Method of arranging raw materials in coke oven and method of manufacturing coke

By unevenly distributing synthetic resins at the ends of the carbonization chamber, the method addresses coke strength reduction and productivity issues in coke production, enhancing the durability of refractory bricks and improving the coke production process efficiency.

JP2024148144AActive Publication Date: 2024-10-17JFE STEEL CORP

Patent Information

Application Number
JP2024031095
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-04
Filing Date
2024-03-01
Publication Date
2024-10-17
Estimated Expiration
2044-03-01

AI Technical Summary

Technical Problem

Existing methods for recycling waste plastics in coke production face challenges such as decreased coke strength, gas leakage, blockage in gas recovery lines, and reduced productivity due to the mixing of synthetic resins with coal, which are not effectively addressed by current technologies.

Method used

The method involves unevenly distributing synthetic resins near the machine side and coke side of the carbonization chamber, concentrating them at both ends, with a ratio of 75% or more of the total resins in these regions, to minimize void formation and crack development, thereby maintaining coke strength.

Benefits of technology

This approach suppresses coke strength degradation, allows for higher resin mixing ratios, reduces crack formation, and enhances the durability of refractory bricks, improving the overall efficiency and productivity of the coke production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024148144000001_ABST
    Figure 2024148144000001_ABST
Patent Text Reader

Abstract

To propose a technology that can suppress a decrease in coke strength when blending a synthetic resin.SOLUTION: There is provided a method for arranging a raw material in a coke oven, comprising: unevenly distributing a synthetic resin near a machine side and near a coke side of a carbonization chamber when the synthetic resin is charged into the coke oven together with raw coal as a coke raw material; dividing the carbonization chamber equally into four or more regions in a longitudinal direction, and distributing more amounts of the synthetic resin to the region in contact with the machine side and the region in contact with the coke side than in other regions; and preferably controlling a sum of the amounts of the synthetic resin distributed to a region in contact with the machine side and a region in contact with the coke side into 75% or more of the amount of the synthetic resin charged into the entire coke oven. There is also provided a method for manufacturing a coke, comprising carbonizing the synthetic resin and raw coal charged according to the method for arranging a raw material in a coke oven.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for arranging raw materials in a coke oven and a method for producing coke when recycling synthetic resins, such as waste plastics, as raw materials for iron making in the coke oven. In the following description, the unit of mass, "t", is 10 3 In this specification, "synthetic resins" includes not only used plastics that are general waste and are called waste plastics, but also plastics that become industrial waste, such as scraps and defective synthetic resins generated in the manufacturing process, and used plastics. [Background technology]

[0002] In recent years, marine pollution caused by waste plastics has become a global problem, and it is said that the amount of waste plastics flowing into the ocean is approximately 8 million tons per year worldwide. Solving marine pollution is one of the goals of the Sustainable Development Goals (SDGs) adopted at the United Nations Summit in 2015. In response to this, Europe has set up the EU Plastics Strategy and is working to strengthen plastic recycling and reduce disposable plastics. In Japan, the Container and Packaging Recycling Law was enacted in 1995, and waste plastic recycling has been promoted from an early stage. In response to the growing momentum for further waste plastic reduction, the Act on Promotion of Resource Circulation Related to Plastics will come into effect in 2022, and further strengthening of waste plastic recycling is required. In the steel industry, a technology has been put into practical use to recycle waste plastics as raw materials for steelmaking by mixing it with coal as a raw material in a coke oven and charging it. It is implemented as a chemical recycling technology for waste plastics under the Container and Packaging Recycling Law. However, it is known that the strength of coke decreases when waste plastics are mixed into coal to produce coke, and the upper limit of the mixing ratio of waste plastics at which the coke strength does not decrease is said to be approximately 1 mass% (Non-Patent Document 1). Therefore, various technologies have been developed to suppress the deterioration of coke strength caused by mixing waste plastics.

[0003] For example, in Patent Document 1, a sintered body having no holes or cracks extending from the surface to the inside and an apparent density of 0.85 to 1.1 g / cm 3 and volume is 6000~200000mm 3 (6~200cm 3 A method of carbonizing plastic granules in a coke oven is disclosed. In order to mold such granules, a method is disclosed in which waste plastics containing thermoplastic resins are heated to a temperature of 180 to 260°C in a molding device that extrudes them from a nozzle, and then extruded from the nozzle while gas is being sucked in, and cooled with water.

[0004] Patent Document 2 discloses a method of pyrolysis recycling in which waste plastics are charged above the raw materials in the coke oven chamber at least one hour after the raw materials are charged into the coke oven chamber. It is said that by utilizing the space above the coke oven, a large amount of waste plastics can be recycled without affecting the strength of the coke. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2009-293032 A [Patent Document 2] JP 2019-135281 A [Non-patent literature]

[0006] [Non-Patent Document 1] Seiji Nomura, Kenji Kato, Tomoyuki Nakagawa, Ikuo Furumaki Journal of the Japan Society of Energy Vol. 81 No. 8 (2002) pp. 728-737 Summary of the Invention [Problem to be solved by the invention]

[0007] However, the conventional techniques have the following problems. The technology disclosed in Patent Document 1 is characterized by plastic granules that do not have holes or cracks that penetrate from the surface to the inside. When molding synthetic resins with a twin-screw extrusion molding machine, a method is adopted in which the synthetic resin molded product extruded from the nozzle is cut with a cutter to align it to a certain length, and it is practically difficult to cut it without cracks or holes. In addition, although the heating temperature is set to 180 to 260°C, it is not specifically described which part of the device the temperature is indicated. Furthermore, when the heating temperature is set to 180°C or higher, gas is generated by thermal decomposition of the synthetic resins, and the accumulated gas becomes voids in the molten synthetic resins, resulting in a problem of a decrease in density. In addition, although it is possible to suppress the decrease in coke strength by changing the properties of the synthetic resins, the decrease in strength due to voids generated in the coke has not been fundamentally solved. In addition, when the synthetic resins addition rate is high, it is difficult to suppress the decrease in coke strength.

[0008] In addition, in the technology disclosed in Patent Document 2, the impact on coke strength can be minimized by separating coal and waste plastics, but since the raw material charging lid must be opened after charging coal to charge waste plastics, in order to prevent gas leakage, it is necessary to strictly control the amount of gas generated so that it does not exceed the amount of gas suction. However, if the amount of gas generated in the carbonization chamber increases or decreases due to fluctuations in the quality of coal or other reasons, it becomes difficult to control, and there is a risk that the generated gas will leak to the outside and cause abnormal combustion. In addition, a large amount of gas generated is sucked in at the top of the carbonization chamber, but when waste plastics are carbonized at the top of the carbonization chamber, a large amount of powdered carbonized waste plastics is sucked in, which may cause blockages in the gas recovery and cleaning line, and these carbonized waste plastics may be mixed into the recovered tar, reducing the quality of the tar recovered as a product. Furthermore, since plastics are charged after the raw materials are charged into the coal tower, a hopper dedicated to waste plastics must be prepared at the top of the coal delivery car, and the number of steps for charging raw materials increases, which is a factor in reducing the productivity of the coke oven.

[0009] The present invention has been made in consideration of the above-mentioned circumstances, and aims to propose a method for arranging raw materials in a coke oven and a method for producing coke that can suppress a decrease in coke strength when synthetic resins are blended. [Means for solving the problem]

[0010] The method of raw material arrangement in a coke oven of the present invention, which advantageously solves the above-mentioned problems, is characterized in that when synthetic resins are charged into a coke oven together with raw coal as coke raw materials, the synthetic resins are concentrated near the machine side and near the coke side of the carbonization chamber.

[0011] The method for converting synthetic resins into raw materials for iron making according to the present invention includes the steps of: (a) dividing the coke chamber into four or more equal regions in the longitudinal direction, and allocating more of the synthetic resins to the region in contact with the machine side and the region in contact with the coke side than to the other regions; (b) the sum of the amounts of the synthetic resins distributed to the area in contact with the machine side and the area in contact with the coke side is 75% or more of the amount of the synthetic resins charged to the entire coke oven; This may be a more preferable solution.

[0012] The method for producing coke according to the present invention, which advantageously solves the above problems, is characterized by carbonizing synthetic resins and raw coal that have been charged into a coke oven by any one of the above methods for placing raw materials in the coke oven. Effect of the Invention

[0013] In the present invention, the synthetic resins are arranged so as to be concentrated at both ends in the longitudinal direction of the coke chamber, so that the mixing ratio of the synthetic resins in other parts is reduced, making it possible to suppress the decrease in coke strength. This makes it possible to process a larger amount of synthetic resins. Although the coke strength is reduced at the ends where the synthetic resins are concentrated, the severely deteriorated parts are crushed into fine coke by the impacts they receive in the subsequent coke transport process and cooling process (coke dry quenching device, wet quenching device, etc.). The fine coke is recovered and can be used as fuel in the iron ore sintering process, etc.

[0014] In addition, since synthetic resins volatilize due to thermal decomposition, when they are mixed with coal and carbonized, voids are generated inside the coke, and cracks propagate from the voids inside the coke. When synthetic resins are dispersed in coal and charged, cracks propagate from the dispersed voids during coking, making the coke more likely to crumble, making it difficult to push and discharge it from the coke oven. However, by concentrating and mixing the synthetic resins on the coke side and machine side, the occurrence of cracks is limited to both ends of the coke cake. This prevents the middle part of the coke cake from collapsing, making it easier to push and discharge the coke.

[0015] Furthermore, it is known that synthetic resins absorb heat when they are thermally decomposed in an oxygen-free environment. If they absorb heat while in contact with the refractory bricks of a coke oven, the temperature drops locally, and thermal stress can reduce the durability of the refractory bricks. However, on the coke side and machine side, heat is removed to a large extent, and the temperature of the refractory bricks is relatively low, so they are less susceptible to the temperature drop caused by heat absorption. This has the effect of suppressing deterioration of the bricks. [Brief description of the drawings]

[0016] [Figure 1] 1A and 1B are schematic diagrams illustrating a method for disposing raw materials in a coke oven according to one embodiment of the present invention, in which (a) is a plan view and (b) is a side view. [Diagram 2]1A and 1B are schematic diagrams illustrating a method for arranging raw materials in a coke oven according to a comparative example, in which (a) is a plan view and (b) is a side view. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] The following is a detailed description of the embodiments of the present invention. The following embodiments are merely examples of equipment and methods for embodying the technical idea of ​​the present invention, and are not intended to limit the configuration to those described below. In other words, the technical idea of ​​the present invention can be modified in various ways within the technical scope described in the claims.

[0018] (How raw materials are arranged in a coke oven) In this embodiment, when coal and molded synthetic resins are supplied as raw materials into the coke oven carbonization chamber, the synthetic resins are arranged unevenly at the ends of the carbonization chamber in the longitudinal direction. That is, they are arranged so that the mixing ratio of synthetic resins (= synthetic resins mass / (coal mass+synthetic resin mass)×100, mass-based percentage) on the coke discharge side [hereinafter referred to as the coke side (C / S)] and the coke extrusion side [hereinafter referred to as the machine side (M / S)] is as high as possible.

[0019] In this embodiment, it is preferable to equally divide the inside of the coke chamber into four or more regions in the longitudinal direction of the coke chamber, and charge the synthetic resins so that the mixing ratio of the synthetic resins in the region in contact with the coke side and the region in contact with the machine side exceeds the mixing ratio of the synthetic resins in the other inner regions. Furthermore, it is more preferable that the mixing ratio ratio is three times or more. In that case, it is preferable that the total mass of the synthetic resins charged in the region in contact with the coke side and the region in contact with the machine side is 75% or more of the total. At this time, the mixing ratio of the synthetic resins in the other inner regions is 50% or less of the average mixing ratio of the synthetic resins in the whole. Therefore, it is possible to suppress the decrease in strength of the coke after carbonization in that region to 50% or less compared to the case where the synthetic resins are evenly distributed. Although the upper limit of the number of regions divided into the coke chamber is not specified, it is preferable to divide the coke chamber into 10 or less, and more preferably into 6 or less, taking into account the installation load of the raw material charging equipment.

[0020] The carbonization chamber of a normal coke oven is a long, narrow rectangular parallelepiped (for example, W0.6m x D15m x H7m). To distribute the raw materials evenly in the carbonization chamber, coal is charged from multiple coal inlets aligned in the longitudinal direction (D direction) of the carbonization chamber. In this case, by increasing the mixing ratio of synthetic resins charged from the inlet closest to the coke side or machine side, it is possible to concentrate and unevenly distribute waste plastics near the coke side or machine side.

[0021] The amount of synthetic resins mixed with coal in this embodiment to be added to the coke oven is not particularly limited, but is preferably 0.5 mass% or more relative to the total raw materials charged to the coke oven in consideration of the environment. More preferably, it is more than 1.0 mass%, and even more preferably, it is more than 3.0 mass%. There is no particular upper limit, but adding more than 5 mass% may reduce the coke strength. In particular, when a large amount of synthetic resins is added, it is preferable to distribute the synthetic resins unevenly in the region near the coke side and the machine side so that the amount of synthetic resins per raw material charged is 1.0 mass% or less in the inner region excluding the region near the coke side and the machine side.

[0022] (Synthetic resin moldings) When the same mass of synthetic resins is added, the more they are added, the lower the coke strength becomes. When synthetic resins are carbonized in coal, they have a high volatile content, which causes voids to form after vaporization, resulting in voids inside the coke after carbonization. Since the voids are the starting points for cracks inside the coke, it is believed that the more voids there are, the more cracks will form, and the lower the coke strength becomes.

[0023] Synthetic resins are molded, for example, with a twin-screw extrusion molding machine to produce a molded product of synthetic resins. The synthetic resins are crushed or granulated in advance and then supplied. In this case, it is preferable to adjust the moisture content of the synthetic resins to 5% by mass or less. By reducing the moisture content of the synthetic resins, the synthetic resins can be molded stably, and the density of the molded product increases. In order to evaporate the moisture of the synthetic resins, various types of dryers, including hot air current dryers, can be used.

[0024] The twin-screw extrusion molding machine suitable for use in this embodiment and capable of molding synthetic resins is arbitrary, and there is no difference in basic structure. The feed material is kneaded by twin screws housed in a casing, and the synthetic resins are extruded through a nozzle installed on a heated plate. The synthetic resins extruded into a cylindrical shape are cut by a rotary cutter and adjusted to a certain length. At this time, the volume per synthetic resin is adjusted by the inner diameter of the nozzle and the cutting speed of the cutter. Usually, nozzles with an inner diameter of 2.0 to 3.0 cmφ are often used. By molding using a large-diameter nozzle with an inner diameter of 4.0 to 6.0 cmφ, it is possible to manufacture large molded products. The mass of synthetic resins per unit increases, and the amount that can be charged with the same number of charged units can be increased.

[0025] The molded synthetic resins are cylindrical with a diameter equal to or slightly larger than the inner diameter of the nozzle, and their length can be adjusted by the rotation speed of the cutter. The length of the molded product is affected by the position and condition of the forming nozzle, so it is difficult to make it a constant length. There is a distribution of molded products ranging from short to long. The volume can be increased by increasing the maximum length of the molded product, but it is preferable that the maximum length in the distribution of molded product lengths is 20 cm or less. This is because the diameter of the charging port at the top of the carbonization chamber of a coke oven is about 40 to 50 cm, and if the maximum length is made any longer, there is a risk of clogging. The average volume of the molded products is 90 cm. 3 More than 150cm is preferable. 3 More than 200cm is preferable. 3The upper limit depends on the size of the charging inlet of the coke oven, but is preferably 1000 cm 3 It is preferable to set the distance to 600 cm or less. 3 It is even more preferable that:

[0026] (Coke manufacturing method) The molded synthetic resins are put into a hopper, cut out at a constant speed by a quantitative feeder, and cut out onto the coal on a belt conveyor that supplies blended coal to a coke oven. In this embodiment, the synthetic resins charged from the charging port closest to the coke side and the machine side are distributed more, and the synthetic resins charged from the other charging ports are distributed less. This reduces the mixing ratio of the synthetic resins inserted from the other charging ports, making it possible to suppress the decrease in coke strength after carbonization in that part. As an index of coke strength, the drum strength index DI150 / 15 can be measured according to the drum strength measurement method shown in the coke testing method of JIS K2151:2004, which is a mass ratio on a sieve after charging into a drum testing machine and rotating it 150 times and then sieving through a sieve with 15 mm openings. When the drum strength index DI150 / 15 is used, it is preferable that the decrease in DI150 / 15 is less than 1 point. It is known that the DI150 / 15 index has a measurement error of about 0.5 points, and a drop in strength of 1 point or more clearly indicates a decrease in coke strength. In coke oven operations, a drop in coke strength (DI150 / 15) of 1 point or more is recognized as a decrease in coke strength, and operations such as improving the quality of the raw coal may be carried out.

[0027] The mixing ratio of synthetic resins is basically controlled by measuring the coal cut-out speed and the synthetic resin cut-out speed in advance, and adjusting each cut-out speed by the feed rate of the quantitative feeder or the gate opening degree, etc., so as to maintain a constant ratio. In addition, it is difficult to directly measure the mixing ratio of synthetic resins in the longitudinal direction (D direction) of the coke oven carbonization chamber. Therefore, it can be estimated from the mixing ratio of synthetic resins in each hopper of the coal delivery car at the top of the coal delivery port of the carbonization chamber. When raw materials are charged into one furnace in a carbonization furnace from multiple charging ports, they are charged simultaneously from each charging port, so the mixing ratio of synthetic resins directly below each charging port is considered to be the same as the mixing ratio of synthetic resins in each hopper of the coal delivery car. The mixing ratio of synthetic resins in each hopper of the coal delivery car can be estimated by installing a camera at the top of each hopper, detecting synthetic resins by image analysis, and calculating the synthetic resin charging mass.

[0028] The synthetic resin molded products should preferably be cut out from a location where the conveyor belt is low after passing through the coal drying facility (CMC). Because the coal is heated and dried in the CMC, if synthetic resin molded products are added before the CMC, there is a risk that they will melt in the CMC. The synthetic resin molded products are fed to the carbonization chamber via the coal tower and coal delivery car together with the blended coal. The synthetic resins are thermally decomposed in the carbonization chamber, and some remain as charcoal, but most are recycled as gas or tar. EXAMPLES

[0029] (Example 1) A mixture of waste plastics mainly composed of thermoplastic resins was crushed, and after confirming that the moisture content was 5% or less, it was extruded from a 40 mmφ nozzle while being heated using a twin-screw extruder, and cut and molded into a cylindrical shape. As shown in Figure 1, the obtained molded product 1 was charged into a carbonization can 3 together with about 40 kg of blended coal 2 used as a coke raw material. When arranging the waste plastic molded products 1, the amount of blended coal 2 was divided into eight, and first, 1 / 8 of the blended coal was laid out in the carbonization can 3. After that, a predetermined amount of waste plastic molded products 1 (1 / 4 of the amount to be charged) was arranged so as to be in contact with one end of the carbonization can 3 in the longitudinal direction. Next, 1 / 8 of the blended coal was further charged, and the density of the charged coal was increased to 830 kg / m 3 The mixture was compressed so that the mixture was uniform. This process was repeated four times, and the waste plastic molded products 1 were arranged so as to be unevenly distributed at one end of the can in the longitudinal direction. FIG. 1(a) is a plan view illustrating the arrangement of the waste plastics in the carbonization can 1. FIG. 1(b) is a side view illustrating the arrangement of the waste plastics in the carbonization can 1. The mixture ratio of the waste plastics to the blended coal mass was set to 3 mass%. After carbonization at 700 to 1100°C for 20 hours in a test carbonization furnace, water was poured from the top to rapidly cool, and then the mixture was dried to obtain coke. The obtained coke was charged into a drum test machine and rotated 150 times according to the drum strength measurement method shown in the coke test method of JIS K2151:2004, and the mass ratio of the sieve on the sieve with 15 mm openings was measured as the drum strength index DI150 / 15. Many cracks were confirmed on the side of the coke after carbonization where the waste plastic molded products 1 were concentrated, and it was presumed that the coke strength in the vicinity of the cracks had decreased. On the other hand, the other cokes were in good condition.

[0030] Comparative Example 1 As shown in FIG. 2, the waste plastic molded products 1 produced by the same method as the invention example were arranged as uniformly as possible in about 40 kg of blended coal 2. When arranging the waste plastic molded products 1, the amount of blended coal 2 was divided into eight parts, and 1 / 8 of the blended coal 1 was first laid in the carbonization can 3. After that, the waste plastic molded products 1 were arranged so that the centers of the waste plastic molded products 1 were located at 1 / 4 and 3 / 4 positions in the length and width directions from one end of the carbonization can 3. At this time, the amount of waste plastic to be charged was set to 1 / 4. This process was repeated four times, and when the carbonization can 3 was divided into four in the longitudinal direction, the mixing ratio of waste plastic was set to the same in each region. FIG. 2(a) is a plan view explaining the arrangement of waste plastics in the carbonization can 1. FIG. 2(b) is a side view explaining the arrangement of waste plastics in the carbonization can 1. The mixing ratio of waste plastics to the blended coal mass was set to 3 mass%. After carbonization in a test carbonization furnace at 700 to 1100°C for 20 hours, the mixture was quenched by pouring water over it from above, and then dried to obtain coke. The obtained coke was charged into a drum testing machine and rotated 150 times according to the drum strength measurement method specified in the coke testing method of JIS K2151:2004, and the mass ratio of the remaining coke on a sieve with 15 mm openings was measured as the drum strength index DI150 / 15.

[0031] A comparison of the drum strengths of the obtained cokes is shown in Table 1. As a reference example, the strength of coke obtained by carbonization of only blended coal is also shown in Table 1. When the waste plastic molded products 1 are evenly distributed in the coal in the carbonization tank 3 as in the comparative example, the drum strength of the coke is significantly reduced compared to the reference example. It was found that by concentrating the waste plastic molded products 1 at one end of the carbonization tank 3 as in the invention example, the decrease in drum strength compared to the reference example is suppressed.

[0032] [Table 1]

[0033] (Example 2) A mixture of waste plastics, mainly consisting of thermoplastic resins, was crushed and confirmed to have a moisture content of 5% or less. The mixture was then extruded from a 40 mmφ nozzle while being heated using a twin-screw extruder, cut into pieces with an axial length of 20 mm or more, and molded into a cylindrical shape. This was mixed with a blended coal for coke ovens to a mixing ratio of 3% by mass, and then charged into the hopper of a coal delivery car at the top of the coke oven as a coke raw material. Four hoppers were installed on the coal delivery car. Of the hoppers, coal mixed with waste plastics was charged into the hoppers closest to the machine side and the coke side, respectively, and only coal was charged into the inner hopper. Next, coke raw materials were simultaneously cut out from the bottom of each hopper of the coal delivery car and charged into the carbonization chamber, so that the waste plastic mixing ratio of the machine side and coke side of the carbonization chamber was 3% by mass, and the waste plastic mixing ratio of the middle part was 0% by mass. At this time, the average mixing ratio of waste plastics in the carbonization chamber was 1.5% by mass. The strength of the coke obtained after carbonization was measured according to the drum strength measurement method shown in the coke test method of JIS K2151:2004. As a result, the value of the drum strength index DI150 / 15, which is the mass ratio of the sieve on a sieve with 15 mm openings after charging into a drum test machine and rotating it 150 times, was 85.7. In addition, the coke cake pushability after carbonization was better than that of Comparative Example 2 described later.

[0034] Comparative Example 2 A mixture of waste plastics mainly composed of thermoplastic resins was crushed and confirmed to have a moisture content of 5% or less. The mixture was then extruded from a 40 mmφ nozzle while being heated using a twin-screw extruder, cut into pieces with an axial length of 20 mm or more, and molded into a cylindrical shape. This was mixed with a blended coal for coke ovens to a mixing ratio of 1.5% by mass, and then evenly charged into the four hoppers of a coal delivery car at the top of the coke oven as a coke raw material. Next, coal was simultaneously cut out from the bottom of each hopper of the coal delivery car so that the mixing ratio of the waste plastics in the carbonization chamber was evenly 1.5% by mass. The strength of the coke obtained after carbonization was measured according to the drum strength measurement method shown in the coke test method of JIS K2151:2004. As a result, the value of the drum strength index DI150 / 15, which is the mass ratio of the sieve on a sieve with a 15 mm mesh after being charged into a drum testing machine and rotated 150 times, was 84.0. In addition, the pushability of the coke cake after carbonization was worse than that of Example 2, and a larger power was required to discharge the coke cake. [Explanation of symbols]

[0035] 1. (Waste plastic) Molded products 2 Blended coal 3. Carbonization chamber

Claims

1. A method for distributing synthetic resins as coke raw materials in a coke oven together with raw coal, the method distributing synthetic resins unevenly in the vicinity of the machine side and the vicinity of the coke side of the coke oven.

2. 2. A method for arranging raw materials in a coke oven as described in claim 1, wherein the carbonization chamber is divided equally into four or more regions in the longitudinal direction, and more synthetic resins are allocated to the region adjacent to the machine side and the region adjacent to the coke side than to the other regions.

3. 3. A method for allocating raw material to a coke oven as described in claim 2, wherein the sum of the amounts of synthetic resins allocated to the area in contact with the machine side and the area in contact with the coke side is 75% or more of the amount of synthetic resins charged to the entire coke oven.

4. A method for producing coke, comprising carbonizing synthetic resins and raw coal charged by the method for disposing raw materials in a coke oven according to any one of claims 1 to 3.

Citation Information

Patent Citations

  • Operation of coke oven

    JP1988317587A

  • Preparation of coke having uniform strength

    JP1993239465A

  • Method for feeding coking coal into coke oven

    JP1994212162A

  • Method for charging coal and waste plastic into coke oven and apparatus for loading coal and waste plastic in coal charging vehicle

    JP1997132780A

  • Treating method for waste plastic with coke oven

    JP2001098277A

Cited By

  • Method for arranging raw materials in a coke oven, and method for producing coke and by-product gases.

    JP2026177660A