Printed wiring board

The printed wiring board's strategic pad and mounting area layout with controlled flux spread addresses the flux adherence issue, ensuring high connection reliability and compact size by separating pads with 0.5 to 1.5 mm distances.

JP2024156359APending Publication Date: 2024-11-06IBIDEN CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023070757
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-24
Publication Date
2024-11-06

AI Technical Summary

Technical Problem

The challenge in existing printed wiring boards is the difficulty in removing flux from the third conductive pad due to its proximity to the first and second pads, which affects the connection reliability between the second pad and the solder bump.

Method used

The printed wiring board design includes a topmost resin insulating layer with distinct mounting areas and pads, separated by a distance of 0.5 to 1.5 mm, and a top conductor layer with metal bumps formed by plating, ensuring flux from one area does not spread to adjacent areas during reflow, thereby maintaining high connection reliability.

Benefits of technology

This design effectively prevents flux adherence to unintended pads, enhancing the connection reliability between the second pad and solder bump, while allowing for a compact board size.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024156359000001_ABST
    Figure 2024156359000001_ABST
Patent Text Reader

Abstract

To provide a printed wiring board having high quality.SOLUTION: A printed wiring board 10 includes: an uppermost resin insulation layer 12 having a first mounting area A1 and a second mounting area A2; an uppermost conductor layer 14 having a plurality of first pads 14a and a plurality of second pads 14b; an upper solder resist layer 16 having a plurality of first openings 16a leading to the first pads 14a, respectively and a plurality of second openings 16b leading to the second pads 14 b, respectively; a metal bump 20 for mounting a first electronic component, the metal bump being formed on each of the first pads 14a; and a solder bump 42 for mounting a second electronic component, the solder bump being formed on each of the second pads 14b. The metal bump 20 is formed by plating, and includes a first portion 24 formed inside the first opening 16a, and a second portion 28 extending from the first portion 24 and formed on the solder resist layer 16 around the first opening 16a. A distance between the first mounting area A1 and the second mounting area A2 is 0.5 mm or more and 1.5 mm or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The technology disclosed in this specification relates to a printed wiring board. [Background technology]

[0002] Patent Document 1 discloses a printed wiring board having a first conductive pad, a second conductive pad, and a third conductive pad. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2021-52104 Summary of the Invention

[0004] In Patent Document 1, a semiconductor chip is mounted on a first conductive pad, and a capacitor is mounted on a third conductive pad. Generally, flux is used when a bump for mounting a semiconductor chip is formed. According to FIG. 1 of Patent Document 1, the first conductive pad and the second conductive pad are arranged close to each other. Therefore, it is expected that the flux for forming the bump for mounting the semiconductor chip will reach the third conductive pad. It is expected that the flux will adhere firmly to the third conductive pad during reflow. In that case, it is expected that it will be difficult to remove the flux from the third conductive pad. [Means for solving the problem]

[0005] The printed wiring board of the present invention comprises a top resin insulating layer having a first mounting area and a second mounting area, a top conductor layer having a plurality of first pads formed on the top resin insulating layer in the first mounting area and a plurality of second pads formed on the top resin insulating layer in the second mounting area, an upper solder resist layer formed on the top resin insulating layer and the top conductor layer and having a plurality of first openings leading to each of the first pads and a plurality of second openings leading to each of the second pads, metal bumps for mounting a first electronic component formed on each of the first pads, and solder bumps for mounting a second electronic component formed on each of the second pads, the metal bumps being formed by plating, the metal bumps being formed of a first portion formed in the first opening and a second portion extending from the first portion and formed on the solder resist layer around the first opening, and the distance (distance X) between the first mounting area and the second mounting area is 0.5 mm or more and 1.5 mm or less.

[0006] In an embodiment of the present invention, a metal bump for mounting a first electronic component is formed on a first pad. When flux is applied onto the metal bump in the first mounting area, the flux spreads from the first mounting area. A distance X between the first mounting area and the second mounting area is 0.5 mm or more. The first mounting area and the second mounting area are far away. Therefore, the flux spreading from the first mounting area is unlikely to reach the second mounting area. During reflow, the flux is unlikely to adhere firmly to the second pad. In the printed wiring board of the embodiment, the connection reliability between the second pad and the solder bump is high. The distance is 1.5 mm or less. The size of the printed wiring board can be reduced. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view illustrating a printed wiring board according to an embodiment. [Figure 2A] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2B] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2C] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2D] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2E] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2F] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2G] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2H] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Figure 2I] 1A to 1C are cross-sectional views each showing a schematic diagram of a method for manufacturing a printed wiring board according to an embodiment. [Diagram 3] FIG. 2 is a plan view showing a schematic view of a mounting area of ​​a printed wiring board according to an embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] <Printed Wiring Board of the Embodiment> Fig. 1 is a cross-sectional view of a printed wiring board 10 according to an embodiment. As shown in Fig. 1, the printed wiring board 10 has a resin insulating layer (uppermost resin insulating layer) 12 disposed on the uppermost part, a conductor layer (uppermost conductor layer) 14 formed on the resin insulating layer 12, and a solder resist layer (upper solder resist layer) 16 formed on the resin insulating layer 12 and the conductor layer 14.

[0009] The resin insulating layer 12 is formed of a resin composition containing an inorganic filler and an epoxy resin. Examples of the inorganic filler include silica and alumina. The resin insulating layer 12 has a first surface F and a second surface B opposite to the first surface F. As shown in FIG. 3, the first surface F of the resin insulating layer 12 has a first mounting area A1 and a second mounting area A2. The first surface F of the resin insulating layer 12 may have a third mounting area A3. The distance X between the first mounting area A1 and the second mounting area A2 is 0.5 mm or more and 1.5 mm or less. The distance Y between the first mounting area A1 and the third mounting area A3 is 0.5 mm or more and 1.5 mm or less. It is preferable that the distance X and the distance Y are different.

[0010] The conductor layer 14 has a plurality of first pads 14a and a plurality of second pads 14b. All of the first pads 14a are formed on the first surface F of the resin insulating layer 12 in the first mounting area A1. All of the second pads 14b are formed on the first surface F of the resin insulating layer 12 in the second mounting area A2. When the third mounting area A3 is present, the conductor layer 14 has a plurality of third pads 14c. All of the third pads 14c are formed on the first surface F of the resin insulating layer 12 in the third mounting area A3.

[0011] The solder resist layer 16 has a plurality of first openings 16a leading to the plurality of first pads 14a, and a second opening 16b leading to the plurality of second pads 14b. When the third pads 14c are present, the solder resist layer 16 has a third opening 16c leading to the plurality of third pads 14c.

[0012] The printed wiring board 10 further has metal bumps 20 formed on each of the first pads 14a and solder bumps 42 formed on each of the second pads 14b. If the third pads 14c are present, the printed wiring board 10 has solder bumps 43 formed on each of the third pads 14c. A first electronic component 51 is mounted on the printed wiring board 10 via the metal bumps 20. A second electronic component 52 is mounted on the printed wiring board 10 via the solder bumps 42. A third electronic component 53 is mounted on the printed wiring board 10 via the solder bumps 43.

[0013] A metal layer 18 is formed between the solder bump 42 and the second pad 14b. If the solder bump 43 is present, the metal layer 18 is formed between the solder bump 43 and the third pad 14c. The metal layer 18 is formed of a metal different from that of the conductor layer 14. An example of the metal layer 18 is gold.

[0014] The metal bump 20 is formed directly on the first pad 14a without the metal layer 18. The metal bump 20 and the first pad 14a are formed of the same kind of metal. The metal bump 20 and the first pad 14a are formed of copper. The metal bump 20 is formed by plating. The metal bump 20 is formed of a first portion 24 formed in the first opening 16a and a second portion 28 on the first portion 24. The first portion 24 and the second portion 28 are integrally formed. The second portion 28 extends onto the solder resist layer 16 around the first opening 16a. As shown in FIG. 2H, the printed wiring board 10 may have a tin layer 29 on the second portion 28. A nickel layer 26 may be formed between the second portion 28 and the tin layer 29. The reflow process changes the shape of the tin layer 29 from a layered shape to a substantially hemispherical shape as shown in FIG. 1. A tin bump 30 is formed on the metal bump 20.

[0015] <Method of manufacturing a printed wiring board according to an embodiment> 2A to 2I show a method for manufacturing the printed wiring board 10 of the embodiment.

[0016] 2A shows an intermediate body having a resin insulating layer 12 having a first surface F and a second surface B, a conductor layer 14 on the first surface F of the resin insulating layer 12, and a solder resist layer 16 on the resin insulating layer 12 and the conductor layer 14. The conductor layer 14 is formed by a semi-additive method. The conductor layer 14 includes a first pad 14a, a second pad 14b, and a third pad 14c. The first surface F of the resin insulating layer 12 has a first mounting area A1, a second mounting area A2, and a third mounting area A3. All of the first pads 14a are formed in the first mounting area A1, all of the second pads 14b are formed in the second mounting area A2, and all of the third pads 14c are formed in the third mounting area A3.

[0017] 2B, a plurality of second openings 16b and a plurality of third openings 16c are formed in the solder resist layer 16 by a laser or the like. Each of the second openings 16b leads to a corresponding one of the second pads 14b. Each of the third openings 16c leads to a corresponding one of the third pads 14c.

[0018] As shown in FIG. 2C, a metal layer 18 made of gold is formed on the second pad 14b and the third pad 14c.

[0019] 2D, a plurality of first openings 16a are formed by a laser or the like in the solder resist layer 16. Each of the first openings 16a reaches a corresponding one of the first pads 14a.

[0020] 2E, a seed layer 36 is formed. The seed layer 36 is formed on the upper surface of the solder resist layer 16, on the inner wall surfaces of the first opening 16a, the second opening 16b, and the third opening 16c, on the first pad 14a exposed from the first opening 16a, on the metal layer 18 exposed from the second opening 16b, and on the metal layer 18 exposed from the third opening 16c.

[0021] As shown in Figure 2F, a plating resist 38 is formed on the seed layer 36. The plating resist 38 has openings 38a for forming the metal bumps 20 (Figure 1).

[0022] 2G, a metal bump 20 is formed by electrolytic plating. The metal bump 20 is formed of a first portion 24 filling the opening 16a and a second portion 28 on the first portion 24. The first portion 24 and the second portion 28 are continuous. A nickel layer 26 and a tin layer 29 are formed on the top portion 24a of the metal bump 20.

[0023] 2H, the plating resist 38 is removed. The seed layer 36 exposed from the metal bumps 20 is removed.

[0024] Flux is applied to the entire surface of the first mounting area A1. All the metal bumps 20 in the first mounting area A1 are covered with flux. The flux in the first mounting area A1 tends to spread outward from the first mounting area A1. In the embodiment, the distance X between the first mounting area A1 and the second mounting area A2 is 0.5 mm or more. Therefore, the first mounting area A1 and the second mounting area A2 are far away. Therefore, the flux spreading from the first mounting area A1 is unlikely to reach the second mounting area A2. As shown in FIG. 2I, a reflow process is performed. A tin bump 30 having a substantially hemispherical shape is formed on the metal bump 20 from the tin layer 29. At this time, the flux does not reach the second pad 14b in the second mounting area A2, so the flux does not adhere to the second pad 14b. The flux is removed.

[0025] Solder bumps 42, 43 are formed on the second pad 14b and the third pad 14c. At this time, the flux (flux in the first mounting area A1) for forming the tin bump 30 is not fixed to the second pad 14b and the third pad 14c. Therefore, the connection reliability between the second pad 14b and the solder bump 42 is high. The connection reliability between the third pad 14c and the solder bump 43 is high. The printed wiring board 10 of the embodiment (see FIG. 1) is obtained. The seed layer 36 is not shown in FIG. 1. [Explanation of symbols]

[0026] 10: Printed wiring board 12: Resin insulation layer 14: Conductive layer 14a: 1st pad 14b: 2nd pad 16: Solder resist layer 16a: 1st opening 16b: 2nd opening 18: Metal layer 20: Metal bump 24 :1st part 24a: Top 26: Nickel layer 28:Second part 36: Seed layer 38: Plating resist 38a:Aperture 42: Solder bump 51: First electronic component 52: Second electronic component A1: First mounting area A2: Second mounting area X: distance Y :Distance

Claims

1. a top resin insulating layer having a first mounting area and a second mounting area; a top conductor layer having a plurality of first pads formed on the top resin insulating layer in the first mounting area and a plurality of second pads formed on the top resin insulating layer in the second mounting area; an upper solder resist layer formed on the uppermost resin insulating layer and the uppermost conductor layer, the upper solder resist layer having a plurality of first openings leading to each of the first pads and a plurality of second openings leading to each of the second pads; a metal bump for mounting a first electronic component formed on each of the first pads; a solder bump for mounting a second electronic component formed on each of the second pads; A printed wiring board having The metal bump is formed by plating, and the metal bump is formed of a first portion formed within the first opening and a second portion extending from the first portion and formed on the solder resist layer around the first opening, and a distance (distance X) between the first mounting area and the second mounting area is 0.5 mm or more and 1.5 mm or less.

2. 2. The printed wiring board of claim 1, further comprising a third mounting area, a distance (distance Y) between the first mounting area and the third mounting area being 0.5 mm or more and 1.5 mm or less, and the distances X and Y being different.

Citation Information

Patent Citations

  • Printed wiring board and method for manufacturing the same

    JP2021052104A