Individually packaged absorbent article and manufacturing method of package product formed by storing individually packaged absorbent articles in package

By using a paper packaging sheet with specific friction coefficients and composition, absorbent articles are effectively stacked and printed, enhancing production efficiency and appearance while reducing waste.

JP2024143330APending Publication Date: 2024-10-11DAIO PAPER CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023055946
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Absorbent articles like sanitary napkins and incontinence pads, when packaged in paper sheets with smooth surfaces, tend to slip against each other during stacking, reducing production efficiency and giving a cheap impression, while paper sheets with high smoothness are suitable for printing but not for stacking.

Method used

The absorbent articles are individually packaged with a paper packaging sheet having a variation in average coefficient of friction (MMD) of 0.050 or less before printing and a coefficient of static friction of 0.60 or more after printing, ensuring they do not slip when stacked, and the packaging sheet contains at least 20% recycled fibers or fiber bundles to enhance friction.

Benefits of technology

This configuration allows for proper printing and prevents a decrease in production efficiency by maintaining the absorbent articles in a stable stacked state, avoiding a cheap appearance and feel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143330000001_ABST
    Figure 2024143330000001_ABST
Patent Text Reader

Abstract

To achieve both printing appropriateness and avoidance of a decline in production efficiency, even when a plurality of individually packaged absorbent articles are stacked and stored in a package.SOLUTION: An individually packaged absorbent article is formed by individually packaging an absorbent article with a paper packaging sheet. An exposed surface of the packaging sheet being exposed when individually packaging the absorbent article is printed, an MMD of the exposed surface before printing is 0.050 or less, and a coefficient of static friction between exposed surfaces of the plurality of individually packaged absorbent articles after printing is 0.60 or more.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing an individually packaged absorbent article and a packaged product in which the individually packaged absorbent article is housed in a package. [Background technology]

[0002] 2. Description of the Related Art Absorbent articles such as sanitary napkins, panty liners, incontinence pads, etc. are generally provided in a package.

[0003] Patent Document 1 discloses a technology in which the surface of a package containing absorbent articles is provided with an uneven matte layer on the outermost layer to increase surface friction and prevent the package from falling apart when displayed. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2020-196541 A Summary of the Invention [Problem to be solved by the invention]

[0005] Absorbent articles such as sanitary napkins, panty liners, and incontinence pads are individually wrapped in a wrapping sheet and stored in a package as individually packaged absorbent articles for reasons such as ensuring hygiene during storage and improving convenience during carrying. Since the wrapping sheet individually wraps the absorbent article, the amount of waste generated after use is greater than that of a package. Therefore, in recent years, from the viewpoint of environmental issues, there has been a trend toward making wrapping sheets out of paper materials instead of conventional nonwoven fabrics or plastic films.

[0006] Incidentally, the individually packaged absorbent article as described above is carried in a state in which the absorbent article is contained in a packaging sheet. Therefore, it may be preferable to print on the surface of the packaging sheet so that it is not recognized as an absorbent article at first glance. In order to enhance the design by printing on the packaging sheet, it is considered to use paper with a high surface smoothness and high printability as the packaging sheet.

[0007] On the other hand, individually packaged absorbent articles are stored in a package in a state where multiple individually packaged absorbent articles are stacked on top of each other. Therefore, if paper with a smooth surface is used as the packaging sheet, the individually packaged absorbent articles may slip easily when stacking multiple individually packaged absorbent articles and storing them in a package, which may reduce production efficiency. In addition, paper with a smooth surface has an appearance and feel similar to so-called copy paper, giving a cheap impression.

[0008] The present invention has been made in consideration of the problems associated with the conventional technology as described above, and aims to provide an individually packaged absorbent article that can achieve both printability and avoidance of reduced production efficiency, even when multiple pieces are stacked and contained in a package. [Means for solving the problem]

[0009] In order to achieve the above object, the present invention provides An individually packaged absorbent article in which an absorbent article is individually packaged in a paper packaging sheet, The packaging sheet is printed on an exposed surface that is exposed when the absorbent article is individually packaged, The exposed surface has an MMD (mean coefficient of friction variation) of 0.050 or less before printing, and the static friction coefficient between the exposed surfaces of a plurality of individually packaged absorbent articles after printing is 0.60 or more.

[0010] In the present invention configured as described above, the MMD of the exposed surface of the absorbent article when individually packaged is 0.050 or less before printing, which makes the absorbent article suitable for printing. Furthermore, the static friction coefficient between the exposed surfaces of multiple individually packaged absorbent articles after printing is 0.60 or more, which makes the individually packaged absorbent articles less likely to slip when stacked and packaged in a package, thereby avoiding a decrease in production efficiency. Furthermore, the static friction coefficient between the exposed surfaces of multiple individually packaged absorbent articles after printing is 0.60 or more, which makes the individually packaged absorbent articles less likely to give a cheap impression in appearance and touch.

[0011] The packaging sheet may also be configured so that the blending ratio of recycled fibers is 20% or more.

[0012] In such a configuration, the coefficient of static friction between the exposed surfaces of the individually packaged absorbent articles after printing is applied is large.

[0013] The packaging sheet may also include fiber bundles.

[0014] In this configuration as well, the coefficient of static friction between the exposed surfaces of the individually packaged absorbent articles is increased after printing has been applied.

[0015] Also, as a method for producing a packaged product in which individually packaged absorbent articles are contained in a package, A step of printing on the packaging sheet; a step of placing the absorbent article on the packaging sheet, folding the packaging sheet so that the printed surface is exposed, and wrapping the absorbent article to manufacture the individually packaged absorbent article; The method may further include a step of stacking a plurality of the individually packaged absorbent articles and housing them in a package. Effect of the Invention

[0016] According to the present invention, even when a plurality of pieces are stacked and housed in a package, it is possible to achieve both printability and avoid a decrease in production efficiency. [Brief description of the drawings]

[0017] [Figure 1] 1 is a plan view showing one embodiment of an individually packaged absorbent article of the present invention. [Diagram 2] 2 is a plan view of the individually packaged absorbent article shown in FIG. 1 in an unfolded state. [Diagram 3] FIG. 2 is a cross-sectional view of II shown in FIG. [Figure 4] FIG. 2 is an enlarged view of part II shown in FIG. [Diagram 5] 5 is a flow chart for illustrating a process for producing a packaged product in which the individually packaged absorbent articles shown in FIGS. 1 to 4 are housed in a package. [Figure 6] FIG. 5 is a diagram showing a state in which the individually packaged absorbent articles shown in FIGS. 1 to 4 are contained in a package. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In each drawing, unless otherwise specified, the same or corresponding components are denoted by the same reference numerals and the description thereof will be omitted.

[0019] <Overall configuration of individually packaged absorbent article> Fig. 1 is a plan view showing one embodiment of an individually packaged absorbent article of the present invention. Fig. 2 is a plan view of the individually packaged absorbent article 100 shown in Fig. 1 in an unfolded state, as viewed from the inner surface of the packaging sheet 10 or from the skin side of the absorbent article 1. Fig. 3 is a cross-sectional view taken along line II shown in Fig. 1.

[0020] 1 to 3, the present embodiment is an individually packaged absorbent article 100 including a packaging sheet 10 and an absorbent article 1 individually packaged by the packaging sheet 10. As shown in Fig. 2, the packaging sheet 10 has an elongated shape, for example, in an unfolded state, and has a longitudinal direction (vertical direction) D1 and a lateral direction (lateral direction) D2 perpendicular to the longitudinal direction. The longitudinal direction D1 and the lateral direction D2 of the packaging sheet 10 also correspond to the longitudinal direction and the lateral direction of the absorbent article 1, respectively.

[0021] <Absorbent articles> The absorbent article 1 packaged in the packaging sheet 10 has a shape for being worn so as to face the excretion opening of bodily fluids (menstrual blood, vaginal discharge, urine, etc.), and is, for example, a flat and elongated article. Specific examples of the absorbent article 1 include sanitary napkins, panty liners (discharge sheets), light incontinence pads, etc.

[0022] As shown in FIG. 2, for example, the absorbent article 1 has a liquid-permeable top sheet 3, a liquid-impermeable back sheet (not shown), and an absorbent body 4 disposed between the top sheet 3 and the back sheet.

[0023] The back sheet may be a sheet material having at least water impermeability, such as an olefin resin sheet, such as polyethylene or polypropylene. A laminated nonwoven fabric in which a nonwoven fabric is laminated on a polyethylene sheet, or a laminated sheet of nonwoven fabric in which a waterproof film is interposed to ensure substantial liquid impermeability may be used. A material having moisture permeability may also be used.

[0024] A porous or non-porous nonwoven fabric, a porous plastic sheet, etc. are preferably used as the top sheet 3. Examples of material fibers constituting the nonwoven fabric include olefins such as polyethylene and polypropylene, synthetic fibers such as polyester and polyamide, regenerated fibers such as rayon and cupra, and blends of these fibers, as well as natural fibers such as cotton, which may be used alone or in combination of two or more kinds.

[0025] The absorbent body 4 is not limited as long as it is a material capable of absorbing and retaining body fluids, but preferably contains cotton-like pulp and a water-absorbing polymer. As the water-absorbing polymer, superabsorbent polymer granular powder (superabsorbent polymer (SAP)), superabsorbent fiber (SAF)), and a combination thereof can be used. As the pulp, there can be mentioned chemical pulp obtained from wood, cellulose fiber such as dissolving pulp, and artificial cellulose fiber such as rayon and acetate. As the pulp, hardwood pulp obtained from hardwoods, softwood pulp obtained from softwoods, or a mixture thereof can be used. Furthermore, the pulp can be recycled pulp regenerated from used pulp.

[0026] The thickness of the absorbent body 4 may be 0.5 to 25 mm. The absorbent body 4 may have a bulging structure in an area corresponding to the bodily fluid discharge outlet (area corresponding to the bodily fluid discharge outlet) and an area behind the area corresponding to the bodily fluid discharge outlet facing the gluteal crease. The absorbent body 4 has a size and shape that does not protrude from the top sheet 3 and the back sheet, and at the front and rear edge portions of the absorbent body, the outer edges of the back sheet and the top sheet 3 are joined by an adhesive such as hot melt, heat sealing, ultrasonic sealing, or other adhesive means.

[0027] 2, side sheets 7 may be provided along the longitudinal direction D1 on both ends in the short side direction D2 on the outer lateral sides of the absorbent body 4. As the side sheets 7, a water-repellent treated nonwoven fabric or a hydrophilic treated nonwoven fabric may be used.

[0028] 1 to 3, the absorbent article 1 is a so-called wingless type without wings, but it may be configured as an article with wings that extend to each side. The wings may be formed by joining the side sheet and the back sheet.

[0029] Furthermore, an anti-slip adhesive portion may be provided on the back sheet side (non-skin side, i.e., the side facing the underwear when worn) of the absorbent article 1 to prevent the absorbent article 1 from slipping off the underwear when attached to the underwear. The anti-slip adhesive portion is formed, for example, in the shape of multiple strips extending in the longitudinal direction D1 or the lateral direction D2.

[0030] The overall length of the absorbent article 1 can be 140 to 430 mm, and the width of the absorbent article 1 (the width of the main body excluding the wings if the absorbent article has wings) can be 40 to 130 mm.

[0031] <Wrapping sheet> The packaging sheet 10 in this embodiment is paper. Using a paper packaging sheet 10 can contribute to reducing plastic use and achieving the Sustainable Development Goals. Paper can also impart a unique texture, such as the appearance and feel of a natural material.

[0032] The packaging sheet 10 is made of, for example, Unryu paper, and is printed on the surface that is exposed when the absorbent article 1 is individually packaged. The packaging sheet 10 is not limited to Unryu paper as long as it satisfies the conditions described below. The conditions before and after printing on the packaging sheet 10 will be described later.

[0033] The dimensions of the packaging sheet 10 depend on the size and shape of the absorbent article 1 to be packaged, and for example, when the packaging sheet 10 is fully unfolded (not folded back), the length in the longitudinal direction D1 (sometimes simply referred to as the length) can be 100 to 450 mm, and the length in the transverse direction D2 (sometimes simply referred to as the width) can be 70 to 250 mm. In the illustrated example, the packaging sheet 10 has a rectangular shape when unfolded, but may have a shape such as an oblong shape.

[0034] <Packaging structure of individually packaged absorbent articles> As shown in Figs. 1 and 3, the absorbent article 1 is folded together with the packaging sheet 10 to be packaged, and an individually packaged absorbent article 100 is formed. When folding, as shown in Fig. 2, the absorbent article 1 is first placed on the inner surface of the packaging sheet 10 so that the back sheet side of the absorbent article 1 faces the inner surface of the packaging sheet 10. Then, the packaging sheet 10 and the absorbent article 1 are both folded in the longitudinal direction D1 at a first fold line F1 and a second fold line F2 along the width direction D2. More specifically, a first region R1 including one end 11 of the packaging sheet 10 in the longitudinal direction D1 is folded back in the longitudinal direction D1 at the first fold line F1, and a second region R2 including the other end 12 of the packaging sheet 10 in the longitudinal direction D1 is folded back at the second fold line F2. The region between the first region R1 and the second region R2 of the packaging sheet 10 is a third region R3. In the illustrated example, the packaging sheet 10 is folded so that the second region R2 is folded first and the first region R1 overlaps the outer surface of the second region R2 (FIGS. 1 and 2), but the folding order of the first region R1 and the second region R2 may be reversed. After the packaging sheet 10 and the absorbent article 1 are thus folded in three together (inner three fold) to wrap the absorbent article 1, both edges in the short direction D2 are sealed along the long direction D1, and the sealed portion 15 is formed.

[0035] Such a packaging format in which the absorbent article is folded in three or more can be formed relatively easily, can hygienically wrap the absorbent article 1, and also allows easy removal of the absorbent article 1. Note that the folding format is not limited to folding in three, and may be folded in four or more, or may be folded in half.

[0036] Furthermore, the individually packaged absorbent article 100 is provided with a fastening tape 30 in the vicinity of an edge of the first region R1 (one end 11 of the packaging sheet 10) and in the center in the short-side direction D2. As shown in FIG. 1, the fastening tape 30 can be provided across the first region R1 and the second region R2 so as to straddle one end 11 of the packaging sheet 10. By providing the fastening tape 30, when opening the individually packaged absorbent article 100, a user can hold the fastening tape 30 and lift and pull the first region R1, making opening easier. At that time, the first region R1 is peeled off from the second region R2 located thereunder.

[0037] <Sealing section> 1, in the individually packaged absorbent article 100, the regions on both edges in the short-side direction D2 where the absorbent article 1 is not present are sealed to form sealed portions 15. In this embodiment, the sealed portions 15 are formed by pressing the packaging sheets 10 together in the thickness direction by passing them through a pair of heated rolls.

[0038] 1, the sealed portion 15 is formed, for example, over the entire length in the longitudinal direction D1 of the individually packaged absorbent article 100. This is preferable from the viewpoint of preventing dirt, dust, or accidentally fingers or small objects from entering through the short edge (obtaining a sealable property).

[0039] The range in the short-side direction D2 in which the seal portion 15 is provided is, for example, a range up to 20 mm from the edge in the short-side direction D2. The seal portion 15 may be formed over the entire range, or may be formed in a portion of the range, for example, at a position away from the edge in the short-side direction D2. The length (width) of the seal portion 15 itself in the short-side direction D2 is preferably 3 to 15 mm. The inner edge of the seal portion 15 in the short-side direction D2 may extend linearly along the longitudinal direction D1, or may extend in a curved manner, for example, in a wavy manner.

[0040] FIG. 4 is an enlarged view of part II shown in FIG.

[0041] As shown in FIG. 4, the seal portion 15 includes, for example, a plurality of pressure-bonded portions (or joint portions) 15a that are spaced apart from each other in a plan view. Each pressure-bonded portion 15a is a portion in which packaging sheets 10 are joined together by pressure bonding in the thickness direction. In the illustrated example, the portion other than the plurality of pressure-bonded portions 15a is a non-joined portion in which the packaging sheets 10 are not joined together. In this way, since the plurality of pressure-bonded portions 15a are scattered apart from each other, the packaging sheets can be easily peeled apart from each other when opening the package, and the ease of opening can be improved, compared to, for example, a case in which the packaging sheets 10 are joined together continuously over the entire surface of the seal portion 15. In addition, it is possible to prevent both edges of the individually packaged absorbent article 100 from becoming excessively hard and impairing the feel.

[0042] 4, the shape of each of the compression-bonding parts 15a in plan view is a square, but is not limited to the shape shown in the figure, and may be, for example, a rectangle, a quadrangle other than a square such as a parallelogram, a polygon other than a quadrangle, a circle, an ellipse, a heart, a star, a teardrop, etc. The size of each of the compression-bonding parts 15a may be, for example, a square with one side measuring 0.25 to 2.5 mm, or a size having an area equivalent thereto.

[0043] <Manufacturing process of individually packaged absorbent articles> FIG. 5 is a flow chart for illustrating the process of producing a packaged product in which the individually packaged absorbent articles 100 shown in FIGS. 1 to 4 are housed in a package.

[0044] When manufacturing the individually packaged absorbent article 100 configured as described above, first, printing is applied to the packaging sheet 10 (step S1). Note that printing on the packaging sheet 10 is applied to the exposed surface that is exposed when the packaging sheet 10 individually packages the absorbent article 1.

[0045] Here, as described above, when printing is applied to the packaging sheet 10 in order to enhance the design of the individually packaged absorbent article 100, it is considered to use paper with high printability as the packaging sheet 10. Here, it is considered to improve the printability by using paper with a high surface smoothness and smoothness.

[0046] Therefore, an experiment was conducted to measure the MMD (mean coefficient of friction variation), which is an index of the smoothness of the paper surface, for various papers that could be used as the packaging sheet 10, and to determine whether the papers have high printability. In this experiment, the MMD was measured using a KES friction tester. The measurement conditions were as follows: a terminal wound with piano wire was used as the terminal, and the surface was traced over a distance of 30 mm at a speed of 1 mm / sec while applying a load of 50 g.

[0047] [Table 1] As shown in Table 1, in Example 1, the smooth surface of rayon PM (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 14 gsm was measured. In Example 2, the rough surface of rayon PM (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 14 gsm was measured. In Example 3, the smooth surface of Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 17 gsm was measured. In Example 4, the rough surface of Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 17 gsm was measured. In Example 5, the smooth surface of Kinshachi paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 24.4 gsm was measured. In Example 6, the rough surface of Kinshachi paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 24.4 gsm was measured. In Comparative Example 1, the smooth surface of crepe paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 18 gsm was measured. Rayon PM is a paper made up of 15% rayon and 85% pulp.

[0048] The MMD in Comparative Example 1 was 0.052. The MMD in Example 1 was 0.011, and the MMD in Example 2 was 0.017. The MMD in Example 3 was 0.014, and the MMD in Example 4 was 0.021. The MMD in Example 5 was 0.008, and the MMD in Example 6 was 0.013. The paper in Comparative Example 1 has a crepe finish on the surface, which results in low smoothness.

[0049] In Table 1, the printability is evaluated by marking "x" for cases where the ink was not evenly applied to the printed surface, resulting in blank areas, i.e., so-called missing prints, and "o" for cases where no missing prints occurred. As shown in Table 1, printing missing occurred in Comparative Example 1, while printing missing occurred in Examples 1 to 6. Furthermore, in Comparative Example 1, there was a tendency for wrinkles to easily occur on the surface after printing, which is thought to lead to the printing missing.

[0050] These results show that paper with a surface MMD of 0.050 or less before printing is suitable for use as packaging sheet 10, and by using this paper, printing can be applied to the surface of packaging sheet 10 to improve its design.

[0051] After printing is applied to the packaging sheet 10, the absorbent article 1 is placed on the packaging sheet 10, and the packaging sheet 10 is folded in three together with the absorbent article 1 so that the printed surface is exposed, thereby encasing the absorbent article 1.

[0052] Thereafter, both edges of the individually packaged absorbent article 100 in the short-side direction D2 are sealed along the long-side direction D1 to form the sealed portions 15 (step S2).

[0053] The step of printing on the packaging sheet 10, the step of wrapping the absorbent article 1 in the packaging sheet 10, and the step of forming the sealed portion 15 may be performed while the packaging sheet 10 is in a long state. In this case, after the sealed portion 15 is formed, the packaging sheet 10 is cut into a single piece to form the individually packaged absorbent article 100.

[0054] The individually packaged absorbent article 100 thus manufactured is then housed in a package, and a packaged product in which the individually packaged absorbent article 100 is housed in a package is completed (step S3).

[0055] FIG. 6 is a diagram showing a state in which the individually packaged absorbent article 100 shown in FIGS. 1 to 4 is contained in a package.

[0056] As shown in FIG. 6, the individually packaged absorbent articles 100 manufactured as described above are contained in a package in a state where a plurality of individually packaged absorbent articles 100 are stacked. In this case, if a paper with high smoothness and high printability is used as the packaging sheet 10, the individually packaged absorbent articles 100 tend to slip against each other. Therefore, the stacked individually packaged absorbent articles 100 will come apart on the conveying line that conveys the individually packaged absorbent articles 100. In particular, the separation is likely to occur in the fiber direction of the paper. Here, the above-mentioned individually packaged absorbent articles 100 may be automatically contained in the package on the conveying line. Therefore, if the stacked individually packaged absorbent articles 100 come apart, the separated individually packaged absorbent articles 100 will have to be manually contained in the package, which reduces production efficiency.

[0057] Therefore, an experiment was conducted to measure the coefficient of static friction between various papers that may be used as the packaging sheet 10 after printing, and to see whether the papers would come apart when inserted into a package. In this experiment, the coefficient of static friction was measured using a tribo-friction tester. The measurement conditions were such that 2 cm x 2 cm pieces of paper were moved against each other over a distance of 50 mm at a speed of 43 mm / sec while applying a load of 70 g.

[0058] [Table 2] As shown in Table 2, the rough surface of rayon PM with a basis weight of 14 gsm was measured as Comparative Example 1. The smooth surface of Unryu paper with a basis weight of 17 gsm was measured as Comparative Example 2. The rough surface of Unryu paper with a basis weight of 17 gsm was measured as Example 1.

[0059] The static friction coefficient in Comparative Example 1 was 0.577, and the static friction coefficient in Comparative Example 2 was 0.562. On the other hand, the static friction coefficient in Example 1 was 0.603.

[0060] In Table 2, those that broke apart when inserted into the package are marked with an "X" and those that did not break apart are marked with an "O". As shown in Table 2, in Comparative Examples 1 and 2, breakage occurred, but in Example 1, no breakage occurred.

[0061] From these results, if the packaging sheet 10 is made of paper with a static friction coefficient of 0.60 or more between the paper surfaces exposed after printing, the individually packaged absorbent articles 100 are less likely to slip apart when stacked and stored in a package. This makes it possible to avoid a decrease in production efficiency when the individually packaged absorbent articles 100 are stored in a package. In addition, the appearance and feel are less likely to give a cheap impression.

[0062] Here, the relationship between the ease of sliding between the individually packaged absorbent articles 100 and the blending ratio of the recycled fibers as described above will be described.

[0063] For various papers that could be used as the packaging sheet 10, the coefficient of static friction between the papers after printing was measured, and an experiment was conducted to see whether the blending ratio of recycled fibers affects the loosening that occurs when the paper is inserted into a package. In this experiment, the coefficient of static friction was measured using a tribo-friction tester. The measurement conditions were as follows: 2 cm x 2 cm pieces of paper were moved against each other over a distance of 50 mm at a speed of 43 mm / sec while applying a load of 70 g.

[0064] [Table 3] As shown in Table 3, measurements were taken on the rough surface of rayon PM with a basis weight of 14 gsm as Comparative Example 1. Measurements were taken on the rough surface of Unryu paper with a basis weight of 17 gsm as Example 1. In this case, the blending ratio of recycled fibers was 15% in Comparative Example 1, and the blending ratio of recycled fibers was 20 to 25% in Example 1.

[0065] The static friction coefficient in Comparative Example 1 was 0.577, while the static friction coefficient in Example 1 was 0.603.

[0066] In Table 3, those that came apart when inserted into the package are marked with an "X" and those that did not come apart are marked with an "O". As shown in Table 3, the rough surface of the rayon PM in Comparative Example 1 came apart, but the rough surface of the Unryu paper in Example 1 did not come apart.

[0067] From these results, if the packaging sheet 10 is made of paper with a recycled fiber content of 20% or more, multiple individually packaged absorbent articles 100 are less likely to slip apart when stacked and stored in a package, which makes it possible to avoid a decrease in production efficiency when the individually packaged absorbent articles 100 are stored in a package.

[0068] Here, the relationship between the ease of sliding between the individually packaged absorbent articles 100 as described above and the paper fiber bundles will be described.

[0069] As mentioned above, Unryu paper has a high coefficient of static friction between sheets of paper, making it difficult for the paper to slip. Here, Unryu paper contains fiber bundles made by twisting rayon fibers into a string shape and weaving them into bundles, which gives the paper a large uneven surface.

[0070] In this way, in paper containing fiber bundles, the coefficient of static friction increases as the surface unevenness increases. As a result, by using paper containing fiber bundles, not limited to Unryu paper, for the packaging sheet 10, when the individually packaged absorbent articles 100 are stacked and stored in a package after printing, they are less likely to come apart.

[0071] In the above-described embodiment, Unryu paper has been described as being particularly effective, but the effects of the present invention can be obtained with any paper, as long as the MMD of the exposed surface before printing is 0.050 or less, and the static friction coefficient between the exposed surfaces of multiple individually packaged absorbent articles after printing is 0.60 or more.

[0072] Although the present invention has been described above based on the embodiments, the present invention is not limited to these embodiments. The above-mentioned embodiments can be variously changed, modified, substituted, added, deleted, and combined within the scope of the claims, and these also belong to the technical scope of the present invention. In addition, the above-mentioned components can be arbitrarily combined. [Explanation of symbols]

[0073] 1. Absorbent articles 3 Top sheet 4. Absorber 7 Side seat 10 Packaging Sheet 11 Longitudinal end 12 Other end in the longitudinal direction 15 Seal part 15a Crimping part 30 Fastening Tape 100 individually packaged absorbent articles D1 Longitudinal direction of packaging sheet D2 Short side of packaging sheet F1 First fold line F2 Second fold line R1 1st area R2 2nd area R3 3rd area

Claims

1. An individually packaged absorbent article in which an absorbent article is individually packaged in a paper packaging sheet, The packaging sheet is printed on an exposed surface that is exposed when the absorbent article is individually packaged, The exposed surface has an MMD of 0.050 or less before printing, and the static friction coefficient between the exposed surfaces of a plurality of individually packaged absorbent articles after printing is 0.60 or more.

2. The individually packaged absorbent article according to claim 1 , wherein the packaging sheet contains recycled fibers at a blending ratio of 20% or more.

3. The individually packaged absorbent article of claim 1 , wherein the packaging sheet comprises fiber bundles.

4. A method for producing a packaged product in which the individually packaged absorbent article according to any one of claims 1 to 3 is contained in a package, comprising the steps of: A step of printing on the packaging sheet; a step of placing the absorbent article on the packaging sheet, folding the packaging sheet so that the printed surface is exposed, and wrapping the absorbent article to manufacture the individually packaged absorbent article; and stacking a plurality of the individually packaged absorbent articles and housing them in a package.

Citation Information

Patent Citations

  • Package structure of absorptive article

    JP2020196541A