Automotive window laminate structure, thermoplastic laminate sheet structure for use in an automotive window laminate structure, and method for producing the automotive window laminate structure by a hot press lamination process
The frameless automotive window laminate structure with a thermoplastic laminate sheet and bonding layers addresses the challenges of thick functional layers by providing easier manufacturing, improved sealing, and reduced weight, ensuring longevity and functional integrity.
Patent Information
- Application Number
- JP2024527559
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-15
- Filing Date
- 2022-11-14
- Publication Date
- 2024-12-05
AI Technical Summary
Automotive window laminate structures face challenges with thick functional layers that are difficult to automate, heavy, and prone to environmental degradation due to gaps in sealing, which affects their longevity and manufacturing efficiency.
A frameless design using a thermoplastic laminate sheet structure with bonding layers that extend around the functional layer, forming a seal to prevent moisture ingress, and using thinner functional layers with specific bonding materials like TPU and EVA to reduce wrinkles and weight.
The solution enables easier manufacturing, improved sealing, reduced weight, and enhanced durability of automotive window laminates by eliminating the need for frame layers and minimizing wrinkles, while maintaining functional integrity.
Smart Images

Figure 2024544926000001_ABST
Abstract
Description
[Technical field]
[0001] SUMMARY OF THE DISCLOSURE The present invention relates to automotive window laminate structures, thermoplastic laminate sheet structures for use in automotive window laminate structures, and methods for producing automotive window laminate structures by a heat and pressure lamination process. [Background technology]
[0002] Nowadays, functional layers comprising at least one active film layer such as polymer dispersed liquid crystal (PDLC), electrochrome and other functional films such as suspended particle devices (SPD) are widely used in architectural glass, but also, more exceptionally, in the automotive industry. There are several reasons for this, because, in general, the automotive industry has high demands, both in terms of safety regulations and quality issues. By way of example, approval in the automotive industry requires passing not only destructive tests such as dropping a steel ball from a certain height onto the window laminate structure, but also less destructive tests such as optical performance and boiling tests.
[0003] All active or functional layers such as SPD, PDLC or electrochrome have in common that they are constructed from two opposing thermoplastic layers, often ITO-coated PET, PEN, PC or PMMA layers, provided with a conductive coating on the mutually facing faces, with an active film layer between them. All have in common that when an electric current flows from the first conductive layer through the liquid crystal to the second conductive layer, the crystals orient with the electric current, resulting in a change in color, light transmission and / or haze level. When such a layer is incorporated into a laminated glass structure, it is referred to as a functional layer, in particular an active functional layer. The incorporation is generally carried out by a lamination process using a tie layer and a frame layer. In this respect, the term "active" can be understood as a layer having an active functionality, such as being switchable between different states, for example between a state in which the layer is substantially transparent and a state in which the layer is substantially opaque or between transparent and opaque.
[0004] Generally, the thermoplastic laminated sheet structure with the functional layer and the bonding layer does not extend to the edge of the glass sheets of the automotive window laminated structure. In fact, the encapsulation around the thermoplastic laminated sheet structure is present to prevent the glass sheets from breaking. Especially in the areas where there is no functional layer allocated between the glass sheets and where the bonding layer extends beyond the functional layer, the openings / gaps in these areas need to be compensated in terms of thickness. The reason why the functional layer does not extend to the edge of the glass sheets is mainly to prevent weather conditions, moisture, oxygen, salt (from coastal environments or road deicing), window wiping liquid, etc. from coming into contact with the functional layer or with the conductive coating of either of its layers. Contact between such environments and the thermoplastic laminated structure may cause the laminated structure to fail or even to fail altogether. In particular, moisture and plasticizers may affect the molecular structure of the active film of the functional layer. Generally, said functional layer has a thickness comparable to that of the bonding layer. A separate PVB frame layer is used to fill the gap between the two bonding layers where no functional layer is present. This prevents the glass from breaking, but does not properly seal the functional layer, which can result in moisture or other undesirable elements penetrating from around the frame layer, which can affect the lifespan of the functional layer as described.
[0005] A current trend in automobiles is the reduction of the weight of components. This trend is also present in window structures. This is particularly challenging considering the requirements set for those structures regarding safety. In general, the functional layers of automotive window laminate structures are relatively thick. However, this has three disadvantages. Firstly, thick functional layers require a frame layer to prevent the glass from breaking. Placing such a frame layer is a process that is difficult to automate and has to be done very carefully, which slows down production. Secondly, these thicker functional layers are very heavy, which is a disadvantage for the automotive industry. Thirdly, typical functional layers have the disadvantage that it is difficult to seal them from the environment, which is caused by the fact that they have to be sealed in the frame layer, which can prevent the frame layer from being applied correctly. Summary of the Invention
[0006] SUMMARY OF THE PRESENT EMBODIMENT It is therefore a primary object of the present invention to provide an automotive window laminate structure of simpler composition.
[0007] A second object of the present invention is to provide an automobile window laminate structure having improved sealing properties of a functional layer.
[0008] In contrast, the present invention proposes an automotive window laminate structure, comprising a first glass sheet and a second glass sheet, which are parallel and spaced apart from each other, a thermoplastic laminate sheet structure arranged substantially entirely between the first and second glass sheets, the thermoplastic laminate sheet structure comprising at least one functional layer, in particular an active functional layer, having an upper surface and a lower surface, at least two bonding layers, the at least two bonding layers substantially entirely covering the upper and lower surfaces of the at least one functional layer, and a seal configured around the periphery of the thermoplastic laminate sheet structure, in particular the functional layer, for sealing the thermoplastic laminate sheet structure from the environment, the thermoplastic laminate sheet structure extending substantially entirely around the periphery of the first and second glass sheets, the seal being at least partially formed by at least one, preferably both, of the at least two bonding layers along at least a portion of the periphery of the thermoplastic laminate sheet structure.
[0009] The invention thereby allows easier construction of automotive window laminates. Since the thermoplastic laminate sheet structure extends substantially entirely around the first and second glass sheets, no frame layer is required. In other words, the invention relates to a frameless automotive window laminate structure. According to the prior art, a frame layer is present to ensure proper positioning and sealing of the functional layer, but the invention allows this result to be achieved without said frame layer. To enable this, a seal around the periphery of the thermoplastic laminate sheet structure, in particular the functional layer, is at least partially formed by at least one, preferably both bonding layers. In this way, the thermoplastic laminate sheet structure can be positioned around the periphery of the glass sheets, the bonding layers achieving said sealing of the functional layer. Preferably, the seal extends along the entire periphery of the thermoplastic laminate sheet structure, and substantially the entire seal is formed by at least one, preferably two bonding layers. The bonding layers may substantially hermetically surround all sides of the functional layer, and it is conceivable that the bonding layers are in particular directly bonded to all sides of the functional layer so as to form a single homogenous bonding layer enclosure.
[0010] If the seal is partially formed by a bonding layer, there are some further preferences. For example, it is preferred in this respect that at least one bonding layer extends at least partially beyond the periphery of the functional layer. In this way, the bonding layer can seal the portion of the functional layer beyond which it lies. In particular, this embodiment is advantageous when a thermoplastic polyurethane (TPU) is used as the bonding layer. This allows for easier formation of the seal and reduces the cost of the established window laminate.
[0011] It is conceivable and preferred that at least one functional layer is an active layer. In particular, the active functional layer is switchable between a partially transparent state and a partially opaque state. Alternatively, it is conceivable that the active functional layer is configured to switch between different colors. Preferably, the at least one active functional layer is switchable based on a current and / or a voltage applied to the anode and cathode of the functional layer. It is further conceivable that the functional layer comprises segments or crossing segments forming pixels, the segments and / or pixels being switchable independently of each other.
[0012] Preferably, the automotive window laminate structure is a curved automotive window laminate structure. The invention is more advantageous when the glass sheet has at least a single curvature, and optionally the window laminate structure may be a double-curved window laminate structure. The advantageous effects of the invention are even more pronounced in this case. The greater the curvature, the more difficult it is to apply the frame layer around the thermoplastic laminate sheet structure. Also, when the window laminate structure is curved, it is more difficult to apply the seal, which has to do with the fact that a single seal is preferably used, which is typically a piece of Kapton tape. However, it is difficult to warp a single piece of tape without causing wrinkles around the curved thermoplastic laminate sheet structure. On the other hand, when multiple pieces of tape are used, the seal creates areas that are prone to moisture penetration into the thermoplastic laminate sheet structure. On the other hand, the invention solves this problem, since the bonding layer realizes the seal, which is less prone to wrinkles. In particular, since the bonding layer can realize the seal of the functional layer with each other when the bonding layer is brought under conditions that allow them to change shape, such as increased temperature and / or pressure.
[0013] These thicker functional layers suffer from a number of disadvantages, but replacing them with thinner functional layers while still meeting the same automotive requirements is laborious. Thin functional layers are prone to undulations or wrinkles under the pressure lamination process. Waviness or wrinkles can easily be introduced into the laminate, especially when the window has a curvature or double curvature. These waviness or wrinkles can prevent the functional layer from working properly. Especially when such thinner functional layers are applied to large automotive window laminates, excessive wrinkles can be introduced by the pressure lamination process, which affects the parallelism of the active film of the functional layer. The wrinkles are generally oriented in the maximum direction of the functional layer. In addition to the wrinkles, thinner functional layers are more difficult to seal from the environment using the features of the current technology. Therefore, a further object of the present invention is to make the functional layer lighter.
[0014] In a different embodiment of the invention, the thickness of the functional layer is less than 0.30 mm, preferably less than 0.20 mm. More specifically, the functional layer has a thickness of less than 0.15 mm. By using such kind of functional layer, a significant weight reduction can be realized. Preferably, the functional layer of the automotive window laminate structure has a thickness of less than 1000 cm 2 More than 1500cm, preferably 1500cm 2 More preferably, 2000 cm 2 In particular, the functional layer has a surface area of 1000 cm 2 More than 1500cm, preferably 1500cm 2 More preferably, 2000 cm 2 or more. In particular, it has been found that combinations of large functional layers and / or thermoplastic sheets with a thickness of less than 0.30 mm, preferably less than 0.20 mm, are difficult to laminate. For this purpose, preferably at least two bonding layers covering the upper and lower surfaces of the functional layers are composed of ethylene-vinyl acetate (EVA) or thermoplastic polyurethane (TPU). It is conceivable that bonding layers composed of different materials are used, as long as the thermoplastic properties of the different materials are similar to those of TPU and EVA, both of which have relatively low softening points.
[0015] For this purpose, it has been found that the use of polyvinyl butyral (PVB) as a material for the tie layer does not meet the desired results when relatively large and thin functional layers are used. The use of PVB as a tie layer is not suitable for achieving a substantially airtight seal of the functional layers. It has also been found that the softening temperature of PVB is high compared to that of TPU and EVA, making it unsuitable for use in the automotive window laminate structure according to the present invention. However, if a PVB tie layer with a lower softening temperature and preferably even crosslinking becomes available, said future PVB may be considered suitable. In particular, wrinkling of the thin functional layer may not be sufficiently suppressed with PVB. It has been found that the use of TPU and / or EVA provides reliable results with a minimal amount of wrinkling of the functional layer. PVB may not be used according to the present invention as the first set of tie layers, i.e. as the pair of tie layers that are directly applied to the functional layers, but it is conceivable that further pairs of tie layers are provided. This further pair of tie layers, which may be applied to the outer surface of the first pair of tie layers, may be made of any tie layer material, including PVB. If PVB is used as a further tie layer, i.e., directly or indirectly applied to at least one of the main tie layers, the first tie layer should be TPU. It has been found that the combination of EVA and further PVB layers is not mutually compatible. Surprisingly, if at least one thermoplastic layer of the functional layer is thicker than the other layer, at least one tie layer of PVB may be used, instead of both tie layers being TPU or EVA. In particular, one PET layer may be, for example, 180 microns or 150 microns, while the other PET layer is, for example, 100 microns, preferably 50 microns. The PVB layer may in this case be on the side of the thicker PET layer. Preferably, the TPU tie layer is provided on the side of the functional layer facing away from the PVB tie layer. The combination of TPU and PVB tie layers is particularly advantageous because the PVB can provide enhanced structural performance while the TPU can allow for enhanced sealing, especially when the functional layer has a cascading edge where the PET layer on the PVB side extends beyond the edge of the PET layer on the TPU side.This cascade configuration allows the use of a thin functional layer while preventing wrinkles from forming due to the use of TPU on the side of the thin thermoplastic PET layer. Nevertheless, the use of PVB, which is cheaper and can be more easily colored, does not affect wrinkles because it is applied to the thicker thermoplastic PET layer. Thus, the seal is realized by the TPU. Furthermore, the thicker PET layer can act as a flat printed circuit and as a barrier against the plasticizers of the PVB.
[0016] When both bonding layers are made of TPU, a proper seal of the functional layer with a thermoplastic PET layer of 50 microns thickness can be achieved. This allows the formation of a very thin functional layer while preventing the formation of wrinkles between the glass sheets due to the TPU. This configuration can also eliminate the need for a concealment band, which is usually made of black ceramic enamel. Thus, a more aesthetic finish of the automotive window can be achieved by using two TPU bonding layers. That is, a frame layer is not required since the seal can be formed by the TPU bonding layer.
[0017] Preferably, the surface area of the functional layer of the automotive window laminate structure is greater than 1000 cm 2 ~16000cm 2It has been found that for this particular size of window, wrinkles are likely to form in the thermoplastic laminated sheet structure, especially in its functional layer. This problem is more pronounced when using thin thermoplastic laminated sheet structures. In particular, the total thickness of the thermoplastic laminated sheet structure without the bonding layer is in the range of up to 0.1 mm, up to 0.40 mm, preferably up to 0.25 mm. In particular, said wrinkles may form during the lamination of the window and be visible in the final product. This is undesirable as it affects the appearance of the product. Surprisingly, it has been found that the use of at least one specific bonding layer, such as TPU and / or EVA, can eliminate the cause of wrinkles forming in the thermoplastic laminated sheet structure, and thus the cause of wrinkles in the above dimensions of the window. In this respect, the TPU or EVA bonding layer should be directly attached to the functional layer to prevent wrinkles from forming. The TPU or EVA bonding layer is provided on the side of the functional layer facing away from the thick PET layer, when at least one thick PET layer is used as described above. A functional layer with a thin PET layer is more prone to wrinkle formation under the heat of the lamination process, especially when using a thinner PET layer, such as 50 microns to 150 microns thick, in combination with a PVB tie layer adjacent to the thin PET layer. The thin PET layer and the adjacent PVB tie layer have mutually incompatible viscosity parameters during the lamination process, which may cause friction between the layers during the lamination process. Thus, the combination of a TPU or EVA tie layer with a thin PET layer has surprising results, showing a particular compatibility between the thin PET layer of the functional layer and the adjacent TPU or EVA tie layer, especially the TPU tie layer. Optionally, even better results are obtained by pre-bonding the tie layer and the functional layer. An example of a TPU tie layer is model number SF1959 high modulus or SF1964 low modulus manufactured by NovoGenio. The latter for the example is physically crosslinked during the manufacture of the tie layer.
[0018] Preferably, the functional layer is less than 0.30 mm, preferably less than 0.20 mm. By using a relatively thin functional layer, it is possible to achieve hermetic sealing of the functional layer with the bonding layer without the presence of a frame layer. That is, the functional layer extends almost entirely around the glass. This is possible due to the thinness of the functional layer, which overcomes the limited thickness of the bonding layer when softening, and thus eliminates the need to fill gaps between the bonding layers. Preferably, the functional layer is an SPD or electrophoretic layer with a thickness of 10 to 100 microns. More preferably, the functional layer is an electrochrome or PDLC layer with a thickness of 2 to 40 microns. The functional layer may comprise, for example, two thermoplastic layers and one film layer or active layer. Preferably, at least one functional layer comprises at least two thermoplastic layers and at least one film layer between the at least two thermoplastic layers, the film layer having a maximum thickness of 0.05 mm, and at least one of the thermoplastic layers, preferably each, having a maximum thickness of 0.15 mm. Each of the thermoplastic layers may be provided with a conductive coating, preferably an indium tin oxide (ITO) coating, on their mutually facing surfaces. The thermoplastic layers may be composed of polyethylene terephthalate (PET) and / or polyethylene naphthalate (PEN). At least one film layer may in particular be a polymer dispersed liquid crystal device, a suspended particle device, an electrochromic device and / or a microblind. Preferably, at least one of the thermoplastic layers has a maximum thickness of 0.15 mm, preferably 0.1 mm, more preferably 0.05 mm.
[0019] Preferably, at least one, preferably at least two, bonding layers extend beyond the functional layer along at least a portion of the periphery of the at least one functional layer by at least 1 mm, preferably at least 3 mm. Preferably, a portion of the periphery of the at least one functional layer has an offset of at least 1 mm, preferably 3-10 mm, relative to the periphery of the glass sheet. This allows the bonding layer to completely surround the functional layer and thus form a seal of the functional layer. Preferably, the seal extends along the entire periphery of the functional layer. Preferably, the seal is formed by the bonding layer along the entire extent of the seal. It is conceivable that along a portion of the periphery of the thermoplastic laminated sheet structure, the functional layer is not directly sealed by the bonding layer, and this portion may be formed by a connector for supplying power to the functional layer. The connector may be attached to the anode and cathode of the functional layer, and the thermoplastic laminated sheet structure may protrude such that in a portion of the periphery where the connector is connected to the functional layer, there is no localized direct sealing of the functional layer by the bonding layer. On the other hand, it is conceivable that the bonding layer may seal a portion of the periphery where the connector is present, whereby the bonding layer may seal the portion where the connector is present and seal the connector and / or the functional layer.
[0020] It is conceivable that the layers of the thermoplastic laminated sheet structure are prebonded layers, in particular at least two bonding layers are prebonded to the functional layer, the two bonding layers forming an integral encapsulation that substantially entirely encapsulates the functional layer such that the functional layer is hermetically sealed. Prebonding the layers of the thermoplastic laminated sheet structure may allow a more accurate process, since the sealing of the functional layer can be checked before laminating the prebonded laminated sheet structure between the first and second glass sheets. This may be particularly beneficial if a connector is provided on the thermoplastic laminated sheet structure. The connector allows the anode and the cathode of the thermoplastic laminated sheet structure to be brought into contact, which may supply power to the sheet structure. It is conceivable that the connector at least partially protrudes from the laminated sheet structure, the portion where the connector protrudes from the sheet structure being also sealed by the bonding layer. That is to say, substantially no moisture or other undesirable elements can penetrate through the connector into the sheet structure, in particular into the functional layer. Preferably, the bonding layers of the prebonded thermoplastic laminated sheet structure are in a crosslinked state. This further contributes to the toughness of the thermoplastic laminated sheet structure. This may especially contribute to the seal achieved by the tie layer, since the crosslinked state allows the tie layers to form an integral tie layer along the part of the periphery of the functional layer where the tie layer extends beyond the functional layer. The tie layers can still be laminated after crosslinking. Crosslinking usually increases the softening point of the layers. Thus, the conditions for successful lamination may change (i.e., the temperature may need to be higher relative to the pre-crosslinked state). Hard and soft crosslinking (post) may change the viscosity and possibly the final mechanical strength. However, after the gap between the thermoplastic laminate sheet structure and the glass sheet is filled, the higher viscosity (post-crosslinking) tie layer still adheres to the glass, so a lower viscosity is not required. The adhesion of the post-crosslinking tie layer to glass is slightly lower compared to the non-crosslinked variant, but this slightly lower adhesion contributes to impact resistance, since delamination occurs upon impact. The amount of adhesion may be measured by the pummel test, a method well known in the art for testing laminated glass.For this purpose, at least one tie layer comprises at least one cross-linking agent.
[0021] Preferably, the moisture content of at least one layer, preferably all of the tie layers, is 0.3% by weight or less, especially after lamination. The moisture is preferably extracted from the tie layers before and / or during the lamination process. This level of moisture content is beneficial for forming a proper seal of the functional layers. Moisture in the tie layers can cause problems, which often occur at higher temperatures, i.e., for example, during the lamination process. Moisture inside the tie layers can cause reactions with active films, such as liquid crystals, which can lead to irreparable damage to the active films. The moisture content can be measured by known methods. For example, a method for measuring the moisture content before lamination is to use a 1930 cm -1 This can be done by measuring the H-OH band of the bonding layer before lamination. This makes it possible to measure the bonding layer before lamination. On the other hand, to measure the water of moisture content in the laminated structure, it is done by a spectrometer. In particular, it is done at wavelengths from 1650 nm to 1925 nm. Here, the absorption coefficient (AR) is compared with a reference sample. The method is widely accepted in the field of laminated windows for automobiles to measure the moisture and moisture content in laminated glass structures and therefore after lamination. It is important to measure the moisture content after lamination, since the lamination process can affect the moisture content. It was found that if the drying of the bonding layer is done to a super-dry state, there is a higher probability that the moisture level will rise back during the lamination process. Moisture extraction during the initial lamination process by reducing the pressure to a level where the water boils eliminates and improves this problem, since not only the water but also the easily migrating plasticizers are extracted. In addition to all this, the process is faster, since the drying takes several days. This extraction step is particularly advantageous when PDLC is used. The transitional element can result in edge clearing, which is a phenomenon of liquid crystal failure seen locally from the periphery of the film inwards, leaving the edges of the functional film permanently clear, which is quite different from SPD, where the effect of moisture depends on the overall age of the film.
[0022] The present invention further relates to a thermoplastic laminate sheet structure for use in an automotive window laminate structure according to the present invention. The advantages disclosed with respect to automotive windows are also applicable to thermoplastic laminate sheet structures and are hereby incorporated by reference in that regard.
[0023] The present invention further relates to a method for manufacturing an automotive window laminate structure by a hot press lamination process, the method comprising the steps of: a) providing a first and a second glass sheet; b) providing a thermoplastic laminate sheet structure between the first and the second glass sheets, the laminate sheet structure comprising at least one functional layer and at least one, preferably two bonding layers, the functional layer being located between or adjacent to the at least one bonding layer; c) adhering the at least two bonding layers to the first and the second glass sheets by applying an external pressure to the window laminate formed during steps a) and b), in particular to at least one bonding layer, preferably each bonding layer of the window laminate, and increasing its temperature above the glass transition temperature of the bonding layer for a predetermined amount of time; and d) sealing the functional layer by the at least two bonding layers during the period of increasing temperature of step c).
[0024] The method according to the invention allows for a more controlled and easier manufacturing of automotive window laminates. Since there is no film layer around the thermoplastic laminate sheet structure, the thermoplastic laminate sheet structure can be easily placed to fit the periphery or edge of the glass sheet. This eliminates the step of carefully positioning the thermoplastic laminate sheet structure in place on the glass sheet and then placing a frame layer around it. In this way, the thermoplastic laminate sheet structure is more easily placed in the right place. Furthermore, since there is no frame layer, it is easier to apply a better and easier seal of the functional layer. If the functional layer is not sealed, it will deteriorate over time due to moisture penetrating into the functional layer. The seal can substantially hermetically seal the functional layer from the environment. By increasing the temperature, the seal will be achieved by two bonding layers, which can thus form a single bonding layer. It should be noted that the thermoplastic laminate sheet structure and / or the overall automotive window laminate may be brought to a state below the boiling point curve of water measured on the opposite parameter illustration, which is usually close to a vacuum state. Thus, the moisture, especially water, will evaporate very quickly, since the boiling point of water is, for example, 29° C. at 40 mbar, i.e. the temperature and pressure during step c) are such that this point is below the boiling curve of water and thus the water evaporates, which contributes to the formation of a proper seal.
[0025] In a different embodiment, the functional layer is substantially hermetically sealed by the bonding layer in step d). By substantially hermetically sealing the functional layer, moisture is prevented from penetrating into the functional layer. This is particularly important since the functional layer can extend up to 5 mm from the periphery of the glass sheet. Therefore, a proper seal of said bonding layer, which is performed by the frame layer in the window laminate according to the prior art, is very important since the functional layer extends further towards the periphery of the glass compared to the prior art.
[0026] It is conceivable that the thermoplastic laminate sheet structure provided in step b) is a pre-bonded thermoplastic laminate sheet structure. Therefore, the method may further comprise, preferably before step c), a step of pre-bonding the thermoplastic laminate sheet structure provided in step b) such that the thermoplastic laminate sheet structure is a pre-bonded thermoplastic laminate sheet structure. This allows the production to be carried out in sequence, i.e. the thermoplastic laminate sheet structure may be pre-manufactured. This may be beneficial from a logistical point of view, but also from a quality point of view. As the sealing of the functional layer is very important, pre-laminating the thermoplastic laminate sheet structure may be beneficial as it gives the possibility to check whether the seal is properly formed.
[0027] Preferably, the step of pre-bonding the thermoplastic laminated sheet structure comprises the steps of: i) pressing the bonding layer against the functional layer between two opposing rollers, during step i) air between the bonding layer and the functional layer is removed, and at least a portion of the sealing of step d) is achieved simultaneously or substantially immediately after step i). Preferably, during step i), the temperature is increased by increasing the temperature of the area surrounding the rollers or by heating the rollers. By removing air between the bonding layer and the functional layer, in particular its thermoplastic layer, the transparency of the window laminate may be improved. Furthermore, by pre-bonding the functional layer and the bonding layer, the bonding layer is more firmly attached to the functional layer, which may be critical when laminating the window laminate. By pre-bonding the bonding layer to the functional layer, slippage between the bonding layer and the functional layer may be less likely during its lamination between the glass sheets. This may further reduce the chance of wrinkles being introduced into the window laminate. In particular, wrinkles in the functional layer may be reduced, since a stronger pre-assembly is formed by pre-bonding the functional layer between the bonding layers.
[0028] It is also conceivable that the step of pre-bonding the thermoplastic laminated sheet structure comprises the steps of: i) providing two substantially flat, preferably rigid plates, preferably made of polymethyl methacrylate (PMMA) or splayed ethylene propylene diene monomer (EPDM), on the upper and lower faces of the thermoplastic laminated sheet structure, in particular rigid plates with a higher coefficient of thermal expansion than glass; and ii) applying an external pressure to the laminated package provided during step i) and increasing the temperature of at least a part of the laminated package until the bond between the bonding layer and the functional layer is realized. A further advantage of this method of pre-bonding the thermoplastic laminated sheet structure is that it can be carried out under vacuum. More particularly, the flat plates can extend beyond the periphery of the thermoplastic laminated sheet structure. In this way, the thermoplastic laminated sheet structure may be totally surrounded by the flat plates, which can be attached to each other by a frame or an adhesive. Preferably, the air between the two plates can be removed by sucking the air out to form a vacuum. This further provides additional pressure to be exerted on the thermoplastic laminated sheet structure, and under the application of heat, a pre-bonded thermoplastic laminate can be realized. Preferably, the temperature of said at least part of the laminate package is raised during step ii) to between 60 and 140° C. Preferably, two rigid splayed EPDM plates together form a flexible clamp, whereby, after the temperature is raised above the glass transition temperature in step ii), the entire stack is pre-formed by pressing it into a predefined three-dimensional shape, preferably a doubly curved three-dimensional shape, such that after cooling the plates may return to their substantially flat initial shape, while the so-called memory of the thermoplastic laminate structure is reset to the three-dimensional shape and, as a result, still retains this three-dimensional shape.
[0029] Preferably, the step of pre-bonding the thermoplastic laminated sheet structure further comprises the steps of: iii) providing at least one layer of adhesive thermoplastic sheet material, preferably adhesive thermoplastic polyurethane, between the upper and lower surfaces of the thermoplastic laminated sheet structure and two substantially flat, preferably rigid plates, respectively, before step ii); and iv) removing said adhesive thermoplastic layer and said substantially flat, rigid plates applied during step iii) after the bonding between the bonding layer and the functional layer is achieved during step ii). It is preferred that the bonding layer does not stick to the plates, since it can become relatively soft at elevated temperatures. For this purpose, a layer of thermoplastic sheet material, such as an interleaved separation layer or interleaved sheet, may be adhered to the outer surface of the bonding layer. In this way, at elevated temperatures, the thermoplastic sheet does not stick to the plates, making the thermoplastic laminated sheet structure removable after pre-bonding. It is further preferred that the interleaved sheet is removed after pre-bonding, which can be achieved by ensuring that the surface of the interleaving does not stick to the bonding layer, for example by an anti-sticking agent or coating, or by selecting the material of the interleaving so that it does not stick. Generally, the rollers or plates used in pre-bonding are believed to have anti-stick surfaces that prevent them from sticking to the thermoplastic laminate sheet structure. The interleaved layer is believed to be composed of polytetrafluoroethylene (PTFE).
[0030] Preferably, the method further comprises a moisture extraction step, preferably before step c), which comprises subjecting the thermoplastic laminate sheet structure to a vacuum, preferably a deep vacuum of 95% vacuum or more, or subjecting the thermoplastic structure to a predefined condition, preferably a temperature and pressure below the boiling curve of water, which allows the moisture to evaporate. It has been found that by subjecting the thermoplastic laminate sheet structure to a vacuum, more moisture can be extracted from the thermoplastic laminate sheet structure. It is considered that the moisture extraction step can be before step c), but also before pre-bonding the thermoplastic laminate. The moisture extraction step is carried out under conditions where the combination of temperature and pressure is below the boiling curve of water, in this way the water to evaporate can be extracted from the bonding layer and / or the sheet structure. By further reducing the moisture content before the actual lamination or pre-bonding process, moisture inside the bonding layer can be prevented from damaging the functional layer during lamination and / or pre-bonding, especially when the temperature is elevated. This is mainly because moisture present in the thermoplastic laminate sheet structure can affect the liquid crystal, i.e. the functional layer, when the temperature is elevated due to chemical reactions occurring between the moisture and the functional layer.
[0031] Preferably, said vacuum conditions are maintained for 10 minutes or more, preferably 30 minutes or more, more preferably 60 minutes or more. In this way, it was found that a thermoplastic laminated sheet structure could be realized with a moisture content of less than 0.3%. That is, the moisture content is reduced to 0.3% or less, preferably 0.2% or less. In particular, said moisture content is measurable after the lamination process. It was found that having this level of moisture content maintains a higher quality of the functional layer during the lamination and / or pre-bonding process. The moisture content can be measured by known methods. For example, a method for measuring the moisture content before lamination is the 1930 cm -1This can be done by measuring the H-OH band of the thermoplastic laminated sheet structure before lamination. This allows to measure the thermoplastic laminated sheet structure before lamination. On the other hand, to measure the water of moisture content in the laminated structure, it is done by a spectrometer. In particular, it is done at wavelengths from 1650 nm to 1925 nm. Here, the absorbance (AR) is compared with a reference sample. The method is widely accepted in the field of laminated windows for automobiles to measure the moisture and moisture content in laminated glass structures and therefore after lamination. It is important to measure the moisture content after lamination, since the lamination process can affect the moisture content. It was found that if the drying of the bonding layer is done to a super-dry state, there is a higher probability that the moisture level will rise back during the lamination process. Moisture extraction during the initial lamination process by reducing the pressure to a level where the water boils eliminates and improves this problem, since not only the water but also the easily migrating plasticizers are extracted. In addition to all this, the process is faster, since the drying takes several days.
[0032] Preferably, the method further comprises a preheating step prior to step b), in which the thermoplastic laminate sheet structure or at least the bonding layer thereof is preheated to a temperature of 35-55°C, preferably 40-50°C. By preheating the laminate prior to step b), the difference in the thermal expansion coefficients of glass and the thermoplastic laminate sheet structure can be reduced. This can be particularly advantageous when use of prebonded thermoplastic laminate sheet structures is made. Preferably, preheating can be applied until the desired temperature of the thermoplastic laminate sheet structure is reached.
[0033] Preferably, during step c), the temperature is increased at a minimum rate of 3° C. per minute, preferably 5° C. per minute, more preferably 10° C. per minute. It has been found that by allowing a fast temperature increase, wrinkling of the functional layer is reduced. This can be particularly advantageous when the use of pre-bonded thermoplastic laminate sheet structures is made. A fast temperature increase ensures that the outer parts of the thermoplastic laminate sheet structure, such as the bonding layers, have already reached the softening onset temperature and can adhere to the glass sheet, while internally the temperature may still be lower, which makes the internal parts hold together more firmly and reduces the possibility of the sheets of the thermoplastic laminate sheet structure slipping against each other. [Brief description of the drawings]
[0034] [Figure 1] FIG. 1 illustrates a cross-sectional view of an embodiment of an automotive window laminate. [Diagram 2] FIG. 2 shows a thermoplastic laminate sheet structure for use in an automotive window laminate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0035] The invention will now be described in more detail with reference to the following drawings.
[0036] FIG. 1 shows a non-limiting embodiment of an automotive window laminate 1 according to the present invention. The simplified embodiment schematic representation shows a first and a second glass sheet 2, 3, which are spaced apart and substantially parallel. A thermoplastic laminated sheet structure 4 is provided between the first and second glass sheets 2, 3. The thermoplastic laminated sheet structure 4 comprises at least two bonding layers 5, with a functional layer 6 provided between the two bonding layers 5. Preferably, the bonding layer 5 bonds the functional layer to the glass sheets 2, 3. However, in addition to bonding the functional layer 6 to the glass sheets 2, 3, it is considered that the bonding layer 5 performs a further function. That is, preferably, the bonding layer 5 at least partially seals the functional layer 6 from the environment along at least a part of the periphery of the functional layer 6. In this way, the bonding layer 5 may prevent moisture from penetrating into the functional layer 6, which may increase the life of the functional layer 6. The circled edge A of the automotive window laminate 1 is shown in more detail at the bottom in an enlarged view. End A (enlarged portion) shows that the bonding layer 5 surrounds the functional layer 6, such as forming a seal. Preferably, the bonding layer 5 extends to the periphery of the first and second glass sheets 2, 3. The functional layer 6 preferably extends from the periphery of the bonding layer 5 to a distance D. This may allow the bonding layer 5 to substantially entirely surround the functional layer 6, such as to substantially hermetically seal it from the surroundings. As shown, the automotive window laminate 1 is substantially free of a frame structure or frame layer that is typically provided by the prior art. That is, the functional layer 6 extends from the periphery of the glass sheets 2, 3 to a distance D that may be, for example, 5 to 10 mm. This allows the automotive window laminate 1 to have a larger functional surface, thereby reducing the surface of the black masking that is provided in the part of the window where the frame layer or frame structure is usually present.
[0037] FIG. 2 shows a thermoplastic laminated sheet structure 4 according to an advantageous embodiment. The thermoplastic laminated sheet structure 4 comprises at least two bonding layers 5, with a functional layer 6 between the two bonding layers 5. Preferably, the functional layer is bonded to a glass sheet, which is not shown in this figure for the sake of clarity. However, it is conceivable that at least one of the bonding layers 5 performs a further function in addition to bonding the functional layer 6 to the glass sheets 2, 3. That is, preferably, the bonding layer 5 at least partially seals the functional layer 6 from the surroundings along at least a part of the periphery of the functional layer 6. In this way, the bonding layer 5 may prevent moisture from penetrating into the functional layer 6, which may increase the lifespan of the functional layer 6. A particular embodiment of the thermoplastic laminated sheet structure 4 shown in this figure comprises a cascade structure. In particular, the lower bonding layer 5 may be thicker, such as PVB, as shown in the figure. This may be the case when the functional layer 6 has an asymmetric composition, i.e. one thermoplastic PET layer 7 of the functional layer 6 is thicker compared to the other. In particular, the lower thermoplastic PET layer 7 has a thickness of 100-150 microns in this figure, while the upper thermoplastic PET layer 7 has a thickness of about 50 microns. On the side of the thicker thermoplastic PET layer 7, a thicker PVB tie layer 5 can be arranged. This is possible because the thicker PET layer 7 can prevent the penetration of plasticizers. On the side of the thinner PET layer 7 of the functional layer, a tie layer 5 made of TPU is provided. The TPU tie layer is more compatible with the thinner PET layer 7 of the functional layer 6 and, due to its lower softening temperature, can prevent the formation of wrinkles in the functional layer 6, especially during lamination. Furthermore, the TPU tie layer 5 makes it possible to form a seal 10 around the edge 9 of the functional layer 6. This figure is a specific example and does not limit the inventive concept of the present invention.
Claims
1. 1. A method for manufacturing an automotive window laminate structure by a heat and pressure lamination process, comprising: a) providing first and second glass sheets; b) providing a thermoplastic laminate sheet structure between the first and second glass sheets, the thermoplastic laminate sheet structure comprising at least one functional layer and at least two bonding layers, the functional layer being located between the at least two bonding layers; c) adhering the at least two bonding layers to the first and second glass sheets by applying external pressure to the window laminate formed during steps a) and b), in particular to at least one bonding layer, and preferably each bonding layer, of the window laminate and raising its temperature above the glass transition temperature of the bonding layer for a predetermined amount of time; d) sealing the functional layer by the at least two bonding layers during the temperature increase of step c); A method for providing the above.
2. The method of claim 1 , wherein during step d), the functional layer is substantially hermetically sealed by the tie layer.
3. 3. The method according to claim 1 or 2, further comprising, preferably before step c), a step of pre-bonding the thermoplastic laminate sheet structure provided in step b), such that the thermoplastic laminate sheet structure is a pre-bonded thermoplastic laminate sheet structure.
4. The step of pre-bonding the thermoplastic laminate sheet structure comprises: i) pressing the bonding layer against the functional layer between two opposing rollers; The method according to claim 3, wherein during step i) air is removed between the bonding layer and the functional layer, and at least a portion of the sealing in step d) is achieved simultaneously with or substantially immediately after step i).
5. The step of pre-bonding the thermoplastic laminate sheet structure comprises: i) providing two substantially flat rigid plates, preferably constructed from polymethyl methacrylate (PMMA) or ethylene propylene diene monomer (EPDM), on top and bottom surfaces of the thermoplastic laminate sheet structure; ii) applying an external pressure to the laminated package provided during step i) and increasing the temperature of at least a portion of the laminated package until a bond between the bonding layer and the functional layer is achieved; The method of claim 3 comprising:
6. The method of claim 5, wherein the temperature of said at least a portion of said laminated package is elevated to 60-140° C. during step ii).
7. The pre-binding step further comprises: iii) before step ii), providing at least one layer of adhesive thermoplastic sheet material, preferably adhesive thermoplastic polyurethane, between said upper and lower surfaces of said thermoplastic laminate sheet structure and each of said two substantially flat rigid plates; iv) removing the layer of adhesive thermoplastic applied during step iii) and the substantially flat rigid plate after the bond between the bonding layer and the functional layer has been achieved during step ii); The method of claim 5 or 6, further comprising:
8. 8. The method according to any one of claims 1 to 7, further comprising a moisture extraction step, preferably before step c), which comprises subjecting the thermoplastic laminate sheet structure to a vacuum, preferably deep vacuum conditions of 95% vacuum or more, or subjecting the thermoplastic laminate sheet structure to predetermined conditions, preferably a temperature and pressure below the boiling curve of water, allowing the moisture to evaporate.
9. 9. The method of claim 8, wherein the vacuum condition is maintained for at least 10 minutes, preferably at least 30 minutes, more preferably at least 60 minutes.
10. 10. The method according to any one of claims 1 to 9, further comprising a pre-heating step prior to step b), in which the thermoplastic laminated sheet structure or at least the bonding layer thereof is pre-heated to a temperature of 35-55°C, preferably 40-50°C.
11. 11. The method according to any one of claims 1 to 10, wherein during step c) the temperature is increased at a minimum rate of 3°C per minute, preferably 5°C per minute, more preferably 10°C per minute.
12. 12. The method of any one of claims 1 to 11, wherein the pre-bonded thermoplastic laminate sheet structure is imparted with a double curvature.
13. 13. An automotive window laminate structure obtainable by the method according to any one of claims 1 to 12.
14. a first glass sheet and a second glass sheet which are parallel and spaced apart from one another; a thermoplastic laminate sheet structure disposed substantially entirely between the first and second glass sheets, the thermoplastic laminate sheet structure comprising: At least one functional layer having an upper surface and a lower surface; at least two tie layers substantially entirely covering the upper and lower surfaces of the at least one functional layer; A thermoplastic laminate sheet structure comprising: a sealing portion configured to surround the thermoplastic laminated sheet structure, in particular the functional layer, in order to seal the thermoplastic laminated sheet structure from the surroundings; Equipped with 1. An automotive window laminate structure, wherein the thermoplastic laminate sheet structure extends substantially entirely around the periphery of the first and second glass sheets, and the seal is at least partially formed by the at least two bonding layers along at least a portion of the periphery of the thermoplastic laminate sheet structure.
15. 15. The automotive window laminate structure according to claim 14, wherein the automotive window laminate structure is in particular a curved laminate structure.
16. The functional layer of the automotive window laminate structure has a thickness of 1000 cm 2 More than 1500 cm, preferably 2 More preferably, 2000 cm 2 16. An automotive window laminate structure according to claim 14 or 15, having the above surface.
17. 17. An automotive window laminate structure according to any one of claims 14 to 16, wherein the thickness of the functional layer is less than 0.30 mm, preferably less than 0.20 mm.
18. 18. An automotive window laminate structure according to any one of claims 14 to 17, wherein the at least one functional layer comprises at least two thermoplastic layers and at least one film layer between the at least two thermoplastic layers, the film layer having a maximum thickness of 0.05 mm, and at least one, preferably each, of the thermoplastic layers having a maximum thickness of 0.15 mm, preferably 0.10 mm, more preferably 0.05 mm.
19. 19. The automotive window laminate structure of any one of claims 14 to 18, wherein the at least two tie layers covering the upper and lower surfaces of the functional layer are composed of ethylene-vinyl acetate (EVA) or thermoplastic polyurethane (TPU).
20. 20. An automotive window laminate structure as claimed in any one of claims 14 to 19, wherein the layers of the thermoplastic laminate sheet structure are pre-bonded layers, in particular the at least two bonding layers are pre-bonded to the functional layer, and the two bonding layers form an integral encapsulation portion that substantially entirely encapsulates the functional layer such that the functional layer is hermetically sealed.
21. 21. The automotive window laminate structure of claim 20, wherein the bonding layer of the pre-bonded thermoplastic laminate sheet structure comprises at least one cross-linking agent such that the bonding layer of the thermoplastic laminate sheet structure is in a cross-linked state.
22. 22. An automotive window laminate structure as claimed in any one of claims 14 to 21, wherein at least one, preferably at least two, bonding layers extend beyond the at least one functional layer along at least a portion of its periphery by at least 1 mm, preferably at least 3 mm.
23. 23. An automotive window laminate structure according to any one of claims 14 to 22, wherein at least one, and preferably all, bonding layers have a moisture content of 0.3% by weight or less.
24. A thermoplastic laminate sheet structure for use in an automotive window laminate structure obtainable by the method according to any one of claims 1 to 11.
Citation Information
Patent Citations
Laminated window glass
JP2013505188A
Composite pane having multiple composite layers and method of manufacturing same
JP2019527631A
Laminated glass and laminate used therein
WO2012050078A1
Laminated glass
WO2017099167A1
Laminated glass