Wafer processing method
The wafer processing method using a sheet without an adhesive layer addresses debris scattering and cracking issues by facilitating easy annular protrusion removal, ensuring high-quality and productive chip production.
Patent Information
- Application Number
- JP2023085165
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-24
- Publication Date
- 2024-12-05
AI Technical Summary
The existing methods for removing the annular convex portion from wafers during chip division result in scattering of processing debris, adherence of debris to the adhesive tape, and require strong forces to separate the annular protrusion, leading to potential cracking and reduced productivity.
A wafer processing method involving the use of a sheet without an adhesive layer, fixed to the wafer via thermocompression bonding, which allows for easy removal of the annular protrusion without debris adherence and reduces the need for UV irradiation, thereby maintaining wafer quality and increasing productivity.
The method effectively prevents debris from adhering to the wafer, reduces the risk of cracking, and enhances productivity by eliminating the need for UV irradiation, resulting in high-quality device chips.
Smart Images

Figure 2024168460000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for processing a wafer having a back surface with an annular convex portion on the outer periphery and a circular concave portion formed in an area surrounded by the annular convex portion. [Background technology]
[0002] Device chips are mounted on electronic devices such as mobile phones and personal computers. Device chips are usually manufactured by thinning a wafer, which has multiple devices such as ICs (Integrated Circuits) formed on its front side, by grinding it from its back side, and then dividing the wafer into individual devices.
[0003] The grinded and thinned wafer has a reduced rigidity and is prone to cracking. Therefore, a circular recess is formed by grinding an area of the back surface of the wafer corresponding to a device formation area where multiple devices are formed, and the surrounding area is left as an annular protrusion. This annular protrusion functions to reinforce the thinned circular recess while the wafer is being transported (see, for example, Patent Document 1).
[0004] On the other hand, when dividing the wafer into individual chips, the annular convex portion becomes an obstacle to division, and therefore it is necessary to remove the annular convex portion from the wafer in advance. When removing the annular convex portion, an adhesive tape is applied to the entire back surface of the wafer, including the circular concave portion and the annular convex portion, and the wafer is held by a holding table via the adhesive tape. The holding table has a convex shape corresponding to the circular concave portion of the wafer, and the circular concave portion is aligned with this convex shape. Then, an annular dividing groove is formed in the wafer held by the holding table, and the annular convex portion is removed (see, for example, Patent Document 2).
[0005] Also, as another method for removing the annular convex portion from the wafer, an adhesive tape is attached to the surface of the wafer, the wafer is held by suction on a flat holding table via the adhesive tape, and a dividing groove is formed in the wafer to cut out the annular convex portion (see, for example, Patent Document 3). [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2007-173487 A [Patent Document 2] JP 2011-61137 A [Patent Document 3] JP 2012-54275 A Summary of the Invention [Problem to be solved by the invention]
[0007] Regardless of the method used to remove the annular convex portion, an annular frame is attached to the outer periphery of the adhesive tape attached to the wafer. At this time, the wafer is accommodated in an opening formed in the annular frame. Then, when the wafer is processed to form a dividing groove, processing debris is generated from the wafer and scattered around. Some of the scattered processing debris adheres to the adhesive tape exposed in the opening of the annular frame. Then, during the wafer transport, processing, etc., some of the processing debris may scatter again and adhere to the wafer, causing a problem.
[0008] In addition, after forming a dividing groove in the wafer and separating the annular convex portion, the separated annular convex portion is peeled off from the adhesive tape. However, since the annular convex portion is strongly attached to the adhesive tape having the glue layer before being separated from the wafer, a large force is required to separate the annular convex portion from the adhesive tape. In addition, the large force applied to the annular convex portion may cause the annular convex portion to break and fragments to scatter onto the wafer.
[0009] Therefore, it is conceivable to attach an adhesive tape having a glue layer whose adhesive strength is reduced by ultraviolet irradiation to the wafer and the annular frame. In this case, when peeling off the annular convex portion cut off from the wafer from the adhesive tape, the adhesive tape is irradiated with ultraviolet rays in the area overlapping with the annular convex portion to reduce the adhesive strength of the glue layer. At this time, a shielding member is used to prevent ultraviolet rays from being irradiated to the area overlapping with the circular concave portion.
[0010] However, in order to irradiate the area overlapping with the annular convex portion with ultraviolet light with sufficient intensity, the size of the area that can be shielded by the shielding member is limited. Therefore, the adhesive tape is also irradiated with ultraviolet light in the area overlapping with the outer periphery of the circular concave portion, and the adhesive strength of the adhesive tape is reduced in this area. If the wafer is divided in the area where the adhesive strength of the adhesive tape is reduced, the wafer is not sufficiently supported in that area, resulting in low quality processing. Therefore, it is necessary to narrow the area used for device formation on the surface of the wafer, which reduces productivity.
[0011] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a wafer processing method for processing a wafer having an annular convex portion with high quality and high productivity. [Means for solving the problem]
[0012] According to one aspect of the present invention, there is provided a method for processing a wafer having an annular convex portion on the outer periphery of its back surface and a circular concave portion formed in an area surrounded by the annular convex portion on the back surface, the method including a wafer unit formation step of forming a wafer unit by fixing a sheet without a glue layer to the surface of the wafer and fixing an annular frame to the outer periphery of the sheet, a holding step after the wafer unit formation step of holding the wafer on a holding table via the sheet, a dividing step after the holding step of forming a dividing groove in the circular concave portion of the wafer and separating the annular convex portion from the wafer, and a removal step after the dividing step of removing the annular convex portion from the sheet.
[0013] Preferably, in the wafer unit forming step, the sheet is fixed to the wafer by heating and pressing the sheet to thermocompression bond the sheet to the wafer. Effect of the Invention
[0014] In a wafer processing method according to one aspect of the present invention, a wafer unit is formed by fixing a sheet having no adhesive layer to a wafer and an annular frame. Since the sheet has no adhesive layer, even if processing debris generated when forming a dividing groove in the wafer comes into contact with the sheet, the processing debris is not attached to the sheet. Furthermore, even if the annular convex portion is broken when removing the sheet and the resulting fragments come into contact with the sheet, the fragments are not attached to the sheet. Furthermore, processing debris and fragments that come into contact with the sheet are easily removed from the sheet by cleaning.
[0015] Also, unlike when the annular protrusion is strongly attached to an adhesive tape by a glue layer, when it is fixed to a sheet without a glue layer, it is relatively easy to remove. Therefore, no large force is applied to the annular protrusion to be removed, and it is less likely to break or produce fragments. Therefore, processing waste or fragments that come into contact with the sheet will not be transferred to the wafer (device chip) and degrade the quality of the device chip.
[0016] Furthermore, there is no need to irradiate the sheet with ultraviolet light in order to remove the annular protrusion from the sheet, and there is no need to narrow the area used for device formation on the surface of the wafer on the assumption that ultraviolet light will be irradiated, which increases the productivity of device chips.
[0017] Therefore, one aspect of the present invention provides a wafer processing method for processing a wafer having an annular protrusion with high quality and high productivity. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1(A) is a perspective view that typically shows the back surface side of a wafer, and FIG. 1(B) is a perspective view that typically shows the front surface side of the wafer. [Diagram 2] FIG. 2(A) is a cross-sectional view that typically shows a thermocompression bonding apparatus, and FIG. 2(B) is a cross-sectional view that typically shows the thermocompression bonding apparatus in a first stage of a wafer unit formation step. [Diagram 3]FIG. 3(A) is a cross-sectional view showing a schematic diagram of a thermocompression bonding apparatus in a second stage of the wafer unit formation step, and FIG. 3(B) is a cross-sectional view showing a schematic diagram of a thermocompression bonding apparatus in a third stage of the wafer unit formation step. [Figure 4] FIG. 11 is a cross-sectional view showing a schematic diagram of a thermocompression bonding apparatus in a fourth stage of the wafer unit forming step. [Diagram 5] FIG. 2 is a perspective view illustrating a wafer unit. [Figure 6] FIG. 6(A) is a perspective view that typically shows the wafer unit in the holding step, and FIG. 6(B) is a cross-sectional view that typically shows the wafer unit in the holding step. [Figure 7] FIG. 7(A) is a perspective view that typically shows the wafer unit in the dividing step, and FIG. 7(B) is a cross-sectional view that typically shows the wafer unit in the dividing step. [Figure 8] FIG. 8(A) is a perspective view that typically shows the wafer unit in the removing step, and FIG. 8(B) is a cross-sectional view that typically shows the wafer unit in the removing step. [Figure 9] 3 is a flowchart showing a flow of each step of a wafer processing method according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] An embodiment according to one aspect of the present invention will be described with reference to the accompanying drawings. Fig. 1(A) is a perspective view showing a schematic view of the back surface 11b side of a wafer 11, and Fig. 1(B) is a perspective view showing a schematic view of the front surface 11a side of the wafer 11. First, the wafer 11 processed by the wafer processing method according to this embodiment will be described.
[0020] The wafer 11 is a disk-shaped single crystal substrate made of a semiconductor material such as silicon (Si) or silicon carbide (SiC). However, there is no limitation on the shape, structure, size, etc. of the wafer 11. As shown in Fig. 1(B) , a plurality of planned division lines 19 are set in a lattice pattern on the front surface 11a side of the wafer 11. Devices 21 such as ICs and LSIs are formed in each of the areas partitioned by the plurality of planned division lines 19.
[0021] An outer peripheral region surrounding the region on the front surface 11a of the wafer 11 in which the multiple devices 21 are formed is called an outer peripheral surplus region 23. In addition, an outer peripheral surplus region 23 on the front surface 11a of the wafer 11 in which the multiple devices 21 are formed is called a device formation region 25.
[0022] When the wafer 11 on which a plurality of devices 21 are formed is ground from the back surface 11b side to be thinned, and the wafer 11 is divided along the intended division lines 19, a plurality of thin device chips each having a device 21 are obtained. The wafer 11 is divided, for example, by a cutting device equipped with an annular cutting blade. However, the wafer 11 which has been ground and thinned has a reduced rigidity and is easily broken, and is difficult to handle, such as transport.
[0023] 1(A), a region of the back surface 11b of the wafer 11 corresponding to a device formation region 25 in which a plurality of devices 21 are formed is ground to form a circular recess 15, and its periphery is left as an annular protrusion 13. This annular protrusion 13 functions to reinforce the thinned circular recess 15 while the wafer 11 is being transported, etc. This maintains the rigidity of the wafer 11, making it less susceptible to warping or cracking, and facilitating handling.
[0024] However, when attempting to divide the wafer 11 having the annular protrusion 13 on the back surface 11b side by a cutting device along the intended division lines 19, the division grooves formed in the wafer 11 to divide the thin circular recesses 15 cannot cut the thick annular protrusion 13. In other words, the annular protrusion 13 becomes an obstacle to division when dividing the wafer 11 into individual chips.
[0025] Therefore, it is necessary to remove the annular convex portion 13 from the wafer 11 before dividing the wafer 11. In the wafer processing method according to this embodiment, a sheet without an adhesive layer is fixed to the entire surface 11a of the wafer 11 by a method such as thermocompression bonding. The wafer 11 is held by a holding table of the dividing device via the sheet.
[0026] Next, the sheet fixed to the wafer 11 will be described. Figure 3(A) and the like include a cross-sectional view that shows the sheet 27. Figure 5 and the like include a perspective view that shows the sheet 27. The sheet 27 has a diameter larger than the outer diameter of the wafer 11, and does not include a glue layer. The sheet 27 is a thermoplastic sheet.
[0027] The outer periphery of sheet 27 is disposed on a metal annular frame 29 (see FIG. 5, etc.) Sheet 27 is, for example, a flexible resin-based sheet such as a polyolefin-based sheet or a polyester-based sheet, but the material of sheet 27 is not limited thereto.
[0028] Here, the polyolefin sheet is a sheet of a polymer synthesized using an alkene as a monomer. The polyolefin sheet used for the sheet 27 is, for example, a polyethylene sheet, a polypropylene sheet, or a polystyrene sheet, which is transparent or semi-transparent to visible light.
[0029] The polyester-based sheet is a polymer sheet 27 synthesized using dicarboxylic acid (a compound having two carboxyl groups) and diol (a compound having two hydroxyl groups) as monomers. The polyester-based sheet used for the sheet 27 is, for example, a polyethylene terephthalate sheet or a polyethylene naphthalate sheet 27 that is transparent or semi-transparent to visible light.
[0030] From another perspective, the sheet 27 that does not have an adhesive layer and is fixed to the wafer 11 by thermocompression has a storage modulus of 1×10 6 ~1×10 9 Pa, and the storage modulus upon heating is 1×10 6 ~1×10 7 The thermoplastic resin has a viscosity of Pa. Here, "heated" refers to the temperature at which the sheet 27 is thermocompression bonded to the wafer 11. For example, when the sheet 27 is made of polyolefin, the temperature may be 80°C to 100°C.
[0031] A viscoelasticity measuring device "DMA7100" manufactured by Hitachi High-Tech Corporation can be used to evaluate the storage modulus of the thermoplastic resin used as the constituent material of the sheet 27. This viscoelasticity measuring device applies periodic deformation to a sample and measures the resulting stress or strain, thereby making it possible to calculate the temperature dependence and frequency dependence of the storage modulus, loss modulus, loss tangent (tan δ), and other viscoelastic properties of the sample.
[0032] Measurement of the storage modulus of a thermoplastic resin using a viscoelasticity measuring device can be performed, for example, under the conditions of a temperature rise rate of 2°C / min, a measurement temperature range of room temperature to 200°C, and a deformation frequency of 1 Hz. However, the conditions for measuring the storage modulus are not limited to these. Other measuring devices may also be used to measure the storage modulus.
[0033] Since sheet 27 does not have a glue layer (adhesive layer) and does not have sufficient adhesiveness, it cannot be attached to wafer 11 and annular frame 29 as it is. Sheet 27 has thermoplastic properties, and when it is heated to a temperature near its melting point while being joined to wafer 11 under application of a predetermined pressure, it partially melts and can be fixed to wafer 11. In other words, sheet 27 can be thermocompression bonded to wafer 11.
[0034] 5, the outer periphery of the sheet 27 is fixed to a metal annular frame 29. The annular frame 29 has an opening (through hole) 29a having a diameter larger than the diameter of the wafer 11. For example, the sheet 27 is fixed to the annular frame 29 before the wafer 11 is fixed. The method for fixing the sheet 27 to the annular frame 29 is, for example, thermocompression bonding. For example, the sheet 27 is thermocompression bonded to the annular frame 29 together with the wafer 11. Alternatively, the sheet 27 is attached and fixed to the annular frame 29 by an adhesive or the like.
[0035] Finally, when the wafer 11, the sheet 27, and the annular frame 29 are integrated, a wafer unit 31 (see FIG. 5, etc.) is formed. When the wafer unit 31 is formed, the wafer 11 can be handled via the sheet 27, making it easy to handle the wafer 11. Furthermore, when the wafer 11 that is part of the wafer unit 31 is divided, each of the formed device chips continues to be supported by the sheet 27, making it easy to handle the device chips.
[0036] Next, the thermocompression bonding apparatus 2 used when fixing the sheet 27 to the wafer 11 in the wafer processing method according to this embodiment will be described. However, in the wafer processing method according to this embodiment, the thermocompression bonding apparatus 2 does not necessarily have to be used when fixing the sheet 27 to the wafer 11. Figures 2(A) to 4 include cross-sectional views that typically show the thermocompression bonding apparatus 2.
[0037] 2(A) is a cross-sectional view showing a schematic example of a thermocompression bonding apparatus 2. The thermocompression bonding apparatus 2 is, for example, a chamber-like unit having a space capable of accommodating a wafer 11 therein, and has a function of thermocompression bonding a sheet 27 onto the surface 11a of the wafer 11. The thermocompression bonding apparatus 2 has a lower chamber 6 having a concave shape that opens upward, and an upper chamber 4 having a concave shape that is disposed above the lower chamber 6 and opens downward.
[0038] The upper chamber 4 of the thermocompression bonding apparatus 2 includes a first recess 8 connected to a first decompression unit 20 and having a first opening 12. The lower chamber 6 includes a second recess 10 connected to a second decompression unit 22 and having a second opening 14. The first decompression unit 20 and the second decompression unit 22 are, for example, vacuum pumps such as rotary pumps. However, the first decompression unit 20 and the second decompression unit are not limited thereto.
[0039] The thermocompression bonding apparatus 2 also includes a holding table 32 that is disposed in the second recess 10 and holds the wafer 11. The upper chamber 4 and the lower chamber 6 can be closed by aligning the first opening 12 of the upper chamber 4 and the second opening 14 of the lower chamber 6.
[0040] The thermocompression bonding apparatus 2 will be described in more detail. The first opening 12 of the upper chamber 4 and the second opening 14 of the lower chamber 6 have an inner diameter larger than the diameter of the wafer 11. In addition, the first recess 8 of the upper chamber 4 and the second recess 10 of the lower chamber 6 have an outer diameter smaller than the inner diameter of the annular frame 29 disposed on the outer periphery of the sheet 27.
[0041] For example, the upper chamber 4 can be raised and lowered. The second opening 14 of the lower chamber 6 and the first opening 12 of the upper chamber 4 have the same shape, and when the upper chamber 4 is lowered into the lower chamber 6 so that the first opening 12 overlaps with the second opening 14, a space that is isolated from the outside can be formed inside the upper chamber 4 and the lower chamber 6.
[0042] The lower chamber 6 is provided with a table-shaped holding table 32 that supports the wafer 11. The wafer 11 is placed on the holding table 32 with the back surface 11b, on which the annular convex portion 13 and the circular concave portion 15 are formed, facing downward.
[0043] The upper surface of the holding table 32 is a holding surface 34 that supports and holds the wafer 11 from the back surface 11b side. The holding table 32 may include a suction path (not shown) that communicates with the holding surface 34, and a suction source (not shown) that is connected to the suction path. In this case, when a suction force generated by the suction source is applied to the wafer 11 placed on the holding surface 34 of the holding table 32 through the suction path, the wafer 11 can be suction-held by the holding table 32.
[0044] The holding table 32 includes a circular protrusion 34a that mainly supports the circular recess 15 on the back surface 11b of the wafer 11, and an annular support portion 34b that is arranged on the outer periphery of the circular protrusion 34a and mainly supports the annular protrusion 13 of the wafer 11.
[0045] The planar shape of the upper surface of the circular protrusion 34a is a shape that fits into the circular recess 15 of the wafer 11 and is slightly smaller than the circular recess 15. The annular support 34b has a width (distance between the inner and outer peripheries) that is larger than the width (distance between the inner and outer peripheries) of the annular protrusion 13 of the wafer 11. The difference in height between the upper surface of the annular support 34b and the upper surface of the circular protrusion 34a corresponds to the difference in height between the circular recess 15 of the wafer 11 and the annular protrusion 13. In other words, this difference is appropriately determined based on the heights of the circular recess 15 of the wafer 11 and the step portion 17 (see FIG. 1(B)) of the annular protrusion 13.
[0046] A spacer (not shown) is disposed on the upper surface of the annular support portion 34b. The spacer is formed of an elastic material such as a resin layer, and its thickness changes in response to the variation in the difference in height between the circular recess 15 and the annular protrusion 13 of the wafer 11 (the height of the step portion 17). In other words, the holding table 32 can appropriately hold the wafer 11 while responding to the variation in the difference in height between the circular recess 15 and the annular protrusion 13 of the wafer 11.
[0047] The height of the holding table 32 is adjusted so that when the wafer 11 is placed on the holding surface 34, the surface 11a of the wafer 11 and the second opening 14 of the lower chamber 6 are at substantially the same height. Alternatively, the height of the holding table 32 is adjusted so that the second opening 14 of the lower chamber 6 is higher than the surface 11a of the wafer 11.
[0048] An exhaust unit 24 is connected to the ceiling or side wall of the upper chamber 4. The exhaust unit 24 is an exhaust path having one end connected to the first recess 8 of the upper chamber 4 and the other end connected to the first decompression unit 20. A first solenoid valve 28 (e.g., a solenoid valve) that switches the connection state of the upper chamber 4 and the first decompression unit 20 is provided in the exhaust path of the exhaust unit 24. That is, when the first solenoid valve 28 is operated, the upper chamber 4 and the first decompression unit 20 can be switched between a connected state in which they are connected and a disconnected state in which they are disconnected from each other.
[0049] An exhaust unit 26 is connected to the bottom wall or side wall of the lower chamber 6. The exhaust unit 26 is an exhaust path having one end connected to the second recess 10 of the lower chamber 6 and the other end connected to the second decompression unit 22. A second solenoid valve 30 (e.g., a solenoid valve) that switches the connection state of the lower chamber 6 and the second decompression unit 22 is provided in the exhaust path of the exhaust unit 26. That is, when the second solenoid valve 30 is operated, the lower chamber 6 and the second decompression unit 22 can be switched between a connected state in which they are connected and a disconnected state in which they are disconnected from each other.
[0050] When the first solenoid valve 28 is operated to connect the first decompression unit 20 and the upper chamber 4, the internal space 16 of the upper chamber 4 can be decompressed. When the second solenoid valve 30 is operated to connect the second decompression unit 22 and the lower chamber 6, the internal space 18 of the lower chamber 6 can be decompressed.
[0051] The thermocompression bonding apparatus 2 includes a heating unit that heats the wafer 11 placed on the holding table 32 and the sheet 27 placed on the wafer 11. For example, a heater 36 that can function as a heating unit is disposed inside the holding table 32. The heater 36 is, for example, an electric heating wire. When the heater 36 is operated, the wafer 11 is heated and the sheet 27 is heated through the wafer 11.
[0052] However, the heating unit provided in the thermocompression bonding apparatus 2 is not limited to this. For example, a heating unit (not shown) that supplies hot air to the internal space 16 of the upper chamber 4 may be provided in the first recess 8 of the upper chamber 4. The heating unit includes, for example, a blower that generates an air flow and a heater that can heat the air. The sheet 27 can be heated by placing the wafer 11 on the holding table 32, disposing the sheet 27 on the wafer 11, and supplying hot air to the sheet 27 from the heating unit.
[0053] Next, a cutting device used to remove the annular protrusion 13 of the wafer 11 in the wafer processing method according to this embodiment will be described. Fig. 7(A) includes a perspective view that shows the cutting device, and Fig. 7(B) includes a cross-sectional view that shows the cutting device.
[0054] The cutting device 38 includes a holding table 40 that holds the wafer 11 (wafer unit 31 ), and a cutting unit 50 that cuts the wafer 11 held on the holding table 40 .
[0055] The holding table 40 includes a porous member 44 having a circular upper surface approximately the same size as the front surface 11a of the wafer 11, and a frame 42 that houses the porous member 44 and exposes it upward. The frame 42 has an accommodation recess in its upper surface that houses the porous member 44. A suction path (not shown) is formed inside the frame 42, one end of which is connected to the porous member 44 and the other end of which is connected to a suction source (not shown) such as an ejector.
[0056] When the wafer 11 (wafer unit 31) is placed on the holding table 40 and the suction source is activated, negative pressure acts on the wafer 11 through the suction path and the porous member 44. That is, the wafer 11 is sucked and held on the holding table 40 via the sheet 27. The upper surface of the holding table 40 becomes a holding surface 46.
[0057] A rotary drive source (not shown) such as a motor is connected to the holding table 40, and the rotary drive source rotates the holding table 40 around a rotation axis that is generally parallel to the holding surface 46. Furthermore, a plurality of clamps 48 may be provided around the holding table 40 to grip and fix the annular frame 29 that supports the wafer 11 via the sheet 27.
[0058] A cutting unit 50 for cutting the wafer 11 is disposed above the holding table 40. The cutting unit 50 includes a cylindrical spindle 54 disposed along a direction generally parallel to the holding surface 46 of the holding table 40. An annular cutting blade 56 for cutting the wafer 11 is attached to the tip (one end side) of the spindle 54.
[0059] Further, a base end (the other end side) of the spindle 54 is rotatably accommodated in the spindle housing 52. A rotation drive source (not shown) such as a motor is accommodated in the spindle housing 52, and this rotation drive source (not shown) is connected to the base end of the spindle 54. The cutting blade 56 rotates due to the power transmitted from the rotation drive source via the spindle 54.
[0060] The cutting blade 56 attached to the tip of the spindle 54 may be, for example, a hub-type cutting blade (hub blade). The hub blade is integrally formed with an annular base made of metal or the like and an annular cutting edge 58 formed along the outer periphery of the base. The cutting edge 58 of the hub-type cutting blade is formed of an electroformed grinding stone in which abrasive grains made of diamond or the like are fixed by a bonding material such as a nickel plating layer.
[0061] However, a washer-type cutting blade (washer blade) may also be used as the cutting blade 56. The washer blade is configured with an annular cutting edge 58 in which abrasive grains are fixed by a binder made of metal, ceramics, resin, or the like. In any case, the cutting blade 56 can cut the wafer 11 with the annular cutting edge 58.
[0062] The cutting unit 50 is connected to a moving unit (not shown) so that the position at which the cutting blade 56 cuts into the wafer 11 can be adjusted. In addition, the cutting unit 50 is connected to a lifting unit (not shown) so that the height position of the lower end of the annular cutting blade 58 can be changed.
[0063] Next, a removal unit that removes the annular protrusion 13 separated from the wafer 11 from the sheet 27 in the wafer processing method according to this embodiment will be described. Fig. 8(B) includes a cross-sectional view that shows a schematic view of the removal unit 60. Fig. 8(A) includes a perspective view that shows a schematic view of a portion of the removal unit 60.
[0064] The removal unit 60 has cylindrical arms 62 arranged approximately parallel to the height direction. The arms 62 can be moved in the height direction and horizontal direction by, for example, a ball screw type height movement mechanism (not shown) and a horizontal movement mechanism (not shown), respectively.
[0065] A center portion of a disk-shaped base plate 64 is rotatably connected to a lower end portion of the arm portion 62. A rotation drive source (not shown) such as a motor is built into the arm portion 62. The rotation drive source rotates the base plate 64 in a predetermined direction.
[0066] A plurality of removal claw units 66 are provided on the upper portion of the base plate 64. Each removal claw unit 66 has a linear motion mechanism 68. The linear motion mechanism 68 includes a ball screw mechanism (not shown) that moves an advancing / retracting rod 70 forward and backward.
[0067] The advancing / retracting rod 70 includes a nut portion (not shown) slidably connected to a guide portion of the linear motion mechanism 68. The nut portion is rotatably connected to a ball screw (not shown) of the linear motion mechanism 68. By moving the nut portion back and forth by the linear motion mechanism 68, the advancing / retracting rod 70 advances and retreats along its longitudinal direction. In this embodiment, a plurality of advancing / retracting rods 70 are provided. The positions of the plurality of advancing / retracting rods 70 are point symmetrical with respect to the arm portion 62 as the center.
[0068] One longitudinal end (base end) of a rectangular parallelepiped moving block 72 is fixed to the tip of the advancing / retracting rod 70. The advancing / retracting rod 70 is fixed to the moving block 72 so that the longitudinal direction of the advancing / retracting rod 70 and the longitudinal direction of the moving block 72 are perpendicular to each other in a horizontal plane.
[0069] A cylindrical rotating shaft rod 74 is fixed to the other end (tip) of the moving block 72 so as to extend vertically downward. A removal claw 78 is rotatably connected to the lower end of the rotating shaft rod 74 via a bearing 76.
[0070] The removal claws 78 each have a disk-shaped upper claw 78a and a disk-shaped lower claw 78b, and a cylindrical connecting portion 78c that connects the centers of the upper claw 78a and the lower claw 78b. The upper claw 78a and the lower claw 78b are fixed via the connecting portion 78c.
[0071] 8(A), three removal claws 78 are disposed at approximately equal intervals apart from one another along the circumferential direction of the base plate 64, and three lower claws 78b are used to peel the annular protrusion 13 from the sheet 27 and support the peeled annular protrusion 13 at three points. However, the number of removal claws 78, etc. in the removal unit 60 is not limited to three, and the removal unit 60 may have four or more removal claws 78, etc.
[0072] Next, each step of the wafer processing method according to this embodiment will be described in detail. The wafer processing method according to this embodiment is implemented, for example, as a part of a device chip manufacturing method in which the wafer 11 is divided to form device chips. FIG. 9 is a flowchart showing the flow of each step of the wafer processing method (device chip manufacturing method). The wafer processing method according to this embodiment will be described below, but the following description also describes each step of the device chip manufacturing method.
[0073] In the wafer processing method according to this embodiment, first, a wafer unit forming step S10 is performed. In the wafer unit forming step S10, a sheet 27 without a glue layer is fixed to the front surface 11a of the wafer 11, and an annular frame 29 is fixed to the outer periphery of the sheet 27 to form a wafer unit 31. Below, the wafer unit forming step S10 will be described in stages.
[0074] 2(B) is a cross-sectional view showing a schematic diagram of the thermocompression bonding apparatus 2 and the wafer 11 in the first stage of the wafer unit formation step S10. In the first stage of the wafer unit formation step S10, the back surface 11b of the wafer 11 is faced downward and moved above the holding table 32 so that the back surface 11b of the wafer 11 faces the holding surface 34 of the holding table 32.
[0075] Then, the wafer 11 is placed on the holding surface 34 of the holding table 32, and the suction source of the holding table 32 is operated to suction-hold the wafer 11 on the holding table 32. More specifically, the circular recess 15 on the back surface 11b side of the wafer 11 is placed on the circular protrusion 34a of the holding table 32, and the annular protrusion 13 on the back surface 11b side of the wafer 11 is placed on the annular support portion 34b of the holding table 32, and the wafer 11 is suction-held on the holding table 32. At this time, the front surface 11a to which the sheet 27 is thermocompression-bonded is exposed upward.
[0076] Next, in the second stage of the wafer unit formation step S10, the sheet 27 is sandwiched between the upper chamber 4 and the lower chamber 6 of the thermocompression bonding apparatus 2 to seal the internal space 16 of the upper chamber 4 and the internal space 18 of the lower chamber 6. Fig. 3(A) is a cross-sectional view that typically shows the thermocompression bonding apparatus 2 in the second stage of the wafer unit formation step S10.
[0077] An annular frame 29 (see FIG. 5, etc.) may be fixed in advance to the outer periphery of the sheet 27. The sheet 27 is fixed to the annular frame 29 by thermocompression bonding, in which the sheet 27 is heated and pressed against the annular frame 29. Alternatively, the sheet 27 may be thermocompression bonded to the annular frame 29 at the same time as the wafer 11 is thermocompression bonded to the sheet 27.
[0078] Also, an adhesive material may be sandwiched between the annular frame 29 and the sheet 27, and the annular frame 29 and the sheet 27 may be adhered to the annular frame 29 by the adhesive material. Alternatively, the sheet 27 may be provided with a glue layer only on the outer periphery, and attached to the annular frame 29 by the glue layer.
[0079] In the second stage of the wafer unit formation step S10, a frame unit having an annular frame 29 having an opening 29a in the center capable of accommodating a wafer 11, and a sheet 27 having an outer periphery fixed to the annular frame 29, is placed on the lower chamber 6. At this time, the second opening 14 of the lower chamber 6 is blocked by the sheet 27. At this time, the position of the annular frame 29 is adjusted so that the annular frame 29 does not overlap with the first opening 12 and the second opening 14.
[0080] Then, the upper chamber 4 is lowered to sandwich the sheet 27 of the wafer unit 31 between the first opening 12 of the first recess 8 and the second opening 14 of the second recess 10 inside the opening 29a of the annular frame 29, thereby closing the first recess 8 and the second recess 10. At this time, the internal space 16 of the upper chamber 4 is sealed by the sheet 27 and the first recess 8. In addition, the internal space 18 of the lower chamber 6 is sealed by the sheet 27 and the second recess 10.
[0081] Next, in a third stage of the wafer unit formation step S10, the first recess 8 is depressurized by the first depressurization unit 20, and the second recess 10 is depressurized by the second depressurization unit 22. Fig. 3(B) is a cross-sectional view that typically shows the thermocompression bonding apparatus 2 in the third stage of the wafer unit formation step S10.
[0082] In the third stage of the wafer unit formation step S10, the first solenoid valve 28 is operated to connect the first decompression unit 20 and the upper chamber 4. Then, the first decompression unit 20 evacuates the internal space 16 of the first recess 8 of the upper chamber 4 through the exhaust part 24, and the internal space 16 is decompressed. Then, the second solenoid valve 30 is operated to connect the second decompression unit 22 and the lower chamber 6. Then, the second decompression unit 22 evacuates the internal space 18 of the second recess 10 of the lower chamber 6 through the exhaust part 26, and the internal space 18 is decompressed.
[0083] Next, in the fourth stage of the wafer unit formation step S10, the pressure in the first recess 8 is increased to bring the sheet 27 into contact with the front surface 11a of the wafer 11. For example, the sheet 27 is pressed into contact with the wafer 11 by utilizing the pressure difference between the top and bottom of the sheet 27. Figure 4 is a cross-sectional view that typically shows the thermocompression bonding apparatus 2 in the fourth stage of the wafer unit formation step S10.
[0084] In the fourth stage of the wafer unit formation step S10, first, the decompression of the upper chamber 4 by the first decompression unit 20 is stopped. That is, the first solenoid valve 28 is operated to disconnect the first decompression unit 20 from the upper chamber 4. At this time, the second solenoid valve 30 is not operated, and the connection between the second decompression unit 22 and the lower chamber 6 is maintained. In this case, the pressure in the internal space 16 of the upper chamber 4 gradually increases.
[0085] Furthermore, the thermocompression bonding apparatus 2 may be capable of connecting the upper chamber 4 to the outside air through the exhaust unit 24 or the like. In this case, when the upper chamber 4 is connected to the outside air, air flows into the internal space 16 rapidly, and the pressure in the internal space 16 of the upper chamber 4 rapidly increases.
[0086] When the pressure in the internal space 16 of the upper chamber 4 becomes higher than the pressure in the internal space 18 of the lower chamber 6, a downward force is applied to the sheet 27 separating the internal space 16 and the internal space 18. Then, the sheet 27 is pressed toward the surface 11a of the wafer 11.
[0087] In the fourth stage of the wafer unit formation step S10, the sheet 27 is pressed downward to contact the front surface 11a of the wafer 11. Alternatively, the sheet 27 is already in contact with the front surface 11a of the wafer 11 at the start of the fourth stage of the wafer unit formation step S10, and the sheet 27 is pressed toward the wafer 11 in this fourth stage.
[0088] When the fourth stage of the wafer unit formation step S10 is completed, there is no force acting between the sheet 27 and the wafer 11 that is large enough to fix them together. Therefore, in order to fix the sheet 27 to the wafer 11, the sheet 27 is heated and thermocompressed to the surface 11a of the wafer 11.
[0089] Next, as a fifth stage of the wafer unit formation step S10, the heating unit of the thermocompression bonding apparatus 2 is operated to heat the sheet 27. For example, if the thermocompression bonding apparatus 2 has a heater 36 as a heating unit, the heater 36 is operated to heat the sheet 27 together with the wafer 11.
[0090] When sheet 27 is heated to a temperature near its melting point in a state in which sheet 27 is pressed toward wafer 11 due to the pressure difference between internal space 16 of first recess 8 and internal space 18 of second recess 10, sheet 27 is thermocompression-bonded to wafer 11. After sheet 27 is thermocompression-bonded, the heating unit (heater 36) is stopped, and heating of sheet 27 is stopped.
[0091] When performing thermocompression bonding, sheet 27 is preferably heated to a temperature equal to or lower than its melting point. If the heating temperature exceeds the melting point, sheet 27 may melt and become unable to maintain its shape. Furthermore, sheet 27 is preferably heated to a temperature equal to or higher than its softening point. If the heating temperature does not reach the softening point, thermocompression bonding cannot be performed appropriately. In other words, sheet 27 is preferably heated to a temperature equal to or higher than its softening point and equal to or lower than its melting point.
[0092] Furthermore, some sheets 27 may not have a clear softening point. Therefore, when performing the thermocompression bonding, the sheet 27 is preferably heated to a temperature that is at least 20° C. lower than its melting point and is at most its melting point.
[0093] For example, when the polyolefin sheet used as sheet 27 is a polyethylene sheet, the heating temperature is preferably 120° C. to 140° C. When the polyolefin sheet is a polypropylene sheet, the heating temperature is preferably 160° C. to 180° C. When the polyolefin sheet is a polystyrene sheet, the heating temperature is preferably 220° C. to 240° C.
[0094] Furthermore, for example, when the polyester-based sheet used as sheet 27 is a polyethylene terephthalate sheet, the heating temperature is set to 250° C. to 270° C. When the polyester-based sheet is a polyethylene naphthalate sheet, the heating temperature is set to 160° C. to 180° C. However, the heating temperature of sheet 27 is not limited to these.
[0095] The heating unit is stopped to stop heating the sheet 27, the second solenoid valve 30 is operated to disconnect the second decompression unit 22 and the lower chamber 6, the pressure in the internal space 18 of the lower chamber 6 is returned to atmospheric pressure, and then the upper chamber 4 is raised. Then, as shown in Fig. 5, a wafer unit 31 is obtained in which the sheet 27, the wafer 11, and the annular frame 29 are integrated together. This completes the wafer unit formation step S10.
[0096] In the wafer processing method according to this embodiment, after the wafer unit forming step S10, a holding step S20 is performed in which the wafer 11 is held on a holding table 40 of a cutting device 38 via a sheet 27. Fig. 6(A) is a perspective view that typically shows the wafer unit 31 in the holding step S20, and Fig. 6(B) is a cross-sectional view that typically shows the wafer unit 31 in the holding step S20.
[0097] In the holding step S20, the wafer unit 31 is carried out from the thermocompression bonding apparatus 2, and the wafer unit 31 is placed on the holding table 40 of the cutting apparatus 38. At this time, the position of the wafer 11 is adjusted so that the front surface 11a side of the wafer 11 faces the holding surface 46 and the center of the holding surface 46 and the center of the front surface 11a of the wafer 11 overlap with each other.
[0098] Thereafter, the suction source (not shown) of the holding table 40 is operated to suction-hold the wafer 11 on the holding table 40 via the sheet 27. Also, the annular frame 29 of the wafer unit 31 is gripped by clamps 48 disposed on the outer periphery of the holding table 40. As a result, the back surface 11b side of the wafer 11 is exposed upward.
[0099] In the wafer processing method according to this embodiment, after the holding step S20, a dividing step S30 is performed in which a dividing groove is formed in the circular recess 15 of the wafer 11 and the annular protrusion 13 is separated from the wafer 11. Fig. 7(A) is a perspective view showing a cutting device 38 in the dividing step S30, and Fig. 7(B) is a cross-sectional view showing a cutting device 38 in the dividing step S30. Figs. 8(A) and 8(B) show a dividing groove 33 formed in the wafer 11.
[0100] The position where the dividing groove 33 of the wafer 11 is to be formed is set in a circular region centered on the center of the circular recess 15. In particular, the position where the dividing groove 33 is to be formed is adjusted so that the cutting edge 58 does not cut into the step portion 17 between the annular convex portion 13 and the circular recess 15 shown in Fig. 1(A). In the dividing step S30, first, the cutting unit 50 is moved so that the cutting edge 58 of the cutting blade 56 is positioned above the region where the dividing groove 33 is to be formed.
[0101] Next, the rotary drive source provided inside the spindle housing 52 is operated to start the rotation of the cutting blade 56, and the cutting unit 50 is lowered to make the cutting edge 58 cut into the wafer 11. Then, the cutting unit 50 is lowered to a height position where the lower end of the cutting edge 58 reaches the sheet 27, and the holding table 40 starts to rotate. Then, when the holding table 40 rotates once or more, a circular separation groove 33 is formed in the wafer 11, and the annular convex portion 13 is separated from the wafer 11. In other words, the annular convex portion 13 and the circular concave portion 15 are separated.
[0102] When the cutting unit 50 cuts the wafer 11, cutting chips and frictional heat are generated from the wafer 11 and the cutting edge 58 of the cutting blade 56. Therefore, when the cutting blade 56 cuts into the wafer 11, cutting water composed of pure water or the like is supplied to the cutting blade 56 and the wafer 11. Then, the cutting chips and frictional heat generated by cutting the wafer 11 are taken in and removed by the cutting water.
[0103] Here, unlike the wafer processing method according to the present embodiment, when a dicing tape with a glue layer is used instead of the sheet 27, the cutting chips may adhere to the glue layer when the cutting water containing the cutting chips reaches the dicing tape. In this case, the cutting chips may separate from the dicing tape in a subsequent process, and may reach and adhere to the wafer 11. If the cutting chips adhere to the wafer 11, this causes a problem because it reduces the quality of the device chips formed from the wafer 11.
[0104] In contrast, in the wafer processing method according to this embodiment, sheet 27 does not have a glue layer. Therefore, even if cutting water that has taken in cutting debris reaches sheet 27, the cutting debris is unlikely to adhere to sheet 27. Even if cutting debris adheres to sheet 27, the cutting debris is easily removed from sheet 27. Therefore, the transfer of cutting debris from sheet 27 to wafer 11 is unlikely to occur, and the quality degradation of device chips due to cutting debris is unlikely to occur.
[0105] In the wafer processing method according to this embodiment, after the dividing step S30, a removing step S40 is performed in which the annular convex portion 13 separated from the wafer 11 is removed from the sheet 27. Fig. 8(A) is a perspective view that typically shows the wafer unit 31 in the removing step S40, and Fig. 8(B) is a cross-sectional view that typically shows the wafer unit 31 and the removing unit 60 in the removing step S40.
[0106] 8(B) includes a cross-sectional view showing the annular protrusion 13 when it is removed from the sheet 27 in the removal step S40. After the annular protrusion 13 is cut off from the wafer 11, the annular protrusion 13 is pulled up and peeled off from the sheet 27. Then, the portion of the wafer 11 that was the circular recess 15 remains on the sheet 27. That is, a wafer unit 31 is obtained in which the wafer 11 from which the annular protrusion 13 has been removed, the sheet 27, and the annular frame 29 are integrated together. The wafer 11 is then divided to obtain individual device chips.
[0107] The removing step S40 is performed, for example, by the function of the removing unit 60. The removing unit 60 is incorporated, for example, in the cutting device 38. However, the removing unit 60 does not have to be incorporated in the cutting device 38, and the removing step S40 may be performed outside the cutting device 38. Below, the removing step S40 will be described taking as an example a case where the removing unit 60 is incorporated in the cutting device 38 and the removing step S40 is performed by the removing unit 60 on the holding table 40.
[0108] 8(A) and 8(B), for example, the removing step S40 is performed on the holding table 40 following the dividing step S30. In the removing step S40, first, the base plate 64 of the removing unit 60 is placed above the wafer 11. Then, the base plate 64 is lowered with the removing claws 78 protruding outward so that the removing claws 78 are positioned outside the wafer 11.
[0109] The arm 62 is lowered until the lower claws 78b of the removal claws 78 are positioned at the boundary between the sheet 27 and the annular protrusion 13, and then the lowering is stopped. Next, the removal claws 78 are moved toward the inside of the base plate 64. At this time, the lower claws 78b are moved inward by, for example, 1.6 mm from the outer circumferential edge of the wafer 11. In the removal step S40, the removal claws 78 are inserted into the boundary between the sheet 27 and the annular protrusion 13 with the multiple removal claws 78 positioned approximately evenly spaced apart from one another along the circumferential direction of the wafer 11.
[0110] Next, the base plate 64 is rotated around the arm 62 as a rotation axis to rotate the multiple removal claws 78 along the outer periphery of the wafer 11, while the arm 62 and the base plate 64 are raised to move the multiple removal claws 78 upward. The rotation speed of the removal claws 78 is, for example, 10° / s, and each removal claw 78 is rotated 140° over 14 seconds. The lifting speed of the removal claws 78 is, for example, 0.14 mm / s. The annular protrusion 13 is removed from the sheet 27 (wafer unit 31) as a result of the annular protrusion 13 being separated from the sheet 27.
[0111] In this embodiment, the operation of rotating the multiple removal claws 78 around the wafer 11 and the operation of moving the multiple removal claws 78 upward are performed in combination, so that the time required to remove the annular protrusion 13 from the sheet 27 can be shortened compared to when each operation is performed individually.
[0112] In addition, since the annular projection 13 is moved in a predetermined direction away from the sheet 27 as the removal claw 78 rotates, there is an advantage that the annular projection 13 will not reattach to the sheet 27.
[0113] Furthermore, the removal claw 78 has an upper claw 78a in addition to a lower claw 78b. The annular protrusion 13 that has been peeled off from the sheet 27 may rise vigorously, but by providing the upper claw 78a, the rise of the annular protrusion 13 can be limited to the range between the upper claw 78a and the lower claw 78b. This makes it possible to prevent the annular protrusion 13 from falling.
[0114] When removing the annular protrusion 13 from the sheet 27 in this manner, an excessive load may occasionally be applied to the annular protrusion 13, causing cracks or chips in the annular protrusion 13. The resulting chips and fragments may fall onto the sheet 27 between the wafers 11 of the wafer unit 31 and the annular frame 29.
[0115] However, since the sheet 27 does not have an adhesive layer, debris, pieces, etc. do not stick to the sheet 27. For example, when the wafer unit 31 is washed with a washing device, etc., such debris, pieces, etc. are very easily removed and do not remain on the sheet 27.
[0116] Also, unlike when the annular protrusion 13 is strongly attached to an adhesive tape by an adhesive layer, it is relatively easy to remove the annular protrusion 13 when it is fixed to the sheet 27 that does not have an adhesive layer. Therefore, a large force is not applied to the annular protrusion 13 to be removed, and it is unlikely to break or produce fragments. Therefore, fragments do not scatter and adhere to the device chips formed by dividing the wafer 11, and deterioration of the quality of the device chips is prevented.
[0117] Furthermore, there is no need to irradiate the sheet 27 with ultraviolet rays in order to remove the annular protrusion from the sheet 27, and there is no need to narrow the area used for device formation on the front surface 11a of the wafer 11 on the assumption that ultraviolet rays will be irradiated. Therefore, the productivity of device chips is also improved.
[0118] In the above embodiment, the dividing step S30 is described as forming the dividing grooves 33 in the wafer 11 using the cutting device 38 equipped with the cutting blade 56, but one aspect of the present invention is not limited to this. That is, in the dividing step S30, a laser processing device (not shown) capable of irradiating the wafer 11 with a laser beam to laser-process the wafer 11 may be used.
[0119] For example, a laser beam including a wavelength component absorbed by the wafer 11 is irradiated onto an area of the wafer 11 where the dividing groove 33 is to be formed, thereby ablation processing the wafer 11. Alternatively, a laser beam including a wavelength component that transmits through the wafer 11 is focused onto an area of the wafer 11 where the dividing groove 33 is to be formed, a modified layer is formed on the wafer 11 along that area, and the wafer 11 is divided using the modified layer as the dividing starting point.
[0120] Even in these cases, according to the wafer processing method according to one aspect of the present invention, the annular convex portion 13 cut out from the wafer 11 can be easily removed from the sheet 27. At this time, no large load is applied to the annular convex portion 13, and even if the annular convex portion 13 is broken or the like and fragments fall onto the sheet 27, the fragments are easily removed from the sheet 27. Therefore, the fragments do not adhere to the device chip later, and a high-quality device chip is formed.
[0121] In addition, the structures, methods, and the like according to the above-described embodiments and modifications may be modified as appropriate without departing from the scope of the present invention. The above-described embodiments and modifications may be combined as appropriate. [Explanation of symbols]
[0122] 11 Wafers 11a surface 11b Back side 13 Annular protrusion 15 Circular recess 17 Step 19 Division line 21 Devices 23 Surplus outer area 25 Device Formation Area 27 sheets 29 Annular Frame 29a opening 31 Wafer Unit 33 Dividing Trenches 2 Thermocompression bonding equipment 4 Upper chamber 6 Lower Chamber 8 First recess 10 Second recess 12 First opening 14 Second opening 16,18 Interior space 20 First decompression unit 22 Second decompression unit 24 Exhaust section 26 Exhaust section 28 First solenoid valve 30 Second solenoid valve 32 Holding Table 34 Holding surface 34a Circular protrusion 34b Annular support 36 Heater 38 Cutting equipment 40 Holding Table 42 Frame 44 Porous Materials 46 Holding surface 48 Clamp 50 Cutting Unit 52 Spindle housing 54 Spindle 56 Cutting Blade 58 Cutting edge 60 Removal Units 62 Arm 64 Base plate 66 Removal Claw Unit 68 Linear motion mechanism 70 Advance / retract rod 72 Moving Blocks 74 Rotating shaft rod 76 Bearing 78 Removal nail 78a Upper claw 78b Lower claw 78c Connection
Claims
1. A method for processing a wafer having an annular convex portion on an outer periphery of a rear surface and a circular concave portion formed in an area of the rear surface surrounded by the annular convex portion, comprising the steps of: a wafer unit forming step of forming a wafer unit by fixing a sheet having no adhesive layer on the surface of the wafer and fixing an annular frame to an outer periphery of the sheet; a holding step of holding the wafer on a holding table via the sheet after the wafer unit forming step; a dividing step of forming a dividing groove in the circular recess of the wafer after the holding step and separating the annular protrusion from the wafer; a removing step of removing the annular convex portion from the sheet after the dividing step.
2. 2. The method for processing a wafer according to claim 1, wherein in the wafer unit forming step, the sheet is fixed to the wafer by heating and pressing the sheet to thermocompression bond the sheet to the wafer.
Citation Information
Patent Citations
Method of processing wafer and device
JP2007173487A
Method of processing wafer, and apparatus for removing annular projection
JP2011061137A
Wafer processing method
JP2012054275A