Leader tape and transfer foil roll

A leader tape with defined friction coefficients and tension addresses the issues of loosening and folding in transfer machines, ensuring stable transfer foil operation.

JP2024143059AInactive Publication Date: 2024-10-11TOPPAN HOLDINGS INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023055540
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The increased transfer speed of transfer foil in transfer machines leads to issues such as loosening or folding back of the leader tape into a bellows shape, causing slip-off or blocking of the transfer foil, particularly in machines with intermittent supply methods.

Method used

A leader tape with specific friction coefficients and a winding tension is used to connect the core and transfer foil, preventing loosening and folding, while maintaining effective winding around the core.

Benefits of technology

The solution effectively suppresses loosening and folding of the leader tape, ensuring stable transfer foil operation without slip-off or blocking, even at high speeds.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143059000001_ABST
    Figure 2024143059000001_ABST
Patent Text Reader

Abstract

To provide a leader tape capable of suppressing inconvenience such as slackening or bellows-shaped folding of the leader tape in a transfer foil roll.SOLUTION: A leader tape 4 which connects a core and a tape-like transfer foil 3 wound on the core comprises: a first surface 4a; and a second surface 4b facing a side opposite to the first surface 4a. The static friction coefficient of the first surface 4a with respect to the second surface 4b is 0.6 or higher, and the dynamic friction coefficient of the first surface 4a with respect to the second surface 4b is 0.21 or higher.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a leader tape and a transfer foil roll. [Background technology]

[0002] Conventionally, various security methods have been proposed for information recording media related to personal authentication, such as passports, visa stickers, or cards. For example, passports must be readable by both visual inspection and optical character recognition, according to the so-called ICAO (International Civil Aviation Organization) regulations. As image displays containing this type of personal recognition information, there are known ones that have an image pattern formed based on image information on a card substrate such as polyvinyl chloride, or ones that have a so-called OVD (Optical Variable Device) image, represented by an image obtained by using an optical thin film (which can obtain effects such as color shift by optical design) using a hologram, a diffraction grating, or multilayer interference in addition to the above image pattern.

[0003] One method for attaching an OVD to an article is to transfer a transfer foil containing the OVD in a transfer machine. Some transfer machines sequentially pay out the transfer foil from a transfer foil roll, which is a tape-like transfer foil wound around a cylindrical or cylindrical core, and transfer and attach the transfer foil to multiple articles at an attachment section.

[0004] There are bobbin-wound (traverse-wound) transfer foil rolls in which the transfer foil is wound around a bobbin so that the diameter of the transfer foil roll can be reduced in consideration of the space constraints on the installation of the transfer machine. In bobbin-wound transfer foil rolls, the tape-shaped transfer foil is wound around the core while being shifted in the axial direction of the core.

[0005] For transfer foils used for security purposes, it is important to manage the number of transfer foils. In other words, all of the transfer foil wound around the core must be attached to an item. For this reason, in transfer foil rolls for security purposes, the core and the transfer foil are connected by a leader tape so that all of the tape-like transfer foil reaches a position away from the core (the attachment part of the transfer machine).

[0006] Patent Document 1 discloses a grooved bobbin in which anti-slip treatment is applied to the outer surface of the bobbin around which thread, film, paper, cloth, etc. are wound. In the configuration of Patent Document 1, the anti-slip treatment suppresses the occurrence of slippage between the thread, film, paper, cloth, etc. and the outer surface of the bobbin. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2007-197179 A Summary of the Invention [Problem to be solved by the invention]

[0008] In recent years, the transfer speed of the transfer foil in the transfer machine has improved, and the speed at which the transfer foil is unwound from the transfer foil roll has also increased. As a result, the acceleration of the rotation of the transfer foil roll, which occurs when the transfer foil is started and stopped being unwound from the bobbin-wound transfer foil roll, also increases. Due to the large acceleration and deceleration of the rotation, the leader tape of the transfer foil roll loosens or is folded back in an accordion-like shape. If the leader tape loosens, when the transfer foil roll is removed from the transfer machine and the axial direction of the core is oriented vertically, the transfer foil slides off the core (the roll-shaped transfer foil collapses), which is a problem. In addition, if the leader tape is folded back in an accordion-like shape, a force greater than expected acts on the part of the transfer foil wound in a roll shape, causing a problem called blocking, in which overlapping transfer foils adhere to each other. In transfer machines that use an up-down transfer method in which transfer foil is intermittently supplied to the application section of the transfer machine, the transfer foil is fed out from the transfer foil roll intermittently, i.e., the transfer foil roll rotates and stops frequently, making the above-mentioned problems particularly likely to occur.

[0009] In order to prevent the leader tape from loosening on the transfer roll and from folding back like an accordion, it is possible to increase the winding tension of the leader tape and the transfer foil around the core. However, when the winding tension of the leader tape and the transfer foil is increased on a bobbin-wound transfer foil roll, blocking occurs, in which overlapping transfer foils stick to each other.

[0010] Even if the core is treated to prevent slippage by taking into consideration the configuration of Patent Document 1, it is difficult to reduce problems such as the leader tape loosening or folding back like an accordion.

[0011] In view of the above-mentioned problems, an object of the present invention is to provide a leader tape and a transfer foil roll that can suppress problems such as the leader tape becoming loose or being folded back like an accordion in a transfer foil roll. [Means for solving the problem]

[0012] One aspect of the present invention is a leader tape that connects a core and a tape-like transfer foil wound around the core, the leader tape having a first surface and a second surface facing the opposite side to the first surface, wherein the static friction coefficient of the first surface against the second surface is 0.6 or more, and the dynamic friction coefficient of the first surface against the second surface is 0.21 or more.

[0013] One aspect of the present invention is a transfer foil roll including a core, a tape-like transfer foil wound around the core, and a leader tape connecting the core and the transfer foil. The leader tape and the transfer foil are wound around the core in order. Effect of the Invention

[0014] According to the present invention, problems such as the leader tape becoming loose or being folded back like an accordion in a test transfer foil roll can be effectively prevented. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1 is a diagram showing a schematic diagram of a transfer foil roll according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic diagram showing a state before a leader tape and a transfer foil are wound around a core in a transfer foil roll according to one embodiment of the present invention. [Diagram 3] FIG. 3 is a cross-sectional view showing the layer structure of the leader tape and transfer foil in FIG. [Figure 4] FIG. 2 is a diagram for explaining a method for measuring the static and dynamic friction coefficients of a sample film. [Diagram 5] 1 is a table showing the evaluation of the transfer foil rolls of Experimental Examples 1 to 7 with respect to loosening and folding back of the leader tape, and blocking of the transfer foil. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, one embodiment of the present invention will be described with reference to FIGS. As shown in FIGS. 1 and 2, the transfer foil roll 1 of this embodiment includes a core 2, a transfer foil 3, and a leader tape 4.

[0017] The core 2 has an outer peripheral surface that is circular when viewed from the axial direction. The core 2 illustrated in Fig. 2 is cylindrical, but may be, for example, columnar. The core 2 of this embodiment is a cardboard tube.

[0018] The transfer foil 3 is formed in a tape shape extending in one direction so as to be wound around the core 2. The transfer foil 3 is transferred to a transfer target such as a printed material by applying transfer heat and pressure using a hot stamp or the like.

[0019] The specific configuration of the transfer foil 3 is not particularly limited. The transfer foil 3 may be, for example, a known one. The transfer foil 3 illustrated in Fig. 3 has a foil base layer 31, a release layer 32, a relief layer 33, a reflective layer 34, and an adhesive layer 35, which are sequentially stacked on one side of the foil base layer 31. The release layer 32, the relief layer 33, and the reflective layer 34 constitute the OVD portion 30.

[0020] The foil base layer 31 protects the OVD portion 30 (the release layer 32, the relief layer 33 and the reflective layer 34) until the transfer foil 3 is transferred to a transfer target object. The foil base layer 31 can be a single-layer or multi-layer plastic film. The plastic film can be manufactured by an extrusion method, a solution casting method, or a calendar method. The extrusion method can be an inflation method or a T-die method. The plastic film can be a stretched or unstretched film. The material of the plastic film can be a thermoplastic resin or a soluble resin. The thermoplastic resin can be, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), or PP (polypropylene). The foil base layer 31 can also be, for example, paper, synthetic paper, plastic multi-layer paper, or resin-impregnated paper, depending on the application or purpose.

[0021] The release layer 32 adheres closely to the relief layer 33 and is supported to an extent that it can be peeled off from the foil base layer 31. The release layer 32 peels off from the foil base layer 31 when the transfer foil 3 is thermally transferred to a transfer target body. The release layer 32 is exposed on the outermost surface after transfer, and protects the relief layer 33 and the reflective layer 34 from external damage. Examples of the material of the release layer 32 include simple substances such as polyolefin resin, polyester resin, polyvinyl resin, polyurethane resin, and polyacrylic acid resin, as well as copolymers of these resins.

[0022] The relief layer 33 has a fine uneven structure 331 on the surface in contact with the reflective layer 34. The fine uneven structure 331 may be a structure including only concave portions, a structure including only convex portions, or a structure including both concave portions and convex portions. The uneven structure 331 allows the OVD section 30 to exhibit desired optical properties such as diffraction, light reflection suppression, isotropic or anisotropic light scattering, refraction, polarization / wavelength selective reflection, transmission, and light reflection suppression. Specific examples of the uneven structure 331 include a moth-eye structure and a deep lattice structure. Examples of the material of the relief layer 33 include polyolefin resin, polyester resin, polyvinyl resin, polyurethane resin, polyacrylic acid resin, and copolymers of these resins.

[0023] The reflective layer 34 is formed by deposition or the like on the relief layer 33. Examples of the material of the reflective layer 34 include metal oxides such as alumina and silica.

[0024] The adhesive layer 35 may be made of any material as long as it has the property of softening when heated, and may contain, for example, acrylic resin, polyester resin, or silica. The adhesive layer 35 may also contain, for example, a resin component and spacer particles. The resin component of the adhesive layer 35 contains a thermoplastic resin with a glass transition temperature lower than room temperature and defines the thickness of the adhesive layer 35. The spacer particles of the adhesive layer 35 have a particle size larger than the thickness of the layer formed by the resin component. Some of the spacer particles protrude from the resin component.

[0025] The transfer foil 3 illustrated in FIG. 3 further includes a backcoat layer 36 overlapping the other surface of the foil base layer 31 . The surface of the backcoat layer 36 has a dynamic friction coefficient of 0.30 or less and a continuous load scratch strength of 9.5 g or more. The inventors' studies have revealed that a backcoat layer 36 with such physical properties generates almost no dust due to wear even when moved at a high speed of about 4 m / sec in a thermal transfer device. A dynamic friction coefficient of 0.30 or less is believed to contribute to reducing the amount of friction caused by high speed movement. A continuous load scratch strength of 9.5 g or more is believed to contribute to high hardness, which makes the backcoat layer less susceptible to wear.

[0026] The backcoat layer 36 may be a composite material (composite material) of a binder resin 361 and auxiliary particles 362. The binder resin 361 can impart heat resistance and hardness to the backcoat layer 36. The binder resin 361 may contain an aromatic compound. The aromatic compound may be cellulose acetate, polyamideimide, or a mixture or copolymer thereof. The cellulose acetate may have a glass transition temperature in the range of 150° C. or more and 800° C. or less, and a melting point of 230° C. or more. The polyamideimide may have a molecular weight in the range of 5,000 to 30,000.

[0027] The auxiliary particles 362 may be resin beads. The resin beads may be mainly composed of an aliphatic compound. The aliphatic compound may be a surfactant, a fluororesin, or a mixed resin thereof. The aliphatic compound may also be a compound modified with amine or fluorine. This can improve the slipperiness and heat resistance of the auxiliary particles 362. The auxiliary particles 362 of the resin beads mainly composed of an aliphatic compound are wax particles.

[0028] The auxiliary particles 362 may include a plurality of types of particles formed from different types of resins. The auxiliary particles 362 may also include resin beads of different sizes (particle diameters). That is, the auxiliary particles 362 may include a plurality of types of resin beads with different average particle diameters. Furthermore, the auxiliary particles 362 may include particles of the same size but different types of resins, particles of the same size but different types of resins, or particles of both different sizes and types of resins. By including particles of the same size but formed from different types of resins, it is possible to easily obtain both the required static and dynamic friction coefficients. By including particles of the same type of resin but different sizes, it is possible to adjust the slipperiness. By including resin beads (particles) of different sizes and different types of resins, it is possible to obtain appropriate static and dynamic friction coefficients. The resin beads mainly composed of an aliphatic compound improve the slipperiness of the surface of the backcoat layer 36. In other words, the slipperiness between the backcoat layer 36 and a guide that comes into contact with the backcoat layer 36 when the transfer foil 3 is transported is improved.

[0029] The surfactant may be amide wax, carnauba wax, or polyethylene wax. That is, the auxiliary particles 362 may be composed of, for example, amide wax as a main component. The melting point of the amide wax may be in the range of 70°C or more and 130°C or less. The auxiliary particles 362 composed mainly of amide wax have high hardness and form a chemical bond with the binder resin 361. As a result, by being located in the backcoat layer 36, the rigidity of the backcoat layer 36 is increased and wear is suppressed. If the binder resin 361 is polyamideimide, the chemical bond becomes stronger and the effect is enhanced.

[0030] The melting point of the surfactant may be higher than the thermal transfer temperature of the transfer foil 3, i.e., higher than the melting point or glass transition point (Tg) of the adhesive layer 35 (e.g., the resin component of the adhesive layer 35). In this case, the surfactant is less likely to adhere to the hot stamp that comes into contact with the backcoat layer 36 during transfer of the transfer foil 3, and maintenance frequency can be reduced.

[0031] The auxiliary particles 362 may be composed mainly of, for example, a fluororesin. The fluororesin may be polytetrafluoroethylene (PTFE). The melting point of PTFE may be in the range of 300°C or more and 800°C or less, and the molecular weight may be 1,000,000 (1,000,000) or more. If the glass transition point (Tg) of the resin beads is higher than the thermal transfer temperature, i.e., higher than the melting point or Tg of the resin component in the adhesive layer 35, the resin beads are less likely to adhere to the hot stamp, and the frequency of maintenance can be reduced. The auxiliary particles 362 mainly composed of fluorine-based resin have high hardness. As a result, by the auxiliary particles 362 being located in the backcoat layer 36, the rigidity of the backcoat layer 36 can be increased and wear can be suppressed. In addition, since the surface tension of the auxiliary particles 362 mainly composed of fluorine-based resin is low, by having a part of the auxiliary particles 362 protrude from the surface of the backcoat layer 36, slipperiness is imparted to the backcoat layer 36 and an increase in friction is suppressed.

[0032] The backcoat layer 36 described above can be a composite of the binder resin 361 which is an aromatic compound and the auxiliary particles 362 which are wax particles or resin beads mainly composed of an aliphatic compound.

[0033] The protruding height of the auxiliary particles 362 on the surface of the backcoat layer 36 (the surface that comes into contact with the hot stamp) may be lower than the protruding height of the spacer particles on the surface of the adhesive layer 35. Here, the protruding height of the auxiliary particles 362 can be defined as the height at which the auxiliary particles 362 protrude from the layer formed by the binder resin 361. This makes it possible to suppress or prevent blocking between the stacked transfer foils 3 that occurs due to the winding state when the transfer foil 3 is wound into a roll.

[0034] As shown in FIG. 2, the leader tape 4 is formed in the shape of a tape extending in one direction, similar to the transfer foil 3. The leader tape 4 connects the core 2 and the transfer foil 3. A first end in the longitudinal direction of the leader tape 4 is fixed to the outer peripheral surface of the core 2, for example, by a fixing portion 5. A second end of the leader tape 4 is connected to an end in the longitudinal direction of the transfer foil 3, for example, by a connecting portion 6. The fixing portion 5 and the connecting portion 6 may be, for example, an adhesive or an adhesive tape. The width of the leader tape 4 is preferably equal to the width of the transfer foil 3. In addition, when connecting the leader tape 4 and the transfer foil 3, it is preferable to align both ends of the leader tape 4 with both ends of the transfer foil 3 in the width direction.

[0035] 3, the leader tape 4 has a first surface 4a and a second surface 4b facing the opposite side to the first surface 4a. The static friction coefficient of the first surface 4a with respect to the second surface 4b of the leader tape 4 is 0.6 or more. The kinetic friction coefficient of the first surface 4a with respect to the second surface 4b is 0.21 or more.

[0036] Furthermore, the Ssk (skewness) of the first surface 4a of the leader tape 4 is 1.0 or more, and the Sku (kurtosis) of the first surface 4a is 10 or more.

[0037] The leader tape 4 of this embodiment has a tape base layer 41 and an additional layer 42 formed on the tape base layer 41. The tape base layer 41 forms a second surface 4b of the leader tape 4. The additional layer 42 forms a first surface 4a of the leader tape 4.

[0038] The tape base layer 41 may be, for example, the same as the foil base layer 31 of the transfer foil 3 described above. That is, the tape base layer 41 may be a plastic film similar to the foil base layer 31, such as a PET film, a PEN film, or a PP film.

[0039] The additional layer 42 is formed so that the first surface 4a of the leader tape 4 has the above-mentioned characteristics. The additional layer 42 may be made of the same material as the adhesive layer 35 of the transfer foil 3 described above. That is, the additional layer 42 may contain, for example, an acrylic resin, a polyester resin, or silica.

[0040] The additional layer 42 may contain a filler such as silica for the purpose of adjusting the dynamic friction coefficient of the first surface 4a of the leader tape 4. The particle diameter of the filler in the additional layer 42 may be, for example, 1.0 μm or more. By adding a filler with a particle diameter of 1.0 μm or more to the resin (e.g., acrylic resin, polyester resin) that mainly constitutes the additional layer 42, the dynamic friction coefficient of the first surface 4a of the leader tape 4 can be reduced. That is, when the amount of filler with a particle diameter of 1.0 μm or more added to the resin that constitutes the additional layer 42 increases, the dynamic friction coefficient of the first surface 4a of the leader tape 4 decreases. Note that adding nanosilica having a particle size of less than 1.0 μm to the resin of the additional layer 42 does not decrease the dynamic friction coefficient of the first surface 4a of the leader tape 4. For this reason, nanosilica is not included in the filler of the additional layer 42 in the present application.

[0041] The amount of filler contained in the additional layer 42 may be, for example, 0.05 or more and 0.6 or less, in terms of mass ratio to the resin that mainly constitutes the additional layer 42. When the mass ratio of the filler to the resin in the additional layer 42 is 0.05 or more, the occurrence of blocking can be suppressed. Furthermore, when the mass ratio of the filler to the resin is 0.6 or less, the ink for forming the additional layer 42 can be applied to the tape base layer 41.

[0042] The static and dynamic friction coefficients of the first surface 4a against the second surface 4b of the leader tape 4 can be measured by a method conforming to ASTM D1894, for example. In this measurement method, first, as shown in Fig. 4, a base film 100 corresponding to the tape substrate layer 41 (second surface 4b of the leader tape 4) and a sample film 200 corresponding to the additional layer 42 (first surface 4a of the leader tape 4) are prepared. The size of the base film 100 and the sample film 200 in a plan view is 63.5 cm square. Next, the sample film 200 is overlapped on the base film 100, and the sample film 200 is moved at a speed of 150 mm / min in a direction along the contact surface between the base film 100 and the sample film 200 (for example, the direction of arrow D1 in Fig. 4). In this way, the static friction coefficient and dynamic friction coefficient of the sample film 200 with respect to the base film 100 are measured.

[0043] In the transfer foil roll 1 shown in Fig. 1, the core 2 and the transfer foil 3 are connected by the leader tape 4 as shown in Fig. 2, and the leader tape 4 and the transfer foil 3 are wound around the core 2 in order. In this embodiment, the leader tape 4 and the transfer foil 3 are wound around the core 2 so that the first surface 4a of the leader tape 4 and the adhesive layer 35 of the transfer foil 3 face the core 2 (outer peripheral surface) side. The winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 is 0.2 N / mm or more and 0.32 N / mm or less. The magnitude of the winding tension may be set appropriately depending on, for example, the friction coefficient (static friction coefficient, dynamic friction coefficient) of the first surface 4a relative to the second surface 4b of the leader tape 4. For example, the winding tension may be set to be larger as the friction coefficient of the first surface 4a of the leader tape 4 becomes smaller.

[0044] 1, the leader tape 4 and the transfer foil 3 are wound in a bobbin shape. That is, the leader tape 4 and the transfer foil 3 are wound around the core 2 while being shifted in the axial direction of the core 2 so that their widthwise ends overlap. The leader tape 4 and the transfer foil 3 are wound around the core 2 while reciprocating between both ends of the core 2 in the axial direction.

[0045] As described above, in the transfer foil roll 1 having the leader tape 4 of this embodiment, the leader tape 4 and the transfer foil 3 are wound around the core 2 so that the first surface 4a of the leader tape 4 faces the core 2. Therefore, the first surface 4a of the leader tape 4 contacts the core 2. In addition, the leader tape 4 is wound around the core 2 multiple times, so that the leader tapes 4 overlap each other. The static friction coefficient of the first surface 4a against the second surface 4b of the leader tape 4 is 0.6 or more, and the dynamic friction coefficient of the first surface 4a against the second surface 4b is 0.21 or more. Therefore, the first surface 4a of the leader tape 4 is unlikely to slip against the core 2 or the second surface 4b of the leader tape 4. As a result, even if the acceleration of the rotation of the transfer foil roll 1 generated when the transfer foil 3 is started and stopped in the transfer foil roll 1 is large, the problems of the leader tape 4 being loosened or folded back in a bellows shape in the transfer foil roll 1 can be effectively suppressed.

[0046] In addition, in the leader tape 4 of this embodiment, the first surface 4a has an Ssk (skewness) of 1.0 or more, and an Sku (kurtosis) of the first surface 4a of the leader tape 4 of 10 or more. Therefore, the first surface 4a of the leader tape 4 is unlikely to slip relative to the core 2 or the second surface 4b of the leader tape 4. This makes it possible to suppress problems such as the leader tape 4 loosening on the transfer foil roll 1 or folding back in an accordion-like shape, even if the acceleration of the rotation of the transfer foil roll 1, which occurs when the payout of the transfer foil 3 on the transfer foil roll 1, is large.

[0047] Moreover, the leader tape 4 of this embodiment has a tape base layer 41 forming the second surface 4b, and an additional layer 42 forming the first surface 4a, which is formed by overlapping the tape base layer 41. Therefore, compared to when the leader tape 4 is a single layer, the characteristics of the first surface 4a of the leader tape 4 (the static friction coefficient and kinetic friction coefficient of the first surface 4a with respect to the second surface 4b, and Ssk and Sku of the first surface 4a) can be set simply and appropriately.

[0048] In addition, in the transfer foil roll 1 of this embodiment, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 is 0.2 N / mm or more and 0.32 N / mm or less. By having the winding tension of the leader tape 4 and the transfer foil 3 of 0.2 N / mm or more, even if the acceleration of the rotation of the transfer foil roll 1 that occurs when the transfer foil 3 in the transfer foil roll 1 starts and stops is large, it is possible to suppress problems such as the leader tape 4 in the transfer foil roll 1 loosening or folding back in an accordion-like shape. In addition, by having the winding tension of the leader tape 4 and the transfer foil 3 of 0.32 N / mm or less, it is possible to prevent blocking (a phenomenon in which overlapping transfer foils 3 in the transfer foil roll 1 stick to each other).

[0049] Furthermore, in the transfer foil roll 1 of this embodiment, if the additional layer 42 of the leader tape 4 is made of the same material as the adhesive layer 35 of the transfer foil 3, the process of forming the additional layer 42 on the tape base layer 41 when manufacturing the leader tape 4 and the process of forming the adhesive layer 35 on the reflective layer 34 when manufacturing the transfer foil 3 can be performed in the same device when manufacturing the transfer foil roll 1. This allows the leader tape 4 to be manufactured more cheaply and efficiently than when the additional layer 42 of the leader tape 4 is made of a different material from the adhesive layer 35 of the transfer foil 3.

[0050] Furthermore, in the transfer foil roll 1 of this embodiment, when the tape base layer 41 of the leader tape 4 is made of the same material as the foil base layer 31 of the transfer foil 3, the process of forming the tape base layer 41 and the process of forming the foil base layer 31 can be carried out in the same device. This allows the leader tape 4 to be manufactured even more cheaply and efficiently.

[0051] Furthermore, in the transfer foil roll 1 of this embodiment, since the core 2 is a cardboard tube, it is possible to improve the handleability of the transfer foil roll 1. For example, when the core 2 is a cardboard tube, when the transfer foil roll 1 is attached to the rotating shaft of a transfer machine, the inner peripheral surface of the cardboard tube can be deformed so that the cardboard tube fits onto the rotating shaft, and the transfer foil roll 1 can be attached to the rotating shaft. In addition, since the cardboard tube has an appropriate surface roughness, it is possible to effectively prevent the leader tape 4 from slipping against the outer circumferential surface of the core 2 which is a cardboard tube.

[0052] In the transfer foil roll 1 of this embodiment, the surface of the backcoat layer 36 of the transfer foil 3 has a dynamic friction coefficient of 0.30 or less and a continuous load scratch strength of 9.5 g or more. By providing the backcoat layer 36 with such physical properties, high-speed thermal transfer can be performed satisfactorily.

[0053] In the transfer foil roll 1 of this embodiment, when the transfer foil 3 has a backcoat layer 36 having a binder resin 361 of cellulose acetate or polyamideimide and auxiliary particles 362 mainly composed of amide wax, friction and wear with the transfer device are suppressed even during high-speed thermal transfer. As a result, high-speed thermal transfer can be performed well.

[0054] In the transfer foil roll 1 of this embodiment, when the transfer foil 3 has a backcoat layer 36 having a binder resin 361 of cellulose acetate or polyamideimide and auxiliary particles 362 mainly composed of fluorine-based resin, friction and wear with the transfer device are suppressed even during high-speed thermal transfer. As a result, high-speed thermal transfer can be performed well. Furthermore, the auxiliary particles 362, which are mainly composed of fluorine-based resin, have high heat resistance due to the strong bond between carbon and fluorine. Therefore, by exposing the auxiliary particles 362 on the surface of the backcoat layer 36, the auxiliary particles 362 are not crushed, and contact between the hot stamp and the binder resin 361 during thermal transfer is reduced. As a result, contamination of the hot stamp during thermal transfer can be prevented.

[0055] (Experimental Example) The leader tape 4 and the transfer foil roll 1 of the above-described embodiment will be further described below with reference to Experimental Examples 1 to 7. The technical scope of the present invention is not limited in any way by the specific contents of Experimental Examples 1 to 7 shown below.

[0056] The transfer foil rolls of Experimental Examples 1 to 6 were prepared as follows. 3, a tape-shaped transfer foil 3 is prepared by sequentially laminating a release layer 32, a relief layer 33, a reflective layer 34, and an adhesive layer 35 on one surface of a foil base layer 31. The transfer foil 3 was prepared by a known method. Furthermore, an ink for forming an additional layer is applied to one surface of the tape base layer 41 so that the film thickness after drying (dry film thickness) is 4 to 5 μm, and then dried to form an additional layer 42. In this manner, the leader tape 4 is produced. The method for forming the additional layer 42 is the same as the method for forming the adhesive layer 35 in the transfer foil 3.

[0057] 2, a first end of the leader tape 4 is fixed to the outer peripheral surface of the core 2, and a second end of the leader tape 4 is connected to an end of the transfer foil 3. After that, the leader tape 4 and the transfer foil 3 are wound around the core 2 in a bobbin shape so that the first surface 4a of the leader tape 4 and the adhesive layer 35 of the transfer foil 3 face the core 2 (see FIG. 1). In this way, the transfer foil rolls of Experimental Examples 1 to 6 were produced. The transfer foil roll of Experimental Example 7 was produced in the same manner as the transfer foil rolls of Experimental Examples 1 to 6, except that the leader tape was composed only of a tape base layer.

[0058] FIG. 5 shows the Ssk (skewness) and Sku (kurtosis) of the first surface 4a (surface on the core 2 side) of the leader tape of the transfer foil rolls of Experimental Examples 1 to 7, the winding tension of the leader tape and transfer foil 3, and the evaluation results by tests.

[0059] (Experimental Example 1) First, the materials of the tape base layer 41 and the additional layer 42 of the leader tape 4 in Experimental Example 1 will be described. "Parts" refers to parts by mass unless otherwise specified. ·Tape base layer 41 PET film (thickness 38 μm) · Ink for forming additional layers Acrylic resin 49 parts Polyester Resin 1 part Silica (average particle size 8.0 μm) 1.5 parts Silica (average particle size 14.0 μm) 1 part Nanosilica (average particle size 10 to 15 nm) 32 parts Methyl ethyl ketone 12 parts Toluene 2 parts

[0060] In the leader tape 4 of experimental example 1, by forming an additional layer 42 using the ink for forming the additional layer described above, the Ssk (skewness) of the first surface 4a of the leader tape 4 becomes 3.0 and the Sku (kurtosis) of the first surface 4a becomes 30. In leader tape 4 in Experimental Example 1, the static friction coefficient of first surface 4a against second surface 4b of leader tape 4 is 0.973 to 1.015, and the kinetic friction coefficient of first surface 4a against second surface 4b is 0.240 to 0.295. In the transfer foil roll of Experimental Example 1, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 was set to 0.17 N / mm.

[0061] (Experimental Example 2) In the transfer foil roll of Experimental Example 2, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 was set to 0.21 N / mm. The materials of each layer of leader tape 4, Ssk (skewness) and Sku (kurtosis) of first surface 4a of leader tape 4, and the static and dynamic friction coefficients of first surface 4a against second surface 4b of leader tape 4 are the same as in Experimental Example 1.

[0062] (Experimental Example 3) In the transfer foil roll of Experimental Example 3, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 was set to 0.25 N / mm. The materials of each layer of leader tape 4, Ssk (skewness) and Sku (kurtosis) of first surface 4a of leader tape 4, and the static and dynamic friction coefficients of first surface 4a against second surface 4b of leader tape 4 are the same as in Experimental Example 1.

[0063] (Experimental Example 4) In the transfer foil roll of Experimental Example 4, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 was set to 0.33 N / mm. The materials of each layer of leader tape 4, Ssk (skewness) and Sku (kurtosis) of first surface 4a of leader tape 4, and the static and dynamic friction coefficients of first surface 4a against second surface 4b of leader tape 4 are the same as in Experimental Example 1.

[0064] (Experimental Example 5) The tape base layer 41 of the leader tape 4 in Experimental Example 5 is the same as that in Experimental Example 1. The material of the additional layer 42 in Experimental Example 5 will be described below. · Ink for forming additional layers Acrylic resin 37 parts Polyester Resin 1 part Silica (average particle size 8.0 μm) 1 part Nanosilica (average particle size 10 to 15 nm) 50 parts Methyl ethyl ketone 9.5 parts Toluene 1.5 parts

[0065] In the leader tape 4 of experimental example 5, by forming an additional layer 42 using the ink for forming the additional layer described above, the Ssk (skewness) of the first surface 4a of the leader tape 4 becomes 1.0 and the Sku (kurtosis) of the first surface 4a becomes 10. In the leader tape 4 of Experimental Example 5, the static friction coefficient of the first surface 4a against the second surface 4b of the leader tape 4 is 1.37, and the kinetic friction coefficient of the first surface 4a against the second surface 4b is 0.59. In the transfer foil roll of Experimental Example 5, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 was set to 0.21 N / mm, the same as in Experimental Example 2.

[0066] (Experimental Example 6) In the transfer foil roll of Experimental Example 6, the winding tension of the leader tape 4 and the transfer foil 3 relative to the core 2 was set to 0.25 N / mm, the same as in Experimental Example 3. The materials of each layer of the leader tape 4, as well as the Ssk (skewness) and Sku (kurtosis) of the first surface 4a of the leader tape 4, and the static and dynamic friction coefficients of the first surface 4a against the second surface 4b of the leader tape 4 are the same as in experimental example 5.

[0067] (Experimental Example 7) The leader tape in the transfer foil roll of Experimental Example 7 was composed only of the lead base material layer similar to that of Experimental Example 1, that is, only of a PET film (thickness 38 μm). In the leader tape of Experimental Example 7, the Ssk (skewness) of the first surface 4a of the leader tape was −0.6, and the Sku (kurtosis) of the first surface 4a was 3. In the leader tape of Experimental Example 7, the static friction coefficient of the first surface 4a against the second surface 4b of the leader tape is 0.578 to 0.589, and the kinetic friction coefficient of the first surface 4a against the second surface 4b is 0.196 to 0.202. In the transfer foil roll of Experimental Example 7, the winding tension of the leader tape and the transfer foil 3 around the core 2 was set to 0.25 N / mm, the same as in Experimental Examples 3 and 6.

[0068] (Experimental Method) Each of the transfer foil rolls in the above-mentioned experimental examples 1 to 7 was attached to a predetermined drive shaft, and the transfer foil roll was rotated and suddenly stopped five times. The rotation speed of the transfer foil roll was set so that the payout speed of the transfer foil 3 was equivalent to 60 m / min.

[0069] (Evaluation of leader tape slack) In the transfer foil rolls of experimental examples 1 to 7 after the above-mentioned experiments, when the axial direction of core 2 was oriented vertically, if the transfer foil 3 slid off core 2, it was marked as × (defect: loose leader tape), and if the transfer foil 3 did not slide off core 2, it was marked as ○ (no defect: no slack in leader tape).

[0070] (Evaluation of leader tape turn-back) In addition, in the transfer foil rolls of experimental examples 1 to 7 after the above-mentioned experiments, if the leader tape had a bellows-like fold, it was marked as × (defective), and if the leader tape did not have a bellows-like fold, it was marked as ○ (no defect).

[0071] (Blocking evaluation) In addition, in the transfer foil rolls of Experimental Examples 1 to 7 after the above-mentioned experiments, cases where blocking occurred were marked with × (defective), and cases where blocking did not occur were marked with ◯ (no defect).

[0072] As shown in FIG. 5, in the transfer foil rolls of Experimental Examples 1 and 7, blocking was "○", but loosening of the leader tape and folding back of the leader tape were both "×". In the transfer foil roll of Experimental Example 1, it is considered that the loosening of the leader tape and folding back of the leader tape occurred because the winding tension was small at 0.17 N / mm. In the transfer foil roll of Experimental Example 7, it is considered that the loosening of the leader tape and folding back of the leader tape occurred because the static friction coefficient of the first surface 4a of the leader tape against the second surface 4b was 0.578 to 0.589 and the dynamic friction coefficient was small at 0.196 to 0.202, and the Ssk (skewness) of the first surface 4a of the leader tape was small at -0.6 and the Sku (kurtosis) of the first surface 4a was small at 3.

[0073] In the transfer foil roll of Experimental Example 4, both the leader tape loosening and the leader tape folding back were rated as “○”, but the blocking was rated as “×”. This is considered to be due to the winding tension of the leader tape and the transfer foil 3 against the core 2 being large at 0.33 N / mm.

[0074] On the other hand, in the transfer foil rolls of Experimental Examples 2, 3, 5, and 6, the leader tape loosening, the leader tape folding back, and the blocking were all rated as "○." In other words, it was confirmed that in the transfer foil rolls of Experimental Examples 2, 3, 5, and 6, the leader tape did not loosen or fold back in an accordion-like shape, and the blocking problem did not occur.

[0075] Although the embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and can be modified as appropriate without departing from the spirit of the present invention.

[0076] In the present invention, the leader tape 4 is not limited to a multi-layer structure as in the above embodiment, but may be, for example, a single layer structure.

[0077] In the present invention, the leader tape 4 and the transfer foil 3 may be wound around the core 2 without being shifted in the axial direction of the core 2, for example. [Explanation of symbols]

[0078] 1 Transfer foil roll 2 cores 3 Transfer foil 4 Leader Tape 4a Front page 4b Second side 31 Foil base material layer 32 Peeling layer 33 Relief Layer 34 Reflective layer 35 Adhesive layer 41 Tape base layer 42 Additional layers

Claims

1. A leader tape that connects a core and a tape-shaped transfer foil that is wound around the core, A first surface and a second surface facing opposite the first surface, a static friction coefficient of the first surface with respect to the second surface is 0.6 or more; A leader tape having a dynamic friction coefficient of said first surface relative to said second surface of 0.21 or greater.

2. The Ssk (skewness) of the first surface is 1.0 or more, 2. The leader tape according to claim 1, wherein the Sku (kurtosis) of the first surface is 10 or more.

3. 3. The leader tape of claim 1, further comprising: a tape base layer forming the second surface; and an additional layer overlying the tape base layer and forming the first surface.

4. A core, a tape-like transfer foil wound around the core, and the leader tape according to claim 1 or 2 that connects the core and the transfer foil, The leader tape and the transfer foil are wound around the core in that order to form a transfer foil roll.

5. The transfer foil roll according to claim 4, wherein a winding tension of the leader tape and the transfer foil around the core is 0.2 N / mm or more and 0.32 N / mm or less.

6. the leader tape having a tape base layer forming the second surface and an additional layer overlying the tape base layer forming the first surface; The transfer foil has a foil base layer, and a release layer, a relief layer, a reflective layer, and an adhesive layer, which are sequentially superimposed on one surface of the foil base layer; The transfer foil roll according to claim 4 , wherein the additional layer is made of the same material as the adhesive layer.

7. The transfer foil roll according to claim 6 , further comprising a back coat layer overlapping the other surface of the foil base layer.

8. the backcoat layer is a composite of a binder resin containing an aromatic compound and auxiliary particles mainly composed of an aliphatic compound, the adhesive layer contains a thermoplastic resin having a glass transition temperature lower than room temperature, a resin component that defines a thickness of the adhesive layer, and spacer particles that have a particle size larger than a thickness of a layer formed by the resin component and a part of which protrudes from the resin component; a height at which the auxiliary particles protrude from the binder resin is lower than a height at which the spacer particles protrude from the resin component; 8. The transfer foil roll according to claim 7, wherein the surface of the backcoat layer has a dynamic friction coefficient of 0.30 or less and a continuous load scratch strength of 9.5 g or more.

9. The transfer foil roll according to claim 8 , wherein the auxiliary particles of the backcoat layer contain a surfactant having a melting point higher than the melting point or glass transition point of the adhesive layer.

10. The transfer foil roll according to claim 8 , wherein the backcoat layer contains the binder resin of cellulose acetate or polyamideimide, and the auxiliary particles mainly composed of amide wax.

11. The transfer foil roll according to claim 8 , wherein the backcoat layer contains the binder resin of cellulose acetate or polyamideimide, and the auxiliary particles mainly composed of a fluorine-based resin.

12. 5. The transfer foil roll according to claim 4, wherein the core is a paper tube.

13. The transfer foil roll according to claim 4 , wherein the leader tape and the transfer foil are wound around the core while being shifted in the axial direction of the core.

Citation Information