Method and addition liquid for recovering performance of stable liquid

An anionic copolymer-based additive liquid addresses the performance degradation of stabilizing liquids by improving viscosity and reducing filtration in construction methods, effectively preventing excavated wall collapse.

JP2024147441APending Publication Date: 2024-10-16KURITA WATER INDUSTRIES LTD +1
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
JP2023060460
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-03
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Existing stabilizing liquids used in cast-in-place pile and underground continuous wall construction methods deteriorate due to contamination and cement components, leading to reduced performance in preventing excavated wall collapse.

Method used

An additive liquid composed of an anionic copolymer containing monomer units derived from acrylamide and acrylic acid or their salts, with specific molecular weight and anionic degree, is added to restore the performance of deteriorated stabilizing liquids.

Benefits of technology

The additive liquid effectively restores the performance of stabilizing liquids by improving viscosity and reducing filtration water, enhancing the ability to prevent excavated wall collapse.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147441000001_ABST
    Figure 2024147441000001_ABST
Patent Text Reader

Abstract

To provide a method and an addition liquid for recovering performance of a stable liquid used for preventing collapse of an excavated wall surface in a cast-in-place pile construction method or an underground continuous wall construction method.SOLUTION: Provided is an addition liquid composed of an aqueous liquid including an anionic copolymer containing a monomeric unit derived from an acrylamide and a structural unit derived from an acrylic acid or its salt. The addition liquid is applied to recovery of performance of a stable liquid used for preventing collapse of an excavated wall surface in a cast-in-place pile construction method or an underground continuous wall construction method. Provided is also a method for recovering the performance of the stable liquid, including addition of the addition liquid to the stable liquid used to prevent collapse of the excavated wall surface in the cast-in-place pile construction method or the underground continuous wall construction method.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method and an additive liquid for restoring the performance of a stabilizing solution. More specifically, the present invention relates to a method and an additive liquid for restoring the performance of a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method. [Background technology]

[0002] In cast-in-place pile construction and diaphragm wall construction, a stabilizing solution is used to prevent the collapse of the excavated wall surface. Stabilizing solutions containing bentonite and carboxymethylcellulose as the main components (hereinafter sometimes referred to as bentonite CMC stabilizing solution) are widely used. The mixing ratio of the main components bentonite and carboxymethylcellulose, and the amount of secondary components such as dispersants (polycarboxylates) and calcium sealants (sodium carbonate and sodium bicarbonate) are adjusted according to the construction conditions such as the soil composition and hardness of the ground to be excavated, the groundwater level and water quality, and the excavation depth.

[0003] The performance required of the stabilizing solution varies slightly depending on the excavation method, but mainly includes preventing the collapse of the borehole wall, transporting and separating the excavated soil to the ground, and good replacement performance when pouring concrete. In particular, the ability to prevent collapse (wall construction) is important. The stabilizing solution is used repeatedly, but it gradually deteriorates due to the mixing of excavated soil and the influence of cement components when pouring concrete. Stabilizing solution that has deteriorated (for example, decreased viscosity, increased viscosity, increased amount of filtered water, high specific gravity, decreased pH, gelation, decay, etc.) has deteriorated in the above-mentioned performance, so it may be continued to be used in the excavation method while its performance is restored by various methods.

[0004] As a method for regenerating a stabilizing liquid with deteriorated performance, for example, Patent Document 1 discloses a method for improving the wall-forming properties of drilling mud (stabilizing liquid), which is characterized by adding to the deteriorated mud a mud film forming agent for drilling mud, which comprises a (co)polymer (x') having an unsaturated carboxylic acid and / or its salt (a) as its main constituent unit, and which has a weight average molecular weight Mw of 200,000 to 3,000,000.

[0005] Patent Document 2 discloses a method for dispersing reusable stabilizing liquid in a stabilizing liquid excavation method, characterized in that 0.05 to 1.0% of a mixture of 25 to 75 parts by weight of sodium carboxymethylcellulose having an average degree of polymerization of 500 or less and an average degree of substitution of 0.6 to 0.9M / C6 produced from regenerated cellulose, 25 to 50 parts by weight of sodium polyacrylate having an average degree of polymerization of 20 to 100, and 5 to 25 parts by weight of sodium carbonate (total 100 parts by weight) is added to deteriorated stabilizing liquid.

[0006] Patent Document 3 discloses that a dispersant for drilling mud, which is composed of a polyacrylate, a polymethacrylate or a copolymer thereof and has a weight average molecular weight Mw of 10,000 to 14,000, can be used to regenerate deteriorated drilling mud (stabilizing liquid). [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2005-036239 A [Patent Document 2] Japanese Patent Application Publication No. 5-9468 [Patent Document 3] JP 2000-87023 A Summary of the Invention [Problem to be solved by the invention]

[0008] An object of the present invention is to provide a method and an additive for restoring the performance of a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method. [Means for solving the problem]

[0009] As a result of investigations conducted in order to achieve the above object, the present invention, which includes the following aspects, has been completed. [1] An aqueous liquid containing an anionic copolymer containing a monomer unit derived from acrylamide and a structural unit derived from acrylic acid or a salt thereof, An additive liquid for restoring the performance of the stabilizing liquid used to prevent the collapse of excavated walls in cast-in-place pile construction or underground diaphragm wall construction.

[0010] [2] The additive solution according to [1], wherein the anionic copolymer further contains at least one selected from the group consisting of a structural unit derived from an N-substituted (meth)acrylamide or a salt thereof, a structural unit derived from methacrylamide, and a structural unit derived from methacrylic acid or a salt thereof.

[0011] [3] The additive liquid according to [1] or [2], wherein the anionic copolymer has an anionic degree of 4 to 55 mol %.

[0012] [4] The additive liquid according to any one of [1] to [3], wherein the anionic copolymer has a weight average molecular weight of 500,000 to 2,500,000.

[0013] [5] The additive liquid according to any one of [1] to [4], further comprising at least one selected from the group consisting of a dispersant and a calcium sequestering agent.

[0014] [6] A method for restoring the performance of a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method, comprising adding the additive solution according to any one of [1] to [5] to the stabilizing solution.

[0015] [7] A method for restoring the performance of a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method, comprising adding to the stabilizing solution described in any one of [1] to [5] above and at least one selected from the group consisting of a dispersant and a calcium sequestering agent.

[0016] [8] The method according to [6] or [7], wherein the amount of the additive liquid is such that the amount of the anionic copolymer is 0.05 parts by mass or more per 100 parts by mass of the stabilizing liquid. Effect of the Invention

[0017] Since the additive liquid of the present invention is an aqueous liquid containing a polymer, by simply adding it to a stabilizing liquid whose performance has deteriorated as described above at an excavation site, the performance of the stabilizing liquid can be easily and quickly restored. The method of the present invention, which includes adding the additive solution of the present invention to a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method, can restore the performance of the stabilizing solution. The stabilizing solution whose performance has been restored by the method of the present invention or the like may hereinafter be referred to as a regenerated stabilizing solution. [Brief description of the drawings]

[0018] [Figure 1] FIG. 2 is a disassembled view showing an example of a pressure filtration cell used for evaluating wall-forming properties. [Diagram 2] FIG. 2 is a diagram showing an example of a pressure filtration tester used for evaluating wall-forming properties. [Diagram 3] FIG. 1 is a diagram showing the results of Examples 1-1 to 1-6. [Figure 4] FIG. 1 is a diagram showing the results of Examples 2-1 to 2-5. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] The additive liquid of the present invention is intended to restore the performance of a stabilizing liquid used to prevent the collapse of an excavated wall surface in a cast-in-place pile method or a diaphragm wall method. The cast-in-place pile method or the diaphragm wall method is one of the well-known foundation construction methods in the field of construction and civil engineering.

[0020] The additive liquid of the present invention is an aqueous liquid containing an anionic copolymer. The aqueous liquid is an aqueous solution, an aqueous dispersion, or an aqueous suspension, and is preferably an aqueous solution.

[0021] The anionic copolymer used in the present invention contains a structural unit derived from acrylamide (see formula (1a)) and a structural unit derived from acrylic acid (see formula (2a)) or a salt thereof, and if necessary, further contains at least one selected from the group consisting of a structural unit derived from N-substituted (meth)acrylamide or a salt thereof, a structural unit derived from methacrylamide (see formula (1b)), and a structural unit derived from methacrylic acid (see formula (2b)) or a salt thereof. The anionic copolymer is preferably water-soluble.

[0022] TIFF2024147441000002.tif26150

[0023] TIFF2024147441000003.tif32150

[0024] TIFF2024147441000004.tif26150

[0025] TIFF2024147441000005.tif32150

[0026] Examples of the salt of acrylic acid include metal salts such as lithium salt, sodium salt, potassium salt, calcium salt, barium salt, iron salt, cobalt salt, nickel salt, copper salt, zinc salt, and aluminum salt, and organic ammonium salts such as ammonium salt, trialkylamine salt, monoethanolamine salt, diethanolamine salt, triethanolamine salt, and pyridine salt. Of these, sodium salt is preferred.

[0027] Examples of the salt of methacrylic acid include metal salts such as lithium salt, sodium salt, potassium salt, calcium salt, barium salt, iron salt, cobalt salt, nickel salt, copper salt, zinc salt, and aluminum salt, and organic ammonium salts such as ammonium salt, trialkylamine salt, monoethanolamine salt, diethanolamine salt, triethanolamine salt, and pyridine salt. Of these, sodium salt is preferred.

[0028] N-substituted (meth)acrylamides are those in which one or two hydrogen atoms of the amino group (-NH2) in acrylamide or methacrylamide are replaced by unsubstituted or substituted hydrocarbon groups, or the amino group (-NH2) is quaternized (-N + R4) where R may be the same unsubstituted or substituted hydrocarbon group or different unsubstituted or substituted hydrocarbon groups.

[0029] Examples of unsubstituted hydrocarbon groups include alkyl groups such as methyl, ethyl, propyl, isopropyl, butyl, isobutyl, secondary butyl, tertiary butyl, pentyl, and hexyl; cycloalkyl groups such as cyclopropyl, cyclopentyl, cyclohexyl, and cyclooctyl; alkenyl groups such as vinyl, allyl, 1-propenyl, isopropenyl, 2-butenyl, 1,3-butadienyl, 2-pentenyl, and 2-hexenyl; cycloalkenyl groups such as cyclopropenyl, cyclopentenyl, and cyclohexenyl; alkynyl groups such as ethynyl, 1-propynyl, and 2-propynyl; aryl groups such as phenyl, tolyl, xylyl, naphthyl, methylnaphthyl, anthryl, phenanthryl, and biphenyl; Examples of the aryl group include aralkyl groups such as a benzyl group, a phenethyl group, a naphthylmethyl group, and a naphthylethyl group.

[0030] Examples of the substituent in the substituted hydrocarbon group include a halogeno group, a sulfo group, a sulfino group, a sulfeno group, a hydroxy group, an aldehyde group, a carbonyl group, an oxo group, a carboxy group, an amino group, a nitro group, a cyano group, an aminosulfonyl group, an alkylsulfonyl group, and an arylsulfonyl group.

[0031] Specific examples of N-substituted (meth)acrylamides include N-alkyl (meth)acrylamides such as N-methyl (meth)acrylamide, N-ethyl (meth)acrylamide, and N-isopropylacrylamide; N,N-dialkyl (meth)acrylamides such as N,N-dimethyl (meth)acrylamide and N,N-diethyl (meth)acrylamide; N-hydroxyalkyl (meth)acrylamides such as N-hydroxymethyl (meth)acrylamide and N-hydroxyethyl (meth)acrylamide; N,N-dihydroxyalkyl (meth)acrylamides such as N,N-dihydroxymethyl (meth)acrylamide and N,N-dihydroxyethyl (meth)acrylamide; N-carboxyalkyl (meth)acrylamides such as N-carboxymethyl (meth)acrylamide and N-carboxyethyl (meth)acrylamide; and N,N-dicarboxyalkyl (meth)acrylamides. Examples include N-sulfoalkyl (meth)acrylamides such as N-(1-sulfo-2-methylpropan-2-yl)-(meth)acrylamide (also known as 2-(meth)acryloylamino-2-methylpropane-1-sulfonic acid); N,N-disulfoalkyl (meth)acrylamide; N-(3-dimethylaminopropyl)(meth)acrylamide; acryloylaminopropyltrimethylammonium chloride, and methacryloylaminopropyltrimethylammonium chloride. Among these, N-substituted acrylamide is preferred, N-sulfoalkylacrylamide (see formula (3)) or a salt thereof is more preferred, and N-(1-sulfo-2-methylpropan-2-yl)-(meth)acrylamide or a salt thereof is even more preferred. Examples of salts of N-sulfoalkylacrylamide include metal salts such as lithium salt, sodium salt, potassium salt, calcium salt, barium salt, iron salt, cobalt salt, nickel salt, copper salt, zinc salt, and aluminum salt; ammonium salt; organic ammonium salts such as trialkylamine salt, monoethanolamine salt, diethanolamine salt, triethanolamine salt, and pyridine salt; and phosphonium salt. Among these, sodium salt is preferred.

[0032] TIFF2024147441000006.tif38150A in formula (3) is an alkanediyl group (an atomic group formed by removing two hydrogen atoms from an alkane).

[0033] The anionic copolymer used in the present invention may further have structural units derived from other monomers. Examples of other monomers include polyfunctional unsaturated carboxylic acids (anhydrides) or salts thereof, such as maleic anhydride, maleic acid, fumaric acid, and itaconic acid; (meth)acrylic acid alkyl esters, such as methyl (meth)acrylate, ethyl (meth)acrylate, butyl (meth)acrylate, and 2-ethylhexyl (meth)acrylate; esters of polyhydric alcohols and (meth)acrylic acid, such as ethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, propyne glycol di(meth)acrylate, and butanediol di(meth)acrylate; carboxylic acid vinyl esters, such as allyl (meth)acrylate, vinyl acetate, and propyl acetate; glycidyl (meth)acrylate; unsaturated sulfonic acids or salts thereof, such as vinyl sulfonic acid, allyl sulfonic acid, methallyl sulfonic acid, styrene sulfonic acid, and 2-hydroxy-3-allyloxypropanesulfonic acid; (meth)acrylonitrile; styrene monomers, such as styrene, α-methylstyrene, p-methylstyrene, and chloromethylstyrene; Examples of the monomer include N-vinyl amides or N-allylamides such as N-vinylformamide, N-vinylacetamide, and N-vinylpyrrolidone; vinylpyridine, vinylimidazole, and allylamine; dimethylaminoethyl acrylate, acryloyloxyethyl trimethylammonium chloride, methacryloyloxyethyl trimethylammonium chloride, and acryloyl 2-hydroxypropyl acrylate.

[0034] The structural unit in the anionic copolymer is formed by addition polymerization of the ethylenically unsaturated bond in the monomer. For example, the structural unit derived from acrylamide is represented by formula (Ia), the structural unit derived from acrylic acid is represented by formula (IIa), the structural unit derived from N-sulfoalkylacrylamide is represented by formula (III), and the structural unit derived from itaconic acid is represented by formula (IV).

[0035] TIFF2024147441000007.tif26150

[0036] TIFF2024147441000008.tif26150

[0037] TIFF2024147441000009.tif45150

[0038] TIFF2024147441000010.tif38150Note that n in formulas (Ia), (IIa), (III) and (IV) each independently represents the number of structures in []. * is a bond. A is an alkanediyl group (an atomic group with a structure in which two hydrogen atoms have been removed from an alkane).

[0039] The anionic copolymer used in the present invention has a lower limit of anionic degree (which can be adjusted by the ratio of anionic monomers) of preferably 4 mol%, more preferably 7 mol%, even more preferably 8 mol%, even more preferably 10 mol%, and most preferably 30 mol%, and an upper limit of anionic degree is preferably 65 mol%, more preferably 60 mol%, even more preferably 55 mol%, even more preferably 53 mol%, and most preferably 50 mol%. The anionic degree of the anionic copolymer can be determined by measurement using a titration method (Japan Sewage Works Agency, 2015. Chapter 12 Sludge dewatering equipment [Reference material] 274 Journal of Japan Society on Water Environment Setting the optimal drug dosing rate of polymer flocculant in the centrifugal dewatering process of sewage digestion sludge Sludge analysis method. Standard specifications for machinery and equipment 2015 edition. Sewage Works Support Center, Tokyo, pp. 12-141-12-144.). In addition, the anionic degree of the anionic copolymer can be calculated from the ratio of structural units constituting the anionic copolymer when the ratio is known, and can be calculated from the anionic colloid equivalent value when the species of monomer from which the structural units constituting the anionic copolymer are derived is known.

[0040] The anionic copolymer used in the present invention has a weight average molecular weight of preferably 200,000 or more, more preferably 250,000 or more, even more preferably 280,000 or more, still more preferably 300,000 or more, and most preferably 500,000 or more. The upper limit of the weight average molecular weight is not particularly limited as long as an aqueous liquid can be prepared, and is preferably 4 million, more preferably 3.5 million, even more preferably 3 million, and still more preferably 2.5 million. The weight average molecular weight is measured by gel permeation chromatography (GPC) using a standard polymer (pullulan = [(CH 10 O5) n ] m ) can be determined by comparison with the molecular weight of

[0041] The anionic copolymer used in the present invention is not limited by its production method, and can be obtained by, for example, solution polymerization, aqueous solution polymerization, gel polymerization, suspension polymerization, reverse phase suspension polymerization, or the like.

[0042] The amount of the anionic copolymer contained in the aqueous liquid is not particularly limited as long as it is possible to recover a predetermined amount of filtrate, and is, for example, preferably 0.5 to 50 mass%, more preferably 1 to 40 mass%, even more preferably 2 to 35 mass%, and even more preferably 5 to 30 mass%.

[0043] The additive liquid of the present invention may contain, in addition to the anionic copolymer, auxiliary additives such as a dispersant, a surfactant, a thickener, a foam stabilizer, a calcium sequestering agent, a pH adjuster, etc. The auxiliary additives are preferably added to the additive liquid of the present invention in the form of an aqueous liquid. Examples of polymer dispersants (preferably having a weight average molecular weight of 1,000 to 100,000) include polyalkylene polyamines, polyethylene glycols, sorbitan alkyl esters, sodium polyacrylate, and sodium polystyrene sulfonate. Examples of low molecular weight dispersants include sodium alkylsulfonate, sodium alkylcarboxylate, alkylammonium salts, alkylamine salts, alkyl ethylene oxide adducts, and monoglycerides. Examples of calcium sequestrants include sodium carbonate, sodium bicarbonate, sodium tripolyphosphate, pentasodium triphosphate, sodium tetrapolyphosphate, sodium pyrophosphate, sodium hexametaphosphate, citric acid, glycolic acid, gluconic acid, trinitric acid, ethylenediaminetetraacetate (EDTA), and hydroxyethylenediaminetetraacetic acid. Examples of pH adjusters include hydroxides and carbonates of alkali metals such as sodium and potassium, hydroxides of alkaline earth metals such as calcium and magnesium, alkylamines such as methylamine, monoethanolamine, dimethylamine, isopropylamine, dipropylamine, trimethylamine, monoethylamine, triethylamine, methylethylamine, monoisopropylamine, phentolamine, methylpropylamine, and diisopropylamine, alkanolamines such as monoethanolamine and isopropanolamine, ammonia, and pyridine.

[0044] The stabilizing solution to which the additive solution of the present invention is applied is that which has been used to prevent the collapse of an excavated wall surface in a cast-in-place pile method or a diaphragm wall method (hereinafter, sometimes referred to as used stabilizing solution). Compared to an unused stabilizing solution, the used stabilizing solution may have changed in quality, for example, in viscosity reduction or increase, in the amount of filtered water increased, in the specific gravity increased, in the pH reduction, in the gelation, or in the decay or change in quality.

[0045] The used stabilizing liquid contains clayey soil or excavated soil and water, and, if necessary, dispersants, thickeners, air bubble stabilizers, calcium sequestering agents, pH adjusters, etc. The used stabilizing liquid may contain sodium carboxymethylcellulose, which has been used conventionally, or the anionic copolymer used in the present invention. The used stabilizing liquid may further contain cement, excavated sand, soil with a large amount of coarse particles, gravelly soil, etc. Note that the coarse particles are soil particles with a particle size of more than 75 μm and 75 mm or less. Gravelly soil is soil containing a large amount of gravel. Gravel is generally soil particles with a particle size of 2 mm or more.

[0046] The amount of clay or excavated soil contained in the used stabilizing solution may be relatively lower or higher than the amount of clay or excavated soil contained in the unused stabilizing solution. In that case, the used stabilizing solution can be replenished with clay or excavated soil, or water. The amount of clay or excavated soil that can be contained in the regenerated stabilizing solution is not particularly limited as long as it can prevent the collapse of the excavated wall surface. For example, the lower limit is preferably 10 g, more preferably 15 g, and the upper limit is preferably 270 g, more preferably 150 g, per 1 kg of water contained in the regenerated stabilizing solution. In addition, the amount of clay or excavated soil contained in the regenerated stabilizing solution of the present invention can be, for example, an amount that provides a specific gravity of 1.02 to 1.20 during excavation in the underground diaphragm wall construction method, and an amount that provides a specific gravity of 1.01 to 1.10 during slime treatment. It should be understood by those skilled in the art that the amount of water to be replenished should take into account the water contained in the additive solution and the auxiliary additive aqueous solution of the present invention.

[0047] Examples of clayey soil include bentonite, montmorillonite, smectite, sepiolite, attapulgite, sericite, illite, talc, chlorite, zeolite, glauconite, kaolinite, and hydrated magnesium silicate, with bentonite being preferred in terms of effectiveness. Barite, chalk, iron oxide, and the like can also be used to increase the density of the used stabilizing solution.

[0048] Excavated soil is soil generated at an excavation site, and in the stabilizing liquid, it is preferable that the soil has a high fine particle content, for example, 50% or more fine particle content. Note that fine particles are soil particles with a particle size of less than 75 μm.

[0049] The amount of the additive solution of the present invention that can be added to the used stabilizing solution is not particularly limited, as long as it can restore the performance of the stabilizing solution used to prevent the collapse of the excavated wall surface in the cast-in-place pile construction method or the diaphragm wall construction method. The amount of the additive solution of the present invention that can be added to the used stabilizing solution is, for example, an amount in which the above-mentioned anionic copolymer is preferably 0.01 to 30 g, more preferably 0.05 to 25 g, per 1 kg of water contained in the regenerated stabilizing solution. Alternatively, the amount of the additive solution of the present invention that can be added is, for example, an amount of the anionic copolymer that is preferably 0.01 parts by mass or more, more preferably 0.05 parts by mass or more, and even more preferably 0.1 parts by mass or more, per 100 parts by mass of the used stabilizing solution.

[0050] A secondary additive may be added to the used stabilizing solution together with the additive solution of the present invention. The secondary additive is preferably added to the used stabilizing solution in the form of an aqueous solution. The amount of the secondary additive that can be added to the used stabilizing solution is not particularly limited as long as it can prevent the collapse of the excavation wall surface. For example, for 1 kg of water contained in the regenerated stabilizing solution, the lower limit of the amount of the dispersant to be added is preferably 10 g, more preferably 20 g, and the upper limit of the amount of the calcium sequestering agent to be added is preferably 10 g, more preferably 20 g, and the upper limit of the amount of the calcium sequestering agent to be added is preferably 50 g, more preferably 40 g. Alternatively, the amount of the dispersant or calcium sequestering agent to be added is, for example, preferably 0.01 parts by mass or more, more preferably 0.05 parts by mass or more, and even more preferably 0.1 parts by mass or more, respectively, for 100 parts by mass of the used stabilizing solution.

[0051] Next, the effect of restoring the performance of a used stabilizing solution by the additive solution of the present invention will be described with reference to the following examples.

[0052] (Method of evaluating wall construction) In accordance with the API standard, the drain tube 7, packing 13, screen wire mesh 12, filter paper 11, packing 10, and cylinder cell 8 were assembled in this order, and about 300 ml of muddy water was poured into the cylinder cell 8, which was then sealed with the packing 9 and top cover 6. This was then attached to the frame 3 and fixed with the pressure screw 2 to produce the pressurized filtration tester 1 (filtration area: 45 cm 2) was assembled (see Figures 1 and 2). A compressor was used to create a pressure of 3 kgf / cm 2 The filtrate flowing out of the drain tube 7 was received in the measuring cylinder 4, and the amount (ml) was measured.

[0053] (anionic copolymer) The following aqueous liquids containing anionic copolymers were prepared. Aqueous liquid I: Aqueous solution containing 15% by mass of a copolymer of acrylamide and sodium acrylate with a weight average molecular weight of 300,000 and an anionic degree of 10 mol%. Aqueous liquid II: An aqueous solution containing 3% by mass of a copolymer of acrylamide and sodium acrylate with a weight average molecular weight of 1.4 million and an anionic degree of 30 mol%. Aqueous liquid III: An aqueous solution containing 9% by mass of a copolymer of acrylamide and sodium acrylate having a weight average molecular weight of 500,000 and an anionic degree of 30 mol%. Aqueous liquid IV: An aqueous solution containing 15% by mass of a copolymer of acrylamide and sodium acrylate having a weight average molecular weight of 300,000 and an anionic degree of 30 mol%. Aqueous liquid V: An aqueous solution containing 15% by mass of a copolymer of acrylamide and sodium acrylate having a weight average molecular weight of 300,000 and an anionic degree of 50 mol%. Aqueous liquid VI: An aqueous solution containing 15% by mass of a copolymer of acrylamide and sodium itaconate having a weight average molecular weight of 400,000 and an anionic degree of 10 mol%. Aqueous liquid VII: An aqueous solution containing 15% by mass of a copolymer of acrylamide and sodium itaconate having a weight average molecular weight of 400,000 and an anionic degree of 50 mol%.

[0054] (Preparation of deterioration stabilizing solution) A stabilizing solution was obtained by mixing 2.0 parts by mass of bentonite, 0.2 parts by mass of carboxymethylcellulose sodium salt (CMCNa salt), and 97.8 parts by mass of tap water. This stabilizing solution was mixed with 6.3 parts by mass of clay (Toti clay) and 0.7 parts by mass of ordinary Portland cement, and left for 2 weeks to obtain deteriorated stabilizing solution (used stabilizing solution) A.

[0055] Example 1-1 0.67 parts by mass of aqueous solution I was added to 100 parts by mass of deteriorated stabilizing solution A to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 1.

[0056] Example 1-2 100 parts by mass of the deteriorated stabilizing solution A was mixed with 3.33 parts by mass of the aqueous solution II to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 1.

[0057] Example 1-3 1.11 parts by mass of the aqueous solution III was added to 100 parts by mass of the deteriorated stabilizing solution A to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 1.

[0058] Example 1-4 0.67 parts by mass of the aqueous solution IV was added to 100 parts by mass of the deteriorated stabilizing solution A to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 1.

[0059] Example 1-5 0.67 parts by mass of aqueous solution V was added to 100 parts by mass of deteriorated stabilizing solution A to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 1.

[0060] Example 1-6 The wall-forming ability of deteriorated stabilizer A was evaluated. The results are shown in Table 1.

[0061] [Table 1]

[0062] On a different day, a deteriorated stabilizing solution B was obtained in the same manner as in the preparation of the deteriorated stabilizing solution. The wall-forming ability of the deteriorated stabilizing solution B was lower than that of the deteriorated stabilizing solution A.

[0063] Example 2-1 0.67 parts by mass of aqueous solution I was added to 100 parts by mass of deteriorated stabilizing solution B to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 2.

[0064] Example 2-2 0.67 parts by mass of the aqueous solution IV was added to 100 parts by mass of the deteriorated stabilizing solution B to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 2.

[0065] Example 2-3 0.67 parts by mass of aqueous solution V was added to 100 parts by mass of deteriorated stabilizing solution B to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 2.

[0066] Example 2-4 0.67 parts by mass of aqueous solution VI was added to 100 parts by mass of deteriorated stabilizing solution B to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 2.

[0067] Example 2-5 0.67 parts by mass of aqueous solution VII was added to 100 parts by mass of deteriorated stabilizing solution B to obtain a regenerated stabilizing solution. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 2.

[0068] [Table 2]

[0069] On another day, using the same method as in the preparation of the deteriorated stabilizing solution, deteriorated stabilizing solution C was obtained. The wall-forming ability of deteriorated stabilizing solution C was lower than that of deteriorated stabilizing solution B.

[0070] Example 3-1 To 100 parts by mass of the deteriorated stabilizer C, 0.2 parts by mass of sodium polyacrylate (dispersant) and 0.4 parts by mass or 0.73 parts by mass of the aqueous liquid I were added to obtain regenerated stabilizers. The wall-forming properties of each regenerated stabilizer were evaluated. The results are shown in Table 3.

[0071] Example 3-2 0.2 parts by mass of sodium polyacrylate (dispersant) and 0.4 parts by mass or 0.73 parts by mass of aqueous liquid IV were added to 100 parts by mass of deteriorated stabilizer C to obtain regenerated stabilizers. The wall-forming ability of each regenerated stabilizer was evaluated. The results are shown in Table 3.

[0072] Example 3-3 To 100 parts by mass of the deteriorated stabilizer C, 0.2 parts by mass of sodium polyacrylate (dispersant) and 0.4 parts by mass or 0.73 parts by mass of the aqueous liquid V were added to obtain regenerated stabilizers. The wall-forming properties of each regenerated stabilizer were evaluated. The results are shown in Table 3.

[0073] [Table 3]

[0074] Example 4-1 To 100 parts by mass of the deteriorated stabilizer C, 0.2 parts by mass of sodium polyacrylate (dispersant), 0.2 parts by mass of sodium carbonate (calcium sequestering agent), and 0.4 parts by mass of aqueous liquid I were added to obtain a regenerated stabilizer. The wall-forming ability of the regenerated stabilizer was evaluated. The results are shown in Table 4.

[0075] Example 4-2 0.2 parts by mass of sodium polyacrylate (dispersant), 0.2 parts by mass of sodium carbonate (calcium sequestering agent), and 0.4 parts by mass of aqueous liquid IV were added to 100 parts by mass of deteriorated stabilizer C to obtain a regenerated stabilizer. The wall-forming ability of the regenerated stabilizer was evaluated. The results are shown in Table 4.

[0076] Example 4-3 A regenerated stabilizing solution was obtained by adding 0.2 parts by mass of sodium polyacrylate (dispersant), 0.2 parts by mass of sodium carbonate (calcium sequestering agent), and 0.4 parts by mass of aqueous solution V to 100 parts by mass of deteriorated stabilizing solution C. The wall-forming ability of the regenerated stabilizing solution was evaluated. The results are shown in Table 4.

[0077] [Table 4]

[0078] As shown by the above results, when the additive solution of the present invention is added to the used stabilizing solution, the amount of filtrate is reduced and the wall-forming property is improved. By appropriately changing the ratio of the additive solution of the present invention to the secondary additives such as dispersants or calcium sequestering agents depending on the deterioration state of the used stabilizing solution, the used stabilizing solution can be effectively regenerated. [Explanation of symbols]

[0079] 1: Pressure filtration tester 2: Presser screw 3: Frame 4: Measuring cylinder 5: Support 6:Top lid 7: Drain tube 8: Cylinder cell 9:Packing 10:Packing 11: Filter paper 12: Screen wire mesh 13:Packing 14: Payment valve

Claims

1. An aqueous liquid containing an anionic copolymer containing a monomer unit derived from acrylamide and a structural unit derived from acrylic acid or a salt thereof. An additive liquid for restoring the performance of the stabilizing liquid used to prevent the collapse of excavated walls in cast-in-place pile construction or underground diaphragm wall construction.

2. The additive liquid according to claim 1, wherein the anionic copolymer further contains at least one selected from the group consisting of a structural unit derived from an N-substituted (meth)acrylamide or a salt thereof, a structural unit derived from methacrylamide, and a structural unit derived from methacrylic acid or a salt thereof.

3. 2. The additive liquid according to claim 1, wherein the anionic copolymer has an anionic degree of 4 to 55 mol %.

4. The additive liquid according to claim 1, wherein the anionic copolymer has a weight average molecular weight of 500,000 to 2,500,000.

5. 2. The additive solution according to claim 1, further comprising at least one selected from the group consisting of a dispersant and a calcium sequestering agent.

6. A method for restoring the performance of a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method, comprising adding the additive solution described in claim 1 to the stabilizing solution.

7. A method for restoring the performance of a stabilizing solution used to prevent the collapse of an excavated wall surface in a cast-in-place pile construction method or a diaphragm wall construction method, comprising adding the additive solution according to claim 1 and at least one selected from the group consisting of a dispersant and a calcium sequestering agent to the stabilizing solution.

8. The method according to claim 6, wherein the amount of the additive liquid is such that the amount of the anionic copolymer is 0.05 parts by mass or more per 100 parts by mass of the stabilizing liquid.

Citation Information

Patent Citations

  • Modifier for excavated clays

    JP1991076989A

  • Water-based circulated excavation slurry

    JP1994057245A

  • Mud pressure shielding method

    JP1994193382A

  • Fluid for digging

    JP1995126619A

  • Adjusting agent for digging slurry

    JP1997310069A