Semiconductor device

By introducing metal elements and dopants into oxide semiconductor films, the process enhances transistor performance, addressing limitations in oxide semiconductor transistors and achieving high-speed, high-performance semiconductor devices.

JP2024147700AActive Publication Date: 2024-10-16SEMICON ENERGY LAB CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2024113893
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2011-06-10
Filing Date
2024-07-17
Publication Date
2024-10-16
Estimated Expiration
2032-05-29

AI Technical Summary

Technical Problem

Transistors using oxide semiconductors face challenges in achieving high electrical characteristics such as on-current and field-effect mobility, limiting their performance and speed in semiconductor devices.

Method used

A manufacturing process involving the introduction of metal elements and dopants into an oxide semiconductor film through heat treatment and implantation methods, forming low resistance regions across the channel length direction to enhance on-characteristics and enable high-speed operation.

Benefits of technology

The process results in transistors with high on-current and field-effect mobility, enabling high-speed response and high-performance semiconductor devices with improved reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147700000001_ABST
    Figure 2024147700000001_ABST
Patent Text Reader

Abstract

To provide a transistor including an oxide semiconductor with a high ON characteristic, and a high-performance semiconductor device including a transistor capable of high-speed response and high-speed driving.SOLUTION: In a manufacturing process for a transistor including an oxide semiconductor film 403 including a channel formation region 409, low-resistance regions 414a and 414b including a metal element introduced by a thermal process in contact with a film containing the metal element, and a dopant introduced through the film 407 containing the metal element by an injection method are formed in the oxide semiconductor film. The low-resistance regions are formed with the channel formation region held therebetween in a channel length direction.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device.

[0002] In this specification, a semiconductor device is a device that can function by utilizing semiconductor characteristics. Generally speaking, electro-optical devices, semiconductor circuits, and electronic devices are all semiconductor devices. [Background technology]

[0003] A transistor (thin film transistor) is made using a semiconductor thin film formed on a substrate with an insulating surface. The technology of constructing thin-film transistors (also called TFTs) is attracting attention. It is widely used in electronic devices such as ICs and image display devices. Silicon-based semiconductor materials are widely known as semiconductor thin films that can be used in transistors. As another material, oxide semiconductors are attracting attention.

[0004] As for transistors using oxide semiconductors, In transistors using oxide semiconductors, higher electrical characteristics are required. For the purpose of achieving good electrical characteristics, low-resistance source and drain regions are fabricated using an aluminum reaction method. Techniques for forming regions have been reported (for example, see Non-Patent Document 1). [Prior art documents] [Non-patent literature]

[0005] [Non-Patent Document 1] N. Morosawa et al. SID 11 DIGEST pp.479-482 Summary of the Invention [Problem to be solved by the invention]

[0006] The on-state characteristics (e.g., on-state current and field-effect mobility) of a transistor using an oxide semiconductor This improvement will enable high-speed response and high-speed operation in semiconductor devices, resulting in higher performance semiconductors. The device can be realized.

[0007] In view of the above, one embodiment of the present invention provides a transistor including an oxide semiconductor and having excellent on-state characteristics. One of our goals is to provide

[0008] Furthermore, one embodiment of the present invention provides a high-performance semiconductor device having a transistor capable of high-speed response and high-speed operation. An object of the present invention is to provide a semiconductor device. [Means for solving the problem]

[0009] In a manufacturing process of a transistor including an oxide semiconductor film including a channel formation region, The metal element is introduced into the semiconductor film by heat treatment in contact with the film containing the metal element. and a dopant introduced through a film containing the metal element by an implantation method. The low resistance regions are formed on both sides of the channel formation region in the channel length direction. Complete.

[0010] Examples of the film containing a metal element include a metal film, a metal oxide film, and a metal nitride film.

[0011] The metal elements in the film containing metal elements include aluminum (Al), titanium (Ti), molybdenum (Mo), and tin (Ti). Butan (Mo), Tungsten (W), Hafnium (Hf), Tantalum (Ta), Lanthanum La, barium (Ba), magnesium (Mg), zirconium (Zr), and nickel One or more selected from the group consisting of nickel (Ni) and zinc (Ni) can be used. As the film, a metal film containing one or more selected from any of the above metal elements, a metal oxide film, or a metal nitride film (e.g., titanium nitride film, molybdenum nitride film, tungsten nitride film) In addition, dopants such as phosphorus (P) and boron (B) can be added to the film containing metal elements. The composition may also contain a phosphate ester.

[0012] A film containing a metal element is formed in contact with the oxide semiconductor film, and the film containing a metal element and the oxide semiconductor By performing heat treatment in a state in contact with the film, the film containing the metal element is converted into the oxide semiconductor film. The heat treatment is preferably carried out in an oxygen atmosphere. Heat treatment can be performed under reduced pressure or nitrogen atmosphere. The heating temperature is 100°C or higher and 70°C or lower. The temperature may be 0° C. or lower, preferably 200° C. to 400° C. A metal element having conductivity is introduced into the oxide semiconductor film by heat treatment. For example, a film containing an element becomes a film containing a metal element having insulating properties. By heat treatment to introduce metal elements into the film, the metal film becomes a metal oxide film or a metal nitride film. When a metal oxide film or a metal nitride film has insulating properties, it can be used as an insulating film. It is possible.

[0013] The dopant is an impurity that changes the electrical conductivity of the oxide semiconductor film. , Group 15 elements (typically phosphorus (P), arsenic (As), and antimony (Sb)), Uranium (B), Aluminum (Al), Nitrogen (N), Argon (Ar), Helium (He) , Neon (Ne), Indium (In), Fluorine (F), Chlorine (Cl), Titanium (Ti) and zinc (Zn).

[0014] The dopant may be contained in a film containing a metal element.

[0015] The dopant is implanted into a film containing a metal element (metal film, metal oxide film, or metal nitride film). The dopant is introduced into the oxide semiconductor film by passing through the oxide film. Implantation method, ion doping method, plasma immersion ion implantation method, etc. In this case, the dopant may be a single ion or a hydride or fluorine ion. It is preferable to use cations of fluoride and chloride.

[0016] The dopant concentration in the low resistance region is 5×10 18 atoms / cm 3 More than 1×10 22 atoms / cm 3 It is preferable that:

[0017] After the dopant introduction treatment, a heat treatment may be performed. This may also serve as a heat treatment in the process of introducing metal elements from the film.

[0018] In the manufacturing process, a step of introducing a metal element from a film containing a metal element by heat treatment, The order of the steps of introducing the dopant by the injection method is not limited, and either step may be performed first or later. It is also acceptable to carry out the test multiple times.

[0019] For example, a metal film is used as the film containing a metal element, and a heat treatment is performed in an oxygen atmosphere to oxidize the metal film. When introducing a metal element into a semiconductor film, the dopant is introduced before the heat treatment. The dopant passes through the metal film, and if the dopant is introduced after the heat treatment, the dopant It will pass through the oxide film.

[0020] The present invention provides a method for manufacturing a semiconductor device comprising the steps of: forming a channel in a channel length direction; As a result, the transistor has high on-characteristics (e.g., on-current and field-effect mobility), High-speed operation and high-speed response are possible.

[0021] Therefore, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. can be provided.

[0022] One embodiment of the invention disclosed in this specification is a semiconductor device including an oxide semiconductor film having a channel formation region. In the oxide semiconductor film, the resistance is higher between the channel formation region and the adjacent channel formation region. The low resistance region is formed by forming a low resistance region containing a metal element and a dopant, and the low resistance region is an oxide semiconductor a film containing a metal element is formed in contact with the oxide semiconductor film, introducing a metal element from a film containing the metal element into the oxide semiconductor film by performing heat treatment in a state in which the metal element is introduced; and introducing a dopant into the oxide semiconductor film through a film containing a metal element. The present invention relates to a method for manufacturing a semiconductor device.

[0023] One embodiment of the invention disclosed in this specification is a semiconductor device including an oxide semiconductor film having a channel formation region. A gate insulating film and a gate electrode layer are formed on the oxide semiconductor film so as to overlap with a channel formation region. A stack of layers is selectively formed to form an oxide semiconductor film over the oxide semiconductor film, the gate insulating film, and the gate electrode layer. A film containing a metal element is formed in contact with a part of the conductor film, and a gate insulating film and a gate electrode layer are formed on the mask. a dopant is selectively introduced into the oxide semiconductor film through a film containing a metal element; The oxide semiconductor film into which the dopant is introduced and the film containing a metal element are heated to introduce the dopant. A metal element is introduced from a film containing a metal element into the oxide semiconductor film. The channel forming region is sandwiched between two regions, each of which has a lower resistance than the channel forming region and contains metal elements and dopants. The present invention relates to a method for manufacturing a semiconductor device in which a low-resistance region including a first insulating film is formed.

[0024] One embodiment of the invention disclosed in this specification is a semiconductor device including an oxide semiconductor film having a channel formation region. A gate insulating film and a gate electrode layer are formed on the oxide semiconductor film so as to overlap with a channel formation region. A stack of layers is selectively formed to form an oxide semiconductor film over the oxide semiconductor film, the gate insulating film, and the gate electrode layer. A film containing a metal element is formed in contact with a part of the conductive film, and The metal element is introduced from the film containing the metal element to the oxide semiconductor film by heating the film, and the gate insulating film and A film containing a metal element is formed on the oxide semiconductor film into which a metal element has been introduced by using the gate electrode layer as a mask. The dopant is selectively introduced through the oxide semiconductor film, and the channel formation region is sandwiched between the oxide semiconductor film. A low-resistance region containing a metal element and a dopant is formed, the resistance of which is lower than that of a channel formation region. The present invention relates to a method for manufacturing a semiconductor device.

[0025] In the above structure, the oxide semiconductor film before the step of forming the film containing a metal element is Alternatively, a heat treatment (dehydration or dehydrogenation treatment) may be performed to release moisture.

[0026] In addition, oxygen, which is a main component material of an oxide semiconductor, can be removed by the dehydration or dehydrogenation treatment. In the oxide semiconductor film, oxygen is released and the amount of the oxide semiconductor film is reduced. In the area where the oxygen is removed, oxygen vacancies exist, and these oxygen vacancies cause fluctuations in the electrical characteristics of the transistor. Therefore, donor levels are generated.

[0027] Therefore, oxygen is preferably supplied to the oxide semiconductor film that has been subjected to dehydration or dehydrogenation treatment. By supplying oxygen to the oxide semiconductor film, oxygen vacancies in the film can be filled. Cut.

[0028] For example, an oxide insulating film containing a large amount (excessive amount) of oxygen, which serves as an oxygen supply source, can be used as an oxide semiconductor film. By providing the oxide insulating film in contact with the oxide semiconductor film, oxygen can be supplied from the oxide insulating film to the oxide semiconductor film. In the above structure, the oxide semiconductor film and the oxide insulating film that have been subjected to the heating step can be reduced. The heating step is performed in a state where the oxide semiconductor film is partially in contact with the oxide semiconductor film, thereby supplying oxygen to the oxide semiconductor film. This is also possible.

[0029] In addition, oxygen (at least oxygen radiative) may be added to the oxide semiconductor film that has been subjected to the dehydration or dehydrogenation treatment. Oxygen may be supplied to the film by introducing oxygen into the film. The oxygen introduction method includes ion implantation, ion doping, plasma immersion, etc. For example, ion implantation, plasma treatment, etc. can be used.

[0030] Further, the oxide semiconductor film provided in the transistor is preferably a crystalline oxide semiconductor. A film state in which the oxygen content is excessive compared to the stoichiometric composition ratio in the film state. In this case, the oxygen content is preferably set to a value exceeding the stoichiometric composition ratio of the oxide semiconductor. Alternatively, the oxygen content is set to a level that exceeds the amount of oxygen in the case of a single crystal. Oxygen may also exist between the lattices of the compound semiconductor.

[0031] Hydrogen or moisture is removed from the oxide semiconductor, and the semiconductor is highly purified to minimize the amount of impurities contained therein. By supplying oxygen to compensate for oxygen vacancies, an I-type (intrinsic) oxide semiconductor or an I-type By doing so, it is possible to obtain an oxide semiconductor that is as close to an intrinsic oxide semiconductor as possible. To bring the Fermi level (Ef) of a semiconductor to the same level as the intrinsic Fermi level (Ei) Therefore, by using the oxide semiconductor film in a transistor, the Reduces the variation in threshold voltage Vth of transistors and the threshold voltage shift ΔVth It is possible. Effect of the Invention

[0032] Metal elements are introduced from a film containing metal elements formed in contact with an oxide semiconductor, and the metal elements are implanted into the oxide semiconductor. By introducing a dopant, a low-resistance region containing a metal element and a dopant is formed in the oxide semiconductor film. The oxide semiconductor layer includes a low resistance region sandwiching the channel formation region in the channel length direction. By having a dielectric film, the transistor has on-characteristics (e.g., on-current and field-effect transition This allows for high speed operation and high speed response.

[0033] Therefore, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. can be provided. [Brief description of the drawings]

[0034] [Figure 1] 1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Diagram 2] 1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Diagram 3] 1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Figure 4] 1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Diagram 5]1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Figure 6] 1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Figure 7] 1A to 1C illustrate one embodiment of a semiconductor device. [Figure 8] 1A to 1C illustrate one embodiment of a semiconductor device and a manufacturing method thereof; [Figure 9] 1A to 1C illustrate one embodiment of a semiconductor device. [Figure 10] 1A to 1C illustrate one embodiment of a semiconductor device. [Figure 11] 1A to 1C illustrate one embodiment of a semiconductor device. [Figure 12] 1A to 1C illustrate one embodiment of a semiconductor device. [Figure 13] FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0035] Hereinafter, embodiments of the invention disclosed in this specification will be described in detail with reference to the drawings. However, the invention disclosed in this specification is not limited to the following description, and the forms and details thereof may be changed in various ways. It will be easily understood by those skilled in the art that the invention disclosed in this specification can be modified in any manner. The present invention should not be construed as being limited to the description of the following embodiments. The ordinal numbers 2 are used for convenience and do not indicate the order of steps or stacking. In addition, the present specification does not indicate specific names as matters for identifying the invention. do not have.

[0036] (Embodiment 1) In this embodiment mode, one mode of a semiconductor device and a manufacturing method of the semiconductor device will be described with reference to FIGS. In this embodiment, a transistor including an oxide semiconductor film is used as an example of a semiconductor device. Shows.

[0037] The structure of the transistor is not particularly limited, and may be, for example, a top gate structure or a bottom gate structure. The transistor can be of the staggered type, planar type, etc. The structure can be a single gate structure with one gate region or a double gate structure with two gate regions. A triple gate structure may be formed in which three gates are formed. A dual-gate type has two gate electrode layers arranged on the same substrate with a gate insulating film between them. good.

[0038] The transistor 440 shown in FIGS. 1A to 1F is a top-gate transistor. Here is an example.

[0039] As shown in FIG. 1F, the transistor 440 has an insulating surface on which the insulating film 436 is provided. A channel forming region 409, low resistance regions 404a and 404b, and a low resistance The oxide semiconductor film 403 including the resistor regions 406a and 406b, the source electrode layer 405a, the drain The transistor 4 has a gate electrode layer 405b, a gate insulating film 402, and a gate electrode layer 401. A film 407 containing a metal element is formed on the substrate 40 .

[0040] 1A to 1F illustrate an example of a method for manufacturing the transistor 440. FIG.

[0041] First, an insulating film 436 is formed over a substrate 400 having an insulating surface.

[0042] There is no significant limitation on the substrate that can be used for the substrate 400 having an insulating surface. In either case, it is necessary to have heat resistance sufficient to withstand subsequent heat treatment. Glass substrates such as borosilicate glass and aluminoborosilicate glass, ceramic substrates, A quartz substrate, a sapphire substrate, etc. can be used. In addition, a silicon substrate, a silicon carbide substrate, etc. can be used. Any single crystal semiconductor substrate, polycrystalline semiconductor substrate, compound semiconductor substrate such as silicon germanium A semiconductor device having a semiconductor element on a substrate such as a silicon-on-insulator (SOI) substrate can also be used. may be used as the substrate 400.

[0043] A semiconductor device may be manufactured using a flexible substrate as the substrate 400. In order to manufacture such a semiconductor device, a transistor including an oxide semiconductor film 403 is formed on a flexible substrate. Alternatively, a transistor including the oxide semiconductor film 403 may be formed on another substrate. The photoresist 440 may be fabricated and then peeled off and transferred to a flexible substrate. In order to separate and transfer the transistor to a flexible substrate, It is preferable to provide a release layer on the

[0044] The insulating film 436 is formed by depositing silicon oxide by plasma CVD or sputtering. , silicon oxide, aluminum oxide, aluminum oxide nitride, hafnium oxide, oxide Gallium, silicon nitride, silicon oxynitride, aluminum nitride, aluminum oxynitride or a mixture of these materials.

[0045] The insulating film 436 may be a single layer or a stacked layer. It is preferable to use an insulating film. In this embodiment, the insulating film 436 is formed by a sputtering method. A silicon oxide film formed using the method is used.

[0046] Next, the oxide semiconductor film 403 is formed over the insulating film 436 .

[0047] Since the insulating film 436 is in contact with the oxide semiconductor film 403, at least the oxide semiconductor film It is preferable that the amount of oxygen contained is greater than the stoichiometric composition ratio. When a silicon oxide film is used, SiO 2+α (However, α>0). By using such an insulating film 436, oxygen can be supplied to the oxide semiconductor film 403. By supplying oxygen to the oxide semiconductor film 403, the oxide semiconductor film 403 can have good characteristics. This can compensate for the oxygen deficiency in the material.

[0048] For example, the insulating film 436 containing a large amount (excessive amount) of oxygen, which serves as an oxygen supply source, is formed on the oxide semiconductor film 4 By providing the insulating film 436 in contact with the oxide semiconductor film 403, oxygen can be supplied from the insulating film 436 to the oxide semiconductor film 403. At least a part of the oxide semiconductor film 403 and the insulating film 436 are in contact with each other. Oxygen may be supplied to the oxide semiconductor film 403 by performing heat treatment in this state. .

[0049] In the process of forming the oxide semiconductor film 403, hydrogen or water is added to the oxide semiconductor film 403. In order to prevent the inclusion of the oxide semiconductor film 403, a sputtering process was performed as a pretreatment for the formation of the oxide semiconductor film 403. The substrate on which the insulating film 436 is formed is preheated in a preheating chamber of the deposition apparatus, and the substrate and the insulating film are It is preferable to desorb and exhaust impurities such as hydrogen and moisture adsorbed on the film 436. The exhaust means provided in the auxiliary heating chamber is preferably a cryopump.

[0050] The oxide semiconductor used for the oxide semiconductor film 403 is at least indium (In). It is preferable that the material contains In or zinc (Zn). It is particularly preferable that the material contains In and Zn. A stabilizer for reducing the variation in electrical characteristics of a transistor using the oxide. In addition, it is preferable to have gallium (Ga) in addition to the above. It is preferable that the alloy contains tin (Sn) as a stabilizer. It is preferable that the stabilizer contains aluminum (Al). It is preferable to do so.

[0051] Other stabilizers include the lanthanides lanthanum (La) and cerium ( Ce), praseodymium (Pr), neodymium (Nd), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), hol Ho, Erbium, Thulium, Ytterbium, Ru The element may contain one or more of the elements tetraethynyl (Te) and tetraethynyl (Lu).

[0052] For example, oxide semiconductors include indium oxide, tin oxide, zinc oxide, and oxides of binary metals. In-Zn oxide, Sn-Zn oxide, Al-Zn oxide, Zn-Mg oxide, Oxides, Sn-Mg oxides, In-Mg oxides, In-Ga oxides, ternary metal oxides In-Ga-Zn oxide (also written as IGZO), In-Al-Zn oxide Oxides, In-Sn-Zn oxides, Sn-Ga-Zn oxides, Al-Ga-Zn oxides oxides, Sn-Al-Zn oxides, In-Hf-Zn oxides, In-La-Zn oxides In-Ce-Zn oxides, In-Pr-Zn oxides, In-Nd-Zn oxides , In-Sm-Zn oxide, In-Eu-Zn oxide, In-Gd-Zn oxide, In-Tb-Zn oxide, In-Dy-Zn oxide, In-Ho-Zn oxide, I n-Er-Zn oxide, In-Tm-Zn oxide, In-Yb-Zn oxide, In -Lu-Zn ​​oxides, In-Sn-Ga-Zn oxides, which are oxides of quaternary metals, I n-Hf-Ga-Zn oxide, In-Al-Ga-Zn oxide, In-Sn-Al- Zn-based oxide, In-Sn-Hf-Zn-based oxide, In-Hf-Al-Zn-based oxide are used. There can be.

[0053] In this case, for example, In-Ga-Zn oxide is a material containing In, Ga, and Zn as main components. The ratio of In, Ga, and Zn does not matter. Metal elements other than a and Zn may be present.

[0054] In addition, as an oxide semiconductor, InMO3(ZnO) m (m>0 and m is not an integer) In addition, M may be selected from Ga, Fe, Mn, and Co. It indicates one or more metal elements. In2SnO5 (ZnO) n A material expressed as (n>0, and n is an integer) may be used.

[0055] For example, In:Ga:Zn=1:1:1 (=1 / 3:1 / 3:1 / 3) or In:G In-Ga-Zn oxide with an atomic ratio of a:Zn=2:2:1 (=2 / 5:2 / 5:1 / 5) The oxides of In:Sn:Zn=1: 1:1(=1 / 3:1 / 3:1 / 3), In:Sn:Zn=2:1:3(=1 / 3:1 / 6:1 / 2) or In:Sn:Zn=2:1:5(=1 / 4:1 / 8:5 / 8) It is advisable to use an In-Sn-Zn oxide having a molecular ratio or an oxide having a composition close to that.

[0056] However, the present invention is not limited to these, and can be applied to any semiconductor characteristics (mobility, threshold, variation, etc.) required. In order to obtain the required semiconductor characteristics, the appropriate composition should be used. Carrier concentration, impurity concentration, defect density, atomic ratio of metal elements to oxygen, interatomic bond length, density It is preferable to make the above appropriate.

[0057] For example, high mobility can be obtained relatively easily with In-Sn-Zn oxides. Therefore, in the case of In-Ga-Zn oxides, the mobility can be increased by lowering the defect density in the bulk. It can be done.

[0058] For example, the atomic ratio of In, Ga, and Zn is In:Ga:Zn=a:b:c(a+b+ The composition of the oxide with the atomic ratio of In:Ga:Zn=A:B:C (A+B+C = 1), a, b, and c are in the vicinity of the oxide composition (aA) 2 +(bB) 2 + (cC) 2 ≦r 2 It means that the following condition is satisfied. For example, r can be set to 0.05. The same is true for other oxides.

[0059] The oxide semiconductor may be single-crystalline or non-single-crystalline. In the latter case, it may be amorphous or polycrystalline. In addition, the structure may include a portion having crystallinity in the amorphous state, or a non-amorphous structure. That's fine too.

[0060] Since it is relatively easy to obtain a flat surface for an amorphous oxide semiconductor, This can reduce interface scattering when fabricating a transistor, and can be achieved relatively easily and with relatively high quality. Therefore, high mobility can be obtained.

[0061] In addition, in a crystalline oxide semiconductor, defects in the bulk can be further reduced, and the surface By improving the flatness of the oxide semiconductor, it is possible to obtain a mobility equal to or higher than that of an oxide semiconductor in an amorphous state. In order to improve the flatness of the surface, it is preferable to form an oxide semiconductor on a flat surface. Specifically, the average surface roughness (Ra) is 1 nm or less, preferably 0.3 nm or less, and more preferably It is preferable to form the surface on a thickness of 0.1 nm or less.

[0062] In addition, Ra is the arithmetic mean roughness defined in JIS B0601 that can be applied to the surface. This is a three-dimensional extension of the method, which is based on the averaging of the absolute value of the deviation from the reference surface to the specified surface. This can be expressed as a "value" and is defined by the following formula:

[0063]

number

[0064] In the above, S0 is the measurement surface (coordinates (x1, y1) (x1, y2) (x2, y1 )(x2, y2)) and Z0 is the average height of the measurement surface. Ra refers to the strength of the atomic force microscope (AFM). It can be evaluated using OPE.

[0065] Therefore, a planarization process is performed on a region of the insulating film 436 that is in contact with the oxide semiconductor film 403. The planarization treatment may be, but is not limited to, a polishing treatment (e.g., a chemical Chemical Mechanical Polishing (CMP) ) method, dry etching treatment, and plasma treatment can be used.

[0066] The plasma treatment may be, for example, a reverse sputtering treatment in which argon gas is introduced to generate plasma. Reverse sputtering is a process in which RF is applied to the substrate side in an argon atmosphere. This method involves applying voltage using a power supply to generate plasma in the vicinity of the substrate to modify the surface. Instead of the argon atmosphere, nitrogen, helium, oxygen, etc. may be used. When the cleaning is performed, powdery substances (also called particles or dust) adhering to the surface of the insulating film 436 are removed. (c) can be removed.

[0067] As the planarization process, the polishing process, the dry etching process, and the plasma process may be performed multiple times. In addition, when performing the steps in combination, the order of the steps is not particularly limited. It is not limited to this but may be appropriately set in accordance with the unevenness of the surface of the insulating film 436.

[0068] As the oxide semiconductor film 403, an oxide semiconductor film containing crystals and having crystallinity (a crystalline oxide The crystalline state of the crystalline oxide semiconductor film is determined by the crystal axis The directions may be in a random state or may have a certain orientation.

[0069] For example, the crystalline oxide semiconductor film may be an oxide semiconductor film having crystals with a c-axis approximately perpendicular to the surface. A nitride semiconductor film can be used.

[0070] An oxide semiconductor layer including crystals having a c-axis approximately perpendicular to the surface (hereinafter, referred to as a crystalline oxide semiconductor layer) The layer (also called the layer) is neither a single crystal structure nor an amorphous structure, and has a c-axis orientation. The crystals included C-Axis Aligned Crystals (also called CAACs). It has an oxide that contains

[0071] CAAC-OS is a type of nanocrystal that has a c-axis orientation and a triangular shape when viewed from the ab plane, surface, or interface direction. or hexagonal atomic arrangement, and on the c axis, the metal atoms are in a layered or oxide-bonded arrangement. The atomic structures are arranged in layers, and on the ab plane (or surface or interface), the atomic structures are aligned along the a axis. It is an oxide semiconductor that contains crystals with different b-axis orientations (rotated around the c-axis). .

[0072] In a broad sense, CAAC-OS is a non-single crystal that has three crystals perpendicular to the ab plane. The atomic arrangement is a square or hexagon, or an equilateral triangle or equilateral hexagon, and the c-axis direction is When viewed from the direction perpendicular to the surface, the metal atoms are arranged in layers or the metal atoms and oxygen atoms are arranged in layers. This refers to materials that

[0073] CAAC-OS is not a single crystal, but it is not composed only of amorphous matter. CAAC-OS contains crystallized parts (crystalline parts), but one crystalline part and another crystalline part Sometimes the boundaries between the parts cannot be clearly distinguished.

[0074] A part of oxygen constituting CAAC-OS may be replaced by nitrogen. The c-axes of the individual crystal parts constituting the CAAC-OS are aligned in a certain direction (for example, The direction may be perpendicular to the surface of the plate, the surface of the CAAC-OS, the film surface, the interface, etc. In the CAAC-OS, the normal to the ab plane of each crystal part is in a certain direction (e.g., the base The direction may be perpendicular to the plate surface, surface, film surface, interface, etc.

[0075] By using the crystalline oxide semiconductor film, the electric field of the transistor can be reduced by irradiation with visible light or ultraviolet light. Thus, the change in electrical characteristics can be further suppressed, resulting in a highly reliable semiconductor device.

[0076] There are three methods for obtaining a crystalline oxide semiconductor film having a c-axis orientation. The oxide semiconductor film is formed at a film formation temperature of 200° C. to 500° C., and a surface of the oxide semiconductor film is roughly The second method is to form a thin film and then heat it at 200°C or higher for 70°C. The third method is to align the c-axis approximately perpendicular to the surface by heat treatment at 0°C or less. After the first layer is thinly formed, it is heated at 200℃ to 700℃ to form the second layer. This method involves forming a film and orienting the c-axis approximately perpendicular to the surface.

[0077] The thickness of the oxide semiconductor film 403 is 1 nm to 200 nm (preferably 5 nm to 30 nm). nm or less) and sputtering and MBE (Molecular Beam Epitaxial Growth) axy method, CVD method, pulsed laser deposition method, ALD (Atomic Layer Deposition In addition, the oxide semiconductor film 403 can be formed by a sintered-position method or the like. This is done by setting multiple substrate surfaces roughly perpendicular to the sputtering target surface. The sputtering equipment that produces a thin film is the so-called CP sputtering equipment (Columnar Plasma Sputtering The film may be formed using a uttering system.

[0078] Note that the oxide semiconductor film 403 is formed under conditions in which a large amount of oxygen is contained (for example, The film is formed by sputtering in a 100% oxygen atmosphere. (preferably, the oxide semiconductor has a stoichiometric composition ratio in a crystalline state, and Preferably, the membrane is a membrane containing regions in which the amount of

[0079] Examples of targets for forming the oxide semiconductor film 403 by a sputtering method include The composition ratio of the oxide was In2O3:Ga2O3:ZnO=1:1:2 [molar ratio]. In-Ga-Zn film is formed using a target. For example, a gold alloy having a molar ratio of In2O3:Ga2O3:ZnO=1:1:1 may be used. Metal oxide targets may also be used.

[0080] The filling rate of the metal oxide target is 90% or more and 100% or less, preferably 95% or more. By using a metal oxide target with a high filling rate, the film can be formed. In addition, the oxide semiconductor film can be a dense film.

[0081] The sputtering gas used in forming the oxide semiconductor film is hydrogen, water, a hydroxyl group, or hydrogen. It is preferable to use a high-purity gas from which impurities such as oxides have been removed.

[0082] The substrate is held in a film-forming chamber that is kept in a reduced pressure state. Then, the remaining moisture in the film-forming chamber is removed. A sputtering gas from which hydrogen and moisture have been removed is introduced, and the substrate 40 is sputtered using the above target. In order to remove residual moisture in the deposition chamber, an oxide semiconductor film 403 is formed on the substrate. type vacuum pumps, such as cryopumps, ion pumps, titanium sublimation pumps It is preferable to use a turbo molecular pump with a cold trap as the exhaust means. The deposition chamber evacuated using a cryopump may be, for example, Hydrogen atoms, water (H2O) and other compounds that contain hydrogen atoms (preferably compounds that contain carbon atoms) Since gases such as impurities and impurities are exhausted from the deposition chamber, the oxide semiconductor film 403 formed in the deposition chamber is The concentration of substances can be reduced.

[0083] In addition, the insulating film 436 and the oxide semiconductor film 403 can be successively formed without exposure to the air. It is preferable that the insulating film 436 and the oxide semiconductor film 403 are formed in succession without exposure to air. By doing so, it is possible to prevent impurities such as hydrogen and moisture from being adsorbed on the surface of the insulating film 436. do.

[0084] In addition, excess hydrogen (including water and a hydroxyl group) is removed (dehydrated or The temperature for the heat treatment is 300° C. or higher and 700° C. or lower. The temperature should be below ℃ or below the distortion point of the substrate. Heat treatment should be performed under reduced pressure or in a nitrogen atmosphere. For example, the substrate can be introduced into an electric furnace, which is one type of heat treatment device, and an oxide semiconductor The film is subjected to a heat treatment at 450° C. for 1 hour in a nitrogen atmosphere.

[0085] The heat treatment device is not limited to an electric furnace, and may be a heat treatment device using heat conduction or heat from a heating element such as a resistance heating element. A device that heats the workpiece by radiation may be used. For example, a GRTA (Gas Reactor Transformer) apid Thermal Anneal) equipment, LRTA (Lamp Rapid T RTA (Rapid Thermal Anneal) equipment, etc. al) equipment can be used. The LRTA equipment can be a halogen lamp, a metal halide lamp, lamp, xenon arc lamp, carbon arc lamp, high pressure sodium lamp, high pressure mercury lamp This is a device that heats the workpiece by radiating light (electromagnetic waves) emitted from a lamp or other light source. The GRTA device is a device that uses high-temperature gas to perform heat treatment. Inert gases such as argon or nitrogen that do not react with the workpiece during heat treatment An active gas is used.

[0086] For example, the substrate is placed in an inert gas heated to a high temperature of 650°C to 700°C as a heat treatment. After heating for several minutes, GRTA may be performed in which the substrate is taken out of the inert gas.

[0087] Note that the heat treatment for dehydration or dehydrogenation is performed after the formation of the oxide semiconductor film 403. Before the formation of the film containing oxygen or before the step of introducing oxygen into the oxide semiconductor film 403, This may be performed at any time during the process of manufacturing resistor 440.

[0088] When heat treatment for dehydration or dehydrogenation is performed before the oxide semiconductor film is processed into an island shape, Therefore, oxygen contained in the insulating film 436 can be prevented from being released by heat treatment. Therefore, it is preferable.

[0089] In the heat treatment, nitrogen or a rare gas such as helium, neon, or argon is used. It is preferable that the nitrogen or hydrogen introduced into the heat treatment device is not included. The purity of rare gases such as sodium, neon, and argon is preferably 6N (99.9999%) or higher. is 7N (99.99999%) or more (i.e. impurity concentration is 1 ppm or less, preferably 0.1 It is preferable to set the concentration to less than ppm.

[0090] After the oxide semiconductor film 403 is heated by heat treatment, high-purity oxygen gas, high-purity 100°C nitrous oxide gas or ultra dry air (CRDS (Cavity Ring Down Laser Dispersion) When measured using a dew point meter using the optical method, the moisture content is 20 ppm (-55°C in dew point equivalent). (air having a concentration of 1 ppm or less, preferably 10 ppb or less) may be introduced. It is preferable that the oxygen gas or nitrous oxide gas does not contain water, hydrogen, etc. Alternatively, the purity of the oxygen gas or nitrous oxide gas introduced into the heat treatment device is preferably 6N or more. or 7N or more (i.e., impurity concentration in oxygen gas or nitrous oxide gas is 1 ppm or less, Preferably, the concentration is 0.1 ppm or less. The action of dehydration or dehydrogenation reduces the amount of impurities present in the process. By supplying oxygen, which is the main component of oxide semiconductors, The semiconductor film 403 can be highly purified and made electrically I-type (intrinsic).

[0091] Note that the oxide semiconductor film may be processed into an island shape, or may be left in a film shape without being processed. In addition, an element isolation region made of an insulating film that isolates the oxide semiconductor film for each element may be provided. good.

[0092] In this embodiment, the formed oxide semiconductor film is subjected to a photolithography process to form island-shaped oxide films. The oxide semiconductor film 403 is then processed into an island-shaped oxide semiconductor film 403. The resist mask may be formed by an inkjet method. Since no photomask is used, the manufacturing cost can be reduced.

[0093] Note that the etching of the oxide semiconductor film may be dry etching or wet etching. For example, an etchant used for wet etching of an oxide semiconductor film may be used. The cleaning solution can be a mixture of phosphoric acid, acetic acid, and nitric acid. O07N (manufactured by Kanto Chemical Co., Ltd.) may also be used.

[0094] Next, a source electrode layer and a drain electrode layer (the same layer as this A conductive film that will become a wiring (including the wiring) is formed. The conductive film is resistant to subsequent heat treatment. As a conductive film used for the source electrode layer and the drain electrode layer, for example, A metal film containing an element selected from the group consisting of I, Cr, Cu, Ta, Ti, Mo, and W, or the above-mentioned Metal nitride films containing elements (titanium nitride film, molybdenum nitride film, tungsten nitride film) ) or the like can be used. In addition, either the upper or lower side of a metal film such as Al or Cu can be used. Both are covered with a high melting point metal film such as Ti, Mo, W, etc. or a metal nitride film of these metals (titanium nitride film, A layered structure of a molybdenum nitride film, a tungsten nitride film, etc. may also be used. The conductive film used for the electrode layer and the drain electrode layer may be formed of a conductive metal oxide. Good. Conductive metal oxides include indium oxide (In2O3) and tin oxide (SnO2 ), zinc oxide (ZnO), indium oxide tin oxide (In2O3-SnO2), indium oxide In2O3-ZnO or these metal oxide materials with silicon oxide It is possible to use one containing

[0095] A resist mask is formed on the conductive film by a photolithography process, and selective etching is performed. After forming the source electrode layer 405a and the drain electrode layer 405b by this, a resist mask In this embodiment, the source electrode layer 405a and the drain electrode layer 405b are A tungsten film having a thickness of 10 nm is formed. In this manner, the source electrode layer 405a and the drain electrode layer 405b are When the electrode layer 405b is thin, the coverage of the gate insulating film 442 formed thereon is good. In addition, the source electrode layer 405a passes through the source electrode layer 405a and the drain electrode layer 405b. In addition, a dopant can be introduced into the oxide semiconductor film 403 under the drain electrode layer 405b. Cut.

[0096] Next, the oxide semiconductor film 403, the source electrode layer 405a, and the drain electrode layer 405b were A covering gate insulating film 442 is formed (see FIG. 1A).

[0097] In order to improve coverage of the gate insulating film 442, the oxide semiconductor film 403 and the source The above-described planarization treatment may also be performed on surfaces of the electrode layer 405a and the drain electrode layer 405b. In particular, when a thin insulating film is used as the gate insulating film 442, It is preferable that the surfaces of the source electrode layer 405a and the drain electrode layer 405b have good flatness. I wish.

[0098] The thickness of the gate insulating film 442 is set to 1 nm or more and 100 nm or less. The E method, CVD method, pulsed laser deposition method, ALD method, etc. can be used appropriately. The gate insulating film 442 is formed by forming a plurality of substrate surfaces approximately perpendicular to the sputtering target surface. The film is formed using a sputtering device that forms a film in the set state, a so-called CP sputtering device. Good too.

[0099] The material of the gate insulating film 442 is a silicon oxide film, a gallium oxide film, an aluminum oxide film, or the like. a silicon nitride film, a silicon oxynitride film, an aluminum oxynitride film, or a nitride oxide film. The gate insulating film 442 can be formed using a silicon film. It is preferable that the gate insulating film 442 contains oxygen in the portion in contact with the gate insulating film 442. It is preferable that oxygen is present in the bulk in an amount exceeding the stoichiometric ratio. For example, when a silicon oxide film is used as the gate insulating film 442, SiO 2+α (where α>0). In this embodiment, the gate insulating film 442 is made of SiO 2+ α (where α>0) is used. This silicon oxide film is used as the gate insulator. By using the oxide semiconductor film 442, oxygen can be supplied to the oxide semiconductor film 403, and the characteristics can be improved. In addition, the gate insulating film 442 can improve the characteristics of the transistor to be manufactured. It is preferable to form the gate insulating film 442 in consideration of the noise and the step coverage of the gate insulating film 442.

[0100] The material of the gate insulating film 442 is hafnium oxide, yttrium oxide, hafnium Silicate (HfSi x O y (x>0, y>0)), nitrogen-doped hafnium silicate HfSiO x N y (x>0, y>0)), hafnium aluminate (HfAl x O y (x>0, y>0)), and the use of high-k materials such as lanthanum oxide for the gate In addition, the gate insulating film 442 may have a single-layer structure or a stacked structure. It may also be a structure.

[0101] Then, the gate electrode layer 401 is formed by plasma CVD or sputtering. The gate electrode layer 401 is formed on the insulating film 442. The material of the gate electrode layer 401 is molybdenum, titanium, tantalum, or the like. Metallic materials such as zinc, tungsten, aluminum, copper, chromium, neodymium, and scandium The gate electrode layer can be formed using a material selected from the group consisting of fluorine, ... 401 is a semiconductor, typically a polycrystalline silicon film doped with impurity elements such as phosphorus Alternatively, a silicide film such as nickel silicide may be used. It may have a layered structure or a laminated structure.

[0102] The material of the gate electrode layer 401 is indium tin oxide or indium oxide containing tungsten oxide. Indium oxide, indium zinc oxide with tungsten oxide, indium zinc oxide with titanium oxide Indium oxide, indium tin oxide with titanium oxide, indium zinc oxide, silicon oxide A conductive material such as indium tin oxide doped with the above-mentioned conductive material can also be used. It is also possible to use a laminated structure of an electrically conductive material and the above-mentioned metal material.

[0103] In addition, a layer of the gate electrode layer 401 in contact with the gate insulating film 442 is made of a metal oxide film containing nitrogen. In-Ga-Zn-O films containing nitrogen, In-Sn-O films containing nitrogen, etc. film, In-Ga-O film containing nitrogen, In-Zn-O film containing nitrogen, Sn In-O film, nitrogen-containing In-O film, and metal nitride film (InN, SnN, etc.) can be used. These films have a work function of 5 electron volts or more, preferably 5.5 electron volts or more. When used as a gate electrode layer, the threshold voltage of the electrical characteristics of a transistor is made positive. Thus, a so-called normally-off switching element can be realized.

[0104] Next, the gate insulating film 442 is etched using the gate electrode layer 401 as a mask to form an oxide A part of the semiconductor film 403 is exposed, and a gate insulating film 402 is formed (see FIG. 1B).

[0105] Next, the oxide semiconductor film 403, the source electrode layer 405a, the drain electrode layer 405b, A metal oxide semiconductor film is formed on the gate insulating film 402 and the gate electrode layer 401. A film 417 containing the element is formed (see FIG. 1C).

[0106] Examples of the film 417 containing a metal element include a metal film, a metal oxide film, and a metal nitride film. .

[0107] The metal elements in the film containing metal elements include aluminum (Al), titanium (Ti), molybdenum (Mo), and tin (Ti). Butan (Mo), Tungsten (W), Hafnium (Hf), Tantalum (Ta), Lanthanum La, barium (Ba), magnesium (Mg), zirconium (Zr), and nickel One or more selected from the group consisting of nickel (Ni) and zinc (Ni) can be used. As the film, a metal film containing one or more selected from any of the above metal elements, a metal oxide film, or a metal nitride film (e.g., titanium nitride film, molybdenum nitride film, tungsten nitride film) In addition, dopants such as phosphorus (P) and boron (B) can be added to the film containing metal elements. In this embodiment, the film 417 containing a metal element has a conductive property. .

[0108] The film 417 containing a metal element is formed by a plasma CVD method, a sputtering method, a deposition method, or the like. The thickness of the film 417 containing the metal element is set to 5 nm or more and 30 nm or less. That's good.

[0109] In this embodiment, an aluminum film having a thickness of 10 nm is used as the film 417 containing a metal element. It is formed by a tarring method.

[0110] Next, the oxide semiconductor film 40 3 through a film 417 containing a metal element, a source electrode layer 405a, and a drain electrode layer 405b. The dopant 421 is selectively introduced through the etch to form low resistance regions 414a and 414b ( See Figure 1(D).

[0111] In this embodiment, the source electrode layer 405a and the drain electrode layer 405b are formed as thin films. Therefore, the oxide semiconductor film under the source electrode layer 405a and the drain electrode layer 405b is also doped. In this example, a source electrode 421 is introduced to form low resistance regions 414a and 414b. The thickness of the electrode layer 405a and the drain electrode layer 405b and the conditions for introducing the dopant 421 are different. That is, the oxide semiconductor film 403 under the source electrode layer 405a and the drain electrode layer 405b In the case where the dopant 421 is not introduced, even if it is introduced, the concentration is low and the source electrode layer 405a Alternatively, the resistance of the region may be higher than that of the low-resistance region other than the region under the drain electrode layer 405b. be.

[0112] The dopant 421 is an impurity that changes the electrical conductivity of the oxide semiconductor film 403. The 421st group of elements includes group 15 elements (typically phosphorus (P), arsenic (As), and antimony). Sb), Boron (B), Aluminum (Al), Nitrogen (N), Argon (Ar) , Helium (He), Neon (Ne), Indium (In), Fluorine (F), Chlorine (Cl ), titanium (Ti), and zinc (Zn) may be used. can.

[0113] The dopant may be contained in the film 417 containing a metal element.

[0114] The dopant 421 is implanted into the film 417 containing the metal element, the source electrode layer 405a, The dopant passes through the drain electrode layer 405b and is introduced into the oxide semiconductor film 403. The methods for introducing 421 include ion implantation, ion doping, and plasma immersion. Ion implantation or the like can be used. In this case, the dopant 42 It is preferable to use the elemental ion of 1 or the hydride, fluoride, or chloride ions.

[0115] The dopant 421 introduction process is performed by controlling the injection conditions such as the acceleration voltage and the dose amount, and the amount of gold to be passed through. The thickness of the metal-containing film 417 can be appropriately set and controlled. For example, boron can be used to When implanting boron ions using the ion implantation method, the acceleration voltage is 15 kV and the dose is 1×10 15 ions / cm 2 Preferably, the dose is 1×10 13 ions / cm 2 5×10 or more 16 ions / cm 2 The following would suffice.

[0116] The concentration of dopant 421 in the low resistance region is 5×10 18 atoms / cm 3 1 more ×10 22 atoms / cm 3 It is preferable that:

[0117] The dopant may be introduced while the substrate 400 is being heated.

[0118] Note that the treatment of introducing the dopant 421 into the oxide semiconductor film 403 may be performed multiple times. A plurality of dopants may be used.

[0119] After the introduction of the dopant 421, a heat treatment may be performed. The temperature is 300°C to 700°C, preferably 300°C to 450°C, for 1 hour in an oxygen atmosphere. It is preferable to carry out the heating under nitrogen atmosphere, reduced pressure, or air (ultra-dry air). Processing may be carried out.

[0120] When the oxide semiconductor film 403 is a crystalline oxide semiconductor film, the dopant 421 is introduced. In this case, a heat treatment is performed after the introduction of the dopant 421. By this, the crystallinity of the oxide semiconductor film 403 can be restored.

[0121] Next, heat treatment is performed while the metal-element-containing film 417 and the oxide semiconductor film 403 are partly in contact with each other. The heat treatment is preferably carried out in an oxygen atmosphere. The heat treatment is preferably carried out in a nitrogen atmosphere under reduced pressure. The heating temperature is 100° C. or higher and 700° C. or lower, preferably 200° C. or lower. The temperature should be from 0°C to 400°C.

[0122] For example, the substrate is introduced into an electric furnace, which is one of the heat treatment devices, and the film 417 containing a metal element and The oxide semiconductor film 403 is subjected to heat treatment at 300° C. in an oxygen atmosphere for one hour.

[0123] The heat treatment device is not limited to an electric furnace, and may be a heat treatment device using heat conduction or heat from a heating element such as a resistance heating element. A device that heats the workpiece by radiation may be used. For example, a GRTA (Gas Reactor Transformer) apid Thermal Anneal) equipment, LRTA (Lamp Rapid T RTA (Rapid Thermal Anneal) equipment, etc. al) equipment can be used. The LRTA equipment can be a halogen lamp, a metal halide lamp, lamp, xenon arc lamp, carbon arc lamp, high pressure sodium lamp, high pressure mercury lamp This is a device that heats the workpiece by radiating light (electromagnetic waves) emitted from a lamp or other light source. The GRTA device is a device that uses high-temperature gas to perform heat treatment. Inert gases such as argon or nitrogen that do not react with the workpiece during heat treatment An active gas is used.

[0124] For example, the substrate is placed in an inert gas heated to a high temperature of 650°C to 700°C as a heat treatment. After heating for several minutes, GRTA may be performed in which the substrate is taken out of the inert gas.

[0125] Heat treatment is carried out in a vacuum of nitrogen, oxygen, or ultra-dry air (water content of 20 ppm or less, preferably 1 ppm). m or less, more preferably 10 ppb or less of air), or rare gases (argon, helium, etc. The above-mentioned nitrogen, oxygen, ultra-dry air, or rare gas atmosphere may be used. It is preferable that the gas does not contain water, hydrogen, etc. Or the purity of the rare gas is 6N (99.9999%) or more, preferably 7N (99.999 99%) or more (i.e., impurity concentration is 1 ppm or less, preferably 0.1 ppm or less). is preferred.

[0126] By the heat treatment, a metal element is introduced from the film 417 containing a metal element into the oxide semiconductor film 403. As a result, low-resistance regions 404a and 404b are formed in the oxide semiconductor film 403. A low-resistance region 404a containing a dopant and a metal element is disposed between the channel forming region 409. , 404b, and low resistance regions 406a, 406b containing dopants are formed. The low resistance regions 404a and 404b containing a dopant and a metal element are more resistive than the low resistance regions 404a and 404b containing a dopant and a metal element. The resistance of the first and second resistive regions 406a and 406b can be lower than that of the second and third resistive regions 406a and 406b.

[0127] In this embodiment, boron is used as the dopant and aluminum is used as the metal element. , low resistance regions 404a, 404b contain boron and aluminum, and low resistance region 406a , 406b contains boron.

[0128] In addition, a processing step for introducing a metal element from the film 417 containing a metal element to the oxide semiconductor film 403 is performed. By the heat treatment, the film 417 containing the metal element becomes the film 407 containing the metal element. For example, The metal film used as the film containing an element 417 was a metal oxide insulator as the film containing a metal element 407. Such a metal oxide film can be used as an insulating film. In this study, an aluminum film was used as the film 417 containing a metal element, so the aluminum was oxidized by heat treatment. Since the aluminum oxide film is a metal oxide insulating film, it is used as an insulating film. It is possible.

[0129] Through the above steps, the transistor 440 of this embodiment is manufactured (see FIG. 1E). In the channel length direction, low resistance regions 404a, 404b, and low resistance By including the oxide semiconductor film 403 including the regions 406a and 406b, The transistor 440 has high on-characteristics (e.g., on-current and field-effect mobility), and is capable of high-speed operation and high-speed response. The answer becomes possible.

[0130] The low resistance regions 404a, 404b and the low resistance regions 406a, 406b are source regions or drain regions. By providing the low resistance regions 404a and 404b, Therefore, the channel formation region 409 formed between the low resistance regions 404a and 404b is added. In addition, the electric field generated by the oxide in the low resistance regions 406a and 406b can be reduced. The semiconductor film 403 is electrically connected to the source electrode layer 405a and the drain electrode layer 405b. By this, the oxide semiconductor film 403, the source electrode layer 405a, and the drain electrode layer 4 The contact resistance with 05b can be reduced.

[0131] Another insulating film may be stacked over the film 407 containing a metal element, which is a metal oxide insulating film.

[0132] In addition, the film 407 containing the metal element may be removed. For example, if the film 407 containing the metal element is conductive, If the metal element-containing film 407 has the above-mentioned characteristic, the metal element-containing film 407 is removed and another insulating film 416 is formed as shown in FIG. It can be formed.

[0133] FIG. 6A corresponds to FIG. 1E, and a metal element is provided to cover the transistor 440. If the film 407 containing a metal element is insulating, it can be used as it is. However, if it is conductive or if you want to provide another insulating film, it is better to use gold. The metal element-containing film 407 is then removed (see FIG. 6(B)).

[0134] Then, the insulating film 416 is formed to cover the transistor 440 (see FIG. 6C).

[0135] The insulating film 416 is formed by mixing impurities such as water and hydrogen into the insulating film 416 by a method such as sputtering. In addition, the insulating film 416 is preferably formed by using a method that does not contain excess oxygen. The oxide semiconductor film 403 can be supplied with oxygen by using a film containing the oxygen.

[0136] In this embodiment, a silicon oxide film having a thickness of 100 nm is formed as the insulating film 416 by sputtering. The silicon oxide film is formed by sputtering. Typically, under an argon atmosphere, oxygen atmosphere, or a mixture of rare gas and oxygen atmosphere. This can be done.

[0137] In the same manner as in the formation of the oxide semiconductor film, in order to remove residual moisture in the deposition chamber of the insulating film 416, It is preferable to use an adsorption type vacuum pump (such as a cryopump). The concentration of impurities contained in the insulating film 416 formed in the deposition chamber evacuated by using a vacuum pump can be reduced. In addition, as an exhaust means for removing residual moisture in the deposition chamber of the insulating film 416, a turbo A molecular pump plus a cold trap may also be used.

[0138] The insulating film 416 is formed using a sputtering gas of hydrogen, water, a hydroxyl group, or hydrogen. It is preferable to use a high-purity gas from which impurities such as oxides have been removed.

[0139] When the insulating film 416 is stacked, typically, an aluminum oxide film, an oxide film, or the like can be used in addition to a silicon oxide film. An inorganic insulating film such as a silicon oxide nitride film, an aluminum oxide nitride film, or a gallium oxide film is used. For example, the insulating film 416 may be a silicon oxide film and an aluminum oxide film. A stack of the above can be used.

[0140] The film 407 containing a metal element or the insulating film 416 provided over the oxide semiconductor film 403 The aluminum oxide film that can be used is resistant to both impurities such as hydrogen and moisture, and oxygen. In contrast, it has a high blocking effect that prevents substances from passing through the membrane.

[0141] Therefore, the aluminum oxide film is free from hydrogen, which is a variable factor during and after the manufacturing process. Impurities such as moisture may be mixed into the oxide semiconductor film 403, and the main components of the oxide semiconductor may be The oxide semiconductor film 403 functions as a protective film for preventing oxygen, which is a material, from being released from the oxide semiconductor film 403.

[0142] In addition, a planarizing insulating film may be formed to reduce surface irregularities caused by the transistors. The smoothing insulating film is made of organic materials such as polyimide, acrylic, and benzocyclobutene resins. In addition to the above organic materials, low-dielectric constant materials (low-k materials) can be used. In addition, by stacking a plurality of insulating films made of these materials, A planarizing insulating film may be formed.

[0143] In this embodiment, a planarization insulating film 415 is formed over the metal element-containing film 407 or the insulating film 416. In addition, the metal element-containing film 407 or the insulating film 416 and the planarization insulating film 415 are formed. Openings reaching the source electrode layer 405a and the drain electrode layer 405b are formed, and the source electrodes are The wiring layer 465a electrically connects to the drain electrode layer 405b. Form 5b (see FIG. 1(F) and FIG. 6(D)).

[0144] As shown in FIGS. 3A to 3F, the source electrode layer 405a and the drain electrode layer 40 5b, the metal element-containing film 407, the insulating film 41, and the like, such as the wiring layer 465a and the wiring layer 465b. It may also be provided on the 6.

[0145] In the case of FIG. 3, a source electrode layer 405a and a source electrode layer 405b are formed by covering a part of the oxide semiconductor film 403 as in FIG. Since the drain electrode layer 405b is not formed, the channel overlapping with the gate electrode layer 401 is Metal elements and dopants are introduced into the regions other than the oxide formation region 409. In the semiconductor film 403, the low resistance regions formed on both sides of the channel formation region 409 are The transistor 4 is made up of low resistance regions 404a and 404b that all contain metal elements and dopants. The number becomes 45.

[0146] Note that in the example of the semiconductor device illustrated in FIG. 3F, a metal oxide insulating film is provided over the transistor 445. The metal element-containing film 407 and the insulating film 416 are laminated. The openings formed in the film 407 and the insulating film 416 reach the low resistance regions 404a and 404b. A source electrode layer 405a and a drain electrode layer 405b are formed.

[0147] As shown in FIGS. 7A and 7B, a sidewall structure is formed on the side surface of the gate electrode layer 401. Sidewall insulating layers 412a and 412b may be provided. After forming an insulating film covering the gate electrode layer 401, this is subjected to RIE (Reactive ion etching). Anisotropic etching using reactive ion etching (RIE) method A sidewall insulating layer 412a having a sidewall structure is formed on the sidewall of the gate electrode layer 401 in a self-aligned manner. Here, the insulating film is not particularly limited. For example, OS (Tetraethyl-Ortho-Silicate) or silane, etc. and acid Silicon oxide with good step coverage is used, which is formed by reacting silicon with nitrogen or nitrous oxide. The insulating film can be formed by thermal CVD, plasma CVD, atmospheric CVD, and bias ECRCVD. It can be formed by a method such as low temperature oxidation (LTO) or sputtering. Silicon oxide formed by the low temperature oxidation method It may be used.

[0148] In the case of FIG. 7(A) and FIG. 7(B), the gate insulating film 402 is a gate electrode layer 401 and a sidewall insulating layer 402. The gate insulating film can be etched using 12a and 412b as a mask to form the gate insulating film.

[0149] In addition, in FIG. 7(A) and (B), when the insulating film is etched, the insulating film on the gate electrode layer 401 is The film is removed to expose the gate electrode layer 401, but the insulating film is left on the gate electrode layer 401. The sidewall insulating layers 412a and 412b may be formed in such a shape. A protective film may be formed on the electrode layer 401. In this manner, the gate electrode layer 401 is protected. This makes it possible to prevent the gate electrode layer from being thinned during etching. The etching method may be a dry etching method or a wet etching method. A filtering method can be used.

[0150] When the step of forming the sidewall insulating layers 412a and 412b is performed before the step of introducing the dopant, As shown in FIG. 7A, the sidewall insulating layers 412a and 412b are also formed during the dopant introduction process. The oxide semiconductor film 403 under the sidewall insulating layers 412a and 412b is doped with dopant to serve as a mask. The transistor 420a has a structure in which no oxide is introduced.

[0151] On the other hand, the step of forming the sidewall insulating layers 412a and 412b is performed after the step of introducing the dopant. In this case, as shown in FIG. 7B, the sidewall insulating layers 412a and 41 Since the insulating layer 412a and the insulating layer 412b do not function as a mask, the oxide semiconductor film 403 under the insulating layer 412a and the insulating layer 412b A dopant is introduced into the semiconductor substrate 406, and the semiconductor substrate 406 has a structure including low resistance regions 406c and 406d containing the dopant. This becomes transistor 420b.

[0152] The oxide semiconductor film 403 which is highly purified and in which oxygen vacancies are filled is free of impurities such as hydrogen and water. The hydrogen concentration in the oxide semiconductor film 403 is 5×10 19 atoms / cm 3 Less than or equal to 5×10 18 atoms / cm 3 The following is an oxide semiconductor. The hydrogen concentration in the film 403 was measured by secondary ion mass spectrometry (SIMS). It is measured by Mass Spectrometry (MSM).

[0153] The oxide semiconductor film 403 has very few carriers (close to zero). The concentration is 1×10 14 / cm 3 Less than 1 x 10 12 / cm 3 Less than, even more preferred Or 1×10 11 / cm 3 is less than.

[0154] The oxide film produced by the present embodiment is highly purified and contains an excess of oxygen to compensate for the oxygen deficiency. The transistor 440 using the organic semiconductor film 403 has a current value in an off state (off current value ) per 1 μm of channel width at room temperature is 100 zA / μm (1 zA (zeptoampere) is 1×10 -21 A) or less, preferably 10zA / μm or less, more preferably 1zA / μm or less It is possible to lower it to a level of 100 yA / μm or less, more preferably.

[0155] As described above, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. A body device can be provided.

[0156] (Embodiment 2) In this embodiment mode, another embodiment of a semiconductor device and a manufacturing method of the semiconductor device will be described with reference to FIGS. The parts and steps having the same or similar functions as those in the above embodiment are the same as those in the above embodiment. The embodiment can be carried out in the same manner as in the first embodiment, and the repeated explanation will be omitted. The details are omitted.

[0157] In this embodiment, in a method for manufacturing a semiconductor device according to the disclosed invention, An example in which the step of introducing a metal element into the semiconductor layer is carried out prior to the step of introducing a dopant will be described.

[0158] 2A to 2D show an example of a method for manufacturing the transistor 440 of this embodiment.

[0159] FIG. 2A corresponds to FIG. 1C, and has an insulating surface on which an insulating film 436 is provided. On a substrate 400, an oxide semiconductor film 403, a source electrode layer 405a, a drain electrode layer 405 b, a gate insulating film 402, a gate electrode layer 401, and a film 417 containing a metal element are formed. do.

[0160] In this embodiment, an aluminum film having a thickness of 10 nm is used as the film 417 containing a metal element. It is formed by a tarring method.

[0161] Next, heat treatment is performed while the metal-element-containing film 417 and the oxide semiconductor film 403 are partly in contact with each other. The heat treatment is preferably carried out in an oxygen atmosphere. The heat treatment is preferably carried out in a nitrogen atmosphere under reduced pressure. The heating temperature is 100° C. or higher and 700° C. or lower, preferably 20 The temperature should be between 0°C and 400°C.

[0162] For example, the substrate is introduced into an electric furnace, which is one of the heat treatment devices, and the film 417 containing a metal element and The oxide semiconductor film 403 is subjected to heat treatment at 300° C. in an oxygen atmosphere for one hour.

[0163] By the heat treatment, a metal element is introduced from the film 417 containing a metal element into the oxide semiconductor film 403. As a result, low resistance regions 426a and 426b are formed (see FIG. 2(B)). a, 426b contain metal elements.

[0164] In addition, a processing step for introducing a metal element from the film 417 containing a metal element to the oxide semiconductor film 403 is performed. By the heat treatment, the film 417 containing the metal element becomes the film 407 containing the metal element. For example, The metal film used as the film containing an element 417 was a metal oxide insulator as the film containing a metal element 407. Such a metal oxide film can be used as an insulating film. In this study, an aluminum film was used as the film 417 containing a metal element, so the aluminum was oxidized by heat treatment. Since the aluminum oxide film is a metal oxide insulating film, it is used as an insulating film. It is possible.

[0165] Next, the oxide semiconductor film 40 3 through a film 407 containing a metal element, a source electrode layer 405a, and a drain electrode layer 405b. A dopant 421 is selectively introduced through the silicon dioxide film 402 to form low resistance regions 404a and 404b.

[0166] In this embodiment, the source electrode layer 405a and the drain electrode layer 405b are formed as thin films. Therefore, the oxide semiconductor film under the source electrode layer 405a and the drain electrode layer 405b is also doped. In this example, a source electrode 421 is introduced to form low resistance regions 406a and 406b. The thickness of the electrode layer 405a and the drain electrode layer 405b and the conditions for introducing the dopant 421 are different. That is, the oxide semiconductor film 403 under the source electrode layer 405a and the drain electrode layer 405b In some cases, the dopant 421 is not introduced.

[0167] In this embodiment, boron is used as the dopant 421, and boron ions are implanted by ion implantation. Inject the nicotine.

[0168] Therefore, in the oxide semiconductor film 403, the dopant and the and low resistance regions 404a and 404b containing a metal element, and low resistance region 406a containing a dopant. , 406b are formed. Note that low resistance regions 404a, 406b containing dopants and metal elements are formed. The resistance of the low-resistance regions 404b is lower than that of the low-resistance regions 406a and 406b containing the dopant. can be done.

[0169] Through the above steps, the transistor 440 of this embodiment is manufactured (see FIG. 2C). In the channel length direction, low resistance regions 404a, 404b, and low resistance By including the oxide semiconductor film 403 including the regions 406a and 406b, The transistor 440 has high on-characteristics (e.g., on-current and field-effect mobility), and is capable of high-speed operation and high-speed response. The answer becomes possible.

[0170] The low resistance regions 404a, 404b and the low resistance regions 406a, 406b are source regions or drain regions. By providing the low resistance regions 404a and 404b, Therefore, the channel formation region 409 formed between the low resistance regions 404a and 404b is added. In addition, the electric field generated by the oxide in the low resistance regions 406a and 406b can be reduced. The semiconductor film 403 is electrically connected to the source electrode layer 405a and the drain electrode layer 405b. By this, the oxide semiconductor film 403, the source electrode layer 405a, and the drain electrode layer 4 The contact resistance with 05b can be reduced.

[0171] In this embodiment, a planarization insulating film 415 is formed over the film 407 containing a metal element. The source electrode layer 405a and the drain electrode layer 405b are formed on the metal element-containing film 407 and the planarization insulating film 415. An opening is formed so as to reach the electrode layer 405b, and the source electrode layer 405a and the drain electrode layer 40 5b (see FIG. 2(D)). .

[0172] As described above, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. A body device can be provided.

[0173] This embodiment mode can be implemented in appropriate combination with other embodiment modes.

[0174] (Embodiment 3) In this embodiment mode, another embodiment of a semiconductor device and a manufacturing method of the semiconductor device will be described with reference to FIGS. The parts and steps having the same or similar functions as those in the above embodiment are the same as those in the above embodiment. The embodiment can be carried out in the same manner as in the first embodiment, and the repeated explanation will be omitted. The details are omitted.

[0175] In this embodiment mode, the source electrode layer and the drain electrode An example of a method for manufacturing a transistor having a different connection structure between a metal oxide layer and an oxide semiconductor film will be described.

[0176] 4A to 4F show an example of a method for manufacturing the transistor 450 in this embodiment. vinegar.

[0177] First, an insulating film 436 is formed on a substrate 400 .

[0178] Next, a source electrode layer and a drain electrode layer (formed from the same layer as this A conductive film that will become the wiring (including the wiring) is formed.

[0179] A resist mask is formed on the conductive film by a photolithography process, and selective etching is performed. After forming the source electrode layer 405a and the drain electrode layer 405b by this, a resist mask Remove.

[0180] Then, an oxide semiconductor layer is formed over the insulating film 436, the source electrode layer 405a, and the drain electrode layer 405b. A conductive film 403 is formed. A gate insulating film 442 is formed so as to cover the oxide semiconductor film 403. (See Figure 4(A)).

[0181] A gate electrode layer 401 is formed on the gate insulating film 442 .

[0182] Next, the gate insulating film 442 is etched using the gate electrode layer 401 as a mask to form an oxide A part of the semiconductor film 403 is exposed, and a gate insulating film 402 is formed (see FIG. 4B).

[0183] Next, the source electrode layer 405a, the drain electrode layer 405b, the oxide semiconductor film 403, and the gate A metal oxide semiconductor film is formed on the gate insulating film 402 and the gate electrode layer 401. A film 417 containing the element is formed (see FIG. 4C).

[0184] In this embodiment, an aluminum film having a thickness of 10 nm is used as the film 417 containing a metal element. It is formed by a tarring method.

[0185] Next, the oxide semiconductor film 40 3, a dopant 421 is selectively introduced through a film 417 containing a metal element to form a low resistance region. 414a and 414b are formed (see FIG. 4(D)).

[0186] In this embodiment, phosphorus is used as the dopant 421, and an oxide semiconductor The film 403 is implanted with phosphorus ions.

[0187] The concentration of dopant 421 in the low resistance region is 5×10 18 atoms / cm 3 1 more ×10 22 atoms / cm 3 It is preferable that:

[0188] After the introduction of the dopant 421, a heat treatment may be performed. The temperature is 300°C to 700°C, preferably 300°C to 450°C, for 1 hour in an oxygen atmosphere. It is preferable to carry out the heating under nitrogen atmosphere, reduced pressure, or air (ultra-dry air). Processing may be carried out.

[0189] Next, heat treatment is performed while the metal-element-containing film 417 and the oxide semiconductor film 403 are partly in contact with each other. The heat treatment is preferably carried out in an oxygen atmosphere. The heat treatment is preferably carried out in a nitrogen atmosphere under reduced pressure. The heating temperature is 100° C. or higher and 700° C. or lower, preferably 20 The temperature should be between 0°C and 400°C.

[0190] For example, the substrate is introduced into an electric furnace, which is one of the heat treatment devices, and the film 417 containing a metal element and The oxide semiconductor film 403 is subjected to heat treatment at 300° C. in an oxygen atmosphere for one hour.

[0191] By the heat treatment, a metal element is introduced from the film 417 containing a metal element into the oxide semiconductor film 403. As a result, low-resistance regions 404a and 404b are formed in the oxide semiconductor film 403. A low-resistance region 404a containing a dopant and a metal element is disposed between the channel forming region 409. , 404b are formed. Note that low resistance regions 404a, 404b containing dopants and metal elements are 04b can be a low resistance.

[0192] In this embodiment, phosphorus is used as the dopant and aluminum is used as the metal element. The low resistance regions 404a, 404b include phosphorus and aluminum.

[0193] In addition, a processing step for introducing a metal element from the film 417 containing a metal element to the oxide semiconductor film 403 is performed. By the heat treatment, the film 417 containing the metal element becomes the film 407 containing the metal element. For example, The metal film used as the film containing an element 417 was a metal oxide insulator as the film containing a metal element 407. Such a metal oxide film can be used as an insulating film. In this study, an aluminum film was used as the film 417 containing a metal element, so the aluminum was oxidized by heat treatment. Since the aluminum oxide film is a metal oxide insulating film, it is used as an insulating film. It is possible.

[0194] Through the above steps, the transistor 450 of this embodiment is manufactured (see FIG. 4E). The channel forming region 409 is sandwiched between low resistance regions 404a and 404b in the channel length direction. By having the nitride semiconductor film 403, the transistor 450 has an on-characteristic (e.g., The electrons in the electron-doped semiconductor have high current and field-effect mobility, enabling high-speed operation and high-speed response.

[0195] The low resistance regions 404a and 404b can function as a source region and a drain region. By providing the low resistance regions 404a and 404b, The electric field applied to the channel forming region 409 formed between the gate electrodes 04b can be reduced. In addition, in the low resistance regions 404a and 404b, the oxide semiconductor film 403 and the source electrode layer 4 The drain electrode layer 405a and the drain electrode layer 405b are electrically connected to each other. The contact resistance between the film 403 and the source electrode layer 405a and the drain electrode layer 405b is reduced. This can be done.

[0196] In this embodiment, a planarization insulating film 415 is formed over the film 407 containing a metal element. The source electrode layer 405a and the drain electrode layer 405b are formed on the metal element-containing film 407 and the planarization insulating film 415. An opening is formed so as to reach the electrode layer 405b, and the source electrode layer 405a and the drain electrode layer 40 5b (see FIG. 4(F)). .

[0197] As described above, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. A body device can be provided.

[0198] This embodiment mode can be implemented in appropriate combination with other embodiment modes.

[0199] (Embodiment 4) In this embodiment mode, another embodiment of a semiconductor device and a manufacturing method of the semiconductor device will be described with reference to FIGS. The parts and steps having the same or similar functions as those in the above embodiment are the same as those in the above embodiment. The embodiment can be carried out in the same manner as in the first embodiment, and the repeated explanation will be omitted. The details are omitted.

[0200] In this embodiment, in a method for manufacturing a semiconductor device according to the disclosed invention, An example in which the step of introducing a metal element into the semiconductor layer is carried out prior to the step of introducing a dopant will be described.

[0201] 5A to 5D illustrate an example of a method for manufacturing the transistor 450 of this embodiment.

[0202] FIG. 5A corresponds to FIG. 4C, and has an insulating surface on which an insulating film 436 is provided. On the substrate 400, a source electrode layer 405a, a drain electrode layer 405b, and an oxide semiconductor film 40 3, a gate insulating film 402, a gate electrode layer 401, and a film 417 containing a metal element are formed. do.

[0203] In this embodiment, an aluminum film having a thickness of 10 nm is used as the film 417 containing a metal element. It is formed by a tarring method.

[0204] Next, heat treatment is performed while the metal-element-containing film 417 and the oxide semiconductor film 403 are partly in contact with each other. The heat treatment may be performed in an oxygen atmosphere.

[0205] For example, the substrate is introduced into an electric furnace, which is one of the heat treatment devices, and the film 417 containing a metal element and The oxide semiconductor film 403 is subjected to heat treatment at 300° C. in an oxygen atmosphere for one hour.

[0206] By the heat treatment, a metal element is introduced from the film 417 containing a metal element into the oxide semiconductor film 403. As a result, low resistance regions 426a and 426b are formed (see FIG. 5(B)). a, 426b contain metal elements.

[0207] In addition, a processing step for introducing a metal element from the film 417 containing a metal element to the oxide semiconductor film 403 is performed. By the heat treatment, the film 417 containing the metal element becomes the film 407 containing the metal element. For example, The metal film used as the film containing an element 417 was a metal oxide insulator as the film containing a metal element 407. Such a metal oxide film can be used as an insulating film. In this study, an aluminum film was used as the film 417 containing a metal element, so the aluminum was oxidized by heat treatment. Since the aluminum oxide film is a metal oxide insulating film, it is used as an insulating film. It is possible.

[0208] Next, the oxide semiconductor film 40 3 through a film 407 containing a metal element, a source electrode layer 405a, and a drain electrode layer 405b. A dopant 421 is selectively introduced through the silicon dioxide film 402 to form low resistance regions 404a and 404b.

[0209] In this embodiment, phosphorus is used as the dopant 421, and phosphorus ions are implanted by ion implantation. Perform the injection.

[0210] Therefore, in the oxide semiconductor film 403, the dopant and the Low resistance regions 404a and 404b containing dopants and metal elements are formed. The low resistance regions 404a, 404b including may be low resistance.

[0211] Through the above steps, the transistor 450 of this embodiment is manufactured (see FIG. 5C). The channel forming region 409 is sandwiched between low resistance regions 404a and 404b in the channel length direction. By having the nitride semiconductor film 403, the transistor 450 has an on-characteristic (e.g., The electrons in the electron-doped semiconductor have high current and field-effect mobility, enabling high-speed operation and high-speed response.

[0212] The low resistance regions 404a and 404b can function as a source region and a drain region. By providing the low resistance regions 404a and 404b, The electric field applied to the channel forming region 409 formed between the gate electrodes 04b can be reduced. In addition, in the low resistance regions 404a and 404b, the oxide semiconductor film 403 and the source electrode layer 4 The drain electrode layer 405a and the drain electrode layer 405b are electrically connected to each other. The contact resistance between the film 403 and the source electrode layer 405a and the drain electrode layer 405b is reduced. This can be done.

[0213] In this embodiment, a planarization insulating film 415 is formed over the film 407 containing a metal element. The source electrode layer 405a and the drain electrode layer 405b are formed on the metal element-containing film 407 and the planarization insulating film 415. An opening is formed so as to reach the electrode layer 405b, and the source electrode layer 405a and the drain electrode layer 40 5b (see FIG. 5(D)). .

[0214] As described above, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. A body device can be provided.

[0215] This embodiment mode can be implemented in appropriate combination with other embodiment modes.

[0216] (Embodiment 5) In this embodiment mode, another embodiment of a semiconductor device and a manufacturing method of the semiconductor device will be described with reference to FIGS. The parts and steps having the same or similar functions as those in the above embodiment are the same as those in the above embodiment. The embodiment can be carried out in the same manner as in the first embodiment, and the repeated explanation will be omitted. The details are omitted.

[0217] In this embodiment, an example of a bottom-gate transistor is shown in FIGS. The transistor 410 shown in FIG. 1 is called a channel protection type (also called a channel stop type). This is one of the bottom-gate structures and is also called an inverted staggered transistor.

[0218] 8A to 8F illustrate an example of a method for manufacturing the transistor 410. FIG.

[0219] First, a conductive film is formed on a substrate 400 having an insulating surface, and then a first photolithography process is performed. A gate electrode layer 401 is formed through a process.

[0220] A gate insulating film 402 is formed on the gate electrode layer 401. An oxide semiconductor film 403 is formed over the gate insulating film 402 .

[0221] A portion of the oxide semiconductor film 403 overlapping with the gate electrode layer 401 functions as a channel protective film. An insulating film 427 is formed (see FIG. 8A).

[0222] The insulating film 427 may be formed using a material and a method similar to those of the insulating film 416. Typically, the insulating film 427 is formed using a silicon oxide film. Silicon film, silicon oxynitride film, aluminum oxide film, aluminum oxynitride film, halide film gallium oxide film, silicon nitride film, aluminum nitride film, silicon oxide nitride film A single layer or a laminate of an inorganic insulating film such as a com film or an aluminum nitride oxide film can be used. .

[0223] The insulating film 427 in contact with the oxide semiconductor film 403 (when the insulating film 427 has a stacked structure, When the oxide semiconductor film 403 is made to contain a large amount of oxygen, 3.

[0224] Next, a gate electrode layer 401, a gate insulating film 402, an oxide semiconductor film 403, and an insulating film 42 A film 417 containing a metal element is formed in contact with part of the oxide semiconductor film 403 over the oxide semiconductor film 407 (FIG. 8(B)).

[0225] In this embodiment, an aluminum film having a thickness of 10 nm is used as the film 417 containing a metal element. It is formed by a tarring method.

[0226] Next, the oxide semiconductor film 40 3, a dopant 421 is selectively introduced through a film 417 containing a metal element to form a low resistance region. 414a and 414b are formed (see FIG. 8(C)).

[0227] In this embodiment, the insulating film 427 that functions as a channel protective film is formed by introducing a dopant 421. A separate resist mask is formed to mask the dopant 421. Alternatively, a channel etch type transistor without a channel protection film may be used. In the case of a diode, a separate resist mask can be formed and dopants can be selectively introduced. stomach.

[0228] In this embodiment, boron is used as the dopant 421, and an oxide semiconductor is formed by ion implantation. Boron ions are implanted into the body film 403 .

[0229] The concentration of dopant 421 in the low resistance region is 5×10 18 / cm 3 More than 1×10 22 / cm 3 It is preferable that:

[0230] After the introduction of the dopant 421, a heat treatment may be performed.

[0231] Next, heat treatment is performed while the metal-element-containing film 417 and the oxide semiconductor film 403 are partly in contact with each other. The heat treatment may be performed in an oxygen atmosphere.

[0232] For example, the substrate is introduced into an electric furnace, which is one of the heat treatment devices, and the film 417 containing a metal element and The oxide semiconductor film 403 is subjected to heat treatment at 300° C. in an oxygen atmosphere for one hour.

[0233] By the heat treatment, a metal element is introduced from the film 417 containing a metal element into the oxide semiconductor film 403. As a result, low-resistance regions 404a and 404b are formed in the oxide semiconductor film 403. A low-resistance region 404a containing a dopant and a metal element is disposed between the channel forming region 409. , 404b are formed. Note that low resistance regions 404a, 404b containing dopants and metal elements are 04b can be a low resistance.

[0234] In this embodiment, boron is used as the dopant and aluminum is used as the metal element. The low resistance regions 404a and 404b contain boron and aluminum.

[0235] In addition, a processing step for introducing a metal element from the film 417 containing a metal element to the oxide semiconductor film 403 is performed. By the heat treatment, the film 417 containing the metal element becomes the film 407 containing the metal element (FIG. 8(D) reference).

[0236] Next, the film 407 containing a metal element is removed, and the source An electrode layer 405a and a drain electrode layer 405b are formed. In the case where the insulating film has conductivity, the insulating film is not removed, and the source electrode layer 405a and the drain electrode layer 405b are left as masks. The source electrode layer 405a and the drain electrode layer 405b are formed by etching the mask. May be used as part of 05b.

[0237] Through the above steps, the transistor 410 of this embodiment is manufactured (see FIG. 8E). The channel forming region 409 is sandwiched between low resistance regions 404a and 404b in the channel length direction. By having the nitride semiconductor film 403, the transistor 410 has an on-characteristic (e.g., The electrons in the electron-doped semiconductor have high current and field-effect mobility, enabling high-speed operation and high-speed response.

[0238] The low resistance regions 404a and 404b can function as a source region and a drain region. By providing the low resistance regions 404a and 404b, The electric field applied to the channel forming region 409 formed between the gate electrodes 04b can be reduced. In addition, in the low resistance regions 404a and 404b, the oxide semiconductor film 403 and the source electrode layer 4 The drain electrode layer 405a and the drain electrode layer 405b are electrically connected to each other. The contact resistance between the film 403 and the source electrode layer 405a and the drain electrode layer 405b is reduced. This can be done.

[0239] In this embodiment, an insulating film 416 is formed as a protective film over the transistor 410 (see FIG. 8). (See (F)).

[0240] As described above, by using the transistor with excellent electrical characteristics, a high-performance and highly reliable semiconductor device can be obtained. A body device can be provided.

[0241] This embodiment mode can be implemented in appropriate combination with other embodiment modes.

[0242] (Embodiment 6) In this embodiment mode, another embodiment of a method for manufacturing a semiconductor device will be described. A part or a part having a similar function and a process can be performed in the same manner as in the above embodiment. In addition, detailed explanations of the same parts will be omitted.

[0243] Note that in this embodiment, the transistors 440 and 441 described in any of Embodiments 1 to 5 are Applicable to 45, 420a, 420b, 450, 410.

[0244] In this embodiment, in a manufacturing method of a semiconductor device according to the disclosed invention, The oxide semiconductor film 403 that has been subjected to the oxidation treatment is treated with oxygen (at least oxygen radicals and oxygen atoms). ions, or oxygen ions) are introduced to supply oxygen into the film.

[0245] By the dehydration or dehydrogenation treatment, oxygen, which is a main component material of the oxide semiconductor, is simultaneously In the oxide semiconductor film 403, oxygen is released and the amount of oxygen is reduced. In the area where the oxygen is removed, oxygen vacancies exist, and these oxygen vacancies cause fluctuations in the electrical characteristics of the transistor. Therefore, donor levels are generated.

[0246] Therefore, by supplying oxygen to the oxide semiconductor film 403 that has been subjected to the dehydration or dehydrogenation treatment, By supplying oxygen to the oxide semiconductor film 403, oxygen vacancies in the film are filled. By using the oxide semiconductor film in a transistor, the oxide semiconductor film can be effectively used. Reduces the variation in threshold voltage Vth of transistors and the threshold voltage shift ΔVth In addition, the threshold voltage can be shifted in the positive direction to make the transistor normally It can also be turned off.

[0247] In this embodiment, oxygen is introduced into the oxide semiconductor film 403 as an example. The introduction of the insulating film 402, the gate insulating film 442, and the insulating This may be applied to the film 436, the film 407 containing a metal element, the insulating film 416, the insulating film 427, and the like. The gate insulating film 402, the gate insulating film 442, and the insulating film 436 in contact with the oxide semiconductor film 403 Oxygen is introduced into the metal element-containing film 407, the insulating film 416, and the insulating film 427 to make them oxygen-excessive. This enables oxygen to be supplied to the oxide semiconductor film 403.

[0248] The oxygen introduction method includes ion implantation, ion doping, plasma immersion An implantation method, a plasma treatment, or the like can be used.

[0249] In the step of introducing oxygen into the oxide semiconductor film 403, The dopant may be introduced directly into the oxide semiconductor film or may be introduced through other films such as a gate insulating film or an insulating film. When oxygen is introduced through another film, it is possible to use an ion implantation method or an ion doping method. The plasma immersion ion implantation method, etc. can be used. In the case of directly introducing a hydrogen atom into an exposed oxide semiconductor film, plasma treatment or the like can be used. can.

[0250] The introduction of oxygen into the oxide semiconductor film 403 is performed by the transistors 440, 445, 420a, and 42 In the cases of 400b and 450, the source electrode layer 405 is formed on the exposed oxide semiconductor film 403. a) After forming the drain electrode layer 405b, the gate insulating film 442 or the gate insulating film 402 is formed. After that, the gate electrode layer 401 is formed, the film 417 containing the metal element is formed, and then the film 40 containing the metal element is formed. 7, after the insulating film 416, or after the planarization insulating film 415 is formed.

[0251] In addition, oxygen is introduced into the oxide semiconductor film 403 in the transistor 410. After the insulating film 427 is formed on the oxide semiconductor film 403, the film 417 containing a metal element is formed. After forming the film 407 containing a metal element, the source electrode layer 405a and the drain electrode layer 405b are formed. This can be performed after the formation of the insulating film 416 or after the formation of the insulating film 416 .

[0252] In this manner, oxygen is introduced into the oxide semiconductor film after the dehydration or dehydrogenation treatment. In addition, the oxide semiconductor that has been subjected to the above-mentioned dehydration or dehydrogenation treatment may be used. Oxygen may be introduced into the membrane multiple times.

[0253] For example, the oxygen concentration in the oxide semiconductor film 403 introduced by the oxygen introduction step is set to 1 ×10 18 atoms / cm 3 5×10 or more 21 atoms / cm 3 It is preferable to It is.

[0254] In an oxide semiconductor, oxygen is one of the main components. The oxygen concentration in the conductive film was measured by SIMS (Secondary Ion Mass Spectroscopy) It is difficult to estimate the thickness of the oxide semiconductor precisely using methods such as rheometry. It can be said that it is difficult to determine whether or not oxygen has been intentionally added to the conductive film.

[0255] By the way, oxygen has 17 O and 18There are isotopes such as O and their existence in nature The ratios of these atoms in the oxygen system are known to be approximately 0.037% and 0.204% of all oxygen atoms, respectively. In other words, the concentrations of these isotopes in the oxide semiconductor film can be measured by a method such as SIMS. Therefore, it is possible to estimate the oxide semiconductor concentration by measuring these concentrations. It may be possible to estimate the oxygen concentration in the conductive film more accurately. By measuring the concentration of oxygen, it may be possible to determine whether oxygen has been intentionally added to the oxide semiconductor film. stomach.

[0256] In addition, in the case of directly introducing oxygen into the oxide semiconductor film as in this embodiment, The insulating film that comes into contact with the body membrane does not necessarily have to be a film that contains a lot of oxygen. The insulating film in contact with the oxide semiconductor film is a film containing a large amount of oxygen, and oxygen is directly introduced into the oxide semiconductor film. In this case, multiple oxygen supply methods may be used.

[0257] In order to prevent the introduced oxygen from being released from the oxide semiconductor film again, and to prevent hydrogen, water, etc. from being introduced In order to prevent impurities contained in the oxide semiconductor film from being recontaminated into the oxide semiconductor film, A film with a high blocking effect against impurities is used as an insulating film covering the oxide semiconductor film. For example, it is preferable to provide a barrier against both impurities such as hydrogen and moisture, and oxygen. It is advisable to use an aluminum oxide film or the like which has a high blocking effect.

[0258] After oxygen is introduced into the oxide semiconductor film, a heating step is preferably performed.

[0259] Oxygen is introduced into an oxide semiconductor film that has been subjected to dehydration or dehydrogenation treatment to supply oxygen into the film. By this, the oxide semiconductor film can be highly purified and made electrically i-type (intrinsic). Cut.

[0260] A transistor having an oxide semiconductor film that is highly purified and electrically i-type (intrinsic) is Fluctuations in electrical characteristics are suppressed, and the device is electrically stable.

[0261] As described above, a semiconductor device using an oxide semiconductor and having stable electrical characteristics is provided. Therefore, a highly reliable semiconductor device can be provided.

[0262] This embodiment mode can be implemented in appropriate combination with other embodiment modes.

[0263] (Embodiment 7) A semiconductor device having a display function using the transistor as an example described in any one of Embodiments 1 to 6. A semiconductor device (also called a display device) can be manufactured. A system-on-panel is formed by forming part or the whole circuit on the same substrate as the pixel section. It is possible.

[0264] In FIG. 9A, a pixel portion 4002 provided on a first substrate 4001 is surrounded by a A sealant 4005 is provided and the semiconductor device is sealed with a second substrate 4006. In A), a region surrounded by a sealant 4005 on a first substrate 4001 and The semiconductor layer is formed of a single crystal semiconductor film or a polycrystalline semiconductor film on a separately prepared substrate in a different region. A scanning line driver circuit 4004 and a signal line driver circuit 4003 are also mounted. A signal line driver circuit 4003 and a scanning line driver circuit 4004 or a signal line driver circuit 4005 are provided to the pixel portion 4002. Various signals and potentials are transmitted through the FPC (Flexible Printed Circuit). )Powered by 4018a and 4018b.

[0265] In FIG. 9B and FIG. 9C, a pixel portion 4002 is provided on a first substrate 4001, and a scanning A sealant 4005 is provided so as to surround the line driver circuit 4004. A second substrate 4006 is provided on the substrate 4002 and the scanning line driver circuit 4004. The pixel portion 4002 and the scanning line driver circuit 4004 are formed by a first substrate 4001 and a sealant 4002. The display element is sealed by the second substrate 4005 and the second substrate 4006. In C), the area surrounded by the sealant 4005 on the first substrate 4001 and The semiconductor layer is formed of a single crystal semiconductor film or a polycrystalline semiconductor film on a separately prepared substrate in a different region. In FIG. 9B and FIG. 9C, a signal line driver circuit 4003 is mounted. A signal line driver circuit 4003 and a scanning line driver circuit 4004 or a signal line driver circuit 4005 are provided to the pixel portion 4002. The various signals and potentials are supplied from the FPC4018.

[0266] In addition, in FIG. 9B and FIG. 9C, a signal line driver circuit 4003 is formed separately, and the first substrate 4 001, but the present invention is not limited to this configuration. Alternatively, only a part of the signal line driver circuit or a part of the scanning line driver circuit may be formed and mounted. It may be formed separately and mounted.

[0267] The method of connecting the separately formed drive circuit is not particularly limited, and may be any of the following: ip On Glass) method, wire bonding method, or TAB (Tape A A method such as a utomated bonding method can be used. This is an example in which a signal line driver circuit 4003 and a scanning line driver circuit 4004 are implemented by the OG method. FIG. 9B shows an example in which a signal line driver circuit 4003 is mounted by the COG method, and FIG. 4003) is an example in which a signal line driver circuit 4003 is mounted by the TAB method.

[0268] The display device includes a panel in which a display element is sealed, and a controller for the panel. and modules in which ICs, etc., including the above, are mounted.

[0269] In this specification, the term "display device" refers to an image display device, a display device, or an optical device. Also refers to connectors, such as FPC or TAB tape. Modules with TCP attached, TAB tape or TCP with printed wiring board attached The IC (integrated circuit) is directly mounted on the installed module or display element using the COG method. The display device includes all of the modules installed in the display device.

[0270] The pixel portion and the scanning line driver circuit provided on the first substrate have a plurality of transistors. The transistor described in any one of Embodiments 1 to 6 can be used. do.

[0271] Examples of display elements provided in the display device include liquid crystal elements (also called liquid crystal display elements), light-emitting elements ( The light-emitting element can be used as a light-emitting display element. This category includes elements whose brightness can be controlled, specifically inorganic EL (Electroluminescent) Luminescence, organic electroluminescence, etc. Also, electronic ink, etc. A display medium whose contrast changes depending on use can also be applied.

[0272] One mode of a semiconductor device will be described with reference to FIGS. 9 and 10. FIG. 10 shows a semiconductor device according to the embodiment of the present invention. This corresponds to a cross-sectional view at MN.

[0273] As shown in FIGS. 9 and 10, the semiconductor device has a connection terminal electrode 4015 and a terminal electrode 4016. The connection terminal electrode 4015 and the terminal electrode 4016 are connected to the terminals of the FPC 4018. The electrode is electrically connected to the anisotropic conductive film 4019 .

[0274] The connection terminal electrode 4015 is formed from the same conductive film as the first electrode layer 4030. 016 is a transistor having the same conductor as the source and drain electrode layers of the transistors 4010 and 4011. It is formed of a conductive film.

[0275] A pixel portion 4002 and a scanning line driver circuit 4004 are provided on a first substrate 4001. 9 and 10, the transistors included in the pixel portion 4002 are 4004 and a transistor 4011 included in the scanning line driver circuit 4004. In FIG. 10A, an insulating film 4020 is provided over the transistors 4010 and 4011. 10B, an insulating film 4021 is further provided. Reference numeral 23 denotes an insulating film that functions as a base film.

[0276] The transistor 4010 and the transistor 4011 may be any of the transistors according to Embodiments 1 to 6. In this embodiment, the transistor shown in Embodiment 1 can be used. 4 shows an example in which a transistor having a structure similar to that of the transistor 440 is used.

[0277] The transistor 4010 and the transistor 4011 have a channel formation region in the channel length direction. The transistor has an oxide semiconductor film including a low-resistance region sandwiched therebetween. The on-characteristics (e.g., on-current and field effect transition) of the transistor 4010 and the transistor 4011 are It has a high mobility, allowing for high-speed operation and high-speed response. It can also be miniaturized.

[0278] Therefore, the semiconductor device according to the present embodiment shown in FIGS. 9 and 10 is a high-performance and highly reliable semiconductor device. A conductor device can be provided.

[0279] The transistor 4010 provided in the pixel portion 4002 is electrically connected to a display element. The display element is not particularly limited as long as it can display an image. can be used.

[0280] FIG. 10A shows an example of a liquid crystal display device using a liquid crystal element as a display element. In the liquid crystal element 4013, which is a display element, a first electrode layer 4030 and a second electrode layer 4040 are 031 and a liquid crystal layer 4008. The liquid crystal layer 4008 is sandwiched between the alignment films 4003 and 4008. The second electrode layer 4031 is provided with insulating films 4032 and 4033 that function as a second The first electrode layer 4030 and the second electrode layer 4031 are disposed on the substrate 4006 side. The structure is such that the layers are stacked via 008.

[0281] Also, 4035 is a columnar spacer obtained by selectively etching the insulating film. It is provided to control the thickness (cell gap) of the liquid crystal layer 4008. A pacer may be used.

[0282] When liquid crystal elements are used as display elements, thermotropic liquid crystal, low molecular weight liquid crystal, high molecular weight liquid crystal, etc. For example, a liquid crystal, a polymer-dispersed liquid crystal, a ferroelectric liquid crystal, an antiferroelectric liquid crystal, etc. can be used. Depending on the conditions, the liquid crystal material (liquid crystal composition) can be in a cholesteric phase, a smectic phase, or a cubic phase. The phases shown are biaxial, chiral nematic, isotropic, etc.

[0283] In addition, the liquid crystal layer 4008 may be made of a liquid crystal composition that exhibits a blue phase without using an alignment film. The blue phase is one of the liquid crystal phases. When the temperature of a cholesteric liquid crystal is increased, the cholesteric The blue phase is a phase that appears just before the transition from the black phase to the isotropic phase. The blue phase can be expressed by using a liquid crystal composition in which the above-mentioned liquid crystals are mixed. In order to widen the range of the blue phase, a polymerizable monomer and a polymerization initiator are added to the liquid crystal composition that exhibits the blue phase. The liquid crystal layer can be formed by adding a polymer stabilizer. The liquid crystal composition that exhibits this phase has a short response time and is optically isotropic, so no alignment treatment is required. The viewing angle dependence is small. Also, since there is no need to provide an alignment film, rubbing treatment is not required. Therefore, electrostatic damage caused by the rubbing process can be prevented, and the manufacturing process This reduces defects and damage to the liquid crystal display device during the manufacturing process. A transistor including an oxide semiconductor film can be prevented from being affected by static electricity. This can cause the electrical characteristics of the transistor to vary significantly and deviate from the design range. A liquid crystal display device having a transistor including an oxide semiconductor film and capable of exhibiting a blue phase can be provided. It is more effective to use a crystalline composition.

[0284] The specific resistance of the liquid crystal material is 1×10 9 Ω cm or more, preferably 1×10 11 Ω cm or more, and more preferably 1×10 12 In addition, this specification The resistivity values ​​stated herein are those measured at 20°C.

[0285] The size of the storage capacitor provided in the liquid crystal display device is determined by the lead of the transistor arranged in the pixel portion. The capacitance is set so that the charge can be held for a predetermined period of time, taking into account factors such as the capacitance of the capacitor. The size of the oxide film may be set in consideration of the off-state current of the transistor. By using a transistor having a semiconductor film, the liquid crystal capacitance of each pixel is It is sufficient to provide a storage volume having a size of 1 / 3 or less, preferably 1 / 5 or less, of the capacity of the do.

[0286] The transistor including the oxide semiconductor film disclosed in this specification has a current value in an off state ( Therefore, the retention time of electric signals such as image signals can be extended. When the power is on, the write interval can be set longer. This reduces the frequency of CPU operation, thereby reducing power consumption.

[0287] In addition, a transistor including an oxide semiconductor film disclosed in this specification has high field-effect mobility. For example, a transistor capable of such high-speed operation is By using this transistor in a liquid crystal display device, the switching transistor in the pixel section and the The driver transistors used for the other circuits can be formed on the same substrate. Since it is not necessary to use a semiconductor device formed of a silicon wafer or the like as a driving circuit, Therefore, the number of parts in the semiconductor device can be reduced. By using a transistor capable of achieving this, a high-quality image can be provided. It is also possible to achieve high reliability as a semiconductor device.

[0288] There are two types of LCD displays: TN (Twisted Nematic) and IPS (In-P lane-Switching) mode, FFS (Fringe Field Switching) mode ching) mode, ASM(Axially Symmetric aligned) Micro-cell mode, OCB (Optical Compensated B) irefringence mode, FLC (Ferroelectric Liqui d Crystal) mode, AFLC (AntiFerroelectric Liq. uid Crystal) mode can be used.

[0289] In addition, normally black type liquid crystal display devices, such as those using a vertical alignment (VA) mode, The liquid crystal display device may be a transmission type liquid crystal display device. There are several types of vertical alignment modes, including: For example, MVA (Multi-Domain Vertical Alignment) mode, PVA (Patterned Vertical Alignment) mode , ASV (Advanced Super View) mode, etc. can be used. The present invention can also be applied to VA type liquid crystal display devices. VA type liquid crystal display devices are: It is a type of method for controlling the arrangement of liquid crystal molecules in a liquid crystal display panel. VA type liquid crystal display devices are When no voltage is applied, the liquid crystal molecules are oriented vertically to the panel surface. In addition, a pixel is divided into several regions (subpixels), each of which is oriented in a different direction. This is called multi-domain or multi-domain design, which is designed to defeat molecules in a complex manner. The following method can be used.

[0290] In addition, in display devices, they are used as black matrices (light-shielding layers), polarizing members, phase difference members, reflectors, etc. Optical members (optical substrates) such as a prevention member are provided as appropriate. For example, a polarizing substrate and a retardation substrate Alternatively, a backlight or a sidelight may be used as the light source. It's fine.

[0291] The display method in the pixel section uses the progressive method, interlace method, etc. In addition, the color elements controlled by pixels when displaying colors are RGB (R is The color is not limited to the three colors red, green, and blue. For example, RGBW (W stands for white). , or RGB plus one or more colors such as yellow, cyan, magenta, etc. The size of the display area may be different for each dot of the color element. The present invention is not limited to color display devices, but is applicable to monochrome display devices. It is also possible.

[0292] In addition, a light-emitting element that utilizes electroluminescence is used as a display element included in the display device. The light-emitting element utilizing electroluminescence is made of a light-emitting material They are classified according to whether they are organic or inorganic compounds. Generally, the former are called organic E The latter is called an inorganic EL element.

[0293] In an organic EL element, electrons and holes are released from a pair of electrodes by applying a voltage to the light-emitting element. are injected into layers containing light-emitting organic compounds, causing a current to flow. The rears (electrons and holes) recombine to form an excited state in the light-emitting organic compound. When the excited state returns to the ground state, light is emitted. Such a light-emitting element is called a current-excitation type light-emitting element.

[0294] Inorganic EL elements are divided into dispersion-type inorganic EL elements and thin-film-type inorganic EL elements according to their element structure. Dispersion-type inorganic EL elements have a light-emitting layer in which particles of a light-emitting material are dispersed in a binder. The emission mechanism is a donor-acceptor reaction that utilizes the donor and acceptor levels. Thin-film inorganic EL elements are made by sandwiching a light-emitting layer between dielectric layers. The structure is sandwiched between electrodes, and the light emission mechanism utilizes the inner shell electron transition of metal ions. In this example, the light-emitting element is an organic EL element. do.

[0295] In order to extract light emitted from the light-emitting element, at least one of the pair of electrodes needs to be light-transmitting. Then, a transistor and a light emitting element are formed on the substrate, and light is emitted from the surface opposite the substrate. The top emission is from the top surface, the bottom emission is from the surface on the substrate side, and the bottom emission is from the surface on the substrate side and the opposite side to the substrate. There are light emitting devices with a double-sided emission structure that emits light from both sides, and light emitting devices of any emission structure can be used. It is possible.

[0296] FIG. 10B shows an example of a light-emitting device using a light-emitting element as a display element. The photoelement 4513 is electrically connected to the transistor 4010 provided in the pixel portion 4002. The light-emitting element 4513 includes a first electrode layer 4030, an electroluminescent layer 4511, The second electrode layer 4031 has a stacked structure, but is not limited to the structure shown. The configuration of the light emitting element 4513 can be changed appropriately according to the direction of the light extracted from the light emitting element 4513. Cut.

[0297] The partition 4510 is formed using an organic insulating material or an inorganic insulating material, particularly a photosensitive resin. An opening is formed on the first electrode layer 4030 using a material, and the sidewall of the opening is a continuous curved It is preferable to form the inclined surface so that the inclined surface is formed with a certain rate.

[0298] The electroluminescent layer 4511 may be composed of a single layer or may be composed of a plurality of layers stacked together. It doesn't matter whether it is done or not.

[0299] In order to prevent oxygen, hydrogen, moisture, carbon dioxide, and the like from entering the light-emitting element 4513, the second electrode layer A protective film may be formed on the insulating film 4031 and the partition wall 4510. The protective film may be made of silicon nitride. A silicon nitride oxide film, a DLC film, etc. can be formed on the first substrate 400. The space sealed by the first substrate 4001, the second substrate 4006, and the sealant 4005 is filled with a filler 45. 14 is provided and sealed. In this way, it is highly airtight and degassing is possible to prevent exposure to the outside air. Protective films with low damage (laminated films, UV-cured resin films, etc.) and covering materials It is preferable to package (enclose) the

[0300] Filler 4514 can be inert gas such as nitrogen or argon, or ultraviolet curing resin or Thermosetting resin can be used, and PVC (polyvinyl chloride), acrylic, polyimide, etc. Mido, epoxy resin, silicone resin, PVB (Polyvinyl Butyral) or EVA (Elastomer) For example, nitrogen may be used as a filler. stomach.

[0301] If necessary, a polarizing plate or a circular polarizing plate (including an elliptical polarizing plate) may be provided on the light-emitting surface of the light-emitting element. Optical films such as retardation plates (λ / 4 plates, λ / 2 plates) and color filters may be provided as appropriate. In addition, the polarizing plate or the circular polarizing plate may be provided with an anti-reflection film. Anti-glare treatment can be applied to diffuse reflected light and reduce glare.

[0302] It is also possible to provide electronic paper that drives electronic ink as a display device. Electronic paper is also called an electrophoretic display (electrophoretic display) and is a paper-based display. It is possible to make a display that is as easy to read as a regular display, consumes less power than other displays, and is thinner and lighter in size. This has the advantage that

[0303] The electrophoretic display device may have various forms, but it has a first particle having a positive charge and A microcapsule containing a negatively charged second particle and a negatively charged second particle is introduced into a solvent or solute. By applying an electric field to the microcapsules, The particles in the cell are moved in opposite directions to each other, and only the color of the particles that have gathered on one side is displayed. In addition, the first particles or the second particles contain a dye, and they do not migrate in the absence of an electric field. The color of the first particle and the color of the second particle are different (including colorless). )

[0304] In this way, the electrophoretic display device is a so-called This is a display that utilizes the dielectrophoretic effect.

[0305] The microcapsules dispersed in a solvent are called electronic ink. The electronic ink can be printed on surfaces such as glass, plastic, fabric, and paper. A color display is also possible by using a color filter or particles having a pigment.

[0306] The first particles and the second particles in the microcapsules are made of a conductive material, an insulating material, Semiconductor materials, magnetic materials, liquid crystal materials, ferroelectric materials, electroluminescent materials, A material selected from the group consisting of magnetochromic material, magnetophoretic material, and a composite material thereof. Just use it.

[0307] In addition, display devices using the twist ball display method can also be used as electronic paper. The twist ball display method uses black and white spherical particles as the display element. The insulating layer is disposed between a first electrode layer and a second electrode layer, and the first electrode layer and the second electrode layer are electrically connected to each other. This is a method of displaying information by controlling the orientation of spherical particles by applying a potential difference to the electrode layer. be.

[0308] In addition, in FIG. 9 and FIG. 10, the first substrate 4001 and the second substrate 4006 are made of Ga. In addition to the glass substrate, a flexible substrate can also be used. For example, a light-transmitting plastic substrate can be used. As for plastic, FRP (Fibreglass) is suitable. SS-Reinforced Plastics) plate, PVF (Polyvinyl Fluoride) ) film, polyester film or acrylic resin film can be used. If light transmission is not required, metal substrates such as aluminum and stainless steel (metal filters) can be used. For example, aluminum foil may be covered with a PVF film or polyester film. It is also possible to use a sheet sandwiched between films.

[0309] In this embodiment, the insulating film 4020 is a film containing a metal element, which is converted into a metal oxide film by heat treatment. An aluminum oxide film is used as the insulating film.

[0310] The aluminum oxide film provided as the insulating film 4020 over the oxide semiconductor film is resistant to hydrogen, moisture, and the like. The membrane has a high blocking effect against both impurities such as urea and oxygen. stomach.

[0311] Therefore, the aluminum oxide film is free from hydrogen, which is a variable factor during and after the manufacturing process. The intrusion of impurities such as moisture into the oxide semiconductor film and the intrusion of the oxide semiconductor into the main component material The oxide semiconductor film functions as a protective film for preventing release of oxygen from the oxide semiconductor film.

[0312] The insulating film 4021 functioning as a planarizing insulating film is made of acrylic, polyimide, or benzosilane. Heat-resistant organic materials such as clobutene resins, polyamides, and epoxies can be used. In addition to the above organic materials, low-k materials and siloxane resins are also available. , PSG (phosphorus glass), BPSG (borophosphorus glass), etc. can be used. The insulating film may be formed by stacking a plurality of insulating films made of these materials.

[0313] The method for forming the insulating film 4021 is not particularly limited. Depending on the material, it may be formed by sputtering, S OG method, spin coating, dip, spray coating, droplet ejection method (inkjet method, etc.), Printing method (screen printing, offset printing, etc.), doctor knife, roll coater, car A ten coater, a knife coater, or the like can be used.

[0314] A display device transmits light from a light source or a display element to display an image. All thin films such as the substrate, insulating film, and conductive film installed in the part are designed to be transparent to light in the visible light wavelength range. It shall be translucent.

[0315] A first electrode layer and a second electrode layer (a pixel electrode layer, a common electrode layer, a pair of electrodes) for applying a voltage to the display element In the case of the electrode layer, the direction of the light to be extracted, the location of the electrode layer, and The light transmitting property or the light reflecting property can be selected depending on the pattern structure of the electrode layer.

[0316] The first electrode layer 4030 and the second electrode layer 4031 are made of indium oxide containing tungsten oxide. oxide, indium zinc oxide with tungsten oxide, indium oxide with titanium oxide Indium tin oxide containing titanium oxide, indium tin oxide, indium zinc oxide , indium tin oxide doped with silicon oxide, graphene, and other light-transmitting conductive materials Fees can be used.

[0317] The first electrode layer 4030 and the second electrode layer 4031 are made of tungsten (W) or molybdenum. (Mo), zirconium (Zr), hafnium (Hf), vanadium (V), niobium (N b) Tantalum (Ta), Chromium (Cr), Cobalt (Co), Nickel (Ni), Titanium Metals such as titanium (Ti), platinum (Pt), aluminum (Al), copper (Cu), and silver (Ag), It can be formed by using one or more of the following metals: Cut.

[0318] The first electrode layer 4030 and the second electrode layer 4031 are made of a conductive polymer (conductive polymer). The conductive polymer may be a conductive composition containing a conductive polymer. For example, a so-called π-electron conjugated conductive polymer can be used. or its derivatives, polypyrrole or its derivatives, polythiophene or its derivatives, or a copolymer of two or more of aniline, pyrrole and thiophene or a derivative thereof Conductors, etc.

[0319] In addition, since transistors are easily damaged by static electricity, etc., a protection circuit for protecting the driver circuit is also required. It is preferable that the protection circuit is configured using a non-linear element.

[0320] As described above, by using the transistor described in any of Embodiments 1 to 6, various It is possible to provide semiconductor devices having various functions.

[0321] (Embodiment 8) The transistor shown in any one of the first to sixth embodiments is used to read information on an object. Therefore, a semiconductor device having an image sensor function for detecting a reflected light can be manufactured.

[0322] FIG. 11A shows an example of a semiconductor device having an image sensor function. FIG. 11B is a cross-sectional view showing a part of the photosensor. .

[0323] The photodiode 602 has one electrode connected to a photodiode reset signal line 658 and the other One electrode of the transistor 640 is electrically connected to the gate of the transistor 640. One of the source or drain is connected to the photosensor reference signal line 672, and the other of the source or drain is connected to the photosensor reference signal line 672. The other terminal is electrically connected to one of the source and drain terminals of the transistor 656. The transistor 656 has a gate connected to a gate signal line 659 and a source or drain connected to a photodiode. The sensor output signal line 671 is electrically connected to the sensor output signal line 671.

[0324] Note that in the circuit diagrams in this specification, a transistor including an oxide semiconductor film is not clearly shown. To make it easy to understand, the symbol for a transistor using an oxide semiconductor film is marked with “OS.” In FIG. 11A, a transistor 640 and a transistor 656 are the same as those in the first embodiment. The transistors described in any of the above to 6 can be used, and are transistors including an oxide semiconductor film. In this embodiment, a transistor having a structure similar to that of the transistor 440 described in Embodiment 1 is used. An example of applying a transistor is shown below.

[0325] FIG. 11B shows a photodiode 602 and a transistor 640 in the photosensor. 6 is a cross-sectional view of the substrate 601 (TFT substrate) having an insulating surface. A photodiode 602 and a transistor 640 are provided to function as a photodiode. A substrate 613 is provided on the board 602 and the transistor 640 using an adhesive layer 608. There are.

[0326] An insulating film 631, an interlayer insulating film 633, and an interlayer insulating film 634 are provided on the transistor 640. The photodiode 602 is provided on the interlayer insulating film 633. 3 and an electrode layer 642 provided on an interlayer insulating film 634. , a first semiconductor film 606a, a second semiconductor film 606b, and a third semiconductor film 606c are formed in this order from the interlayer insulating film 633 side. It has a structure in which a semiconductor film 606c is laminated.

[0327] The electrode layer 641 is electrically connected to a conductive layer 643 formed on the interlayer insulating film 634. 642 is electrically connected to the conductive layer 645 via the electrode layer 641. The conductive layer 645 is The photodiode 602 is electrically connected to the gate electrode layer of the transistor 640. It is electrically connected to the transistor 640 .

[0328] Here, the first semiconductor film 606a is a semiconductor film having a p-type conductivity, and the second semiconductor film A high resistance semiconductor film (I-type semiconductor film) is used as 606b, and an n-type semiconductor film is used as the third semiconductor film 606c. A pin-type photodiode in which semiconductor films having different conductivity types are stacked is shown as an example.

[0329] The first semiconductor film 606a is a p-type semiconductor film, and is an amorphous semiconductor film containing an impurity element that imparts p-type. The first semiconductor film 606a can be formed of a group 13 silicon film. Using semiconductor material gas containing impurity elements (e.g. boron (B)), plasma CVD method Silane (SiH4) can be used as the semiconductor material gas. i2H6, SiH2Cl2, SiHCl3, SiCl4, SiF4, etc. may also be used. In addition, after forming an amorphous silicon film that does not contain impurity elements, the film is then subjected to diffusion or ion implantation. Impurity elements may be introduced into the amorphous silicon film by using an ion implantation method or the like. It is preferable to diffuse the impurity element by heating or the like after introducing the impurity element. In this case, the method for forming the amorphous silicon film includes the LPCVD method, the vapor phase growth method, Alternatively, a sputtering method or the like may be used. It is preferable to form the film so that the thickness is 0 nm or less.

[0330] The second semiconductor film 606b is an I-type semiconductor film (intrinsic semiconductor film) and is made of amorphous silicon. The second semiconductor film 606b is formed by amorphous silicon using a semiconductor material gas. A fast silicon film is formed by plasma CVD. The semiconductor material gas is silane. (SiH4) can be used. Alternatively, Si2H6, SiH2Cl2, SiHCl3, S iCl4, SiF4, etc. may be used. The second semiconductor film 606b is formed by LPCVD. The second semiconductor film 606b may be formed by vapor deposition, sputtering, or the like. It is preferable to form the film so that the thickness is 00 nm or more and 1000 nm or less.

[0331] The third semiconductor film 606c is an n-type semiconductor film, and is an amorphous film containing an impurity element that imparts n-type conductivity. The third semiconductor film 606c is formed of a fast silicon film. It is formed by the plasma CVD method using a semiconductor material gas containing silicon (e.g. phosphorus (P)). Silane (SiH4) can be used as the semiconductor material gas. SiH2Cl2, SiHCl3, SiCl4, SiF4, etc. may also be used. After forming an amorphous silicon film that does not contain elements, the material is then doped with silicon using diffusion or ion implantation. An impurity element may be introduced into the amorphous silicon film by ion implantation or the like. After the element is introduced, the impurity element may be diffused by heating or the like. The method for forming the amorphous silicon film includes the LPCVD method, the vapor phase growth method, or the sputtering method. The thickness of the third semiconductor film 606c is 20 nm or more and 200 nm or less. It is preferable to form it so that the bottom is facing downward.

[0332] The first semiconductor film 606a, the second semiconductor film 606b, and the third semiconductor film 606c are Instead of an amorphous semiconductor, a polycrystalline semiconductor may be used. Semi Amorphous Semiconductor (SAS )) may be used.

[0333] Microcrystalline semiconductors are metastable, intermediate between amorphous and single crystal, when considering the Gibbs free energy. In other words, a semiconductor that has a third state that is stable in terms of free energy The crystals are of a short-range order and have lattice distortion. Microcrystalline silicon, a typical example of a microcrystalline semiconductor, is a type of Raman The spectrum shows single crystal silicon at 520 cm -1 It is shifted to the lower wavenumber side. That is, 520 cm, which indicates single crystal silicon. -1 and 480 cm, which indicates amorphous silicon. - 1 The Raman spectrum of microcrystalline silicon has a peak between the two. Contains at least 1 atomic % or more of hydrogen or halogen to terminate the ring bonds. In addition, it contains rare gas elements such as helium, argon, krypton, and neon. By increasing the thickness of the semiconductor film, the lattice distortion is further promoted, and the stability is increased, resulting in a good microcrystalline semiconductor film. .

[0334] This microcrystalline semiconductor film is formed by a high-frequency plasma CVD method with a frequency of several tens to several hundreds of MHz. Alternatively, it can be formed by a microwave plasma CVD apparatus with a frequency of 1 GHz or more. Representative examples include SiH4, Si2H6, SiH2Cl2, SiHCl3, SiCl4, and S It can be formed by diluting silicon-containing compounds such as iF4 with hydrogen. In addition to compounds containing hydrogen (e.g. silicon hydride) and hydrogen, helium, argon, krypton, neon forming a microcrystalline semiconductor film by diluting the semiconductor film with one or more rare gas elements selected from the group consisting of fluorine and fluorine; In these cases, the flow rate ratio of hydrogen to the compound containing silicon (e.g., silicon hydride) is 5 times or more and 200 times or less, preferably 50 times or more and 150 times or less, and more preferably 100 times Furthermore, in the gas containing silicon, carbide gases such as CH4, C2H6, GeH 4. Germanium gas such as GeF4, F2, etc. may be mixed in.

[0335] In addition, the mobility of holes generated by the photoelectric effect is smaller than that of electrons, so Photodiodes exhibit better characteristics when the p-type semiconductor film side is used as the light receiving surface. From the surface of the substrate 601 on which the in-type photodiode is formed, the photodiode 602 This example shows how the light received by the semiconductor film is converted into an electrical signal. Since light from the semiconductor film side having the pattern becomes disturbance light, the electrode layer uses a conductive film with light blocking properties. In addition, the n-type semiconductor film side can be used as the light receiving surface.

[0336] The interlayer insulating film 633 and the interlayer insulating film 634 are made of an insulating material. , sputtering method, plasma CVD method, SOG method, spin coating, dip, spray Coating, droplet ejection method (inkjet method, etc.), printing method (screen printing, offset printing, etc.) ), doctor knife, roll coater, curtain coater, knife coater, etc. It can be achieved.

[0337] In this embodiment, the insulating film 631 is a film containing a metal element, which is converted into a metal oxide film by heat treatment. The insulating film 631 is formed by sputtering or plasma. The film can be formed by a chemical vapor deposition (CVD) method.

[0338] The aluminum oxide film provided as the insulating film 631 over the oxide semiconductor film is resistant to hydrogen, moisture, and the like. High blocking effect that prevents impurities and oxygen from passing through the membrane .

[0339] Therefore, the aluminum oxide film is free from hydrogen, which is a variable factor during and after the manufacturing process. The intrusion of impurities such as moisture into the oxide semiconductor film and the intrusion of the oxide semiconductor into the main component material The oxide semiconductor film functions as a protective film for preventing release of oxygen from the oxide semiconductor film.

[0340] The interlayer insulating films 633 and 634 function as planarizing insulating films to reduce surface irregularities. The interlayer insulating films 633 and 634 are preferably made of, for example, polyimide or acrylic. Heat-resistant organic resins such as resins, benzocyclobutene-based resins, polyamides, and epoxy resins In addition to the above organic insulating materials, low-dielectric materials can be used. k materials), siloxane resin, PSG (phosphorus glass), BPSG (borophosphorus glass), etc. A single layer or a laminate of these can be used.

[0341] By detecting light 622 incident on the photodiode 602, information on the detected object is obtained. When reading the information of the detected object, a light source such as a backlight is used. It can be used.

[0342] As described above, the oxide semiconductor including the low resistance region sandwiching the channel formation region in the channel length direction is The transistor having the thin film has high on-characteristics (e.g., on-current and field effect mobility). This allows high-speed operation and high-speed response. Also, miniaturization can be achieved. By using the capacitor, a high-performance and highly reliable semiconductor device can be provided.

[0343] This embodiment mode can be implemented in appropriate combination with the configurations described in other embodiments. It is.

[0344] (Embodiment 9) The transistor shown in any one of the first to sixth embodiments is a transistor having a plurality of transistors stacked. The present invention can be suitably used for a semiconductor device having an integrated circuit on a semiconductor device. As an example of a semiconductor device, a storage medium (memory element) will be described.

[0345] In this embodiment, a first transistor formed on a single crystal semiconductor substrate A second transistor is formed using a semiconductor film above the transistor 140 via an insulating film. A semiconductor device including the transistor 162 is manufactured. The transistors exemplified in any one of the above items 1 to 6 can be suitably used for the transistor 162. In this embodiment, the transistor 162 is the transistor shown in Embodiment 1. 4 shows an example in which a transistor having a structure similar to that of transistor 440 is used.

[0346] The semiconductor materials and structures of the stacked transistors 140 and 162 may be the same. In this embodiment, a suitable circuit for a storage medium (memory element) is The following are examples in which transistors having the above materials and structures are used.

[0347] 12A and 12B are diagrams showing an example of the structure of a semiconductor device. FIG. 12A shows a cross section of the semiconductor device. 12(B) shows a plan view of the semiconductor device. This corresponds to the cross sections taken along lines C1-C2 and D1-D2 in FIG. 12(B). FIG. 12A shows an example of a circuit diagram in which the semiconductor device is used as a memory element. The semiconductor device shown in FIG. 12(B) has a transistor using a first semiconductor material in the lower part. The second semiconductor material is used as the second semiconductor material. In the embodiment, the first semiconductor material is a semiconductor material other than an oxide semiconductor, and the second semiconductor material is The oxide semiconductor is a semiconductor material other than the oxide semiconductor. Use of ruthenium, silicon germanium, silicon carbide, gallium arsenide, etc. In addition, organic semiconductor materials may be used. Transistors using such semiconductor materials can easily operate at high speed. The characteristics of transistors using solid semiconductors enable them to retain electric charge for long periods of time.

[0348] A method for manufacturing the semiconductor device in FIG. 12 will be described with reference to FIGS.

[0349] The transistor 140 is disposed on a substrate 185 that includes a semiconductor material (such as silicon). A channel forming region 116 is formed by arranging impurity layers 116 so as to sandwich the channel forming region 116. A region 120, a metal compound region 124 in contact with the impurity region 120, and a channel forming region 1 A gate insulating film 108 is provided on the gate insulating film 108. The electrode 110 is a ferroelectric material.

[0350] The substrate 185 containing the semiconductor material may be a single crystal semiconductor substrate such as silicon or silicon carbide, a multi-crystal The semiconductor substrates used are crystalline semiconductor substrates, compound semiconductor substrates such as silicon germanium, and SOI substrates. Generally, an "SOI substrate" is a substrate in which a silicon semiconductor film is provided on an insulating surface. In this specification, however, it refers to a substrate having a structure in which a material other than silicon is formed on an insulating surface. In other words, the term "SOI substrate" includes a semiconductor film having a structure in which a semiconductor film is provided. The film is not limited to a silicon semiconductor film. In addition, the SOI substrate may be made of an insulating material such as a glass substrate. The present invention also includes a configuration in which a semiconductor film is provided on a substrate via an insulating film.

[0351] The method for producing SOI substrates is to implant oxygen ions into a mirror-polished wafer and then heat it at high temperatures. By this, an oxide layer is formed at a certain depth from the surface, and the chips in the surface layer are removed. A method for eliminating microvoids formed by hydrogen ion irradiation and a method for forming microvoids by heat treatment. A method of cleaving a semiconductor substrate by using a long distance, or a method of growing a single crystal semiconductor film on an insulating surface by crystal growth For example, a method for forming a film may be used.

[0352] For example, ions are added from one surface of a single crystal semiconductor substrate to form a single crystal semiconductor substrate. A weakened layer is formed at a certain depth from the surface of the single crystal semiconductor substrate, and An insulating film is formed on one of the substrates. The single crystal semiconductor substrate and the element substrate are stacked with the insulating film between them. In the laminated state, a crack is generated in the weakened layer, and the single crystal semiconductor substrate is separated at the weakened layer. A heat treatment is performed to form a single crystal semiconductor film on the element substrate as a semiconductor film from the single crystal semiconductor substrate. The SOI substrate produced by the above method can also be used favorably.

[0353] An element isolation insulating layer 106 is provided on the substrate 185 so as to surround the transistor 140. In order to achieve high integration, the transistor 140 is It is preferable to have a structure that does not have a sidewall insulating layer that becomes a sidewall. When the characteristics of the gate electrode 140 are important, a side wall is provided on the side of the gate electrode 110. A wall insulating layer may be provided to provide impurity regions 120 including regions with different impurity concentrations.

[0354] The transistor 140 using a single crystal semiconductor substrate can operate at high speed. By using this transistor as a read transistor, data can be read at high speed. Two insulating films are formed to cover the transistor 140. As a process before forming the stator 162 and the capacitance element 164, the two insulating layers are subjected to CMP processing. Then, the planarized insulating film 128 and the insulating film 130 are formed, and at the same time, the upper surface of the gate electrode 110 is Expose.

[0355] The insulating film 128 and the insulating film 130 are typically a silicon oxide film, a silicon oxynitride film, or an oxide Aluminum film, aluminum oxynitride film, silicon nitride film, aluminum nitride film, nitride An inorganic insulating film such as a silicon oxide film or an aluminum nitride oxide film can be used. The film 128 and the insulating film 130 are formed by using a plasma CVD method, a sputtering method, or the like. It is possible.

[0356] In addition, organic materials such as polyimide, acrylic resin, and benzocyclobutene resin can be used. In addition to the above organic materials, low-dielectric constant materials (low-k materials) can also be used. When using organic materials, an insulating film can be formed by wet methods such as spin coating and printing. 128 and an insulating film 130 may be formed.

[0357] Note that the insulating film 130 that is in contact with the semiconductor film is a silicon oxide film.

[0358] In this embodiment, the insulating film 128 is a 50 nm-thick oxynitride film formed by a sputtering method. A silicon film is formed, and an oxide film having a thickness of 550 nm is formed as the insulating film 130 by a sputtering method. A silicon film is formed.

[0359] A semiconductor film is formed on the insulating film 130 that has been sufficiently planarized by CMP processing. In this study, we used an In-Ga-Zn oxide target for the semiconductor film and sputtered it. An oxide semiconductor film is formed.

[0360] Next, the oxide semiconductor film is selectively etched to form an island-shaped oxide semiconductor film 144. A source electrode or drain electrode 142 a is formed on the oxide semiconductor film 144. The rain electrode 142b is formed.

[0361] A gate insulating film 146 and a gate electrode layer 148 are formed over the oxide semiconductor film. 148 is formed by forming a conductive layer and then selectively etching the conductive layer. The gate insulating film 146 is formed by depositing an insulating film using the gate electrode layer 148 as a mask. It is formed by etching.

[0362] The gate insulating film 146 is formed by depositing an oxide film using a plasma CVD method, a sputtering method, or the like. Silicon film, silicon nitride film, silicon oxynitride film, silicon oxynitride film, aluminum oxide film Aluminum film, aluminum nitride film, aluminum oxynitride film, aluminum nitride oxide film, aluminum oxide film, A fluorine film or a gallium oxide film can be formed.

[0363] A gate electrode 110, a source electrode or a drain electrode 142a, a source electrode or a drain electrode A conductive layer that can be used for the electrode 142b can be formed by a PVD method such as a sputtering method. The conductive layer can be formed by a CVD method such as a plasma CVD method. The materials are selected from Al, Cr, Cu, Ta, Ti, Mo, and W, or the above-mentioned elements. The elements such as Mn, Mg, Zr, Be, Nd, and Sc can be used. Any one of these materials or a combination of two or more of these materials may be used.

[0364] The conductive layer may have a single layer structure or a laminated structure of two or more layers. A single layer structure of a titanium nitride film or titanium film, a single layer structure of an aluminum film containing silicon, Two-layer structure with titanium film laminated on titanium nitride film, two-layer structure with titanium film laminated on titanium nitride film Examples include a three-layer structure in which a titanium film, an aluminum film, and a titanium film are laminated. In addition, when the conductive layer has a single-layer structure of a titanium film or a titanium nitride film, the conductive layer has a tapered shape. A source electrode or drain electrode 142a and a source electrode or drain electrode 142 It has the advantage of being easy to process into b.

[0365] Next, an oxide semiconductor layer is formed on the oxide semiconductor layer 144, the gate insulating film 146, and the gate electrode layer 148. A film containing a metal element is formed in contact with a part of the conductive film 144. In this embodiment, An aluminum film is formed as the film containing elements.

[0366] The dopant (in this embodiment, boron) is introduced into the oxide semiconductor film 144 through the film containing a metal element. The oxide semiconductor film 144 containing a dopant and the film containing a metal element are in contact with each other. The heat treatment is performed in a state in which the metal element is transferred from the film containing the metal element to the oxide semiconductor film 144. A low-resistance region containing a dopant and a metal element is formed in the oxide semiconductor film 144. Therefore, a low resistance region containing a dopant and a metal element is formed on both sides of the channel forming region. A transistor 162 including the oxide semiconductor film 144 including the oxide semiconductor region can be manufactured.

[0367] The oxide semiconductor film 144 including the low-resistance region is provided between the channel formation region in the channel length direction. By this, the transistor 162 has on-characteristics (e.g., on-current and field-effect mobility) This enables high-speed operation and high-speed response.

[0368] The low resistance region can function as a source region or a drain region. By providing the low-resistance region, the electric field applied to the channel forming region formed between the low-resistance regions is reduced. In addition, in the low resistance region, the oxide semiconductor film 144 and the source electrode The source or drain electrode 142a and the source or drain electrode 142b are electrically connected to each other. By connecting the oxide semiconductor film 144 and the source electrode or drain electrode 142 a, and the contact resistance with the source electrode or the drain electrode 142b can be reduced. .

[0369] In addition, the metal element is introduced from the film containing the metal element by a heat treatment. The film containing the metal element is the film 150 containing the metal element. For example, the metal film used as the film containing the metal element is The metal element-containing film 150 becomes a metal oxide insulating film. In this embodiment, the film containing the metal element is aluminum. The aluminum oxide film is made of a metal. Since it is an oxide insulating film, it can be used as an insulating film.

[0370] An aluminum oxide film provided as a film 150 containing a metal element over the oxide semiconductor film 144 The blocking effect (blocking effect) is to prevent impurities such as hydrogen and moisture, as well as oxygen, from passing through the membrane. The effect is high.

[0371] Therefore, the aluminum oxide film is free from hydrogen, which is a variable factor during and after the manufacturing process. Impurities such as moisture may be mixed into the oxide semiconductor film 144, and the main components of the oxide semiconductor may be The oxide semiconductor film 144 functions as a protective film for preventing oxygen, which is a material, from being released from the oxide semiconductor film 144.

[0372] In addition, the film 150 containing the metal element is removed, or a separate film is laminated on the film 150 containing the metal element. An insulating film may be formed.

[0373] The insulating film is a silicon oxide film formed by plasma CVD or sputtering. Silicon nitride film, silicon oxynitride film, silicon oxynitride film, aluminum nitride film, oxide Aluminum film, aluminum oxynitride film, aluminum nitride oxide film, hafnium oxide film Alternatively, a gallium oxide film can be used.

[0374] On the film 150 including a metal element, a source electrode or a drain electrode 142a is overlapped. An electrode layer 153 is formed in the region.

[0375] Next, the insulating film 152 is formed over the transistor 162 and the film 150 containing a metal element. The insulating film 152 can be formed by using a sputtering method, a CVD method, or the like. , silicon oxide, silicon oxynitride, silicon nitride, hafnium oxide, aluminum oxide The insulating layer 10 can be formed using a material including an inorganic insulating material such as the above.

[0376] Next, a source electrode is formed on the gate insulating film 146, the film 150 containing a metal element, and the insulating film 152. Alternatively, an opening is formed that reaches the drain electrode 142b. The opening is formed without using a mask or the like. This is done by selective etching using a metal oxide or the like.

[0377] Thereafter, a wiring 156 that contacts the source electrode or drain electrode 142b is formed in the opening. 12 shows the connection point between the source electrode or drain electrode 142b and the wiring 156. is not shown.

[0378] The wiring 156 is formed by a PVD method such as a sputtering method, a plasma CVD method, or the like. After forming a conductive layer using the VD method, the conductive layer is etched to form The material of the conductive layer is selected from Al, Cr, Cu, Ta, Ti, Mo, and W. The elements mentioned above and alloys containing the elements mentioned above can be used. Mn, Mg, Z Any one of R, Be, Nd, and Sc, or a combination of two or more of these materials may be used. The details are similar to those of the source electrode or drain electrode 142a.

[0379] Through the above steps, the transistor 162 and the capacitor 164 are completed. The oxide semiconductor film 144 is highly purified and contains excess oxygen to compensate for oxygen vacancies. Therefore, the transistor 162 has suppressed fluctuations in electrical characteristics, and The capacitor 164 is electrically stable. Electrode layer 153.

[0380] If capacitance is not required, the capacitor 164 may not be provided.

[0381] FIG. 12C shows an example of a circuit diagram in which the above semiconductor device is used as a memory element. In FIG. 12C, one of the source electrode and the drain electrode of the transistor 162 is One of the electrodes of the capacitor 164 and the gate electrode of the transistor 140 are electrically connected. In addition, the first wiring (also called the source line) and the transistor The source electrode of 140 is electrically connected to the second wiring (2nd Line: bit line Also referred to as a drain electrode of the transistor 140 is electrically connected to A third wiring (also called a first signal line) and the source of the transistor 162 The other of the drain electrode and the drain electrode is electrically connected to a fourth wiring (4th Line The second signal line (also referred to as a second signal line) is electrically connected to the gate electrode of the transistor 162. A fifth line (also called a word line) and a capacitance element 16 The other electrode of 4 is electrically connected.

[0382] The transistor 162 including an oxide semiconductor has an extremely low off-state current. Therefore, by turning off the transistor 162, the source of the transistor 162 One of the electrodes or drain electrodes of the capacitor 164 and the transistor 140 The potential of the node (hereinafter, node FG) that is electrically connected to the gate electrode of By providing the capacitance element 164, This makes it easier to hold the charge given to the gate FG and to read out the held information. become.

[0383] When storing (writing) information in the semiconductor device, the potential of the fourth wiring is first This sets the potential at which the transistor 162 is turned on, thereby turning the transistor 162 on. Thus, the potential of the third wiring is supplied to the node FG, and a predetermined amount of charge is accumulated in the node FG. Here, the charges that give two different potential levels (hereinafter, low level Either a charge or a high level charge is given. The potential of the fourth wiring is set to a potential at which the transistor 162 is turned off. By turning off 162, node FG is in a floating state, so As described above, a certain amount of charge is stored in the node FG. By storing and holding information, the memory cell can store information.

[0384] Since the off-state current of the transistor 162 is extremely small, the charge supplied to the node FG is Therefore, no refresh operation is required or the refresh operation is It is possible to reduce the frequency of the laser operation extremely, and power consumption is significantly reduced. In addition, even if there is no power supply, the memory contents can be retained for a long period of time. It is possible.

[0385] When reading out the stored information, a predetermined potential (constant potential) is applied to the first wiring. When an appropriate potential (read potential) is applied to the fifth wiring in this state, the potential is held at the node FG. Depending on the amount of charge transferred, transistor 140 assumes different states. If 40 is an n-channel type, then when a high-level charge is held at node FG, The apparent threshold voltage V of the transistor 140 th_H A low-level charge is applied to node FG. The apparent threshold voltage V of transistor 140 when held th_L Lower Here, the apparent threshold is the threshold voltage required to turn the transistor 140 on. Therefore, the potential of the fifth wiring is V th _H and V th_L By setting the potential V0 between For example, if a high level charge is applied during writing, The potential of the wire 5 is V0 (> V th_H ), transistor 140 is in the "on state." When a low-level charge is applied, the potential of the fifth wire becomes V0( <V th _L ), transistor 140 remains in the “off state.” The potential of the wiring is controlled to read out the on / off state of the transistor 140 (second The stored information can be read out by detecting the potential of the wiring.

[0386] In addition, when the stored information is rewritten, a predetermined amount of electricity is consumed by the rewriting. By supplying a new potential to the node FG that holds the load, the node FG is Specifically, the potential of the fourth wiring is held when the transistor 162 is turned on. This causes the transistor 162 to be turned on. A potential (electric potential related to new information) is supplied to node FG, and a predetermined amount of charge is stored in node FG. After that, the potential of the fourth wiring is set to a potential at which the transistor 162 is turned off. By turning off the transistor 162, the node FG receives the new information. That is, a predetermined amount of charge is stored in the node FG by the first write. While the charge is held, the same operation as the first write (second write) is performed. , it is possible to overwrite the stored information.

[0387] The transistor 162 described in this embodiment is a highly purified oxygen-free transistor disclosed in this specification. The oxide semiconductor film 144 contains an oxide semiconductor film containing an excess of ZnO. By using such a transistor, the off-state current of the transistor can be sufficiently reduced. As a result, a semiconductor device capable of retaining stored contents for an extremely long period of time can be obtained.

[0388] As described above, the oxide semiconductor including the low resistance region sandwiching the channel formation region in the channel length direction is The transistor having the thin film has a low off-current and good on-characteristics (e.g., on-current and field effect). The high mobility (resulting mobility) allows for high-speed operation and high-speed response. In addition, miniaturization can be achieved. By using the transistor, a high-performance and highly reliable semiconductor device can be provided. Cut.

[0389] As described above, the configurations, methods, etc. described in this embodiment may be used in conjunction with the configurations, methods, etc. described in other embodiments. They can be used in any suitable combination.

[0390] (Embodiment 10) The semiconductor device disclosed in this specification can be applied to various electronic devices (including game machines). The electronic device can be, for example, a television device (television or television receivers), computer monitors, digital cameras, digital video cameras digital photo frames, mobile phones (also called mobile phones or mobile phone devices), ), portable game machines, personal digital assistants, audio playback devices, pachinko machines and other large game machines, etc. Examples of electronic devices including the semiconductor device described in the above embodiment will be described. Reveal.

[0391] FIG. 13A shows a notebook personal computer, which includes a main body 3001 and a housing 300 2, a display unit 3003, a keyboard 3004, etc. By applying the semiconductor device shown in any one of the above to 9 to the display portion 3003, high performance and It is possible to provide a highly reliable notebook personal computer.

[0392] FIG. 13B shows a portable digital assistant (PDA), which includes a display unit 3023 and a display unit 3024 on a main body 3021. An external interface 3025 and operation buttons 3024 are provided. The stylus 3022 is an accessory of the semiconductor device shown in any one of the first to ninth embodiments. By applying the body device to the display unit 3023, a mobile information terminal with higher performance and reliability can be obtained. (PDA).

[0393] FIG. 13C shows an example of an electronic book. For example, the electronic book has a housing 2701 and The housing 2701 and the housing 2703 are made up of two housings. The opening and closing operations can be performed with the shaft portion 2711 as an axis. With this configuration, it becomes possible to operate like a paper book.

[0394] A display unit 2705 is incorporated in the housing 2701, and a display unit 2707 is incorporated in the housing 2703. The display unit 2705 and the display unit 2707 are configured to display a continuous screen. Alternatively, a different screen may be displayed. For example, a text is displayed on the right display unit (display unit 2705 in FIG. 13C) and An image can be displayed on the display portion (the display portion 2707 in FIG. 13C). The semiconductor device shown in any one of 1 to 9 can be applied to the display portion 2705 and the display portion 2707. As a result, a high-performance and highly reliable electronic book can be obtained. When using a transmissive or reflective LCD device, it is expected that it will be used in relatively bright conditions. Therefore, solar panels will be installed to generate electricity and charge the battery. It is also possible to use a lithium-ion battery as the battery, which can reduce the size of the device. This has the advantage that

[0395] FIG. 13C shows an example in which an operating unit and the like are provided in the housing 2701. For example, The housing 2701 includes a power supply 2721, operation keys 2723, a speaker 2725, etc. The operation keys 2723 can be used to turn pages. A keyboard and a pointing device may be provided on the rear of the housing. On the front and sides, there are external connection terminals (earphone terminal, USB terminal, etc.), a recording medium insertion part, etc. Furthermore, the electronic book may be configured to have a function as an electronic dictionary. You may do so.

[0396] The electronic book may be configured to transmit and receive information wirelessly. It is also possible to purchase and download desired book data from the server. be.

[0397] FIG. 13D shows a mobile phone, which is composed of two housings, a housing 2800 and a housing 2801. The housing 2801 includes a display panel 2802, a speaker 2803, a microphone, and a 2804, pointing device 2806, camera lens 2807, external connection terminal The housing 2800 also includes a solar cell for charging the mobile phone. The housing 28 is provided with an antenna, a memory slot 2810, and an external memory slot 2811. The semiconductor device according to any one of the first to ninth embodiments is incorporated in a display panel. By applying this to the 2802 panel, a high-performance and highly reliable mobile phone can be achieved. .

[0398] The display panel 2802 is equipped with a touch panel, and the image displayed on the display panel 2802 is shown in FIG. The multiple operation keys 2805 are indicated by dotted lines. It also implements a boost circuit to boost the input voltage to the voltage required for each circuit.

[0399] The display direction of the display panel 2802 changes appropriately depending on the usage mode. Since it has a camera lens 2807 on the same surface as 2802, video telephony is possible. The speaker 2803 and the microphone 2804 are not limited to voice calls, but can also be used for video calls, Recording and playback are possible. Furthermore, the housing 2800 and the housing 2801 can be slid. As shown in 13(D), the device can be folded from the unfolded state to the overlapped state, making it suitable for carrying. This makes it possible to miniaturize the device.

[0400] The external connection terminal 2808 can be connected to various cables such as AC adapters and USB cables. It is possible to charge the battery and to communicate data with a personal computer, etc. A recording medium can be inserted into the memory slot 2811 to accommodate larger amounts of data storage and transfer. do.

[0401] In addition to the above functions, even if the device has infrared communication function, TV reception function, etc. good.

[0402] FIG. 13(E) shows a digital video camera, which includes a main body 3051, a display unit (A) 3057, An eyepiece 3053, an operation switch 3054, a display unit (B) 3055, a battery 3056, etc. The semiconductor device according to any one of the first to ninth embodiments is configured as a display device. By applying this to the display part (A) 3057 and the display part (B) 3055, a high-performance and highly reliable device can be achieved. The imaging device may be a digital video camera.

[0403] FIG. 13F shows an example of a television device. The television device includes a housing 96. The display unit 9603 is incorporated in the camera 01. The display unit 9603 can display images. In addition, in this embodiment, a structure in which a housing 9601 is supported by a stand 9605 is used. The semiconductor device described in any one of Embodiments 1 to 9 is applied to the display portion 9603. This makes it possible to provide a television apparatus with high performance and high reliability.

[0404] The television device can be operated using an operation switch on the housing 9601 or a separate remote control. In addition, the remote control device can be operated by transmitting the information output from the remote control device. A display unit for displaying information may be provided.

[0405] The television set is assumed to be equipped with a receiver and a modem. It can receive television broadcasts and can also communicate by wire or wirelessly via a modem. By connecting to a network, communication can be one-way (sender to receiver) or two-way (sender to It is also possible to communicate information between the sender and the recipient, or between the recipients themselves.

[0406] This embodiment mode can be implemented in appropriate combination with the configurations described in other embodiments. It is.

Claims

[Claim 1] forming an oxide semiconductor film including a channel formation region; forming low-resistance regions, each of which has a lower resistance than the channel formation region and contains a metal element and a dopant, on either side of the channel formation region in the oxide semiconductor film; The low resistance region is a step of forming a film containing the metal element in contact with the oxide semiconductor film, and performing heat treatment while the oxide semiconductor film and the film containing the metal element are in contact with each other to introduce the metal element from the film containing the metal element into the oxide semiconductor film; and a step of introducing the dopant into the oxide semiconductor film through the film containing the metal element.

Citation Information

Patent Citations

  • Semiconductor storage device

    JP2001053164A

  • Semiconductor storage device

    JP2002093924A

  • Semiconductor device

    US20110101351A1