Double-sided adhesive tape for adhering polishing pads from which air bubbles can be easily expelled, and chemical mechanical polishing apparatus using said adhesive tape
The double-sided adhesive tape with a bubble discharge pattern effectively addresses the issue of air bubbles in polishing pads, ensuring uniform performance and improved adhesion, thereby extending the pad's lifespan.
Patent Information
- Application Number
- JP2024536159
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-17
- Filing Date
- 2022-11-16
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2042-11-16
AI Technical Summary
Existing double-sided adhesive tapes used to secure CMP polishing pads to surface plates often form air bubbles, which impair the flatness and adhesive force, leading to non-uniform polishing performance and premature wear.
A double-sided adhesive tape with a bubble discharge pattern formed by protruding lines on the lower surface, allowing easy removal of air bubbles by applying pressure.
The adhesive tape ensures uniform polishing performance and strong adhesion, extending the life of the polishing pad by preventing air bubbles from forming and facilitating their removal.
Smart Images

Figure 2024545262000001_ABST
Abstract
Description
[Technical Field]
[0001] This application claims the benefit of priority based on Korean Patent Application No. 10-2021-0182176 dated December 17, 2021, and all contents disclosed in the documents of that Korean patent application are incorporated herein by reference.
[0002] The present invention relates to a double-sided adhesive tape for adhering a polishing pad, from which air bubbles can be easily removed, and a chemical mechanical polishing apparatus to which the adhesive tape is applied. [Background technology]
[0003] Double-sided adhesive tapes are widely used to bond components and prevent or fill gaps between surfaces, for example, to seal electronic devices, to apply protective films to the devices to absorb shock, and to secure CMP polishing pads to platens.
[0004] When the CMP polishing pad is fixed to the surface plate, a double-sided adhesive tape with a relatively large area is used. When such a double-sided adhesive tape with a large area is used, air bubbles often form on the adhesive surface. These air bubbles cause problems such as impairing the flatness of the polishing pad surface and weakening the adhesive strength.
[0005] Specifically, when the polishing pad is fixed to the platen, a double-sided adhesive tape is used to bond the lower surface of the polishing pad to the upper surface of the platen. If air bubbles form between the double-sided adhesive tape and the upper surface of the platen, the flatness of the upper surface of the polishing pad is impaired and the adhesive strength of the polishing pad is weakened. In particular, when flatness is impaired as described above, it is difficult to achieve uniform polishing performance, and the protruding portions due to the air bubbles wear out more quickly.
[0006] Conventionally, when air bubbles occur at the interface as described above, they are removed by applying pressure to the double-sided adhesive tape from above to push the air bubbles to the edge, but this method often makes it impossible to remove the air bubbles.
[0007] Therefore, there is a need to develop a method for easily removing such bubbles. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] Korean Patent Publication No. 10-2013-0043589 Summary of the Invention [Problem to be solved by the invention]
[0009] The present invention has been devised to solve the above-mentioned problems of the prior art, The object of the present invention is to provide a double-sided adhesive tape for adhering a polishing pad, which can easily remove air bubbles that occur on the bonding surface when the double-sided adhesive tape is used, and a chemical mechanical polishing apparatus to which the double-sided adhesive tape is applied. [Means for solving the problem]
[0010] In order to achieve the above object, the present invention provides an upper release film layer; a first adhesive layer; an adhesive tape substrate laminated on the lower surface of the first adhesive layer; a second adhesive layer laminated on the lower surface of the adhesive tape substrate; and The double-sided adhesive tape for adhering a polishing pad includes an air bubble discharge pattern-formed sheet layer laminated on the lower surface of the second adhesive layer and having an air bubble discharge pattern formed on the laminate surface with protruding lines.
[0011] In one embodiment of the present invention, the air bubble release patterned sheet layer may be laminated in a state where a pattern formed by protruding lines is recessed into the lower surface of the second adhesive layer.
[0012] In one embodiment of the present invention, the upper release film layer and the bubble-releasing patterned sheet layer may be removed at the time of use.
[0013] In one embodiment of the present invention, the second adhesive layer may be adhered to a surface from which air bubbles are desired to be removed.
[0014] In one embodiment of the present invention, the pattern formed by the protruding lines may be a stripe pattern or a polygonal pattern.
[0015] In one embodiment of the present invention, the polygonal pattern may be a quadrangular pattern formed by intersecting straight protruding lines.
[0016] In one embodiment of the present invention, the cross section of the protruding line in the width direction may be a polygon, a circle with a part cut off at the bottom, or an ellipse with a part cut off at the bottom.
[0017] In one embodiment of the present invention, the maximum width of the projecting lines may be 50 μm to 250 μm, and the height may be 5 μm to 30 μm.
[0018] In one embodiment of the present invention, the rectangular pattern may have a width between two sides that are not adjacent to each other of 300 μm to 1000 μm.
[0019] In one embodiment of the present invention, the air bubble discharge pattern molded sheet layer may include a molded sheet having an air bubble discharge pattern formed by protruding lines on one side thereof, and a base film adhered to the other side of the molded sheet.
[0020] The present invention also provides A polishing pad; a platen on which the polishing pad is fixed, The polishing pad is fixed to the surface plate using the double-sided adhesive tape for adhering a polishing pad of the present invention.
[0021] In one embodiment of the present invention, the lower surface of the polishing pad is adhered to the first adhesive layer of the double-sided adhesive tape, The second adhesive layer of the double-sided adhesive tape may be attached to the upper surface of the surface plate. [Effects of the Invention]
[0022] The double-sided adhesive tape for adhering polishing pads of the present invention has a trench portion on the outer adhesive surface of the adhesive layer that allows air bubbles to be expelled, thereby providing the effect that if air bubbles occur at the adhesive interface, the bubbles can be easily expelled outside the adhesive interface by applying pressure.
[0023] In addition, the chemical mechanical polishing apparatus of the present invention has excellent flatness of the upper surface of the polishing pad, exhibits uniform polishing performance, and the polishing pad adheres strongly to the platen, thereby improving the service life of the polishing pad. [Brief explanation of the drawings]
[0024] [Figure 1] 1 is a cross-sectional view schematically showing one embodiment of a double-sided adhesive tape for adhering a polishing pad according to the present invention. [Figure 2] 1 is an exploded cross-sectional view schematically showing one embodiment of a double-sided adhesive tape for adhering a polishing pad according to the present invention. [Figure 3] 1 is a perspective view showing one embodiment of a molded sheet included in the double-sided adhesive tape for adhering a polishing pad of the present invention. [Figure 4] 1 is a photograph showing the adhesive state of a conventional double-sided adhesive tape for a polishing pad. [Figure 5] FIG. 1 is a cross-sectional view schematically showing the form of bubbles generated when a polishing pad is adhered using a conventional double-sided adhesive tape for a polishing pad. [Figure 6]FIG. 2 is a cross-sectional view schematically showing another embodiment of the double-sided adhesive tape for adhering a polishing pad of the present invention. [Figure 7] 1 is a cross-sectional view showing a state in which a polishing pad is adhered to a surface plate using the double-sided adhesive tape for adhering a polishing pad of the present invention. [Figure 8] 1 is a perspective view schematically illustrating an embodiment of a chemical mechanical polishing apparatus according to the present invention. [Figure 9] Photographs showing the removal of air bubbles when the double-sided adhesive tape for adhering a polishing pad of the present invention is used (Example 1) and when a conventional double-sided adhesive tape for adhering a polishing pad is used (Comparative Example 1). [Figure 10] 1 is a photograph showing an evaluation of whether or not the double-sided adhesive tape for adhering a polishing pad of the present invention has liquid penetration (when ink is used). [Figure 11] 3 is a photograph showing the test process and results for measuring adhesive strength after inducing liquid penetration of the double-sided adhesive tape for adhering a polishing pad of the present invention (Example 1) and a conventional double-sided adhesive tape for adhering a polishing pad (Comparative Example 1). [Figure 12] 2 is a photograph showing the surface of the second adhesive layer included in the double-sided adhesive tape for bonding a polishing pad of the present invention. DETAILED DESCRIPTION OF THE INVENTION
[0025] The present invention will now be described in detail with reference to the accompanying drawings, so that those skilled in the art can easily understand the present invention. However, the present invention may be embodied in various different forms and is not limited to the embodiments described herein. Like reference numerals are used throughout the specification to refer to like parts.
[0026] When a component is said to be "connected to, comprised in, or provided on" another component, it should be understood that it may be directly connected to or provided on the other component, but there may also be other components between them. On the other hand, when a component is said to be "directly connected to, comprised in, or provided on" another component, it should be understood that there are no other components between them. Meanwhile, other expressions describing the relationship between components, such as "on top of" and "directly on top of," or "between" and "immediately between," or "adjacent to" and "directly adjacent to," should be interpreted similarly.
[0027] FIG. 1 is a cross-sectional view schematically showing one embodiment of the double-sided adhesive tape for adhering a polishing pad of the present invention, and FIG. 2 is an exploded cross-sectional view schematically showing one embodiment of the double-sided adhesive tape for adhering a polishing pad of the present invention.
[0028] As shown in Figures 1 and 2, the double-sided adhesive tape (100) for adhering a polishing pad of the present invention is characterized by comprising an upper release film layer (10), a first adhesive layer (20), an adhesive tape substrate (30) laminated on the lower surface of the first adhesive layer, a second adhesive layer (40) laminated on the lower surface of the adhesive tape substrate, and an air bubble release pattern forming sheet layer (50) laminated on the lower surface of the second adhesive layer and including an air bubble release pattern formed on the laminate surface by protruding lines.
[0029] FIG. 3 is a perspective view showing one embodiment of the molded sheet layer (50) contained in the double-sided adhesive tape (100) for adhering a polishing pad of the present invention.
[0030] In one embodiment of the present invention, the bubble release patterned sheet layer (50) may be laminated in a state in which a pattern (52) formed of protruding lines is recessed into the lower surface of the second adhesive layer (40), as shown in FIG.
[0031] As described above, when the pattern (52) formed by the protruding lines is laminated in a recessed state on the lower surface of the second adhesive layer (40), when the air bubble release pattern forming sheet layer (50) is removed during use, the air bubble release pattern (42) is engraved on the lower surface of the second adhesive layer (40) that was attached to it.
[0032] Therefore, when the double-sided adhesive tape (100) for adhering a polishing pad is adhered to the upper surface of a surface plate (70, FIG. 7) by the second adhesive layer (40), even if air bubbles are generated between the polishing pad (60, FIG. 7) and the surface plate (70), they can be easily removed by the engraved air bubble discharge pattern (e.g., trench). Figure 7 shows a schematic diagram of the double-sided adhesive tape (100) for adhering a polishing pad of the present invention positioned between the polishing pad (60) and the surface plate (70), fixing the polishing pad (60) to the surface plate (70).
[0033] The double-sided adhesive tape (100) for adhering a polishing pad is adhered between a polishing pad (60) and a surface plate (70) with the upper release film layer (10) and the air bubble release patterned sheet layer (50) removed, as shown in Figure 7. Figure 12 shows a photograph of the shape of the second adhesive layer (40) with the upper release film layer (10) and the air bubble release patterned sheet layer (50) removed.
[0034] In one embodiment of the present invention, the second adhesive layer (40) may be adhered to a surface from which air bubbles need to be removed, such as a surface plate (70).
[0035] According to the prior art, when a polishing pad is fixed to a surface plate using a double-sided adhesive tape for adhering a polishing pad as described above, air bubbles often form between the double-sided adhesive tape and the surface plate, as shown in Figures 4 and 5, and it is very difficult to remove such air bubbles.
[0036] When air bubbles exist between the polishing pad and the platen, the flatness of the upper surface of the polishing pad is impaired and the adhesive strength of the polishing pad is weakened. In particular, when flatness is impaired as described above, it is difficult for the polishing pad to exhibit uniform polishing performance, and the protruding portions due to the air bubbles wear out more quickly.
[0037] However, when the double-sided adhesive tape (100) for adhering a polishing pad of the present invention is used, the above problems can be easily solved.
[0038] In one embodiment of the present invention, the pattern 52 formed by the protruding lines may be formed as a stripe pattern or a polygonal pattern.
[0039] The polygonal pattern may be formed in various shapes with linear protruding lines, for example, a polygon such as a triangle, a square, a pentagon, or a hexagon, and the shape of the polygon is not particularly limited.
[0040] In one embodiment of the present invention, the polygonal pattern may be a square pattern formed by linearly projecting lines intersecting each other. For example, such a square pattern may have a shape as shown in Figure 3. Such a square pattern forms linearly engraved air bubble discharge patterns (42, e.g., trenches) on the lower surface of the second adhesive layer (40), which may be advantageous for efficiently removing air bubbles.
[0041] In one embodiment of the present invention, the cross section of the protruding line in the width direction may be a polygon, a circle with a part cut off at the bottom, or an ellipse with a part cut off at the bottom. The polygon may be, for example, a triangle, a rectangle, etc., but is not limited thereto.
[0042] In one embodiment of the present invention, the maximum width of the protruding lines (FIG. 3, A) may be 50 μm to 250 μm, preferably 140 μm to 180 μm, and the height (FIG. 3, B) may be 5 μm to 30 μm, preferably 7 μm to 15 μm. If the maximum width of the protruding lines is smaller than the above-mentioned range, the efficiency of air bubble removal may decrease, and if it exceeds the above-mentioned range, the adhesive strength of the second adhesive layer (40) may decrease, which is not preferable.
[0043] In the above, the maximum width of the protruding line may be formed at the lowest end of the protruding line where the protruding line joins with a surface on which the protruding line is not formed, provided that if the cross section of the protruding line in the width direction is a circle with a part cut off at the bottom or an oval with a part cut off at the bottom, the maximum width may not be formed at the lowest end of the protruding line.
[0044] In one embodiment of the present invention, the width between two non-adjacent sides of the quadrangular pattern (FIG. 3, C) may be 300 μm to 1000 μm, preferably 500 μm to 650 μm. If the width between the two sides is smaller than the above-mentioned range, the adhesive strength of the second adhesive layer (40) may decrease, and if it exceeds the above-mentioned range, the efficiency of removing bubbles may decrease, which is not preferable.
[0045] In the quadrilateral pattern, there may be two widths between two sides that are not adjacent to each other, and these two widths may be formed to have the same size.
[0046] 6 is a cross-sectional view schematically illustrating another embodiment of the double-sided adhesive tape for adhering a polishing pad according to the present invention. As shown in FIG. 6, the air bubble release pattern-formed sheet layer (50) may include a molded sheet (54) having an air bubble release pattern formed of protruding lines on one side thereof, and a base film (55) adhered to the other side of the molded sheet. In this case, the molded sheet (54) and the base film (55) adhered to the other side of the molded sheet may be separated separately when using the double-sided adhesive tape for adhering a polishing pad (200), or they may be provided in an adhered state and separated at the same time.
[0047] FIG. 8 is a perspective view showing a schematic diagram of one embodiment of a chemical mechanical polishing apparatus (300) of the present invention.
[0048] The chemical mechanical polishing apparatus (300) of the present invention includes a polishing pad (60) and a platen (70) to which the polishing pad is fixed, and the polishing pad is fixed to the platen using the double-sided adhesive tape (not described) for adhering a polishing pad of the present invention.
[0049] The chemical mechanical polishing apparatus 300 of the present invention is characterized by the absence of air bubbles between the double-sided adhesive tape for adhering the polishing pad and the platen 70. Therefore, the chemical mechanical polishing apparatus 300 of the present invention exhibits excellent flatness of the upper surface of the polishing pad 60, exhibits uniform polishing performance, and the polishing pad 60 is strongly adhered to the platen 70, thereby improving the service life of the polishing pad.
[0050] In the chemical mechanical polishing apparatus (300), the lower surface of the polishing pad (60) may be adhered to the first adhesive layer (10) of the double-sided adhesive tape, and the upper surface of the platen (70) may be adhered to the second adhesive layer (40) of the double-sided adhesive tape.
[0051] In addition to the above-described characteristic components, the chemical mechanical polishing apparatus 300 may further include a polishing head 80, a conditioner 90, and a polishing slurry supply nozzle 94. In addition to the above-described components, the chemical mechanical polishing apparatus 300 may also include, without limitation, other components that are included in chemical mechanical polishing apparatuses known in the art.
[0052] The present invention will be described in detail below using examples and comparative examples. However, the examples according to the present invention can be modified into various other forms, and the scope of the present invention should not be construed as being limited to the examples described in detail below. The examples of the present invention are provided to explain the present invention in more detail to those skilled in the art.
[0053] Example 1: Production of double-sided adhesive tape for adhering polishing pads A 55 μm thick first adhesive layer was laminated on the top surface of a 50 μm thick PET adhesive tape substrate using an acrylic adhesive, and a 25 μm thick PET release film was laminated on the top surface of the first adhesive layer.
[0054] Next, the bottom surface of the adhesive tape substrate was turned upward, and a 40 μm thick second adhesive layer was laminated using a rubber-based adhesive. A molded sheet having a rectangular pattern (FIG. 3, 52) formed with protruding lines on one side and a bubble release pattern molded sheet having a substrate film bonded to the other side of the molded sheet were prepared, and the rectangular pattern was laminated so that it was recessed into the second adhesive layer to produce a double-sided adhesive tape for adhering a polishing pad.
[0055] The molded sheet layer film was manufactured by applying a polyethylene resin to a thickness of 35 μm on a 75 μm thick PET substrate film, and before the polyethylene resin hardened, pressing the upper surface with a molding roller to form a rectangular pattern (52, FIG. 3) formed with protruding lines, followed by hardening.
[0056] Comparative Example 1: Production of double-sided adhesive tape for adhering polishing pads As in Example 1, an upper release film layer, a first adhesive layer, an adhesive tape substrate, and a second adhesive layer were laminated.
[0057] A 25 μm thick PET release film was laminated on the lower surface of the second adhesive layer to prepare a double-sided adhesive tape for adhering a polishing pad.
[0058] Test Example 1: Evaluation of air bubble removal ability The bubble-removing patterned sheet was removed from the double-sided adhesive tape for adhering a polishing pad prepared in Example 1, and the lower surface of the second adhesive layer was adhered to an acrylic platen and pressed to remove bubbles.
[0059] Meanwhile, the release film was removed from the second adhesive layer of the double-sided adhesive tape for adhering a polishing pad prepared in Comparative Example 1, and the lower surface of the second adhesive layer was attached to an acrylic platen and pressurized to remove air bubbles.
[0060] The results of the experiment are shown in Figure 9. As can be seen in Figure 9, in Example 1, in which the double-sided adhesive tape for adhering a polishing pad of the present invention was adhered, no air bubbles remained after air bubbles were removed by applying pressure, but in Comparative Example 1, in which a conventional double-sided adhesive tape without an air bubble release patterned sheet was used, many air bubbles remained even after air bubbles were removed by applying pressure.
[0061] Test Example 2: Evaluation of adhesive strength and shear strength Using samples of the double-sided adhesive tape for adhering polishing pads of Example 1 and Comparative Example 1 adhered to an acrylic surface plate in the same manner as in Test Example 1, adhesive strength and shear strength were measured.
[0062] The adhesive strength was measured using a tensile strength tester (UTM), and the shear strength was measured using a tensile strength tester (UTM). The measurement results are shown in Table 1 below.
[0063] [Table 1]
[0064] (Note) Permanent side: The side where the double-sided adhesive tape is attached to the pad (bottom). Removal side: The side where the double-sided adhesive tape is attached to the CMP platen (= embossed surface). From Table 1, it was confirmed that the adhesive strength and shear strength of the double-sided adhesive tape for adhering polishing pads of Example 1 are at the same level as those of Comparative Example 1, despite the fact that the double-sided adhesive tape for adhering polishing pads of Example 1 includes a bubble discharge pattern on the second adhesive surface, and are also at a level suitable for use.
[0065] Test Example 3: Evaluation of adhesive residue Using a sample of the double-sided adhesive tape for adhering a polishing pad of Example 1 adhered to an acrylic surface plate in the same manner as in Test Example 1, the degree of adhesive residue generation was evaluated.
[0066] Specifically, after the double-sided adhesive tape for adhering a polishing pad was adhered to the acrylic surface plate, the double-sided adhesive tape was removed 10 hours later, and it was confirmed whether or not any residue remained.
[0067] As a result of the experiment, it was confirmed that when the double-sided adhesive tape was removed, no residue remained on the surface plate.
[0068] Test Example 4: Evaluation of side liquid penetration and adhesive strength after liquid penetration (1) Side liquid penetration test A side liquid penetration test was carried out using a sample of the double-sided adhesive tape for adhering a polishing pad of Example 1, which was adhered to an acrylic surface plate in the same manner as in Test Example 1 above.
[0069] Specifically, ink was supplied to the edge of the double-sided adhesive tape for adhering polishing pads adhered to the acrylic surface plate, and after 10 hours, it was checked whether the ink had penetrated into the edge. As a result of the test, as shown in Figure 10, no ink penetration into the edge of the double-sided adhesive tape for adhering polishing pads was observed.
[0070] (2) Evaluation of adhesive strength after induced liquid penetration Samples of double-sided adhesive tapes for adhering polishing pads of Example 1 and Comparative Example 1 were prepared and attached to an acrylic surface plate in the same manner as in Test Example 1, and used.
[0071] As shown in Figure 11, water was supplied to the edge of each sample of double-sided adhesive tape for adhering polishing pads, and after maintaining it for 10 hours, the adhesive strength was measured using a tensile strength tester (UTM). The results are shown in Figure 11.
[0072] From the table in Figure 11, it was confirmed that the double-sided adhesive tape for adhering a polishing pad of Example 1 had adhesive strength after liquid penetration at the same level as Comparative Example 1, despite having an air bubble release pattern on the second adhesive surface.
[0073] While the present invention has been described with reference to the preferred embodiments set forth above, various modifications and variations can be made without departing from the spirit and scope of the invention, and it is therefore intended by the appended claims to cover all such modifications and variations as fall within the spirit and scope of the invention. [Explanation of symbols]
[0074] 10 Upper release film layer 20 First adhesive layer 30 adhesive tape substrate 40 second adhesive layer 42 air bubble discharge pattern 50 air bubble discharge pattern forming sheet layer 52 Pattern formed by protruding lines 54 Molded sheet 55 Base film 60 Polishing pad 70 Surface plate 80 Polishing head 82 Wafer 92 Conditioner 94 Polishing slurry supply nozzle 100, 200: Double-sided adhesive tape for adhering polishing pads 300 Chemical mechanical polishing equipment
Claims
1. An upper release film layer; A first adhesive layer; an adhesive tape substrate laminated on a lower surface of the first adhesive layer; a second adhesive layer laminated on a lower surface of the adhesive tape substrate; and A double-sided adhesive tape for adhering a polishing pad, comprising an air bubble discharge pattern shaped sheet layer laminated on the lower surface of the second adhesive layer and including an air bubble discharge pattern formed on the laminated surface with protruding lines.
2. 2. The double-sided adhesive tape for adhering a polishing pad according to claim 1, wherein the bubble release patterned sheet layer is laminated in a state in which a pattern formed of protruding lines is recessed into the lower surface of the second adhesive layer.
3. 2. The double-sided adhesive tape for adhering a polishing pad according to claim 1, wherein the upper release film layer and the air bubble releasing patterned sheet layer are removed when in use.
4. 4. The double-sided adhesive tape for adhering a polishing pad according to claim 3, wherein the second adhesive layer is adhered to a surface from which removal of air bubbles is required.
5. 2. The double-sided adhesive tape for adhering a polishing pad according to claim 1, wherein the pattern formed by the protruding lines is a stripe pattern or a polygonal pattern.
6. 6. The double-sided adhesive tape for adhering a polishing pad according to claim 5, wherein the polygonal pattern is a quadrangular pattern formed by intersecting linear protruding lines.
7. 2. The double-sided adhesive tape for adhering a polishing pad as described in claim 1, characterized in that the widthwise cross section of the protruding line is a polygon, a circle with a part of the lower side cut off, or an ellipse with a part of the lower side cut off.
8. 2. The double-sided adhesive tape for adhering a polishing pad according to claim 1, wherein the maximum width of the protruding lines is 50 μm to 250 μm and the height is 5 μm to 30 μm.
9. 9. The double-sided adhesive tape for adhering a polishing pad according to claim 8, wherein the rectangular pattern has a width between two non-adjacent sides of 300 μm to 1000 μm.
10. 2. The double-sided adhesive tape for adhering a polishing pad as described in claim 1, characterized in that the air bubble discharge pattern molded sheet layer includes a molded sheet having an air bubble discharge pattern formed of protruding lines on one side thereof, and a base film adhered to the other side of the molded sheet.
11. A polishing pad; a platen to which the polishing pad is fixed; 13. A chemical mechanical polishing apparatus, comprising: a polishing pad fixed to said platen using the double-sided adhesive tape for adhering a polishing pad according to claim 1.
12. The lower surface of the polishing pad is adhered to the first adhesive layer of the double-sided adhesive tape, 12. The chemical mechanical polishing apparatus of claim 11, wherein an upper surface of a platen is attached to the second adhesive layer of the double-sided adhesive tape.
Citation Information
Patent Citations
Polishing pad, sample suction pad, and sample polishing apparatus and method
JP2000306870A
Pressure-sensitive adhesive tape
JP2004315609A
Double-faced adhesive tape and its manufacturing method
JP2008098356A
Tape for fixing polishing pad and polishing pad
JP2016074052A
Adhesive sheet
JP2018203836A