Non-volatile Memory Cell
A non-volatile memory cell using an electrically polarizable storage layer with a magnetically frustrated layer addresses data density, power, and durability issues, enabling efficient, non-destructive reading and low power consumption.
Patent Information
- Application Number
- JP2021506738
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-08-07
- Filing Date
- 2019-08-06
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2039-08-06
AI Technical Summary
Existing non-volatile memory technologies face challenges in terms of data density, power consumption, reliability, and durability, with NAND-Flash being too expensive and other technologies like STT-RAM, FRAM, and PCM having limitations in scalability, performance, and energy efficiency.
A non-volatile memory cell utilizing a storage layer made of an electrically insulating and polarizable material with a magnetically frustrated layer, where data is stored as electrical polarization direction, allowing for non-destructive reading and reduced power consumption by measuring tunnel resistance.
The solution provides improved data storage performance with lower power consumption, higher durability, and increased data density by leveraging magnetic frustration effects for accurate reading without altering the polarization state, suitable for high-temperature environments.
Smart Images

Figure 0007564089000001 
Figure 0007564089000002 
Figure 0007564089000003
Abstract
Description
[Technical field]
[0001] The present invention relates to non-volatile memory (NVM) cells and methods for reading data from non-volatile memory cells. [Background technology]
[0002] The present invention aims to bridge the gap between high performance, volatile and power inefficient computer random access memory (RAM) and low performance, low cost non-volatile data storage (such as hard disk drives (HDDs)).
[0003] In terms of improving data storage performance, the main candidate is NAND-Flash. NAND-Flash is the mainstream technology in solid-state drives (SSDs), but as a replacement for HDDs it is currently too expensive and cannot be used as RAM due to its low endurance, performance and energy efficiency. Improved HDD technologies such as heat-assisted magnetic recording (HAMR) also suffer from poor performance and reliability issues. The main competitors in the non-volatile memory technologies under development are spin-transfer torque RAM (STT-RAM, which suffers from limited scalability and requires relatively high current densities to switch states), ferroelectric RAM (FRAM, which uses destructive read and suffers from low endurance), phase-change memory (PCM, which is energy inefficient and relies on expensive and toxic materials), resistive RAM (RRAM, which uses destructive read / reset and suffers from sneak path issues in passive memory arrays), and multi-cell devices based on these principles.
[0004] New memory technologies have various shortcomings in terms of data density, power consumption, and reliability (endurance).
[0005] WO2018 / 109441 discloses a memory cell comprising a storage layer made of a ferromagnetic material having a thickness of 20-50 nm capable of recording data as a magnetization direction, a piezoelectric layer made of an anti-perovskite piezoelectric material, and a strain-inducing layer, the anti-perovskite piezoelectric material selectively having a first type effect on the storage layer and a second type effect on the storage layer depending on the strain of the piezoelectric layer, and the strain-inducing layer induces a strain in the piezoelectric layer to switch from the first type effect to the second type effect. This utilizes the change in strain of the piezoelectric layer to result in a change in interaction with the storage layer. The stored data is read by measuring the capacitance of the structure, no current flows during reading.
[0006] US 2016 / 043307 discloses a multiferroic tunnel junction (MFTJ) formed by two ferromagnetic (FM) layers (such as iron) sandwiching a ferroelectric (FE) layer (such as (Ba,Sr)TiO3). Tunneling electroresistance (TER) is used to read data stored as electric polarization of the FE layer. Tunneling electroresistance utilizes the change in the tunneling resistance of the ferroelectric layer due to asymmetric screening of polarization caused by the coupling change at the two FM / FE interfaces when switching the FE polarization of the FE layer.
[0007] Lukashev et al., Phys Rev B 84, 134420(2011) present first-principles calculations of electromagnetic effects in ferroelectric / piezomagnetic junctions. Summary of the Invention [Means for solving the problem]
[0008] The present invention provides a nonvolatile memory cell comprising a memory layer made of an electrically insulating and electrically polarizable material capable of recording data as a direction of electric polarization, a magnetically frustrated layer on one side of the memory layer, and a conductive electrode on the other side of the memory layer, the memory layer having a thickness of 10 nm or less, the magnetically frustrated layer undergoing a different change in density of states than the conductive electrode in response to a change in electric polarization in the memory layer, such that a tunnel resistance of the memory layer between the conductive electrode and the magnetically frustrated layer depends on the direction of electric polarization of the memory layer.
[0009] Due to magnetic frustration, a magnetically frustrated layer experiences a much larger change in density of states due to a change in the electric polarization of the storage layer than a non-magnetically frustrated layer (e.g., conventionally used ferromagnetic materials such as iron). This results in a significant difference in tunnel resistance with a change in polarization of the storage layer. The relatively small thickness of the storage layer allows the tunnel resistance to be measured. Thus, measuring the tunnel resistance of the storage layer increases the ease and reliability of reading data stored in the storage layer as the direction of electric polarization. The NVM according to the present invention exhibits a larger difference in resistance between the up / down polarization states compared to other ferroelectric or multiferroic tunnel junctions. This results in a better "dynamic range" for the NVM. The NVM according to the present invention exhibits a much smaller net magnetic moment for each bit compared to other MTJs (MRAM) and MFTJs based on ferromagnetic materials. This results in a closer packing of bits without mutual magnetic bridges. In addition, the large difference in tunneling resistance allows a smaller applied potential difference, and a correspondingly smaller tunneling current, to be used when reading data from the device.
[0010] The NVM according to the invention does not need to pass a current to switch the FE polarization of the storage layer in order to write data to the storage layer. This is a key advantage of the invention compared to STT-MRAM. Only an electric field is sufficient to write data to the storage layer. The negligible write current reduces power consumption and heat generation, which are desirable properties for non-volatile memory cells. This advantage over STT-MRAM is shared by an alternative storage method (FRAM). However, unlike FRAM, reading data from the NVM according to the invention is not destructive, and a smaller volume of FE material is used in the storage layer, reducing the energy required for writing. Previous versions of MRAM used an external magnetic field to write data; the use of an electric field to both write and read data in the storage layer is an additional advantage of the NVM according to the invention.
[0011] In one embodiment, the storage layer is a ferroelectric material, which exhibits stable polarization states, which enhances the stability and non-volatility of data stored in the storage layer.
[0012] In one embodiment, the thickness of the storage layer is 0.1 nm or more, more preferably 0.4 nm or more, and most preferably 1 nm or more, which makes the manufacturing easier and provides good stability of the electric polarization.
[0013] The preferred thickness of the storage layer is 5 nm or less, more preferably 3 nm or less. These limitations reduce the applied voltage required to drive a tunneling current through the storage layer, thereby reducing the energy required to read data from a non-volatile memory cell.
[0014] In one embodiment, the storage layer is A' x A´´ (1-x) B´ y B´´ (1-y)The storage layer is preferably made of a material selected from the group consisting of BaTiO3, SrTiO3, (Ba,Sr)TiO3, Ba(Zr,Ti)O3, PbTiO3 or Pb(Zr,Ti)O3. A' and A'' are one or more selected from the group consisting of Ca, Sr, Ba, Bi, Pb, La, and B' and B'' are one or more selected from the group consisting of Ti, Zr, Mo, W, Nb, Sn, Sb, In, Ga, Cr, Mn, Al, Co, Fe, Mg, Ni, Zn, Bi, Hf, Ta. Preferably, the storage layer comprises BaTiO3, SrTiO3, (Ba,Sr)TiO3, Ba(Zr,Ti)O3, PbTiO3 or Pb(Zr,Ti)O3. These materials are ferroelectric oxides that can be stably polarized electrically even at temperatures above 220K. The storage layer may be ZnO doped with Li and / or Be. ZnO is suitable as a material for the storage layer because it has alignment with the perovskite structure at the interface, can be stably polarized electrically, and can be grown at a lower temperature than the above-mentioned perovskite oxides.
[0015] In one embodiment, the storage layer has a perovskite structure or a structure that can be grown in crystalline form on a layer having a perovskite structure. Most perovskite structures exhibit the stable polarization state, electrical insulation and physical stability required for the storage layer of the present invention.
[0016] In one embodiment, the storage layer is Bi4Ti3O 12 Such materials can make the storage layer robust in high temperature environments.
[0017] In one embodiment, the conductive electrodes are paramagnetic, ferrimagnetic, ferromagnetic or antiferromagnetic materials, which material types exhibit magnetic order and respond differently to changes in the polarization state in the storage layer than a magnetically frustrated layer, as required in the present invention.
[0018] In one embodiment, the conductive electrode has an antiperovskite structure. The antiperovskite lattice is exactly the same as the perovskite lattice. The only difference is that oxygen is replaced by metal (e.g. Mn) at the face-centered positions. Many antiperovskite structures exhibit magnetic properties that are favorable for the present invention, as well as good physical stability and electrical conductivity, as required for non-volatile memories. This is particularly advantageous when combined with a storage layer of a perovskite structure, since the interface between such similar structures results in a stronger and more physically durable memory cell.
[0019] In one embodiment, the conductive electrode is selected from the group consisting of MnFeN, MnZnC, MnAlC, MnGaC, MnN, Mn 4-x Ni x N,Mn 4-x Sn x It is made of a material selected from the group consisting of N, Pt, Au and Al, which are known to exhibit favorable ferromagnetic, ferrimagnetic or paramagnetic properties as required for the conductive electrodes of the present invention.
[0020] In one embodiment, the magnetically frustrated layer has an anti-perovskite structure. Anti-perovskite materials can exhibit the magnetic frustration properties required for a magnetically frustrated layer, as well as good physical properties and electrical conductivity. In addition, the anti-perovskite structure can result in stronger, more physically durable memory cells and / or lower lattice mismatch when used in combination with a perovskite storage layer material.
[0021] In one embodiment, the magnetically frustrated layer is a piezomagnetic material, which is an example of a material that exhibits the magnetic frustration required for the magnetically frustrated layer of the present invention.
[0022] In one embodiment, the magnetically frustrated layer is Mn 3-x A x Ga 1-y By N 1-z or Mn 3-x A x Ni 1-y B y N 1-z Mn3GaN or Mn3NiN, or Mn3GaN or Mn3NiN-based, such as: where A and B are one or more elements selected from the list including Ag, Al, Au, Co, Cu, Fe, Ga, Ge, In, Ir, Ni, Pd, Pt, Rh, Sb, Si, Sn, Zn. Such materials exhibit strong magnetic frustration. Mn3GaN is preferred, as it exhibits the largest observed magnetic capacitance.
[0023] In a further embodiment, the magnetically frustrated layer is Mn 3-x A x Sn 1-y B y N 1-z The magnetically frustrated layer is Mn3SnN or Mn3SnN-based, such as: A and B are one or more elements selected from the list including Ag, Al, Au, Co, Cu, Fe, Ga, Ge, In, Ir, Ni, Pd, Pt, Rh, Sb, Si, Sn, Zn. Preferably, the magnetically frustrated layer is Mn3SnN depleted by about 10% in N. This maximizes the response of the magnetic moment to the reduction in symmetry caused by the polarization of the storage layer in the adjacent layer. It also has the highest Neel temperature of about 475K. In one embodiment, the magnetically frustrated layer is Mn3SnN 0.9 These materials advantageously exhibit a high Neel temperature, above which the desired properties are lost as the material becomes paramagnetic rather than antiferromagnetic. Materials from this group are known to exhibit strong magnetic frustration, as required for the magnetically frustrated layer of the present invention.
[0024] In one embodiment, the lattice mismatch between the storage layer and the magnetically frustrated layer and / or between the storage layer and the conductive electrode is less than ±10%, preferably less than ±1%. The chemical composition of the magnetically frustrated layer and the storage layer can be tailored to achieve such a low lattice mismatch. Reducing the lattice mismatch between the various layers has the advantage of minimizing the lattice strain that occurs at the interface regions of the various layers. Reducing the strain at the interfaces can increase the mechanical life of the non-volatile memory cell structure.
[0025] In one embodiment, there is provided a method of reading data from a non-volatile memory cell comprising a storage layer storing data as a direction of electric polarization, the storage layer sandwiched between a conductive electrode and a magnetically frustrated layer, the conductive electrode and the magnetically frustrated layer differing in change in density of states in response to a change in electric polarization of the storage layer, the method comprising measuring a tunneling resistance between the conductive electrode and the magnetically frustrated material, thereby determining the electric polarization direction of the storage layer and reading data stored in the storage layer. As the direction of electric polarization of the storage layer changes, the magnetically frustrated layer causes a large change in tunneling resistance through the storage layer. This is advantageous as it improves the accuracy of reading data from the storage layer.
[0026] In one embodiment, data is read from the storage layer by applying a potential difference between the conducting electrode and the magnetically frustrated layer and measuring the tunneling current. If the electronic states of the conducting electrode and the magnetically frustrated layer are well aligned (in momentum space), a small potential difference between these two layers can drive a tunneling current through the storage layer. If the electronic states of the conducting electrode and the magnetically frustrated layer are not well aligned (in momentum space), the tunneling resistance increases significantly, meaning that a small potential difference applied between the two layers can only drive a much smaller tunneling current through the storage layer. Thus, a large difference in the tunneling resistance means that a small potential difference can be used to accurately measure the polarization direction of the storage layer. This is advantageous because even if the electronic states of the conducting electrode and the magnetically frustrated layer are well aligned (in momentum space), the small tunneling current driven through the storage layer during readout uses very little power, which generates very little heat.
[0027] In one embodiment, the potential difference applied between the conductive electrode and the magnetically frustrated layer to read data from the storage layer is lower than the potential difference required to change the electric polarization of the storage layer. This is advantageous because it reduces the risk of inadvertently changing the polarization direction of the storage layer (i.e., rewriting the data stored in the storage layer). By utilizing the tunnel resistance, a non-destructive read can be performed. This is advantageous compared to FRAM, which needs to be rewritten after reading, causing further fatigue to the memory cell.
[0028] In one embodiment, the storage layer 10 has a magnetic order due to the proximity of the conductive electrode 20 and the magnetically frustrated layer 30. The probability of tunneling through the storage layer 10 depends on the spin polarization state of the tunneling electrons. This has the beneficial effect of increasing the change in tunneling resistance through the storage layer 10 when the electric polarization direction of the storage layer 10 is changed.
[0029] An embodiment of the present invention will now be described, by way of example only, with reference to and shown in the accompanying drawings, in which: [Brief description of the drawings]
[0030] [Figure 1] FIG. 1 is a schematic diagram of the lattice and magnetic structures of an antiperovskite piezomagnetic material (Mn3NiN). [Diagram 2] FIG. 2 is a schematic cross-sectional view of the nonvolatile magnetic memory cell in the first embodiment. [Diagram 3] FIG. 3 shows the effect of polarization of the storage layer on the density of states of the magnetically frustrated layer. The y-axis shows the difference in density of states (DOS) of the magnetically frustrated material between electric polarization states “1” (DOS “1”) and “0” (DOS “0”) of the storage layer. The x-axis shows energy (E) relative to the Fermi energy (EF). [Figure 4] FIG. 4 is a schematic diagram of a conductive electrode, a storage layer, and a magnetically frustrated layer in accordance with one embodiment of the present invention, illustrating two examples of stable polarization states in the storage layer.
[0031] The present invention exploits the properties of magnetically frustrated materials with non-collinear antiferromagnetic ground states. An example of a class of materials that exhibits magnetic frustration are piezomagnetic materials. In such materials, there exists an antiferromagnetic interaction between the magnetic moments of nearest neighboring atoms (Mn in the illustrated example). Due to the lattice structure of the material, it is not possible to arrange these atomic moments such that all interactions between the spins are antiparallel. A configuration is obtained in which the overall spin is net zero. On the other hand, the magnetic order is unstable with respect to the breaking of the symmetry of the cubic lattice. In the context of the present invention, the magnetic moments change size upon application of an applied electric field.
[0032] Figure 1 shows the structure of a manganese-based antiperovskite material (Mn3NiN). As shown in Figure 1, it is not possible to arrange the atomic spin orientations (indicated by the arrows) of the Mn atoms such that all interactions between the spins of the Mn atoms are antiparallel. Therefore, the system is described as magnetically frustrated. The material occupies a state where the net spin is zero.
[0033] The present invention utilizes the magnetic frustration property and its effect on density of states when a magnetically frustrated layer and an electric polarization layer in contact with the magnetically frustrated layer interact. Figure 2 shows a schematic cross-sectional view of a non-volatile magnetic (NVM) memory cell in a first embodiment. The NVM cell comprises a storage layer 10. Data can be stored in the storage layer 10 as the direction of electric polarization.
[0034] Typically, the direction of electric polarization in the storage layer 10 is perpendicular to the plane in which the storage layer 10 resides, but this is not necessarily the case. Electric polarization can be induced by applying an electric field across the storage layer 10. When the applied electric field is removed, the electric polarization is maintained (the storage layer 10 is stably electric polarizable). Thus, the storage layer 10 can store at least one bit of data, “1” or “0”, where “1” or “0” respectively corresponds to one of two stable polarization directions. That is, this is a two-state non-volatile memory.
[0035] The storage layer 10 may be composed of a ferroelectric material. Because ferroelectric materials exhibit a stable electric polarization, data may be stored in the storage layer 10 as a direction of polarization (e.g., either an up or down electric polarization). This data is retained even when the electric field that induced the polarization is removed.
[0036] The storage layer 10 has a thickness sufficient to exhibit quantum tunneling upon application of a low voltage (e.g., about 1 mV or less for a storage layer thickness of 1-10 nm). The thickness of the storage layer 10 is 0.1 nm or more, more preferably 0.4 nm or more, and most preferably 1 nm or more. Increasing the thickness facilitates fabrication. Increasing the thickness of the storage layer 10 is also preferred because a sufficiently large electron tunnel barrier is formed to prevent tunneling current from passing through the storage layer 10 in cases where the density of states in momentum space of the conducting electrodes and the magnetically frustrated layer are not well aligned. This is advantageous because the difference in tunneling resistance is larger at different polarizations, making it easier to accurately read data from the storage layer 10. The stability of the polarization of the storage layer 10 increases with the thickness of the storage layer 10, so the thickness of the storage layer 10 is preferably 0.1 nm or more. Also, if the storage layer 10 is too thin, the capacitance of the three layers will be too high, preventing the operation of the NVM due to charging of the device during writing.
[0037] The thickness of the storage layer 10 is 10.0 nm or less, more preferably 5.0 nm or less, and most preferably 3.0 nm or less. The thinner the storage layer 10, the lower the potential difference required to drive a tunneling current through the storage layer 10 when the momentum space density of states of the conductive electrode 20 and the magnetically frustrated layer 30 are well aligned. If the storage layer 10 is too thick, the tunneling current may be too small and difficult to detect. The lower potential difference reduces the risk of inadvertently changing the electric polarization of the storage layer 10 when reading data, and also reduces power consumption and heat generation when reading data. The maximum and minimum thickness limits provide an acceptable tradeoff between stability of the stored data (preferably with a thicker storage layer 10) and minimizing the applied voltage required to drive a tunneling current through the barrier during reading (preferably with a thinner storage layer 10). The thickness is preferably in the range of 0.4 nm to 10.0 nm, and more preferably in the range of 0.4 nm to 5.0 nm.
[0038] The memory layer 10 is preferably made of a ferroelectric oxide, and more preferably made of a ferroelectric oxide having a stable FE polarization even at temperatures above 220 K (preferably above 500 K). x A´´ (1-x) B´ y B´´ (1-y) O3, where A' and A'' are one or more selected from the group consisting of Ca, Sr, Ba, Bi, Pb, La, and B' and B'' are one or more selected from the group consisting of Ti, Zr, Mo, W, Nb, Sn, Sb, In, Ga, Cr, Mn, Al, Co, Fe, Mg, Ni, Zn, Bi, Hf, Ta. Specific examples include BaTiO3, (Ba,Sr)TiO3, and PbTiO3. Bi4Ti3O 12 Perovskite-related structures such as: Such materials may allow the storage layer 10 to be robust in high temperature environments.
[0039] ZnO can be used as the storage layer 10 even though it is not a perovskite material because it can retain a stable electric polarization when doped with Li or Be (i.e., it is ferroelectric).
[0040] The storage layer 10 may have a perovskite structure. This is particularly advantageous when the layer in contact with the storage layer 10 has a perovskite or antiperovskite structure. This is due to the viewpoint of electronic structure between adjacent layers as well as mechanical durability. Selecting layers to be all perovskite or antiperovskite is one way to help achieve a desired lattice mismatch between layers (less than ±10%, preferably less than ±1%). The desired lattice mismatch between layers (less than ±10%, preferably less than ±1%) helps mechanical stability as well as quantum mechanical interaction between layers. ZnO is a preferred material for the storage layer 10 because it achieves good crystallinity at low annealing temperatures.
[0041] On one side of the storage layer 10 is provided a magnetically frustrated layer 30 made of a material exhibiting magnetic frustration as described above. The storage layer 10 and the magnetically frustrated layer 30 are in contact with each other. The electric polarization (e.g., up or down) of the storage layer 10 results in different spin orientations in adjacent magnetically frustrated layers 30, as shown in Figures 3A and B.
[0042] FIG. 3 shows a simulation of how the density of states of the magnetically frustrated layer 30 changes with the change in polarization direction of the storage layer 10. The electric polarization of the storage layer 10 results in an electric field being applied to the adjacent magnetically frustrated layer 30. This electric field significantly changes the orientation of the magnetic spins in the regions of the magnetically frustrated layer 30 adjacent to the storage layer 10. The density of states of the magnetically frustrated layer 30 strongly depends on the orientation and size of the magnetic moment in the structure of the magnetically frustrated layer 30. That is, as shown in FIG. 3, the polarization direction of the storage layer 10 significantly changes the density of states of the adjacent magnetically frustrated layer 30. The difference in the tunnel resistance is proportional to the difference in the density of states. It can be seen that Mn3SnM is particularly suitable for NVM devices.
[0043] The present invention utilizes the phenomenon shown in FIG. 3 to read out data stored in the memory layer 10 as the electric polarization direction.
[0044] 2, the conductive electrode 20 is further provided on the opposite side of the magnetically frustrated layer 30 from the storage layer 10. The conductive electrode 20 and the storage layer 10 are in contact with each other.
[0045] The magnetic order of the magnetically frustrated layer 30 changes differently than the magnetic order of the conductive electrode 20 in response to changes in the electric polarization direction in the storage layer 10. The material of the conductive electrode 20 is not important, so long as it exhibits this appropriately and is conductive.
[0046] The material of the conductive electrode 20 may have a magnetic order, and therefore may be a paramagnetic, ferrimagnetic, ferromagnetic or antiferromagnetic material. The conductive electrode 20 may have a perovskite or antiperovskite structure, the advantages of which are similar to those described above for the magnetically frustrated layer 30 and the storage layer 10.
[0047] The conductive electrode 20 is made of MnFeN, MnZnC, MnAlC, MnGaC, MnN, Mn 4-x Ni x N,Mn 4-x Sn x The magnetically frustrated layer 30 may be made of a material selected from the group consisting of Mn, Pt, Au and Al. They all have an anti-perovskite structure with Mn at the same position as the magnetically frustrated layer 30, so that it can be assumed that the electronic states in the polarization direction of one storage layer are well aligned. Other examples of materials are Pt, Au and Al.
[0048] The conductive electrode 20 may be derived from a perovskite oxide such as lanthanum strontium manganite (LSMO).
[0049] The magnetically frustrated layer 30 may have an anti-perovskite structure. The magnetically frustrated layer 30 may be a piezomagnetic material. The magnetically frustrated layer may be Mn 3-x A x Ga 1-y B y N 1-z or Mn 3-x A x Ni 1-y B y N 1-z The magnetically frustrated layer may be MnGaN or MnNiN or MnGaN or MnNiN-based, such as: where A and B are one or more elements selected from the list including Ag, Al, Au, Co, Cu, Fe, Ga, Ge, In, Ir, Ni, Pd, Pt, Rh, Sb, Si, Sn, Zn.3-x A x Sn 1-y B y N 1-z The magnetically frustrated layer 30 may be Mn3SnN or Mn3SnN-based, such as Mn3SnN, where A and B are one or more elements selected from the list including Ag, Al, Au, Co, Cu, Fe, Ga, Ge, In, Ir, Ni, Pd, Pt, Rh, Sb, Si, Sn, Zn. 1-x (0.01≦x≦0.2) is preferable, and Mn3SnN 0.9 More preferably, the magnetically frustrated layer 30 is Mn3GaN (which exhibits high magnetic capacitance) or Mn3NiN (which has been extensively studied and is low cost). This provides the greatest response of the magnetic moment to the loss of symmetry caused by the polarization of the storage layer in the adjacent layers. It also has the highest Neel temperature of about 475 K. Alternatively, the magnetically frustrated layer 30 is preferably Mn3GaN (which exhibits high magnetic capacitance) or Mn3NiN (which has been extensively studied and is low cost).
[0050] FIG. 4 shows an example of a possible arrangement of the conductive electrode 20, the storage layer 10 and the magnetically frustrated layer 30. In this case, the conductive electrode 20 is Mn3FeN, the storage layer 10 is BaTiO3 and the magnetically frustrated layer is Mn3NiN. All three materials have perovskite or anti-perovskite type structures, which minimize the lattice mismatch between the layers. The lattice mismatch creates strain in the interface regions between the layers, which can result in mechanical fatigue and cracks during use. It is therefore beneficial to minimize the lattice mismatch between the layers. It is therefore preferred to have the lattice mismatch between the storage layer 10 and the magnetically frustrated layer 30 and / or between the storage layer 10 and the conductive electrode 20 be less than ±10%, preferably less than ±1%.
[0051] 4 shows two electric polarization directions (on the left and right) of the storage layer 10. These correspond to two data values (and an intermediate unpolarized state) that can be stored in the storage layer 10.
[0052] The operation of one embodiment of the present invention will now be described in detail with reference to the accompanying drawings.
[0053] In the non-volatile memory according to the invention, data can be stored in the storage layer 10 as a direction of potential polarization (upward or downward as shown in the figure). The data is written to the storage layer 10 by applying an electric field to the storage layer 10 across the non-volatile memory cell. The electric field can be applied, for example, by a first electrode 40 arranged on the opposite side of the storage layer 10 from the conductive electrode 20 and a second electrode 50 arranged on the opposite side of the storage layer 10 from the magnetically frustrated layer 30. The data is then written to the storage layer 10 by applying a potential difference between the first electrode 40 and the second electrode 50 that is large enough to cause a stable electric polarization of the storage layer 10 to appear in the desired direction. To rewrite the data stored in the storage layer 10, a potential difference is applied in the opposite direction that is large enough to reverse the electric polarization of the storage layer 10.
[0054] Due to the polarization of the storage layer 10, a potential difference exists across the storage layer 10. This potential difference creates an electric field that spreads a few atomic layers into the conductive electrode 20 and into the magnetically frustrated layer 30. The materials of the conductive electrode 20 and the magnetically frustrated layer 30 behave differently when exposed to the electric field created by the polarization of the storage layer 10. This electric field affects the magnetic polarization of both the conductive electrode 20 and the magnetically frustrated layer 30. On the other hand, the magnetically frustrated layer 30 can experience a very large change in magnetic polarization caused by the electric field created by the electric polarization of the storage layer 10.
[0055] In one embodiment, the conductive electrode 20 has a density of states that is relatively unaffected by the polarization of the storage layer 10. As shown in FIG. 3 and described above, the polarization of the storage layer 10 has a strong effect on the density of states of the magnetically frustrated layer 30.
[0056] To read data stored in the storage layer 10, a potential difference is applied across the storage layer 10 in a manner similar to that for writing data, the magnitude of the potential difference when reading is less than that required to change the electrical polarization state of the storage layer 10. This prevents data from being overwritten.
[0057] The applied potential difference during readout operates a tunneling current between the conductive electrode 20 and the magnetically frustrated layer 30 through the storage layer 10. The tunneling resistance is strongly dependent on the magnetic polarization of the magnetically frustrated layer 30, which in turn is strongly influenced by the electric polarization of the storage layer 10. If the electronic states of the conductive electrode 20 and the magnetically frustrated layer 30 are well aligned in momentum space, the tunneling resistance of the storage layer 10 will be low and therefore a current above a predetermined magnitude will flow through the storage layer 10. On the other hand, if the densities of states of the conductive electrode 20 and the magnetically frustrated layer 30 are not well aligned in momentum space, the tunneling resistance of the storage layer 10 will be significantly higher and the current will be lower (e.g., below a predetermined magnitude). Thus, by measuring the tunneling current flowing through the storage layer 10 and determining whether the measured current is above or below a predetermined magnitude, the electric polarization direction of the storage layer 10 can be determined.
[0058] In one embodiment, the potential difference applied between the conductive electrode 20 and the magnetically frustrated layer 30 to read data from the storage layer 10 is lower than the potential difference required to change the electric polarization of the storage layer 10. This is beneficial because it reduces the risk of inadvertently changing the polarization direction of the storage layer 10 (i.e., inadvertently rewriting the data stored in the storage layer 10). In addition, because a smaller potential difference is used, a smaller tunneling current can flow through the storage layer 10 during reading. This reduces the power used and the heat generated during reading. The use of a tunneling resistor allows for a non-destructive read. This is advantageous compared to FRAM, which must be rewritten after reading, causing further wear on the memory cell.
[0059] In one embodiment, the storage layer 10 has a magnetic order due to the proximity of the conductive electrode 20 and the magnetically frustrated layer 30. In this case, the probability of passage through the storage layer 10 depends on the spin polarization state of the tunneling electrons. This has the beneficial effect of increasing the change in tunnel resistance through the storage layer 10 when the electric polarization direction of the storage layer 10 changes. When individual NVM cells are combined into an array, the greater the change in tunnel resistance of each NVM cell, the smaller the error rate of the array. In addition, the greater the change in tunnel resistance with the change in electric polarization direction of the storage layer 10, the smaller the potential difference used to read data. As discussed above, a smaller potential difference used to read data stored in the storage layer 10 is advantageous in several ways.
[0060] The present invention uses a frustrated antiferromagnet as the sensitive electrode for the FE polarization in the tunnel junction. Ferromagnets are conventionally used in this context. The read mechanism is therefore more reliable due to the strong dependence of the tunnel resistance on the direction of polarization of the storage layer 10, i.e. the Tunnel Piezomagnetoresistance (TMPR) effect by using a magnetically frustrated material instead of a non-magnetically frustrated ferromagnet. The advantage compared to MRAM is that the total magnetic moment of the active layer is significantly reduced due to its antiferromagnetic order.
[0061] TMPR contributes in two ways: (a) the alignment (in momentum space) of available electronic states at the interface between the conductive electrode 20 and the magnetically frustrated layer 30, and (b) the transmission probability through the storage layer 10 as a function of the electron moment and spin state.
[0062] The conduction electrode 20 has a density of states in momentum space that is relatively unaffected by the polarization of the storage layer 10. The polarization of the storage layer 10 has a strong effect on the density of states of the magnetically frustrated layer 30. For a given electron angular momentum, if there is a corresponding high density of states in both the conduction electrode 20 and the magnetically frustrated layer 30, the tunneling resistance will be low. This is why the tunneling resistance is strongly dependent on the polarization of the storage layer 10. This is contribution (a).
[0063] Contribution (b) depends on the thickness and composition of the storage layer 10 as well as the alignment of the available states based on contribution (a). When the electronic states in both the conductive electrode 20 and the magnetically frustrated layer 30 are available and well aligned in momentum space, the "filtering" properties of the storage layer 10 start to play a role. If the magnetic order of the storage layer 10 is induced by the adjacent magnetic electrodes (conductive electrode 20 and magnetically frustrated layer 30), a spin filtering effect (electrons can or cannot pass through the storage layer 10 based on their spin polarization) can additionally occur. Furthermore, ferroelectric materials such as BaTiO3 and SrTiO3 can promote magnetic order in thin films adjacent to the ferromagnetic or antiferromagnetic layers. This can be further promoted if the perovskite structure is shared by the storage layer 10 and the magnetically frustrated layer 30. Finally, the resistance depends on the thickness of the storage layer 10, which is not used in readout since it does not change between the 1 / 0 states. If the density of states is well aligned, then by applying a small electric field (contribution (b)), electrons will pass through the storage layer 10, which allows the direction of polarization of the storage layer 10 to be determined and data to be read from the device. Readout is achieved by applying a small voltage (or electric field) and measuring the current through the junction (the two contributions are related when applying a small electric field to read out the cell). Contribution (a) is based on the "ground state properties" of the material (electron density of states), while contribution (b) also takes into account the "excited state properties", i.e. the response of the system to an applied voltage.
[0064] Both of the two contributions depend on the direction of the electric polarization of the storage layer 10, which can be detected as a difference in resistance (e.g., higher or lower than a certain level). The associated read current is much smaller than the current required to write information in a standard magnetic NVM (e.g., spin-transfer torque RAM), and therefore requires very low Joule heating and energy. The storage layer 10 may promote magnetic ordering due to its proximity to the magnetically ordered electrodes (conductive electrode 20 and magnetically frustrated layer 30). This promotes contribution (b), which is reduced for thicker storage layers 10. Therefore, the thickness of the storage layer 10 is preferably 0.1 nm to 10 nm. More preferably, the thickness of the storage layer 10 is 0.4 nm to 10 nm. This is because a thickness of 0.4 nm or more, which is the minimum value, can improve the stability of the polarization direction of the storage layer 10, and thus the stability of the data stored in the storage layer 10. TPMR can also operate using only contribution (a). The piezomagnetic response of Mn-based antiperovskite nitrides is driven by a reduction in cubic symmetry, but in the present invention the distortion is replaced by a local electric field provided by the storage layer 10. Only a few atomic layers adjacent to the storage layer 10 are affected by this field, but this is sufficient to modify the tunnel resistance.
[0065] The conductive electrode 20 and the magnetically frustrated layer 30 are made of different materials and have different atomic compositions at the interface, so the behavior of the conductive electrode 20 and the magnetically frustrated layer 30 are not symmetrical, otherwise the tunnel resistance would be the same in both electric polarization directions of the conductive electrode 20 and the magnetically frustrated layer 30.
[0066] Due to the resistive readout, the memory cell of the present invention can be integrated into standard 2D arrays (used in DRAM and STT-RAM) where each cell uses a single access transistor. Compared to magnetic NVM, the stray field in each cell is negligible or identical, allowing for high storage density. As the information is stored in the storage layer 10, many of the remaining characteristics (write time, retention time, and energy per write operation) are comparable to those of ferroelectric memory cells.
[0067] The present invention proposes a novel, easily implemented, non-volatile method for memory and data storage applications that outperforms existing technologies in terms of power consumption, temperature stability, durability and speed, works at high temperatures (over 180°C) and consumes very little power, thus addressing future applications such as devices in the IoT domain.
[0068] The layers of the device can be fabricated using any thin film deposition method optimized for the desired layer. For example, pulsed laser deposition (PLD) can be used. Examples of growth conditions for each thin film are shown below. The NVM described herein can be fabricated using methods, conditions and materials as shown in WO2018 / 109441, the entire contents of which are incorporated herein by reference. Examples are shown below, but are not limited to these.
[0069] Step 1: Select and clean the substrate Any suitable oxide substrate (e.g., MgO, SrTiO3, Nb:SrTiO3, (LaAlO3) 0.3 (Sr2TaAlO6) 0.7 ) or Si can be used as the substrate. Prior to growth, the substrate is cleaned by a standard solvent cleaning procedure, which can be acetone, then isopropanol, and finally distilled water for 3 minutes in an ultrasonic bath with N2 blow drying after each solvent step. In one embodiment, the substrate can be the second electrode 50.
[0070] Step 2: Growth of several layers (PLD and magnetron sputtering) The thin films are deposited by PLD using a KrF excimer laser (λ = 248 nm). x Sr 1-x TiO3, BaZr x Ti 1-x The stoichiometric single-phase targets of O3, Mn3SnN and Mn3GaN provide 0.8 J / cm2 at 10 Hz. 2 The vascular endothelial cell is removed by laser using a fluency of 100 nm.
[0071] Layer 1 (second electrode 50) Thin films of 100 nm SrRuO3 are grown at 700°C–780°C under O2 partial pressures of 50–300 mTorr. After deposition, the grown films are then post-annealed in situ at the growth temperature for 20 min under O2 partial pressure of 600 Torr. The samples are then cooled to room temperature at a rate of 10°C / min under O2 partial pressure of 600 Torr. A 100 nm Nb:SrTiO3 thin film is grown at 700 °C under an O2 partial pressure of 0–60 mTorr. After growth, the sample is cooled to room temperature at a rate of 10 °C / min under an O2 partial pressure of 600 Torr.
[0072] Layer 2 (a magnetically frustrated layer 30 of Mn3XN (where X is any suitable element)) For example, a 100 nm Mn3SnN thin film is grown at 300°C-550°C under a N2 partial pressure of 0-12 mTorr. After growth, the sample is cooled to room temperature at a rate of 10°C / min under a N2 partial pressure of 0-12 mTorr. Also, 100 nm Mn3GaN is grown at 300°C-550°C under N2 partial pressure of 0-12 mTorr. After growth, the sample is cooled to room temperature at a rate of 10°C / min under N2 partial pressure of 0-12 mTorr.
[0073] Layer 3 (electrically polarizable material of storage layer 10) 0.1-10nm BaTiO3(Ba x Sr 1-x TiO3 or BaZr x Ti 1-x Thin films of O3) are grown at 750-800 °C under an O2 partial pressure of 150-300 mTorr. After growth, the samples are cooled to room temperature at a rate of 10 °C / min under an O2 partial pressure of 600 Torr.
[0074] Layer 4 (Conductive Electrode 20) The thin films are 100 nm metal films (e.g., Pt, Au) or conductive perovskite films (e.g., SrRuO3, Nb:SrTiO3). A 100 nm Pt thin film is grown by DC magnetron sputtering. The sample is heated to 800 °C in ultra-high vacuum and annealed for 1 h. The Pt thin film is deposited with a DC power of 100 W. After growth, the sample is cooled to room temperature at a rate of 10 °C / min under vacuum. Also, 100 nm SrRuO3 thin films are grown at 700°C–780°C under O2 partial pressures of 50–300 mTorr. After deposition, the grown films are then post-annealed in situ at the growth temperature for 20 min under O2 partial pressure of 600 Torr. The samples are then cooled to room temperature at a rate of 10°C / min under O2 partial pressure of 600 Torr. A 100 nm Nb:SrTiO3 thin film is grown at 700 °C under an O2 partial pressure of 0–60 mTorr. After growth, the sample is cooled to room temperature at a rate of 10 °C / min under an O2 partial pressure of 600 Torr.
[0075] Layer 5 (first electrode 40) A 100 nm thin metal film (e.g., Pt, Au, Al). A 100 nm Pt thin film is grown by DC magnetron sputtering. The sample is heated to 800 °C in ultra-high vacuum and annealed for 1 h. The Pt thin film is deposited with a DC power of 100 W. After growth, the sample is cooled to room temperature at a rate of 10 °C / min under vacuum.
[0076] Step 3: Photolithography Standard photolithography processes have been implemented to apply the array patterns: in a 2D device, all layers can be deposited and then patterned.
[0077] Step 4: Etching A standard argon ion milling process or other suitable chemical or physical etching technique is implemented to remove material and transfer the pattern from the photolithography onto the sample.
Claims
1. A storage layer made of an electrically insulating and electrically polarizable material capable of recording data as a direction of electric polarization; a magnetically frustrated layer on one side of the storage layer; a conductive electrode on the other side of the storage layer; Equipped with The thickness of the memory layer is 0.1 nm or more and 10 nm or less, The memory layer has a unit lattice of a material constituting the memory layer, the magnetically frustrated layer experiences a different change in density of states in response to a change in electric polarization in the storage layer than the conductive electrode, such that a tunneling resistance of the storage layer between the conductive electrode and the magnetically frustrated layer depends on a direction of electric polarization of the storage layer. Non-volatile memory cells.
2. The non-volatile memory cell of claim 1 , wherein the storage layer is a ferroelectric material.
3. The non-volatile memory cell according to claim 1 , wherein the thickness of the memory layer is 0.4 nm or more.
4. The non-volatile memory cell according to claim 1 , wherein the thickness of the storage layer is 5 nm or less.
5. The memory layer is A' x A´´ (1-x) B´ y B´´ (1-y) O 3 A nonvolatile memory cell as described in any one of claims 1 to 4, wherein A' and A'' are made of a material selected from the group consisting of Ca, Sr, Ba, Bi, Pb, La, and B' and B'' are selected from the group consisting of Ti, Zr, Mo, W, Nb, Sn, Sb, In, Ga, Cr, Mn, Al, Co, Fe, Mg, Ni, Zn, Bi, Hf, Ta.
6. 5. The non-volatile memory cell according to claim 1, wherein the storage layer is made of ZnO doped with Li or Be.
7. The memory layer is Bi 4 Ti 3 O 12 5. The nonvolatile memory cell according to claim 1, which is made of a material having a perovskite-related structure such as
8. 8. The non-volatile memory cell of claim 1, wherein the conductive electrode is a paramagnetic material, a ferrimagnetic material, a ferromagnetic material or an antiferromagnetic material.
9. 9. The non-volatile memory cell of claim 1, wherein the conductive electrode has an anti-perovskite structure.
10. The conductive electrode is Mn 3 FeN,Mn 3 ZnC,Mn 3 AlC,Mn 3 GaC,Mn 4 N,Mn 4-x Ni x N,Mn 4-x Sn x 10. The non-volatile memory cell of claim 1, wherein the non-volatile memory cell is made of a material selected from the group consisting of N, Pt, Au and Al.
11. 11. The non-volatile memory cell of claim 1, wherein the magnetically frustrated layer has an anti-perovskite structure.
12. 12. The non-volatile memory cell of claim 1, wherein the magnetically frustrated layer is a piezomagnetic material.
13. The magnetically frustrated layer is made of Mn 3-x A x Ga 1-y B y N 1-z or Mn 3-x A x Ni 1-y B y N 1-z Like, Mn 3 GaN or Mn 3 NiN, or Mn 3 GaN or Mn 3 13. A non-volatile memory cell according to any one of claims 1 to 12, which is NiN-based, and A and B are one or more elements selected from the list including Ag, Al, Au, Co, Cu, Fe, Ga, Ge, In, Ir, Ni, Pd, Pt, Rh, Sb, Si, Sn, Zn.
14. The magnetically frustrated layer is made of Mn 3-x A x Sn 1-y B y N 1-z Like, Mn 3 SnN or Mn 3 13. A non-volatile memory cell according to any one of claims 1 to 12, which is SnN-based, where A and B are one or more elements selected from the list including Ag, Al, Au, Co, Cu, Fe, Ga, Ge, In, Ir, Ni, Pd, Pt, Rh, Sb, Si, Sn, Zn.
15. 15. The non-volatile memory cell of claim 1, wherein a lattice mismatch between the storage layer and the magnetically frustrated layer and / or between the storage layer and the conductive electrode is less than ±10%.
16. 1. A method of reading data from a non-volatile memory cell having a storage layer that stores data as a direction of electric polarization, comprising: the storage layer is sandwiched between a conductive electrode and a magnetically frustrated layer; the conductive electrode and the magnetically frustrated layer have different changes in density of states in response to changes in electric polarization of the storage layer; The method comprises measuring a tunneling resistance between the conductive electrode and the magnetically frustrated layer, thereby determining an electric polarization direction of the storage layer and reading data stored in the storage layer.
17. The measurement of the tunnel resistance is applying a potential difference between the conductive electrode and the magnetically frustrated layer; and measuring the current.
17. The method of claim 16.
18. The method of claim 17 , wherein the potential difference is less than the potential difference required to change the electric polarization of the storage layer.
19. 19. The method of claim 16, wherein the storage layer has a magnetic order resulting from the proximity of the conductive electrode and the magnetically frustrated layer.
20. The method according to any one of claims 16 to 19, wherein the non-volatile memory cell is a non-volatile memory cell according to any one of claims 1 to 15.
Citation Information
Patent Citations
Method for storing digital information and storage element
EP2207177A2
MRAM-based programmable magnetic device for generating random numbers
EP3062215A1
Nonvolatile memory element and method for manufacturing the same
JP2012084765A
Magnetic random access memory (MRAM) cell and method for writing and reading MRAM cell by using self reference read operation
JP2013093558A
Magnetoresistance effect element, thermal history sensor, and spin glass utilization type magnetic memory
JP2018026481A