Infrared sensor element, infrared sensor, and method for manufacturing infrared sensor element

By using a harder insulating film to cover semiconductor materials, the growth of grains is suppressed, improving thermoelectric properties and precision in infrared sensor elements.

JP2024143829APending Publication Date: 2024-10-11SEIKO NPC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023056731
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The growth of grains in semiconductor materials used in thermocouples during the film formation process for infrared sensor elements is uncontrolled, leading to degraded thermoelectric properties due to increased thermal conductivity.

Method used

A second insulating film made of a harder material than the semiconductor material is formed to cover at least the upper surface and side surfaces, suppressing grain growth during heat treatment and controlling grain size.

Benefits of technology

The thermoelectric properties are improved by controlling grain size, reducing resistance and conductivity, and minimizing substrate distortion, thereby enhancing the precision and quality of the infrared sensor element.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143829000001_ABST
    Figure 2024143829000001_ABST
Patent Text Reader

Abstract

To provide an infrared sensor element, an infrared sensor, and a method for manufacturing an infrared sensor element that facilitate control of the grain size of a semiconductor material forming a thermocouple and can improve thermoelectric characteristics.SOLUTION: An infrared sensor element 11 comprises: a first insulating film 101 formed on a surface of a substrate 84; and a thermocouple 75 formed on the first insulating film 101. The thermocouple 75 has a pair of semiconductor materials 751, 752, and a second insulating film 102 formed of an insulating material having higher hardness than the semiconductor materials 751, 752. The second insulating film 102 is formed to cover at least top faces 75A of the semiconductor materials 751, 752.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an infrared sensor element, an infrared sensor, and a method for manufacturing an infrared sensor element. [Background technology]

[0002] 2. Description of the Related Art Conventionally, a thermocouple in a thermopile-type infrared sensor element is known that uses a pair of semiconductor materials (for example, see Patent Document 1).

[0003] It is known that in semiconductor materials used as thermocouples, grains grow during the film formation process for forming the semiconductor material, and the grain size after film formation affects thermal conductivity (see Patent Document 2). If the grains of the semiconductor material grow excessively, and the thermal conductivity increases, there is a risk of the thermoelectric properties being reduced. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2014-77783 A [Patent Document 2] JP 2017-017068 A Summary of the Invention [Problem to be solved by the invention]

[0005] Incidentally, in the manufacturing process of an infrared sensor element using a pair of semiconductor materials as a thermocouple as in Patent Document 1, a heat treatment may be performed in a separate process after the film formation process for forming the semiconductor material. In such a case, after the film formation process for forming the semiconductor material, the grain growth of the semiconductor material is further promoted by the heat treatment in the other process, which poses a problem that it is not easy to control the grain size.

[0006] The present invention has been made to solve the above-mentioned problems, and has an object to provide an infrared sensor element, an infrared sensor, and a method for manufacturing an infrared sensor element that can easily control the grain size of the semiconductor material that constitutes a thermocouple and improve the thermoelectric characteristics. [Means for solving the problem]

[0007] The infrared sensor element according to a first aspect of the present invention comprises a first insulating film formed on a surface of a substrate, and a thermocouple formed on the first insulating film, the thermocouple having a pair of semiconductor materials and a second insulating film formed of an insulating material harder than the semiconductor materials, and the second insulating film is formed so as to cover at least a part or all of an upper surface of the semiconductor material.

[0008] According to the first aspect, the second insulating film made of an insulating material harder than the semiconductor material is formed so as to cover at least the upper surface of the semiconductor material, so that the grain growth of the semiconductor material is suppressed by heat treatment in a step other than the step of forming the semiconductor material, which makes it easier to control the grain size of the semiconductor material constituting the thermocouple, and improves the thermoelectric properties.

[0009] According to a second aspect of the present invention, in the infrared sensor element according to the first aspect, the second insulating film is made of silicon nitride.

[0010] According to the second aspect, since the second insulating film is made of silicon nitride, the intrusion of oxygen into the second insulating film is suppressed, and the oxidation of the semiconductor material can be prevented. As a result, the resistance value of the semiconductor material is reduced and the conductivity is excellent, thereby improving the thermoelectric characteristics.

[0011] In an infrared sensor element according to a third aspect of the present invention, in the configuration described in the first or second aspect, the substrate comprises a frame body formed in a frame shape, a heat absorption portion formed inside the frame body, and a beam portion connecting the frame body and the heat absorption portion, and the thermocouple is formed along the extension direction of the beam portion.

[0012] According to the third aspect, the substrate is connected by the beam between the frame formed in a frame shape and the heat absorbing part formed inside the frame. The thermocouple is formed along the extension direction of the beam of the substrate. In this structure in which the thermocouple made of semiconductor material is supported by the beam, the beam of the substrate is likely to be distorted by the heat treatment in the manufacturing process. However, by improving the control of the grain size of the semiconductor material by the above-mentioned second insulating film, the distortion of the substrate can be suppressed, and as a result, the accuracy of the shape, dimensions, etc. of the element can be improved.

[0013] In an infrared sensor element according to a fourth aspect of the present invention, in the configuration described in the first or second aspect, the second insulating film is formed so as to cover part or all of the upper surface and both side surfaces of the semiconductor material.

[0014] According to the fourth aspect, since the upper surface and both side surfaces of the semiconductor material are covered with the second insulating film, the grain growth of the semiconductor material is suppressed during heat treatment in a step other than the step of forming the semiconductor material, which makes it easier to control the grain size of the semiconductor material constituting the thermocouple, and improves the thermoelectric properties.

[0015] In the infrared sensor element according to the fifth aspect of the present invention, in the configuration described in the first or second aspect, the second insulating film is formed so as to cover a part or all of the upper surface of the semiconductor material, and the side surfaces along the thickness direction of the semiconductor material and the second insulating film are arranged in the same plane.

[0016] According to the fifth aspect, since the side surfaces along the thickness direction of the semiconductor material and the second insulating film are arranged on the same plane, the semiconductor material and the second insulating film can be etched simultaneously, thereby improving manufacturing efficiency.

[0017] According to a sixth aspect of the present invention, in the infrared sensor element according to the first or second aspect, the first insulating film and the second insulating film are formed of the same material.

[0018] According to the sixth aspect, since the first insulating film and the second insulating film are formed of the same material, the upper and lower surfaces of the semiconductor material are covered with insulating films having a harder material than the semiconductor material, and the grain growth of the semiconductor material is suppressed by heat treatment in a step other than the step of forming the semiconductor material. As a result, it is easy to control the grain size of the semiconductor material constituting the thermocouple, and the thermoelectric properties can be improved.

[0019] In a seventh aspect of the present invention, in the configuration described in the first or second aspect, the infrared sensor element further includes a third insulating film formed on the first insulating film and covering the semiconductor material and the second insulating film, and the third insulating film is formed of an insulating material having a lower hardness than the semiconductor material.

[0020] According to the seventh aspect, since the semiconductor material and the third insulating film covering the second insulating film are made of an insulating material having a lower hardness than the semiconductor material, it is possible to suppress distortion of the substrate that occurs when the insulating film is hardened by heat treatment in the film formation step of the third insulating film. As a result, the stress generated in the semiconductor material is reduced, and peeling and distortion of the thermocouple are suppressed, thereby improving the quality.

[0021] An infrared sensor according to an eighth aspect of the present invention includes the infrared sensor element according to any one of the above aspects and the substrate on which the infrared sensor element is supported, and a package in which the infrared sensor element is sealed.

[0022] According to the eighth aspect, it is possible to easily control the grain size of the semiconductor material constituting the thermocouple, thereby improving the thermoelectric characteristics.

[0023] A manufacturing method of an infrared sensor element according to a ninth aspect of the present invention is a manufacturing method of an infrared sensor element according to any of the above aspects, and includes a film formation step of forming the second insulating film so as to cover at least a part or all of an upper surface of the semiconductor material, and a film formation step of forming a third insulating film on the first insulating film so as to cover the semiconductor material and the second insulating film.

[0024] According to the ninth aspect, the grain growth of the semiconductor material is suppressed during the heat treatment in the step of forming the third insulating film, which is performed after the step of forming the second insulating film, making it easier to control the grain size of the semiconductor material constituting the thermocouple, and improving the thermoelectric characteristics. Effect of the Invention

[0025] According to the present invention, it is possible to easily control the grain size of the semiconductor material constituting the thermocouple, and improve the thermoelectric characteristics. [Brief description of the drawings]

[0026] [Figure 1] 1 is a perspective cross-sectional view of an infrared sensor according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a perspective view showing the infrared sensor with the lid substrate removed. [Diagram 3] 3 is a cross-sectional view of the infrared sensor element taken along line III-III in FIG. 2. [Figure 4] 4 is a cross-sectional view of the infrared sensor element taken along line IV-IV in FIG. 2. [Diagram 5] 1 is a schematic cross-sectional view showing a semiconductor device including an infrared sensor element according to an embodiment. [Figure 6] 5A to 5C are schematic cross-sectional views for explaining an example of a manufacturing process of the infrared sensor element according to the embodiment. [Figure 7]4 is a cross-sectional view showing an infrared sensor element according to a first modified example of the present embodiment, which corresponds to FIG. 3. [Figure 8] 5 is a cross-sectional view showing an infrared sensor element according to a second modified example of the present embodiment, which corresponds to FIG. 3. FIG. [Figure 9] 5 is a cross-sectional view showing an infrared sensor element according to a second modified example of the present embodiment, the cross-sectional view corresponding to FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0027] Hereinafter, an embodiment of the present invention will be described with reference to Fig. 1 to Fig. 5. In the embodiments and modifications described below, the same reference numerals may be used to designate corresponding configurations, and the description thereof may be omitted. In the following description, expressions indicating relative or absolute arrangements, such as "parallel", "orthogonal", "center", and "coaxial", do not only strictly indicate such arrangements, but also indicate a state in which the components are relatively displaced with a tolerance or an angle or distance that provides the same function.

[0028] <Infrared sensor 1> Fig. 1 is a perspective cross-sectional view of the infrared sensor 1. Fig. 2 is a perspective view showing the infrared sensor 1 with the lid substrate 22 removed. As shown in Figs. 1 and 2, the infrared sensor 1 includes a package 10 and an infrared sensor element 11 sealed in the package 10. In the following description, the thickness direction of the infrared sensor element 11 is defined as the Z direction (facing direction), and two directions perpendicular to the Z direction are defined as the X direction (first direction) and the Y direction (second direction), respectively.

[0029] <Package 10> The package 10 is a so-called vacuum package. Specifically, the package 10 includes a base substrate 21 and a lid substrate 22.

[0030] The base substrate 21 is a rectangular plate with the thickness direction being in the Z direction. A recess 24 that opens toward the +Z side is formed on a first surface 21a (surface facing the +Z side) of the base substrate 21. The recess 24 is formed in the center of the base substrate 21 in a plan view seen from the Z direction. Therefore, the first surface 21a of the base substrate 21 surrounds the periphery of the recess 24 in a plan view. The base substrate 21 is formed from a material such as silicon.

[0031] 1, the lid substrate 22 is formed in a cup shape that opens to the -Z side in a cross-sectional view along the Z direction. Specifically, the lid substrate 22 includes a top wall portion 31 and a peripheral wall portion 32 that extends from the outer periphery of the top wall portion 31 to the -Z side. The top wall portion 31 faces the base substrate 21 in the Z direction. The top wall portion 31 is formed so that its outer shape in a plan view is the same as that of the base substrate 21. The -Z side end face of the peripheral wall portion 32 is joined to the outer periphery of the first surface 21a of the base substrate 21 along the entire periphery. As a result, the portion surrounded by the base substrate 21 and the lid substrate 22 constitutes an accommodation space S1 that accommodates the infrared sensor element 11. In this embodiment, the accommodation space S1 is preferably sealed in a vacuum (or reduced pressure). However, the accommodation space S1 may be filled with a gas (argon, krypton, etc.) having excellent heat insulating properties.

[0032] The lid substrate 22 is preferably made of a material having a high infrared transmittance. As such a material, silicon, germanium, chalcogenide glass, and the like are preferably used. That is, in the infrared sensor 1 of this embodiment, infrared rays emitted from the target are incident into the storage space S1 through the lid substrate 22. In this embodiment, the storage space S1 is formed by two substrates, the base substrate 21 and the lid substrate 22, but the present invention is not limited to this configuration. For example, the storage space S1 may be formed by overlapping three or more substrates. In this embodiment, the storage space S1 is formed by overlapping substrates, but the storage space S1 may be formed by assembling a metal can to the base substrate 21, for example. In addition, the package 10 may be provided with a lens or the like to efficiently supply infrared rays to the infrared sensor element 11.

[0033] <Infrared sensor element 11> 1 and 2, the infrared sensor element 11 is a so-called thermopile type sensor element formed with a membrane structure. The infrared sensor element 11 receives infrared rays and generates a thermoelectromotive force in response to a temperature change caused by the infrared rays. The infrared sensor element 11 is accommodated in an accommodation space S1. Specifically, the infrared sensor element 11 includes a frame body 49, a heat absorbing portion 50, a first beam portion (beam portion) 51, and a second beam portion (beam portion) 52.

[0034] The frame body 49 is a thin-film substrate formed into a rectangular frame shape in a plan view. The frame body 49 is provided on the first surface 21a of the base substrate 21 so as to surround the periphery of the recess 24. In one example of this embodiment, the frame body 49 is made of silicon or the like.

[0035] The heat absorbing part 50 is formed in a rectangular (square) plate shape with the Z direction as the thickness direction. The heat absorbing part 50 extends along the Y direction and includes a first side (connecting side) 50a and a second side (connecting side) 50b that face each other in the X direction, and a third side 50c and a fourth side 50d that extend along the X direction and face each other in the Y direction. The heat absorbing part 50 is disposed inside the frame 49 at a position facing the recess 24 in the Z direction. In the illustrated example, the outer shape of the heat absorbing part 50 in a plan view is smaller than the outer shape of the recess 24 as viewed from the Z direction. The outer shape of the heat absorbing part 50 in a plan view can be changed as appropriate. The outer shape of the heat absorbing part 50 in a plan view may be a polygonal shape, a circle, or the like other than a rectangular shape. Furthermore, in this embodiment, the facing direction of the heat absorbing part 50 and the base substrate 21 is the Z direction. In this case, the opposing direction is the direction in which the substrate 21 overlaps with the base substrate 21 when viewed from either the X direction or the Y direction.

[0036] The first beam portion 51 and the second beam portion 52 are provided at positions on the outer periphery of the heat absorbing portion 50 that are rotationally symmetric (two-fold symmetric in the illustrated example) with respect to the center O of the heat absorbing portion 50 as viewed from the Z direction. Specifically, the first beam portion 51 is provided at the -Y side end of the first side 50a of the heat absorbing portion 50. The second beam portion 52 is provided at the +Y side end of the second side 50b of the heat absorbing portion 50. In the following description, the first beam portion 51 is used as an example for description, and a description of the configuration of the second beam portion 52 corresponding to the first beam portion 51 is omitted as appropriate.

[0037] The first beam portion 51 is formed in an L-shape when viewed from the Z direction. The first beam portion 51 includes a protruding portion (first extending portion) 60 and a connecting portion (second extending portion) 61.

[0038] The protruding portion 60 protrudes from the first side 50a of the heat absorbing portion 50 to the -X side. That is, the protruding portion 60 is connected to the heat absorbing portion 50 at a base end (first end: end on the heat absorbing portion 50 side). The base end of the protruding portion 60 functions as a hot junction of the infrared sensor element 11. The protruding portion 60 is formed so that the dimension (width) in the Y direction and the dimension (thickness) in the Z direction are uniform over the entire X direction.

[0039] The connection portion 61 extends from a tip portion (third end portion: end portion opposite to the heat absorbing portion 50) of the protruding portion 60 to the +Y side. The connection portion 61 extends along the first side 50a of the heat absorbing portion 50 while being spaced apart from the first side 50a in the X direction. The connection portion 61 is formed so that the dimensions in the X direction and the dimensions in the Z direction are uniform over the entire Y direction. The tip portion (second end portion: end portion opposite to the protruding portion 60) of the connection portion 61 is connected to the frame body 49. The tip portion of the connection portion 61 functions as a cold junction in the infrared sensor element 11.

[0040] Similar to the first beam portion 51, the second beam portion 52 includes a protruding portion (first extending portion) 70 and a connecting portion (second extending portion) 71. The protruding portion 70 protrudes from the second side 50b of the heat absorbing portion 50 toward the +X side. The connection portion 71 extends from the tip of the protruding portion 70 to the -Y side. The connection portion 71 extends along the second side 50b of the heat absorbing portion 50 while being spaced apart from the second side 50b in the X direction. The tip of the connection portion 71 (the end opposite to the protruding portion 60) is connected to the frame 49. Therefore, the heat absorbing portion 50 is supported by the frame 49 via the beam portions 51, 52.

[0041] As shown in FIG. 2, each beam 51, 52 is provided with a thermocouple 75 formed along the extending direction of each beam 51, 52. The thermocouple 75 is formed of a pair of conductive materials. In this embodiment, the pair of conductive materials is formed of a pair of semiconductor materials. Each semiconductor material extends on each beam 51, 52 so as to bridge between the frame 49 and the heat absorbing part 50. The pair of semiconductor materials constituting the thermocouple 75 are connected at the end on the heat absorbing part 50 side. The end of the thermocouple 75 on the heat absorbing part 50 side is arranged across the boundary between the base end (hot junction) of the protruding part 60 (or the protruding part 70) and the heat absorbing part 50. The end of the thermocouple 75 on the frame 49 side is arranged across the boundary between the tip end (cold junction) of the connecting part 61 (or the connecting part 71) and the frame 49.

[0042] <Thermocouple 75> Next, the thermocouple 75 will be described in detail with reference to Fig. 3 and Fig. 4. Fig. 3 is a cross-sectional view of the infrared sensor element 11 taken along line III-III in Fig. 2. Fig. 4 is a cross-sectional view of the infrared sensor element 11 taken along line IV-IV in Fig. 2.

[0043] 3 and 4, the infrared sensor element 11 has a substrate 84 which constitutes a frame 49, a heat absorbing portion 50, a first beam portion 51, and a second beam portion 52, a first insulating film 101 formed on the surface of the substrate 84, and a thermocouple 75 formed on the first insulating film 101. The first insulating film 101 is formed of silicon nitride, for example.

[0044] The thermocouple 75 has a first semiconductor material 751 and a second semiconductor material 752 as a pair of semiconductor materials. The first semiconductor material 751 and the second semiconductor material 752 can be used as a pair of different materials having different polarities of Seebeck coefficients. The first semiconductor material 751 is, for example, P-type polysilicon. The second semiconductor material 752 is, for example, N-type polysilicon. The first semiconductor material 751 and the second semiconductor material 752 are formed on the same plane on the upper surface of the first insulating film 101.

[0045] Further, the thermocouple 75 has a second insulating film 102 formed so as to cover the upper surface 75A and both side surfaces 75B of each of the semiconductor materials 751, 752. More specifically, the upper surface 75A and both side surfaces 75B of each of the semiconductor materials 751, 752 are in contact with the second insulating film 102. As an example, the second insulating film 102 is formed of silicon nitride. That is, in this embodiment, the upper surface 75A, both side surfaces 75B, and the lower surface 75C of each of the semiconductor materials 751, 752 are covered with an insulating film formed of silicon nitride.

[0046] The silicon nitride forming the first insulating film 101 and the second insulating film 102 is an insulating material having a higher hardness than the P-type and N-type polysilicon forming the first semiconductor material 751 and the second semiconductor material 752. Therefore, it is possible to suppress the growth of grains in each of the semiconductor materials 751, 752 due to heat treatment after the formation of the first insulating film 101 and the second insulating film 102.

[0047] Here, "high hardness" means that at least one of the Vickers hardness [HV] and the bending strength [MPa] is high, and preferably both of them are high. As an example, the thickness of the first semiconductor material 751 and the second semiconductor material 752 can be set to 200 [nm] to 500 [nm], and the thickness (film thickness) of the second insulating film 102 can be set to 15 [nm] to 200 [nm]. Within the above numerical range, the thickness of the second insulating film 102 can be set to be smaller than the thickness of the first semiconductor material 751 and the second semiconductor material 752, and preferably, the thickness of the second insulating film 102 is set to 15[%] or less of the thickness of the first semiconductor material 751 and the second semiconductor material 752.

[0048] 4 shows a cross section of the end portion of thermocouple 75 on the heat absorbing section 50 side. At the end portion of thermocouple 75 on the heat absorbing section 50 side, an end portion of first semiconductor material 751 and an end portion of second semiconductor material 752 are disposed across the boundary portion between the base end portion (hot junction) of protruding section 60 (or protruding section 70) and heat absorbing section 50, and are electrically connected.

[0049] In one example of this embodiment, the first semiconductor material 751 and the second semiconductor material 752 are connected by the conductive material 108 through the contact hole 106. Also, an infrared absorbing film 110 is formed so as to cover the conductive material 108 (hot junction).

[0050] The first semiconductor material 751 and the second semiconductor material 752 are formed on a first insulating film 101 formed on the substrate 84. In addition, a second insulating film 102 covering the first semiconductor material 751 and the second semiconductor material 752 is formed on the first insulating film 101. A third insulating film 103 is further formed on the first insulating film 101 to cover the semiconductor materials 751, 752 and the second semiconductor material 752. As an example, the third insulating film 103 is an oxide film formed of silicon oxide. The third insulating film 103 may also be referred to as an interlayer insulating film. The silicon oxide forming the third insulating film 103 is an insulating material having a lower hardness than the P-type and N-type polysilicon forming the first semiconductor material 751 and the second semiconductor material 752 .

[0051] In this embodiment, a conductive material 108 is formed on the third insulating film 103. A contact hole 106 is formed in the third insulating film 103 between the first semiconductor material 751 and the second semiconductor material 752 and the conductive material 108. An infrared absorbing film 110 is formed on the third insulating film 103 covering the conductive material 108, thereby constituting the heat absorbing portion 50. In FIGS. 3 and 4, the third insulating films 103 are illustrated as an integrated unit. In addition, in FIGS. 1 and 2, the third insulating film 103 and the infrared absorbing film 110 are omitted from illustration.

[0052] The conductive material embedded in the contact holes 106 and the conductive material 108 are, for example, aluminum. The infrared absorbing film 110 may be made of silicon oxide, silicon nitride, a gold black film, or the like.

[0053] Next, an example of a manufacturing process for the infrared sensor element 1 will be described with reference to Fig. 5 and Fig. 6(A) to Fig. 6(D). Fig. 5 is a schematic cross-sectional view of a semiconductor device S1 including an infrared sensor 1. As shown in this figure, the semiconductor device S1 constitutes a monolithic IC in which the infrared sensor 1 and a peripheral circuit section 2 are formed on a common base substrate 21. The peripheral circuit section 2 includes, as an example, a transistor section 201.

[0054] The transistor section 201 is composed of a MOSFET, for example. The transistor section 201 has a transistor region 202 formed in a part of the upper layer region of the base substrate 21, and a gate electrode 204 provided on the transistor region 202 via an oxide insulating film 203. The transistor region 202 is formed by implanting an impurity of a predetermined conductivity type at an appropriate concentration.

[0055] That is, the semiconductor device S1 has a base substrate 21 on which the peripheral circuit section 2 is formed, and a substrate 84 on which the infrared sensor element 11 is formed, and is configured by disposing the substrate 84 on the base substrate 21.

[0056] 6(A) shows a process of forming a semiconductor material. In this process, a first semiconductor material 751 and a second semiconductor material 752 are formed on a first insulating film 101 formed on the surface of a substrate 84. As an example, each semiconductor material is given a corresponding conductivity type by forming a semiconductor layer on the first insulating film 101 and injecting P-type or N-type impurity ions into the semiconductor layer. Then, by pattern forming using photolithography, the first and second semiconductor materials 751, 752 are formed in elongated shapes along the extension direction of the beam portions 51, 52 of the substrate 84.

[0057] 6(B) shows the film formation step of the second insulating film 102. In this step, the second insulating film 102 is formed so as to cover the first and second semiconductor materials 751, 752. By this film formation step, the second insulating film 102 comes into contact with the upper surface 75A and both side surfaces 75B of the first and second semiconductor materials 751, 752.

[0058] Next, the substrate 84 is disposed on the base substrate 21, and the transistor section 201 is formed (peripheral circuit section forming process). In the peripheral circuit section forming process, ions of a predetermined conductive impurity are implanted into a part of the upper layer region of the base substrate 21 to form the transistor region 202. Thereafter, as shown in FIG. 6(C), the base substrate 84 is heated in an oxygen atmosphere to oxidize the surface of the transistor region 202 and form the oxide insulating film 203. The heating temperature at this time is, for example, 700° C. to 900° C., and the infrared sensor element 11 disposed on the base substrate 21 is also heated. Here, the first and second semiconductor materials 751 and 752 have contact surfaces (upper surface 75A and both side surfaces 75B) with the second insulating film 102, and the growth of grains at the contact surfaces due to heat treatment during the formation of the oxide insulating film 203 is suppressed.

[0059] After the oxide insulating film 203 is formed, a semiconductor layer made of polysilicon is formed on the oxide insulating film 203. Impurity ions of a conductivity type corresponding to the gate electrode 204 are implanted into the semiconductor layer. Thereafter, the semiconductor layer is etched together with the oxide insulating film 203 to form the gate electrode 204. As a result, the gate electrode 204 is formed on the transistor region 202 of the base substrate 21 via the oxide insulating film 203.

[0060] 6(D), a film formation step is performed to form a third insulating film 103 on the upper surface of the base substrate 21. Thereafter, a contact hole 106 is formed in the third insulating film 103, and a conductive material 108 is deposited and patterned into a desired wiring pattern shape. An infrared absorbing film 110 is formed on the third insulating film 103 to serve as the heat absorbing portion 50. In this way, the infrared sensor element 11 is formed.

[0061] Finally, the entire base substrate 21 is annealed (heat treated) to activate the semiconductor layer of the transistor section 201, thereby forming the infrared sensor element 1 and the peripheral circuit section 2 on the base substrate 21. The heating temperature at this time is, for example, 400°C to 1000°C. Here too, the infrared sensor element 11 arranged on the base substrate 21 is heated, but the growth of grains in the first and second semiconductor materials 751, 752 at the contact surfaces with the second insulating film 102 is suppressed.

[0062] (Action and Effects) In the infrared sensor 1 of this embodiment, infrared rays radiated from an object pass through the top wall portion 31 of the lid substrate 22 and enter the infrared absorbing film 110 of the heat absorbing portion 50. This causes the temperature of the heat absorbing portion 50 to rise. The heat absorbed by the heat absorbing portion 50 is transferred to the protruding portions 60, 70 at the beam portions 51, 52, and then transferred to the package 10 through the connecting portions 61, 71. At this time, a thermoelectromotive force is generated in the thermocouple 75 based on the temperature difference between the base ends (hot junctions) of the protruding portions 60, 70 and the tip ends (cold junctions) of the connecting portions 61, 71. In the infrared sensor element 11, the thermoelectromotive forces generated in the thermocouples 75 are added together and output as an electrical signal.

[0063] In this embodiment, the second insulating film 102 is made of an insulating material having a higher hardness than the first semiconductor material 751 and the second semiconductor material 752 constituting the thermocouple 75, and is formed so as to cover the upper surface 75A and both side surfaces 75B of the semiconductor materials 751 and 752, so that the grain growth of the semiconductor material is suppressed by heat treatment in a process other than the process of forming the semiconductor material. As a result, it is easy to control the grain size of the semiconductor material constituting the thermocouple, and the thermoelectric characteristics can be improved.

[0064] In addition, in this embodiment, since the second insulating film 102 is made of silicon nitride, it is possible to suppress the intrusion of oxygen into the second insulating film 102 and prevent oxidation of the semiconductor materials 751, 752. As a result, the resistance value of each of the semiconductor materials 751, 752 is reduced and the conductivity is excellent, thereby improving the thermoelectric characteristics.

[0065] In this embodiment, the substrate 84 of the infrared sensor element 11 is connected between the frame 49 formed in a frame shape and the heat absorbing portion 50 formed inside the frame 49 by the beams 51 and 52. The thermocouple 75 is formed along the extending direction of the beams 51 and 52 of the substrate 84. In this manner, in a structure in which the thermocouple 75 made of a semiconductor material is supported by the beams 51 and 52, the beams 51 and 52 of the substrate 84 are likely to be distorted by heat treatment in the manufacturing process. However, by improving the control of the grain size of the semiconductor material by the second insulating film 102 described above, the distortion of the substrate 84 can be suppressed, and as a result, the accuracy of the shape, dimensions, etc. of the element can be improved.

[0066] Moreover, in this embodiment, since the first insulating film 101 and the second insulating film 102 are formed of the same material, the upper surface 75A and the lower surface 75C of each of the semiconductor materials 751, 752 are covered with an insulating film having a harder hardness than each of the semiconductor materials 751, 752. This suppresses the growth of grains of the semiconductor material during heat treatment in a process other than the process of forming the semiconductor material. As a result, it becomes easier to control the grain size of the semiconductor material that constitutes the thermocouple 75, and the thermoelectric characteristics can be improved.

[0067] Furthermore, in this embodiment, the third insulating film 103 covering the semiconductor materials 751, 752 and the second insulating film 102 is made of an insulating material having a lower hardness than the semiconductor materials 751, 752. This makes it possible to suppress distortion of the substrate 84 that occurs when the insulating film is hardened during heat treatment in the film formation process of the third insulating film 103. As a result, stress generated in the semiconductor materials 751, 752 is reduced, and peeling and distortion of the thermocouple 75 are suppressed, thereby improving quality.

[0068] Since the infrared sensor 1 of this embodiment is equipped with the above-mentioned infrared sensor element 11, it is possible to easily control the grain size of the first semiconductor material 751 and the second semiconductor material 752 that constitute the thermocouple 75, thereby improving the thermoelectric characteristics.

[0069] 6(B) to 6(D), the grain growth of the semiconductor materials 751 and 752 is suppressed during the heat treatment in the step of forming the third insulating film, which is performed after the step of forming the second insulating film. As a result, it is easy to control the grain size of the semiconductor material constituting the thermocouple 75, and the thermoelectric characteristics can be improved.

[0070] <First Modification of Infrared Sensor Element> The technical scope of the present invention is not limited to the above-mentioned embodiment, and various modifications can be made within the scope of the present invention. For example, in the above-mentioned embodiment, the second insulating film 102 is formed to cover the upper surface 75A and both side surfaces 75B of the first semiconductor material 751 and the second semiconductor material 752, but this is not limited. For example, as in an infrared sensor element 111A according to a first modification shown in FIG. 7, the second insulating film 102 may be formed to cover the upper surface 75A of the first semiconductor material 751 and the second semiconductor material 752. In this infrared sensor element 111A, the side surfaces along the thickness direction of each semiconductor material 751, 752 and the second insulating film 102 are arranged on the same plane.

[0071] In this configuration, after the second insulating film 102 is formed on the semiconductor layer forming the first semiconductor material 751 and the second semiconductor material 752, each of the semiconductor materials 751, 752 and the second insulating film 102 can be etched simultaneously, thereby improving manufacturing efficiency.

[0072] Furthermore, in the above configuration, the second insulating film 102 having high hardness is in contact with the upper surface of the semiconductor material, which is greatly affected by heat treatment, so that it is possible to suppress the growth of grains in each of the semiconductor materials 751, 752 during heat treatment in other processes performed after the film formation process of the second insulating film 102.

[0073] <Second Modification of Infrared Sensor Element> In the above embodiment, the first semiconductor material 751 and the second semiconductor material 752 are formed on the first insulating film 101, but the present invention is not limited to this. The first semiconductor material 751 and the second semiconductor material 752 may be arranged in a laminated state, as in an infrared sensor element 111B according to a second modified example shown in Fig. 8 and Fig. 9.

[0074] As shown in FIG. 8, in the infrared sensor element 111B according to the second modification, a first semiconductor material 751 is formed on a first insulating film 101, a second insulating film 102 covering the first semiconductor material 751 is formed on the first insulating film, a second semiconductor material 752 is formed on the second insulating film, and a second insulating film 102 covering the second semiconductor material 752 is formed on the second insulating film. The two second insulating films 102 formed on the semiconductor materials 751 and 752 cover the upper surfaces of the first semiconductor material 751 and the second semiconductor material 752, respectively. In addition, the side surfaces of the semiconductor materials 751 and 752 and the two second insulating films are arranged on the same plane along the thickness direction. The vertical relationship of the first semiconductor material 751 and the second semiconductor material 752 in the stacked state is not particularly limited, and the lower layer side may be composed of the second semiconductor material 752.

[0075] 9, contact holes for obtaining electrical connection are formed at the ends of the semiconductor materials 751, 752. In this modification, as in the above embodiment, the ends of the semiconductor materials 751, 752 on the heat absorption portion 50 side are electrically connected to each other via the contact holes 106 and the conductive material 108.

[0076] In the manufacturing method of the infrared sensor element 111B having such a configuration, a semiconductor layer for forming the first semiconductor material 751 is provided on the first insulating film 101 formed on the substrate 84, a second insulating film 102 covering the first semiconductor material 751 is formed thereon, a semiconductor layer for forming the second semiconductor material 752 is provided on the second insulating film 102, and a second insulating film 102 covering the second semiconductor material 752 is formed thereon. Then, the two semiconductor layers and the two second insulating films 102 are simultaneously etched to form the first semiconductor material 751, the second semiconductor material 752, and the two second insulating films 102. Then, a third insulating film 103 covering the semiconductor materials 751, 752, and the second insulating film 102 is formed on the first insulating film 101, and a contact hole 106 is formed. Then, a conductive material 108 is deposited and patterned into a desired wiring pattern shape. Finally, an infrared absorbing film 110 is formed on the third insulating film 103 to form the heat absorbing portion 50. In this way, the infrared sensor element 111B is formed.

[0077] Also, in the above configuration, the second insulating film 102 having high hardness contacts the upper surface of the semiconductor material, which is greatly affected by heat treatment, so that it is possible to suppress the growth of grains in each of the semiconductor materials 751, 752 during heat treatment in other processes performed after the film formation process of the second insulating film 102.

[0078] Furthermore, by arranging the first semiconductor material 751 and the second semiconductor material 752 in a stacked state, it is possible to arrange twice the number of thermocouples in a given unit area as in the above embodiment, thereby increasing the sensitivity of the infrared sensor.

[0079] In the above embodiment, the beams 51, 52 are formed in an L-shape having the protrusions 60, 70 and the connecting portions 61, 71, but the present invention is not limited to this configuration. The shape of the beams 51, 52 can be changed as appropriate as long as the cross-sectional area of ​​the base end is larger than the cross-sectional area of ​​the tip end. In this case, the beams may extend in a straight line or a curved line. In the above-described embodiment, the beams 51 and 52 are provided at positions that are dyad-symmetrical to the heat absorbing unit 50, but the present invention is not limited to this configuration. Any number of beams can be provided at any positions on the heat absorbing unit 50. In the above-described embodiment, a configuration in which one infrared sensor element 11 is sealed in one package 10 has been described as an example, but a configuration in which multiple infrared sensor elements 11 are arranged in an array in one package 10 may also be used.

[0080] In the above embodiment and each modified example, the first insulating film 101 is configured to be made of silicon nitride, but the present invention is not limited to this and may be configured to be made of silicon oxide. In addition, in the above embodiment and each modified example, the third insulating film 103 is configured to be made of silicon oxide, but the present invention is not limited to this, and the third insulating film 103 may be configured to be made of silicon nitride.

[0081] In the above embodiment and each modified example, the upper surface 75A and both side surfaces 75B of the first and second semiconductor materials 751, 752 are entirely covered with the second insulating film 102, but the present invention is not limited to this and may be configured to cover only a part of the upper surface 75A and both side surfaces 75B of the first and second semiconductor materials 751, 752. For example, the end portions (contact portions between the first semiconductor material 751 and the second semiconductor material 752) where the contact holes 106 are provided on the upper surfaces 75A and both side surfaces 75B of the first and second semiconductor materials 751, 752 may not be covered with the second insulating film 102.

[0082] In addition, within the scope of the invention, it is possible to replace the components in the above-described embodiments with well-known components, and it is also possible to combine the above-described modified examples as appropriate. [Explanation of symbols]

[0083] 1. Infrared sensor 10 Packages 11 Infrared sensor element 84 Substrate 75 Thermocouple 101 First insulating film 102 Second insulating film 103 Third insulating film 751 First Semiconductor Materials (Semiconductor Materials) 752 Secondary Semiconductor Materials (Semiconductor Materials)

Claims

1. A first insulating film formed on a surface of a substrate; a thermocouple formed on the first insulating film; The thermocouple includes a pair of semiconductor materials and a second insulating film formed of an insulating material having a hardness higher than that of the semiconductor materials, The second insulating film is formed so as to cover at least a part or the whole of the upper surface of the semiconductor material. Infrared sensor element.

2. the second insulating film is formed of silicon nitride; 2. The infrared sensor element according to claim 1.

3. The substrate is A frame formed in a frame shape; A heat absorbing portion formed on the inside of the frame; a beam portion connecting the frame body and the heat absorbing portion, The thermocouple is formed along the extending direction of the beam portion.

3. The infrared sensor element according to claim 1 or 2.

4. The second insulating film is formed so as to cover a part or all of the upper surface and both side surfaces of the semiconductor material.

3. The infrared sensor element according to claim 1 or 2.

5. The second insulating film is formed so as to cover a part or the whole of the upper surface of the semiconductor material, and the side surfaces of the semiconductor material and the second insulating film along a thickness direction are arranged on the same plane.

3. The infrared sensor element according to claim 1 or 2.

6. the first insulating film and the second insulating film are formed of the same material; 3. The infrared sensor element according to claim 1 or 2.

7. a third insulating film formed on the first insulating film and covering the semiconductor material and the second insulating film; The third insulating film is formed of an insulating material having a lower hardness than the semiconductor material.

3. The infrared sensor element according to claim 1 or 2.

8. The infrared sensor element according to claim 1 or 2, the infrared sensor element includes a substrate on which the infrared sensor element is supported; a package in which the infrared sensor element is sealed; An infrared sensor comprising:

9. A method for manufacturing the infrared sensor element according to claim 1 or 2, comprising the steps of: forming the second insulating film so as to cover at least a part or all of the top surface of the semiconductor material; forming a third insulating film on the first insulating film to cover the semiconductor material and the second insulating film; A method for manufacturing an infrared sensor element.

Citation Information

Patent Citations

  • Thermopile infrared detector

    CN112951974A

  • Sensor and method for manufacturing the same

    JP2001326367A

  • Thermopile infrared sensor, and inspection method therefor

    JP2002340668A

  • Infrared sensor

    JP2006184151A

  • Infrared detection element and manufacturing method therefor

    JP2009031197A