Composition for biosensors and biosensor

The biosensor composition forms a single enzyme-polymer layer using specific polymers and solvents, addressing compatibility issues and denaturation challenges, resulting in improved manufacturing ease and performance.

WO2024205276A1PCT designated stage expired Publication Date: 2024-10-03I COREBIO INC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2024/003976
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Existing biosensors requiring multiple layers with incompatible polymers and enzymes are difficult to manufacture, limiting commercialization and performance due to enzyme denaturation by organic solvents and compatibility issues.

Method used

A biosensor composition that mixes enzymes and polymers to form a single layer, using amphipathic polyurethane polymers with specific water absorption and ductility, along with solvents like tetrahydrofuran, to prevent enzyme leakage and enhance substrate permeability, allowing for high-accuracy sensing without separate enzyme and polymer layers.

Benefits of technology

This approach simplifies biosensor manufacturing, improves service life, sensitivity, and response speed while eliminating interference from blood substances, making the biosensor easier to commercialize with excellent performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2024003976_03102024_PF_FP_ABST
    Figure KR2024003976_03102024_PF_FP_ABST
Patent Text Reader

Abstract

The composition for biosensors according to various embodiments of the present invention, which is a composition for forming an enzyme-polymer monolayer, comprises an enzyme, a polymer, and a solvent. The biosensor according to various embodiments of the present invention includes: an ion-selective membrane; and an enzyme layer disposed on the ion-selective membrane, wherein the enzyme layer comprises an enzyme and a polymer.
Need to check novelty before this filing date? Find Prior Art

Description

Composition for biosensor and biosensor

[0001] Various embodiments of the present invention relate to a composition for a biosensor and a biosensor. Specifically, the present invention relates to a composition for a biosensor and a biosensor capable of forming a single layer by mixing polymers and enzymes that are difficult to mix.

[0002] As a biosensor for measuring urea in blood, existing voltage-based biosensors consist of an outer membrane layer permeable only to specific substrates, an enzyme layer capable of metabolizing the substrate, and an inner selective membrane layer that selectively allows metabolites to pass through. To fabricate a sensor with such a complex layer structure, compatibility between each layer is crucial. Furthermore, the significant time required for sensor fabrication hinders commercialization.

[0003] Meanwhile, the outer membrane layer is mainly composed of a polymer membrane and is soluble in organic solvents, whereas the enzymes in the enzyme layer are mostly water-soluble and can be denatured by organic solvents, making it difficult to mix the two layers.

[0004] The present invention is intended to solve the above-described problem, and to provide a composition for a biosensor and a biosensor that are easy to commercialize and have excellent performance by mixing polymers and enzymes that are difficult to mix and forming a single layer.

[0005] A composition for a biosensor according to various embodiments of the present invention comprises an enzyme, a polymer, and a solvent.

[0006] A biosensor according to various embodiments of the present invention comprises an ion-selective membrane; and an enzyme layer disposed on the ion-selective membrane, wherein the enzyme layer comprises an enzyme and a polymer.

[0007] Since the composition for a biosensor of the present invention includes both an enzyme and a polymer, when applied to a biosensor, there is no need to form an enzyme layer and a polymer layer separately, and the composition can be formed as a single layer.

[0008] The biosensor composition of the present invention utilizes a polymer with excellent substrate permeability and enzyme entrapment, thereby preventing enzyme leakage. Furthermore, it eliminates the influence of interfering substances in blood, enabling highly accurate sensing.

[0009] The biosensor of the present invention can be manufactured simply because there is no need to form the enzyme layer and polymer layer separately, and is easy to commercialize.

[0010] The biosensor of the present invention has excellent service life and sensitivity, and can have fast response characteristics.

[0011] Figure 1 is a schematic diagram of a biosensor according to various embodiments of the present invention.

[0012] Figure 2 is NH4 + This is a sensitivity graph regarding the evaluation results of the ion-selective electrode.

[0013] Figure 3 is NH4 + This is a linear graph of the evaluation results of ion-selective electrodes.

[0014] Figure 4 is a sensitivity graph regarding the results of urea performance evaluation according to polymer type.

[0015] Figure 5 is a linear graph showing the results of urea performance evaluation according to polymer type.

[0016] Figure 6 is a sensitivity graph regarding the results of urea performance evaluation according to solvent type.

[0017] Figure 7 is a linear graph showing the results of urea performance evaluation according to solvent type.

[0018] Figure 8 is a sensitivity graph regarding the results of urea performance evaluation according to the presence or absence of a cross-linking agent.

[0019] Figure 9 is a linear graph showing the results of urea performance evaluation according to the presence or absence of a cross-linking agent.

[0020] Figures 10 and 11 are graphs regarding the results of urea sensor evaluation in a flow device.

[0021] Figure 12 is a graph comparing the performance of the reference equipment in the flow device.

[0022] Figure 13 is a correlation graph of the reference equipment (COBAS) with the results of evaluating a biological sample in a flow device.

[0023] Figure 14 is an accuracy graph showing the results of evaluating a biological sample in a flow device.

[0024] Figure 15 is a graph of the results of urea sensor evaluation in a flow device, showing slope change over time.

[0025] Below, various embodiments of this document are described. The embodiments and terminology used herein are not intended to limit the technology described in this document to specific embodiments, but should be understood to encompass various modifications, equivalents, and / or alternatives of the embodiments.

[0026]

[0027] Composition for biosensor

[0028] A composition for a biosensor according to various embodiments of the present invention is a composition for forming an enzyme-polymer monolayer, and may include an enzyme, a polymer, and a solvent. Since the composition for a biosensor of the present invention includes both an enzyme and a polymer, when applied to a biosensor, there is no need to form an enzyme layer and a polymer layer separately, and the composition can be formed as a monolayer.

[0029] The enzyme included in the composition for a biosensor may include at least one selected from the group consisting of urease, glucose oxidase, glucose dehydrogenase, lactate oxidase, and lactate dehydrogenase. For example, when urease is used as the enzyme, the composition of the present invention can be used as a composition for a urea biosensor.

[0030] The enzyme may be included in an amount of 0.1 wt% to 10 wt% relative to the total composition. Preferably, the enzyme may be included in an amount of 0.1 wt% to 4 wt% relative to the total composition. This allows the composition to have a viscosity suitable for sensor fabrication.

[0031] The polymer included in the composition for the biosensor may be an amphiphilic polyurethane. For example, the polymer may be an aliphatic polyether-based thermoplastic polyurethane (TPU) or an ether-based hydrophilic urethane.

[0032] Specifically, the polymer may have a water absorption capacity of 20% to 120% as measured by ASTM D570, and a ductility of 300% to 640% as measured by ASTM D412. If both the water absorption capacity and ductility are satisfied, a biosensor can be manufactured using a composition mixed with an enzyme. In other words, if a polymer exceeding the values ​​is used, the viscosity may become too high or suspended solids may be generated when mixing the enzyme, making it difficult to manufacture a biosensor.

[0033] Polymers can be porous. Enzymes can be positioned within the pores of these porous polymers. Polymers that satisfy these properties exhibit excellent substrate permeability and can entrap enzymes, preventing their leakage. Therefore, when applied to biosensors, they can extend the sensor's lifespan and provide superior sensitivity and rapid response. Furthermore, they can eliminate the influence of interfering substances in blood, enabling highly accurate sensing.

[0034] The polymer may be included in an amount of 0.1 wt% to 10 wt% relative to the total composition. Preferably, the polymer may be included in an amount of 0.1 wt% to 4 wt% relative to the total composition. This allows the composition to have a viscosity suitable for fabricating a sensor.

[0035] The solvent may include at least one selected from the group consisting of tetrahydrofuran, cyclohexanone, chloroform, methanol, ethanol, propanol, 2-methoxyethanol, and 2-ethoxyethanol. Such solvents can be used in a composition containing both a polymer and a solvent because they dissolve the polymer without destroying the enzyme.

[0036] For example, if the polymer has a water absorption capacity of 120% and a ductility of 640%, the solvent can be used alone. On the other hand, if the polymer has a water absorption capacity of less than 120% and a ductility of less than 640%, a mixture of the two types of solvents can be used.

[0037] Meanwhile, the composition for a biosensor according to various embodiments of the present invention may further include a cross-linking agent. The cross-linking agent may include at least one selected from the group consisting of glutaraldehyde, glyoxal, malonic dialdehyde, and succinic dialdehyde. The cross-linking agent can enhance the capture and leakage prevention properties of the enzyme by increasing the size of the enzyme through cross-linking between enzymes and inhibiting leakage out of the polymer membrane.

[0038]

[0039] biosensor

[0040] A biosensor according to various embodiments of the present invention can be manufactured using the composition described above.

[0041] Specifically, referring to FIG. 1, the biosensor (10) may include a substrate (100), an electrode (200), a hydrogel layer (300), an ion-selective membrane (400), and an enzyme layer (500).

[0042] The substrate (100) can support an electrode (200), a hydrogel layer (300), an ion-selective membrane (400), and an enzyme layer (500).

[0043] The electrode (200) may include at least one selected from the group consisting of silver (Ag), silver chloride (AgCl), platinum, and gold. Specifically, the electrode (200) may include Ag / AgCl manufactured by oxidizing a silver (Ag) electrode.

[0044] The hydrogel layer (300) is a hydrogel layer and can be placed on the electrode (200). For example, the hydrogel layer (300) can be formed from a solution containing MES buffer, sodium chloride (NaCl), potassium chloride (KCl), calcium chloride (CaCl2), ammonium chloride (NH4Cl), and polyvinyl alcohol (PVA).

[0045] The ion-selective membrane (400) is an ammonium ion (NH4 + ) can be placed on the hydrogel layer (300) as a layer that selectively detects ion-selective ions. The ion-selective membrane (400) can be formed from a solution containing c-PVC (carboxylated polyvinylchloride), nonactin, dioctyl adipate (DOA), (potassium tetrakis(4-chlorophenyl)borate (KTpClPB) and a solvent.

[0046] The enzyme layer (500) can be formed from the biosensor composition described above. The enzyme layer (500) can be a single layer comprising an enzyme (510) and a polymer (520). That is, the present invention can be simply manufactured and is easy to commercialize because there is no need to form the enzyme layer and the polymer layer separately.

[0047]

[0048] Hereinafter, the present invention will be described in detail through examples and experimental examples. However, the following examples and experimental examples are only intended to illustrate the present invention, and the present invention is not limited to the following examples and experimental examples.

[0049]

[0050] Examples 1 to 10: Biosensor manufacturing

[0051] 1. Manufacturing of ion-selective electrodes

[0052] (1) Electrode preparation

[0053] The silver electrode is oxidized with 0.3 M FeCl3 for 30 minutes to form silver / silver oxide (Ag / AgCl).

[0054] (2) NH4 for ion-selective membrane + cocktail making

[0055] Dissolve 33 mg c-PVC (1.8% carboxylated polycvinnylchloride), 2 mg nonactin, 66 mg DOA (Dioctyl adipate), and 0.2 mg KTpClPB (potassium tetrakis(4-chlorophenyl)borate) in 400 μL of THF (tetrahydrofuran).

[0056] (3) Hydrogel manufacturing

[0057] Dissolve 100 mM NaCl, 3 mM KCl, 1 mM CaCl2, and 10 mM NH4Cl in 300 mM MES buffer solution, then dissolve PVA (poly vinyl alcohol) at a concentration of 40 mg / ml.

[0058] (4) NH4 + cocktail and hydrogel dispensing

[0059] Dispense 60 nL of hydrogel onto the prepared silver / silver oxide electrode using a dispenser and dry for 30 minutes at 20°C and a relative humidity of 20% or less. After drying the hydrogel, NH4 is added using a dispenser. + Dispense 600 nL of cocktail and dry overnight (more than 12 hours) at 20°C and relative humidity of 20% or less.

[0060] 2. Enzyme layer preparation

[0061] (1) Polymer solution manufacturing

[0062] It was manufactured using the polymer according to Table 1 below and the solvent according to Table 2 below. At this time, 40 mg of the polymer according to Table 1 below was added to 1 ml of the solvent and dissolved on a hot plate at 300 rpm and 100°C for 1 hour. Alternatively, it was dissolved at room temperature instead of 100°C for 5 to 6 hours.

[0063] Name Type Water Absorption (ASTM D570 measurement standard) Ductility (ASTM D412 measurement standard) Polymer 1 (Comparative example) Aliphatic polyether TPU 130% 640% Polymer 2 (Examples 1, 8, 9, 10) 120% 640% Polymer 3 (Example 2) 120% 300% Polymer 4 (Example 3) 20% 350% Polymer 5 (Example 4) 30% 350% Polymer 6 (Example 5) 110% 400% Polymer 7 (Comparative example) Aliphatic elastomer 50% 290% Polymer 8 (Comparative example) Aromatic elastomer 15% 650% Polymer 9 (Example 6) Ether-based hydrophilic urethane 70% 450% Polymer 10 (Example 7) Ether-based hydrophilic urethane90%500%

[0064]

[0065] Polymer typePolymer concentration (wt%)Solvent typeTurbidity after dissolution 1 Creation of floats 2 Suitability for sensor manufacturing 3Polymer 142-methoxyethanol 325THF:CHX = 4:1426CHCl 3325 Polymer 24THF 527CHCl 3527CHX 527 42-methoxyethanol 55 106 2-methoxyethanol 516 82-methoxyethanol 426 102-methoxyethanol 426 Polymer 342-methoxyethanol 415THF 415CHCl 3415CHX 415THF:CHX = 4:1538 Polymer 442-methoxyethanol 415THF 415CHCl 3415CHX 415THF:CHX = 4:1538 Polymer 542-methoxyethanol 516THF 516CHCl 3516CHX 516THF:CHX = 4:1538 Polymer 642-methoxyethanol 426THF:CHX = 4:1538Polymer 742-methoxyethanol 112THF 112CHCl 3 112CHX 112THF:CHX=4:1112Polymer 842-methoxyethanol 213THF 123CHCl 3 112CHX 112THF:CHX=4:1112Polymer 942-methoxyethanol 213THF 415CHCl 3 415CHX 415THF / CHX 437Polymer 1042-methoxyethanol 325THF 415CHCl 3 415CHX 415THF / CHX 437

[0066]

[0067] THF: tetrahydrofuran, CHX: Cyclohexanone, CHCl3: Chloroform

[0068] 1 Turbidity after dissolution: Dissolve the polymer in each solvent and evaluate the turbidity level (0: high turbidity, 5: low turbidity, high score is suitable for sensor production)

[0069] 2 Suspension formation: Dissolve the polymer in each solvent and evaluate the degree of suspension formation (0: high degree of formation, 5: low degree of formation, high score is suitable for sensor production)

[0070] 3Sensor manufacturing suitability: calculated as 1+2 (0~3: impossible to manufacture, 4~6: difficult to manufacture, 7~9: possible to manufacture, 10: very suitable)

[0071]

[0072] (2) Preparation of urease solution

[0073] Dissolve 5 mg of urease in 90 μL of DI water by shaking with a voltex. The urease used here is in powder form and is from Calzyme with an activity of 100 U / mg.

[0074] (3) Preparation of enzyme layer solution (polymer solution + urease solution)

[0075] Prepare an enzyme layer solution by mixing 90 μL of urease solution with 120 μL of polymer solution.

[0076] (4) Dispensing enzyme layer solution

[0077] Dispense 600 nL of enzyme layer solution onto the prepared ion-selective electrode using a dispenser and dry overnight (more than 12 hours) at 20°C and a relative humidity of 20% or less.

[0078]

[0079] Meanwhile, referring to Tables 1 and 2 above, it can be seen that sensor manufacturing is possible only when using polymers (polymers 2 to 6 and 9 to 10) that have a water absorbency of 20 to 120% and a ductility of 300 to 640%. That is, when polymer 1 has a ductility of 640% but a water absorbency exceeds 120%, or polymer 7 has a water absorbency of 50% but a ductility of less than 300%, or polymer 8 has a water absorbency of less than 20% and a ductility of more than 640%, sensor manufacturing was impossible.

[0080] In addition, when the water absorption capacity of the polymer was 120% and the ductility was 640%, such as polymer 2, the sensor could be manufactured using a single solvent. On the other hand, when the water absorption capacity of the polymer was less than 120% and the ductility was less than 640%, such as polymers 3 to 6 and 9 to 10, the sensor could be manufactured only when a mixed solvent was used.

[0081] The sensors using the polymer solution that enabled the sensor production in Table 2 above are named Examples 1 to 10, and are summarized in Table 3 below.

[0082] Example Polymer type Solvent type Example 1 Polymer 2 Sole solvent (2-methoxyethanol) Example 2 Polymer 3 Mixed solvent (THF:CHX = 4:1) Example 3 Polymer 4 Mixed solvent (THF:CHX = 4:1) Example 4 Polymer 5 Mixed solvent (THF:CHX = 4:1) Example 5 Polymer 6 Mixed solvent (THF:CHX = 4:1) Example 6 Polymer 9 Mixed solvent (THF / CHX) Example 7 Polymer 10 Mixed solvent (THF / CHX) Example 8 Polymer 2 Sole solvent (THF) Example 9 Polymer 2 Sole solvent (CHCl3) Example 10 Polymer 2 Sole solvent (CHX)

[0083] Example 11: Biosensor Manufacturing

[0084] The ion-selective electrode was manufactured in the same manner as in Examples 1 to 10 above, but the enzyme layer was manufactured using the following process.

[0085] (1) Polymer solution manufacturing

[0086] 40 mg of polymer 10 was added to 1 ml of THF:CHX (4:1) solvent and dissolved at 300 rpm and 100°C for 1 hour.

[0087] (2) Preparation of urease solution

[0088] 5 mg of urease was dissolved in 85 μL of DI water, 5 μL of glutaraldehyde as a cross-linking agent was added, and the mixture was stirred for 10 minutes.

[0089] (3) Preparation of enzyme layer solution and (4) dispensing of enzyme layer solution were prepared in the same manner as described above.

[0090]

[0091] Experimental Example 1: NH4 in a conventional device + Evaluation of ion-selective electrodes

[0092] NH4 using the sensor according to the above Example 1 + The sensitivity to NH4Cl was evaluated. Specifically, 1 M NH4Cl standard solution was added dropwise in a 0.1 M MOPS buffer environment to change the concentration to 1, 5, 10, 30, and 50 mM. + The results of the sensitivity test were obtained.

[0093] As a result, referring to the sensitivity graph of Fig. 2, it can be seen that the voltage increases as the amount of NH4Cl standard solution added increases. Also, referring to the linear graph of Fig. 3, NH4 + It can be seen that the voltage increases depending on the concentration of NH4. That is, + It can be seen that the sensitivity to ions is excellent.

[0094] Experimental Example 2: Evaluation of urea sensor performance according to polymer type in a conventional device.

[0095] In order to evaluate urea performance according to the type of polymer, the above examples 1 to 7 were used. Specifically, 1 M urea standard solution was added dropwise in a 0.1 M MOPS buffer environment, and the sensitivity results for urea were obtained by changing the concentration to 1, 5, 10, 30, and 50 mM.

[0096] As a result, referring to FIG. 4 and Table 4 below, it can be seen that the voltage increases as the amount of urea standard solution added increases. In addition, referring to FIG. 5 and Table 4 below, it can be seen that the voltage increases with the urea concentration. That is, it can be seen that the sensitivity performance for urea is excellent. Although the sensitivity results of each example show differences, the results are similar to the sensitivity (51 mv / dec.) for the response to ammonium ion in the results of Experimental Example 1 above, and it can be seen that the developed sensor metabolizes urea into ammonium ion, and the metabolite ammonium ion selectively permeates through the ion-selective membrane to provide a response.

[0097]

[0098] Slope(mV / dec.)R 2 Example 157.4 ± 1.20.9784 ± 0.0023 Example 242.8 ± 2.20.9832 ± 0.0069 Example 343.6 ± 0.40.9832 ± 0.0010 Example 449.8 ± 0.60.9884 ± 0.0011 Example 548.4 ± 0.60.9864 ± 0.0015 Example 662.1 ± 0.30.9990 ± 0.0020 Example 749.4 ± 1.00.9905 ± 0.0011

[0099] Experimental Example 3: Evaluation of urea sensor performance according to solvent type in a conventional device.

[0100] In order to evaluate urea performance according to solvent type, the above examples 1, 8, 9 and 10 were used for evaluation. Specifically, 1 M urea standard solution was added dropwise in a 0.1 M MOPS buffer environment, and the sensitivity results for urea were obtained by changing the concentration to 1, 5, 10, 30 and 50 mM.

[0101] As a result, referring to FIG. 6 and Table 5 below, it can be seen that the voltage increases as the amount of urea standard solution added increases. In addition, referring to FIG. 7 and Table 5 below, it can be seen that the voltage increases with the urea concentration. Meanwhile, in the case of polymer 2, it can be seen that the sensitivity to urea is the best when 2-methoxyethanol is used as a solvent.

[0102]

[0103] Polymer type Solvent type Slope (mV / dec.) R 2 Example 1 Polymer 2 Solvent 1 (2-methoxyethanol) 50.3 ± 0.9 0.99 16 ± 0.0004 Example 8 Solvent 2 (THF) 40.1 ± 1.2 0.99 72 ± 0.0008 Example 9 Solvent 3 (CHC3) 38.6 ± 0.8 0.99 78 ± 0.0005 Example 10 Solvent 4 (CHX) 44.7 ± 1.3 0.98 83 ± 0.0018

[0104] Experimental Example 4: Evaluation of urea sensor performance with and without cross-linking agent in a conventional device.

[0105] In order to evaluate the urea performance according to the presence or absence of a cross-linker, the above examples 7 and 11 were used. Specifically, a 1 M urea standard solution was added dropwise in a 0.1 M MOPS buffer environment, and the sensitivity results for urea were obtained by varying the concentration to 1, 5, 10, 30, and 50 mM.

[0106] As a result, referring to FIG. 8 and Table 6 below, it can be seen that the voltage increases as the amount of urea standard solution added increases. In addition, referring to FIG. 9 and Table 6 below, it can be seen that the voltage increases with the urea concentration. In other words, it can be seen that the sensitivity to urea is excellent regardless of the presence or absence of a cross-linking agent.

[0107] Slope(mV / dec.)R 2Example 749.4 ± 1.00.9905 ± 0.0011Example 1148.5 ± 0.90.9912 ± 0.0010

[0108]

[0109] Experimental Example 5: Evaluation of Urea Sensor Performance in a Flow Device

[0110] The performance of the urea sensor was evaluated in a flow device using Example 1. The flow device was comprised of a urea sensor, a temperature controller, a test solution, a valve for flowing the test solution, a peristaltic pump, and a PC for collecting sensor signals.

[0111] Specifically, to confirm urea sensitivity, assay solutions containing 0.5, 1, 5, 10, and 30 mM urea in a 0.1 M MOPS buffer-based solution were prepared and flowed at regular intervals to evaluate the performance of the sensor.

[0112] As a result, referring to FIGS. 10 and 11, it can be seen that the voltage increases according to the urea concentration. That is, it can be seen that the flow device also has excellent sensitivity to urea.

[0113] Experimental Example 6: Comparison of Reference Equipment Performance in a Flow Device

[0114] Using Example 1, the performance of the flow device was compared with that of the reference equipment. The reference equipment was COBAS C111.

[0115] As a result, referring to FIG. 12, it can be seen that the sensor according to the embodiment has performance almost equivalent to that of the reference equipment.

[0116] Experimental Example 7: Evaluation of Biological Samples in a Flow Device

[0117] Using Example 1, the performance of the flow device was compared with that of a reference device based on a biological sample (plasma). The reference device was COBAS C111.

[0118] As a result, referring to FIGS. 13 and 14, it can be seen that the sensor according to the embodiment has performance and accuracy almost equivalent to that of the reference equipment.

[0119] Experimental Example 8: Evaluation of Urea Sensor Performance in a Flow Device

[0120] The change in slope over time was confirmed using Examples 1 to 7 and 11.

[0121] To specifically confirm the urea sensitivity, assay solution 1 containing 0.5 mM urea and assay solution 2 containing 30 mM urea were prepared in a 0.1 M MOPS buffer-based solution and flowed at regular intervals to evaluate the service life of the sensor.

[0122] As a result, referring to Fig. 15, it can be seen that Example 1 has the best service life as there is almost no change in slope over time.

[0123] Specifically, Examples 7 and 11 are the results of comparing the life-time according to the presence or absence of a cross-linking agent in the same composition. The performance of the initial sensors was similar, but the sensor with the cross-linking agent maintained its sensor performance over time compared to the sensor without the cross-linking agent, indicating that the cross-linked enzyme was more captured in the polymer membrane and the service life was improved.

[0124]

[0125] The features, structures, effects, etc. described in the above-described embodiments are included in at least one embodiment of the present invention, and are not necessarily limited to just one embodiment. Furthermore, the features, structures, effects, etc. exemplified in each embodiment can be combined or modified in other embodiments by those skilled in the art to which the embodiments pertain. Therefore, the contents related to such combinations and modifications should be construed as falling within the scope of the present invention.

[0126] In addition, although the above description focuses on embodiments, these are merely examples and do not limit the present invention. Those skilled in the art to which the present invention pertains will appreciate that various modifications and applications not exemplified above are possible without departing from the essential characteristics of the present embodiments. For example, each component specifically shown in the embodiments can be modified and implemented. In addition, differences related to such modifications and applications should be interpreted as being included within the scope of the present invention defined in the appended claims.

Claims

1. A composition for forming an enzyme-polymer monolayer, A composition for a biosensor comprising an enzyme, a polymer and a solvent.

2. In paragraph 1, A composition for a biosensor, characterized in that the enzyme comprises at least one selected from the group consisting of urease, glucose oxidase, glucose dehydrogenase, lactate oxidase, and lactate dehydrogenase.

3. In paragraph 1, A composition for a biosensor, characterized in that the polymer is an amphiphilic polyurethane.

4. In paragraph 1, A composition for a biosensor, characterized in that the polymer has a water absorption capacity of 20% to 120% as measured by ASTM D570 and a ductility of 300% to 640% as measured by ASTM D412.

5. In paragraph 1, A composition for a biosensor, characterized in that the solvent comprises at least one selected from the group consisting of tetrahydrofuran, cyclohexanone, chloroform, methanol, ethanol, propanol, 2-methoxyethanol, and 2-ethoxyethanol.

6. In paragraph 1, A composition for a biosensor, characterized in that it further comprises a cross-linking agent.

7. In paragraph 6, A composition for a biosensor, characterized in that the crosslinking agent comprises at least one selected from the group consisting of glutaraldehyde, glyoxal, malonic dialdehyde, and succinic dialdehyde.

8. Ion-selective membrane; and comprising an enzyme layer disposed on the ion-selective membrane; A biosensor characterized in that the enzyme layer comprises an enzyme and a polymer.

9. In paragraph 8, A biosensor characterized in that the enzyme layer is a single layer containing an enzyme and a polymer.

10. In paragraph 8, A biosensor characterized in that the enzyme comprises at least one selected from the group consisting of urease, glucose oxidase, glucose dehydrogenase, lactate oxidase, and lactate dehydrogenase.

11. In paragraph 8, A biosensor, characterized in that the polymer is an amphiphilic polyurethane.

12. In paragraph 8, A biosensor characterized in that the polymer has a water absorption capacity of 20% to 120% as measured by ASTM D570 and a ductility of 300% to 640% as measured by ASTM D412.

13. In paragraph 8, A biosensor, characterized in that the enzyme layer further comprises a cross-linking agent.

14. In paragraph 13, A biosensor, characterized in that the cross-linking agent comprises at least one selected from the group consisting of glutaraldehyde, glyoxal, malonic dialdehyde, and succinic dialdehyde.

15. In paragraph 14, A biosensor characterized in that the cross-linking agent cross-links between the enzymes.

16. In paragraph 8, The above polymer contains pores, A biosensor characterized in that an enzyme is inserted into the pore.

Citation Information

Patent Citations

  • Bio-sensor for measuring urea and method of making the same

    KR100141779B1

  • Porous monolithic organic network membrane immobilized enzyme and preparation method thereof

    KR1020140122651A

  • Inter-floor noise prevention material and its construction structure

    KR1020230030143A

  • Health functional food composition for improving intestinal health containing psyllium hull

    KR1020230037761A

  • KR20210042686A