Process for producing metal oxide by spray-roasting nitrate
The spray roasting of nitrates in a torrefaction furnace, combined with gas cooling and multi-stage absorption, addresses the challenges of chloride ion issues and particle size control in producing metal oxides, resulting in high-purity products with efficient production.
Patent Information
- Application Number
- JP2024051781
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2024-03-27
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-03-27
AI Technical Summary
Existing spray roasting methods using chlorides to produce metal oxides face challenges with high thermal decomposition temperatures, leading to excessive chlorine ions and unsuitable product purity and particle size control.
A process involving the spray roasting of nitrates in a torrefaction furnace, followed by gas cooling, metal oxide collection, and multi-stage gas absorption to produce metal oxides, utilizing a Venturi preconcentrator and alkaline scrubbing to manage chloride ions and control particle size and purity.
The process achieves high-purity metal oxides with controlled particle size and improved manufacturing efficiency, avoiding chloride ion exceedance and ensuring low process temperatures.
Smart Images

Figure 2024144350000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the technical field of roasting processes, and in particular to a process for producing metal oxides by spray roasting of nitrates. [Background technology]
[0002] The spray roasting method is a very promising material preparation method. Compared with traditional preparation techniques, it has many advantages, such as controllable particle size, high product purity, good particle dispersibility, high production efficiency, and low process temperature, and has been applied in many fields of material science.
[0003] In existing technologies such as the system for producing tricobalt tetroxide using a spray roasting method disclosed in Chinese Patent No. 201921313792.2 and the system for producing tricobalt tetroxide using a spray roasting method and its production process disclosed in Chinese Patent No. 201910747775.8, when chlorides are used to produce metal oxides in a spray roasting furnace, the chlorides have a high thermal decomposition temperature and are difficult to decompose, so the chloride ions in the metal oxides tend to exceed the standard. Since these technologies are not suitable for producing metal oxides, a roasting process suitable for metal oxides is required. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Chinese Patent No. 201921313792.2 [Patent Document 2] Chinese Patent No. 201910747775.8 Summary of the Invention
[0005] It is an object of the present invention to provide a process for producing metal oxides by spray roasting of nitrates.
[0006] In order to achieve the above objectives, the present invention is implemented by the following technical solutions.
[0007] The present invention includes the following steps S1 to S6.
[0008] In S1, the nitrate solution is filtered to remove impurities, then concentrated in a pre-concentrator and fed to a roasting furnace. The nitrate solution is sprayed under pressure into the roasting furnace by a roasting furnace feed pump to carry out spray roasting decomposition. The nitrate decomposition products include metal oxides, NO2 gas and water vapor.
[0009] In S2, the furnace gas from the roaster is transported to the pre-concentrator, where the roaster gas generated after spraying and roasting nitrates in the roaster is cooled by the pre-concentrator, and at the same time, the newly introduced nitrate solution is concentrated and the dust in the roaster gas is removed.
[0010] In S3, the metal oxide is dropped from the bottom of the roasting furnace, and the conveying air generated by the conveying fan and filtered by the filter conveys the metal oxide powder to the powder silo, where the metal oxide is cooled as it passes through the conveying air. A sintered plate dust collector is installed at the top of the powder silo, and a packaging machine for packaging the metal oxide is installed at the bottom of the powder silo.
[0011] In S4, the roaster gas that has passed through the pre-concentrator is fed into a primary cooling tower, a primary absorption tower, a secondary cooling tower, a secondary absorption tower, or a multi-stage cooling tower and an absorption tower that are staggered from each other, where the NO2 gas is absorbed to produce regenerated nitric acid. When the absorption is complete, the temperature of the roaster gas is lowered and then the gas is fed into the exhaust gas fan.
[0012] In S5, a liquid alkali scrubber installed behind the exhaust gas fan scrubs the roaster gas again.
[0013] In S6, the gas that has passed through the scrubbing tower is cleaned with a wet electrostatic precipitator and then discharged to the outside through a chimney.
[0014] Preferably, the preconcentrator is a Venturi preconcentrator. The preconcentrator reduces the temperature of the roaster gas from 300-500°C to 95°C or less and concentrates the nitrate solution to 15-35%. In step S1, the reaction temperature in the roaster is 400-850°C. In step S4, the temperature of the roaster gas is reduced to 40°C or less as soon as the absorption is completed.
[0015] Further, the roaster includes a roaster body, a rotary valve, a furnace body exhaust pipe, a combustion assembly conduit, a gas regulating valve, an air regulating valve, an exhaust temperature detector, an exhaust temperature detector, an exhaust pressure detector, a furnace body temperature detector, a conduit front stage temperature detector, a conduit rear stage temperature detector, a spray nozzle, a solution regulating valve, a water supply regulating valve, and a compressed air regulating valve, a lower end exhaust port of the roaster body is connected to the rotary valve, an exhaust port is provided at an upper end of the roaster body, the exhaust port of the roaster body is connected to one end of the furnace body exhaust pipe, a discharge end of the spray nozzle is located at an upper stage in the roaster body, a combustion end of the combustion assembly conduit is located inside the roaster body, the gas regulating valve and the air regulating valve are provided at a supply end of the combustion assembly conduit, and the gas regulating valve and the air regulating valve are provided at a supply end of the combustion assembly conduit, Located outside the roasting furnace body, the discharge temperature detector is provided at the supply end of the rotary valve, the exhaust temperature detector and the exhaust pressure detector are provided on the outer walls of the supply end and the discharge end of the roasting furnace body exhaust pipe, respectively; the roasting furnace body temperature detector is a plurality of furnace body temperature detectors, each of which is provided on the side wall of the roasting furnace body; the front-end temperature detector and the rear-end temperature detector are provided on the side walls of the discharge end and the supply end of the combustion assembly roasting furnace, respectively; the supply end of the spray nozzle is simultaneously connected to the discharge ends of the feedwater regulating valve, the compressed air regulating valve and the solution regulating valve; the supply end of the solution regulating valve is connected to a solution supply assembly, the supply end of the feedwater regulating valve is connected to a feedwater assembly, and the supply end of the compressed air regulating valve is connected to an air supply device.
[0016] As an improvement, a block crusher and a crusher drive motor are provided between the discharge end of the roasting furnace body and the rotary valve, the supply end of the block crusher is connected to the discharge end of the roasting furnace body, the discharge end of the block crusher is connected to the rotary valve, and the drive end of the block crusher is connected to the drive output shaft of the crusher drive motor.
[0017] Preferably, the number of the spray nozzles is multiple, and all of the multiple spray nozzles are located at an upper stage in the roasting furnace body.
[0018] As an improvement, an air flow sensor is provided between the combustion assembly conduit and the air regulating valve, a gas flow sensor is provided between the combustion assembly conduit and the gas regulating valve, and a flame detector is provided in the combustion assembly conduit, a sensing end of the flame detector being located within the combustion assembly conduit.
[0019] The beneficial effects of the present invention are as follows:
[0020] The present invention is a process for producing metal oxide by spray roasting nitrate. Compared with the prior art, the present invention improves the process and equipment based on the prior art, and uses nitrate spray pyrolysis to produce ternary battery materials, thereby improving the purity of metal oxide and avoiding the chloride ion exceeding the standard. The improved roasting furnace has the advantages of controllable particle size, high product purity, good particle dispersibility, high production efficiency, and low process temperature, which is worthy of popularization and application. [Brief description of the drawings]
[0021] [Figure 1] FIG. 1 is a flow diagram illustrating the process of the present invention. [Diagram 2] FIG. 2 is a schematic diagram showing the structure of a roasting furnace of the present invention. [Diagram 3] FIG. 2 is a schematic diagram showing the structure of the combustion assembly of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] The present invention will be further described below in conjunction with the drawings and specific examples, but the illustrative examples and descriptions of the present invention are intended to interpret the present invention and are not intended to limit the present invention.
[0023] As shown in FIG. 1, the present invention includes the following steps S1 to S6.
[0024] In S1, the nitrate solution is filtered to remove impurities, then concentrated in a pre-concentrator and fed to a roasting furnace. The nitrate solution is sprayed under pressure into the roasting furnace by a roasting furnace feed pump to carry out spray roasting decomposition. The nitrate decomposition products include metal oxides, NO2 gas, and water vapor (which also contains oxygen, NO, NO2, N2O3, and N2O4, and is mainly composed of NO2).
[0025] In S2, the furnace gas from the roaster is transported to the preconcentrator, where the roaster gas (NO2, H2O, combustion exhaust gas, dust) generated after spraying and roasting nitrates in the roaster is cooled by the preconcentrator to lower the temperature of the roaster gas from 300-500°C to below 95°C, while concentrating the newly introduced nitrate solution (concentrating the nitrate solution to 15-35%) and removing the dust in the roaster gas.
[0026] In S3, the metal oxide is dropped from the bottom of the roasting furnace, and the conveying air generated by the conveying fan and filtered by the filter conveys the metal oxide powder to the powder silo, the metal oxide is cooled as it passes through the conveying air, and is cleaned and purified by the sintered plate dust collector installed at the top of the powder silo. The purified air is then discharged, and the powder at the bottom collected by the sintered plate dust collector is dropped back into the powder silo, and a packaging machine for packaging the metal oxide is installed at the bottom of the powder silo.
[0027] In S4, the roaster gas that has passed through the pre-concentrator is fed into a primary cooling tower, a primary absorption tower, a secondary cooling tower, a secondary absorption tower, or a multi-stage cooling tower and an absorption tower that are staggered from each other, where the NO2 gas is absorbed to produce regenerated nitric acid. When the absorption is complete, the temperature of the roaster gas is lowered and then the gas is fed into the exhaust gas fan.
[0028] In S5, a liquid alkali (or ammonia water) scrubber installed behind the exhaust gas fan scrubs the roaster gas again, and the scrubbed wastewater is discharged to a sewage treatment plant for treatment to meet the emission standards.
[0029] In S6, the gas that has passed through the scrubbing tower is removed by a wet electrostatic precipitator and then put into a chimney to be discharged to the outside, and the washing wastewater from the wet electrostatic precipitator is also discharged to a wastewater treatment plant for treatment. The temperature of the flue gas is less than 40°C, the water vapor content is less than 10%, and other indicators are lower than China's emission standards. As another technical solution, the gas that has passed through the scrubbing tower can also be denitrified by selective catalytic reduction (SCR) denitrification technology to make the nitrogen oxides reach the standard value, and then put into a chimney to be discharged to the outside.
[0030] The absorption of nitrogen oxides is carried out by the method of cooling + absorption + cooling + absorption, which produces HNO3 and helps to increase its concentration. The production of nitric acid by absorbing nitrogen oxides is an exothermic reaction, and low temperatures are favorable for the absorption of nitrogen oxides, so the roaster gas needs to be cooled to below 35°C. Dilute nitric acid is useful for absorbing nitrogen oxides, and the dilute nitric acid produced by secondary absorption is used as the absorbing liquid in the primary absorption tower, and nitric acid is produced at the bottom of the primary absorption tower and discharged into the nitric acid tank.
[0031] Preferably, the preconcentrator is a Venturi preconcentrator. The preconcentrator reduces the temperature of the roaster gas from 300-500°C to 95°C or less, and concentrates the nitrate solution to 15-35%. In step S1, the reaction temperature in the roaster is 400-850°C (if the temperature is lower than 400°C, the reaction efficiency is significantly reduced, and if the temperature is higher than 850°C, the particle morphology of the generated metal oxide is affected). In step S4, the temperature of the roaster gas is reduced to 40°C or less as soon as the absorption is completed.
[0032] As shown in FIG. 2 and FIG. 3, the roaster includes a roaster body 1, a rotary valve 8, a furnace body exhaust pipe 11, a combustion assembly duct 2, a gas regulating valve 15, an air regulating valve 16, an exhaust temperature detector 10, an exhaust temperature detector 12, an exhaust pressure detector 13, a furnace body temperature detector 14, a duct front stage temperature detector 17, a duct rear stage temperature detector 18, a spray nozzle 3, a solution regulating valve 4, a water supply regulating valve 5 and a compressed air regulating valve 6. The lower end outlet of the roaster body 1 is connected to the rotary valve 8, an exhaust port is provided at the upper end of the roaster body 1, the exhaust port of the roaster body 1 is connected to one end of the furnace body exhaust pipe 11, the discharge end of the spray nozzle 3 is located at the upper stage in the roaster body 1, the combustion end of the combustion assembly duct 2 is located inside the roaster body 1, the gas regulating valve 15 and the air regulating valve 16 are provided at the supply end of the combustion assembly duct 2, and the gas regulating valve 15 and the air regulating valve 16 are provided at the supply end of the combustion assembly duct 2. The air regulating valve 16 is located outside the roasting furnace body 1, the discharge temperature detector 10 is provided at the supply end of the rotary valve 8, the exhaust temperature detector 12 and the exhaust pressure detector 13 are provided on the outer walls of the supply end and the discharge end of the furnace body exhaust pipe 11, respectively, the furnace body temperature detector 14 is multiple, and the multiple furnace body temperature detectors 14 are provided on the side walls of the roasting furnace body 1, the front-stage temperature detector 17 and the rear-stage temperature detector 18 are provided on the side walls of the discharge end and the supply end of the combustion assembly duct 2, respectively, the supply end of the spray nozzle 3 is simultaneously connected to the discharge ends of the feedwater regulating valve 5, the compressed air regulating valve 6 and the solution regulating valve 4, the supply end of the solution regulating valve 4 is connected to the solution supply assembly, the supply end of the feedwater regulating valve 5 is connected to the feedwater assembly, and the supply end of the compressed air regulating valve 6 is connected to an air supply device.
[0033] As an improvement, a block crusher 7 and a crusher drive motor 9 are provided between the discharge end of the roasting furnace main body 1 and the rotary valve 8, the supply end of the block crusher 7 is connected to the discharge end of the roasting furnace main body 1, the discharge end of the block crusher 7 is connected to the rotary valve 8, and the drive end of the block crusher 7 is connected to the drive output shaft of the crusher drive motor 9.
[0034] Preferably, the spray nozzle 3 is provided in a plurality of locations, and all of the spray nozzles 3 are located at an upper stage within the roasting furnace body 1 .
[0035] As an improvement, an air flow sensor 19 is provided between the combustion assembly duct 2 and the air regulating valve 16, a gas flow sensor 20 is provided between the combustion assembly duct 2 and the gas regulating valve 15, and a flame detector 21 is provided in the combustion assembly duct 2, and a detection end of the flame detector 21 is located inside the combustion assembly duct 2.
[0036] At the outlet of the combustion assembly conduit 2, a conduit front stage temperature detector 17 is provided to detect the temperature when the high-temperature gas enters the inside of the roasting furnace after the end of combustion, and the temperature is controlled to 800-1200°C to better complete the pyrolysis reaction in the roasting furnace. When only one thermometer is used for detection, only the combustion reaction temperature of the high-temperature gas is detected, and the gas temperature after the end of combustion is not detected, which is disadvantageous to accurately control the reaction temperature in the roasting furnace. The installation of the conduit front stage temperature detector 17 to detect the temperature when the high-temperature gas enters the inside of the roasting furnace after the end of combustion is helpful in controlling the reaction temperature in the roasting furnace, improving the reaction efficiency, and controlling the metal oxide particles.
[0037] The atomization method of the solution entering the roasting furnace adopts multi-material atomization, which reduces the size of the atomized particles and makes it easier to carry out the spray roasting reaction. A furnace body temperature detector 14 is installed in the straight section of the roasting furnace to detect the temperature of each stage inside the roasting furnace, which is advantageous for controlling the reaction temperature inside the roasting furnace.
[0038] The roasting process in the roasting furnace includes the following steps 1 to 5.
[0039] In step 1, the solution is fed into the spray nozzle 3 through the solution adjusting valve 4, and compressed air is also fed into the spray nozzle 3 through the compressed air adjusting valve 6 to atomize the solution into particles of 10-300 μm. These are then sprayed into the inside of the roasting furnace body 1 for spray roasting.
[0040] In step 2, a pyrolysis reaction is carried out inside the roasting furnace body 1 to produce metal oxides and nitrogen oxides.
[0041] In step 3, the nitrogen oxide gas and combustion exhaust gas produced by the reaction, and excess air are discharged from the top of the roasting furnace body 1, and the temperature and pressure are detected by the exhaust temperature detector 12 and the exhaust pressure detector 13, and the gas in the roasting furnace body 1 is then sent to the subsequent cooling and absorption step.
[0042] In step 4, the metal oxide produced by the reaction is fed from the bottom of the roasting furnace body 1 through a block crusher 7 and a rotary valve 8 into a powder conveying system.
[0043] In step 5, the gas and air that have entered the combustion assembly through the gas regulating valve 15 and the air regulating valve 16 are combusted in the combustion assembly flame duct 2, and the high-temperature gas after combustion is introduced into the roasting furnace body 1 so as to supply heat to the reaction inside the roasting furnace body 1. EXAMPLES
[0044] In S1, the nitrate solution is filtered to remove impurities, then concentrated in a preconcentrator and fed to a roasting furnace. The nitrate solution is then sprayed under pressure into the roasting furnace by a roasting furnace feed pump to carry out spray roasting decomposition.
[0045] In S2, the furnace gas from the roaster is transported to the pre-concentrator, and the roaster gas generated after spraying and roasting nitrates in the roaster is cooled by the pre-concentrator to lower the temperature of the roaster gas from 300°C to below 85°C, while concentrating the nitrate solution to 15% and removing dust from the roaster gas.
[0046] In S3, the metal oxide is dropped from the bottom of the roasting furnace, and the conveying air generated by the conveying fan and filtered by the filter conveys the metal oxide powder to the powder silo, the metal oxide is cooled as it passes through the conveying air, and is cleaned and purified by the sintered plate dust collector installed at the top of the powder silo, and the purified air is discharged, and the powder at the bottom collected by the sintered plate dust collector is dropped back into the powder silo, and a packaging machine for packaging the metal oxide is installed at the bottom of the powder silo.
[0047] In S4, the roaster gas that has passed through the pre-concentrator is fed into a primary cooling tower, a primary absorption tower, a secondary cooling tower, a secondary absorption tower, or a multi-stage cooling tower and an absorption tower that are staggered from each other, where the NO2 gas is absorbed to produce regenerated nitric acid. When the absorption is complete, the temperature of the roaster gas is lowered and then the gas is fed into the exhaust gas fan.
[0048] In S5, a liquid alkali (or ammonia water) scrubber installed behind the exhaust gas fan scrubs the roaster gas again, and the scrubbed wastewater is discharged to a sewage treatment plant for treatment to meet the emission standards.
[0049] In S6, the gas that has passed through the scrubbing tower is cleaned with a wet electrostatic precipitator and then discharged to the outside through a chimney, and the washing wastewater from the wet electrostatic precipitator is also discharged to a sewage treatment plant for treatment. The temperature of the flue gas is less than 40°C, the water vapor content is less than 10%, and other indicators are lower than China's emission standards.
[0050] The metal oxides roasted in Example 1 above were tested and their technical parameters are shown in Table 1 below.
[0051] Particle size characteristic parameter table 1 (unit: μm) JPEG2024144350000002.jpg18170
[0052] Here, D represents the diameter, and 03, 06 ... 97, 98 represent percentages. For example, D03 = 0.88 μm means that when the cumulative distribution ratio from small particle diameters to large particle diameters reaches 3% in the particle size distribution of particles, the corresponding particle diameter value is 0.88 μm. In this embodiment, the median diameter (D50) is 20 μm, the volume-based average diameter D[4,3] is 24.39 μm, and the area-based average diameter D[3,2] is 5.76 μm. EXAMPLES
[0053] The difference from Example 1 is that the preconcentrator reduces the temperature of the roaster gas from 500°C to 90°C and concentrates the nitrate solution to 35%.
[0054] The roasted metal oxides in Example 2 above were tested and their technical parameters are shown in Table 2 below.
[0055] Particle size characteristic parameter table 2 (unit: μm) JPEG2024144350000003.jpg18170
[0056] Here, D represents the diameter, and 03, 06 ... 97, 98 represent percentages. For example, D03 = 0.6 μm means that when the cumulative distribution ratio from small particle diameters to large particle diameters reaches 3% in the particle size distribution of the particles, the corresponding particle diameter value is 0.6 μm. In this embodiment, the median diameter (D50) is 10.0 μm, the volume-based average diameter D[4,3] is 12.09 μm, and the area-based average diameter D[3,2] is 2.85 μm. EXAMPLES
[0057] The difference from Example 1 is that the preconcentrator reduces the temperature of the roaster gas from 380°C to 80°C and concentrates the nitrate solution to 25%.
[0058] The roasted metal oxides in Example 3 above were tested and their technical parameters are shown in Table 3 below.
[0059] Particle size characteristic parameter table 3 (unit: μm) JPEG2024144350000004.jpg17170
[0060] Here, D represents the diameter, and 03, 06 ... 97, 98 represent percentages. For example, D03 = 0.79 μm means that when the cumulative distribution ratio from small particle diameters to large particle diameters reaches 3% in the particle size distribution of particles, the corresponding particle diameter value is 0.79 μm. In this embodiment, the median diameter (D50) is 4.9 μm, the volume-based average diameter D[4,3] is 3.98 μm, and the area-based average diameter D[3,2] is 0.83 μm.
[0061] As can be seen from the results of Examples 1 to 3 above, the technical effects obtained by the process parameters of Example 3 are superior to those of Examples 1 and 2.
[0062] The technical solution of the present invention is not limited to the above specific embodiments, and all technical modifications made according to the technical solution of the present invention shall fall within the protection scope of the present invention. [Explanation of symbols]
[0063] In the diagram, there is a roasting furnace main body 1, a combustion assembly conduit 2, a spray nozzle 3, a solution regulating valve 4, a water supply regulating valve 5, a compressed air regulating valve 6, a block crusher 7, a rotary valve 8, a drive motor for the crusher 9, an exhaust temperature detector 10, a furnace main body exhaust pipe 11, an exhaust temperature detector 12, an exhaust pressure detector 13, a furnace main body temperature detector 14, a gas regulating valve 15, an air regulating valve 16, a pre-conduit temperature detector 17, a post-conduit temperature detector 18, an air flow sensor 19, a gas flow sensor 20, and a flame detector 21.
Claims
1. In step S1, the nitrate solution is filtered to remove impurities, concentrated in a preconcentrator, and fed to a roasting furnace. The nitrate solution is sprayed under pressure into the roasting furnace by a roasting furnace feed pump to perform spray roasting decomposition. The nitrate decomposition products include metal oxides, NOx, and the like. 2 Step S1 includes gas and water vapor; Step S2: conveying the furnace gas from the roasting furnace to a preconcentrator, cooling the roasting furnace gas generated after spraying and roasting the nitrate in the roasting furnace by the preconcentrator, and simultaneously concentrating the newly introduced nitrate solution and removing dust from the roasting furnace gas; Step S3: dropping the metal oxide from the bottom of the roasting furnace, and conveying air generated by a conveying fan and filtered by a filter conveying the metal oxide powder to a powder silo, and the metal oxide is cooled as it passes through the conveying air; Step S3: providing a sintered plate dust collector at the top of the powder silo and a packaging machine at the bottom of the powder silo for packaging the metal oxide; The roaster gas that has passed through the preconcentrator is introduced into a primary cooling tower, a primary absorption tower, a secondary cooling tower, a secondary absorption tower, or a multi-stage cooling tower and an absorption tower that are staggered from each other, and NOx is removed therein. 2 Step S4: absorbing the gas to generate regenerated nitric acid, and as soon as the absorption is completed, lowering the temperature of the roasting furnace gas and then feeding it into the exhaust gas fan; The liquid alkali washing tower installed behind the exhaust gas fan includes step S5 of washing the roasting furnace gas again, and step S6 of removing dust from the gas that has passed through the washing tower with a wet electrostatic precipitator and discharging it to the outside through a chimney. The roasting furnace includes a roasting furnace body (1), a rotary valve (8), a furnace body exhaust pipe (11), a combustion assembly vent (2), a gas regulating valve (15), an air regulating valve (16), an exhaust temperature detector (10), an exhaust temperature detector (12), an exhaust pressure detector (13), a furnace body temperature detector (14), a vent front stage temperature detector (17), and a vent rear stage temperature detector (18). The roasting furnace body (1) includes a lower end outlet connected to the rotary valve (8), an exhaust port is provided at the upper end of the roasting furnace body (1), the exhaust port of the roasting furnace body (1) is connected to one end of the furnace body exhaust pipe (11), the discharge end of the spray nozzle (3) is located at an upper stage in the roasting furnace body (1), the combustion end of the combustion assembly flame (2) is located inside the roasting furnace body (1), the gas regulating valve (15) and the air regulating valve (16) are connected to the lower end outlet of the roasting furnace body (1), an exhaust port is provided at the upper end of the roasting furnace body (1), the exhaust port of the roasting furnace body (1) is connected to one end of the furnace body exhaust pipe (11), the discharge end of the spray nozzle (3) is located at an upper stage in the roasting furnace body (1), the combustion end of the combustion assembly flame (2) is located inside the roasting furnace body (1), the gas regulating valve (15) and the air regulating valve (16) are connected to the upper end of the roasting furnace body (1), The gas regulating valve (15) and the air regulating valve (16) are located outside the roasting furnace body (1); the exhaust temperature detector (10) is located at the supply end of the rotary valve (8); the exhaust temperature detector (12) and the exhaust pressure detector (13) are respectively provided on the outer walls of the supply end and the discharge end of the furnace body exhaust pipe (11); the furnace body temperature detector (14) is multiple, and the multiple furnace body temperature detectors (14) are respectively provided on the side walls of the roasting furnace body (1); the duct front stage temperature detector (17) and the feed end of the spray nozzle (3) is simultaneously connected to the discharge ends of the feed water regulating valve (5), the compressed air regulating valve (6) and the solution regulating valve (4), the feed end of the solution regulating valve (4) is connected to a solution supply assembly, the feed end of the feed water regulating valve (5) is connected to a feed water assembly, and the feed end of the compressed air regulating valve (6) is connected to an air supply device.
2. 2. The process for producing metal oxides by spray roasting nitrates as claimed in claim 1, wherein the preconcentrator is a Venturi preconcentrator.
3. The process for producing metal oxides by spray roasting nitrates according to claim 1, characterized in that the preconcentrator reduces the temperature of the roaster gas from 300-500°C to below 95°C and concentrates the nitrate solution to 15-35%.
4. The process for producing metal oxide by spray roasting nitrate according to claim 1, wherein in step S1, the reaction temperature in the roasting furnace is 400 to 850°C.
5. 2. The process for producing metal oxides by spray roasting nitrates according to claim 1, wherein in step S4, the temperature of the roaster gas is lowered to below 40° C. as soon as the absorption is completed.
6. 2. The process for producing metal oxides by spray roasting nitrates according to claim 1, characterized in that a block crusher (7) and a crusher drive motor (9) are provided between the discharge end of the roasting furnace body (1) and the rotary valve (8), the supply end of the block crusher (7) is connected to the discharge end of the roasting furnace body (1), the discharge end of the block crusher (7) is connected to the rotary valve (8), and the drive end of the block crusher (7) is connected to the drive output shaft of the crusher drive motor (9).
7. 2. The process for producing metal oxides by spray roasting nitrates according to claim 1, characterized in that the number of spray nozzles (3) is multiple, and all of the multiple spray nozzles (3) are located at an upper stage in the roasting furnace body (1).
8. 2. The process for producing metal oxides by spray roasting nitrates according to claim 1, characterized in that an air flow sensor (19) is provided between the combustion assembly conduit (2) and the air regulating valve (16), a gas flow sensor (20) is provided between the combustion assembly conduit (2) and the gas regulating valve (15), and a flame detector (21) is provided in the combustion assembly conduit (2), and a detection end of the flame detector (21) is located inside the combustion assembly conduit (2).
Citation Information
Patent Citations
Method and device for extracting or recovering acid from acid solution
JP1997188502A
Process for recovering acid from metal-dissolved acid solution
JP2000264609A
Process for the production or recovery of acids from metalliferous solutions of such acids
US5149515A
Method and system for recycling stainless steel mixed acid pickling sludge
WO2023019719A1
System and production process for producing cobaltosic oxide through spray roasting method
CN110526303A