Sensor element and sensor element manufacturing method
The sensor element's innovative design with a cavity, convex, and thin portions in the protective layer addresses inefficiencies in existing designs, enhancing protection and responsiveness by optimizing thickness distribution.
Patent Information
- Application Number
- JP2023054709
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
AI Technical Summary
Existing sensor elements with porous protective layers are inefficient in protecting the tip portion of the main body, leading to increased power consumption, prolonged gas diffusion time, and reduced responsiveness due to the need for a thicker protective layer.
A sensor element design featuring a cavity on the distal end with a porous protective layer that includes a water droplet blocking structure and a thin portion, where the thin portion is positioned away from the cavity's longitudinal extension, and a convex portion covering the cavity, reducing heat capacity and enhancing responsiveness.
The design effectively protects the sensor element from thermal shock while minimizing power consumption and improving responsiveness by optimizing the protective layer's thickness distribution.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a sensor element for detecting a gas component and a method for manufacturing the sensor element. [Background technology]
[0002] A sensor element made of ceramics is used to detect the concentration of gas components such as NOx or oxygen. Such a sensor element is used at high temperatures. If water droplets adhere to the body of a high-temperature sensor element, the body may be damaged by thermal shock.
[0003] Patent Document 1 discloses a sensor element in which the periphery of the main body is covered with a porous protective layer to protect the main body from thermal shock.
[0004] Patent Document 2 also discloses a sensor element whose main body is covered with a porous protective layer. This porous protective layer has recesses on its surface that capture water droplets. The recesses quickly dry the water droplets and prevent damage to the porous protective layer.
[0005] Patent Document 3 also discloses a sensor element whose main body is covered with a porous protective layer. Patent Document 3 discloses a porous protective layer in which the thickness of the corners that are vulnerable to water droplets is increased in order to prevent damage to the porous protective layer from water droplets. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2016-109685 A [Patent Document 2] JP 2009-080111 A [Patent Document 3] JP 2019-039693 A Summary of the Invention [Problem to be solved by the invention]
[0007] However, the sensor elements of Patent Documents 1 to 3 cannot effectively protect the most vulnerable part, the tip part of the body, and therefore require a thick porous protective layer. A thick porous protective layer requires a long time to produce, and causes problems such as increased power consumption at start-up due to increased heat capacity and poor response of the sensor element due to increased gas diffusion time.
[0008] An object of the present invention is to solve the above-mentioned problems. [Means for solving the problem]
[0009] [Item 1] One aspect of the present invention is a sensor element comprising a body having a cavity at the tip side for taking in gas, and a porous protective layer covering the outer peripheral surface at the tip side of the body, the porous protective layer comprising a water droplet blocking structure covering at least a portion of the tip surface of the body overlapping with the cavity in a longitudinal direction perpendicular to the tip surface, and a thin portion covering the tip surface around the water droplet blocking structure. The sensor element described above protects the portion of the tip surface of the body where stress is concentrated and the tip surface is most likely to break, overlapping with the cavity in the longitudinal direction with the water droplet blocking structure, and provides a thin portion around the water droplet blocking structure, thereby efficiently protecting the necessary portion with the porous protective layer. As a result, the sensor element can reduce the heat capacity of the tip and improve the responsiveness of the sensor element. [Item 2] In the sensor element according to item 1, the cavity may extend along the longitudinal direction, and the water droplet prevention structure may be a convex portion of the porous protective layer having a thickness greater than that of the thin portion. This sensor element can realize the water droplet prevention structure with the simplest structure. [Item 3] In the sensor element according to item 1 or 2, the main body may be formed in a rectangular parallelepiped shape extending long in the longitudinal direction, and the main body may have a flat plate shape in which a dimension in a width direction perpendicular to the longitudinal direction is larger than a dimension in a thickness direction perpendicular to the longitudinal direction and the width direction, and the water droplet prevention structure may be located in the center of the width direction and the thickness direction on the tip surface. [Item 4] In the sensor element according to any one of items 1 to 3, the thin portion may be formed at a position that avoids an extension line of the longitudinal direction of the cavity. This sensor element can prevent damage to the body due to adhesion of water droplets. [Item 5] In the sensor element according to any one of items 1 to 4, a ratio B / A of a difference B between a thickness C of the thin portion and a thickness A of the water droplet prevention structure to the thickness A of the water droplet prevention structure may be in a range of 0.05 to 0.6. This sensor element can achieve both productivity of the porous protective layer and resistance to damage to the main body due to adhesion of water droplets. [Item 6] In the sensor element according to any one of items 1 to 4, a ratio B / A of a difference B between a thickness C of the thin portion and a thickness A of the waterdrop prevention structure to the thickness A of the waterdrop prevention structure may be in a range of 0.1 to 0.58. This sensor element is more preferable in terms of productivity and resistance to damage to the body due to adhesion of water droplets. [Item 7] In the sensor element according to any one of items 1 to 6, the cavity may be open to the tip surface. [Item 8] Another aspect of the present invention is a method for manufacturing a sensor element having a body having a cavity at the tip end side for taking in gas components and a porous protective layer covering the outer peripheral surface at the tip end side of the body, the method comprising: a first spraying step of forming the porous protective layer on the side surface of the body by plasma spraying; and a second spraying step of forming the porous protective layer on the tip end surface of the body by plasma spraying, the second spraying step being performed by arranging a spray gun so as to face the tip end surface, and aligning the nozzle center of the spray gun, which has the highest film formation efficiency, on a longitudinal extension line perpendicular to the tip end surface of the cavity, to form the porous protective layer having a thick convex portion covering at least the portion overlapping with the cavity in the longitudinal direction, and a thin portion covering the tip end surface around the convex portion. The above-mentioned method for manufacturing a sensor element can more efficiently manufacture the porous protective layer because it is not necessary to move the nozzle center of the spray gun significantly in the second spraying step. [Item 9] Another aspect of the present invention is a method for manufacturing a sensor element having a body having a cavity at the tip side for taking in gas components and a porous protective layer covering the outer peripheral surface of the tip side of the body, the method comprising: a first spraying step of forming the porous protective layer on the side surface of the body by a spraying method; and a second spraying step of forming the porous protective layer on the tip surface of the body by a spraying method, the second spraying step being performed by arranging a spray gun so as to face the tip surface, and aligning the nozzle center at which the film formation efficiency of the spray gun is highest on a longitudinal extension line perpendicular to the tip surface of the cavity, thereby forming the porous protective layer having a thick convex portion covering at least the portion overlapping with the cavity in the longitudinal direction on the tip surface, and a thin portion covering the tip surface around the convex portion. The above-mentioned method for manufacturing a sensor element can more efficiently manufacture the porous protective layer because it is not necessary to move the nozzle center of the spray gun significantly in the second spraying step. Effect of the Invention
[0010] The above-described sensor element and method of manufacturing the sensor element can make the porous protective layer thin while protecting the main body from thermal shock. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a vertical sectional view of a sensor element according to an embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 3A is an explanatory diagram of the first thermal spraying step, and FIG. 3B is an explanatory diagram of the second thermal spraying step. [Figure 4] FIG. 4 is a schematic cross-sectional view of the sensor element of Comparative Example 1. As shown in FIG. [Diagram 5] FIG. 5A is a schematic cross-sectional view of the sensor elements of Comparative Examples 2 and 3, and FIG. 5B is an explanatory view of the second thermal spraying step of Comparative Examples 2 and 3. [Figure 6] FIG. 6A is a schematic cross-sectional view of a sensor element of Example 1, and FIG. 6B is a schematic cross-sectional view of a sensor element of Example 2. [Figure 7] FIG. 7 is a schematic cross-sectional view of the sensor element of the third embodiment. [Figure 8] FIG. 8 is a table showing the positions of the thin portions of the sensor elements of Comparative Examples 1 to 3 and Examples 1 to 5, the thickness A of the convex portions, the difference B between the thicknesses of the thin portions and the convex portions, the ratio B / A between the difference and the thickness of the convex portions, the evaluation results of water resistance, and the evaluation results of productivity. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The sensor element 10 according to this embodiment shown in FIG. 1 is used in a gas sensor that detects the concentration of a gas component such as NOx in an automobile exhaust gas. The sensor element 10 has a main body 12 and a porous protective layer 14. The main body 12 has a long rectangular parallelepiped shape and extends long in the longitudinal direction, which is the left-right direction of the figure. The main body 12 has a thickness direction in the up-down direction of the figure and a width direction in the direction perpendicular to the paper surface of the figure. The main body 12 has a flat plate shape with the dimension in the thickness direction smaller than the dimension in the width direction. The porous protective layer 14 covers the outer surface near the tip of the main body 12 to protect the main body 12 from thermal shock.
[0013] The main body 12 has a structure in which a plurality of ceramic layers having oxygen ion conductivity, such as zirconia (ZrO2), are laminated. Specifically, the main body 12 has, from the bottom of the figure, a first layer 16, a second layer 18, a third layer 20, a fourth layer 22, and a fifth layer 24. The layers are bonded together and integrated. A wiring pattern is provided at a predetermined location between each layer. The first layer 16 and the second layer 18 of the main body 12 may be made of an insulating material, such as alumina.
[0014] The fourth layer 22 is provided with a cavity 26. The cavity 26 is a hollow portion formed inside the main body 12 to take in and measure the gas components to be measured. The cavity 26 is formed near the tip of the main body 12 (on the left side of the figure). The cavity 26 extends in the longitudinal direction. The cavity 26 introduces the gas to be measured into the main body 12 from an opening 26a. In the illustrated example, the opening 26a is located on the tip surface 12a of the main body 12. The position of the opening 26a of the cavity 26 is not necessarily limited to the tip surface 12a of the main body 12, and may be formed in a portion other than the tip surface 12a, such as a side surface 12b in the width direction of the main body 12. The opening 26a of the cavity 26 is not limited to a hollow portion, and may be a gas inlet such as a porous material.
[0015] The cavity 26 is divided by a plurality of diffusion rate-controlling sections 30. The cavity 26 divided by the diffusion rate-controlling sections 30 constitutes a plurality of chambers 32. The chamber 32 closest to the tip is the gas inlet section 32a, and the second chamber 32 from the tip is the buffer space 32b. The third chamber 32 from the tip is the first chamber 32c, the fourth chamber 32 from the tip is the second chamber 32d, and the fifth chamber 32 from the tip is the third chamber 32e. The first chamber 32c is the chamber 32 in which the oxygen concentration of the inflowing gas component is adjusted. The second chamber 32d is the chamber 32 in which the oxygen concentration of the measured gas component is further reduced. The third chamber 32e is the chamber 32 in which the measured gas component is measured.
[0016] A part of the wiring pattern of the main body 12 constitutes a heater 34, a reference electrode 36, a main pump electrode 38, an auxiliary pump electrode 40, a measurement electrode 42, and an outer electrode 44. The heater 34 is located between the first layer 16 and the second layer 18. The heater 34 generates heat by the supplied current and heats the sensor element 10 to a predetermined operating temperature.
[0017] The reference electrode is located between the second layer 18 and the third layer 20. The reference electrode is in contact with the third layer 20 and is in contact with a reference gas (eg, the atmosphere) through a reference gas inlet .
[0018] The main pump electrode 38 is provided on the inner circumferential surface of the first chamber 32c. The auxiliary pump electrode 40 is provided on the inner circumferential surface of the second chamber 32d. The measurement electrode 42 is located in the third chamber 32e and provided on the third layer 20. The outer electrode 44 is provided on the outer surface of the fifth layer 24. Description of the other electrodes and wiring of the main body 12 is omitted.
[0019] The oxygen partial pressure in the first chamber 32c is detected by the first oxygen detection cell 50. The first oxygen detection cell 50 is an electrochemical cell composed of the main pump electrode 38, the third layer 20, and the reference electrode 36. The first oxygen detection cell 50 generates a potential difference between the main pump electrode 38 and the reference electrode 36 according to the oxygen partial pressure in the first chamber 32c. The oxygen in the first chamber 32c is adjusted by the main pump cell 48. The main pump cell 48 is an electrochemical cell composed of the main pump electrode 38, the fifth layer 24, and the outer electrode 44. The main pump cell 48 introduces oxygen into the first chamber 32c or discharges oxygen from the first chamber 32c through the fifth layer 24. The main pump cell 48 adjusts the oxygen partial pressure in the first chamber 32c to a predetermined value.
[0020] The oxygen partial pressure in the second chamber 32d is detected by a second oxygen detection cell 52. The second oxygen detection cell 52 is composed of an auxiliary pump electrode 40, a third layer 20, and a reference electrode 36. The detection value of the second oxygen detection cell 52 is used to control the auxiliary pump cell 54. The auxiliary pump cell 54 is composed of an auxiliary pump electrode 40, a fifth layer 24, and an outer electrode 44. The auxiliary pump cell 54 exhausts oxygen from inside the second chamber 32d to reduce the oxygen concentration of the internal gas.
[0021] The concentration of the measurement target gas (for example, NO) in the third chamber 32e is detected by the measurement pump cell 56. The measurement pump cell 56 is composed of the measurement electrode 42, the third layer 20, and the reference electrode .
[0022] The porous protective layer 14 covers the outer peripheral surface of the tip side of the main body 12. Specifically, the porous protective layer 14 covers the tip surface 12a located at the tip of the main body 12 and the four side surfaces 12b adjacent to the tip surface 12a. The porous protective layer 14 is formed of a porous body. The porous protective layer 14 has a structure in which ceramic particles are bonded while forming pores. Examples of materials for the porous protective layer 14 include alumina, zirconia, spinel, cordierite, titania, and magnesia. The porosity of the porous protective layer 14 is, for example, 5% by volume to 40% by volume. The porous protective layer 14 may have a multilayer structure having an inner layer 66 (FIG. 7) and an outer layer 68 (FIG. 7) with different porosities. In the multilayer structure of the porous protective layer 14, it is preferable that the inner layer 66 has a larger porosity.
[0023] The porous protective layer 14 of this embodiment has a thin portion 58 and a convex portion 60 (water droplet prevention structure) at the tip portion 14a covering the tip surface 12a. The thin portion 58 is a portion that is relatively thin at the tip portion 14a of the porous protective layer 14 covering the tip surface 12a. The thin portion 58 reduces the amount of the porous protective layer 14, thereby reducing the heat capacity of the porous protective layer 14. In addition, the thin portion 58 shortens the diffusion path of the measurement gas through the porous protective layer 14 required to reach the opening 26a of the cavity 26. Therefore, the thin portion 58 can make the measurement gas reach the cavity 26 more quickly, thereby increasing the response speed of the sensor element 10.
[0024] The thin portion 58 has a lower ability to protect the main body 12 from water droplets than the protruding portion 60. Therefore, the thin portion 58 is formed at a position that avoids the longitudinal extension of the cavity 26, which is a portion of the main body 12 where cracks are relatively unlikely to occur. In other words, the thin portion 58 is formed at a position outside the range surrounded by a line extending in the longitudinal direction of the cavity 26. As shown in Figures 1 and 2, the thin portion 58 is formed near the peripheral portion of the tip surface 12a.
[0025] The protrusion 60 is a portion of the tip 14a that is formed to be relatively thick, and protrudes in a convex shape from the thin portion 58 toward the tip. As shown in Figs. 1 and 2, the protrusion 60 is located at the center in the thickness direction and the center in the width direction of the main body 12. Since the protrusion 60 is thicker than the thin portion 58, it prevents water droplets adhering to the surface from reaching the main body 12. In other words, the protrusion 60 constitutes the water droplet blocking structure of this embodiment.
[0026] In the main body 12, the portion of the cavity 26 on the tip surface 12a that is extended in the longitudinal direction is prone to stress concentration and is prone to breakage due to thermal shock. Similarly, even when the opening 26a of the cavity 26 is formed on the side surface 12b of the main body 12, the longitudinal extension of the cavity 26 on the tip surface 12a is prone to cracking due to stress concentration. Therefore, in this embodiment, a protrusion 60 is provided so as to cover the longitudinal extension of the cavity 26 on the tip surface 12a that is prone to breakage due to thermal shock. As shown in Figures 1 and 2, in this embodiment, the protrusion 60 is located approximately in the center in the width direction and thickness direction so as to cover the tip surface 12a on the longitudinal extension of the cavity 26.
[0027] The thickness A of the protrusion 60 may be, for example, 300 μm or more. The difference B in thickness between the thin portion 58 and the protrusion 60 may be, for example, 5 to 60% of the thickness A of the protrusion 60, more preferably 10 to 58%. That is, the ratio B / A of the difference B to the thickness A is preferably in the range of 0.05 to 0.6, more preferably 0.1 to 0.58. The thickness C of the thin portion 58 may be 40 to 95% of the thickness A of the protrusion 60.
[0028] The sensor element 10 of this embodiment is configured as described above. The sensor element 10 is fabricated by the following method.
[0029] First, the main body 12 is produced by stacking and firing a plurality of green sheets. A method for producing such a main body 12 is described in, for example, JP 2008-164411 A or JP 2009-175099 A.
[0030] Next, the porous protective layer 14 is formed on the surface of the main body 12. The porous protective layer 14 is formed by plasma spraying. The process of forming the porous protective layer 14 includes a first spraying process shown in Fig. 3A and a second spraying process shown in Fig. 3B. As shown in Fig. 3A, the first spraying process is a process of forming the porous protective layer 14 on the four side surfaces 12b of the main body 12.
[0031] In the first spraying step, raw material powder such as alumina powder is sprayed from a plasma spray gun 62 arranged to face the side surface 12b of the main body 12. The plasma spray gun 62 is arranged so that its nozzle center line 63 is perpendicular to the side surface 12b. The nozzle center line 63 is the central axis of the jet of the plasma spray gun 62, and most of the raw material powder is sprayed along the center line. In the first spraying step, the main body 12 is rotated around its longitudinal axis in order to form a porous protective layer 14 of uniform thickness on the four side surfaces 12b. In the first spraying step, the main body 12 moves back and forth in front of the plasma spray gun 62 multiple times.
[0032] 3B, a second spraying process is performed. In the second spraying process, a raw material powder such as alumina powder is sprayed from a plasma spray gun 64 arranged to face the tip surface 12a of the main body 12. The plasma spray gun 64 is arranged so that its nozzle center line 65 faces the longitudinal direction of the main body 12. Furthermore, the plasma spray gun 64 is positioned so that the nozzle center line 65 coincides with the longitudinal extension line of the cavity 26.
[0033] The nozzle center line 65 is the center position of the jet of the plasma spray gun 64, and the density of the raw material powder is the highest. The nozzle center line 65 is the part where the porous protective layer 14 is deposited at the highest speed and the film formation efficiency is the highest. As it moves away from the nozzle center line 65, the density of the raw material powder decreases, and the deposition speed (film formation efficiency) of the porous protective layer 14 decreases. Therefore, when the nozzle center line 65 is aligned with the longitudinal extension line of the cavity 26 (the opening 26a in this embodiment) and sprayed, the protrusion 60 is formed so as to cover the part overlapping with the cavity 26 in the longitudinal direction. In this embodiment, since the cavity 26 is located approximately at the center of the width direction and the thickness direction of the main body 12, the nozzle center line 65 is positioned approximately at the center of the width direction and the thickness direction of the main body 12. In addition, a thin wall portion 58 is formed on the periphery of the protrusion 60. The plasma spray gun 64 may move relative to the body 12 as long as the nozzle centerline 65 does not deviate significantly from the opening 26a of the cavity 26.
[0034] Conventionally, in order to make the porous protective layer 14 of a uniform thickness, it was necessary to uniformize the areas with high film formation efficiency by moving the plasma spray gun 64 or the main body 12, which reduced productivity. In contrast, in the second spraying process, since there is no need to move the plasma spray gun 64 and the film thickness can be non-uniform, the porous protective layer 14 can be formed more efficiently and the plasma spraying can be completed in a shorter time, improving productivity.
[0035] Through the above steps, the sensor element 10 of the present embodiment is completed.
[0036] The manufacturing method of the sensor element 10 of this embodiment can also be performed by a spray method instead of plasma spraying. In this case, a spray gun is used instead of the plasma spray guns 62, 64. In this case, the method may include a first spray step of forming the porous protective layer 14 on the side surface 12b of the main body 12 and a second spray step of forming the porous protective layer 14 on the tip surface 12a of the main body 12. In the second spray step, the center line of the spray gun is positioned at the opening 26a of the cavity 26. As a result, the porous protective layer 14 having the protrusion 60 is formed on the longitudinal extension line of the cavity 26.
[0037] Examples of the sensor element 10 will be described below as examples and comparative examples.
[0038] Comparative Example 1 4, the sensor element 10A of Comparative Example 1 has a porous protective layer 14 formed by a conventional method (Patent Document 1). The porous protective layer 14 of Comparative Example 1 is formed to have a uniform thickness at the tip portion 14a, and does not include portions corresponding to the thin portion 58 and the protruding portion 60. The thickness A of the porous protective layer 14 of Comparative Example 1 at the tip portion 14a was 500 μm.
[0039] (Comparative Examples 2 and 3) As shown in Fig. 5A, the sensor element 10B of Comparative Example 2 has a thin portion 58 and a protruding portion 60 at the tip portion 14a of the porous protective layer 14. However, in the porous protective layers 14 of Comparative Examples 2 and 3, the longitudinal extension line of the cavity 26 (opening 26a) is not covered with the protruding portion 60, but is covered with the thin portion 58. Such a porous protective layer 14 was produced by positioning the nozzle center line 65 of a plasma spray gun 64 at a position different from the extension line of the cavity 26 in the second spraying process shown in Fig. 5B.
[0040] In the porous protective layer 14 of Comparative Example 2, the thickness A of the protrusions 60 was 530 μm. In Comparative Example 2, the difference B in thickness between the thin portion 58 and the protrusions 60 was 130 μm.
[0041] The sensor element 10B of Comparative Example 3 has the same structure as that of Fig. 5A. In the sensor element 10B of Comparative Example 3, the thickness A of the protrusion 60 was 500 µm, and the difference B between the thickness of the thin portion 58 and the thickness of the protrusion 60 was 320 µm.
[0042] (Examples 1 and 2) 6A, the sensor element 10 of Example 1 has a thin portion 58 and a protruding portion 60 at the tip portion 14a of the porous protective layer 14. The protruding portion 60 covers the longitudinal extension of the cavity 26 (opening 26a), and the thin portion 58 is provided at a position that avoids the longitudinal extension of the cavity 26. In Example 1, the thickness A of the protruding portion 60 was 500 μm, and the difference B in thickness between the thin portion 58 and the protruding portion 60 was 50 μm.
[0043] 6B, the sensor element 10 of Example 2 has a thin portion 58 and a protruding portion 60 at the tip portion 14a of the porous protective layer 14. The protruding portion 60 covers the longitudinal extension line of the cavity 26 (opening 26a), and the thin portion 58 is provided at a position that avoids the longitudinal extension line of the cavity 26. In Example 2, the thickness A of the protruding portion 60 was 480 μm, and the difference B between the thicknesses of the thin portion 58 and the protruding portion 60 was 280 μm.
[0044] Example 3 As shown in FIG. 7, the sensor element 10C of Example 3 has a porous protective layer 14C with a two-layer structure. The porous protective layer 14C has an inner layer 66 with a large porosity that contacts the main body 12, and an outer layer 68 formed on the inner layer 66 and with a smaller porosity than the inner layer 66. The inner layer 66 is formed to a uniform thickness by, for example, plasma spraying or a dipping method. The outer layer 68 is formed in a first spraying process (FIG. 3A) and a second spraying process (FIG. 3B). The outer layer 68 has a protruding portion 60 located on the longitudinal extension of the cavity 26, and a thin portion 58 that covers a portion that does not extend along the longitudinal extension of the cavity 26. The thickness A of the protruding portion 60 of the sensor element 10C of Example 3 was 900 μm, and the difference B between the thicknesses of the thin portion 58 and the protruding portion 60 was 300 μm.
[0045] Example 4 The sensor element 10 of Example 4 has a porous protective layer 14 having a cross-sectional shape generally similar to that of Fig. 6B. In Example 4, the thickness A of the protrusion 60 was 500 µm, and the difference B between the thickness of the thin portion 58 and the thickness of the protrusion 60 was 300 µm.
[0046] Example 5 The sensor element 10 of Example 5 has a porous protective layer 14 having a cross-sectional shape generally similar to that of Fig. 6A. In Example 5, the thickness A of the protrusion 60 was 600 µm, and the difference B between the thickness of the thin portion 58 and the thickness of the protrusion 60 was 30 µm.
[0047] (Water resistance evaluation method) The water resistance of the porous protective layers 14, 14C and the productivity were evaluated for the sensor elements 10 to 10C of Comparative Examples 1 to 3 and Examples 1 to 5. The water resistance was evaluated as follows.
[0048] First, the heater 34 was energized to heat the main body 12 to a temperature of 800°C. In this state, the main pump cell 48, the auxiliary pump cell 54, the first oxygen detection cell 50, the second oxygen detection cell 52, etc. were operated in the air atmosphere. The main pump cell 48 was controlled so that the oxygen concentration in the first chamber 32c was maintained at a predetermined constant value. The current supplied to the main pump cell 48 to maintain the oxygen concentration at a constant value was detected as the pump current Ip0. After waiting for the pump current Ip0 of the main pump cell 48 to stabilize, an operation was performed to drip water onto the porous protective layers 14, 14C.
[0049] Thereafter, the presence or absence of cracks in the main body 12 was judged based on whether the pump current Ip0 changed to a value exceeding a predetermined threshold value. When a crack occurs in the main body 12 due to thermal shock caused by water droplets, oxygen is likely to flow into the first chamber 32c through the cracked portion, and the value of the pump current Ip0 increases. Therefore, when the pump current Ip0 exceeds a predetermined threshold value, it is judged that a crack has occurred in the main body 12 due to water droplets. When the amount of water droplets that caused cracks in the main body 12 was less than 7 μL, it was judged as poor (×). When the amount of water droplets that caused cracks was 7 μL or more, it was judged as acceptable (△). When the amount of water droplets that caused cracks was 10 μL or more, it was judged as good (○). When the amount of water droplets that caused cracks was 20 μL or more, it was judged as excellent (◎).
[0050] (Productivity evaluation method) The productivity was evaluated based on the deposition rate of the tip portion 14a of the porous protective layer 14 (second spraying step). The deposition rate of Comparative Example 1 was selected as the standard. When the deposition rate by plasma spraying was equal to or lower than that of Comparative Example 1, it was judged as poor (×). When the deposition rate was 5% or more faster than that of Comparative Example 1, it was judged as fair (△). When the deposition rate was 20% or more faster than that of Comparative Example 1, it was judged as good (◯). When the deposition rate was 30% or more faster than that of Comparative Example 1, it was judged as excellent (◎).
[0051] (Evaluation Results) FIG. 8 shows, for Comparative Examples 1 to 3 and Examples 1 to 5, whether the position of the thin portion 58 is located on the longitudinal extension of the cavity 26, the ratio B / A of the thickness A of the convex portion 60 to the difference B between the thicknesses of the thin portion 58 and the convex portion 60, the evaluation results of water resistance, and the evaluation results of productivity.
[0052] 8, from the results of Comparative Examples 1 to 3 and Examples 1 to 5, it was confirmed that when plasma spraying is performed, the deposition rate (productivity) is improved by providing the porous protective layer 14 with the thin portions 58 and the protruding portions 60. From the viewpoint of productivity, the value of the ratio B / A in the sensor elements 10 to 10C is preferably 0.05 or more. When the value of the ratio B / A is 0.1 or more, the deposition rate is 20% or more faster than that in Comparative Example 1, and higher productivity is obtained.
[0053] Moreover, as shown in Comparative Examples 2 and 3, sufficient water resistance was not obtained when the thin-walled portion 58 was disposed on the extension line of the longitudinal direction of the cavity 26. It was confirmed that, in order to ensure water resistance, as shown in Examples 1 to 5, it is necessary to provide the thin-walled portion 58 at a position that is not on the extension line of the longitudinal direction of the cavity 26.
[0054] From the results of Examples 1 to 5, when the ratio B / A value was in the range of 0.05 to 0.6, the water resistance was fair (△) or better. Also, when the ratio B / A value was 0.58 or less, the water resistance was good (◯) or excellent (◎), and higher water resistance was obtained.
[0055] From the results of Examples 1 to 5, it was confirmed that both water resistance and productivity can be achieved when the ratio B / A of the difference B in the thickness between the thin portion 58 and the protruding portion 60 and the thickness A of the protruding portion 60 is in the range of at least 0.05 to 0.6. Furthermore, when the ratio B / A is in the range of 0.1 to 0.58, more suitable water resistance and productivity can be obtained.
[0056] The present invention is not limited to the above disclosure, and various configurations may be adopted without departing from the gist of the present invention. That is, the water droplet prevention structure is not limited to the protrusions 60, and may be a dense portion (a portion having a porosity lower than that of the thin portion 58 or a portion having a porosity of approximately 0%) that makes it difficult for water droplets to penetrate. In this case, the thickness A of the water droplet prevention structure may be the same as the thickness C of the thin portion 58, or may be thinner than the thickness of the thin portion 58. [Explanation of symbols]
[0057] 10, 10A, 10B, 10C...sensor element 12...main body 12a...Tip surface 12b...Side surface 14, 14C...Porous protective layer 26...Cavity 26a...Opening 58...Thin wall portion 60…Convex part
Claims
1. A body having a cavity at a tip end for taking in gas; a porous protective layer covering an outer peripheral surface of the tip side of the main body, The porous protective layer is A water droplet prevention structure that covers at least a portion of the tip surface of the main body that overlaps with the cavity in a longitudinal direction perpendicular to the tip surface; a thin portion covering the tip surface around the water droplet prevention structure; A sensor element comprising:
2. 2. The sensor element according to claim 1, The cavity extends along the longitudinal direction, The water droplet blocking structure is a protrusion of the porous protective layer having a thickness greater than that of the thin portion.
3. 2. The sensor element according to claim 1, wherein the main body is formed in a rectangular parallelepiped shape extending long in the longitudinal direction, and the main body has a flat plate shape in which a dimension in a width direction perpendicular to the longitudinal direction is larger than a dimension in a thickness direction perpendicular to the longitudinal direction and the width direction, The water droplet prevention structure is located at the center of the tip surface in the width direction and the thickness direction.
4. 2. The sensor element according to claim 1, wherein the thin portion is formed at a position that does not lie on an extension line of the cavity in the longitudinal direction.
5. 5. The sensor element according to claim 1, wherein a ratio B / A of a difference value B between a thickness C of the thin portion and a thickness A of the water droplet prevention structure and the thickness A of the water droplet prevention structure is in a range of 0.05 to 0.
6.
6. 5. The sensor element according to claim 1, wherein a ratio B / A of a difference value B between a thickness C of the thin portion and a thickness A of the water droplet prevention structure and the thickness A of the water droplet prevention structure is in a range of 0.1 to 0.
58.
7. 5. The sensor element according to claim 1, wherein the cavity opens to the tip surface.
8. A method for manufacturing a sensor element having a body having a cavity at a tip end side for taking in a gas component, and a porous protective layer covering an outer peripheral surface at the tip end side of the body, comprising: a first spraying step of forming the porous protective layer on a side surface of the main body by plasma spraying; A second spraying step of forming the porous protective layer on the tip surface of the main body by plasma spraying, The second spraying step is a method for manufacturing a sensor element, in which a spray gun is positioned to face the tip surface, and a nozzle center of the spray gun at which the film formation efficiency is highest is aligned on a longitudinal extension line perpendicular to the tip surface of the cavity, and plasma spraying is performed to form the porous protective layer on the tip surface, the porous protective layer having a thick convex portion covering at least a portion that overlaps with the cavity in the longitudinal direction, and a thin portion covering the tip surface around the convex portion.
9. A method for manufacturing a sensor element having a body having a cavity at a tip end side for taking in a gas component, and a porous protective layer covering an outer peripheral surface at the tip end side of the body, comprising: a first spraying step of forming the porous protective layer on a side surface of the main body by a spraying method; A second spraying step of forming the porous protective layer on the tip surface of the main body by a spraying method, The second spraying step is a method for manufacturing a sensor element, in which a spray gun is positioned to face the tip surface, and a nozzle center at which the film formation efficiency by the spray gun is highest is aligned with a longitudinal extension line perpendicular to the tip surface of the cavity and sprayed, thereby forming the porous protective layer on the tip surface, the porous protective layer having a thick convex portion covering at least the portion overlapping with the cavity in the longitudinal direction, and a thin portion covering the tip surface around the convex portion.
Citation Information
Patent Citations
Gas concentration detecting element and method of manufacturing the same
JP2009080111A
Gas sensor element and gas sensor
JP2016109685A
Gas sensor element and gas sensor
JP2019039693A