Uniform trench in semiconductor device and method for fabricating same

By employing trench fill structures with controlled depth and width ratios, the non-uniformity of trench isolation structures in CMOS image sensors is addressed, enhancing depth uniformity and improving device performance.

JP7560529B2Active Publication Date: 2024-10-02TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2022199939
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-07-01
Filing Date
2022-12-15
Publication Date
2024-10-02
Estimated Expiration
2042-12-15

AI Technical Summary

Technical Problem

The non-uniform depth of trench isolation structures in CMOS image sensors leads to potential damage of transfer transistors during the etching process due to loading effects, affecting device performance.

Method used

The implementation of trench fill structures with convex and concave bottom surfaces and controlled width ratios to achieve uniform trench depths, reducing the depth difference between straight and intersecting portions.

Benefits of technology

This approach enhances the depth uniformity of trench isolation structures by up to 40% and improves device performance by 5-10%, minimizing damage to transfer transistors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007560529000001
    Figure 0007560529000001
  • Figure 0007560529000002
    Figure 0007560529000002
  • Figure 0007560529000003
    Figure 0007560529000003
Patent Text Reader

Abstract

To provide a semiconductor structure, a semiconductor device, and a method of manufacturing the semiconductor device having a radiation sensitive region separated by a trench isolation structure.SOLUTION: A semiconductor device has a trench isolation structure including a first trench filling (isolation) structure on a second substrate 112 and a second trench filling (isolation) structure on the substrate. The first trench filling structure has a first width and a convex bottom surface. The second trench filling structure has a concave bottom surface 124Bs and a second width 124Bw that is greater than the first width.SELECTED DRAWING: Figure 4B
Need to check novelty before this filing date? Find Prior Art

Description

[Background technology]

[0001] Semiconductor image sensor devices are used to sense incident visible or non-visible radiation, such as visible or infrared light. These image sensors utilize an array of pixels, which may include photodiodes and transistors, to absorb (e.g., sense) incident radiation and convert the sensed radiation into an electrical signal. An example of a semiconductor image sensor is the complementary metal-oxide-semiconductor (CMOS) image sensor. CMOS image sensors are used in a variety of applications, such as computers, digital cameras, mobile phones, tablets, goggles, scientific instruments, etc. Summary of the Invention [Problem to be solved by the invention]

[0002] During the etching process of forming the trench, a trench with a larger width may have a larger depth due to the loading effect of the plasma etching process. Therefore, how to avoid damage to the transfer transistor of the CMOS image sensor in the trench isolation structure during the etching process has become an important issue in the industry. [Means for solving the problem]

[0003] In some embodiments, a semiconductor structure includes a first trench fill structure on a substrate and a second trench fill structure on the substrate, the first trench fill structure having a first width and a convex bottom surface, and the second trench fill structure having a concave bottom surface and a second width greater than the first width.

[0004] In some embodiments, the semiconductor device includes a first chip. The first chip includes a plurality of pixels on a first side of the first chip, and first and second trench fill structures isolating the plurality of pixels. The first trench fill structure has a convex bottom surface. The second trench fill structure is in contact with the first trench fill structure. The second trench fill structure has a concave bottom surface. The semiconductor device further includes a second chip bonded to a second side of the first chip. The second side is opposite the first side.

[0005] In some embodiments, a method includes forming a first pattern on a substrate having a first width and a second pattern having a second width greater than the first width, forming a third pattern in the second pattern having a third width less than the second width, and forming a first trench on the substrate below the first pattern and a second trench below the second and third patterns. Effect of the Invention

[0006] A semiconductor device and a method for manufacturing the same are provided, which are capable of improving the uniformity of the depth of a trench isolation structure and the device performance of the semiconductor device. [Brief description of the drawings]

[0007] The accompanying drawings are included to provide a further understanding of the principles of the invention, and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.

[0008] [Figure 1] FIG. 1 is a cross-sectional view of a semiconductor device having radiation sensitive regions separated by trench isolation structures in accordance with some embodiments. [Diagram 2] FIG. 2 is a partial isometric view of a semiconductor device having radiation sensitive regions separated by trench isolation structures in accordance with some embodiments. [Diagram 3]FIG. 3 is a partial plan view of a semiconductor device having radiation sensitive regions separated by trench isolation structures in accordance with some embodiments. [Figure 4] 4A and 4B are partial cross-sectional views of a semiconductor device having radiation sensitive regions separated by trench isolation structures in accordance with some embodiments. [Diagram 5] 5A and 5B are partial plan views of additional trench fill structures of semiconductor devices in accordance with some embodiments. [Figure 6] FIG. 6 is a flow diagram illustrating a method of forming a semiconductor device having radiation sensing regions separated by trench isolation structures in accordance with some embodiments. [Figure 7] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 8] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 9] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 10] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 11] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 12] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 13]7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 14] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 15] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 16] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 17] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 18] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 19] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 20] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 21] 7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments. [Figure 22]7-22B are plan and cross-sectional views of semiconductor devices having radiation sensing regions separated by trench isolation structures at various stages of a fabrication process according to some embodiments.

[0009] Exemplary embodiments are now described with reference to the drawings, in which like reference numbers generally indicate identical, functionally similar, and / or structurally similar elements. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The following disclosure provides many different embodiments or examples for implementing different features of the provided subject matter. To simplify the invention, specific examples of components and arrangements are described below. These are, of course, merely examples and are not intended to be limiting. For example, forming on a first feature or on a second feature in the following description may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which the first and second features are not in direct contact, but an additional feature is formed between the first and second features. Furthermore, the present invention may repeat reference numbers and / or letters in various examples. This repetition is for purposes of simplicity and clarity and does not, in itself, dictate a relationship between the various embodiments and / or configurations discussed.

[0011] Additionally, spatially relative terms such as "below," "downward," "lower," "upward," "above," and the like may be used herein for ease of description to describe the relationship of one element or feature to another element or feature as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation shown in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptions used herein may be similarly interpreted accordingly.

[0012] It should be noted that the use of terms such as "one embodiment," "an embodiment," "exemplary embodiment," "exemplary," and the like in this specification indicates that a described embodiment may include a particular feature, structure, or characteristic, but not all embodiments necessarily include the particular feature, structure, or characteristic. Furthermore, such terms do not necessarily refer to the same embodiment. Furthermore, when a particular feature, structure, or characteristic is described in the context of one embodiment, it is believed to be within the knowledge of one of ordinary skill in the art to apply such feature, structure, or characteristic in the context of other embodiments, whether or not expressly described.

[0013] It is to be understood that the phraseology or terminology used herein is for the purpose of description rather than of limitation and should be interpreted by one of ordinary skill in the art in light of the teachings presented herein.

[0014] In some embodiments, the terms "about" and "substantially" can refer to a given amount of a value that varies within 5% of that value (e.g., ±1%, ±2%, ±3%, ±4%, ±5% of that value). These values ​​are merely examples and are not intended to be limiting. The terms "about" and "substantially" can refer to a percentage of a value that would be interpreted by one of ordinary skill in the art in light of the teachings provided herein.

[0015] A CMOS image sensor includes a semiconductor substrate (e.g., a silicon substrate) having an array of pixels or radiation sensitive regions formed therein. As disclosed herein, the terms "radiation sensitive region" and "pixel" are used interchangeably throughout the specification. The radiation sensitive region (or pixel) is configured to convert incident radiation into an electrical signal. The CMOS image sensor further includes a transfer transistor, a diffusion well, a source follower, a reset transistor, and in-pixel circuitry to distribute and process the electrical signal. The electrical signal is then passed to a signal processing element attached to the CMOS image sensor. For this reason, the pixel array covers a multilevel metallization layer (e.g., an interconnect structure) configured to allocate the electrical signal generated in the radiation sensitive region to the appropriate processing element.

[0016] The multi-layer metallization layer includes an interconnect structure formed on a first surface of the semiconductor substrate (herein referred to as the "front" surface of the semiconductor substrate). Additionally, the pixel array extends into the semiconductor substrate and is configured to receive radiation from a second surface of the semiconductor substrate opposite the front side of the semiconductor substrate. Here, the second surface of the semiconductor substrate that receives this radiation (and is opposite the front side of the semiconductor substrate) is referred to as the "back" surface of the semiconductor substrate.

[0017] Adjacent radiation sensing regions (or pixels) in the semiconductor substrate are electrically isolated with isolation structures, such as deep trench isolation (DTI) structures, to minimize crosstalk and signal loss between the radiation sensing regions. Each grid structure is aligned with the above-mentioned isolation structures (and formed on the back surface of the semiconductor substrate). Each said grid structure provides optical isolation between adjacent pixels or radiation sensing regions. Adjacent grid structures collectively form a cell.

[0018] By way of example and not limitation, the substrate having the radiation sensitive regions (or pixels), the processing elements, the multi-layer metallization layers, and the grating structure formed thereon may be attached via a wafer bonding structure to an application specific integrated circuit (ASIC) formed on a different substrate, which may be, for example, a CMOS wafer (fabricated separately from the CMOS image sensor device) configured to perform the signal processing operations described above.

[0019] A challenge for CMOS image sensors is the non-uniform depth of the trench isolation structures. The trench isolation structures can isolate radiation sensing regions horizontally and vertically. The trench isolation structures can meet at intersections. The intersections of the trench isolation structures can have a larger width than the horizontal and vertical straight portions. During the etching process to form the trenches, the trenches with the larger widths can have a larger depth due to the loading effect of the plasma etching process. The transfer transistors of the CMOS image sensor are located below the trench isolation structures. As a result, the deeper trenches at the intersections can damage at least a portion of the transfer transistors, degrading the device performance of the CMOS image sensor.

[0020] Various embodiments of the present invention provide examples of semiconductor devices having radiation sensing regions separated by trench isolation structures (e.g., separated by substantially uniform trench isolation structures) and examples of methods for fabricating the same. According to some embodiments, the semiconductor device may include an ASIC chip bonded to a first side (e.g., front side) of an image sensor chip. The image sensor chip may have a CMOS image sensor on its second side (e.g., back side). The radiation sensing regions of the CMOS image sensor may be isolated by trench isolation structures. The trench isolation structures may have straight portions between adjacent radiation sensing regions and intersection portions where the straight portions intersect. The intersection portions may have a width greater than the width of the straight portions. In some embodiments, the intersection trenches between the radiation sensing regions may form additional patterns at the intersection portions. As a result, the intersection portions may have a depth substantially the same as the depth of the straight portions. In some embodiments, the straight portions of the trench isolation structures may have a convex bottom surface and the intersection portions may have a concave bottom surface. In some embodiments, the difference between the depth of the intersection portions and the depth of the straight portions may range between about 1 Å and about 8000 Å. The ratio of the difference to the depth of the straight portions may be less than about 20%. In some embodiments, having additional patterns at the intersections can improve the depth uniformity of the trench isolation structures at the straight portions and intersections by about 20% to about 40%, and can improve the device performance of the CMOS image sensor by about 5% to about 10%.

[0021] FIG. 1 is a cross-sectional view of a semiconductor device 100 having radiation sensing regions 122 separated by a trench isolation structure 124 according to some embodiments. According to some embodiments, the trench isolation structure 124 may be a substantially uniform trench isolation structure. As shown in FIG. 1, the semiconductor device 100 may include a first chip 110 and a second chip 120 joined at an interface 130. The first chip 110 may be joined to a first side 120s1 of the second chip 120. In some embodiments, the first chip 110 may be an ASIC chip and may include a first substrate 102, a first dielectric layer 104, an application specific circuit 106, and a first interconnect structure 108. In some embodiments, the second chip 120 may be an image sensor chip having an image sensor device and may include a second substrate 112, a second dielectric layer 114, a second interconnect layer 118, a float device 116, a radiation sensing region 122, and a trench isolation structure 124. The radiation sensitive region 122 and the trench isolation structure 124 may be disposed on a second side 120s2 opposite the first side 120s1.

[0022] The first and second substrates 102 and 112 can each comprise a semiconductor material, such as silicon and germanium. In some embodiments, the first and second substrates 102 and 112 can comprise a crystalline silicon substrate (e.g., a wafer). In some embodiments, the first and second substrates 102 and 112 can comprise (i) an elemental semiconductor, such as germanium; (ii) a compound semiconductor, such as silicon carbide, gallium arsenide, gallium phosphide, indium arsenide, indium arsenide, and / or indium antimony; (iii) an alloy semiconductor, including silicon germanium carbide, silicon germanium, gallium arsenide phosphide, gallium indium phosphide, gallium indium arsenide, gallium indium arsenide phosphide, aluminum indium arsenide, and / or aluminum gallium arsenide; or (iv) a combination thereof. In some embodiments, the first and second substrates 102 and 112 can comprise the same semiconductor material. In some embodiments, the first and second substrates 102 and 112 may comprise different semiconductor materials. Additionally, the first and second substrates 102 and 112 may be doped depending on the design requirements (e.g., p-type substrates or n-type substrates). In some embodiments, the first and second substrates 102 and 112 may comprise silicon and may be doped with a p-type dopant (e.g., boron, indium, aluminum, or gallium) or an n-type dopant (e.g., phosphorus or arsenic).

[0023] Referring to FIG. 1, the first dielectric layer 104 can be disposed on the first substrate 102, and the second dielectric layer 114 can be disposed on the second substrate 112. The first and second dielectric layers 104 and 114 can be bonded at an interface 130. In some embodiments, the first and second dielectric layers 104 and 114 can each include a dielectric material such as silicon oxide (SiO2), silicon oxynitride (SiON), silicon nitride (SiNx), silicon oxycarbide (SiOC), silicon oxynitride carbide (SiOCN), and combinations thereof. In some embodiments, the first and second dielectric layers 104 and 114 can include the same dielectric material. In some embodiments, the first and second dielectric layers 104 and 114 can include different dielectric materials from each other. In some embodiments, the first and second dielectric layers 104 and 114 can include a stack of dielectric layers and can bond the first chip 110 to the second chip 120 .

[0024] In some embodiments, after bonding the first dielectric layer 104 to the second dielectric layer 114 at the interface 130, the first interconnect structure 108 can be bonded to the second interconnect structure 118 for electrical connection. The bond between the first chip 110 and the second chip 120 can include a dielectric-dielectric bond between the first dielectric layer 104 and the second dielectric layer 114 and a metal-metal bond between the first interconnect structure 108 and the second interconnect structure 118. The bond between the first chip 110 and the second chip 120 can be referred to as a "wafer bond." In some embodiments, the dielectric-dielectric bond can include an oxide-oxide bond. In some embodiments, the first dielectric layer 104 can have a vertical distance 104t (e.g., thickness) along the Z-axis in a range from about 2 μm to about 8 μm. The second dielectric layer 114 can have a vertical distance 114t (e.g., thickness) along the Z-axis in a range from about 2 μm to about 8 μm.

[0025] 1, the first interconnect structure 108 may be disposed in the first dielectric layer 104, and the second interconnect structure 118 may be disposed in the second dielectric layer 114. In some embodiments, each of the first and second interconnect structures 108 and 118 may include one or more metal lines and / or metal vias. The first and second interconnect structures 108 and 118 can include aluminum (Al), tungsten (W), copper (Cu), ruthenium (Ru), molybdenum (Mo), nickel (Ni), bismuth (Bi), scandium (Sc), titanium (Ti), cobalt (Co), silver (Ag), titanium nitride (TiN), tantalum nitride (TaN), tungsten nitride (WN), titanium carbide (TiC), titanium aluminum carbide (TiAlC), tantalum aluminum carbide (TaAlC), metal alloys, and other suitable conductive materials. The first and second interconnect structures 108 and 118 can connect the image sensor in the radiation sensitive region 122 on the second chip 120 to the application specific circuitry 106 on the first chip 110.

[0026] The application specific circuitry 106 may be disposed on the first substrate 102 and may be connected to the image sensor devices on the second chip 120 via first and second interconnect structures 108 and 118 and the float devices 116. The application specific circuitry 106 may include analog-to-digital converters (ADCs), counters, memory storage devices, and combinations thereof, to process the electrical signals generated by the image sensor devices on the second chip 120.

[0027] Referring to FIG. 1, the radiation sensing region 122 and the trench isolation structure 124 can be disposed on the second side 120s2 of the second chip 120. In some embodiments, the radiation sensing region 122 can include semiconductor materials such as silicon, germanium, and silicon germanium depending on the desired radiation wavelength. For example, silicon can be used for visible light applications (e.g., wavelengths between about 380 nm and 740 nm) and germanium can be used for infrared applications (e.g., wavelengths between about 940 nm and 1550 nm). Silicon germanium can be used for wavelengths between visible and infrared. By way of example and not limitation, additional materials that can be used for the radiation sensing region 122 include III-V group semiconductor materials such as gallium arsenide, gallium phosphide, indium phosphide, and gallium nitride. In some embodiments, the radiation sensing region 122 can include an image sensor device to convert sensed incident radiation into an electrical signal for further processing within the first chip 110.

[0028] In some embodiments, the float device 116 can be disposed in the second substrate 112 and between the radiation sensing region 122 and the second interconnect structure 118. In some embodiments, the float device 116 can include a transfer transistor and transfer an electrical signal generated by the radiation sensing region 122 to the second interconnect structure 118. In some embodiments, as shown in FIGS. 1 and 2, at least a portion of the float device 116 can be disposed under the trench isolation structure 124. FIG. 2 is an isometric view of a region 150 in the semiconductor device 100 shown in FIG. 1 according to some embodiments. For simplicity of illustration, the trench isolation structure 124 is not shown in FIG. 2.

[0029] The trench isolation structure 124 may be disposed between adjacent radiation sensing regions 122 to minimize crosstalk and signal loss between the radiation sensing regions 122. FIG. 3 is a plan view of a region 150 in the semiconductor device 100 shown in FIGS. 1 and 2 according to some embodiments. FIG. 4A is a cross-sectional view of the semiconductor device 100 taken along line A-A' shown in FIG. 3 according to some embodiments. FIG. 4B is a cross-sectional view of the semiconductor device 100 taken along line B-B' shown in FIG. 3 according to some embodiments. As shown in FIGS. 3, 4A, and 4B, the trench isolation structure 124 may include a straight portion 124A and an intersection portion 124B. The straight portion 124A may extend horizontally or vertically between adjacent radiation sensing regions 122. The intersection portion 124B may be located at the intersection of the horizontal straight portion and the vertical straight portion of the trench isolation structure 124.

[0030] 3, 4A, and 4B, the straight portion 124A of the trench isolation structure 124 can have a width 124Aw along line A-A' (e.g., the x-axis) in the range of about 40 nm to about 100 nm. The intersection portion 124B of the trench isolation structure 124 can have a width 124Bw along line B-B' in the range of about 80 nm to about 400 nm. In some embodiments, the ratio of width 124Bw to width 124Aw can be in the range of about 2 to about 4 due to corner rounding of the radiation sensing region 122 during formation of the trench isolation structure 124.

[0031] Referring to FIG. 4A, the straight portion 124A of the trench isolation structure 124 may have a depth 124Ad in the range of about 2 μm to about 4 μm along the Z axis. In some embodiments, the ratio of the depth 124Ad to the width 124Aw of the straight portion 124A may be in the range of about 20 to about 100. The ratio of the depth 124Ad to the width 124Aw may be referred to as the aspect ratio of the straight portion 124A of the trench isolation structure 124. Referring to FIG. 4B, the intersection portion 124B of the trench isolation structure 124 may have a depth 124Bd in the range of about 2 μm to about 4 μm along the Z axis. In some embodiments, the ratio of the depth 124Bd to the width 124Bw of the intersection portion 124B may be in the range of about 5 to about 50. The ratio of the depth 124Bd to the width 124Bw may be referred to as the aspect ratio of the intersection 124B of the trench isolation structure 124. In some embodiments, due to the high aspect ratio of the trench isolation structure 124, the trench isolation structure 124 may also be referred to as a deep trench isolation (DTI) structure. In some embodiments, the trench isolation structure 124 may be formed by filling the trench with an isolation material, such as silicon oxide and a high-k dielectric material. The term "high-k" may refer to a high dielectric constant. In the field of semiconductor device structures and manufacturing processes, high-k may refer to a dielectric constant greater than that of SiO2 (e.g., greater than about 3.9). High-k dielectric materials may include hafnium oxide (HfO2), zirconium oxide (ZrO2), and other suitable high-k dielectric materials. In some embodiments, the isolation material may fill the trench and may be deposited on the second side 120s2 of the second chip 120. Thus, the trench isolation structure 124 can also be referred to as a trench fill structure.

[0032] In some embodiments, the difference between the depths 124Ad and 124Bd may be less than about 8000 Å. The ratio of the difference to the depth 124Ad (i.e., the ratio of [depth 124Bd-depth 124Ad] to [depth 124Ad]) (referred to as the depth difference ratio) may be less than about 20%. If the difference is greater than about 8000 Å or the ratio is greater than about 20%, the intersection portion 124B of the trench isolation structure 124 may have a greater depth, which may damage the float device 116 below the trench isolation structure 124. By reducing the depth difference between the straight portion 124A and the intersection portion 124B of the trench isolation structure 124, the semiconductor device 100 may have a trench isolation structure 124 with a substantially uniform depth. As a result, damage to the float device 116 below the intersection portion 124B may be reduced, and the device performance of the semiconductor device 100 may be improved. In some embodiments, by making the depth difference ratio of the trench isolation structures 124 smaller than about 20%, the depth uniformity of the trench isolation structures 124 can be improved by about 20% to about 40%. According to some embodiments, by improving the depth uniformity, the device performance of the semiconductor device 100 can be improved by about 5% to about 10%.

[0033] 4A and 4B, the straight portion 124A of the trench isolation structure 124 can have a convex bottom surface 124As, and the intersection portion 124B can have a concave bottom surface 124Bs. As shown in FIG. 4B, the concave bottom surface 124Bs of the intersection portion 124B can include a first convex portion 124p1, a second convex portion 124p2, and a concave portion 124r. In some embodiments, the first convex portion 124p1 can have a width 124p1w in the range of about 40 nm to about 200 nm along the line B-B'. The second convex portion 124p2 can have a width 124p2w in the range of about 40 nm to about 200 nm along the line B-B'. In some embodiments, the ratio of the difference between the widths 124p1w and 124p2w to the width 124Bw (i.e., the ratio of [width 124p1w-width 124p2w] to [width 124Bw]) may be less than about 20%. If the ratio of the difference to the width 124Bw is greater than about 20%, the intersection portion 124B of the trench isolation structure 124 will have a greater depth, which may damage the float device 116 below the trench isolation structure 124.

[0034] In some embodiments, the distance 124pr along the Z axis between the recess 124r and the protrusions 124p1 and 124p2 may range from about 10 Å to about 2000 Å. The ratio of the distance 124pr to the depth 124Ad may range from about 0.02% to about 5%. If the distance is greater than about 2000 Å or the ratio is greater than about 5%, the intersections 124B of the trench isolation structures 124 may have a greater depth, which may damage the float device 116 below the trench isolation structures 124. If the distance is less than about 10 Å or the ratio is less than about 0.02%, the manufacturing cost of forming the trench isolation structures 124 may increase.

[0035] 5A and 5B are partial plan views of additional trench fill structures of the semiconductor device 100 according to some embodiments. In some embodiments, as shown in FIGS. 5A and 5B, the semiconductor device 100 can include trench fill structures 524A1 and 524B1 and trench fill structures 524A2 and 524B2. The trench fill structures 524A1 and 524A2 can have a width 524Aw along line A-A'. The trench fill structures 524B1 and 524B2 can have a width 524Bw along line B-B'. The ratio of the width 524Bw to the width 524Aw can range from about 2 to about 100. The depth difference ratio between the trench fill structures 524A1 and 524B1 and between the trench fill structures 524A2 and 524B2 can be less than about 20%. As a result, trench fill structures 524A1, 524B1, 524A2, and 524B2 can have a substantially uniform depth. According to some embodiments, by making the depths of trench fill structures 524A1, 524B1, 524A2, and 524B2 substantially uniform, device performance of semiconductor device 100 can be improved by about 5% to about 10%.

[0036] In some embodiments, as shown in FIG. 1, the semiconductor device 100 may further include a color filter 152, a metal grid 154, and a microlens 156. The color filter 152 may be disposed on the second side 120s2 of the second chip 120 and covering the radiation sensing region 122. In some embodiments, the color filter 152 may include red, green, and blue filters. The metal grid 154 may be disposed on the second side 120s2 of the second chip 120 and covering the trench isolation structure 124. The color filter 152 may be disposed between sidewalls of the metal grid 154. The microlens 156 may be disposed on the second side 120s2 of the second chip 120 and covering the color filter 152, and therefore may be disposed to cover the radiation sensing region 122. Incident radiation may enter the radiation sensing region 122 through the microlens 156, the color filter 152, and the isolation material on the second side 120s2 of the second chip 120.

[0037] FIG. 6 is a flow diagram illustrating an example of a method 600 for forming a semiconductor device 100 having radiation sensing regions separated by trench isolation structures according to some embodiments. In some embodiments, the trench isolation structures may be substantially uniform to one another. The method 600 is not limited to forming trench isolation structures in the semiconductor device 100. The method 600 may be applied to forming trench isolation structures in other suitable semiconductor devices, such as three-dimensional (3D) deep trench capacitors (DTC), 3D metal-insulator-metal (MIM) capacitors, and shallow trench isolation and silicon trenches in CMOS devices. Additional processes may be performed between the operations of the method 600, but are not described here for the sake of brevity. The additional processes may be provided before, during, and / or after the method 600. One or more of these additional processes will now be briefly described. Furthermore, it is not necessary to perform all of the operations provided herein. Also, some of the operations may be performed simultaneously or in a different order than that shown in FIG. 6. In some embodiments, one or more other operations may be performed in addition to, or instead of, the operations described hereinafter.

[0038] By way of example, the operations shown in Figure 6 will be described with reference to an example manufacturing process for forming the semiconductor device 100 shown in Figures 7-22B. Figures 7-22B show plan and cross-sectional views of a semiconductor device 100 having radiation sensing regions 122 separated by trench isolation structures 124 (e.g., substantially uniform trench isolation structures) at various stages of a manufacturing process according to some embodiments. Components in Figures 7-22B will be described using the same annotations as components in Figures 1-4B.

[0039] Referring to FIG. 6, the method 600 begins in operation 610 with a process of forming a first pattern having a first width and a second pattern having a second width greater than the first width on a substrate. For example, as shown in FIG. 7, FIG. 8A, and FIG. 8B, a first pattern 724A and a second pattern 724B can be formed on the second substrate 112. In some embodiments, as shown in FIG. 7, the first pattern 724A can be a straight line portion and the second pattern 724B can be an intersection portion of the pattern 724 formed on the second substrate 112. The first pattern 724A can have a first width 724Aw in a range of about 40 nm to about 100 nm along a line A-A'. The second pattern 724B can have a second width 724Bw in a range of about 80 nm to about 400 nm along a line B-B'. In some embodiments, the second width 724Bw may be greater than the first width 724Aw, and the ratio of the second width 724Bw to the first width 724Aw may be in the range of about 2 to about 4 due to the R chamfering effect during formation of the first and second patterns 724A and 724B.

[0040] Forming the first and second patterns 724A and 724B may include forming a mask layer 732 on the second substrate 112 and patterning the mask layer 732. The mask layer 732 may be blanket deposited on the second substrate 112 by chemical vapor deposition (CVD), physical vapor deposition (PVD), and / or other suitable deposition methods. The composition of the mask layer 732 may be SiO x , SiN x, SiON, and / or other suitable materials. The patterning process includes depositing a photoresist on the mask layer 732, exposing the photoresist to a pattern, performing a post-exposure bake process, and developing the photoresist to form a masking element comprising the photoresist. The masking element can be used to sequentially remove exposed areas of the mask layer 732 by one or more etching processes while protecting covered areas of the hard mask layer 732. In some embodiments, the mask layer 732 can have a thickness along the Z-axis in a range from about 10 nm to about 1000 nm.

[0041] 6, in operation 620, a third pattern may be formed in the second pattern. The third pattern may have a third width that is less than the second width. For example, as shown in FIGS. 9A-12, a third pattern 1136 may be formed in the second pattern 724B. The third pattern 1136 may have a width 1136w that is less than the second width 724Bw. In some embodiments, forming the third pattern 1136 may include depositing a coating layer 934 on the first and second patterns 724A and 724B, forming a mask structure 1036 on the coating layer 934 and above the second pattern 724B, and etching the mask structure 1036 and the coating layer 934.

[0042] In some embodiments, the coating layer 934 can be blanket deposited on the mask layer 732 to cover the first and second patterns 724A and 724B. In some embodiments, the coating layer 934 can include a carbon-based dielectric material blanket deposited by CVD, PVD, atomic layer deposition (ALD), and / or other deposition techniques. In some embodiments, the coating layer 934 can be a bottom anti-reflection coating (BARC) including a carbon-based dielectric material. The coating layer 934 can fill the openings of the first and second patterns 724A and 724B.

[0043] 10B, following deposition of the coating layer 934, a mask structure 1036 may be formed above the second pattern 724. In some embodiments, the mask structure 1036 may be formed by a patterning process. The patterning process includes depositing a photoresist on the coating layer 934, exposing the photoresist to a pattern, performing a post-exposure bake process, and developing the photoresist to form the mask structure 1036. In some embodiments, the mask structure 1036 may include a carbon-based or silicon-based photoresist. In some embodiments, the mask structure 1036 may include one or more layers of a dielectric material.

[0044] In some embodiments, as shown in FIG. 10B, the mask structure 1036 can have a width 1036w in the range of about 40 nm to about 600 nm along the line B-B′. The width 1036w can be larger or smaller than the second width 724Bw depending on the subsequent etching process. After a series of etching processes, the width 1036w of the mask structure 1036 can be reduced. In some embodiments, the ratio of the width 1036w to the second width 724Bw can be in the range of about 50% to about 150%. If the ratio is less than about 50%, the first and second patterns 724A and 724B may not form a trench having a substantially uniform depth after the subsequent etching process. If the ratio is more than about 150%, the second pattern 724B may be blocked by the mask structure 1036 and may not form a trench in the second substrate 112.

[0045] As shown in FIGS. 11A, 11B, and 12, following the formation of the mask structure 1036, the mask structure 1036 and the coating layer 934 can be etched to form the third pattern 1136. In some embodiments, the mask structure 1036 and the coating layer 934 can be etched by a dry etching process. In some embodiments, the dry etching process can be a directional etching process performed at a temperature of about 0° C. to about 60° C. and a pressure of about 10 mTorr to about 100 mTorr. The dry etching process can use an etchant including oxygen plasma and argon plasma. After the dry etching process, the coating layer 934 in the first pattern 724A can be removed to leave a portion of the coating layer 934 in the second pattern 724B to form the third pattern 1136. In some embodiments, the third pattern 1136 can have a width 1136w along the line B-B′. The width 1136w can be less than the width 124Bw. In some embodiments, the width 1136w may range from about 60 nm to about 300 nm.

[0046] 6, in operation 630, a first trench is formed under the first pattern and a second trench is formed under the second and third patterns. For example, as shown in FIGS. 13A and 13B, a first trench 1324A can be formed under the first pattern 724A, and a second trench 1324B can be formed under the second and third patterns 724B and 1136. In some embodiments, the first and second trenches 1324A and 1324B can be formed by a plasma etching process. In some embodiments, the plasma etching process can etch the semiconductor material with an etchant including chlorine (Cl2) or hydrogen bromide (HBr). In some embodiments, the etchant can include a fluorine-based plasma, such as sulfur hexafluoride (SF6), nitrogen trifluoride (NF3), and carbon tetrafluoride (CF4). In some embodiments, the plasma etch process can include a Bosch etch process that uses an etchant SF6 during the etch cycle and perfluoroisobutylene (C4F8) during the deposition cycle. In some embodiments, the plasma etch process can include an etchant that includes CF4, difluoromethane (CH2F2), trifluoromethane (CHF3), C4F8, octafluorocyclopentene (C5F8), hexafluoropropene (C3F6), argon, oxygen, and combinations thereof to etch SiO2. xIn some embodiments, the plasma etching process can be performed at a temperature between about 0° C. and about 60° C. and a pressure between about 10 mTorr and about 100 mTorr. In some embodiments, the plasma etching process can be performed for about 20 minutes to about 60 minutes to form the first and second trenches 1324A and 1324B.

[0047] In some embodiments, the first trench 1324A in the second substrate 112 can have a depth 1324Ad along the Z axis in a range of about 2 μm to about 4 μm. As shown in FIG. 4A, the depth 1324Ad can be substantially the same as the depth 124Ad. The second trench 1324B in the second substrate 112 can have a depth 1324Bd along the Z axis in a range of about 2 μm to about 4 μm. As shown in FIG. 4B, the depth 1324Bd can be substantially the same as the depth 124Bd. In some embodiments, the first trench 1324A and the second trench 1324B can have substantially the same depth. The difference between the depth 1324Ad and the depth 1324Bd can be less than about 8000 Å. The ratio of the difference to the depth 1324Ad (i.e., the ratio of [depth 1324Ad-depth 1324Bd] to [depth 1324Ad]) (also referred to as the depth difference ratio) may be less than about 20%. In some embodiments, after the plasma etching process, a protrusion 112p may be formed on the second substrate 112 at the bottom surface of the second trench 1324B. As shown in FIG. 13B, the distance 112pr between the upper surface of the protrusion 112p and the bottom surface of the second trench 1324B may be in the range of about 10 Å to about 2000 Å, similar to the distance 124pr shown in FIG. 4B. The ratio of the distance 112pr to the depth 1324Ad may be in the range of about 0.02% to about 5%. In some embodiments, the distances 112p1w and 112p2w along line B-B' between the protrusion 112p and adjacent sidewalls of the second trench 1324B can range from about 40 nm to about 200 nm. The ratio of the difference between the widths 112p1w and 112p2w to the width 124Bw (i.e., the ratio of [width 112p1w-width 112p2w] to [width 1324Bw]) can be less than about 20%.

[0048] By reducing the depth difference between the first trench 1324A and the second trench 1324B, the semiconductor device 100 can have trenches of substantially uniform width with a depth difference ratio of less than about 20%. As a result, damage to the float device 116 below the second trench 1324B can be reduced, and the device performance of the semiconductor device 100 can be improved. In some embodiments, by having the third pattern 1136, the depth uniformity of the first and second trenches 1324A and 1324B can be improved by about 20% to about 40%. By improving the depth uniformity of the first and second trenches 1324A and 1324B, the device performance of the semiconductor device 100 can be improved by about 5% to about 10%.

[0049] As shown in FIGS. 4A and 4B, following the formation of the first trench 1324A and the second trench 1324B, the trench isolation structure 124 may be formed. The formation of the trench isolation structure 124 may include filling the first trench 1324A and the second trench 1324B with a dielectric material, such as silicon oxide. In some embodiments, the dielectric material may be deposited using a deposition method suitable for the flowable dielectric material. For example, flowable chemical vapor deposition (FCVD) may be used to deposit the flowable silicon oxide. After filling the first trench 1324A and the second trench 1324B, the radiation sensing region 122 may be formed on the second substrate 112 and between the trench isolation structures 124. Subsequently, a chemical mechanical polishing (CMP) process may be used to remove the mask layer 732 and planarize the top surfaces of the trench isolation structure 124 and the radiation sensing region 122.

[0050] In some embodiments, the third pattern can be formed in the second pattern without the additional patterning process shown in FIG. 10A and FIG. 10B. For example, a self-aligned patterning process can be used to form the third pattern 2036, as shown in FIG. 14-FIG. 22B. A first pattern 1424A and a second pattern 1424B can be formed on the second substrate 112, as shown in FIG. 14, FIG. 15A, and FIG. 15B. In some embodiments, the first pattern 1424A can be a straight portion of the pattern 1424 formed on the second substrate 112, and the second pattern 1424B can be an intersection portion, as shown in FIG. 14, FIG. 15A, and FIG. 15B. The first pattern 1424A can have a first width 1424Aw in the range of about 40 nm to about 100 nm along the line A-A'. The second pattern 1424B can have a second width 1424Bw ranging from about 80 nm to about 400 nm along line B-B'. In some embodiments, the width 1424Bw can be greater than the width 1424Aw, and the ratio of the width 1424Bw to the width 1424Aw can range from about 2 to about 4 due to the radius chamfer effect during forming the first and second patterns 1424A and 1424B.

[0051] Forming the first and second patterns 1424A and 1424B includes forming a first etch stop layer (ESL) 1438 on the second substrate 112, forming a mask layer 1432 on the first ESL 1438, forming a second ESL 1442 on the mask layer 1432, and patterning the second ESL 1442 and the mask layer 1432. The first ESL 1438, the mask layer 1432, and the second ESL 1442 may be blanket deposited, in order, on the second substrate 112 by CVD, PVD, and / or other suitable deposition methods. The composition of the mask layer 1432 is SiO x , SiN x The components of the first and second ESLs 1438 and 1442 may include SiN, SiON, and / or other suitable materials.x , silicon carbide (SiC), silicon carbonitride (SiCN), and / or other suitable materials. In some embodiments, first and second ESLs 1438 and 1442 can comprise the same dielectric material. In some embodiments, mask layer 1432 can comprise a dielectric material having a different etch rate than the dielectric material of first and second ESLs 1438 and 1442. In some embodiments, first and second ESLs 1438 and 1442 can comprise SiN x and the mask layer 1432 can include SiO x may include.

[0052] The patterning process includes depositing photoresist on the second ESL 1442, exposing the photoresist to a pattern, performing a post-exposure bake process, and developing the photoresist to form a masking element comprising the photoresist. The masking element can be used to sequentially remove the exposed areas of the second ESL 1442 and the mask layer 1432 by one or more etching processes while protecting the covered areas of the second ESL 1442. In some embodiments, the first ESL layer 1438 can have a thickness 1438t along the Z-axis in a range from about 1 nm to about 50 nm. The mask layer 1432 can have a thickness 1432t along the Z-axis in a range from about 10 nm to about 1000 nm. The second ESL 1442 can have a thickness 1442t along the Z-axis in a range from about 1 nm to about 50 nm.

[0053] As shown in FIGS. 17A and 17B, following the formation of the first and second patterns 1424A and 1424B, a dielectric layer 1644 can be deposited on the second ESL 1442. In some embodiments, the dielectric layer 1644 can be blanket deposited on the second ESL 1442 by CVD, ALD, and / or other suitable deposition methods. After depositing the dielectric layer 1644, the first pattern 1424A can be filled and the second pattern 1424B can have an opening. In some embodiments, the dielectric layer 1644 can have a thickness 1644t in the range of about 50 nm to about 100 nm. In some embodiments, the dielectric layer 1644 can be SiO. x , SiON, and / or other suitable materials.

[0054] 17A and 17B, following deposition of the dielectric layer 1644, a coating layer 1746 may be deposited on the dielectric layer 1644. In some embodiments, the coating layer 1746 may be blanket deposited on the dielectric layer 1644 by CVD, ALD, and / or other suitable deposition methods. After depositing the coating layer 1746, the second pattern 1424B may be filled. In some embodiments, the coating layer 1746 may be a BARC layer including a carbon-based dielectric material.

[0055] As shown in FIGS. 18A-21, following deposition of the coating layer 1746, a third pattern 2036 can be formed in the second pattern 1424B. Formation of the third pattern 2036 can include etching the coating layer 1746, etching the dielectric layer 1644, and etching the first and second ESLs 1438 and 1442. As shown in FIGS. 18A and 18B, the coating layer 1746 can be etched by a plasma etching process to form a first mask structure 1846 in the openings of the second pattern 1424B. In some embodiments, the plasma etching process can include an etchant, such as an oxygen plasma. In some embodiments, after the plasma etching process, the first mask structure 1846 can have a thickness 1846t along the Z-axis in a range of about 50 nm to about 100 nm.

[0056] As shown in FIGS. 19A and 19B, following the etching of the coating layer 1746, the dielectric layer 1644 can be etched. In some embodiments, the dielectric layer 1644 can be etched by a plasma etching process. The plasma etching process can be a directional etching process and can include fluorine-based etchants, argon, oxygen, and other suitable etchants. After the plasma etching process, the dielectric layer 1644 in the first pattern 1424A can be removed. Portions of the dielectric layer 1644 can be left in the openings of the second pattern 1424B and below the first mask structure 1846 to form a second mask structure 1944.

[0057] As shown in FIGS. 20A, 20B, and 21, following the etching of the dielectric layer 1644, the first and second ESLs 1438 and 1442 can be etched. In some embodiments, the first and second ESLs 1438 and 1442 can be etched by a plasma etching process. The plasma etching process can include an etchant such as CF4 and other suitable etchants. After the plasma etching process, the second ESL 1442 and the exposed first ESL 1438 can be removed. A portion of the first ESL 1438 can be left in the opening of the second pattern 1424B and below the second mask structure 1944 to form a third mask structure 2038. In some embodiments, the second mask structure 1944 and the third mask structure 2038 can function as a third pattern 2036. Because there is no additional patterning process to form the third pattern 2036, the formation of the third pattern 2036 can be referred to as a self-aligned patterning process. In some embodiments, the third pattern 2036 can have a width 2036w along line B-B'. The width 2036w can be less than the width 1424Bw. In some embodiments, the width 2036w can be in the range of about 60 nm to about 300 nm.

[0058] As shown in FIGS. 22A and 22B, following the formation of the third pattern 2036, the first and second trenches 2224A and 2224B can be formed. In some embodiments, the first trench 2224A can be formed below the first pattern 1424A and the second trench 2224B can be formed below the second and third patterns 1424B and 2036 by a plasma etching process. The plasma etching process can be the same as the plasma etching process that forms the first and second trenches 1324A and 1324B shown in FIGS. 13A and 13B. In some embodiments, the first and second trenches 2224A and 2224B can have substantially the same depth. In some embodiments, after the plasma etching process, a protrusion 2212p can be formed on the second substrate 112 at the bottom of the second trench 2224B. In some embodiments, the distances 2212p1w and 2212p2w along the line B-B' between the adjacent sidewalls of the protrusion 2212p and the second trench 2224B can range from about 40 nm to about 200 nm. The ratio of the difference between the width 212p1w and the width 212p2w to the width 2224Bw (i.e., the ratio of [width 212p1w-width 212p2w] to [width 2224Bw]) can be less than about 10%. Compared with the trenches 1324A and 1324B of FIG. 13A and FIG. 13B, the trenches 2224A and 2224B formed by the self-aligned patterning process can improve the depth uniformity, resulting in an improved symmetric protrusion 2212p.

[0059] The formation of the first and second trenches 2224A and 2224B can be followed by the formation of the trench isolation structure 124 shown in Figures 4A and 4B, the formation of the radiation sensing region 122, and a subsequent CMP process. Although the present invention describes a method for forming the trench isolation structure 124 (e.g., having a substantially uniform depth) in the semiconductor device 100, the method may be applied to the formation of trenches of substantially uniform depth having different widths for use in other semiconductor devices.

[0060] Various embodiments of the present invention provide examples of semiconductor devices 100 having radiation sensing regions 122 separated by deep trench isolation structures 124 (e.g., substantially uniform trench isolation structures). According to some embodiments, the semiconductor device 100 may include a first chip 110 bonded to a first side 120s1 of a second chip 120. The second chip 120 may have radiation sensing regions 122 on its second side 120s2. The radiation sensing regions 122 may be isolated by trench isolation structures 124. The trench isolation structures 124 may have straight portions 124A between adjacent radiation sensing regions 122 and intersection portions 124B where the straight portions 124A intersect. The intersection portions 124B may have a width 124Bw that is greater than the width 124Aw of the straight portions 124A. In some embodiments, the intersection portions 124Bw between the radiation sensing regions 122 may form a third pattern 1136 or a third pattern 2036 at the intersection portions. As a result, the intersection portion 124Bw can have a depth 124Bd that is substantially the same as the depth 124Ad of the straight portion 124A. In some embodiments, the straight portion 124A of the trench isolation structure 124 can have a convex bottom surface 124As, and the intersection portion 124B can have a concave bottom surface 124Bs. In some embodiments, the difference between the depth 124Ad and the depth 124Bd can range between about 1 Å and about 8000 Å. The ratio of the difference to the depth 124Ad of the straight portion 124A can be less than about 20%. In some embodiments, having the third pattern 1136 or 2036 at the intersection portion can improve the depth uniformity of the trench isolation structure 124 at the straight portion 124A and the intersection portion 124B by about 20% to about 40%, and can improve the device performance of the semiconductor device 100 by about 5% to about 10%.

[0061] In some embodiments, a semiconductor structure includes a first trench fill structure on a substrate and a second trench fill structure on the substrate, the first trench fill structure having a first width and a convex bottom surface, and the second trench fill structure having a concave bottom surface and a second width greater than the first width. In one embodiment, the first trench filling structure has a first depth. The second trench filling structure has a second depth. A ratio of the difference between the first and second depths to the first depth is less than 20%. In one embodiment, the second trench filling structure further includes a protrusion and a recess at the concave bottom surface. A distance between the protrusion and the recess is in the range of 10 Å to 2000 Å. In one embodiment, a ratio of the distance to the depth of the first trench filling structure is in the range of 0.02% to 5%. In one embodiment, the first trench filling structure has a depth. A ratio of the depth to the first width is in the range of 20 to 100. In one embodiment, the depth is in the range of 2 μm to 4 μm. In one embodiment, the second trench filling structure has a depth. A ratio of the depth to the second width is in the range of 5 to 50. In one embodiment, a ratio of the second width to the first width is in the range of 2 to 100. In one embodiment, the first width is in the range of 40 nm to 100 nm, and the second width is in the range of 80 nm to 400 nm.

[0062] In some embodiments, the semiconductor device includes a first chip. The first chip includes a plurality of pixels on a first side of the first chip, and first and second trench fill structures isolating the plurality of pixels. The first trench fill structure has a convex bottom surface. The second trench fill structure is in contact with the first trench fill structure. The second trench fill structure has a concave bottom surface. The semiconductor device further includes a second chip bonded to a second side of the first chip. The second side is opposite the first side. In one embodiment, the first trench filling structure has a first depth. The second trench filling structure has a second depth. A ratio of the difference between the first and second depths to the first depth is less than 20%. In one embodiment, the second trench filling structure includes a protrusion and a recess at a concave bottom surface. A ratio of the distance between the protrusion and the recess to the depth of the first trench filling structure is in the range of 0.02%-5%. In one embodiment, the first trench filling structure has a first width. The second trench filling structure has a second width. A ratio of the second width to the first width is in the range of 2-100.

[0063] In some embodiments, a method includes forming a first pattern on a substrate having a first width and a second pattern having a second width greater than the first width, forming a third pattern in the second pattern having a third width less than the second width, and forming a first trench on the substrate below the first pattern and a second trench below the second and third patterns. In one embodiment, forming the first and second patterns includes depositing a mask layer on the substrate and etching the mask layer into the first and second patterns. In one embodiment, forming the third pattern includes depositing a dielectric material on the first and second patterns, forming a mask structure on the dielectric material above the second pattern, and etching the dielectric material and the mask structure. In one embodiment, forming the first and second patterns includes depositing a first etch stop layer on the substrate, depositing a mask layer on the first etch stop layer, depositing a second etch stop layer on the mask layer, and etching the mask layer and the second etch stop layer. In one embodiment, forming the third pattern includes depositing a dielectric material on the first and second patterns to fill the first pattern, depositing a coating layer on the dielectric material to fill the second pattern, etching the coating layer and the dielectric material to form a mask structure in the second pattern, and removing the first etch stop layer exposed by the first pattern, the mask structure, and the second pattern. In one embodiment, forming the first trench and the second trench includes etching the substrate having the first, second, and third patterns with a fluorine-based plasma. In one embodiment, the method further includes filling the first and second trenches with a dielectric material.

[0064] It should be understood that the Detailed Description section, and not the Abstract section, is intended to be used to interpret the claims. The Abstract section may set forth one or more, but not all, possible embodiments of the invention contemplated by the inventors, and as such is not intended to limit the scope of the appended claims.

[0065] The foregoing disclosure outlines features of several embodiments so that those skilled in the art may better understand aspects of the present invention. Those skilled in the art will appreciate that they may readily use the present invention as a basis for designing or modifying other processes and structures for carrying out the same purposes and / or achieving the same advantages of the embodiments introduced herein. Those skilled in the art should also appreciate that such equivalent constructions do not depart from the spirit and scope of the present invention, and that various changes, substitutions, and alterations may be made therein without departing from the spirit and scope of the present invention. [Industrial Applicability]

[0066] The present invention provides various embodiments of semiconductor devices having radiation sensitive regions separated by deep trench isolation structures (e.g., substantially uniform trench isolation structures) that can improve device performance of the semiconductor device and depth uniformity of the trench isolation structures at lines and intersections. [Explanation of symbols]

[0067] 100 Semiconductor device 102 First board 104 First dielectric layer 104t vertical distance 106 Circuit 108 First interconnect structure 110 First Chip 112 Second board 112p, 2212p convex 112p1w, 112p2w, 2212p1w, 2212p2w distance / width 114 Second dielectric layer 116 Float Device 118 Second interconnect structure 120 2nd Chip 120s1 1st side 120s2 2nd side 122 Radiation Sensing Area 124 Trench isolation structure 124A Straight section 124B Intersection 124Aw, 124Bw, 124p1w, 124p2w, 524Aw, 524Bw, 1136w, 1036w, 1324Bw, 2036w, 1424Bw, 2224Bw width 124Ad, 124Bd, 1324Ad, 1324Bd Depth 124p1 First protrusion 124p2 Second convex part 124As Convex bottom 124Bs Concave bottom 124pr, 112pr distance 124r Recess 130 Interface 150 areas 152 Color Filter 154 Metal grid 156 Micro Lens 524A1, 524B1, 524A2, 524B2 Trench filling structure 600 ways 610, 620, 630 operations 724A, 1424A 1st pattern 724B, 1424B 2nd pattern 724, 1424 patterns 724Aw, 1424Aw 1st width 724Bw, 1424Bw 2nd width 732, 1432 Mask Layer 732t, 1438t, 1432t, 1442t, 1644t, 1846t thickness 934 Coating layer 1036 Mask Structure 1136, 2036 3rd pattern 1324A, 2224A First Trench 1324B, 2224B 2nd trench 1438 1st ESL 1442 2nd ESL 1644 Dielectric layer 1746 Coating Layer 1846 First Mask Structure 1944 Second Mask Structure 2038 3rd mask structure

Claims

1. a trench isolation structure including a first trench fill structure on a substrate and a second trench fill structure on the substrate; a transfer transistor disposed in the substrate and below the second trench fill structure; Equipped with the first trench fill structure is a straight portion of the trench isolation structure; the first trench fill structure has a first width, a first depth, and a convex bottom surface; the second trench fill structure is an intersection of the trench isolation structure; the second trench fill structure is in contact with the first trench fill structure; The second trench filling structure comprises: A concave bottom surface; a second width greater than the first width; The second trench fill structure has a second depth substantially equal to the first depth. A semiconductor structure having

2. 2. The semiconductor structure of claim 1, wherein a ratio of a difference between the first depth and the second depth to the first depth is less than 20%.

3. 2. The semiconductor structure of claim 1, wherein the second trench fill structure further comprises a protrusion and a recess at the concave bottom surface, a distance between the protrusion and the recess ranges from 10 Å to 2000 Å, and a ratio of the distance to the first depth ranges from 0.02% to 5%.

4. 2. The semiconductor structure of claim 1, wherein a ratio of said first depth to said first width is in the range of 20 to 100, and said first depth is in the range of 2 μm to 4 μm.

5. 2. The semiconductor structure of claim 1, wherein a ratio of said second depth to said second width is in the range of 5-50 and a ratio of said second width to said first width is in the range of 2-100.

6. A first chip; a second chip joined to a second side of the first chip; Including, The first chip is a plurality of pixels on a first side of the first chip; a trench isolation structure isolating the plurality of pixels from one another, the trench isolation structure including straight portions as a first trench fill structure and crossing portions as a second trench fill structure; a transfer transistor disposed within a substrate of the first chip and beneath the second trench fill structure; the first trench fill structure has a convex bottom surface, a first width, and a first depth; the second trench fill structure is in contact with the first trench fill structure; the second trench fill structure has a concave bottom surface, a second width greater than the first width, and a second depth substantially the same as the first depth; The semiconductor device, wherein the second side is opposite the first side.

7. forming a first pattern on a substrate having a first width and a second pattern on a substrate having a second width greater than the first width, the second pattern overlying a transfer transistor disposed in the substrate; forming a third pattern in the second pattern, the third pattern having a third width less than the second width; forming on the substrate a first trench having a first depth below the first pattern and a second trench having a second depth substantially the same as the first depth below the second and third patterns, the first trench constituting a straight portion of an isolation trench and the second trench constituting an intersection portion of the isolation trench, the second trench being connected to the first trench; A method for manufacturing a semiconductor device comprising the steps of:

8. forming the first pattern and the second pattern; depositing a mask layer on the substrate; Etching the mask layer into the first and second patterns; Including, And, forming the third pattern, depositing a dielectric material over the first pattern and the second pattern; forming a mask structure on the dielectric material above the second pattern; Etching the dielectric material and the mask structure; 8. The method of claim 7, comprising:

9. Forming the first pattern and the second pattern, depositing a first etch stop layer over the substrate; depositing a mask layer over the first etch stop layer; depositing a second etch stop layer over the mask layer; Etching the mask layer and the second etch stop layer; Including, And, forming the third pattern, depositing a dielectric material over the first and second patterns to fill the first pattern; depositing a coating layer over the dielectric material to fill the second pattern; Etching the coating layer and the dielectric material to form a mask structure in the second pattern; removing the first etch stop layer exposed by the first pattern, the mask structure, and the second pattern; 8. The method of claim 7, comprising:

10. The method of claim 7, wherein forming the first trench and the second trench comprises etching the substrate having the first, second, and third patterns with a fluorine-based plasma.

Citation Information

Patent Citations

  • Method for forming vertical structures in a semiconductor target layer

    EP3067919A1

  • Semiconductor device and its manufacture

    JP2000156402A

  • Trench element isolation type semiconductor device and its manufacturing method

    JP2002100675A

  • Solid-state image pickup device, manufacturing method thereof, and camera using the same

    JP2005251945A

  • Electronic device manufacturing method and electronic device

    JP2007513782A