Semiconductor Device

The semiconductor device addresses leakage current and electric field concentration issues by using a three-layer drift layer and extended gate electrode, along with a thickened gate oxide film, to improve breakdown voltage and reduce defects, ensuring efficient operation.

JP7563861B2Active Publication Date: 2024-10-08LAPIS SEMICON CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2023115530
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-07-13
Publication Date
2024-10-08
Estimated Expiration
2038-03-29

AI Technical Summary

Technical Problem

Semiconductor devices with LDMOS transistors face issues such as minute leakage currents due to vertical electric fields, leading to defects and reduced withstand voltage, and electric field concentration at STI sections, which increases impact ionization rates and decreases breakdown voltage.

Method used

The semiconductor device incorporates a semiconductor substrate with a source and drain region, a three-layer drift layer with varying impurity concentrations, an extended gate electrode, and a thickened gate oxide film to disperse electric field concentration and reduce leakage currents, thereby improving breakdown voltage.

Benefits of technology

The solution effectively reduces local electric field concentrations, suppresses defects, and enhances withstand voltage by dispersing electric fields and minimizing leakage currents, maintaining high breakdown voltage without increasing on-resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007563861000001
    Figure 0007563861000001
  • Figure 0007563861000002
    Figure 0007563861000002
  • Figure 0007563861000003
    Figure 0007563861000003
Patent Text Reader

Abstract

To provide a semiconductor device including a high breakdown voltage semiconductor element structure capable of reducing local concentration of electric fields, suppressing occurrence of a defect due to a minute leak current, and improving a breakdown voltage.SOLUTION: A semiconductor device includes: a semiconductor substrate; a first conductivity type source region formed in one principal surface of the semiconductor substrate; a first conductivity type drain region formed in the one principal surface and connected to the source region via a channel region; a gate electrode formed on the channel region via an insulation film; a first conductivity type drift region formed between a lower part of the gate electrode and the drain region; a groove including an opening having one end in the lower part of the gate electrode and the other end in a position in contact with the drain region and formed in the semiconductor substrate at a predetermined depth through the drift layer from the one principal surface; and an electric field relaxation unit provided near the one end and for relaxing an electric field generated between the source region and the drain region.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device, for example, a semiconductor device having a high-voltage element with an LDMOS (Laterally Diffused Metal Oxide Semiconductor) transistor structure. [Background technology]

[0002] The LDMOS transistor structure refers to a structure in which impurities near the drain are diffused laterally, and is intended to reduce the electric field strength between the drain and gate. Various studies have been conducted on LDMOS transistors from the viewpoints of the transistor's withstand voltage, on / off resistance, ESD (ElectroStatic Discharge) withstand voltage, etc.

[0003] As a conventional technique related to a semiconductor device having an LDMOS transistor, for example, Patent Document 1 discloses a semiconductor device including an N-type drift diffusion region formed on an upper portion of a semiconductor substrate, a P-type body diffusion region formed on an upper portion of the semiconductor substrate, an N-type source diffusion region formed on an upper portion of the body diffusion region, an insulating film formed in a trench formed on an upper portion of the drift diffusion region and spaced apart from the body diffusion region, an N-type drain diffusion region formed on an upper portion of the drift diffusion region and adjacent to the source diffusion region in the opposite direction as viewed from the insulating film, and a gate electrode formed from above the body diffusion region to above the drift diffusion region and onto the insulating film with a gate insulating film sandwiched therebetween, the drift diffusion region having a substrate inner region and a surface region formed on the substrate inner region and under the gate electrode and containing a higher concentration of N-type impurities than the substrate inner region. Patent Document 1 claims that the above configuration makes it possible to maintain the breakdown voltage performance and reduce the on-resistance in the LDMOS transistor.

[0004] Patent Document 2 discloses a field effect transistor including an N-type drift region disposed between a region of a semiconductor substrate that becomes a channel and an N-type drain, a field oxide film disposed on the drift region, and a P-type first impurity diffusion layer disposed below the drift region in the semiconductor substrate, the drift region having an N-type first drift layer and a second drift layer disposed on the first drift layer and having a higher N-type impurity concentration than the first drift layer. Patent Document 2 claims that the above configuration can improve the drain breakdown voltage in the off state and the drain breakdown voltage in the on state in the field effect transistor.

[0005] Furthermore, Patent Document 3 discloses a semiconductor device comprising: a substrate having a semiconductor layer, an N-type drain drift region formed in a surface layer of the semiconductor layer, a trench formed in the drain drift region, a trench insulating film formed on an inner wall surface of the trench, doped poly-Si arranged in the trench via the trench insulating film, a P-type channel region formed in the surface layer of the semiconductor layer so as to contact the drain drift region, an N-type source region formed in the surface layer of the channel region, an N-type drain region formed in the surface layer of the semiconductor layer on the opposite side of the drain drift region to the source region, a gate insulating film formed on the surface of the channel region, a gate electrode formed on the surface of the gate insulating film and connected to the doped poly-Si, a source electrode connected to the source region, and a drain electrode connected to the drain region. Patent Document 3 discloses that the above configuration ensures ESD resistance in a semiconductor device having an LDMOS transistor.

[0006] The structure of the LDMOS transistor will be described in more detail with reference to Fig. 9. A semiconductor device 70 according to the comparative example shown in Fig. 9 is an example of an LDMOS transistor, and includes a P layer 74, an N-layer 76, a source region 78, a drain region 80, a gate oxide film 86, a gate electrode 88, an STI (Shallow Trench Isolation) portion 94, and a drift layer 98 formed on a substrate 72.

[0007] 9, in the semiconductor device 70, the path through which the drain current Id flows is lengthened by the STI portion 94. Also, the semiconductor device 70 has a three-layer drift layer to improve the trade-off characteristic between the drain breakdown voltage and the on-resistance (generally, to increase the drain breakdown voltage, the on-resistance must be decreased). [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2011-187853 A [Patent Document 2] International Publication No. 2014 / 061254 [Patent Document 3] JP 2008-182106 A Summary of the Invention [Problem to be solved by the invention]

[0009] However, the semiconductor device 70 according to the comparative example has the following problem. That is, in the semiconductor device 70, when a bias voltage (e.g., about 18 V) is applied to the drain terminal 84 and a bias (e.g., about 1.8) is applied to the gate terminal 90, a drain current Id flows between the source and drain. Then, a minute leakage current is generated by an electric field generated on the path of the drain current Id, and this minute leakage current increases defects and the impact ionization rate.

[0010] That is, a minute leakage current may flow through the gate oxide film 86 due to the vertical electric field applied to the gate oxide film 86, resulting in defects. The number of defects increases over time, and as the defects continue, a leakage path may be formed, allowing current to flow freely between the gate electrode 88 and the substrate 72, resulting in breakdown. To improve this, the thickness of the gate oxide film 86 may be increased, but this would involve a trade-off with the value of the current flowing through the gate electrode 88.

[0011] Furthermore, the semiconductor device 70 has a problem in that electric field concentration is likely to occur at the ends of the STI portion 94. That is, in the semiconductor device 70, electric field concentration points E1, E2 are highly likely to occur at the ends of the STI portion 94. When the electric field concentration point E1 or E2 occurs, the impact ionization rate increases in that portion, which may result in a decrease in the breakdown voltage.

[0012] In this regard, the semiconductor devices disclosed in Patent Documents 1 to 3 do not address the problem of the vertical electric field applied to the gate oxide film as described above.

[0013] The present invention has been made to solve the above-mentioned problems, and has an object to provide a semiconductor device having a high-voltage semiconductor element structure that reduces local concentration of an electric field, suppresses the occurrence of defects due to minute leakage currents, and improves the breakdown voltage. [Means for solving the problem]

[0014] a gate electrode having a lower portion at a lower portion of the other end of the trench and formed on the one main surface of the semiconductor substrate via an insulating film; a drift layer of the first conductivity type formed in the one main surface between a lower portion of the gate electrode and the drain region and cut longitudinally by the trench; an electric field relaxation portion provided in the vicinity of the other end of the trench and relaxing an electric field generated between the source region and the drain region; a first region of a second conductivity type different from the first conductivity type and including the source region and formed in the one main surface; and a second region of the first conductivity type including the drain region and formed in the one main surface and having an impurity concentration lower than that of the drift layer, Effect of the Invention

[0015] According to the present invention, it is possible to provide a semiconductor device having a high-voltage semiconductor element structure that reduces local concentration of an electric field, suppresses the occurrence of defects due to minute leakage currents, and improves the breakdown voltage. [Brief description of the drawings]

[0016] [Figure 1] 1 is a cross-sectional view showing an example of a configuration of a semiconductor device according to a first embodiment. [Diagram 2] 2 is a cross-sectional view illustrating the operation of the semiconductor device according to the first embodiment; FIG. [Diagram 3] FIG. 11 is a cross-sectional view showing an example of a configuration of a semiconductor device according to a second embodiment. [Figure 4] FIG. 11 is a cross-sectional view showing an example of a configuration of a semiconductor device according to a third embodiment. [Diagram 5] FIG. 13 is a cross-sectional view showing an example of a configuration of a semiconductor device according to a fourth embodiment. [Figure 6] FIG. 13 is a cross-sectional view illustrating details of the configuration of a semiconductor device according to a fourth embodiment. [Figure 7] 1A is an example of an electric field distribution in a semiconductor device according to a fourth embodiment, FIG. 1B is a diagram showing the electric field distribution in a semiconductor device according to a comparative example, and FIG. 1C is a comparison of current values ​​between the semiconductor device according to the fourth embodiment and the semiconductor device according to the comparative example. [Figure 8] FIG. 13A is a cross-sectional view of a semiconductor device according to a fifth embodiment, FIG. 13B is a diagram showing an example of an electric field distribution in the semiconductor device according to the fifth embodiment, and FIG. 13C is a diagram showing the electric field distribution in a semiconductor device according to a comparative example. [Figure 9] FIG. 11 is a cross-sectional view showing a configuration of a semiconductor device according to a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings.

[0018] [First embodiment] A semiconductor device 10 according to the present embodiment will be described with reference to Figures 1 and 2. As shown in Figure 1, the semiconductor device 10 includes a semiconductor substrate 12, a P diffusion layer 14 (a region in which P-type impurities are diffused) formed in one main surface 50 of the substrate 12, an N- diffusion layer 16 (a region in which N-type impurities are diffused at a relatively low concentration), a source region 18 in which N-type impurities are diffused, a drain region 20 in which N-type impurities are diffused, a drift layer 38, and an STI portion 34. A PN junction PN is formed by the interface between the P-type diffusion layer 14 and the N- diffusion layer 16.

[0019] The semiconductor device 10 also includes a gate oxide film 26 formed on the main surface 50, a gate electrode 28 formed on the gate oxide film 26, and sidewalls 32-1, 32-2 formed on both sides of the gate oxide film 26 and the gate electrode 28. That is, the semiconductor device 10 is configured as a so-called LDMOS transistor. A source terminal 22, a gate terminal 30, and a drain terminal 24 are connected to the source region 18, the gate electrode 28, and the drain region 20, respectively.

[0020] In MOS transistors, one way to improve the drain breakdown voltage is to lengthen the diffusion region under the gate. However, this results in an increase in on-resistance. The LDMOS transistor, which has an STI section under the gate, aims to improve this point. In LDMOS transistors, an STI section 34 is placed in the diffusion region under the gate to improve the trade-off between breakdown voltage characteristics and on-resistance characteristics. The STI section 34 in the diffusion region reduces the potential and electric field peaks under the gate end, so that the breakdown voltage is maintained with a short diffusion region.

[0021] Furthermore, in the semiconductor device 10, in order to optimize the trade-off between improved driving force and electric field relaxation, three stages of impurity implantation with different depths are further performed to form the drift layer 38, providing a gradient in the impurity concentration. That is, in order to improve the drain withstand voltage (breakdown voltage), the semiconductor device 10 is configured to form a deep insulating layer by the STI portion 34, and to lengthen the path through which the drain current Id flows without increasing the distance in the planar direction.

[0022] The STI section 34 is configured by filling the groove with an insulator (e.g., an oxide film) in the direction from the main surface 50 to the substrate 12, and as described above, has the function of lengthening the path through which the current flows without widening the distance in the planar direction. The drift layer 38 is a three-layer diffusion layer formed by implanting N-type impurities three times, and has the function of improving the trade-off characteristic between the drain breakdown voltage and the on-resistance (generally, the on-resistance must be reduced in order to increase the drain breakdown voltage). In this embodiment, the reason why the impurity is implanted three times when forming the drift layer 38 is to provide a concentration gradient in the drift layer 38. The form of the concentration gradient is not particularly limited, and an optimal concentration gradient may be set in consideration of the path length of the drain current, etc., but in this embodiment, the concentration of at least the impurity implantation layer closest to the substrate 12 is made low. In addition, the number of diffusion layers constituting the drift layer 38 is not limited to three, and at least one may be sufficient, and the drift layer 38 may not be provided in consideration of the strength of the electric field to be relaxed, etc.

[0023] 1, the semiconductor device 10 further includes an extended gate electrode 42, which is a T-shaped electrode connected to the gate electrode 28 and extending through the gate oxide film 26 to the inside of the STI portion 34. There is no particular limitation on the material for forming the extended gate electrode 42, but in this embodiment, polysilicon (polycrystalline silicon) is used.

[0024] The function of the extended gate electrode 42 will be described with reference to FIG.

[0025] As shown in FIG. 9, in the semiconductor device 70 according to the comparative example, there are two electric field concentration points E1 and E2 at the end (edge) of the STI portion 94. In general, if an end (hereinafter, "corner") with a certain angle exists in the electric field, the electric field is likely to concentrate there, and the smaller the angle of the corner (the sharper the acute angle), the more likely the electric field is to concentrate. In other words, in the semiconductor device 70, the electric field is more concentrated at the electric field concentration point E1 than at the electric field concentration point E2. On the other hand, when the electric field in the direction from the source region 78 to the drain region 80 is constant, the peak of the electric field at each corner differs depending on the number of corners present in the electric field. In other words, if there are a large number of corners present in the electric field, the concentration of the electric field is alleviated.

[0026] The extended gate electrode 42 is provided in order to increase the number of corners in the electric field and reduce the peak value of the electric field at each corner, taking the above phenomenon into consideration. As shown in Fig. 2, the extended gate electrode 42 has corners S1, S2, and S3, and therefore electric field concentration points are generated on the side surfaces of the STI portion 34 corresponding to the corners S1, S2, and S3. Therefore, in the semiconductor device 10, three electric field concentration points are generated in addition to the two electric field concentration points E1 and E2 in the semiconductor device 70, for a total of five electric field concentration points, as shown in Fig. 2. As a result, the number of electric field concentration points increases, and the peak potential at each electric field concentration point decreases, improving the breakdown voltage.

[0027] In other words, in the semiconductor device 10, the T-shaped extended gate electrode 42 is embedded in the STI portion 34 to disperse the locations of electric field concentration, thereby alleviating the electric field. This electric field relaxation can be considered to be an electric field relaxation using the so-called field plate effect, and is considered to prevent the trapping of minute leakage currents and an increase in the impact ionization rate. It is preferable to determine the positions of the corners S1, S2, and S3 of the extended gate electrode 42 so that the electric field concentration points occur at positions that do not overlap with the electric field concentration points E1 and E2.

[0028] [Second embodiment] A semiconductor device 10A according to the present embodiment will be described with reference to Fig. 3. The semiconductor device 10A is a configuration in which the configuration of the portion corresponding to the extended gate electrode 42 in the semiconductor device 10 according to the above embodiment is changed. Therefore, the same components as those in the semiconductor device 10 are denoted by the same reference numerals and detailed description thereof will be omitted.

[0029] 3, the semiconductor device 10A includes a second gate electrode 44 embedded in the STI portion 34. The second gate electrode 44 according to the present embodiment is formed of polysilicon, for example, and is connected to the gate terminal 30-2. That is, the semiconductor device 10A includes two gate terminals, that is, the gate terminal 30-1 connected to the gate electrode 28, and the gate terminal 30-2.

[0030] The function of the second gate electrode 44 will be described below.

[0031] First, the second gate electrode 44 has corners S4 and S5. Therefore, as in the semiconductor device 10, the electric field concentration can be dispersed by the field plate effect to reduce the impact ionization rate. That is, two electric field concentration points are generated on the peripheral surface of the STI portion 34 corresponding to the corners S4 and S5, so that a total of four electric field concentration points are generated, including the electric field concentration points E1 and E2 of the semiconductor device 70, and as a result, the peak value of the potential of each electric field concentration point is suppressed, and the breakdown voltage is improved. As described above, it is desirable to shift the positions of the corners S4 and S5 of the second gate electrode 44 from the corners of the STI portion 34 (corners where the electric field concentration points E1 and E2 occur). When the semiconductor device 10A is used in an actual circuit, the gate terminals 30-1 and 30-2 are connected outside the semiconductor device 10A. In this case, the area of ​​the gate electrode increases, so that the gate current increases, and as a result, the drain current Id also increases.

[0032] In the above embodiment, the T-shaped extended gate electrode 42 formed from polysilicon has been described as an example, and in the present embodiment, the L-shaped second gate electrode 44 formed from polysilicon has been described as an example. However, the shape of the polysilicon embedded in the STI portion 34 is not limited to this, and an appropriate shape may be selected taking into consideration the locations where electric field concentration points occur, the number of occurrences, etc.

[0033] [Third embodiment] A semiconductor device 10B according to the present embodiment will be described with reference to Fig. 4. The semiconductor device 10B is a configuration in which the configuration of the portion corresponding to the extended gate electrode 42 in the semiconductor device 10 according to the above embodiment is changed. Therefore, the same components as those in the semiconductor device 10 are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0034] As shown in FIG. 4, in the semiconductor device 10B according to this embodiment, one end T of the STI portion 34 is located below the sidewall 32-2. That is, the positions of the STI portion 34 and the drift layer 38 are shifted toward the drain region 20 (to the right side as viewed from the front in the drawing) with respect to the semiconductor device 70 (see FIG. 9). As described above, an electric field is likely to concentrate at the end T of the STI portion 34. However, this electric field concentration is alleviated by moving the end T of the STI portion 34, which forms an acute angle, away from the position of the gate oxide film 26 and covering the upper part of the end T with an insulator. This embodiment is a form that focuses on this phenomenon.

[0035] That is, in the semiconductor device 10B, the end T of the STI portion 34 is covered with the sidewall 32-2, and the position of the end T is set to a position that is off from the lower part of the gate oxide film 26. The sidewalls 32-1 and 32-2 according to the present embodiment are formed of a nitride film as an example. As a result, in the semiconductor device 10B, the occurrence of defects due to minute leakage current is suppressed. However, if the gate oxide film 26 is far away from the PN junction PN, electric field concentration occurs, and the impact ionization rate increases. Therefore, the position of the PN junction PN needs to be at least below the gate oxide film 26.

[0036] [Fourth embodiment] A semiconductor device 10C according to the present embodiment will be described with reference to Fig. 5 to Fig. 7. The semiconductor device 10C is a semiconductor device 70 (see Fig. 9) in which the shape of the gate oxide film 26 is changed. Therefore, the same components as those in the semiconductor device 10 are denoted by the same reference numerals and detailed description thereof will be omitted.

[0037] As shown in FIG. 5, in the semiconductor device 10C, the STI portion 34 is disposed below the gate electrode 28, and further includes a thick film portion 36 in which the thickness of the gate oxide film 26 is increased at and near one end T of the STI portion 34.

[0038] The semiconductor device 70 according to the comparative example (see FIG. 9) also has a thicker film thickness in the upper layer portion of the STI portion 94. However, since the thick film portion is only in the upper layer portion of the STI portion 94, when the breakdown voltage is reduced mainly due to impact ionization, the vertical electric field cannot be sufficiently relaxed, and the breakdown voltage may not be improved. The present embodiment aims to improve this point and improve the breakdown voltage while maintaining the driving force (current value). That is, the present embodiment aims to improve the trade-off between the breakdown voltage and the driving force by partially thickening the gate oxide film thickness directly above the impact ionization generation position in an LDMOS transistor (a transistor having a high breakdown voltage MOS structure) to relax the vertical electric field and further optimize the width and thickness of the thick film. This is in consideration of the fact that the generation position of impact ionization is a direct factor that determines the breakdown voltage of a semiconductor device, and by taking measures against this generation position, the breakdown voltage is efficiently improved.

[0039] As shown in FIG. 5, the semiconductor device 10C has a thick film portion 36 and the thickness of the gate oxide film 26 on the upper part of the end T of the STI portion 34 on the gate electrode 28 side is increased, so that the vertical electric field applied to the gate oxide film 26 of the thick film portion 36 is reduced. In other words, the vertical electric field for the drain current Id flowing between the source and drain (between the source region 18 and the drain region 20) is reduced. As a result, the semiconductor device 10C can suppress the occurrence of minute leakage current and improve the breakdown voltage. Furthermore, as will be described later, the horizontal length of the thick film portion 36 is short, so that the current value of the drain current Id is also suppressed from decreasing. In other words, it is possible to improve the breakdown voltage without lowering the current value of the drain current Id.

[0040] The configuration of the semiconductor device 10C will be described in more detail with reference to FIG. 6. FIG. 6 is a diagram showing the main parts of the semiconductor device 10C shown in FIG. 5. As shown in FIG. 6, the thick film portion 36 according to this embodiment has a substantially rectangular shape with a horizontal width W and a vertical height H. If the width W is increased or the height H is increased, the breakdown voltage is improved. However, the gate current is reduced, and the driving force is reduced. In other words, it is desirable to determine the width W and height H of the thick film portion 36 while taking into consideration the trade-off between the driving force and the breakdown voltage.

[0041] Next, with reference to FIG. 7, a simulation result of the effect of the thick film portion 36 of the semiconductor device 10C will be described. FIG. 7(a) shows a simulation result of the electric field distribution in the region including the STI portion 34 and the PN junction PN of the semiconductor device 10C having the thick film portion 36 according to the present embodiment, and also shows a graph of the electric field E. FIG. 7(b) shows a similar simulation result of the semiconductor device 70 according to the comparative example not having the thick film portion 36. The thickness of the gate oxide film 86 of the semiconductor device 70 (FIG. 7(b)) is about 440 nm, and in the semiconductor device 10C (FIG. 5), the thick film portion 36 having a thickness (difference) of about 3.2 nm is formed on the gate oxide film 26 having a thickness of 440 nm. That is, the height H of the thick film portion 36 is H=about 443.2 nm. Note that the size of the thick film portion 36 shown here is an example, and is not limited thereto.

[0042] 7(a) and (b), it is clear that the electric field is alleviated (the dark parts are reduced) due to the effect of the thick film portion 36. Also, when comparing the curves of the electric field E, it is clear that in the semiconductor device 70 shown in Fig. 7(b), the electric field E increases monotonically from the substrate side to the vicinity of the end T, whereas in the semiconductor device 10C shown in Fig. 7(a), the electric field E plateaus well below the end T and the peak of the electric field E also decreases.

[0043] 7(c) is a simulation result showing a comparison between the drain current Id of the semiconductor device 10C (curve C1) and the drain current Id of the semiconductor device 70 (curve C2). It can be seen that the semiconductor device 10C is able to pass a drain current Id that is comparable to that of the semiconductor device 70, even though it has the thick film portion 36. In this simulation, the drain current Id of the semiconductor device 10C is actually larger than the drain current of the semiconductor device 70, and it can be said that the driving capability of the semiconductor device 10C is at least not inferior to that of the semiconductor device 70.

[0044] As described above, according to this embodiment, the vertical electric field applied to the gate oxide film 26 is relaxed, so that the generation of minute leakage current in the gate oxide film 26 can be reduced, and as a result, the generation of the insulation film breakdown over time can be suppressed. Note that the insulation film breakdown over time refers to the above-mentioned phenomenon in which the flow of minute leakage current causes defects inside the gate oxide film 26, and these defects continue to form leakage paths, leading to breakdown. In addition, by increasing the thickness of the gate oxide film 26 immediately above the position where impact ionization, which is the direct factor that determines the breakdown voltage, occurs, it is possible to efficiently relax the vertical electric field, making it easier to improve the breakdown voltage.

[0045] [Fifth embodiment] A semiconductor device 10D according to the present embodiment will be described with reference to FIG. 8. The semiconductor device 10D is a configuration in which the drift layer 38 in the semiconductor device 10C according to the above embodiment is replaced with a drift layer 38A. Therefore, the same components as those in the semiconductor device 10C are given the same reference numerals and detailed descriptions are omitted. FIG. 8(a) shows an example of the configuration of the semiconductor device 10D, FIG. 8(b) shows the results of simulating the electric field distribution in the semiconductor device 10D according to the present embodiment, and FIG. 8(c) shows the results of simulating the electric field distribution in the semiconductor device 10C for comparison.

[0046] As shown in FIG. 8(a), in the semiconductor device 10D, a P-type implantation region 40 is formed near the end T of the STI portion 34. The P-type implantation region 40 is a region formed by ion-implanting a P-type impurity into a part of the N-type drift layer 38, and boron can be used as the P-type impurity. In the semiconductor device 10D, a form in which the P-type implantation region 40 is formed in the implantation layer closest to the surface of the three-layer drift layer 38 is exemplified, but the position where the P-type implantation region 40 is formed can be determined in consideration of the position of the electric field concentration point, and it may be formed in the implantation layer below that. In addition, the concentration of the P-type impurity implanted in the P-type implantation region 40 is made lower than the concentration of the N-type impurity implanted in the implantation layer of the drift layer 38. In other words, the P-type implantation region 40 is made to maintain the N-type.

[0047] The P-type implantation region 40 acts to further reduce the vertical electric field applied to the gate oxide film 26. That is, the P-type implantation region 40 reduces the N-type concentration in the drift layer 38 near the end T of the STI portion 34, thereby increasing the resistance and making it difficult for a current to flow. In other words, by lowering the potential directly below the gate oxide film 26, the vertical electric field applied to the gate oxide film 26 can be further reduced than in the semiconductor device 10C. Therefore, the semiconductor device 10D can more effectively suppress the occurrence of minute leakage currents, thereby further suppressing the occurrence of insulation film breakdown over time and improving the breakdown voltage.

[0048] As is clear from a comparison of the simulation results shown in Figures 8(b) and (c), the electric field distribution of the semiconductor device 10D (Figure 8(b)) is more relaxed than the electric field distribution of the semiconductor device 10C (Figure 8(c)).

[0049] Although the semiconductor devices according to the above embodiments (semiconductor devices 10, 10A to 10D) have been described individually, each semiconductor device has a common objective of relaxing the vertical electric field applied to the gate oxide film 26, and the configurations of the semiconductor devices may be combined. For example, in the semiconductor device 10D, a configuration in which the P-type implantation region 40 is formed in the semiconductor device 10C (FIG. 5) having the thick film portion 36 has been described as an example, but the present invention is not limited to this, and the P-type implantation region 40 may be formed in each of the semiconductor devices 10, 10A, and 10B.

[0050] In addition, in each of the above embodiments, drift layer 38 having three injection layers has been described as an example, but this is intended to more efficiently alleviate the electric field. Depending on the level of electric field relaxation, etc., a form having two or one drift layer, or a form without a drift layer may also be used. [Explanation of symbols]

[0051] 10 Semiconductor device 12 Substrate 14 P diffusion layer 16 N-diffusion layer 18 Source Region 20 Drain Region 22 Source terminal 24 Drain terminal 26 Gate oxide 28 Gate electrode 30, 30-1, 30-2 Gate terminal 32-1, 32-2 Sidewall 34 STI Department 36 Thick film section 38, 38A Drift layer 40 P-type injection area 42 Extended gate electrode 44 Second gate electrode 50 Main Surface 70 Semiconductor Devices 72 Substrate 74 P layer 76 N-layer 78 Source Region 80 Drain Region 82 Source terminal 84 Drain terminal 86 Gate oxide 88 Gate electrode 90 Gate terminal 94 STI Department 98 Drift Layer E1, E2 Electric field concentration points PN PN junction S1~S3 corner T end

Claims

1. A semiconductor substrate; a first conductivity type source region formed on one main surface of the semiconductor substrate; a drain region of a first conductivity type formed on the one principal surface; a gate electrode formed on the one principal surface via an insulating film; an STI having one end located under the gate electrode or offset from the gate electrode and a corner portion offset from the one end in a direction from the one principal surface to the semiconductor substrate; an electric field relaxation portion provided in the vicinity of the one end and configured to relax an electric field generated between the source region and the drain region; Including, the electric field mitigation portion has a portion having an L-shaped cross section, the electric field mitigation portion includes a corner portion embedded in the STI, and the electric field mitigation portion has a portion located outside the STI, The gate electrode further has sidewalls formed on both sides of the gate electrode, The one end is disposed under the sidewall on the drain region side. Semiconductor device.

2. The corner of the electric field mitigating portion and the corner of the STI are formed at positions shifted from each other. The semiconductor device according to claim 1 .

3. The STI has the other end at a position in contact with the drain region. The semiconductor device according to claim 1 .

4. a first conductivity type drift layer formed in an in-plane direction of the one principal surface between a lower portion of the gate electrode and the drain region; The semiconductor device according to claim 1 .

5. a first region of a second conductivity type formed in the semiconductor substrate; a second region of the first conductivity type formed in the semiconductor substrate and having an impurity concentration lower than that of the drift layer; Including, an interface between the first region and the second region is located under the gate electrode; the first region separates the source region from the second region; the second region separates the first region from the drain region; The semiconductor device according to claim 4.

6. The drift layer includes a plurality of diffusion layers of a first conductivity type formed at different distances from the one principal surface. The semiconductor device according to claim 4.

7. The electric field mitigation portion is formed of polysilicon. The semiconductor device according to claim 1 .

8. The one end of the STI is positioned away from the bottom of the gate electrode. The semiconductor device according to claim 1 .

Citation Information

Patent Citations

  • Semiconductor device

    JP2008182106A

  • Semiconductor device and production method for the same

    JP2011187853A

  • Semiconductor device and method of manufacturing the same

    JP2017028116A

  • Semiconductor power device and method of fabricating the same

    US20140353749A1

  • Methodology and structure for field plate design

    US20160149007A1