Solvent-free method for deposition of perovskite films
The solvent-free perovskite deposition method using physical and chemical vapor deposition techniques addresses non-uniform thickness issues in traditional methods, enabling efficient coating and film formation on large surfaces.
Patent Information
- Application Number
- JP2021562010
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-04-19
- Filing Date
- 2020-04-17
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2040-04-17
AI Technical Summary
Traditional solvent-based methods for manufacturing perovskite cells result in non-uniform thickness across layers, limiting the ability to coat large surfaces and form efficient multi-stack films.
A solvent-free perovskite deposition method involving physical vapor deposition techniques such as sputtering, electron beam deposition, and chemical vapor deposition, which includes steps like reducing pressure, vaporizing lead targets, and refilling the deposition chamber with salt precursor vapors to deposit perovskite materials on substrates.
Ensures uniform thickness and adherence of perovskite materials on substrates, facilitating efficient coating of large surfaces and formation of multi-stack films without solvents.
Smart Images

Figure 0007572112000001
Abstract
Description
[Technical field]
[0001] This application relates generally to compositions for use in photovoltaic and optoelectronic devices, and more particularly to methods for solvent-free perovskite film deposition. [Background technology]
[0002] The use of photovoltaics (PV), which generates electricity from solar energy or radiation, can offer many advantages, including, for example, a source of power, low or zero emissions, power generation independent of the power grid, durable physical construction (no moving parts), stable and reliable systems, modular construction, relatively quick installation, safe manufacture and use, and good public opinion and acceptance. Summary of the Invention [Problem to be solved by the invention]
[0003] Perovskite materials can be incorporated into one or more aspects of a PV device. PVs using perovskite components are more tolerant to internal defects than silicon-based PVs. This greater tolerance reduces production costs. However, traditional, solvent-based methods of manufacturing perovskite cells can result in non-uniform thickness across layers. This limits the ability to effectively coat large surfaces and form efficient multi-stack films.
[0004] The features and advantages of the present disclosure will be readily apparent to those skilled in the art, and many modifications may be made by those skilled in the art that fall within the spirit of the present invention. [Means for solving the problem]
[0005] In one embodiment, a method of solvent-free perovskite deposition includes loading a lead target and a substrate into a deposition chamber. The method further includes: -6The method further comprises reducing the pressure in the deposition chamber to below 1000 MPa Torr. The method further comprises vaporizing the lead target. The method further comprises backfilling the deposition chamber with vapor of a pre-salt precursor. Finally, the method comprises depositing a perovskite material on the substrate.
[0006] In another embodiment, a method of solvent-free perovskite deposition includes loading a lead powder sample into a crucible. The method further includes placing a substrate face down on top of the powder in the crucible. The method further includes reducing the pressure in the deposition chamber to 200 mTorr. The method further includes sublimating the lead powder sample. Finally, the method includes forming a first deposit on the substrate.
[0007] In yet another embodiment, a method of solvent-free perovskite deposition includes loading a lead salt precursor into a crucible. The method further includes loading a substrate into a sample holder. The method further includes increasing the pressure in the deposition chamber by at least 10. -3 Torr. The method further comprises applying a current to ionize the lead salt precursor. The method further comprises refilling the deposition chamber with vapor of a second salt precursor. Finally, the method comprises depositing a perovskite material on the substrate.
[0008] In yet another embodiment, a method of solvent-free perovskite deposition includes loading a lead salt precursor into a crucible. The method further includes loading a substrate into a sample holder. The method further includes reducing the pressure of the deposition chamber to between 5 Torr and 760 Torr. The method further includes vaporizing the lead salt precursor. The method further includes performing metalorganic vapor phase epitaxy on the vapor. The method further includes backfilling the deposition chamber with vapor of a second salt precursor. Finally, the method includes depositing perovskite material on the substrate under an inert gas. [Brief description of the drawings]
[0009] [Figure 1] 1 is a flow chart of an exemplary method for solvent-free perovskite deposition. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The methods described in this disclosure for depositing perovskites on a substrate can be used to fabricate one or more aspects of PV. Other potential applications include, but are not limited to, batteries, field effect transistors (FETs), light emitting diodes (LEDs), nonlinear optical devices, memristors, capacitors, rectifiers, and / or rectifying antennas. The perovskite material may have the general formula CMX3, where C has one or more cations (e.g., amines, ammonium, phosphonium, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds), M has one or more metals (e.g., including Be, Mg, Ca, Sr, Ba, Fe, Cd, Co, Ni, Cu, Ag, Au, Hg, Sn, Ge, Ga, Pb, In, Tl, Sb, Bi, Ti, Zn, Cd, Hg, and Zr), and X has one or more anions. In certain embodiments, C may include formamidinium or methylammonium. While many of the methods described below are illustrated using lead perovskites, these methods can also be used to prepare lead perovskites containing the desired metal (M) or metal halide (MX n ) may be substituted to obtain other perovskites.
[0011] In certain embodiments, the present disclosure provides methods for depositing perovskites based on physical vapor deposition. In other embodiments, the present disclosure provides methods for depositing perovskites based on chemical vapor deposition. Certain embodiments of physical vapor deposition and chemical vapor deposition are described in detail below.
[0012] In each of the embodiments described below, patterning of the resulting perovskite film may be performed by placing a tight-fitting shadow mask directly over the substrate prior to loading the substrate into the vacuum chamber.
[0013] (Physical Vapor Deposition) Generally, physical vapor deposition generally includes vaporizing deposition materials, transporting the vapor to the target substrate, reacting between metal atoms and reactive gases during the transport stage, and depositing on the substrate. This disclosure includes several embodiments of physical vapor deposition. Specifically, the following methods are described: sputtering, reactive sputtering, electron beam deposition, cathodic arc deposition, pulsed laser deposition, molecular beam epitaxy, close space sublimation, co-evaporation with thermal evaporation and annealing, vapor-assisted solution processing, ion-assisted deposition, and activated reactive evaporation.
[0014] (Sputtering) In one embodiment, a method for solvent-free perovskite deposition includes loading a sputtering chamber with a PbI2 (lead (II) iodide) target and pumping it down to ultra-high vacuum pressure. For example, the pressure may be as low as 10 -6 The system should be evacuated to below 10 Torr. -8 The method further includes loading the specimen attached to the substrate holder into a load lock chamber. The method further includes placing the load lock chamber under high vacuum (10 -3 ~10 -5 The method includes evacuating the sample holder to a high vacuum of 1×10 Torr and transferring the sample holder to a sputtering chamber. -5 The pressure may be less than 1000 Torr. The method further includes applying an inert gas, such as Ar, to the PbI2 target to induce a sputtering effect, backfilling the sputtering chamber with FAI (formamidinium iodide) and / or MAI (methylammonium iodide) vapor, and depositing the perovskite material. The chamber may be backfilled at a rate between 2 and 100 sccm using a mass flow controller (MFC). In an embodiment, the FAI and / or MAI may be introduced at a rate between 5 and 30 sccm. The method contemplates that the first 20 nm of the perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0015] In another embodiment, a method for solvent-free perovskite deposition includes loading a sputtering chamber with a Pb (lead) target and evacuating to ultra-high vacuum pressure. For example, the pressure may be 10 -6 The system should be evacuated to below 10 Torr. -8 The method further includes loading the specimen attached to the substrate holder into a load lock chamber. The method further includes depressurizing the load lock chamber to a high vacuum pressure (10 -3 ~10 -5 Torr) and the sample holder is transferred to a load lock chamber. The method further includes applying an inert gas, such as Ar, to the Pb target to induce a sputtering effect, backfilling the chamber with HI (hydrogen iodide) and one or both of FAI and MAI vapors, and depositing the perovskite material. The chamber may be backfilled with an MFC at a rate between 2-100 sccm. In an embodiment, HI and one or both of MAI and FAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0016] In yet another embodiment, a method for depositing a solvent-free perovskite material includes loading a Pb target (either Pb and HI, or PbI2) into a sputtering chamber and pumping down to ultra-high vacuum pressure. For example, the pressure may be as low as 10 -6 The system should be evacuated to below 10 Torr. -8 The method further includes loading the sample attached to the substrate holder into a load lock chamber and placing the load lock chamber under high vacuum pressure (10 -3 ~10 -5The method includes evacuating the PbI2 target to a pressure of 1000 psi (1000 psi) (Torr) and then transferring the sample holder into the chamber. The method includes applying an inert gas, such as Ar, to the PbI2 target to induce a sputtering effect, continuing with refilling the chamber with HI, and depositing the perovskite material. Refilling the chamber may be performed using an MFC at a rate between 2 and 100 sccm. In an embodiment, HI may be introduced at a rate between 5 and 30 sccm. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is in close contact with the substrate. The method ends by removing the PbI2 film from the chamber and transferring it to a different device, such as a thermal evaporator, for deposition of FAI and / or MAI.
[0017] (Reactive Sputtering) In another embodiment, a method for solvent-free perovskite material deposition includes loading a PbI2 target into a sputtering chamber and pumping down to ultra-high vacuum pressure. For example, the pressure may be 10 -6 The system should be evacuated to below 10 Torr. -8 The method further includes loading the sample attached to the substrate holder into the sputtering chamber. The method further includes placing the load lock chamber under high vacuum pressure (10 -3 ~10 -5 The method includes depressurizing the PbI2 target to a pressure of 1000 psi (1000 psi) (at 1000 psi) (at 1000 psi) (at 1000 psi) and transferring the sample holder to a load lock chamber. The method further includes applying a reactive gas, such as oxygen or nitrogen, to the PbI2 target to induce a sputtering effect, backfilling the chamber with FAI and / or MAI vapor, and depositing the perovskite material. The chamber may be backfilled with an MFC at a rate between 2-100 sccm. In an embodiment, the FAI and / or MAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of the perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0018] In another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb (lead) target into a sputtering chamber and evacuating to ultra-high vacuum pressure. For example, the pressure may be 10 -6 The system should be evacuated to below 10 Torr. -8 The method further includes loading the specimen attached to the substrate holder into a load lock chamber. The method further includes placing the load lock chamber under high vacuum pressure (10 -3 ~10 -5 The vacuum is continued to a pressure of 1000 psi (1000 psi) to a pressure of 1000 psi (1000 psi) (Torr) and the sample holder is transferred to a load lock chamber. The method further includes applying a reactive gas such as oxygen or nitrogen to the Pb target to induce a sputtering effect, backfilling the chamber with HI (hydrogen iodide) and one or both of FAI and MAI vapor, and depositing the perovskite material. The chamber may be backfilled with MFC at a rate between 2-100 sccm. In an embodiment, HI and one or both of MAI and FAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0019] In yet another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb target into a sputtering chamber and pumping down to ultra-high vacuum pressure. For example, the pressure may be 10 -6 The system should be evacuated to below 10 Torr. -8 The method further includes loading the sample attached to the substrate holder into a load lock chamber and placing the load lock chamber under high vacuum (10 -3 ~10 -5The method includes evacuating the Pb target to a pressure of 1000 MPa (0.2 MPa) (at 10 ...
[0020] (Electron Beam Physical Vapor Deposition or Electron Beam Deposition) FIG. 1 shows a method 100 for solvent-free deposition of perovskite materials. Step 102 includes loading a PbI2 target into a deposition chamber. Step 104 includes loading a sample bonded to a substrate holder into the deposition chamber. The method 100 continues at step 106 with high vacuum pressure (5×10 -6 The vacuum is continued to a pressure of 1000 Pa (or less than 1000 Pa). In step 108, an electron beam is applied to the PbI2 target. The method 100 then proceeds to step 110, where the deposition chamber is refilled with the vapor phase of FAI and / or MAI. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, the FAI and / or MAI may be introduced at a rate between 5-30 sccm. Finally, the exemplary method concludes with depositing the perovskite material in step 112. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0021] In another embodiment, a method of solvent-free perovskite material deposition includes loading a deposition chamber with a Pb target and loading a sample bonded to a substrate holder into the deposition chamber. The method further includes applying high vacuum pressure (5×10 -6 The method includes evacuating the chamber to a pressure of 1000 psi (<0.05 Torr) and applying an electron beam to the Pb target. The method continues with backfilling the chamber with HI and formamidine and / or methylamine (MA) vapors and depositing the perovskite material. The chamber may be backfilled with MFC at a rate between 2-100 sccm. In an embodiment, HI and FA and / or MA may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is in close contact with the substrate.
[0022] In yet another embodiment, a method of solvent-free perovskite material deposition includes loading a deposition chamber with a Pb target and loading a sample bonded to a substrate holder into the deposition chamber. The method further includes applying high vacuum pressure (5×10 -6 Torr or less and applying an electron beam to the Pb target. The method continues with refilling the chamber with HI vapor and depositing the perovskite material. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, HI may be introduced at a rate between 5-30 sccm. The method ends by removing the PbI2 film from the chamber and transferring it to a different apparatus, such as a thermal evaporator, for deposition of FAI and / or MAI. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is in close contact with the substrate.
[0023] (Cathodic Arc Physical Vapor Deposition) In one embodiment, a method for solvent-free perovskite material deposition includes loading a Pb target into a deposition chamber and loading a sample bonded to a substrate holder into the deposition chamber. The method further includes subjecting the deposition chamber to ultra-high vacuum pressure (10 -8 ~10 -12 Torr) and applying a cathodic arc to the Pb target. The method continues with backfilling the chamber with HI vapor and depositing the perovskite material. The chamber may be backfilled with an MFC at a rate between 2-100 sccm. In an embodiment, HI may be introduced at a rate between 5-30 sccm. The method ends by removing the PbI2 film from the chamber and transferring it to a different apparatus, such as a thermal evaporator, for deposition of FAI and / or MAI. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0024] (Pulse laser deposition) In one embodiment, a method for solvent-free perovskite material deposition includes loading a PbI2 target into a deposition chamber and loading a sample attached to a substrate holder into the deposition chamber. The method further includes subjecting the deposition chamber to high vacuum pressure (10 -6 ~10 -8 Torr) and applying a pulsed laser to the PbI2 target. The method continues with refilling the chamber with FAI and / or MAI vapor and depositing the perovskite material. The chamber may be refilled at a rate between 2-100 sccm using an MFC. In an embodiment, the FAI and / or MAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0025] In another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb target into a deposition chamber and loading a sample bonded to a substrate holder into the deposition chamber. The method further includes subjecting the deposition chamber to high vacuum pressure (10 -6 ~10 -8 Torr) and applying a pulsed laser to the Pb target. The method continues with refilling the chamber with HI and one or both of MAI or FAI vapor and depositing the perovskite material. The chamber may be refilled at a rate between 2-100 sccm using an MFC. In an embodiment, HI and one or both of MAI and FAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0026] In yet another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb target into a deposition chamber and loading a sample bonded to a substrate holder into the deposition chamber. The method further includes subjecting the deposition chamber to high vacuum pressure (10 -6 ~10 -8 Torr) and applying a pulsed laser to the Pb target. The method continues with refilling the chamber with HI vapor and depositing the perovskite material. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, HI may be introduced at a rate between 5-30 sccm. The method ends by removing the PbI2 film from the chamber and transferring it to a different apparatus, such as a thermal evaporator, for deposition of FAI and / or MAI. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is in close contact with the substrate.
[0027] (Molecular Beam Epitaxy) In one embodiment, a method for solvent-free perovskite material deposition includes loading a Pb target into a deposition chamber and loading a sample bonded to a substrate holder into the deposition chamber. The method further includes subjecting the deposition chamber to ultra-high vacuum pressure (10 -8 ~10 -12 Torr) and applying a molecular beam to the Pb target. The method continues with refilling the chamber with HI vapor and depositing the perovskite material. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, HI may be introduced at a rate between 5-30 sccm. The method ends by removing the PbI2 film from the chamber and transferring it to a different apparatus, such as a thermal evaporator, for deposition of FAI and / or MAI. The method contemplates that the first 20 nm of perovskite is deposited at a rate of about 0.5 Å / sec to ensure that the material is in close contact with the substrate.
[0028] (Proximal Space Sublimation) In one embodiment, the method of solvent-free perovskite material deposition includes loading a PbI2 powder sample into a crucible and placing a substrate face down on top of the sample. The method further includes depressurizing to a low vacuum pressure (~200 mTorr) and sublimating the PbI2 powder sample. The method continues with refilling the chamber with FAI and / or MAI vapor and depositing the perovskite material. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In one embodiment, the FAI and / or MAI may be introduced at a rate between 5-30 sccm. The method contemplates that the deposition of the first 20 nm of perovskite is performed at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0029] In another embodiment, the method of solvent-free perovskite material deposition includes loading a Pb powder sample into a crucible and covering the crucible with the Pb powder sample face down. The method further includes depressurizing to a low vacuum pressure (~200 mTorr), sublimating the Pb sample, and depositing a first film. The method continues with refilling the chamber with HI and one or both of formyl imidamide (FA) or methylamine (MA) vapor and depositing a second film. The chamber may be refilled with an MFC at a rate between 2-100 sccm. In an embodiment, HI and one or both of MA and FA may be introduced at a rate between 5-30 sccm. The method contemplates depositing the first 20 nm at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate. The method contemplates that the deposition of the first 20 nm of perovskite is carried out at a rate of approximately 0.5 Å / sec to ensure that the material adheres closely to the substrate.
[0030] In yet another embodiment, a method of solvent-free perovskite material deposition includes loading a PbI2 powder sample into a crucible and covering the crucible with the PbI2 powder sample face down. The method further includes depressurizing to a low vacuum pressure (~200 mTorr), sublimating the PbI2 powder sample, and depositing a first film. The method further includes replacing the PbI2 powder sample with a MAI and / or FAI powder sample and placing the MAI and / or FAI powder sample face down against the crucible. The method ends with depressurizing to a pressure of 200 mTorr, sublimating the MAI and / or powder sample, and depositing a second film. The method contemplates that the deposition of the first 20 nm is performed at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0031] In yet another embodiment, a method of solvent-free perovskite material deposition includes growing a single crystalline perovskite having the structure ABX3 by any method known to one of skill in the art. The method further includes loading the single crystal into a crucible and loading a substrate face down into a substrate holder. Depending on the size of the crystal, it may be necessary to crush the crystalline perovskite into more uniform pieces using a mortar and pestle. The method further includes reducing pressure to a low vacuum (~200mTorr), sublimating the crystal, and depositing a first film.
[0032] (Thermal evaporation and co-evaporation with annealing) In one embodiment, a method for solvent-free perovskite material deposition includes loading a PbI powder sample into a crucible and loading a substrate into a sample holder. The method further includes subjecting the sample to high vacuum pressure (5×10 -6 The method includes vaporizing the PbI2 powder sample by reducing the pressure to a pressure of 1000 psi (0.1 psi torr or less) and applying a voltage between two metal posts. The method continues with refilling the chamber with FAI and / or MAI vapor and performing deposition. The chamber may be refilled at a rate between 2-100 sccm using an MFC. In an embodiment, the FAI and / or MAI may be introduced at a rate between 5-30 sccm. The method contemplates that the deposition of the first 20 nm is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0033] In another embodiment, a method of solvent-free perovskite material deposition includes loading a PbI powder sample into a first crucible and a MAI and / or FAI sample into a second crucible. The method further includes loading a substrate into a sample holder and applying high vacuum pressure (5×10 -6The method includes depressurizing the substrate to a pressure of 0.1 Torr or less. The method continues with evaporating the PbI2 and MAI and / or FAI samples by applying a voltage between two metal posts to simultaneously deposit the PbI2 and MAI and / or FAI. The method contemplates that the deposition of the first 20 nm is performed at a rate of about 0.5 Å / sec to ensure that the material is in close contact with the substrate.
[0034] In yet another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb sample into a crucible, loading a substrate into a sample holder, and applying high vacuum pressure (5×10 -6 The method further comprises evacuating the chamber to a pressure of 0.1 Pa (or less than 0.1 Torr). The method further comprises depositing the Pb sample by applying a voltage between the two metal posts. The method continues with refilling the chamber with HI and one or both of FAI and MAI vapors and depositing. The chamber may be refilled with an MFC at a rate between 2-100 sccm. In an embodiment, HI and one or both of MAI and FAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of deposition is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0035] In yet another embodiment, a method for solvent-free perovskite material deposition includes loading a PbI powder sample into a crucible, loading a substrate into a sample holder, and applying high vacuum pressure (5×10 -6 The method further includes applying a voltage between the two metal posts to vaporize the PbI2 powder sample and form a first film. The method further includes replacing the PbI2 powder sample with a MAI and / or FAI powder sample and applying a high vacuum pressure (5×10 -6The method continues with depressurizing the pressure to a pressure of 1000 psi (0.1 Torr or less). The method ends with vaporizing the MAI and / or FAI powder sample by applying a voltage between the two metal posts and depositing a second film. The method contemplates that the deposition of the first 20 nm is performed at a rate of about 0.5 Å / sec to ensure that the material adheres closely to the substrate.
[0036] In yet another embodiment, a method of solvent-free perovskite material deposition comprises growing a single crystal perovskite having the structure ABX3 by any method. The method further comprises loading the single crystal into a crucible. In some instances, it may be necessary to crush the crystal in a mortar and pestle to obtain more uniform pieces. The method further comprises loading the sample into a substrate holder. The method further comprises subjecting the deposition chamber to high vacuum pressure (5×10 -6 The method includes reducing the pressure to a pressure of 1000 MPa (below 1000 MPa) and applying a voltage to two metal posts connected to the precursor crucible to vaporize the crystals and deposit a film on the sample.
[0037] (Gas-assisted solution processing or hybrid physical-chemical deposition) In an embodiment, a method of solvent-free perovskite material deposition includes depositing a layer of PbI2 on a film by any of the disclosed methods described above. The PbI2 film may be patterned using a tight-fitting shadow mask. The method further includes depositing a PbI2 film on a film by any of the disclosed methods described above. The PbI2 film may be patterned using a tight-fitting shadow mask. The method further includes depositing a PbI2 film on a film by a vacuum chamber (200 mTorr to 10 -6 The method includes placing the film with the PbI2 layer facing up at a pressure of 100 psi (between 1000 psi and 1000 psi torr) and introducing hydrogen iodide (HI) vapor. The method ends with flowing methylamine (MA) and / or formylimidamide (FA) vapor, which may exist in the vapor phase as tautomeric formamidines, into the reduced pressure chamber. The MA and / or FA vapor may be introduced at a rate between 2-100 sccm using an MFC. In one embodiment, the MA and / or FA vapor may be introduced at a rate between 5-30 sccm.
[0038] In one embodiment, a method of solvent-free perovskite material deposition includes depositing a layer of HPbI3 on a film by any of the methods previously described. The method further includes placing the film in a reduced pressure chamber with the HPbI3 layer facing up. The method ends with flowing methylamine (CH3NH2) and / or formyl imidamide (NH2CHNH) vapor into the reduced pressure chamber. Alternatively, methylamine (CH3NH2) and / or formyl imidamide (NH2CHNH) vapor is first added to PbI2, followed by the addition of HI.
[0039] (Thermal spraying (thermal spray coating)) In one embodiment, the method for solvent-free perovskite material deposition involves spraying a PbI2 sample heated to 20-80°C onto the film at atmospheric pressure and then placing the film in a vacuum chamber (200 mTorr to 10 -6 The method includes placing the vacuum chamber at a pressure of 1000 psi (1000 psi, 1000 Torr). The method ends with flowing the MA and / or FA vapor into the vacuum chamber. The MA and / or FA vapor may be introduced using an MFC at a rate between 2-100 sccm. In one embodiment, the MA and / or FA vapor may be introduced at a rate between 5-30 sccm.
[0040] (Ion plating or ion-assisted deposition) In one embodiment, a method for solvent-free deposition of perovskite material includes loading a deposition chamber with a Pb target, loading a sample bonded to a substrate holder into the deposition chamber, and incubating the chamber for 10 -5 In one embodiment, the chamber is evacuated to below 10 Torr. -8The pressure is reduced to Torr. The method further comprises vaporizing the Pb target by bombarding the source material with particle bombardment. Particle bombardment vaporization may be performed using evaporation, sputtering, arc evaporation, or chemical means. This form of vaporization requires the addition of an inert gas (e.g., Ar) or a reactive gas (e.g., O2 or N2). The method further comprises backfilling the chamber with HI vapor and depositing. The chamber may be backfilled using an MFC at a rate between 2-100 sccm. In an embodiment, HI may be introduced at a rate between 5-30 sccm. The method concludes by removing the PbI2 film from the chamber and transferring it to a different apparatus, such as a thermal evaporator, for deposition of FAI and / or MAI. The method contemplates that the first 20 nm of deposition is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0041] (Activated Reactive Evaporation) In one embodiment, a method for solvent-free perovskite material deposition includes loading a PbI target into a deposition chamber, loading a sample bonded to a substrate holder into the deposition chamber, and applying high vacuum pressure (5×10 -6 The method further comprises evacuating the chamber to a pressure of 100 MPa (0.1 MPa or less) and evaporating a PbI2 target in the presence of a reactive gas and a plasma. The method continues with refilling the chamber with FAI and / or MAI vapor and depositing. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, the FAI and / or MAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of deposition is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0042] In another embodiment, a method for solvent-free perovskite material deposition includes loading a deposition chamber with a Pb target, loading a sample bonded to a substrate holder into the deposition chamber, and applying high vacuum pressure (5×10 -6The method further comprises evacuating the chamber to a pressure of 1000 psi (0.1 MPa torr or less). The method further comprises vaporizing the Pb target in the presence of a reactive gas and a plasma. The method continues with refilling the chamber with HI and one or both of MAI and FAI vapors and depositing. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, HI and one or both of MAI and FAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of deposition is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0043] In yet another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb target into a deposition chamber, loading a sample bonded to a substrate holder into the deposition chamber, and applying high vacuum pressure (5×10 -6 The method further comprises evacuating the chamber to a pressure of about 0.5 Å / sec (or less). The method further comprises vaporizing the Pb target in the presence of the reactive gas and the plasma. The method continues with refilling the chamber with HI vapor and deposition. The chamber may be refilled using an MFC at a rate between 2-100 sccm. In an embodiment, HI may be introduced at a rate between 5-30 sccm. The method concludes by removing the PbI2 film from the deposition chamber and transferring it to a different apparatus, such as a thermal evaporator, for deposition of FAI and / or MAI. The method contemplates that the first 20 nm of deposition is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0044] (chemical film formation) Typically, chemical deposition involves vaporizing a precursor, transporting the vapor to the target substrate, chemical reaction between the precursor vapor and the surface to be coated, and deposition on the substrate. Various precursors may be used for each of the chemical vapor deposition methods described below. Lead precursors contemplated generally include lead alkoxides, lead alkylamides, lead alkyl sulfides, lead alkyl selenides, plumbane, and plumbylene. In an embodiment, the lead precursor is bis(1-dimethylaminio-2-methyl-2-propanolate)lead(II) (Pb(DMAMP)2); bis(2,2,6,6-tetramethyl-3,5,heptanedionato)lead(II) (Pb(THD)2); hexafluoroacetylacetonate lead(II); plumbocene (PbCp2); tetraethyllead(IV); bis[bis(trimethylsilyl)amide]lead(II); or rac-N 2 ,N 3 -di-tert-butane-2,3-diamide lead(II). Contemplated iodine precursors generally include metal iodides and alkylammonium iodide salts. In some embodiments, the iodine precursor may be trimethylsilyl iodide (TMSI), iodine (I2), hydrogen iodide (HI), hydroiodic acid, tin(IV) iodide, or methylammonium iodide. Contemplated formamidinium iodide precursors generally include formamidinium salts, formamidinium precursor reagents (formates, imidine esters, triazines), ammonium salts, and cyanides. In certain embodiments, the formamidinium precursor may be formamidinium iodide (FAI), formamidinium acetate, triethoxyl orthoformate, ethylmethanimidinium iodide, 1,3,5-triazine, ammonia (NH), ammonium iodide (NHI), ammonium hydroxide (NHOH), or hydrogen cyanide (HCN).
[0045] The present disclosure includes several embodiments of physical vapor deposition. In particular, atomic layer deposition, plasma enhanced chemical deposition, metalorganic vapor phase epitaxy, hydride vapor phase epitaxy, thin film vapor solid phase conversion, and liquid phase epitaxy are described.
[0046] (atomic layer deposition) In one embodiment, the method of solvent-free perovskite material deposition includes loading a PbI2 precursor into a deposition chamber and loading a FAI sample into the deposition chamber. The method further includes pumping to a low vacuum pressure (100-500 mTorr), pulsing a first PbI2 precursor for at least 0.015 seconds, waiting 10-30 seconds to provide time for the reaction to occur at the substrate, pulsing a second PbI2 precursor for at least 0.015 seconds, waiting 10-30 seconds to provide time for the reaction to occur at the substrate, and then repeating the cycle until the desired material thickness is obtained. Deposition is typically performed under a carrier gas of N2. In one embodiment, the method requires depositing PbS in the deposition chamber to produce PbI2 prior to loading the PbI2 precursor into the deposition chamber.
[0047] For example, after loading the FAI sample into a deposition chamber and pumping down to a low vacuum pressure, lead(II) acetate is introduced into the chamber and a first deposition is performed. After waiting 30 seconds, trimethylsilyl iodide is introduced into the chamber and a second deposition is performed. The second deposition reacts with the first deposition to form a layer of PbI2. An exemplary method further includes waiting an additional 30 seconds before restarting the cycle by introducing lead(II) acetate into the chamber. Lead(II) acetate and trimethylsilyl iodide may be introduced using an MFC at a rate of 2-100 sccm. In an embodiment, they may be introduced at a rate between 5-30 sccm.
[0048] As another example, after loading an FAI sample into a deposition chamber and pumping down to a low vacuum pressure, PbS is introduced into the chamber and a first deposition is performed. After waiting 30 seconds, TMSI is introduced into the chamber and a second deposition is performed. The second deposition reacts with the first deposition to form a layer of PbI2. The exemplary method further includes waiting an additional 30 seconds before restarting the cycle by introducing PbS. PbS and TMSI may be introduced using an MFC at a rate between 2-100 sccm. In an embodiment, they may be introduced at a rate between 5-30 sccm.
[0049] In another embodiment, a method of solvent-free perovskite material deposition includes loading a PbI2 precursor into a deposition chamber, loading a FAI sample into the deposition chamber, and depressurizing to a low vacuum pressure (100-500 mTorr). In an embodiment, the method requires depositing PbS in the deposition chamber to form PbI2 prior to loading the PbI2 precursor into the deposition chamber. The method further includes alternating between depositing the PbI2 precursor and depositing FAI on the film. The method ends with placing the PbI2 precursor facing upward in the depressurized chamber and flowing MAI and / or FAI vapor into the depressurized (200 mTorr-10-6 Torr) chamber. The MAI and / or FAI vapor may be introduced using an MFC at a rate between 2-100 sccm. In an embodiment, the MAI and / or FAI vapor may be introduced at a rate between 5-30 sccm.
[0050] In each of the aforementioned atomic layer deposition methods, the substrate may be selectively patterned before being placed in the deposition chamber. For example, the patterning may be applied using O2 plasma, ozone cleaning, or other surface modification techniques known to those skilled in the art. The patterning may provide selective areas to which precursor nuclei may adhere.
[0051] (Plasma Enhanced Chemical Vapor Deposition) In one embodiment, a method for solvent-free perovskite material deposition includes the steps of loading a Pb precursor into a crucible, loading a substrate into a sample holder, and applying high vacuum pressure (at least 10 -3 and evacuating the chamber to a pressure of 1000 psi (1000 psi) (at 1000 psi, ...
[0052] In another embodiment, a method for solvent-free perovskite material deposition includes the steps of loading a Pb precursor into a crucible, loading a substrate into a sample holder, and applying high vacuum pressure (at least 10 -3 and evacuating the chamber to a pressure of about 0.5 Å / sec. The method further comprises applying a current to ionize the Pb precursor. The method continues with refilling the chamber with HI and one or both of MAI and FAI and depositing. The chamber may be refilled with an MFC at a rate between 2-100 sccm. In an embodiment, HI and one or both of MAI and FAI may be introduced at a rate between 5-30 sccm. The method contemplates that the first 20 nm of deposition is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0053] In yet another embodiment, a method for solvent-free perovskite material deposition includes the steps of loading a PbI precursor into a crucible, loading a substrate into a sample holder, and subjecting the substrate to high vacuum pressure (at least 10 -3 The method further comprises applying a current to ionize the PbI2 precursor and deposit the film. In some embodiments, a reactive gas may be introduced prior to ionizing the precursor. Any of the reactive gases listed above are suitable. The method further comprises transferring the film to a different device, such as a thermal evaporator, and evaporating the MA and / or FA vapor into a vacuum chamber (200 mTorr to 10 -6 The process continues with flowing a pressure of 1000 psi (1000 Torr). The MA and / or FA vapor may be introduced using an MFC at a rate between 2 and 100 sccm. In some embodiments, the MA and / or FA vapor may be introduced at a rate between 5 and 30 sccm. The method concludes with depositing MAI and / or FAI.
[0054] (Metalorganic vapor phase epitaxy (metalorganic chemical vapor deposition) In an embodiment, a method for solvent-free perovskite material deposition includes loading a Pb precursor into a crucible, loading a substrate into a sample holder, evacuating the chamber to a moderate pressure (between 5 Torr and 760 Torr), and applying either heat or electron flow to the Pb precursor to form Pb vapor. The method further includes subjecting the Pb vapor to a metal-organic vapor phase epitaxy process. The method continues with refilling the chamber with FAI and / or MAI vapor and depositing under an inert carrier gas such as Ar. The chamber may be refilled at a rate between 2 and 100 sccm using an MFC. In an embodiment, FAI and / or MAI vapor may be introduced at a rate between 5 and 30 sccm. The method contemplates that the first 20 nm deposition is performed at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0055] In another embodiment, a method of solvent-free perovskite material deposition includes loading a Pb precursor into a crucible, loading a substrate into a sample holder, evacuating the chamber to a moderate pressure (between 5 Torr and 760 Torr), and applying either heat or electron flow to the Pb precursor to form Pb vapor. The method further includes subjecting the Pb vapor to a metal-organic vapor phase epitaxy process. The method continues with refilling the chamber with HI and one or both of MAI and FAI, and depositing under an inert carrier gas such as Ar. The chamber may be refilled with an MFC at a rate between 2 and 100 sccm. In an embodiment, HI and one or both of MAI and FAI vapor may be introduced at a rate between 5 and 30 sccm. The method contemplates that the first 20 nm deposition is performed at a rate of about 0.5 Å / sec to ensure that the material is intimately attached to the substrate.
[0056] In yet another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb precursor into a crucible, loading a substrate into a sample holder, and evacuating the chamber to a moderate pressure (between 5 Torr and 760 Torr). The method further includes applying one of heat or electron flow to the Pb precursor to generate Pb vapor. The method further includes subjecting the Pb vapor to a metalorganic vapor phase epitaxy process under an inert carrier gas such as Ar. The method continues with the step of transferring the film to an apparatus such as a thermal evaporator to deposit FAI and / or MAI. The method contemplates that the deposition of the first 20 nm is performed at a rate of about 0.5 Å / sec to ensure that the material adheres to the substrate.
[0057] In each of the foregoing embodiments relating to metalorganic vapor phase epitaxy, the Pb precursor may be plumbocene or plumbylene. Any of the other Pb precursors detailed in this disclosure are also suitable.
[0058] (Hydride Vapor Phase Epitaxy) In an embodiment, a method for solvent-free perovskite material deposition includes loading a Pb precursor into a crucible, loading a substrate into a sample holder, evacuating the chamber to a moderate pressure (between 5 Torr and 760 Torr), and applying either heat or electron flow to the Pb precursor to form Pb vapor. The method further includes applying HCl (hydrochloric acid). The method continues with refilling the chamber with HI and one or both of MAI and FAI vapors and deposition. The chamber may be refilled at a rate between 2 and 100 sccm using an MFC. In an embodiment, HI and one or both of MAI and FAI vapors may be introduced at a rate between 5 and 30 sccm. In an embodiment, a carrier gas is used to facilitate deposition. Suitable carrier gases include NH3, H2, and chlorides. The method contemplates that the deposition of the first 20 nm is performed at a rate of about 0.5 Å / sec to ensure that the material adheres closely to the substrate.
[0059] In another embodiment, a method for solvent-free perovskite material deposition includes loading a Pb precursor into a crucible, loading a substrate into a sample holder, and evacuating the chamber to a moderate pressure (between 5 Torr and 760 Torr) and applying either heat or electron flow to the Pb precursor to form Pb vapor. The method further includes applying HCl. The method continues with backfilling the chamber with HI vapor and depositing a film. The chamber may be backfilled with an MFC at a rate between 2 and 100 sccm. In an embodiment, HI may be introduced at a rate between 5 and 30 sccm. In an embodiment, a carrier gas is used to facilitate deposition. Suitable carrier gases include NH3, H2, and chlorides. The method ends with transferring the film to an apparatus such as a thermal evaporator and depositing FAI and / or MAI.
[0060] (Thin film gas-liquid-solid transformation) In an embodiment, the method of solvent-free perovskite material deposition includes applying at least one of heat or electron flow to a metal C (wherein C is a Group I or Group II cation as described in the preferred embodiments), M (e.g., Pb, Sn, etc. as described in the preferred embodiments), or a mixture of metals C and M, to deposit the metal on the substrate. The method further includes direct deposition of liquid metal C or M, or an alloy or compound thereof (e.g., lead (II) acetate trihydrate). The method continues with heating and stabilizing the substrate at a temperature above the melting point of the metal or metal mixture. The method further includes using a substrate surface treatment and an inert porous capping layer to inhibit the liquid metal or metal from drying out from the substrate. The method continues with applying vapors of HX, X2, and / or CX to the chamber to form a thin film of compound CMX3. In an embodiment, vapors of HI, I2 and / or CsI are applied to a chamber containing a liquid metal film of Pb, Cs or Cs and Pb to form a thin film of CsPbI3. In an embodiment, the method further comprises using other compounds to stabilize the CX vapor at elevated temperatures with the C degradation products if C is an organic cation or if the metallic C, M or CM alloy is unstable at the temperatures required to dissolve. Alternative precursor compounds, such as lead(II) acetate trihydrate, may be used.
[0061] (Liquid Phase Epitaxy) Any of the aforementioned thin film vapor-liquid-solid transformation embodiments may be carried out on a crystalline substrate for epitaxial growth purposes. In some embodiments, the substrate may be a single crystal perovskite substrate, or other lattice-matched compound.
[0062] Although several embodiments have been provided in this disclosure, it will be understood that the disclosed systems and methods may be embodied in many other specific forms without departing from the spirit or scope of the disclosure. The examples are illustrative and not restrictive, and are not intended to be limited to the details shown. For example, various elements or components may be combined or integrated into another system, or certain features may be omitted or not implemented.
[0063] Additionally, in various embodiments, the techniques, systems, subsystems, and methods described and illustrated individually or separately may be combined or integrated with other systems, modules, techniques, or methods without departing from the scope of the present disclosure. Other components shown and described that are coupled, directly coupled, or in communication with each other may also be indirectly coupled or in communication electrically, mechanically, or otherwise, through some interface, device, or intermediate member. Other examples of modifications, substitutions, and alterations will be apparent to those skilled in the art and may be implemented without departing from the spirit and scope of the disclosure.
[0064] To assist the Patent Office, and readers of any patents to which this application may be directed, in interpreting the claims appended hereto, it is noted that applicants do not intend any of the appended claims to invoke 35 U.S.C. 112(f), as it exists on the filing date of this application, unless the words "means for" or "step for" are expressly used in a particular claim.
Claims
1. 1. A method for solvent-free perovskite deposition comprising the steps of: loading a lead target and a substrate into a deposition chamber; 5×10 -6 reducing the pressure in the deposition chamber to below 1000 Torr; vaporizing the lead target; refilling the deposition chamber with vapor of a salt precursor, the salt precursor comprising hydrogen iodide; depositing a perovskite material on the substrate; The method comprising:
2. the vaporizing step is performed by applying an electron beam to the lead target; the lead target comprises lead(II) iodide; The method further comprises refilling the deposition chamber with a second salt precursor; 10. The method of claim 1, wherein the second salt precursor comprises a salt selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof.
3. the vaporizing step is performed by applying an electron beam to the lead target; The method further comprises refilling the deposition chamber with a second salt precursor; 10. The method of claim 1, wherein the second salt precursor comprises a salt selected from the group consisting of formamidine, methylamine, and combinations thereof.
4. 10. The method of claim 1, wherein the first 20 nm of deposition is performed at a rate of 0.5 Å / sec.
5. the vaporizing step is performed by applying an electron beam to the lead target; The method further comprises: conveying the perovskite material to a thermal evaporator; depositing a second salt precursor selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof; 2. The method of claim 1, comprising:
6. the vaporizing step is performed by applying a cathodic arc to the lead target; The pressure in the deposition chamber is 10 -8 ~10 -12 Torr range, The salt precursor comprises hydrogen iodide; The method further comprises: conveying the perovskite material to a thermal evaporator; depositing a second salt precursor selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof; 2. The method of claim 1, comprising:
7. the vaporizing step is performed by applying a pulsed laser to the lead target; The pressure in the deposition chamber is 10 -8 ~10 -12 Torr range, 10. The method of claim 1, wherein the salt precursor comprises a salt selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof.
8. The method of claim 1 , wherein the refilling step is performed at a rate in the range of 2 to 100 sccm.
9. 1. A method for solvent-free perovskite deposition comprising the steps of: loading a lead powder sample into a crucible; placing a substrate face down on top of the powder in the crucible in a deposition chamber; reducing the pressure in the deposition chamber to 200 mTorr; sublimating the lead powder sample; forming a first deposition on the substrate; The method comprising:
10. The lead powder sample comprises lead(II) iodide; The method further includes refilling the deposition chamber with vapor of a salt precursor prior to forming the first deposition; the salt precursor comprises a salt selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof; 10. The method of claim 9, wherein the first deposit is a perovskite material.
11. 11. The method of claim 10, wherein the first 20 nm of deposition is performed at a rate of 0.5 Å / sec.
12. moreover, after forming the first deposition, refilling the deposition chamber with hydrogen iodide vapor and one or both of formamidine and methylamine; forming a second deposition on the substrate, the second deposition being a perovskite material; 10. The method of claim 9, having the following structure:
13. The lead powder sample comprises lead(II) iodide; The method further comprises: replacing the remaining lead powder sample in the crucible with a powder of a salt precursor, the salt precursor having a salt selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof; sublimating the salt precursor; forming a second deposition on the substrate, the second deposition being a perovskite material; 10. The method of claim 9, having the following structure:
14. 14. The method of claim 13, wherein the first 20 nm of the deposition is formed at a rate of 0.5 Å / sec.
15. The method of claim 10, wherein the step of refilling is performed at a rate in the range of 2 to 100 sccm.
16. The lead powder sample has the structure ABX 3 10. The method of claim 9, wherein the perovskite is a single crystal having the formula:
17. 1. A method for solvent-free perovskite deposition comprising the steps of: loading a lead salt precursor into a crucible; loading a substrate onto a sample holder in a deposition chamber; The pressure in the deposition chamber is increased by at least 10 -3 Torr; applying an electric current to ionize the lead salt precursor; refilling the deposition chamber with vapor of a second salt precursor; depositing a perovskite material on the substrate; The method comprising:
18. The lead salt precursor comprises lead(II) iodide; the second salt precursor comprises hydrogen iodide; 20. The method of claim 17, further comprising refilling the deposition chamber with vapor of a salt selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof.
19. the lead salt precursor is ionized in the presence of a reactive gas; 20. The method of claim 17, wherein the second salt precursor comprises a salt precursor selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof.
20. 20. The method of claim 19, wherein the reactive gas is selected from the group consisting of water, oxygen, nitrous oxide, ammonia, and nitrogen.
21. 18. The method of claim 17, wherein the lead salt precursor comprises a salt selected from the group consisting of lead alkoxides, lead alkylamides, lead alkyl sulfides, lead alkyl selenides, plumbanes, and plumbylenes.
22. 20. The method of claim 17, wherein the first 20 nm of deposition is performed at a rate of 0.5 Å / sec.
23. The lead salt precursor is bis(1-dimethylaminio-2-methyl-2-propanolate)lead(II) (Pb(DMAMP) 2 ); Bis(2,2,6,6-tetramethyl-3,5,heptanedionato)lead(II) (Pb(THD) 2 ), lead(II) hexafluoroacetylacetonate; plumbocene (PbCp 2 ), tetraethyllead(IV); bis[bis(trimethylsilyl)amide]lead(II); and rac-N 2 , N 3 - di-tert-butane-2,3-diamide lead(II).
24. 1. A method for solvent-free perovskite deposition comprising the steps of: loading a lead salt precursor into a crucible; loading a substrate onto a sample holder in a deposition chamber; reducing the pressure in the deposition chamber to between 5 Torr and 760 Torr; vaporizing the lead salt precursor; performing metalorganic vapor phase epitaxy on the vapor; refilling the deposition chamber with vapor of a second salt precursor; depositing a perovskite material on the substrate under an inert gas; The method comprising:
25. 25. The method of claim 24, wherein the second salt precursor comprises a salt selected from the group consisting of formamidinium iodide, methylammonium iodide, and combinations thereof.
26. the second salt precursor comprises hydrogen iodide; 25. The method of claim 24, further comprising refilling the deposition chamber with hydrogen iodide vapor.
27. 25. The method of claim 24, wherein the vaporizing step is performed by applying one of heat or a current of electrons to the lead salt precursor.
28. 25. The method of claim 24, wherein the lead salt precursor comprises a salt selected from the group consisting of lead alkoxides, lead alkylamides, lead alkyl sulfides, lead alkyl selenides, plumbanes, and plumbylenes.
29. The lead salt precursor is bis(1-dimethylaminio-2-methyl-2-propanolate)lead(II) (Pb(DMAMP) 2 ); Bis(2,2,6,6-tetramethyl-3,5,heptanedionato)lead(II) (Pb(THD) 2 ), lead(II) hexafluoroacetylacetonate; plumbocene (PbCp 2 ), tetraethyllead(IV); bis[bis(trimethylsilyl)amide]lead(II); and rac-N 2 , N 3 - di-tert-butane-2,3-diamide lead(II).
30. 25. The method of claim 24, wherein the first 20 nm of deposition is performed at a rate of 0.5 Å / sec.
Citation Information
Patent Citations
Method for manufacturing lead-containing perovskite type compound oxide sintered compact
JP2002087887A
Method of producing compound oxide membrane, and hydrogen permeation structure
JP2008138255A
Manufacturing system and method for perovskite films for solar cell applications, and perovskite film
JP2017515313A
Method for laser deposition of organic material film or organic-inorganic composite material film