Heat Treatment System

The heat treatment system addresses the issue of inorganic fiber belt breakage by employing heat-resistant rollers with smooth surfaces and adjustable speed control to convey products safely through high-temperature firing processes, ensuring minimal damage and improved product quality.

JP7576202B1Active Publication Date: 2024-10-30NGK CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024097351
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-06-17
Publication Date
2024-10-30
Estimated Expiration
2044-06-17

AI Technical Summary

Technical Problem

Belt made of inorganic fibers used in existing firing devices tends to break due to repeated bending, making them impractical for transporting products to be fired.

Method used

A heat treatment system using a plurality of rollers made of heat-resistant materials that can withstand high temperatures (600°C to 1400°C) and having a smooth surface (Ra6.3 μm or less) to convey products directly, with adjustable conveyance speed control to manage thermal contraction and tensile stress.

Benefits of technology

Prevents damage to the products during conveyance and reduces tensile stress by using heat-resistant rollers with controlled conveyance speed, ensuring high-quality fired products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007576202000001_ABST
    Figure 0007576202000001_ABST
Patent Text Reader

Abstract

To provide a technology more suitable for transporting baked products. [Solution] The heat treatment system includes an unwinding mechanism that unwinds a strip-shaped product to be sintered, a number of rollers that can transport the product unwound by the unwinding mechanism by rotating, and a firing furnace for firing the product transported by the rollers. The rollers are made of a heat-resistant material that can be used in the temperature range of 600°C to 1400°C, and transport the product in contact with the product.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The technology disclosed herein relates to a thermal processing system. [Background technology]

[0002] Patent Document 1 discloses a firing device including a tunnel-type firing furnace and an endless belt of inorganic fibers that passes horizontally through the firing furnace and is driven in a driving direction at a constant speed. In this firing device, a longitudinal green sheet is pulled out from a green sheet roll and fed onto the endless belt, which passes through the firing furnace. The heated ceramic sheet is then wound up by the ceramic sheet roll. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2001-31476 A Summary of the Invention [Problem to be solved by the invention]

[0004] According to Patent Document 1, an endless belt made of inorganic fibers runs around inside and outside the firing furnace. However, the belt made of inorganic fibers is easily broken when repeatedly bent, and therefore has low practicality as a means for transporting the product to be fired.

[0005] This specification discloses a technique suitable for transporting a sintered product while suppressing damage to the product. [Means for solving the problem]

[0006] The heat treatment system disclosed in this specification includes an unwinding mechanism that unwinds a belt-shaped product to be sintered, a plurality of rollers that can transport the product unwound by the unwinding mechanism by rotating, and a firing furnace for firing the product transported by the plurality of rollers. The plurality of rollers are made of a heat-resistant material that can be used in a temperature range of 600°C to 1400°C, and transport the product in contact with the product.

[0007] According to the above configuration, the product to be sintered is directly placed on multiple rollers made of a heat-resistant material that can be used in a high temperature range such as 600°C to 1400°C, and is sintered in a sintering furnace while being transported by the rotation of each roller. [Brief description of the drawings]

[0008] [Figure 1] Schematic diagram of a heat treatment system. [Diagram 2] FIG. 4 is a diagram for explaining roller speed control. [Diagram 3] FIG. 2 is a schematic diagram of a heat treatment system according to another example different from that shown in FIG. 1 . DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] The main features of the embodiments described below are listed below. Note that the technical elements described below are independent technical elements that exhibit technical usefulness alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing.

[0010] According to the heat treatment system disclosed in the present specification, the surfaces of the plurality of rollers that come into contact with the product to be sintered may be smoothed. According to the above-mentioned configuration, the surface of each roller that comes into contact with the baked product is smoothed, so that the rollers can prevent the baked product from being damaged during transport. Also, because a certain degree of slippage occurs between the surface of each roller that comes into contact with the baked product and the baked product, the tensile stress that occurs in the longitudinal direction of the baked product during baking can be mitigated.

[0011] According to the heat treatment system disclosed in the present specification, the surface may have a surface roughness of Ra 6.3 μm or less. According to the above-mentioned configuration, the surface of each roller that comes into contact with the product to be sintered is polished to have a surface roughness of Ra 6.3 μm or less, which specifically prevents each roller from damaging the product to be sintered.

[0012] According to the heat treatment system disclosed in this specification, the rollers may be made of ceramics with an alumina content of 50% to 70%. According to the above-described configuration, the heat treatment system can transport the sintered product using rollers having a composition excellent in thermal shock resistance.

[0013] According to the heat treatment system disclosed in this specification, the system may further include a roller drive control unit capable of changing the conveying speed of at least some of the rollers included in the plurality of rollers in response to shrinkage of the fired product due to the firing. According to the above configuration, the roller drive control unit changes the conveying speed of at least some of the rollers in response to the shrinkage of the baked product, thereby more accurately preventing the occurrence of tensile stress in the baked product.

[0014] According to the heat treatment system disclosed in the present specification, the firing furnace has, from upstream to downstream of the transport by the multiple rollers, a temperature rise region for raising the temperature inside the furnace, a holding region for holding the temperature inside the furnace raised by the temperature rise region, and a cooling region for lowering the temperature inside the furnace. The roller drive control unit may make the transport speed of the rollers located downstream of a predetermined position in the temperature rise region slower than that of the rollers located upstream of the predetermined position. According to the above configuration, the roller drive control unit can slow down the conveying speed of the rollers located downstream of a predetermined position in the temperature rise zone in response to the thermal contraction that occurs in the baked product passing through the temperature rise zone of the baking furnace, thereby specifically suppressing the occurrence of tensile stress in the baked product.

[0015] The heat treatment system disclosed in this specification may further include a winding mechanism that winds up the baked object after being baked in the baking furnace. According to the above configuration, the heat treatment system can easily recover the fired product by the winding mechanism after the fired product has been fired in the firing furnace.

[0016] According to the heat treatment system disclosed in the present specification, the article to be fired may be glass, ceramic, metal, or a mixture thereof. According to the above-mentioned configuration, the heat treatment system can transport an article to be fired, which is glass, ceramics, metal, or a mixture thereof, and obtain a fired product as a result. EXAMPLES

[0017] The embodiments will be described with reference to the drawings. Each drawing is merely an example, and the embodiments are not limited to the contents shown in the drawings. Also, since each drawing is merely an example, some parts may be omitted.

[0018] FIG. 1 shows a schematic diagram of a heat treatment system 10. The heat treatment system 10 includes an unwinding mechanism 20 and a firing furnace 30. The unwinding mechanism 20 holds a roll body 1 on which a long sintered product 2 is wound in a roll shape. The sintered product 2 is strip-shaped. The sintered product 2 is, for example, glass, ceramics, metal, or a mixture of these. Strip-shaped products include woven fibers, nonwoven fabrics, film-shaped products, foil-shaped products, and the like. The unwinding mechanism 20 unwinds (pays out) the sintered product 2 from the roll body 1 by rotating. The sintered product 2 is flexible both before and after it is sintered in the firing furnace 30.

[0019] The firing furnace 30 fires the sintered product 2 in the furnace, i.e., heat-treats it, by generating heat from a heater (not shown). The firing furnace 30 is a thermally insulated structure having a generally rectangular parallelepiped shape that is long in a predetermined conveying direction D1, and has an inlet 34 at one end on the upstream side of the conveying direction D1 and an outlet 35 at the other end on the downstream side of the conveying direction D1. Hereinafter, the upstream and downstream of the conveying direction D1 will simply be referred to as upstream and downstream.

[0020] The roller group 50, which is composed of a plurality of rollers 51 arranged at a predetermined interval along the conveying direction D1, is provided so as to penetrate the inside and outside of the baking furnace 30 through the carry-in entrance 34 and the carry-out exit 35. The roller group 50 may be referred to as a conveying mechanism. The rotation axes of the rollers 51 are parallel to each other and point in a direction perpendicular to the conveying direction D1. The baked product 2 unwound by the unwinding mechanism 20 is placed on the rollers 51 at a position upstream of the carry-in entrance 34. That is, in this embodiment, the baked product 2 is placed directly on each roller 51. Each of the rollers 51 rotates and contacts the baked product 2 to convey the baked product 2 in the conveying direction D1.

[0021] The article 2 to be sintered, transported by the roller group 50, enters the firing furnace 30 from the carry-in entrance 34, and is sintered while being transported inside the firing furnace 30. The article 2 to be sintered after being sintered in the firing furnace 30, which is transported by the roller group 50 and exits the firing furnace 30 from the discharge opening 35, separates from the rollers 51 at a position downstream of the discharge opening 35.

[0022] 1, in the heat treatment system 10, a cutting device 70 and a storage device 80 are provided downstream of the discharge port 35. The sintered product 2 that leaves the sintering furnace 30 from the discharge port 35 is transported to the cutting device 70 by the roller group 50, and cut to a predetermined size by a cutter provided in the cutting device 70. Then, after cutting, the sintered product 3 is collected and stored in the storage device 80.

[0023] 1, the unwinding mechanism 20 is provided at a higher position than the position at which the roller group 50 supports the baked product 2. That is, in this embodiment, it can be understood that the roller group 50 supports and transports the baked product 2 hanging down from the unwinding mechanism 20. It can be understood that the roller group 50 supports the baked product 2 horizontally or approximately horizontally.

[0024] The rollers 51 constituting the roller group 50 are made of a material capable of maintaining a stable shape even when the temperature inside the firing furnace 30 changes or reaches a maximum temperature. In this embodiment, each roller 51 is made of a heat-resistant material that can be used in a temperature range of 600°C to 1400°C. More preferably, assuming that the maximum temperature inside the furnace is 1000°C to 1300°C, each roller 51 may be made of a heat-resistant material that can be used in a high temperature range such as 1000°C to 1300°C. Being usable in these specific temperature ranges also means that the rollers can be used in temperature ranges that do not reach these specific temperature ranges.

[0025] As an example of a suitable composition for the rollers 51, each roller 51 may be made of alumina (Al 2 O 3 The ceramics are made of alumina with a content of 50% to 70%. A specific example of a ceramic containing alumina in such a ratio is mullite. Mullite is a composite of alumina and silica (SiO 2 ) and has a lower coefficient of thermal expansion and excellent thermal shock resistance compared to alumina.

[0026] In this embodiment, the surface of each roller 51 that contacts the product 2 to be sintered is smoothed. The area of ​​the surface of the roller 51 that does not contact the product 2 to be sintered during the transportation of the product 2 to be sintered may not be smoothed. Smoothed means that the roller has been polished in advance. For example, each roller 51 is made of the above-mentioned mullite. Mullite has a larger particle size than alumina and has a rough surface, but the smoothness of the surface can be obtained by polishing. The surface roughness of the surface of each roller 51 that contacts the product 2 to be sintered is, for example, Ra6.3 μm or less. The surface roughness Ra is the arithmetic mean roughness. The surface of each roller 51 that contacts the product 2 to be sintered, i.e., the smoothed surface, may be, for example, within 80% of the length range of the roller 51 in the axial direction of the roller 51, including the center of the roller 51. In this case, for example, both ends of the roller 51 in the axial direction of the roller 51 are not smoothed. However, the range of the smoothed surface of the roller 51 may be symmetrical or asymmetrical in the axial direction of the roller 51 with respect to the center of the roller 51 as the reference.

[0027] Thus, according to this embodiment, the heat treatment system 10 includes an unwinding mechanism 20 that unwinds the belt-shaped product 2 to be sintered, a plurality of rollers 51 that can transport the product 2 unwound by the unwinding mechanism 20 by rotating, and a firing furnace 30 for sintering the product 2 transported by the plurality of rollers 51. The plurality of rollers 51 are made of a heat-resistant material that can be used in a temperature range of 600°C to 1400°C, and contact the product 2 to transport the product 2 to be sintered. That is, the heat treatment system 10 solves the problem that when an inorganic fiber belt is repeatedly rotated inside and outside the firing furnace while being bent, the belt is easily broken and is of low practical use, by using a plurality of rollers 51 as a transport means for the product 2 to be sintered. The product 2 to be sintered is directly placed on the plurality of rollers 51 and transported, so that damage to the product 2 to be sintered during transportation is suppressed.

[0028] Furthermore, according to this embodiment, the surface of each roller 51 that comes into contact with the baked product 2 is smoothed. The surface roughness is, for example, Ra 6.3 μm or less. This makes it possible to prevent the baked product 2 from being damaged during transport by the rollers 51. In addition, a certain degree of slippage occurs between the surface of each roller 51 and the baked product 2. This alleviates the tensile stress that occurs in the longitudinal direction of the baked product 2 due to thermal contraction during baking, and results in a baked product 2 of good quality with reduced damage.

[0029] 2 is a diagram for explaining the roller speed control in this embodiment, and shows a graph showing the temperature profile of the firing furnace 30. As shown in FIG. 1, the firing furnace 30 has three regions 31, 32, and 33 that are connected to each other in the conveying direction D1 and are separated to some extent. That is, the firing furnace 30 has, from upstream to downstream, a temperature rise region 31 that raises the temperature inside the furnace, a holding region 32 that holds the temperature inside the furnace raised by the temperature rise region 31, and a cooling region 33 that lowers the temperature inside the furnace, in this order. Therefore, the carry-in entrance 34 can be regarded as a carry-in entrance to the temperature rise region 31, and the carry-out exit 35 can be regarded as a carry-out exit from the cooling region 33.

[0030] 2, the temperature profile is illustrated by a solid line. The horizontal axis of the graph can be interpreted as a position toward the discharge port 35 in the conveying direction D1 based on the carry-in entrance 34, or as the passage of time based on the time when the sintered article 2 conveyed in the conveying direction D1 leaves the carry-in entrance 34. The temperature profile has a heating profile T1 corresponding to the heating region 31, a holding profile T2 corresponding to the holding region 32, and a cooling profile T3 corresponding to the cooling region 33.

[0031] In the temperature rising region 31, the heater output is set so that the temperature in the furnace rises continuously from room temperature to a predetermined maximum temperature in the conveying direction D1 as shown by the temperature rising profile T1. In the holding region 32, the heater output is set so that the temperature in the furnace is approximately held at the maximum temperature as shown by the holding profile T2. In the cooling region 33, the heater output and the cooler are set so that the temperature in the furnace falls continuously from the maximum temperature to room temperature in the conveying direction D1 as shown by the cooling profile T3.

[0032] In this embodiment of the present invention, the heat treatment system 10 further includes a roller drive control unit 60. The roller drive control unit 60 can change the conveying speed of at least some of the rollers 51 included in the plurality of rollers 51 in response to the shrinkage of the baked object 2 caused by baking. The roller drive control unit 60 includes, for example, one or more motors for rotating the rollers 51, a transmission mechanism for transmitting power from the motors to the rollers 51, and a driver circuit for controlling the driving of the motors, switching of the transmission mechanism, and the like.

[0033] In the graph of Fig. 2, the expansion rate of the product 2 to be sintered transported through the sintering furnace 30 is illustrated by a two-dot chain line. According to Fig. 2, the expansion rate of the product 2 to be sintered gradually increases after entering the temperature-rise zone 31, but starts to decrease at a certain point. Then, while passing through the temperature-rise zone 31, the expansion rate of the product 2 to be sintered turns negative, and the product 2 to be sintered shrinks compared to before the start of the heat treatment. In other words, according to Fig. 2, the product 2 to be sintered thermally shrinks at a certain point while passing through the temperature-rise zone 31, and then this state is maintained until the product has passed through the holding zone 32, and when it proceeds to the cooling zone 33, it thermally shrinks further.

[0034] Such a thermal contraction pattern of the baked product 2 is a result grasped in advance by the inventor through experiments and simulations. Therefore, the roller drive control unit 60 changes the conveying speed of the rollers 51, i.e., the rotation speed of the rollers 51, in response to such a thermal contraction pattern. In FIG. 2, the reference symbols 50a, 50b, and 50c respectively indicate a situation in which the rollers 51 arranged in the baking furnace 30 among the rollers 51 constituting the roller group 50 are further divided into groups (subgroups) according to their positions. In FIG. 2, the subgroups 50a, 50b, and 50c are simplified and shown as rectangles, but in reality, each of the subgroups 50a, 50b, and 50c is composed of a plurality of rollers 51 arranged in the conveying direction D1.

[0035] The first subgroup 50a is made up of some of the rollers 51 belonging to the temperature-rising zone 31, and generally consists of the rollers 51 belonging to the range from the carry-in entrance 34 to a predetermined position where the expansion rate of the baked article 2 turns negative as described above. The second subgroup 50b is made up of generally the rollers 51 not belonging to the first subgroup 50a among the rollers 51 belonging to the temperature-rising zone 31, and the rollers 51 belonging to the holding zone 32. The third subgroup 50c is made up of generally the rollers 51 belonging to the cooling zone 33.

[0036] The roller drive control unit 60 changes the conveying speed of each roller 51 of the second subgroup 50b and the third subgroup 50c out of the first to third subgroups 50a, 50b, and 50c to be slower than the conveying speed of each roller 51 of the first subgroup 50a. This is an example of control in which the conveying speed of the rollers 51 located downstream of a predetermined position in the temperature rising region 31 is slower than that of the rollers 51 located upstream of the predetermined position.

[0037] In Fig. 2, the numerical values ​​in parentheses for each of the first to third subgroups 50a, 50b, and 50c indicate the difference in speed. As an example, when the conveying speed of each roller 51 of the first subgroup 50a is 100%, the roller drive control unit 60 can set the conveying speed of each roller 51 of the second subgroup 50b to 95% and the conveying speed of each roller 51 of the third subgroup 50c to 90%. According to such roller speed control performed by the roller drive control unit 60, even if the thermal shrinkage occurs in the baked product 2 baked in the baking furnace 30, the conveying speed of the rollers 51 located downstream of the predetermined position can be slowed down to appropriately suppress the tensile stress generated in the baked product 2.

[0038] The roller speed control by the roller drive control unit 60 is not limited to the above-mentioned specific example. For example, in the example of Fig. 2, the rollers 51 arranged in the firing furnace 30 are divided into three subgroups with different conveying speeds, but the number of such subgroups may be two, four or more. In addition, the positions at which the subgroups are divided in the firing furnace 30 may be varied depending on the temperature control in the firing furnace 30 and the characteristics of the fired product 2 to be heat-treated.

[0039] FIG. 3 shows a heat treatment system 10 according to an example different from that shown in FIG. 1. Regarding FIG. 3, differences from FIG. 1 will be described. According to FIG. 3, the heat treatment system 10 does not include a cutting device 70 and a storage device 80 downstream of the discharge port 35, but includes a winding mechanism 40. The baked product 2 after being baked in the baking furnace 30 is separated from the roller 51 and wound up by the winding mechanism 40. That is, the winding mechanism 40 rotates to wind up the baked product 2 into a roll and collect it. Furthermore, according to FIG. 3, the baked product 2 is allowed to bend between the unwinding mechanism 20 and the winding mechanism 40 and the roller group 50, and, for example, a configuration that applies tension to the baked product 2 is not particularly included other than the unwinding mechanism 20, the winding mechanism 40, and the roller group 50.

[0040] Although specific examples of the technology disclosed in this specification have been described in detail above, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and variations of the specific examples exemplified above. Furthermore, the technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. Furthermore, the technology exemplified in this specification or drawings achieves multiple objectives simultaneously, and achieving one of the objectives itself has technical utility. [Explanation of symbols]

[0041] 1: Roll body 2: Product to be fired 10: Heat treatment system 20: Unwinding mechanism 30: Kiln 31: Temperature rise area 32: Holding area 33: Cooling area 34: Loading entrance 35: Exit 40: Winding mechanism 50: Roller group 51: Laura 60: Roller drive control unit 70: Cutting device 80: Storage device D1: Transport direction

Claims

1. An unwinding mechanism for unwinding a strip-shaped sintered product; A plurality of rollers each capable of rotating to contact the baked product unwound by the unwinding mechanism and transport the baked product; a baking furnace for baking the baked product transported by the plurality of rollers; The rollers are made of a heat-resistant material that can be used in a temperature range of 600°C to 1400°C. The unwinding mechanism is provided at a position higher than a position where the plurality of rollers support the baked product, A heat treatment system in which the plurality of rollers support and transport the product to be sintered hanging down from the unwinding mechanism.

2. The heat treatment system according to claim 1 , wherein the surfaces of the rollers that come into contact with the product to be baked are smoothed.

3. The heat treatment system of claim 2 , wherein the surface has a surface roughness of Ra 6.3 μm or less.

4. 2. The heat treatment system according to claim 1, wherein the rollers are made of ceramics having an alumina content of 50% to 70%.

5. The heat treatment system according to claim 1 , further comprising a roller drive control unit capable of changing a conveying speed of at least some of the rollers included in the plurality of rollers in response to shrinkage of the baked object due to the baking.

6. the firing furnace has, from the upstream to the downstream of the conveyance by the plurality of rollers, a temperature increasing region for increasing the temperature inside the furnace, a holding region for holding the temperature inside the furnace increased by the temperature increasing region, and a cooling region for decreasing the temperature inside the furnace, The heat treatment system according to claim 5 , wherein the roller drive control unit controls the conveying speed of the rollers located downstream of a predetermined position in the temperature rise region to be slower than that of the rollers located upstream of the predetermined position.

7. The heat treatment system according to claim 1 , further comprising a winding mechanism for winding up the baked object after being baked in the baking furnace.

8. The heat treatment system according to claim 1 , wherein the article to be fired is glass, ceramics, metal, or a mixture thereof.

Citation Information

Patent Citations

  • Roller hearth kiln and its operation method

    JP1998259996A

  • Burning of ceramic sheet and burning apparatus

    JP2001031476A

  • Roller hearth type continuous burning furnace

    JP2002318077A

  • Continuous heating furnace and heating treatment method for object to be treated using the same

    JP2023034757A