H0 generated from the oxidizing agent move inside the nozzle substrate 37, and the part of the nozzle substrate 37 directly below the metal film 44 is oxidized by the oxidizing agent. The excess holes H0 cannot be consumed by the part directly below. For this reason, the holes H0 diffuse inside the nozzle substrate 37 as shown by the arrow A2, and the inner wall surface 303 of the nozzle substrate 37 that is in contact with the solution dissolves. Therefore, as shown by the arrow A3 in FIG. 10, the inner wall surface 303 changes from the state shown by the dashed line to the state shown by the solid line. As a result, the taper angle θ increases.
[0075] The taper angle θ varies depending on the molar concentration volume ratio ρ of hydrogen fluoride to the oxidant. When the oxidant is hydrogen peroxide, the molar concentration volume ratio ρ is expressed by the formula (1). ρ=[HF] / ([HF]+[H2O2]) ···(1)
[0076] In formula (1), [HF] is the molar concentration of hydrogen fluoride contained in the solution. [H2O2] is the molar concentration of hydrogen peroxide solution as an oxidizing agent contained in the solution. The unit of molar concentration is mol / L.
[0077] FIG. 11 is a graph showing the relationship between the molar concentration volume ratio ρ and the taper angle θ. As shown in FIG. 11, there is a relationship between the molar concentration volume ratio ρ and the taper angle θ. FIG. 11 shows an example in which the solution contains hydrogen fluoride and hydrogen peroxide. In this example, if it is desired to increase the taper angle θ, the molar concentration of the oxidizer is increased. If it is desired to decrease the taper angle θ and bring it closer to 0°, the molar concentration of the oxidizer is decreased.
[0078] The molar concentration volume ratio ρ preferably satisfies, for example, 0.47≦[HF] / ([HF]+[H2O2])≦0.78. When the solution contains hydrogen fluoride and hydrogen peroxide, the molar concentration volume ratio ρ being within the above range makes it possible to obtain a tapered hole portion N1 with a taper angle θ of 4° or more and 20° or less. This makes it possible to suppress a decrease in ink speed and to suppress the risk of the meniscus becoming unstable. As a result, it is possible to provide a nozzle substrate 37 with excellent ejection performance.
[0079] It is more preferable that the molar concentration volume ratio ρ satisfies, for example, 0.56≦[HF] / ([HF]+[H2O2])≦0.71. When the solution contains hydrogen fluoride and hydrogen peroxide, the molar concentration volume ratio ρ being within the above range makes it possible to obtain a tapered hole portion N1 with a taper angle θ of 6° or more and 12° or less. This makes it possible to provide a nozzle substrate 37 with even better ejection performance.
[0080] As described above, when the taper angle θ is to be increased, the molar concentration of the oxidizer is increased, and when the taper angle θ is to be close to 0°, the molar concentration of the oxidizer is decreased. Therefore, the molar concentration volume ratio ρ is larger when the first metal-assisted chemical etching is performed than when the second metal-assisted chemical etching is performed. By changing the molar concentration volume ratio ρ between the first metal-assisted chemical etching and the second metal-assisted chemical etching, the tapered hole portion N1 and the cylindrical hole portion N2 can be formed continuously. Therefore, the risk of a step occurring between the tapered hole portion N1 and the cylindrical hole portion N2 can be suppressed. Therefore, it is easy to avoid the occurrence of turbulence of the ink and stagnation of the ink flow. As a result, the risk of problems with print quality such as missing dots can be suppressed.
[0081] For example, when the solution contains hydrogen fluoride and hydrogen peroxide, a tapered hole portion N1 with a taper angle of 8° can be obtained by using a solution containing 7.4 mol / L of hydrogen fluoride and 3.9 mol / L of hydrogen peroxide.
[0082] 2. Second embodiment The second embodiment will be described below. In the following example, for elements having the same actions and functions as those in the first embodiment, the reference numerals used in the description of the first embodiment will be used and detailed descriptions of each will be omitted as appropriate.
[0083] Fig. 12 is a diagram for explaining the first step S1 of the second embodiment. As shown in Fig. 12, the first step S1 of the present embodiment further includes an oxide film forming step S17, a protective film forming step S18, an oxide film etching step S19, and a resist layer removing step S20.
[0084] FIG. 13 is a diagram for explaining the oxide film forming step S17 to the resist layer patterning step S11 in FIG. 12. FIG. 13(a) is a diagram for explaining the oxide film forming step S17. As shown in FIG. 13(a), in the oxide film forming step S17, an oxide film 41 is formed on the first surface 301 of the nozzle substrate 37. The oxide film 41 is specifically a silicon oxide film. For example, the oxide film 41 is formed by a CVD (chemical vapor deposition) method or thermal oxidation. The thickness of the oxide film 41 is not particularly limited, but is, for example, 0.2 μm or more and 1.0 μm or less.
[0085] Fig. 13(b) is a diagram for explaining the protective film forming step S18. As shown in Fig. 13(b), in the protective film forming step S18, a protective film 42 is formed on the second surface 302 of the nozzle substrate 37. The protective film 42 is made of, for example, diamond-like carbon or the like. Diamond-like carbon is abbreviated as DLC. For example, the protective film 42 is formed by a CVD method or a sputtering method.
[0086] Fig. 13(c) is a diagram for explaining the resist layer forming step S10. As shown in Fig. 13(c), in the resist layer forming step S10, a resist layer 43 is formed on the first surface 301 of the nozzle substrate 37. Specifically, the resist layer 43 is formed on the oxide film 41 formed on the first surface 301.
[0087] 13(d) and 13(e) are diagrams for explaining the resist layer patterning step S11. As shown in FIG. 13(d), in the resist layer patterning step S11, the resist layer 43 is patterned so as to have an opening in the first portion 3011 and not to have an opening in the second portion 3012.
[0088] 13(e), reflow baking is performed after the resist layer 43 is patterned. As a result, the surface of the patterned resist layer 43 in the Z2 direction is narrower than the surface in the Z1 direction due to surface tension.
[0089] FIG. 14 is a diagram for explaining the oxide film etching step S19 to the second metal-assisted chemical etching step S14 in FIG.
[0090] Fig. 14(a) is a diagram for explaining the oxide film etching step S19. As shown in Fig. 14(a), in the oxide film etching step S19, a part of the oxide film 41 is removed by etching, thereby patterning the oxide film 41. For example, the part of the oxide film 41 is removed by wet etching using buffered hydrofluoric acid, using a resist layer 43 as a mask. Buffered hydrofluoric acid is abbreviated as BHF.
[0091] In the oxide film etching step S19, a gap G is formed between the first surface 301 and the resist layer 43. That is, in the oxide film etching step S19, a part of the oxide film 41 is removed to such an extent that the gap G is formed. When the nozzle substrate 37 contains silicon, the gap G is easily formed by performing wet etching using hydrofluoric acid. Furthermore, by forming the gap G, the patterned oxide film 41 is covered with the patterned resist layer 43 in a plan view.
[0092] Fig. 14(b) is a diagram for explaining the metal film forming step S12. As shown in Fig. 14(b), in the metal film forming step S12, a metal film 44 is formed on the first surface 301 of the nozzle substrate 37. Specifically, the metal film 44 is formed on the resist layer 43 on the first surface 301.
[0093] As described above, the oxide film 41 is provided between the first surface 301 and the resist layer 43. Furthermore, a gap G is formed between the first surface 301 and the resist layer 43. Therefore, the metal film 44 includes a portion 441 in contact with the first surface 301 and a portion 442 in contact with the resist layer 43. The portion 441 and the portion 442 are not continuous but separated.
[0094] Fig. 14(c) is a diagram for explaining the resist layer removal step S20. As shown in Fig. 9(c), in the resist layer removal step S20, the resist layer 43 is removed. Along with this removal, the portions 442 of the metal film 44 in contact with the resist layer 43 are also removed at the same time. As a result, the metal film 44 composed of a plurality of portions 441 is formed on the first surface 301.
[0095] In this step, the metal film 44 is formed on the first portion 3011, but is not formed on the second portion 3012. Therefore, the metal film 44 overlaps the first portion 3011, but does not overlap the second portion 3012, in a plan view.
[0096] Fig. 14(d) is a diagram for explaining the first metal-assisted chemical etching step S13. As shown in Fig. 14(d), in the first metal-assisted chemical etching step S13, a portion of the nozzle substrate 37 is removed by the first metal-assisted chemical etching to form a tapered hole portion N1.
[0097] Fig. 14(e) is a diagram for explaining the second metal-assisted chemical etching step S14. As shown in Fig. 14(e), a cylindrical hole portion N2 is formed by removing a part of the nozzle substrate 37 by the second metal-assisted chemical etching. The first metal-assisted chemical etching step S13 and the second metal-assisted chemical etching step S14 are performed successively.
[0098] Although not shown, the removal step S15 is performed after the second metal-assisted chemical etching step S14. In the removal step S15, the oxide film 41, the protective film 42, and the metal film 44 are removed. The protective film 42 is removed by, for example, plasma ashing. After the removal step S15, the polishing step S16 is performed. In the polishing step S16, the second surface 302 of the nozzle substrate 37 is polished to remove a portion of the nozzle substrate 37. As a result, a nozzle N including a tapered hole portion N1 and a cylindrical hole portion N2 is formed.
[0099] As described above, the first step S1 of this embodiment includes an oxide film forming step S17 and an oxide film etching step S19. In the oxide film forming step S17, an oxide film 41 is formed on the first surface 301 before forming the resist layer 43. Then, in the resist layer forming step S10, a resist layer 43 is formed on the oxide film 41. In addition, in the oxide film etching step S19, after patterning the resist layer 43 and before forming the metal film 44, the oxide film 41 is etched to open a portion of the oxide film 41 above the first portion 3011.
[0100] In this method, the metal film 44 is formed without using the electroless plating of the first embodiment. In this embodiment, the oxide film 41 is formed between the first surface 301 and the resist layer 43, which makes it easy to pattern the metal film 44 in a later step. In addition, the method of this embodiment is excellent in stability in mass production. Therefore, the yield can be improved. Specifically, since the resist layer 43 and the oxide film 41 each have an opening in the first portion 3011, it is easy to form the metal film 44 corresponding to the first portion 3011, as described above.
[0101] Furthermore, in the oxide film etching step S19, the oxide film 41 is etched to form a gap G between the first surface 301 and the resist layer 43. The formation of the gap G makes it easier to pattern the metal film 44 in a later step compared to when the gap G is not formed. The provision of the gap G makes it easier to divide the metal film 44 into a portion 441 in contact with the first surface 301 and a portion 442 in contact with the resist layer 43 compared to when the gap G is not formed. Therefore, it is easier to form the metal film 44 including the portion 441 in contact with the desired first portion 3011.
[0102] The first step S1 includes a resist layer removal step S20. In the resist layer removal step S20, after forming the metal film 44 on the first surface 301, the resist layer 43 is removed. By removing the resist layer 43, the portion 442 can be removed, and thus the metal film 44 composed of the portion 441 is formed on the first surface 301. This makes it possible to easily form a patterned metal film 44. Even if the metal film 44 has a fine shape, this method makes it possible to easily and highly accurately form the metal film 44 having a desired shape and arrangement pattern with a high yield.
[0103] In this embodiment, the nozzle N is formed by metal-assisted chemical etching, as in the first embodiment. Therefore, a nozzle N having a desired shape can be realized. Specifically, as described above, a nozzle N including a tapered hole portion N1 and a cylindrical hole portion N2 can be realized. Therefore, a nozzle substrate 37 with excellent ejection performance can be obtained. Thus, a liquid ejection head 3 with excellent print quality can be provided.
[0104] 3. Third embodiment The third embodiment will be described below. In the following exemplary embodiment, for elements having the same actions and functions as those in the first embodiment, the reference numerals used in the description of the first embodiment will be used and detailed descriptions of each will be omitted as appropriate.
[0105] Fig. 15 is a diagram showing the flow of a manufacturing method of a nozzle substrate 37 of the third embodiment. As shown in Fig. 15, the first step S1 of this embodiment further includes a protective film forming step S18, a resist layer forming step S10, a protective film etching step S21, and a resist layer removing step S20. In this embodiment, an electric field is applied in the second metal-assisted chemical etching step S14.
[0106] FIG. 16 is a diagram for explaining the protective film etching step S21 to the metal film forming step S12 in FIG.
[0107] Fig. 16(a) is a diagram for explaining the protective film forming step S18. As shown in Fig. 16(a), in the protective film forming step S18, a protective film 42 is formed on the first surface 301 of the nozzle substrate 37. Although not shown, the protective film 42 is also formed on the wall surface of the nozzle substrate 37. The protective film 42 is made of, for example, diamond-like carbon. Diamond-like carbon is abbreviated as DLC. For example, the protective film 42 is formed by a CVD method or a sputtering method. The thickness of the protective film 42 is not particularly limited, but is, for example, 0.1 μm or more and 0.5 μm or less.
[0108] Fig. 16(b) is a diagram for explaining the resist layer forming step S10. As shown in Fig. 16(b), in the resist layer forming step S10, a resist layer 43 is formed on the first surface 301 of the nozzle substrate 37. Specifically, the resist layer 43 is formed on the protective film 42 formed on the first surface 301.
[0109] Fig. 16(c) is a diagram for explaining the resist layer patterning step S11. As shown in Fig. 16(d), in the resist layer patterning step S11, the resist layer 43 is patterned so as to have an opening in the first portion 3011 and not to have an opening in the second portion 3012.
[0110] Fig. 16(d) is a diagram for explaining the protective film etching step S21. As shown in Fig. 16(d), in the protective film etching step S21, the protective film 42 is patterned so as to open the first portion 3011 and not open the second portion 3012, similarly to the resist layer 43 in the resist layer patterning step S11. When the protective film 42 is made of diamond-like carbon, the protective film 42 is patterned by etching using oxygen plasma.
[0111] Fig. 16(e) is a diagram for explaining the metal film forming step S12. As shown in Fig. 16(e), in the metal film forming step S12, a metal film 44 is formed on the first surface 301 of the nozzle substrate 37. Specifically, the metal film 44 is formed on the resist layer 43 on the first surface 301. The metal film 44 includes a portion 441 that contacts the first surface 301 and a portion 442 that contacts the resist layer 43. Since the protective film 42 is provided between the first surface 301 and the resist layer 43, the portion 441 and the portion 442 are not continuous but are separated.
[0112] 17 is a diagram for explaining the resist layer removal step S20 to the second metal-assisted chemical etching step S14 in FIG. 15. FIG. 17(a) is a diagram for explaining the resist layer removal step S20. As shown in FIG. 17(a), in the resist layer removal step S20, the resist layer 43 is removed. Along with this removal, the portion 442 of the metal film 44 in contact with the resist layer 43 is also removed at the same time. As a result, the metal film 44 composed of a plurality of portions 441 is formed on the first surface 301.
[0113] Fig. 17(b) is a diagram for explaining the first metal-assisted chemical etching step S13. As shown in Fig. 17(b), in the first metal-assisted chemical etching step S13, a portion of the nozzle substrate 37 is removed by the first metal-assisted chemical etching to form a tapered hole portion N1.
[0114] Fig. 17(c) is a diagram for explaining the second metal-assisted chemical etching step S14. As shown in Fig. 17(c), a cylindrical hole portion N2 is formed by removing a part of the nozzle substrate 37 by the second metal-assisted chemical etching. The first metal-assisted chemical etching step S13 and the second metal-assisted chemical etching step S14 are performed successively.
[0115] Although not shown, the removal step S15 is performed after the second metal-assisted chemical etching step S14. In the removal step S15, the oxide film 41, the protective film 42, and the metal film 44 are removed. The protective film 42 is removed by, for example, plasma ashing.
[0116] After the removing step S15, a polishing step S16 is performed. In the polishing step S16, the second surface 302 of the nozzle substrate 37 is polished to remove a portion of the nozzle substrate 37. As a result, a nozzle N including a tapered hole portion N1 and a cylindrical hole portion N2 is formed.
[0117] In this embodiment, the nozzle N is formed by metal-assisted chemical etching, as in the first embodiment. Therefore, a nozzle N having a desired shape can be realized. Specifically, as described above, a nozzle N including a tapered hole portion N1 and a cylindrical hole portion N2 can be realized. Therefore, a nozzle substrate 37 with excellent ejection performance can be obtained. Thus, a liquid ejection head 3 with excellent print quality can be provided.
[0118] In addition, in this embodiment, the application of an electric field is used in the metal-assisted chemical etching. Specifically, when the first metal-assisted chemical etching is performed, an electric field is not applied to the solution, and when the second metal-assisted chemical etching is performed, an electric field is applied to the solution. By applying an electric field in this manner, the holes H0 that are generated in excess and form a taper are sucked to the back surface, thereby preventing the taper formation, and the application of an electric field can prevent the taper without the need to replace the etching solution with a different composition. The advantage of this method is that, compared to the case where an electric field is not applied, the formation of the tapered hole portion N1 and the formation of the cylindrical hole portion N2 can be easily and continuously performed.
[0119] Fig. 18 is a cross-sectional view showing a jig 5 used in the first metal-assisted chemical etching step S13. Fig. 19 is a view for explaining the first metal-assisted chemical etching step S13.
[0120] The jig 5 shown in FIG. 18 is used to fix the nozzle substrate 37 in the first metal-assisted chemical etching step S13. The jig 5 includes a base 51, a first member 52, a second member 53, two screws 520 and 530, a plurality of gaskets 54, and an electrode 55. The base 51 is a flat plate-shaped member and has two holes through which the two screws 520 and 530 pass. The first member 52 is a clamp that sandwiches the nozzle substrate 37 and fixes it to the base 51 with the screw 520. The second member 53 is disposed opposite the first member 52. The second member 53 is a clamp that sandwiches the nozzle substrate 37 and fixes it to the base 51 with the screw 530. Each of the first member 52 and the second member 53 is provided with a plurality of gaskets 54. The nozzle substrate 37 is sandwiched between a first member 52 and a second member 53 via a plurality of packings 54 and fixed by screws 520 and 530.
[0121] An electrode 55 is disposed between the second member 53 and the base 51. The electrode 55 is fixed in a state in which it is sandwiched between the second member 53 and the base 51 by a screw 530. A tip portion 550 of the electrode 55 is in contact with the second surface 302 of the nozzle substrate 37.
[0122] In this embodiment, the second surface 302 of the nozzle substrate 37 is not covered with the protective film 42 or the resist layer 43. In this case, the second surface 302 is protected by a plurality of packings 54 so that the solution does not penetrate into the second surface 302 during metal-assisted chemical etching.
[0123] As shown in FIG. 19, in the first metal-assisted chemical etching step S13, a solution 6 is contained in an etching solution tank 50. The jig 5 holding the nozzle substrate 37 is placed in the etching solution tank 50 so as to be immersed in the solution 6. In addition, the working electrode 56 is placed in the etching solution tank 50 so as to be immersed in the solution 6. As the working electrode 56, for example, a platinum mesh electrode is used. The working electrode 56 faces the first surface 301 of the nozzle substrate 37. In addition, the negative side of a DC power supply is attached to the electrode 55, and the positive side of the DC power supply is attached to the working electrode 56. In this state, the first metal-assisted chemical etching step S13 is performed.
[0124] Fig. 20 is a diagram for explaining the first metal-assisted chemical etching step S13, and Fig. 21 is a diagram for explaining the second metal-assisted chemical etching step S14.
[0125] As shown in FIG. 20, in the first metal-assisted chemical etching step S13, the switch 57 is turned off and no electric field is applied to the solution. In this case, holes H0 generated from the oxidizing agent move inside the nozzle substrate 37 as shown by the arrow A1, and the part of the nozzle substrate 37 directly below the metal film 44 is oxidized by the oxidizing agent. In addition, the holes H0 diffuse through the nozzle substrate 37 as shown by the arrow A2, and the inner wall surface 303 of the nozzle substrate 37 that is in contact with the solution is dissolved. Therefore, as shown by the arrow A3, the inner wall surface 303 changes from the state shown by the dashed line to the state shown by the solid line. As a result, in the first metal-assisted chemical etching step S13, a tapered hole portion N1 having a taper angle θ is formed. In addition, in the first metal-assisted chemical etching step S13, the molar concentration volume ratio ρ of the solution 6 in the etching solution tank 50 is set to a desired taper angle θ.
[0126] As shown in FIG. 21, in the second metal-assisted chemical etching step S14, switch 57 is turned on and an electric field is applied to the solution. In this case, no taper is formed, and a straight hole is formed. The hole constitutes a cylindrical hole portion N2. For example, by applying a voltage of 4V or more and 8V or less, a cylindrical hole portion N2 that is a straight hole can be formed.
[0127] When a voltage is applied, the positively charged holes H0 are attracted to the second surface 302 of the nozzle substrate 37 to which a negative voltage is applied, as indicated by the arrow A1. This prevents the holes H0 from diffusing and reaching the inner wall surface 303. As a result, the holes H0 are attracted to the second surface 302, and a straight hole is formed without being tapered.
[0128] As described above, in a state where the molar concentration volume ratio ρ of the solution 6 in the etching solution tank 50 is set to a desired taper angle θ, the formation of the tapered hole portion N1 and the formation of the cylindrical hole portion N2 can be easily switched by switching on and off the electric field of the solution 6. Therefore, it is not necessary to prepare a separate solution with an adjusted molar concentration volume ratio ρ for forming the cylindrical hole portion N2 in an etching solution tank other than the etching solution tank 50. Therefore, the second metal-assisted chemical etching step S14 can be started quickly. In addition, according to the method of this embodiment, the formation of the tapered hole portion N1 and the formation of the cylindrical hole portion N2 can be manufactured in one etching solution tank 50. Therefore, the amount of solution used can be reduced, and costs can be reduced.
[0129] 4. Manufacturing method of liquid ejection head 3 22 is a diagram showing the flow of a manufacturing method for the liquid ejection head 3. As described above, the liquid ejection head 3 has a pressure chamber substrate 32 including the pressure chambers C1, a communication plate 31 laminated on the pressure chamber substrate 32, and a nozzle substrate 37 including the nozzles N and laminated on the communication plate 31. In the example of the first embodiment, the nozzle substrate 37 is made of a semiconductor substrate.
[0130] In the example shown in FIG. 22, in step SS1, a pressure chamber substrate wafer including a plurality of pressure chamber substrates 32, a nozzle substrate wafer including a plurality of nozzle substrates 37, and a communicating plate wafer including a plurality of communicating plates 31 are each individually formed. In step SS2, these wafers are directly bonded. Thereafter, a liquid protective layer is formed on the wall surfaces that form each flow path. The liquid protective layer may be formed before the direct bonding. Also, in step SS3, a sealing substrate wafer including a plurality of sealing substrates 35 is formed, and a liquid protective layer is formed on each flow path including the communicating space Ra, etc.
[0131] The liquid protective layer includes, for example, tantalum oxide or hafnium oxide. The chemical formula of tantalum oxide is represented by TaOx. The chemical formula of hafnium oxide is represented by HfOx. The liquid protective layer is formed, for example, by an ALD (Atomic Layer Deposition) method.
[0132] In step SS4, a sealing substrate wafer is bonded to the pressure chamber substrate wafer, nozzle substrate wafer, and communicating plate wafer to manufacture a structure including these wafers. In step SS5, the structure is cut into chips by laser scrubbing or the like. In step SS6, the chips are mounted on the mounting pads by COF. COF stands for Chip On Film. Then, in step SS7, the vibration absorber 38, housing 36, and case components such as ink piping components are assembled by bonding or the like. This results in the liquid ejection head 3.
[0133] 5. Variations The above-described embodiment may be modified in various ways. Specific modified aspects that may be applied to the above-described embodiment are illustrated below. Two or more aspects selected from the following examples may be combined as appropriate to the extent that they are not mutually contradictory.
[0134] The liquid ejection device 1 exemplified in the first embodiment can be adopted in various devices such as facsimile machines and copy machines, in addition to devices dedicated to printing. The use of the liquid ejection device is not limited to printing. For example, a liquid ejection device that ejects a solution of a color material is used as a manufacturing device that forms a color filter of a display device such as a liquid crystal display panel. Also, a liquid ejection device that ejects a solution of a conductive material is used as a manufacturing device that forms wiring and electrodes of a wiring board. Also, a liquid ejection device that ejects a solution of an organic matter related to a living body is used as a manufacturing device that manufactures, for example, a biochip.
[0135] In the above embodiment, the nozzle substrate 37 is a P-type single crystal silicon substrate, but it may be made of any other material as long as it contains a semiconductor material. Also, the nozzle N has a tapered hole portion N1, but the nozzle N may be made of only a straight hole. [Explanation of symbols]
[0136] 1...liquid ejection device, 3...liquid ejection head, 5...jig, 6...solution, 12...medium, 14...container, 20...control unit, 22...transport mechanism, 24...movement mechanism, 30...flow path structure, 31...communicating plate, 32...pressure chamber substrate, 33...vibration plate, 34...piezoelectric element, 35...sealing substrate, 36...casing, 37...nozzle substrate, 38...vibration absorber, 40...wiring substrate, 41...oxide film, 42...protective film, 43...resist layer, 44...metal film, 50...etching liquid tank , 51...base, 52...first member, 53...second member, 54...packing, 55...electrode, 56...working electrode, 57...switch, 242...conveyor, 244...conveyor belt, 300...individual flow path, 301...first surface, 302...second surface, 303...inner wall surface, 312...throttling portion, 314...communicating flow path, 320...wall surface, 361...supply port, 441...portion, 442...portion, 520...screw, 530...screw, 550...tip portion, 3011...first portion, 3012... Second part, A0...normal line, A1...arrow, A2...arrow, A3...arrow, C1...pressure chamber, G...gap, H...through hole, H0...hole, La...first row, Lb...second row, N...nozzle, N1...tapered hole portion, N2...cylindrical hole portion, R...common space, Ra...communicating space, Rb...common flow path, Rc...space, S1...first step, S10...resist layer forming step, S11...resist layer patterning step, S12...metal film forming step, S13...first metal assisted chemical etching S13...etching step, S14...second metal-assisted chemical etching step, S15...removal step, S16...polishing step, S17...oxide film formation step, S18...protective film formation step, S19...oxide film etching step, S20...resist layer removal step, S21...protective film etching step, SS1...step, SS2...step, SS3...step, SS4...step, SS5...step, SS6...step, SS7...step, θ...taper angle.
Claims
1. A method for manufacturing a liquid ejection head including a pressure chamber substrate including pressure chambers, and a nozzle substrate including nozzles communicating with the pressure chambers and formed of a semiconductor substrate, comprising: A method for manufacturing a liquid ejection head, comprising: a first step of forming the nozzle by performing metal-assisted chemical etching in a state in which a metal film is formed on the nozzle substrate in a first portion of a first surface, which is the surface of the nozzle substrate facing the pressure chamber substrate, and in which the metal film is not formed on the nozzle substrate in a second portion of the first surface not corresponding to the nozzle.
2. The first step comprises: forming a resist layer on the first surface; After forming the resist layer, the resist layer is patterned so as to have an opening in the first portion and no opening in the second portion; forming the metal film on the first surface after patterning the resist layer; 2. The method for manufacturing a liquid ejection head according to claim 1.
3. forming an oxide film on the first surface before forming the resist layer; forming a resist layer on the oxide film; after patterning the resist layer and before forming the metal film, etching the oxide film to open a portion of the oxide film above the first portion; 3. The method for manufacturing a liquid ejection head according to claim 2.
4. forming a gap between the first surface and the resist layer by etching the oxide film; 4. The method for manufacturing a liquid ejection head according to claim 3.
5. In the first step, After forming the metal film on the first surface, the resist layer is removed.
3. The method for manufacturing a liquid ejection head according to claim 2.
6. In the first step, the metal-assisted chemical etching is performed using a solution containing hydrogen fluoride and an oxidizing agent.
2. The method for manufacturing a liquid ejection head according to claim 1.
7. In the first step, a taper angle of the nozzle is adjusted according to a ratio of the hydrogen fluoride to the oxidizing agent.
7. The method for manufacturing a liquid ejection head according to claim 6.
8. The oxidizing agent is hydrogen peroxide.
7. The method for manufacturing a liquid ejection head according to claim 6.
9. In the first step, the molar concentration of the hydrogen fluoride is [HF], the molar concentration of the oxidizing agent is [H 2 O 2 ], 0.47≦[HF] / ([HF]+[H 2 O 2 ])≦0.78; 9. The method for manufacturing a liquid ejection head according to claim 8.
10. In the first step, 0.56≦[HF] / ([HF]+[H 2 O 2 ])≦0.71; 9. The method for manufacturing a liquid ejection head according to claim 8.
11. In the first step, the metal-assisted chemical etching includes a first metal-assisted chemical etching and a second metal-assisted chemical etching subsequent to the first metal-assisted chemical etching; The molar concentration of the hydrogen fluoride is [HF], and the molar concentration of the oxidizing agent is [H 2 O 2 ], the ratio of [HF] / ([HF]+[H 2 O 2 ]) is large, 9. The method for manufacturing a liquid ejection head according to claim 8.
12. In the first step, the metal-assisted chemical etching includes a first metal-assisted chemical etching and a second metal-assisted chemical etching subsequent to the first metal-assisted chemical etching; When performing the first metal-assisted chemical etching, no electric field is applied to the solution, and when performing the second metal-assisted chemical etching, an electric field is applied to the solution.
7. The method for manufacturing a liquid ejection head according to claim 6.
13. The metal film is made of gold.
2. The method for manufacturing a liquid ejection head according to claim 1.
14. A method for manufacturing a nozzle substrate including a nozzle and formed of a semiconductor substrate, comprising: a first step of forming the nozzle by performing metal-assisted chemical etching in a state in which a metal film is formed on the nozzle substrate in a first portion of a first surface of the nozzle substrate corresponding to the nozzle, and in a second portion of the first surface not corresponding to the nozzle, the metal film is not formed on the nozzle substrate; A method for manufacturing a nozzle substrate comprising the steps of:
15. a pressure chamber substrate including a pressure chamber; a nozzle substrate including a nozzle communicating with the pressure chamber, The nozzle substrate is a p-type semiconductor substrate, The nozzle includes a tapered hole portion having a taper angle of 4 to 20 degrees. A liquid ejection head comprising:
Citation Information
Patent Citations
Droplet ejection head and droplet ejection device
JP2022025115A