Method for evaluating the UV protection performance of cosmetics
By employing an applicator with an oil-resistant layer and substrates of different contact angles, the method addresses uneven coatings and inconsistent measurements in cosmetic UV protection evaluations, achieving precise and uniform results across diverse cosmetic types.
Patent Information
- Application Number
- JP2024096211
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-06-13
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-06-13
AI Technical Summary
Existing methods for evaluating the UV protection performance of cosmetics are inaccurate and inefficient, particularly due to variations in measurements caused by substrate contact angles and the adhesion of cosmetic components to metal applicators, leading to uneven coatings and inconsistent results.
The use of a layer of material with oil adhesion prevention properties on the applicator surface, combined with substrates of varying contact angles, allows for the formation of a uniform cosmetic layer, enabling accurate measurement of UV transmittance ratios through spectrophotometry.
This method achieves more stable and accurate UV protection performance evaluations for various cosmetic forms, including solutions, emulsions, powders, and sticks, by minimizing substrate adhesion and ensuring consistent film thickness.
Smart Images

Figure 0007569526000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for evaluating the ultraviolet protection performance of a cosmetic preparation. [Background technology]
[0002] The technical background of the present invention will now be described. Currently, in Japan, SPF (short for Sun Protection Factor), which indicates the ability to protect against UVB rays with wavelengths of 290 to 320 nm, and UVA-PA (Protection grade of UVA), which indicates the ability to protect against UVA rays with wavelengths of 320 to 400 nm, are used as indicators of the UV protection effect of cosmetics. When these measurement results are to be displayed on cosmetics, it is required that the values or grades measured based on the respective measurement method standards (Non-Patent Documents 1 and 2) established by the Japan Cosmetic Industry Association be displayed. Although it is required to display the effect according to the measurement and display methods of each region (Non-Patent Document 3) overseas, the basic measurement method is almost unified. In the measurement method standard, a human back is used, high-power ultraviolet light is irradiated onto the back, and the ultraviolet protection effect is measured based on the results of visual observation of the inflammatory and blackening reactions that occur on the skin. However, using humans is time-consuming and expensive, and it takes a long time to obtain the measurement results. In addition, because of the ethical and medical issues of using humans, in Japan and Europe, studies are being conducted on a measurement method that uses machines to measure the UV protection effect without using humans (Non-Patent Document 4). However, it has been reported that there are many problems with the measurement methods currently being used (Non-Patent Document 5). The inventor's study also found that even when the same sample is used and the same standard is used, the SPF value can vary by up to 20 times.
[0003] This problem can be largely solved by using the method described in Patent Document 1. However, when further investigations were carried out using this method, a new problem arose: when using substrates with different contact angles with water, the measured values of the sample changed significantly (Non-Patent Document 6). Therefore, there was a need to develop a measurement method that would allow highly accurate measurements with as little effort as possible, and the inventions of Patent Documents 2 to 7, mainly Patent Documents 2 and 3, which were invented by the present inventors, made it possible to perform highly accurate measurements. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2018 / 047707 [Patent Document 2] Patent No. 6741261 [Patent Document 3] Patent No. 6842778 [Patent Document 4] Patent No. 5825654 [Patent Document 5] Patent Publication No. 2021-65873 [Patent Document 6] JP 2023-57509 A [Patent Document 7] JP 2023-95723 A [Non-patent literature]
[0005] [Non-Patent Document 1] Japan Cosmetic Industry Association, Cosmetics for UV Protection and UV Protection Effect -SPF and PA Labeling- 2003 Revised Edition [Non-Patent Document 2] Japan Cosmetic Industry Association Japan Cosmetic Industry Association SPF Measurement Method Standard〈2007 revised edition〉 [Non-Patent Document 3] ISO / TR26369 Cosmetics -- Sun protection test methods -- Review and evaluation of methods to assess the photoprotection of sun protectionproducts [Non-Patent Document 4] Colipa Guidelines, Method for in vitro Determination of UVAprotection, 2009 [Non-Patent Document 5] Ruppert, S.; Bimzcok, R.; Klebon, B.; Heinrich, U.; Tronnier, H.; Johncock, W.; Peters, S.; Pfluecker, F.; Rudolph, T.; Floesser-Mueller, H.; Jenni, K.; Kockott, D.; Lademann, J.; Herzog, B.; Bielfeldt, S.; Mendrok-Edinger, C.; Hanay, C.; Zastrow, L. “in vitro SunProtection Factor: Still a Challenge with No Final Answer” Skin Pharmacol.Phys. 2010, 23(4), 201-212. [Non-Patent Document 6] K. Asakura, A. Kuroda, IFSCC Magazine 21(2), 53-57 (2018). Summary of the Invention [Problem to be solved by the invention]
[0006] Cosmetics have different physical properties depending on their composition, such as hydrophilicity, lipophilicity, and intermediate properties between them. When a cosmetic is applied to only one type of substrate with a fixed contact angle with water, some cosmetics can be applied evenly, but other cosmetics cannot be applied evenly, and the cosmetic may undergo phase separation or be repelled from part of the substrate surface, resulting in an uneven coating film with part of the substrate surface exposed. For this reason, even if the measurement accuracy is improved, the measurement still requires preparing substrates with many contact angles in advance and plotting the respective measurement values on a graph in order to grasp the characteristics, and even measuring one product can require a lot of effort, as it is necessary to measure substrates with multiple types of contact angles. This effort is much more than that required for in vivo methods, meaning that it cannot essentially be used as an alternative method. In addition, when more than 200 commercially available cosmetics from around the world were measured using the conventional method, some of the products were found to behave differently from what we expected, so we investigated the cause of this. As a result, because the applicator is made of metal, in cosmetics that have a strong affinity for lipophilic metals, phase separation of the cosmetics occurs in the gap and front part of the applicator. Then, most of the cosmetics adhere to the applicator side, and almost none of the cosmetics remains on the applied surface of the substrate. Furthermore, even in formulations that do not exhibit this phenomenon, we used an infrared imaging microscope to examine the change in the amount of UV absorber in the coating film whose thickness was confirmed to be constant using a rotating film thickness meter. When a stainless steel four-sided applicator was used, it was found that there were areas where the concentration of the UV absorber periodically became high, that is, unevenness in the concentration of the UV absorber occurred depending on the location of the coating film. This meant that accurate measurement was not possible by measuring only the film thickness. In addition, when a corona discharge treatment is performed to prepare a superhydrophilic substrate, the corona discharge treatment device generates strong electromagnetic noise, and may not be usable in office buildings. Furthermore, when a cosmetic is applied to the substrate surface, a coating film having a large uneven striped pattern may result. In this case, if a rotary wet film thickness meter is used to measure the coating film thickness, the measured value will differ greatly from the actual film thickness. In addition, the values obtained by the calculation formula defined in the ISO method shown in Non-Patent Document 4 differ from the data obtained for humans and subjects. An object of the present invention is to provide a method for evaluating the ultraviolet ray transmittance ratio of a cosmetic material which solves the above problems. [Means for solving the problem]
[0007] By adopting the configuration described below, instead of an applicator with a metal (stainless steel) surface, an applicator having an oil-resistant material layer (obtained by wrapping a resin film, etc.) formed on the surface of a cylindrical applicator is used, thereby preventing excessive adhesion of oily components of cosmetics, in particular, to the applicator. Also, instead of using the corona discharge-treated quartz plate itself, multiple types of substrates for evaluating the ultraviolet transmittance ratio with different contact angles, such as transparent substrates for measuring ultraviolet transmittance, which are made superhydrophilic by covering the surface of a quartz plate or the like that has been corona discharged in advance with various materials such as inulin, were adopted. A single type of cosmetic was used on each of the surfaces of these substrates, and a uniform cosmetic layer was formed by an applicator whose surface was made of a material that prevents adhesion of oil. As a result, experimentally, regardless of the nature of the cosmetic (hydrophilic, lipophilic, and intermediate properties thereof, and properties such as liquid, solid, cream, and stick), a thin layer of the cosmetic could be uniformly formed on at least one of the multiple types of substrates for evaluating the ultraviolet transmittance ratio. By adopting such a means, the need to use a corona discharge device for surface treatment of the substrate at the test site was eliminated. As a result, instead of using a rotary wet film thickness meter, it is possible to perform more accurate measurements by comparing the absorbance value of the applied cosmetic layer at a specific wavelength measured by a spectrophotometer with the absorbance value of a 100 μm thick assembly cell at the same specific wavelength, and calculating the thickness of the cosmetic layer. This has resulted in the development of a simpler and more accurate method for evaluating the UV transmittance ratio of cosmetics. Furthermore, the formula for calculating the SPF value and UVA-PF value from the absorbance is not the formula specified by the ISO method, and measurement results that are more closely correlated with human test data have been obtained. In the following, the substrate for evaluating the UV transmittance ratio may sometimes be simply referred to as the "substrate."
[0008] 1. A method for evaluating the UV protection performance of cosmetics, comprising a step of preparing a measurement sample for evaluating the UV protection performance of cosmetics, the preparation step comprising a method of forming a uniform cosmetic application layer on the surface of a transparent substrate for measuring UV transmittance using an applicator formed of a material layer having oil-resistant properties. 2. A method for evaluating the UV protection performance of cosmetics according to claim 1, wherein the material layer having an oil-resistant surface is a layer made of one or more materials selected from the group consisting of polyethylene naphthalate (PEN) film, hydrophilically treated polyester film, hydrophilically treated polyethylene terephthalate film, and fluororesin film, all of which have oil-resistant properties. 3. A method for evaluating the UV protection performance of a cosmetic composition according to 1 or 2, comprising the following steps A to D: A. A process for preparing multiple measurement samples for evaluating the UV protection performance of cosmetics, in which a single type of cosmetic is used to form a uniform cosmetic coating layer on each of multiple types of UV transmission ratio evaluation substrates with different contact angles, using an applicator whose surface is formed of a material layer having adhesion prevention properties. B. A process of measuring the absorbance of a cosmetic material at a standard thickness using an assembled cell, and calculating the SPF and UVA-PF values using the following formula: SPF value calculated by integrating the wavelengths from 290 to 320 nm in 1 nm increments using the formula CF x ΣEE(λ) x I(λ) x Abs(λ) UVA-PF value obtained by integrating from 320 to 400 nm in 1 nm increments using the formula CF × ΣEE(λ) × I(λ) × Abs(λ) Here, CF is the correction factor (=10), EE is the erythemal effect spectrum, I is the solar intensity spectrum, and Abs is the absorbance of sunscreen product. C. A process of selecting the measurement sample with the highest SPF value based on the SPF values obtained for multiple measurement samples, and determining the SPF value and UVA-PF value of the measurement sample as the in vitro SPF value and in vitro UVA-PF value of the one type of cosmetic. D. A process of determining the in vivo SPF equivalent value of the one cosmetic product from the relational equation between the in vivo SPF value and the in vitro SPF value, and further determining the in vivo UVA-PF equivalent value of the one cosmetic product from the relational equation between the in vivo UVA-PF value and the in vitro UVA-PF value. 4. The method for evaluating the UV protection performance of cosmetics according to 3, wherein the multiple types of transparent substrates for measuring UV transmittance having different contact angles are three types: a transparent substrate for measuring UV transmittance having a layer coated with polyisocyanate on its surface, a transparent substrate for measuring UV transmittance having a layer coated with inulin, and a transparent substrate for measuring UV transmittance having a layer coated with hydroxyalkyl cellulose. 5. A method for evaluating UV protection performance according to 3 or 4, characterized in that the relational equation between the in vivo SPF value and the in vitro SPF value, and the relational equation between the in vivo UVA-PF value and the in vitro UVA-PF value are determined by statistically processing the relationship between the SPF value, UVA-PF value or the in vivo UVA-PF value corresponding to the PA classification of the cosmetic obtained by the in vivo method and the SPF value and UVA-PF value determined by steps A to D. 6. The method for evaluating ultraviolet protection performance according to any one of 1 to 5, wherein the cosmetic is a powder cosmetic or a stick-type cosmetic, or a paste-like product obtained by mixing a solid cosmetic with a non-volatile oil. Effect of the Invention
[0009] By adopting the method for evaluating the ultraviolet transmittance ratio of a cosmetic material of the present invention, there is no form of cosmetic material that cannot be evaluated among various forms of cosmetic materials such as solution-type cosmetics, emulsion-type cosmetics, powder-type cosmetics, paste-type cosmetics, stick-type cosmetics, etc., and it has the effect of obtaining more highly accurate, precise, and stable measured values for all forms of cosmetic materials. In particular, highly accurate measurements have not been carried out for powder-type cosmetics and stick-type cosmetics in the past, and this method has made it possible for the first time to carry out measurements for all of the various forms of cosmetic materials mentioned above. [Brief description of the drawings]
[0010] [Figure 1] Evaluation method flow chart [Diagram 2] An example of change in absorbance versus heating time [Diagram 3] External view of the assembly cell installed on the spectrophotometer installation jig [Figure 4] Perspective view of a metal applicator [Diagram 5] Metal applicator viewed from below [Figure 6] Cross-section of a metal applicator [Figure 7] Cross-sectional view of the applicator used in coating process 2 [Figure 8] A perspective view of a cylindrical applicator [Figure 9] Cross-section of a cylindrical applicator [Figure 10] Observation of a coating applied using a stainless steel cylindrical applicator using an infrared imaging microscope [Figure 11] Observation example using an infrared imaging microscope of a coating film applied using a cylindrical applicator with a hydrophilic polyethylene terephthalate film fixed to the surface that comes into contact with the cosmetic during application. [Figure 12] Observation example using an infrared imaging microscope of a coating film applied using a cylindrical applicator with a non-hydrophilized polyethylene terephthalate film fixed to the surface that comes into contact with the cosmetic material during application. [Figure 13] Observation example using an infrared imaging microscope of a coating film applied using a cylindrical applicator with a polyimide tape fixed to the surface that comes into contact with the cosmetic during application. [Figure 14] Observation example using an infrared imaging microscope of a coating film applied using a cylindrical applicator with polyvinyl chloride tape fixed to the surface that comes into contact with the cosmetic during application. [Figure 15] Observation example using an infrared imaging microscope of a coating film applied using a cylindrical applicator with silicone rubber fixed to the surface that comes into contact with the cosmetic during application. [Figure 16] Observation example using an infrared imaging microscope of a coating film applied using a cylindrical applicator with a polyethylene naphthalate film fixed to the surface that comes into contact with the cosmetic during application. [Figure 17-1] Table in APPENDIX I of Non-Patent Document 4 [Figure 17-2] Table in APPENDIX I of Non-Patent Document 4 [Figure 17-3] Table in APPENDIX I of Non-Patent Document 4 DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The present invention will be described in detail below. The method for evaluating the ultraviolet ray transmittance ratio of the present invention, which includes a step of preparing a measurement sample for evaluating the ultraviolet ray protection performance of a cosmetic product, is a measurement method for obtaining a highly accurate and stable ultraviolet ray protection index for various types of cosmetic products, including emulsions, including hydrophilic and lipophilic types, lotions, emulsified foundations, powder cosmetics, oil-based cosmetics, and sprays. As shown in Fig. 1, in the present invention, a plurality of types of substrates are prepared as transparent substrate surfaces for measuring ultraviolet transmittance, such as three types of substrates: an inulin-treated substrate (hydrophilic substrate), a hydroxyalkyl cellulose-treated substrate (neutral substrate), and a polyisocyanate-treated (hydrophobic) substrate (oleophilic substrate). A cosmetic material to be evaluated is applied to these substrates, for example, by carrying out coating steps 1, 2, and 3 in order. The spectrum of ultraviolet light transmitted through these substrates is measured. This is corrected to a spectrum when the cosmetic material is, for example, 20 µm thick. At this time, the absorbance is determined based on the absorbance when the cosmetic material is 100 µm thick, which is determined using a separate assembly cell. Next, from the above three types of substrates, the substrate with the highest SPF value is selected. Based on the SPF and UVA values for the substrate with the highest SPF value, the equivalent in vivo-SPF and in vivo-UVA-PF values are obtained using a specified formula.
[0012] <Cosmetics> The cosmetics in the present invention are a wide variety of cosmetics including makeup products and basic cosmetics. Specifically, they include makeup cosmetics such as hydrophilic (O / W) emulsion sunscreens, lipophilic (W / O) emulsion sunscreens, multi-layer (O / W / O, W / O / W) emulsion sunscreens, and emulsion foundations, makeup bases, sunscreen creams, multi-layer separation sunscreens, non-chemical sunscreens, day essences, day care lotions, hand creams, solid foundations, face powders, blushers, eyeshadows, and other powder cosmetics, lipsticks, oil-based cosmetics such as stick-type sunscreens, spray-type sunscreens, and roll-on sunscreens. In addition, the formulations include liquid, emulsion, cream, lotion, essence, multi-layer separation, oil-based, powder, and sheet. However, they do not include cosmetics whose ultraviolet transmittance ratio is clearly 0% or clearly 100%. The cosmetic material is then applied to the skin, preferably at least one of the face, body, hands and feet, to obtain an ultraviolet ray protection effect. This UV protection effect is generally expressed as an SPF value corresponding to UV-B rays with a wavelength of 290 to 320 nm, a UVA-PF value corresponding to UV-A rays with a wavelength of 320 to 400 nm, or an in vivo UVA-PF value or PPD value corresponding to the PA classification, but is not particularly limited as long as it is an index showing the protection effect of these wavelengths.
[0013] The ultraviolet absorbent added to develop ultraviolet absorbing properties is not particularly limited as long as it is added to a cosmetic. Among such ultraviolet absorbents, oil-soluble ones include cinnamic acid-based ultraviolet absorbents, triazine-based ultraviolet absorbents, benzophenone-based ultraviolet absorbents, benzoic acid-based ultraviolet absorbents, salicylic acid-based ultraviolet absorbents, and dibenzoylmethane-based ultraviolet absorbents. These may be used alone or in combination of two or more. Water-soluble ones include benzophenone-based ultraviolet absorbents, phenylbenzimidazole sulfonic acid and / or 2-hydroxy-4-methoxybenzophenone sulfonic acid. Those that are solid at room temperature include methylene bisbenzotriazolyl tetramethylbutylphenol and trisbiphenyl triazine.
[0014] Examples of pigments that may be contained in the cosmetic composition and that scatter or absorb ultraviolet light include fine particle titanium oxide, fine particle zinc oxide, fine particle cerium oxide, titanium oxide, zinc oxide, titania hydroxide sol, aluminum powder, and gold leaf powder. Furthermore, the cosmetic contains various ingredients that can be blended in cosmetics as ingredients other than these ultraviolet absorbents and / or pigments.
[0015] <Surface of transparent substrate for ultraviolet transmittance measurement> As the surface of the transparent substrate for measuring ultraviolet transmittance used in the present invention, multiple types of substrates for evaluating ultraviolet transmittance ratio with different contact angles are used. In particular, at least two types of substrates are used from three types of substrates (lipophilic substrate, mesophobic substrate, hydrophilic substrate). For example, multiple measurement samples are obtained using such three types of substrates. The three types of substrates have different contact angles with pure water. The contact angle of the substrate for evaluating ultraviolet transmittance ratio in the present invention is the contact angle of the substrate surface with pure water at 25°C. Hereinafter, the surface of the transparent substrate for measuring ultraviolet transmittance may be referred to as "substrate for evaluating ultraviolet transmittance ratio". The substrates for evaluating the ultraviolet transmittance ratio are made by processing ultra-smooth quartz plates or the like, and are provided with a lipophilic layer, a hydrophilic layer, and a contact angle adjusting layer having intermediate properties and exhibiting a contact angle intermediate between these properties, on the surface of each of a plurality of plates that are manufactured by processing ultra-smooth quartz plates or the like, as necessary. Among them, the above three types of substrates are preferable, and transmit ultraviolet rays in the range of 290 to 400 nm. They are also required to have excellent stability over time.
[0016] The hydrophilization pretreatment is a treatment of the plate by physical means such as plasma treatment, arc discharge treatment, corona discharge treatment, etc., to make the plate into a hydrophilic substrate with a contact angle to pure water in the range of 0 to 20°, preferably 0 to 10°, more preferably 0 to 5°. The detailed conditions of these treatments, i.e., the applied voltage, treatment time, etc., can be arbitrarily determined according to the desired contact angle. Furthermore, the atmosphere can be corona discharge treatment in air, or plasma discharge treatment in a vacuum, or in an oxygen or argon atmosphere. Among them, corona discharge treatment of a quartz substrate is preferable. The lipophilic pretreatment can be achieved by coating the plate surface with a compound for exerting lipophilicity, or by subjecting the plate surface to plasma treatment, arc discharge treatment, corona discharge treatment, or the like in an atmosphere of a reactive compound having lipophilicity. In addition, if the plate is made of a material that is easily deformed by external forces, such as polymethyl methacrylate, it is likely to be deformed when applying the cosmetic or when cleaning, and it may be impossible to stably prepare or use a substrate for evaluating the ultraviolet transmittance ratio, which is not preferable. Therefore, a plate that has high mechanical strength and transmits ultraviolet rays in the range of 290 to 400 nm uniformly over the entire wavelength range, such as a quartz plate, is preferable.
[0017] To obtain the above three types of substrates based on the plate, three different types of contact angle adjusting layers are formed on each of the three plates to obtain transparent substrates for measuring ultraviolet transmittance. In the present invention, in order to accurately evaluate the ultraviolet ray transmittance, each of the three types of contact angle adjusting layers formed on the plate surface must be smooth. The degree of smoothness is preferably such that the maximum height of the unevenness is 1 μm or less as determined by the following test method.
[0018] (Method of inspecting unevenness) A thin layer of test liquid (isononyl isononanoate 27% by weight, ethylhexyl methoxycinnamate 6% by weight, titanium oxide dispersion 15% by weight, petrolatum 50% by weight, sorbitan isostearate 2% by weight) was applied onto a plate (quartz plate). Next, a stainless steel applicator with a gap of 1 μm and a width of 10 cm was placed on the layer of test liquid and moved slightly parallel to the plate surface to allow the applicator surface to blend into the layer of test liquid. Furthermore, after precisely smoothing the coating film at a speed of 5 mm / s using the applicator, if the coating film is not shading when viewed through light, the plate surface is free of irregularities, and the plate is deemed to have passed the inspection as having no irregularities when the following lipophilic, intermediate, and hydrophilic substrates are used.
[0019] (Lipophilic substrate) The lipophilic substrate is obtained by smoothing the surface of the plate, carrying out lipophilic pretreatment as necessary, and then forming a lipophilic treatment layer so that the contact angle with pure water at 25°C is in the range of 75 to 85°. As the lipophilic treatment layer, since general urethane resins and urethane acrylates show even higher contact angles, it is necessary to mix other components that reduce the contact angle. In addition, acrylic resins of a grade that can be used for coating are often unsuitable because they have ultraviolet absorption in the wavelength range of 290 to 400 nm. Similarly, ultraviolet curing resins are often unsuitable because the resin after curing has some absorption in the wavelength range of 290 to 400 nm. Therefore, it is preferable to adopt acrylic polyisocyanate, polyurethane, polyurethane acrylate, and copolymer of thiol compound / isocyanate compound / acrylate compound, which may be moisture curable, as a resin that can be applied smoothly and whose contact angle with pure water can be adjusted by adjusting the components and adding other components. These resins have polyol, acrylate, or hydroxyl group-containing acrylate that has hydrophilicity in part of their molecular structure. By adjusting the blending ratio of the polyol, acrylate, and hydroxyl group-containing acrylate components, the contact angle with pure water can be adjusted to 75 to 85 degrees.
[0020] (Intermediate substrate) The intermediate substrate is obtained by smoothing the surface of the plate, carrying out hydrophilic pretreatment or lipophilic pretreatment as necessary, and then forming a layer having intermediate properties between hydrophilicity and lipophilicity. The intermediate substrate surface is preferably one having a contact angle of 50° to 60° with pure water at 25°C. In the case of an intermediate substrate in which the contact angle changes immediately after the formation of the layer having intermediate properties between hydrophilicity and lipophilicity, it is necessary to apply a cosmetic immediately after the formation of the layer having intermediate properties between hydrophilicity and lipophilicity.
[0021] The layer having intermediate properties between hydrophilicity and lipophilicity required to obtain such an intermediate substrate is preferably hydroxyalkyl cellulose (contact angle immediately after coating is 51° to 52°). Alternatively, one or more of the following compounds may be selected and coated on the plate surface to form the layer. Compounds having a sugar skeleton, such as mannose, galactose, xylose, glucose, maltose, lactose, sucrose, trehalose, fructose, cellulose, cellulose derivatives such as hydroxyethyl cellulose, hydroxypropyl cellulose, and carboxymethyl cellulose, trisaccharides such as maltotriose and raffinose, tetrasaccharides such as inulin, oligosaccharides, glucan, agar, α-cyclodextrin, maltodextrin, corn starch, kudzu starch, tapioca starch, potato starch, wheat starch, hydroxyethyl starch, hydroxypropyl starch, tamarind gum, xanthan gum, native gellan gum, and gellan gum, which are solubilized as necessary. In addition, sugar alcohols such as erythritol and xylitol, compounds derived from sugar, and other non-sugar compounds may or may not be blended within the range that does not impair the effects of the present invention. Furthermore, in terms of forming a layer, it is preferable that the material is solid at room temperature and pressure, has no deliquescent property, and is not insoluble in water at room temperature. Not insoluble means that the material has a solubility of 1 g / 100 mL or more in water at room temperature. More preferably, the material has a solubility of 5 g / 100 mL or more.
[0022] (Hydrophilic substrate) The hydrophilic substrate is obtained by forming a layer on the plate using a compound selected from the various compounds and combinations of various compounds used to obtain the intermediate substrate. Among them, a hydrophilic layer can be formed by using tetrasaccharides such as inulin and hydroxyalkyl cellulose. When inulin is used, the contact angle with pure water at 25°C immediately after application is 23° to 26°, and the contact angle 5 minutes after application is 0° to 2.5°. It also has excellent stability over time.
[0023] The method for evaluating the UV protection performance of cosmetics of the present invention involves preparing a measurement sample by thinly coating the cosmetic on three types of substrates (lipophilic substrate, mesophotic substrate, and hydrophilic substrate) that are used for evaluating the UV transmittance ratio. The measurement is based on measuring the sample using a spectrophotometer. An overview of the measurement method is shown in Figure 1, and will be explained using the case of an emulsion sunscreen. [A. A process for preparing a plurality of measurement samples for evaluating the ultraviolet protection performance of a cosmetic, the process being carried out by forming a uniform cosmetic coating layer on each of the surfaces of a plurality of types of ultraviolet transmission ratio evaluation substrates having different contact angles, using one type of cosmetic, with an applicator formed of a material layer having an adhesion prevention surface] <Coating of cosmetics onto a substrate for evaluating the UV transmittance ratio> The following optional coating step 1 and / or coating step 2 are carried out, and then the following coating step 3 is carried out as a preparation step. As a result, a measurement sample is prepared.
[0024] (Coating process 1) A cosmetic is applied to the surface of the substrate for evaluating ultraviolet transmittance ratio using a metal applicator having a gap of 500 μm to 1000 μm. In this case, the substrate for evaluating ultraviolet transmittance ratio is placed on a support substrate made of extra super duralumin or the like having a thickness of 4 to 10 mm, and the cosmetic is applied at a relative moving speed with the metal applicator of 1 to 10 mm / sec, for example, 5 mm / sec. Alternatively, the cosmetic may be spread on the substrate for evaluating ultraviolet transmittance ratio in advance using a spatula for art supplies, and the top of the spread may be smoothed with a metal applicator as necessary.
[0025] As the metallic applicator, for example, those shown in Figs. 4 to 6 can be used. The metallic applicator is moved by a spreading device 1 shown in FIG. The coating spreading device 1 is a device having a coating spreading member 2 and support parts 3 for supporting both ends of the coating spreading member 2 . The spreading member 2 is supported by a structure (not shown) relative to the support part 3, for example, pins on both ends of the spreading member are fitted into grooves extending in the vertical direction in the support part 3, so that the spreading member is capable of moving freely up and down, and the weight of the spreading member allows it to resist the resistance from the cosmetic material to be spread, and to apply the cosmetic material evenly to the substrate. For the purpose of explanation, other parts are not shown in the paint spreading device 1 shown in Figure 4, but it is also possible to provide a component angle, for example, to connect the two support parts 3 to form an integrated paint spreading device. In addition, Figure 5 is a view of the coating spreading device 1 from below (a view of the coating spreading member 2 above from the base B side in Figure 6), and the coating spreading member tip 6 is located at the tip of the coating spreading member 2.
[0026] The material of the spreading member 2 and the support part 3 provided in the spreading device 1 is preferably a metal, and in particular, a material having good dimensional accuracy and being processable, such as stainless steel or duralumin, is preferable. The cross-sectional shape of the spreading member used in the present invention is preferably a polygon. FIG. 6 is a cross-sectional view of the state during coating by the metal applicator. In FIG. 6, a base B for fixing the substrate 4 is provided. Furthermore, as shown in FIG. 5, the angle between the surface of the spreading member facing the moving direction of the spreading device indicated by the arrow and the surface of the substrate 4 to be coated must be 30° or more. If it is less than 30°, the film thickness will not be constant due to the resistance force applied to the spreading member by the cosmetic 5, and the measurement accuracy may be low depending on the cosmetic. Similarly, when the spreading member has a shape such that the angle between the part of the spreading member closest to the substrate and the surface of the substrate to be coated is close to 0°, such as a cylindrical or elliptical cylindrical shape, the film thickness will not be constant due to the resistance force applied to the spreading member. Moreover, the height of the gap formed between the tip 6 of the spreading member and the substrate 4 in the coating process 1 is preferably in the range of 500 μm to 1000 μm.
[0027] The mass of the coating spreading member is preferably 100g or more when used alone, and more preferably 250g or more. If the mass is small, it is easily affected by resistance, which makes it difficult to form a smooth film. If the mass is too large, the substrate and the plate supporting it will be distorted, and the substrate will no longer be flat, which will cause the film thickness to vary depending on the coating area. It is difficult to say how much mass can be applied because it depends on the strength of the substrate and the plate supporting it, but when 5mm thick super duralumin is used, it has been observed that when a load is applied from above the coating spreading member and the load, including its own weight, exceeds 2kg, the substrate will be distorted to a size that cannot be ignored.
[0028] (Coating process 2) As shown in FIG. 7, the applicator used in the coating step 2 is provided with a cylindrical support P having a diameter of 30 to 40 mm at the tip of a rotating shaft. The cylindrical support has an axis passing through the center of the circular end faces at both ends, which is connected to the rotating shaft. A resin sponge-like coating tool S having a rectangular parallelepiped shape with a width of 8 to 12 mm, a length of 30 to 35 mm, and a height of 8 to 12 mm is fixed to this support. At this time, the surface of the resin sponge-like coating tool S is flat, and the flat surface is used so that it is parallel to the surface of the ultraviolet transmittance ratio evaluation substrate 4. Then, while rotating (for example, 200 to 250 rpm in the R direction), the resin sponge-like coating tool is made to come into contact with the layer of the cosmetic applied to the surface of the ultraviolet transmittance ratio evaluation substrate 4 in the coating step 1 (not shown in FIG. 7, but present between the resin sponge-like coating tool S and the surface of the ultraviolet transmittance ratio evaluation substrate 4) and leveled for a predetermined time, thereby making the cosmetic layer formed in the coating step 1 into a thinner coating layer. In this case, it is preferable that the surface area of the resin sponge-like coating tool is larger than that of the substrate for evaluating the ultraviolet transmittance ratio, or the length of the resin sponge-like coating tool S is longer than the width or diameter of the substrate for evaluating the ultraviolet transmittance ratio, and the ends of the sponge-like coating tool do not come into contact with the coating layer of the cosmetic (in FIG. 7, both ends of the resin sponge-like coating tool S extend beyond the ends of the substrate 4 for evaluating the ultraviolet transmittance ratio). In addition, it is preferable that the sponge-like coating tool is made of urethane sponge.
[0029] (Coating process 3 (preparation process)) In the preparation step, a layer (a material layer on the applicator surface to which oils and fats are selectively difficult to adhere) made of a material having a surface with oil adhesion prevention properties (a material having a property that can substantially maintain a dispersion state of other substances dispersed with these oils) having a necessary property for maintaining a dispersion state of the oil contained in the cosmetic or the oil used to make the cosmetic into a measurement sample and other substances dispersed with these oils is formed on the surface of the cosmetic coating layer obtained in the coating step 2, for example, on the surface of a cylindrical applicator. Hereinafter, this layer is referred to as a layer or film that suppresses oil adsorption. Then, using a modified applicator with a gap of 20 to 30 μm on the surface of the substrate for evaluating the ultraviolet transmittance ratio, which is an applicator to which this film is fixed with double-sided tape, the film is applied at a speed of about 5 mm / s to prepare a measurement sample. Here, the layer or film that suppresses oil adsorption has a surface with oil adhesion prevention properties. A measurement sample having a uniform cosmetic coating layer is obtained by this coating step 3. In addition, since coating step 3 is a step for forming a thin cosmetic layer, it is necessary to limit the material of the applicator surface as described above. The above coating steps 1 and 2 are for forming a thicker cosmetic layer. Therefore, the applicator used in coating steps 1 and 2 is not limited to a material having water repellency as described above or a material having a property capable of maintaining a dispersed state with other substances that are substantially dispersed with these oils, as in coating step 3.
[0030] The material with an oil-resistant surface used in the coating process 3 is presumed to have the above properties, have a constant film thickness when made into a material layer, and do not tear or wrinkle during coating. As a result of examining the materials shown in Table 1, it was found that hydrophilic treated films such as hydrophilic treated polyester film and hydrophilic treated polyethylene terephthalate film, and films and layers made of fluororesins such as polyvinylidene fluoride and polyethylene naphthalate (PEN) are preferred. In addition to polyvinylidene fluoride, tetrafluoroethylene, fluorinated ethylene propylene polymer, perfluoroalkoxy polymer, ethylene tetrafluoroethylene copolymer, ethylene chlorotrifluoroethylene copolymer, polychlorotrifluoroethylene, and polyvinyl fluoride are also preferred as fluororesins. Although any of the layers of these materials could be used, polyethylene naphthalate (PEN) film, which has particularly excellent durability, was the most suitable. Layers made of fluororesins also showed good results. In addition, although stainless steel has a contact angle with water of 90°, stainless steel may destroy the emulsion in emulsion-based cosmetics, for example, and as a result, a uniform coating film may not be formed. The contact angles with water shown in Table 1 are contact angles with pure water at 25°C.
[0031] Next, a resin film such as PEN (as a material with a surface that prevents adhesion of oil) having a thickness of 25 μm and a height of unevenness of 1.0 μm or less was attached to a stainless steel cylindrical applicator with a gap of 100 μm without wrinkles using Nichiban's Nicetack (weak adhesion, thickness 60 μm), and the surface was further smoothed with a plastic scraper. The weight of this applicator covered with a resin film such as PEN is light at 266 g, and it was confirmed that the applicator floats up during application of a highly viscous cosmetic material, resulting in an inconsistent film thickness. Therefore, a stainless steel block of 248 g was placed on the applicator, and a total of 508 g was applied. In particular, since the height of the unevenness is 1.0 μm or less, a cosmetic layer with a smooth surface could be formed. The smoother the surface of this resin film, the smoother the surface of the formed cosmetic layer, and the subsequent measurement accuracy can be improved. This characteristic does not change even if the cosmetic material has different properties such as a liquid or solid. Furthermore, all of the materials indicated above as materials whose surfaces have oil-resistant properties showed results similar to those of the above-mentioned PEN in the following examples. It should be noted that no special processing is required for the metal applicator with a gap of 500 μm to 1000 μm used in the above coating process 1. The problem of the applicator floating up during coating becomes evident when the applicator gap is narrow, and is therefore likely to occur in coating processes 1 and 2, but no special measures are required in coating process 1, where the gap is large.
[0032] An example of the cylindrical applicator is shown in FIG. The cylindrical applicator 7 is moved by a spreading device 9 shown in FIG. The coating spreading device 9 is a device having a cylindrical applicator 7 and support parts 8 for supporting both ends of the cylindrical applicator 7. The support parts 8 etc. fix the cylindrical applicator 7 to a frame or the like (not shown), or support the cylindrical applicator 7 so as to be capable of movement required for coating spreading. The cylindrical applicator 7 is supported by a structure (not shown) for the support part 8, for example, pins provided at both ends of the cylindrical applicator 7 are fitted into grooves extending in the vertical direction provided in the support part 8, or the entirety is integrally molded, so that the cylindrical applicator 7 can freely move up and down. The weight of the cylindrical applicator 7 resists the resistance from the cosmetic material to be spread, and the cosmetic material is uniformly applied to the substrate. Alternatively, the cylindrical applicator 7 may be fixed to the support part 8. The cylindrical applicator 7 may be obtained by cutting a single metal block, or by assembling any desired members, to obtain the cylindrical applicator 7 without any joints. For the purpose of explanation, other parts are not shown in the spreading device 9 shown in Figure 8, but it is also possible to provide, for example, a component angle to connect the two support parts 8 to form an integrated spreading device 9. The cylindrical applicator 7 shown in FIG. 8 has a shape in which the coating spreading member 2 of the above-mentioned metallic applicator is replaced with the cylindrical applicator 7. In addition, the cylindrical applicator 7 may or may not have a strictly circular cross section perpendicular to the longitudinal direction of the cylinder. The cylindrical applicator 7 may be circular, but may also have a shape in which four chords are provided on a circle as shown in FIG. 9, with the chords being flat, or may be fan-shaped. Furthermore, the cross section may be elliptical, or may have a shape in which two circles or ellipses overlap, with a flat surface partially provided, instead of the basic circular shape shown in FIG. 9. It is sufficient that the part of the cross section that comes into contact with the cosmetic is a gentle curve or a horizontal plane. The cylindrical shape of the part that comes into contact with the cosmetic is not particularly limited, but the shape of the part that comes into contact with the cosmetic during application may be a curved surface that reflects a cylinder with a cross-sectional diameter of 10 to 30 mm, or a curved surface that reflects an elliptical cross section that is not circular, such as a cross section close to such a curved surface. In the case of a horizontal surface, the width of the minor axis (the length L in FIG. 9, which is parallel to the arrow indicating the direction in which the cylindrical applicator moves relative to the substrate on the gently sloping curved or horizontal plane facing substrate B) is preferably 1.0 to 5.0 mm, and more preferably 1.0 to 3.0 mm.
[0033] Fig. 9 is a diagram showing a state where a cylindrical applicator 7 is moved in the direction of the arrow when applying a cosmetic. The cylindrical applicator 7 is moved relative to the surface of the cosmetic coating layer in the same manner as the cylindrical applicator 7 described above. The part of the cylindrical applicator that corresponds to the tip 6 of the spreading member is the approximately horizontal surface part of the lower end of the cylindrical applicator 7 in Fig. 9, and as the cylindrical applicator moves in the direction of the arrow by this lower end part, excess cosmetic 5 is also moved in the same manner. At this time, it is preferable that the gap formed between the cylindrical applicator 7 and the surface of the substrate 4 is in the range of 500 µm to 1000 µm in the coating step 1.
[0034] Although not shown in Fig. 8, the above-mentioned film that prevents oil from being adsorbed onto the surface of the cylindrical applicator may be wrapped around the entire cylindrical applicator 7 in Fig. 8 to cover the surface of the cylindrical applicator 7, or may be wrapped so as to cover only the lower part of the cylindrical applicator 7 in Fig. 8 that comes into contact with excess cosmetic material 5. When the surface of the cylindrical applicator is covered with a layer made of a material having oil adhesion prevention properties, for example, the film wrapped around the surface of the cylindrical applicator may be fixed with double-sided adhesive tape only to the upper part of the cylindrical applicator 7 that does not come into contact with excess cosmetic material 5. Also, when covering the film so as to cover only the lower part of the cylindrical applicator 7 that comes into contact with excess cosmetic material 5, the film can be fixed with double-sided adhesive film only to the part that does not come into contact with excess cosmetic material 5. As a means for fixing the film to the cylindrical applicator, other known means for fixing a film to an object (such as a clamping member such as a clip, or fixing with an adhesive) can be used instead of fixing with double-sided tape.
[0035] Here, we will explain why it is essential that the surface is made of a film or layer of a material that has oil-resistant properties. A sunscreen agent is applied to a quartz plate that has been made superhydrophilic by corona discharge using a stainless steel applicator with the shape shown in Figure 4, and a coating film is prepared that has been confirmed to have a consistent thickness using a rotary film thickness gauge. An infrared imaging microscope (Thermo Scientific iN10MX Infrared Imaging System All-in-One Microscope FT-IR) is used to measure the absorption wavenumber of 2852 cm, which is one of the characteristic absorption wavenumbers of ultraviolet absorbers. -1 When imaging was performed, it was confirmed that the concentration of the ultraviolet absorber varied depending on the location. This means that the assumption that if the thickness of the cosmetic is constant, the composition of the sunscreen agent in the cosmetic is constant regardless of the location of the coating film has collapsed. In other words, when a stainless steel applicator is used, the measurement value contains a large error. If it is possible to apply the coating using a material that does not change the concentration of the ultraviolet absorber depending on the location, it is possible to significantly reduce the error and perform accurate measurements. Therefore, coating was performed using various materials, and the distribution of the ultraviolet absorber in the coating film obtained at that time was measured using an infrared imaging microscope, and it was found that the concentration of the ultraviolet absorber did not change depending on the location, or the change was slight, when a material with a surface that prevents adhesion of oil was used. On the contrary, since the uniformity of the coating film was maintained with these materials, the reason why the concentration of the ultraviolet absorber varied depending on the location is thought to be that stainless steel is lipophilic, so as the applicator moves, the oily components in the sunscreen agent gradually adsorb to the stainless steel surface, and when the amount of adsorption reaches a certain level, it falls to the substrate side.
[0036] (About the coating process in general) The coating step 1 is a pre-coating step for the coating step 2. The stability of the thickness of the film that can be coated by the applicator in the coating step 2 tends to depend on the amount of the cosmetic on the front side of the applicator. Therefore, the coating step 2 is performed for the purpose of making the amount of the cosmetic constant. In actual use, the user spreads the cosmetic such as a sunscreen with his / her fingers or hands, so the coating step 2 reflects the physical effects such as shearing to make the thickness thinner. However, if the time required for the coating step 2 is long, the volatile components in the cosmetic evaporate and the non-volatile components of the cosmetic are concentrated. Therefore, the coating time is set to 8 to 14 seconds so that even cosmetics that are difficult to apply can be applied uniformly. The coating step 3 is performed to make the cosmetic that became non-uniform in the coating step 2 into a uniform coating film.
[0037] [Table 1]
[0038] (drying process) After the coating step 3, the plate is left in a cool, dark place for one to one and a half hours. At this time, it is possible to irradiate the plate with ultraviolet light. In countries other than Japan, the SPF value of commercially available sunscreens is 100 to 150, and the performance of current SPF analyzers is insufficient to measure these cosmetics. A super-sensitive spectrophotometer that can stably measure absorbance up to about 5.5 is required, but the sample must be placed vertically due to the arrangement of the integrating sphere and the light path of the super-sensitive spectrophotometer. Therefore, a drying process is required for a certain period of time to prevent the coated sample from dripping.
[0039] [Measure the ultraviolet absorption spectrum of the measurement sample] (Process of measuring the absorption spectrum of the cosmetics applied to each substrate using an ultra-high sensitivity spectrophotometer) A 150 mm integrating sphere was installed on a PerkinElmer UV-Visible Spectrophotometer LAMBDA 850+ (measurement sensitivity: absorbance 8). The assembled cell of the measurement sample was fixed so as to match the hole in the center of the anodized aluminum jig in Figure 3, so that the appearance of the assembled cell installed on the jig for installing the spectrophotometer would be as shown in the external photograph of Figure 3. This jig was fixed with double-sided tape to the outside of the light receiving part of the integrating sphere so that it was parallel to the opening of the integrating sphere. With this device, the absorbance in the range of 290 to 400 nm was measured. The reason for using this UV-Vis spectrophotometer, LAMBDA 850+, is that resources.perkinelmer.com describes a measurement example of PerkinElmer's LAMBDA 850+ and LAMBDA 1050+, which has equivalent performance in the UV range, as Materials Characterization: UV / Vis / NIR Spectroscopy; A Spectroscopic in vitro Method for the Calculation of Sunscreen SPF Values. In other words, the measurement of UV protection ability using this device has already been proven.
[0040] This operation was carried out for each of the three types of measurement samples (lipophilic substrate, intermediate substrate, and hydrophilic substrate). It is preferable to obtain data from three different measurement locations per measurement sample. A sample with a reference thickness (reference film thickness) is obtained as follows.
[0041] [B. A process of determining the absorbance of a cosmetic material at a standard thickness using an assembled cell, and determining the SPF value and UVA-PF value using the following formula (for cosmetics other than solid cosmetics)] (Filling the sample into the assembly cell) A jig was prepared to fix an assembled cell (T-20-UV-0.1, manufactured by Tosoh) with an internal space thickness of 100 μm, and the female mold of the assembled cell (the cell with the recess formed) was placed in the cell. After pouring the sample into the recess (100 μm deep) of the cell, a smooth quartz plate of 100 × 100 mm was slowly pressed from above to remove air bubbles in the sample. Since the cell and the quartz plate are parallel in this state, the quartz plate was shifted horizontally to obtain a reference film thickness sample in which the assembled cell was filled with the sample to a thickness of 100 μm. Next, the periphery and back side of the cell were cleaned. The reason for setting the thickness at 100 μm is that when an emulsion is measured at a thickness of 50 μm, the measured absorbance often varies greatly depending on the measurement position. This is because the component composition in the emulsion varies greatly depending on the measurement position at a thickness of 50 μm. On the other hand, with a thickness of 500 μm, there is no variation in absorbance depending on the measurement position even when measuring various cosmetics, but for cosmetics with high SPF values, the absorbance becomes too large and the Beer-Lambert law may not be satisfied. At a thickness of 100 μm, there is variation in absorbance depending on the measurement position, but this can be corrected by multiple measurements, so an assembly cell with a thickness of 100 μm was selected as the reference thickness. In addition, the reason for using a method for filling the sample into the assembled cell in which the cell and a smooth quartz plate are parallel is that when scraping the surface of the assembled cell using the scraping method (a method in which a quartz plate is placed at an angle to smooth the surface of the assembled cell), it was found that with some cosmetics more than the intended amount is scraped off, and in this case the thickness is approximately 80 to 90 μm, so this method was developed to avoid this.
[0042] (Heating process for reference thickness sample) A precision hot plate was prepared and stabilized at 60°C. The above-mentioned reference film thickness sample was placed on the hot plate and left for 15 minutes. After 15 minutes, the sample was collected to obtain a reference film thickness sample. Usually, when measuring multiple reference film thickness samples for business purposes, about 10 assembly cells are placed on the hot plate at the same time, so it is necessary to use a hot plate for physicochemical use that can precisely control the temperature so that there is no uneven heat, and it is preferable to use a large hot plate to avoid sample mix-ups.
[0043] The reason for heating the standard thickness sample is that the thickness of the cosmetic material in the standard thickness sample is 100 μm, so even if it is left for an hour without heating, the state will be different from the state of the cosmetic material on each of the above-mentioned coated substrates. In particular, the amount of residual volatile components changes. Therefore, when several cosmetics were measured, for example, as shown in Figure 2, which shows the relationship between the heating time and absorbance of a certain sunscreen agent at 60 °C, the absorbance of many of them does not change much after 5 minutes of heating, when volatile components such as water and ethanol have mostly evaporated. In Figure 2, the absorbance was measured for each heating temperature. Two samples were obtained by heating for 15 minutes, and the absorbance of each was measured. ). However, it was found that some cosmetics take a little longer, so the cosmetics were heated for 15 minutes with a margin of error to fully remove the volatile components in the cosmetics. In Figure 2, only 15 minutes were measured twice. In addition, the reason for the large decrease in absorbance after 5 minutes of heating is that in emulsions, light is refracted at the interface between the water and oil, causing light scattering (which makes it appear white in visible light), and when the water is removed by heating, this scattered light decreases, resulting in a decrease in absorbance.
[0044] (Spectrophotometer measurement process for standard film thickness sample) The assembled cell is small, 12.5 x 45 mm, and cannot be set in the spectrophotometer as is. Therefore, a black plastic jig was developed and installed as shown in Figure 3 so that the assembled cell can be closely attached to the opening of the integrating sphere of the spectrophotometer. The assembled cell was installed in the opening of the black plastic jig, and the absorbance at a wavelength of 400 nm was measured. The reason for closely attaching the assembled cell to the opening of the integrating sphere is that cosmetics scatter light, and if the assembled cell is not closely attached to the integrating sphere, the effects of scattered light cannot be fully reflected. The reason for using 400 nm light is that it is the closest to visible light in the 290-400 nm wavelength range used to measure ultraviolet light, and is the wavelength that is least affected by light scattering due to fine particles. If it is only the whiteness of the cosmetic, it is possible to use a wavelength such as 660 nm, but when measuring the substrate, it is necessary to measure it separately from the wavelength range of 290-400 nm. Therefore, considering that there is a time limit of measuring the substrate within 1-1.5 hours after coating, it is efficient to use 400 nm. In addition, some cosmetic products, such as lotions, do not absorb or scatter light with a wavelength of 400 nm. In that case, the measurement wavelength is shifted gradually to the shorter wavelength side, such as 380 nm, 360 nm, 340 nm, 320 nm, and 300 nm, and a wavelength that gives a significant difference in absorbance is selected.
[0045] In order to correct for measurement variability in the assembly cell, it is preferable to measure the absorbance at two different points in the assembly cell. In addition, since it was found that there are cosmetics that cause variability in the creation of the standard thickness sample, it is necessary to create the standard thickness sample multiple times. As a preferred example, two standard thickness samples are created, two points in each assembly cell are measured to obtain four absorbance data, and the standard deviation / average value is calculated. If this exceeds 0.2, one more standard thickness sample is added, and the average value of the six absorbance points obtained is used as the absorbance of the corresponding product at a thickness of 100 μm.
[0046] The absorbance of the sample at 100 μm was obtained by the above procedure, and this was converted to 20 μm by multiplying it by 0.2. This is the absorbance of 2 mg / cm on the human back in the in vivo SPF measurement method. 2 The measurements were taken by applying the cosmetic material at a rate of 2mg / cm 2 This is an operation to compare values at a thickness of 20 μm, which corresponds to
[0047] [C. A process of selecting the measurement sample with the maximum SPF value based on the SPF values obtained for multiple measurement samples, and determining the SPF value and UVA-PF value of the measurement sample as the in vitro SPF value and in vitro UVA-PF value of the one type of cosmetic (cosmetic other than solid cosmetic)] Since there are nine absorbance data points for each of the aforementioned boards, if the absorbance at 400 nm is used as the standard, for example, the nine 400 nm absorbance values are compared with the 20 μm absorbance values measured using the above assembly cell, and the entire measurement data is corrected to the 20 μm value. The correction method is simply to calculate the ratio of the absorbance at 400 nm to the absorbance at 20 μm for each wavelength. The average of the corrected data for each wavelength is calculated for each board, and one spectral data is obtained for each board, and this is used to calculate the in vitro SPF value and in vitro UVA-PF value. Then, the board with the highest SPF value among the three boards is selected, and the SPF value and UVA-PF value of that board are determined as the values for that product. Suppose that the cosmetic layer after application is affected by the hydrophilicity (lipophilicity) and other properties of the substrate surface, causing phase separation or dewetting of the cosmetic. As a result, ultraviolet light is more easily transmitted through the substrate as a whole. In other words, a substrate with a uniform cosmetic layer and the lowest ultraviolet light transmittance is a substrate with the maximum SPF value (substrate for evaluating ultraviolet light transmittance ratio). On such a substrate, the cosmetic layer is formed without the cosmetic composition changing its properties, as compared to other substrates. Therefore, by selecting a substrate with the maximum SPF value and determining the SPF value and UVA-PF value thereafter, the inherent properties of the cosmetic can be accurately measured.
[0048] [D. A process for determining the in vivo SPF equivalent value of the one cosmetic product from the relational equation between the in vivo SPF value and the in vitro SPF value, and further determining the in vivo UVA-PF equivalent value of the one cosmetic product from the relational equation between the in vivo UVA-PF value and the in vitro UVA-PF value (common to cosmetics other than solid cosmetics, powder cosmetics, and stick-type cosmetics)] Here, when calculating in vitro SPF values and in vitro UVA-PF values from spectral data, the cosmetics industry often uses the ISO standard calculation formula described in Non-Patent Document 4. However, the inventors' research (Miyuki Fujishiro, Shoichi Yahagi, Akihiro Kuroda, Taisuke Banno, Kouichi Asakura, “Investigation on the validity of in vitro UVA-PFevaluation method for sunscreen samples”, 2nd World Oleoscience Congress (WCOS 2022)) showed that the ISO method calculation formula may not be able to properly reflect differences in absorbance in the UVB region. In addition, from the measurement results of 206 commercially available sunscreens around the world, when the relationship between the UV protection values or indicators displayed on the products and the calculated values obtained by the present invention using the ISO standard calculation formula for both SPF and UVA-PF values was examined, it was found that the coefficient of determination (R2 value) of the linear regression model became very poor. On the other hand, before the ISO standard formula was proposed (1979), another formula had been proposed mainly in the Middle East and South America (Elizangela AbreuDutra et al., "Determination of sun protection factor (SPF) of sunscreens by ultraviolet Spectrophotometry", Brazilian Journal of Pharmaceutical Sciences, 40, 3, 381-385, 2004). This formula calculates the SPF for each wavelength using the following formula: SPF=CF×ΣEE(λ)×I(λ)×Abs(λ) (Formula 1) The SPF calculated for each wavelength is calculated in the range of 290 to 320 nm, and these values are integrated. Here, CF is the correction factor (=10), EE is the erythema effect spectrum, I is the solarintensity spectrum, and Abs is the absorbance of sunscreen product. CF, EE, and I are constants, and EE is shown as a value for each wavelength in the table of APPENDIX I of Non-Patent Document 4 shown in FIG. 17, and I is shown in the same table as the UV-SSR source Wm -2 nm -1 Since the numerical value for each wavelength is shown as , this was used. When the SPF value was calculated using this formula 1, a much larger coefficient of determination was obtained compared to the calculation formula of the ISO standard. Furthermore, since the result of formula 1 shows a better consistency with the human measured value, this formula 1 was used in the present invention (the coefficient of determination of the ISO standard is 0.5336, while that of formula 1 is 0.6792). Also, the following formula UVA=CF×ΣEE(λ)×I(λ)×Abs(λ) (Formula 2) The UVA was calculated for each wavelength in the range of 320 to 400 nm, and the values calculated for each wavelength were integrated. Here, CF, EE, and I are the same as those in the above (Formula 1), where EE is the erythemal effect spectrum, I is the solar intensity spectrum, and Abs is the absorbance of sunscreen product. These are also shown in the table of APPENDIX I of Non-Patent Document 4 shown in FIG. 17. When UVA was calculated using this Formula 2, a much larger value was obtained as compared with the coefficient of determination obtained from the calculation formula of the ISO standard (the coefficient of determination of the ISO standard is 0.5767, while that of Formula 2 is 0.7900). Therefore, in the present invention, the UVA-PF was also calculated using this formula with the wavelength range changed to 320 to 400 nm.
[0049] The in vitro SPF value and in vitro UVA-PF value obtained above cannot be compared directly with the conventional in vivo SPF value or in vivo UVA-PF value. In order to make a comparison, a correlation equation is required. The equations obtained from the measurement results of over 200 commercially available sunscreens around the world (ratio of in vitro SPF value to in vivo SPF value, ratio of in vitro UVA-PF value to in vivo UVA-PF value) (relationship equation between in vivo SPF value and invitro SPF value, and relationship equation between in vivo UVA-PF value and in vitro UVA-PF value) are as shown below, so we will use these to calculate the in vivo SPF equivalent value and the in vivo UVA-PF equivalent value. Relationship between in vivo SPF value and in vitro SPF value: in vivo SPF equivalent value = in vitro SPF value / 0.101 (Equation 3) Relationship between in vivo UVA-PF value and in vitro UVA-PF value: in vivo UVA-PF equivalent value = in vitro UVA-PF value / 2.13 (Equation 4) In addition, in the above measurement results of over 200 commercially available sunscreens from around the world, a comparison was made using both the sunlight spectrum defined by the American Association of Textile Science and Technology (AATCC) and the UV-SSR defined by ISO. As a result, there was not much difference in the UVA-PF results, but the coefficient by AATCC was slightly higher. It seems that it does not matter which one is used in practice. If you want to calculate using the UV-SSR light source specified by the ISO method, you can use UVA-PF: in vivo UVA-PF equivalent value = invitro UVA-PF value / 3.6680.
[0050] Here, we will show how to calculate the formulas (the relationship between the in vivo SPF value and the in vitro SPF value, and the relationship between the in vivo UVA-PF value and the in vitro UVA-PF value) obtained from the measurement results (ratio between the in vitro SPF value and the in vivo SPF value, and the ratio between the in vitro UVA-PF value and the in vivo UVA-PF value) of over 200 commercially available sunscreens from around the world. These formulas statistically process the relationship between the SPF value and UVA-PF value obtained from the above steps A to D and the UVA-PF value labeled on the product. Currently, in vivo values measured using humans are used internationally for SPF. Regarding UVA-PF, some manufacturers display actual values on the package, while others display the PA classification, but all of them use in vivo values measured using humans. When the UVA-PF value is listed, it can be used as it is, but when the PA classification is listed, the range of the in vivo UVA-PF value is specified, so in the present invention, the intermediate value of the range is used as the in vivo UVA-PF value corresponding to the PA classification. Specifically, the in vivo UVA-PF value is 3 for PA+, 6 for PA++, 12 for PA+++, and 24 for PA++++. The in vitro SPF values of all products are calculated using the method of the present invention, and this number is shown on the vertical axis, and the in vivo SPF value shown on the package is shown on the horizontal axis. A linear approximation through the origin was performed, and the approximation formula and the coefficient of determination were obtained. Based on this method, the relationship between the In vivo SPF value and the Invitro SPF value in the above formula 3 was obtained. In the same way, the in vitro UVA-PF values of all products were calculated, and these values were plotted on the vertical axis and the in vivo UVA-PF values shown on the packaging on the horizontal axis. A linear approximation was performed passing through the origin, and the approximation equation and coefficient of determination were obtained. Finally, the relationship between the in vivo UVA-PF values and the in vitro UVA-PF values, as shown in Equation 4 above, was obtained.
[0051] Using the above method, it is possible to create standard film thickness samples with a film thickness of 100 μm using an assembled cell and measure the absorbance of common emulsions, lotions, and spray products, including makeup cosmetics such as liquid foundation. Furthermore, the substrate that maximizes the SPF value is selected, and the in vivo SPF equivalent value and the in vivo UVA-PF equivalent value can be obtained through calculations using the above formulas (1) to (4). Next, we will explain the specific procedures for measuring powder cosmetics such as non-fluid powder foundations and stick-type cosmetics. The methods for calculating the in vivo SPF equivalent and in vivo UVA-PF equivalent are the same as those for the fluid cosmetics mentioned above.
[0052] [B. A process of determining the absorbance of a cosmetic material at a standard thickness using an assembled cell, and determining the SPF value and UVA-PF value using the following formula (powder cosmetic material)] (Filling the sample into the assembly cell) A glass or ceramic plate is placed on the balance, and the powdered cosmetic is placed on it in the shape of a doughnut. A glass or ceramic plate with a smooth surface of about 12 cm square is preferable because it is lightweight and easy to work with. The scattered powder is cleanly removed using a brush. The weight of the powdered cosmetic required per substrate is approximately 1.5 g, and the weight is accurately measured and recorded. A dropper is used to drip approximately 1.5 g of a non-volatile oil that does not absorb in the ultraviolet range into the hole of the doughnut, and the weight is accurately measured and recorded. As a non-volatile oil that does not absorb in the ultraviolet range, non-polar oils and ester oils that tend to mix easily with the powdered cosmetic are preferable, and squalane, which is available internationally and has stable quality, is particularly preferable. The standard for non-volatility is that it is poorly volatile or non-volatile at room temperature and normal pressure, and generally refers to a weight fluctuation of less than 0.1% in 10 minutes. The viscosity of the non-volatile oil used in the present invention is not particularly limited, but for example, a viscosity of about 6 to 1000cs is easy to handle. In addition, it is preferable to use a balance with a top plate capable of measuring 1 mg. After weighing, mix thoroughly on a glass or ceramic plate using a spatula for art supplies until no lumps remain and a uniform paste is formed. It is also important to mix little by little, rather than trying to mix everything at once. In addition, since there may be cases where the powder cosmetic that has not been mixed well is stuck to the back of the spatula, it is necessary to check at the end. When the mixed paste is completed, pour the entire amount of the mixed paste onto the substrate, and carry out the above coating process 1 to coating process 3 in order. The height of the unevenness of the surface of the applicator used in coating process 3 in the part that comes into contact with the cosmetic is 1.0 μm or less. Next, the drying process is omitted, and the spectrophotometer measurement process is carried out. The same applies to solid cosmetics that are not powders.
[0053] For the standard thickness sample, a mixed paste is obtained in the same manner as for the liquid cosmetic, except that the amount of the powder cosmetic and the non-volatile oil that does not absorb in the ultraviolet region are about 1g and about 1g, respectively. Then, as in the case of the liquid cosmetic, the paste is placed in the recess of the assembly cell, left for a few minutes, and then the plate of the assembly cell is placed on top and pressed, and the short side of the assembly cell is held with the fingers and the paste that has come out around the periphery is wiped off. Pressure is slowly applied from one side of the long side of the plate of the assembly cell to remove as many air bubbles as possible. Here, the biggest cause of measurement value fluctuations in the preparation of powder cosmetic samples is the presence of air bubbles that are mixed in during kneading, so when the obtained sample is held up to light, if there are air bubbles, the portion is not measured, and the spectrophotometer measurement process of the standard thickness sample with a thickness of 100 μm is carried out. Also, when placing a large excess amount of paste in the recess of the assembly cell, the air bubbles are easily removed if the plate is pressed against it. Two or more sets of standard thickness samples are prepared.
[0054] Next, for each substrate and standard film thickness sample, the adjusted absorbance obtained by dividing the absorbance value obtained by the weight of the powder cosmetic / (weight of the non-volatile oil + weight of the powder cosmetic) is used as the absorbance of the sample, and the measurement values of the powder cosmetic are obtained in the same manner as the spectrophotometer measurement process for the standard film thickness sample in the case of cosmetics other than solid cosmetics, and the in vivo SPF equivalent value and the in vivo UVA-PF equivalent value are calculated.
[0055] [B. A process of determining the absorbance of a cosmetic material at a standard thickness using an assembled cell and determining the SPF value and UVA-PF value using the following formula (stick-type cosmetic material)] (filling of the sample into the assembled cell) Next, we will explain the procedure for measuring stick-type cosmetics such as lipstick and stick-type sunscreen. For stick-type cosmetics, it is preferable to first measure the substrate and then the standard film thickness sample. This is because there are many cosmetics that do not absorb or scatter light at a wavelength of 400 nm, so it is necessary to determine the measurement wavelength to be used for measuring the standard film thickness sample from the measurement results of the substrate. Place a glass or ceramic plate on the balance, rub about 0.6g of stick-type cosmetics on it with a spatula in a square shape, and accurately measure and record the amount of cosmetics. Next, drop about 2.4g of a non-volatile oil that does not absorb in the ultraviolet range into the center of the square shape, and measure and record it in the same way. Mix little by little using a spatula for art supplies, and when the entire mixture is mixed, transfer the mixed paste to a container such as a disposable aluminum cup for food, and heat it on a hot plate at 60°C for 15 minutes. At this time, it is necessary to check because cosmetics that have not been mixed well may be stuck to the back of the spatula. If phase separation occurs after heating, mix well while it is still warm. The entire amount of the mixed paste is poured onto the substrate, and the above-mentioned coating process 1 to coating process 3 are carried out in that order. The height of the surface irregularities of the part of the applicator used in coating process 3 that comes into contact with the cosmetic is 1.0 μm or less. Next, the drying process is omitted, and the spectrophotometer measurement process is carried out.
[0056] For the standard thickness sample, a mixed paste is obtained in the same manner as for the preparation of the standard thickness sample of the powder cosmetic, except that the amount of the stick cosmetic to be applied is about 0.3 g and the amount of the non-volatile oil that does not absorb in the ultraviolet region is about 1.2 g. Two or more sets of standard thickness samples are prepared in the same manner as for the powder cosmetic.
[0057] Next, for each substrate and standard thickness sample, the adjusted absorbance obtained by dividing the absorbance value by the weight of the stick cosmetic / (weight of the non-volatile oil + weight of the powder cosmetic) is used as the absorbance of the sample, and the same method as for preparing the standard thickness sample of the powder cosmetic is used to obtain the measured value of the stick cosmetic at a thickness of 100 μm. In this process, the height of the unevenness is also 1.0 μm or less.
[0058] Here, in the present invention, a very sensitive measuring device with a measurement sensitivity of the main body reaching an absorbance of 8 is used in the spectrophotometer measurement process, but in the cosmetics industry, a measuring device called an SPF analyzer has been used in the past. There are two typical models, one with a measurement sensitivity of 2 absorbances and the other with a measurement sensitivity of 3 absorbances. On the other hand, as mentioned above, there is an example of a measurement with an absorbance of 8. Although there are differences depending on the product, it seems that the method of the present invention can be implemented without any problems in terms of sensitivity for products with an SPF value of 15 or less even with the two existing models. For products with an SPF value higher than that, some measurement value can be obtained, but it is better to think that it contains a large error factor. As we reported at the aforementioned WCOS 2022, we have confirmed that when the absorbance exceeds 2, the absorbance is displayed significantly differently between measuring devices, and the objectivity of the measurement value cannot be guaranteed unless the sensitivity problem of the measuring device is fully recognized before implementation.
[0059] In addition, the problem of the smoothness of the substrate is noted here. In the cosmetics industry, human skin has texture and unevenness, so the substrate for measurement also needs to be uneven, and development has been promoted. On the other hand, in the present invention, the relationship between the measured values obtained from the in vivo SPF measurement method and the in vivo UVA-PF measurement method and the in vitro SPF and UVA-PF values obtained by the method of the present invention (the above-mentioned in vivo SPF equivalent value calculation formula and the above-mentioned in vivo UVA-PF equivalent value calculation formula) is obtained, and the in vivo SPF and UVA-PF equivalent values are obtained without using the in vitro SPF and UVA-PF values as they are. In the in vivo method, the measurement is performed by pressing the ultraviolet irradiation probe firmly against the back of a human. https: / / solarlight.com / product / model-601-multiport-spf-testing-6-output-solar-simulator / is a catalog of the ultraviolet irradiation device most frequently used in contracted measurements, and it is shown that a 6-unit irradiation probe is used. The ultraviolet irradiation part of this probe is cylindrical and is structured so that ultraviolet light guided by an optical fiber is irradiated from the center. When an 8 mm cylinder is pressed firmly against human skin, the skin is stretched to the maximum extent and becomes flat. In this invention, we are looking for a relationship with the measurement results in this flat state, so we use a smooth measurement plate. The uneven plate is suitable for measuring the effects of ultraviolet rays that consumers are exposed to in real life, rather than the in vivo measurement method described above, and it is considered that it is essentially difficult to compare it with existing in vivo measurement methods. EXAMPLES
[0060] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0061] [Reason why the surface of the applicator used in coating process 3 that comes into contact with the cosmetic should be formed of a material layer that prevents oil adhesion] A test to confirm the change in the coating film when a layer of material that prevents oil adhesion is provided on the coating part of the applicator and when it is not provided. (Measurement conditions) An infrared imaging microscope (Thermo Scientific iN10MX Infrared Imaging System All-in-One Microscope FT-IR) was used, with a measurement interval of 100 μm × 100 μm and a measurement wave number of 2852 cm -1 The transmittance measurement using liquid nitrogen and integration were performed 16 times for each measurement point, and a synthetic quartz plate was used as the reference. The measurement range was 70 mm in the direction of the applicator's movement. This device originally obtained the results of the mapping analysis in color, but in this patent, the white areas indicate higher density (lower transmittance). Measurement sample: Water, zinc oxide, ethanol, ethylhexyl methoxycinnamate, isocetyl myristate, glycerin, propylene glycol, bisethylhexyloxyphenol methoxyphenyl triazine, polyhydroxystearic acid, phenoxyethanol, methicone, xanthan gum, fragrance, EDTA-2Na, biosaccharide gum-1, colorant, (sodium acrylate / sodium acryloyldimethyl taurate) copolymer, isohexadecane, polysorbate 80, and sorbitan oleate (a preparation obtained by selecting and adjusting the components from the infrared spectrum of each component so that the behavior of the ultraviolet absorber (oil layer) becomes clear in infrared observation). Applicator: A cylindrical applicator with a stainless steel surface and a cylindrical applicator with various material layers fixed to the surface were used. Coating conditions: Coating was performed at a speed of 5 mm / s using a precision coating device. Substrate used for coating: A 10 x 10 cm synthetic quartz plate surface was treated for 90 seconds using a corona discharge device (BD-20A Laboratory Corona Treater manufactured by Electro-Technic Products). The treatment was performed using a robot so that the entire surface was treated uniformly. Film Thickness Measurement: Film thickness was measured using a rotary film thickness gauge.
[0062] (Test Results) Figure 10 shows the results of observation with an infrared imaging microscope of a coating applied using a stainless steel cylindrical applicator under the above measurement conditions. The part to the right of -15000 is the part of the coating that is usually used in evaluation tests of UV protection ability. A rotary film thickness meter confirmed that this part had a constant film thickness. The white parts in Figure 10 are parts where the concentration of UV absorber is relatively high. This shows that even if the coating appears to be of a constant and uniform thickness, the concentration of UV absorber is not constant. Figure 11 shows the results of observation with an infrared imaging microscope of a coating film applied using an applicator similar to the cylindrical applicator described above, except that a hydrophilized polyethylene terephthalate film was fixed to the surface that comes into contact with the cosmetic material. In particular, no areas of high concentration of the UV absorber were observed, indicating that stable coating had been achieved. Furthermore, the results of observation with an infrared imaging microscope when a polyethylene terephthalate film that had not been hydrophilized is used are shown in Figure 12. It can be seen that without hydrophilization, there are variations in the concentration of the ultraviolet absorbing agent.
[0063] The results of observation with an infrared imaging microscope of a coating film applied using an applicator with a polyimide tape attached are shown in Figure 13. It can be seen that there is a large variation in the concentration of the UV absorber. The results of observation with an infrared imaging microscope of a coating film applied using an applicator with a polyvinyl chloride tape attached are shown in Figure 14. It can be seen that there is a large variation in the concentration of the UV absorber. The results of observation with an infrared imaging microscope of a coating film applied using an applicator with a silicone rubber fixed to it are shown in Figure 15. It can be seen that there is a large variation in the concentration of the UV absorber. The results of observation with an infrared imaging microscope of a coating film applied using an applicator with a PEN film fixed to it are shown in Figure 16. In particular, no areas of high concentration of UV absorber were observed, indicating that stable coating had been achieved. In this way, various materials were selected based on whether or not they had high-concentration areas, and it was found that PEN and hydrophilized polyethylene terephthalate had excellent coating uniformity.
[0064] Example 1 This section describes an example of a series of steps to obtain the in vivo SPF equivalent value and the in vivo UVA-PF equivalent value of this product using a milky cosmetic product consisting of the ingredients shown in Table 2. The UV protection ability of the milky cosmetic product shown in Table 2 was measured using humans, and the SPF value was 56, and the UVA-PF was 19.9. The spectrophotometer used was a PerkinElmer UV-Visible Spectrophotometer LAMBDA 850+ (measurement sensitivity: absorbance 8) equipped with a 150 mm integrating sphere, and the assembly cell used was a Tosoh T-20-UV-0.1. The drying time for each substrate was 1 hour. In coating process 1, a 500μm stainless steel 4-sided applicator was used to flatten the emulsion-type cosmetic. Next, in coating process 2, a sponge-type urethane (15mm wide, 10mm high, 35mm long) coating tool was attached to the tip of the rotating device, and the rotation coating speed was 260rpm, and the coating was stretched for 12 seconds. PEN was used as the coating material for the cylindrical applicator used in coating process 3 (the cross section of the part that comes into contact with the cosmetic during application is a curved surface that reflects a circle with a diameter of 12mm), and the gap with each substrate was 25μm. The three types of substrates used were an acrylic polyisocyanate-treated plate (contact angle 80° after one week of application of acrylic polyisocyanate), a hydroxyalkyl cellulose-treated plate (contact angle 51°-52° after one week of application of hydroxyalkyl cellulose), and an inulin-coated plate (inulin-coated quartz plate) (contact angle 23°-26° after one week of application of inulin). All of these contact angles were measured with pure water at 25°C.
[0065] [Table 2]
[0066] As substrates for evaluating the ultraviolet transmittance ratio of multiple types with different contact angles, one each of a lipophilic moisture-curing acrylic-based polyisocyanate (simply referred to as polyisocyanate in the table)-treated plate, a hydroxyalkyl cellulose-coated plate, and an inulin-coated plate were prepared. The emulsion shown in Table 2 was applied to the plates as coating step 1 using a stainless steel applicator with a gap of 500 μm. Then, as coating step 2, the emulsion was immediately spread for 12 seconds at 260 rpm using a rotating device with a urethane sponge attached. Then, as coating step 3, a coating film was immediately formed using the above-mentioned PEN-coated cylindrical applicator. The plates were stored in a cool, dark place for 1 hour, and the absorbance was measured at three points on each plate using a spectrophotometer.
[0067] Two sets of assembled cells with a depth of 100 μm were separately prepared and filled with the emulsions shown in Table 2. After filling, the cells were placed on a precision hot plate heated to 60° C. for 15 minutes and then cooled to room temperature. The absorbance at 400 nm was measured at two points in each assembled cell using a spectrophotometer, and a total of four measured values were obtained. The actual measured values were 1.174941, 1.159418, 1.277993, and 1.155809, with an average absorbance of 1.19204, a standard deviation of 0.0579, and a standard deviation / average absorbance of 4.9%. Since the standard deviation / average absorbance of 4.9% was less than 20%, it was decided to carry out the measurements at four points. The average absorbance of 1.19204 is the value at 100 μm, so multiply it by 0.2 for 20 μm to get 0.238408. Using this value as a reference, the spectrum equivalent to a film thickness of 20 μm was calculated by proportional calculation from the absorbance values at 400 nm of the measurements at nine points on each plate.
[0068] Spectral data equivalent to 20 μm was obtained from nine measurement points, and this data was used to calculate the SPF and UVA-PF values according to the above formulas (1) and (2) as Example 1, and the SPF and UVA-PF values according to the ISO method standard calculated in accordance with Non-Patent Document 4 as Comparative Example 1. Note that in the calculation formulas (1) and (2), values using the solar spectrum data defined by AATCC were shown as the solar spectrum. The results are shown in Tables 3 and 4.
[0069] [Table 3]
[0070] [Table 4]
[0071] From Table 3, it can be seen that the hydroxyalkyl cellulose coated plate showed the highest SPF value calculated by formula 1, and the in vitro SPF value of this product was about 6.8, and the in vitro UVA-PF value calculated by formula 2 was about 45.9 measured using the same plate. When this value is calculated using formula 3, the in vivo SPF equivalent is 67.7, and when calculated using formula 4, the in vivo UVA-PF equivalent is also 21.6. In the case of the ISO method, the values are used as they are, so the in vitro SPF value is 296 and the in vitro UVA-PF value is 26.6, which is a large difference between the two. On the other hand, as mentioned above, the in vivo measured values of this product were SPF 56 and UVA-PF 19.9, and it was found that the measurement method of the present invention showed values extremely close to the measured values of the in vivo method compared to the ISO method used as a comparison example. Furthermore, when films made of hydrophilic treated polyester, hydrophilic treated polyethylene terephthalate, polyvinylidene fluoride, tetrafluoroethylene, fluorinated ethylene propylene polymer, perfluoroalkoxy polymer, ethylene tetrafluoroethylene copolymer, ethylene chlorotrifluoroethylene copolymer, polychlorotrifluoroethylene, and polyvinyl fluoride were used instead of the above PEN, a thin layer made of the emulsion shown in Table 2 and having the same properties as the original properties of this emulsion could be formed on a hydroxyalkyl cellulose coated plate, just as when PEN was used.
[0072] Example 2 Measurements were carried out using a commercially available powder cosmetic (face powder). The SPF value listed on the packaging of the commercially available product was 32, the PA classification was +++ (corresponding to a UVA-PF of 8 to 16) (the in vivo UVA-PF value corresponding to the PA classification is 12), and the ingredients were listed as follows: Talc,Perlite, Titanium Dioxide, Ethylhexyl Methoxycinnamate, Dimethicone, AluminumHydroxide, Stearic Acid, Silica, Methicone, Caprylyl Glycol,Ethylhexylglycerin, BHT, Cetyl PEG / PPG-10 / 1 Dimethicone, Tocopherol,Pentaerythrityl Tetra-di-t-butyl Hydroxyhydrocinnamate, (+ / -)Titanium Dioxide,Mica, Iron Oxides
[0073] The lipophilic moisture-curing acrylic-based polyisocyanate-treated plate, the hydroxyalkyl cellulose-coated plate, and the inulin-coated plate were prepared. The powder cosmetic was finely scraped with a spatula and arranged in a doughnut shape on a 12 cm square surface-hardened glass plate. The powder cosmetic weighed 1,500 g. 1,500 g of squalane was added thereto, mixed well with a spatula for art supplies, and the resulting mixed paste was spread on the substrate. This was repeated three times to obtain samples in which the mixed paste was spread on the surface of each substrate. Next, as coating step 1, the mixed paste was flattened using a 500 μm stainless steel four-sided applicator in the same manner as in Example 1 above. Next, as coating step 2, the mixed paste was immediately spread for 12 seconds at 260 rpm using a rotating device with the same urethane sponge fixed thereto as in Example 1 above. Next, in coating step 3, a coating film was immediately formed using the same PEN-coated cylindrical applicator as in Example 1 above, and the absorbance was measured at three points for each plate using a spectrophotometer.
[0074] Using three sets of assembled cells with a recess depth of 100 μm, the mixed paste obtained in the same manner as above, with a powder cosmetic / (powder cosmetic+squalane) value of 0.615, was filled. The absorbance at 400 nm was measured at two points for each assembled cell using a spectrophotometer, and a total of six measured values were obtained. Although four points would be acceptable, six points of data are shown here to show the degree of variation that occurs when actually measuring powder cosmetics using this method. The actual measured values were 4.779588, 4.715465, 4.95402, 4.692718, 5.403312, and 4.901608 for the absorbance, with an average absorbance of 4.907785167, a standard deviation of 0.263589873, and a standard deviation / average absorbance of 5.4%. This average absorbance was measured on a diluted solution, so if we assume that the solution is not diluted and divide the average absorbance value by the above mixture ratio, we get 7.980. Using this value, the absorbance values obtained previously at a total of nine points were corrected for film thickness, and the results are shown in Table 4.
[0075] [Table 5]
[0076] [Table 6]
[0077] Looking at Tables 5 and 6, the lipophilic plate showed the highest SPF value calculated using formula 1. The in vitro SPF value of this product was 5.4, and the in vitro UVA-PF value calculated using formula 2 was 23.5, measured using the same plate. The equivalent in vivo SPF value calculated using formula 3 was 53.3, and the equivalent in vivo UVA-PF value calculated using formula 4 was 11.0. In the case of the ISO method, the values are used as they are, so the in vitro SPF value was 100.6 and the in vitro UVA-PF value was 13.4. Both in vitro UVA-PFs were in the same range as the values displayed on the product, but the ISO method showed a larger difference in SPF value.
[0078] Example 3 Measurements were carried out using a commercially available stick-type sunscreen. The SPF value listed on the package of the commercially available product was 50+, the PA classification was ++++ (corresponding to a UVA-PF of 16-32) (the in vivo UVA-PF value corresponding to the PA classification is 24), and the ingredients were listed as follows: Triethylhexanoin,Isononyl Isononanoate, Polymethylsilsesquioxane, Dimethicone, Nylon-12,Ethylhexyl Methoxycinnamate, Polyethylene, Synthetic Wax,Trimethylpentanediol / Adipic Acid / Glycerin Crosspolymer, ButylMethoxydibenzoylmethane, Dimethicone / Vinyl Dimethicone Crosspolymer, SucrosePolystearate, Polysilicone-15, Menthol, Alumina, Tocopherol, Water, ButyleneGlycol, Saxifraga Sarmentosa Extract, Geranium Robertianum Extract, VacciniumMyrtillus Leaf Extract, Cynara Scolymus (Artichoke) Leaf Extract, BHT,Fragrance
[0079] The lipophilic moisture-curing acrylic-based polyisocyanate-treated plate, the hydroxyalkyl cellulose-coated plate, and the inulin-coated plate were prepared. The cosmetic was rubbed in a square shape on a 12 cm square surface-hardened glass plate using a spatula for art supplies. The cosmetic weighed 0.600 g. 2.400 g of squalane was dropped in the center of the square shape and mixed well using a spatula. The mixed paste was placed in a disposable aluminum cup for food, heated at 60°C for 15 minutes, and then poured into the plate. This was repeated three times to obtain samples in which the mixed paste was spread on the surface of each substrate. Next, as in Example 1 above, the mixed paste was flattened using a 500 μm stainless steel four-sided applicator in the same manner as in Example 1 above. Next, as in Example 2 above, the mixed paste was immediately spread for 12 seconds at 260 rpm using a rotating device with a urethane sponge attached. Next, in coating step 3, similarly to Example 1, a coating film was formed using the PEN-coated cylindrical applicator, and the absorbance was measured at three points for each plate using a spectrophotometer.
[0080] Using two sets of assembled cells with a depth of 100 μm, the mixed paste obtained in the same manner as above, with a powder cosmetic / (powder cosmetic+squalane) value of 0.208, was filled. The above measurements revealed that the cosmetic had almost no absorption at a wavelength of 400 nm, and sufficient absorption at a wavelength of 360 nm, so the measurement wavelength was changed to 360 nm. Four actual absorbance values were obtained: 3.883449, 3.774979, 3.804809, and 3.645621. The average absorbance was 3.777215, the standard deviation was 0.098943, and the standard deviation / average absorbance = 2.6%. Since this average absorbance was measured using diluted solutions, if we assume that the solution was not diluted and divide the average absorbance value by the above mixture ratio, we get 18.2. Using this value, the absorbance values of the nine points obtained earlier were corrected for film thickness, and the results are shown in Tables 5 and 6.
[0081] [Table 7]
[0082] [Table 8]
[0083] Looking at Table 5, the hydroxyalkyl cellulose coated plate showed the highest SPF value based on the 0029 standard. The in vitro SPF value of this product was about 3.2, and the in vitro UVA-PF value measured using the same plate was about 12.0. The in vivo SPF equivalent value calculated from this value using formula 3 was 31.8, and the in vivo UVA-PF equivalent value calculated from formula 4 was 5.6. In the case of the ISO method, the values are used as they are, so the in vitro SPF value was 19.5 and the in vitro UVA-PF value was 3.5. Compared to the product label value, the SPF value was slightly lower according to formulas 3 and 4, and although the UVA-PF values were consistent, both were significantly lower according to the ISO method standard.
[0084] (Comparative Example 1, Example 4) Measurements were carried out using a commercially available pressurized can type sunscreen spray. The SPF value listed on the package of the commercially available product was 100, and the ingredients were listed as follows: avobenzone(3%), homosalate (10%), octisalate (5%), octocrylene (10%), oxybenzone (6%) alcoholdenat., isobutane, VA / butyl maleate / isobornyl acrylate copolymer, caprylylglycol, cyclopentasiloxane, cyclohexasiloxane, fragrance, polyglyceryl-3stearate / isostearate / dimer dilinoleate crosspolymer, lauryl PEG-8 dimethicone, phenylisopropyl dimethicone, ascorbyl palmitate, methyl dihydroabietate, tocopheryl acetate, mineral oil, panthenol, water, Aloe barbadensis leaf extract.
[0085] The above-mentioned lipophilic moisture-curing acrylic-based polyisocyanate-treated plate, hydroxyalkyl cellulose-coated plate, and inulin-coated plate were prepared. The only coating process was spraying sunscreen from above and forming a coating film by running a stainless steel 4-way applicator with a gap of 20 μm at a speed of 5 mm / s. An attempt was made to measure the film thickness using a rotary film thickness gauge, but the film thickness measurement was not possible because the cosmetic was transparent.
[0086] Therefore, when measurements were carried out in accordance with Example 1, a hydroxyalkyl cellulose-coated plate was selected, and the in vitro SPF value was 4.8, and the in vitro UVA-PF value measured using the same plate was 35.6. The in vivo SPF equivalent value calculated from this value using formula 3 was 47.8, and the in vivo UVA-PF equivalent value calculated using formula 4 was similarly 16.7. The film thickness measurement method using the assembled cell used in the present invention is very suitable for cosmetics such as lotions that are transparent in appearance, and cosmetics that generate a lot of unevenness in the coating film.
[0087] (Comparative Example 2, Example 5) Measurements were carried out using a commercially available sunscreen. The SPF value listed on the package of the commercially available product was 8, and the ingredients were listed as follows: Water,Alcohol, Phenylbenzimidazole Sulfonic Acid, Triethanolamine, Camellia SinensisLeaf Extract, Rosmarinus Officinalis (Rosemary) Leaf Extract, Coix Lacryma-JobiMa-yuen Seed Extract, Aloe Barbadensis Leaf Extract, Dipotassium Glycyrrhizate,PEG-12 Dimethicone, Dipropylene Glycol, PEG / PPG-30 / 10 Dimethicone, Dimethicone, Phenyl Trimethicone, Butylene Glycol, Potassium Hydroxide, Menthol, Fragrance
[0088] The above-mentioned lipophilic acrylic-based polyisocyanate-treated plate, hydroxyalkyl cellulose-coated plate, and corona discharge-treated superhydrophilic plate were prepared. Sunscreen was applied from above, and as coating process 1, a stainless steel four-sided applicator with a gap of 500 μm was used to coat the cosmetic material, as in Example 1 above. Then, as coating process 2, as in Example 1 above, the coating was immediately spread at 260 rpm for 12 seconds using a rotating device with a urethane sponge fixed thereto. Then, as coating process 3, a stainless steel four-sided applicator with a gap of 20 μm was used to run the applicator at a speed of 5 mm / s to form a coating film, and the film thickness was measured using a rotary film thickness gauge. The film thickness was 5, 2, and 1 μm in the order of the plates. The SPF values at 20 μm thickness according to the ISO method were 9, 32, and 63, respectively. When the ultra-hydrophilic plate was treated with corona discharge, most of the cosmetic material was stuck to the stainless steel applicator, and some of the components separated into phases and formed a coating film. A similar situation also occurred with the hydroxyalkyl cellulose-coated plate. This was thought to be because metals are lipophilic, and when the sunscreen happens to be a cosmetic material that has a high affinity with metals, even when an applicator with a narrow gap is used, the sunscreen is not properly divided between the top and bottom, and most of it is distributed on the metal side.
[0089] Therefore, when this product was tested in the same manner as in Example 1, no such problems occurred with the PEN-coated cylindrical applicator, and a uniform coating film was formed, proving the effectiveness of the polyethylene naphthalate film. In addition, hydrophilic polyester film, hydrophilic polyethylene terephthalate film, polyvinylidene fluoride film, and general fluororesin film were also tested, and coating films were formed in all of them, confirming the effectiveness of the film. On the other hand, when other film-like materials such as those shown in Table 1 were examined, all of them had problems such as problems with the uniformity of the coating film and the applicator not running smoothly.
[0090] From the above test results, it is evident that the examples of the present invention solve the problems of the comparative examples and are excellent measurement methods applicable to a wide range of cosmetics. [Explanation of symbols]
[0091] 1: Paint spreading device 2: Paint spreading parts 3: Support part 4: Substrate 5: Excessive makeup 6: Tip of paint spreading part 7: Cylindrical applicator 8: Support part 9: Paint spreading device B: Pedestal P: Support S: Resin sponge-like coating tool
Claims
1. A method for evaluating the ultraviolet protection performance of a cosmetic, comprising a step of preparing a measurement sample for evaluating the ultraviolet protection performance of the cosmetic, the preparation step comprising a method of forming a uniform cosmetic application layer on the surface of a transparent substrate for measuring ultraviolet transmittance using an applicator formed of a material layer having an oil-resistant surface.
2. 2. The method for evaluating the ultraviolet protection performance of a cosmetic according to claim 1, wherein the material layer having an oil-resistant surface is a layer made of one or more materials selected from the group consisting of polyethylene naphthalate (PEN) film, hydrophilically treated polyester film, hydrophilically treated polyethylene terephthalate film, and fluororesin film, all of which have oil-resistant properties.
3. A method for evaluating the ultraviolet protection performance of a cosmetic composition according to claim 1 or 2, comprising the following steps A to D: A. A process for preparing a plurality of measurement samples for evaluating the ultraviolet protection performance of a cosmetic, in which a single cosmetic is used to form a uniform cosmetic coating layer on each of a plurality of types of substrates for evaluating ultraviolet transmission ratios having different contact angles, using an applicator whose surface is formed of a material layer having adhesion prevention properties. B. A step of determining the absorbance of a cosmetic material at a standard thickness using an assembled cell, determining the absorbance of the plurality of measurement samples based on the absorbance of the standard thickness, and further determining the SPF value and UVA-PF value of the plurality of measurement samples according to the following formula: SPF value calculated by integrating the wavelengths from 290 to 320 nm in 1 nm increments using the formula CF x ΣEE(λ) x I(λ) x Abs(λ) UVA-PF value obtained by integrating the wavelengths from 320 to 400 nm in 1 nm increments using the formula CF x ΣEE(λ) x I(λ) x Abs(λ) Here, CF is the correction factor (=10), EE is the erythemal effect spectrum, I is the solar intensity spectrum, and Abs is the absorbance of sunscreen product. C. A process of selecting a measurement sample with the highest SPF value based on the SPF values obtained for multiple measurement samples made from one type of cosmetic product, and determining the SPF value and UVA-PF value of the measurement sample as the in vitro SPF value and in vitro UVA-PF value of the cosmetic product. D. A step of determining the in vivo SPF equivalent value of the one cosmetic product from the relational equation between the in vivo SPF value and the in vitro SPF value, and further determining the in vivo UVA-PF equivalent value of the one cosmetic product from the relational equation between the in vivo UVA-PF value and the in vitro UVA-PF value.
4. The method for evaluating the ultraviolet protection performance of cosmetics according to claim 3, wherein the plurality of types of transparent substrates for measuring ultraviolet transmittance having different contact angles are three types: a transparent substrate for measuring ultraviolet transmittance having a layer coated with polyisocyanate on its surface, a transparent substrate for measuring ultraviolet transmittance having a layer coated with inulin, and a transparent substrate for measuring ultraviolet transmittance having a layer coated with hydroxyalkyl cellulose.
5. The method for evaluating UV protection performance according to claim 3, characterized in that the relational equation between the in vivo SPF value and the in vitro SPF value, and the relational equation between the in vivo UVA-PF value and the in vitro UVA-PF value are determined by statistically processing the relationship between the SPF value, UVA-PF value, or the in vivo UVA-PF value corresponding to the PA classification of the cosmetic obtained by the in vivo method, and the SPF value and UVA-PF value determined by steps A to D.
6. 3. The method for evaluating ultraviolet protection performance according to claim 1 or 2, wherein the cosmetic is a powder cosmetic or a stick-type cosmetic, or a paste-like product obtained by mixing a solid cosmetic with a non-volatile oil.
Citation Information
Patent Citations
An applicator for applying a composition that smooths wrinkles and imperfections in skin texture.
JP2016532482A
Evaluation device for UV transmittance of cosmetics and evaluation method
JP2023057509A
Device having diagnosing function
JP1983025654A
Ultra precision coating device
JP2021065873A
Substrate for in-vitro ultraviolet ray protection power measurement of cosmetics
JP2023095723A