Metal structure, method for manufacturing same, and inspection device comprising same
The use of anodic oxide films and stacked metal layers addresses the challenges of cost and complexity in manufacturing metal structures with through holes, achieving strong bonding and improved frequency performance by etching and insulating the inner walls of the holes, enabling efficient and effective production of metal structures with complex geometries.
Patent Information
- Application Number
- PCT/KR2024/095583
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-24
- Filing Date
- 2024-03-19
- Publication Date
- 2024-10-03
AI Technical Summary
Existing methods for manufacturing metal structures with through holes, such as laser irradiation and plating using molds, face challenges including high costs for increasing numbers of holes and limitations in shape complexity and thickness, particularly with photoresist-based molds that struggle to form vertical holes and experience step issues between layers.
A method involving anodic oxide films is proposed, where through holes are created by etching anodic oxide films, with insulating films applied to the inner walls to enhance bonding strength and frequency characteristics, and the structures are formed by stacking metal layers of the same or different materials to achieve complex shapes and improved durability.
This approach allows for cost-effective production of metal structures with complex through hole geometries, improved bonding strength, and enhanced frequency characteristics, minimizing the peeling of insulating films and reducing noise interference in high-frequency inspections.
Smart Images

Figure KR2024095583_03102024_PF_FP_ABST
Abstract
Description
Metal structure, manufacturing method thereof, and inspection device comprising the same
[0001] The present invention relates to a metal structure manufactured using an anodic oxide film, a method for manufacturing the same, and an inspection device having the same.
[0002] In a metal structure having micro-sized through holes, methods for producing the through holes can be considered, such as a method of producing the through holes by irradiating a laser and a method of forming the through holes by plating using a mold.
[0003] The method of creating through-holes by irradiating them with a laser leads to increased manufacturing costs as the number of through-holes increases. Furthermore, it's difficult to implement a variety of through-hole shapes.
[0004] Meanwhile, the method of forming by plating using a mold is advantageous in that manufacturing costs do not increase proportionally even with a large number of through-holes, and the shapes of the through-holes can be implemented in a variety of ways. However, there is a limit to the thickness of the metal structure. More specifically, the mold is made of photoresist, a photosensitive material. If the photoresist is formed thickly all at once, it is impossible to obtain vertical through-holes. While it is possible to form a thick mold by laminating multiple layers of photoresist, this leads to the problem of steps occurring between the layers.
[0005] Therefore, we propose a new method for manufacturing a metal structure having a through hole.
[0006] [Prior Art Literature]
[0007] [Patent Document]
[0008] (Patent Document 1) Republic of Korea Patent Publication No. 10-2017-0068241
[0009] The present invention has been devised to solve the problems of the above-described prior art, and its purpose is to provide a metal structure manufactured using an anodic oxide film, a method for manufacturing the same, and an inspection device having the same.
[0010] In order to solve the above-described problem and achieve the purpose, a metal structure according to one feature of the present invention includes a body made of a metal material having a plurality of through holes and a plurality of micro-trenches having a width and a depth formed on the inner walls of the through holes; and an insulating film formed to extend in the thickness direction of the body along the micro-trenches and formed in the circumferential direction of the through holes.
[0011] Additionally, the plurality of through holes include a first through hole provided with the insulating film and a second through hole not provided with the insulating film.
[0012] Additionally, the body is formed by laminating multiple metal layers of the same material.
[0013] Additionally, the body is formed by laminating multiple metal layers of different materials.
[0014] Additionally, the metal structure is a guide plate.
[0015] Meanwhile, a metal structure according to another feature of the present invention includes a body having a plurality of through holes, wherein at least a portion of the body is formed of an anodic oxide material, and the remaining portion is formed of a metal material, and the through holes provided in the anodic oxide material and the metal material have a width and a depth on their inner walls and are formed to extend in the thickness direction of the body, and have a plurality of micro-trench formed in the circumferential direction of the through holes.
[0016] Meanwhile, an inspection device according to the present invention comprises a body made of a metal material having a plurality of through holes and a plurality of micro-trenches having a width and a depth formed on the inner wall of the through holes; a guide plate including an insulating film formed to extend in the thickness direction of the body along the micro-trenches and formed in the circumferential direction of the through holes; and an electrically conductive contact pin inserted into the through holes.
[0017] Additionally, the electrically conductive contact pin includes at least one of a signal pin and a ground pin.
[0018] Additionally, the guide plate has the insulating film on the inner wall of the through hole into which the signal pin is inserted.
[0019] Meanwhile, a method for manufacturing a metal structure according to one feature of the present invention includes a step of preparing an anodic oxide film; a step of providing an etched portion formed by etching the anodic oxide film; a step of forming a first through-hole by etching the anodic oxide film; and a step of forming an insulating film on the inner wall of the first through-hole.
[0020] Meanwhile, a method for manufacturing a metal structure according to another feature of the present invention includes the steps of: preparing an anodic oxide film; providing an etched portion formed by etching the anodic oxide film; forming a first through hole in the anodic oxide film; and forming a second through hole in the metal portion.
[0021] The present invention provides a micro-trench on the inner wall of a through hole of a body to increase the surface area, and provides an insulating film along the micro-trench to have excellent bonding strength between the body and the insulating film, thereby minimizing the problem of the insulating film peeling off from the body.
[0022] In addition, the present invention provides a metal structure having improved frequency characteristics in high-frequency characteristic inspection when used as a guide plate by having a body including a metal material, a method for manufacturing the same, and an inspection device having the same.
[0023] FIG. 1 is a perspective view of a metal structure according to a preferred first embodiment of the present invention.
[0024] FIGS. 2A to 2L are flowcharts illustrating a method for manufacturing a metal structure of the first embodiment, taken along the line AA of FIG. 1.
[0025] Figure 3 is a plan view of the metal structure of the first embodiment.
[0026] Fig. 4 is a first example of a modification of the metal structure of the first embodiment.
[0027] Fig. 5a is a second-first variation example of the metal structure of the first embodiment, Fig. 5b is a second-second variation example of the metal structure of the first embodiment, and Fig. 5c is a second-third variation example of the metal structure of the first embodiment.
[0028] Figure 6 is a plan view of a metal structure of the second embodiment.
[0029] Figures 7a to 7i are flowcharts of a method for manufacturing a metal structure of the second embodiment.
[0030] Fig. 8 is a diagram showing an example of a first modification of a metal structure of the first embodiment equipped with a probe card.
[0031] Fig. 9 is a diagram showing an example of a first modification of a metal structure of the first embodiment equipped with a test socket.
[0032] The following merely exemplifies the principles of the invention. Therefore, those skilled in the art will be able to implement the principles of the invention and invent various devices within the scope and spirit of the invention, even if not explicitly described or illustrated herein. Furthermore, all conditional terms and embodiments listed herein are expressly intended, in principle, to facilitate understanding of the invention's concepts and should be understood as being solely intended to facilitate understanding and are not intended to be limited to the specifically enumerated embodiments and conditions.
[0033] The above-described purposes, features and advantages will become clearer through the following detailed description with reference to the attached drawings, so that a person having ordinary skill in the art to which the invention pertains can easily practice the technical idea of the invention.
[0034] Embodiments described herein will be described with reference to cross-sectional and / or perspective views, which are ideal exemplary drawings of the present invention. The thicknesses of films and regions, etc., illustrated in these drawings are exaggerated for the purpose of effectively explaining the technical contents. The form of the exemplary drawings may be modified due to manufacturing techniques and / or tolerances. Therefore, embodiments of the present invention are not limited to the specific forms illustrated, but also include changes in form resulting from the manufacturing process. The technical terms used herein are used only to describe specific embodiments and are not intended to limit the present invention. The singular expression includes plural surfaces unless the context clearly indicates otherwise. It should be understood that the terms "comprises" or "includes" herein indicate the presence of a feature, number, step, operation, component, part, or combination thereof described in the present specification, but do not preclude the possibility of the presence or addition of one or more other features, numbers, steps, operations, components, parts, or combinations thereof.
[0035] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the drawings.
[0036] The width direction of the metal structure (MS1, MS2) described below is the ±x direction indicated in the drawing, the length direction of the metal structure (MS1, MS2) is the ±y direction indicated in the drawing, and the thickness direction of the metal structure (MS1, MS2) is the ±z direction indicated in the drawing.
[0037] Hereinafter, a metal structure (MS1) according to a preferred first embodiment of the present invention and a manufacturing method thereof will be described with reference to FIGS. 1 to 3. FIG. 1 is a perspective view of the metal structure (MS1) of the first embodiment, FIGS. 2a to 2l illustrate a manufacturing method of the metal structure (MS1) of the first embodiment, and FIG. 3 is a plan view of the metal structure (MS1) of the first embodiment.
[0038] Referring to FIGS. 1 to 3, a metal structure (MS1) of the first embodiment is configured to include a body (BD) made of a metal material having a plurality of through holes (PH) and a plurality of micro-trenches (NT) having a width and a depth formed on an inner wall (IW) of the through holes (PH), and an insulating film (FL) formed to extend in the thickness direction (±z direction) of the body (BD) along the micro-trenches (NT) and formed in the circumferential direction of the through holes (PH).
[0039] The body (BD) is composed of a metal material. The metal material constituting the body (BD) includes at least one of rhodium (Rd), platinum (Pt), iridium (Ir), palladium (Pd), nickel (Ni), manganese (Mn), tungsten (W), phosphorus (Ph) or an alloy thereof, or a palladium-cobalt (PdCo) alloy, a palladium-nickel (PdNi) alloy, a nickel-phosphorus (NiPh) alloy, a nickel-manganese (NiMn), a nickel-cobalt (NiCo) or a nickel-tungsten (NiW) alloy, copper (Cu), silver (Ag), gold (Au) or an alloy thereof. However, the metal material is not limited thereto, and includes all of them as long as they can improve the physical, chemical and / or electrical properties of the metal structure (MS1) of the first embodiment.
[0040] The body (BD) has a plurality of through holes (PH) that penetrate the body (BD) upwardly and downwardly in the thickness direction (±z direction). As an example, the through holes (PH) include a first through hole (PH1) and a second through hole (PH2). The through holes (PH) may be provided in a shape having a square cross-section. Alternatively, the cross-sectional shape of the through holes (PH) may be provided in a circular cross-section shape or a polygonal cross-section shape other than the circular cross-section shape, but is not limited thereto.
[0041] The body (BD) has micro-trench (NT) with convex peaks and concave valleys repeated in the circumferential direction of the through hole (PH) on the inner wall (IW) of the through hole (PH).
[0042] A plurality of micro-trenches (NT) are formed with a width and depth, and are formed to extend in the thickness direction (±z direction) of the body (BD) and in the circumferential direction of the through hole (PH).
[0043] Specifically, the micro-trench (NT) has a depth in the range of 20 nm to 1 μm, and its width also in the range of 20 nm to 1 μm. Here, since the micro-trench (NT) is caused by the pores (PO) formed during the manufacturing of the anodic oxide film (AL), the width and depth of the micro-trench (NT) have values less than or equal to the range of the diameters of the pores (PO) of the anodic oxide film (AL). Meanwhile, during the manufacturing of the metal structure (MS1) of the first embodiment, during the process of forming the etched portion (EC) in the anodic oxide film (AL), some of the pores (PO) of the anodic oxide film (AL) may be crushed together by the etching service, thereby forming at least some micro-trench (NT) having a depth greater than the range of the diameters of the pores (PO) formed during the anodic oxidation.
[0044] An anodic oxide film (AL) contains numerous pores (PO), and at least a portion of the anodic oxide film (AL) is etched to form an etched portion (EC), and a metal filling is formed in the etched portion (EC) by metal plating, so that a micro-trench (NT) is formed in the inner wall (IW) of the through hole (PH) by contact with the pores (PO) of the anodic oxide film (AL). Such a micro-trench (NT) has the effect of increasing the surface area of the through hole (PH).
[0045] An insulating film (FL) is provided in the form of a thin film on the inner wall (IW) of the through hole (PH). The insulating film (FL) has a width and a depth and extends in the thickness direction of the body (BD) along the micro trench (NT) formed on the inner wall (IW) of the through hole (PH) and is provided in the circumferential direction of the through hole (PH). In other words, the insulating film (FL) covers the surface of the micro trench (NT) along the shape of the micro trench (NT) and is continuously provided along the circumferential direction of the through hole (PH) from the inner wall (IW) of the through hole (PH).
[0046] An insulating film (FL) is provided in the first through hole (PH1) of the body (BD), and is not provided in the second through hole (PH2). In other words, the insulating film (FL) is provided in at least one through hole (PH) among the plurality of through holes (PH) of the body (BD). Accordingly, the metal structure (MS1) of the first embodiment has a first through hole (PH1) in which an insulating film (FL) is formed, and a second through hole (PH2) in which an insulating film (FL) is not formed.
[0047] The micro-trench (NT) increases the surface area of the through hole (PH) of the body (BD), and an insulating film (FL) is provided along the micro-trench (NT) to cover the micro-trench (NT). Accordingly, the bonding strength of the insulating film (FL) with the body (BD) can be improved.
[0048] In other words, the metal structure (MS1) of the first embodiment has an insulating film (FL) formed along the micro-trench (NT) in the through-hole (PH) of the body (BD) whose inner wall (IW) has a large surface area due to the micro-trench (NT). Therefore, even if the metal structure (MS1) of the first embodiment separately forms the insulating film (FL) on the inner wall (IW) of the through-hole (PH) of the body (BD), the problem of peeling of the insulating film (FL) can be minimized due to the high contact strength between the body (BD) and the insulating film (FL).
[0049] The metal structure (MS1) of the first embodiment, when used as a guide plate (GP), has improved frequency characteristics in high-frequency characteristic inspection.
[0050] Specifically, when the metal structure (MS1) of the first embodiment is used as a guide plate (GP), an electrically conductive contact pin (EP) is inserted into a through hole (PH). At this time, the electrically conductive contact pin (EP) includes a signal pin (SG) that transmits an input / output signal, a ground pin (GR) that transmits a ground signal, and a power pin (PW) that transmits a power signal.
[0051] The signal pin (SG) is inserted into the first through hole (PH1) in which an insulating film (FL) is formed.
[0052] Meanwhile, the ground pin (GR) and power pin (PW) are inserted into the second through hole (PH2) where the insulating film (FL) is not formed.
[0053] Many electrically conductive contact pins (EP), which are intended to carry not only power signals but also ground signals, introduce noise into the operational signals, which are input / output signals, which limits the performance of the probe card (PC) as a whole, especially the frequency performance.
[0054] However, according to the present invention, the ground pin (GR) and the power pin (PW) are electrically connected to the metal part (MP), so that noise is not generated in the operating signal of the signal pin (SG), thereby improving the high-frequency characteristic inspection performance.
[0055] Hereinafter, a method for manufacturing a metal structure (MS1) of a first embodiment will be described with reference to FIGS. 2A to 2L. The method for manufacturing a metal structure (MS1) of the first embodiment includes a step of preparing an anodic oxide film (AL), a step of forming an etched portion (EC) by etching the anodic oxide film (AL), a step of forming a first through-hole (PH1) by etching the anodic oxide film (AL), and a step of forming an insulating film (FL) on an inner wall (IW) of the first through-hole (PH1).
[0056] First, a step is performed to prepare an anodic oxide film (AL).
[0057] An anodic oxide film (AL) refers to a film formed by anodizing a base metal, and pores (PO) refer to holes formed in the process of forming an anodic oxide film (AL) by anodizing a metal. For example, if the base metal is aluminum (Al) or an aluminum alloy, an anodic oxide film (AL) made of aluminum oxide (Al2O3) is formed on the surface of the base metal when the base metal is anodized. However, the base metal is not limited thereto, and includes Ta, Nb, Ti, Zr, Hf, W, Sb, or alloys thereof.
[0058] The anodic oxide film (AL) formed as above is vertically divided into a barrier layer (BL) without pores (PO) formed inside, and a porous layer (PL) with pores (PO) formed inside. When the base material on which the anodic oxide film (AL) having the barrier layer (BL) and the porous layer (PL) is formed on the surface is removed, only the anodic oxide film (AL) made of aluminum oxide (Al2O3) remains. The anodic oxide film (AL) may be formed in a structure in which the barrier layer (BL) formed during anodic oxidation is removed and penetrates the upper and lower portions of the pores (PO), or may be formed in a structure in which the barrier layer (BL) formed during anodic oxidation remains as it is and seals one end of the upper and lower portions of the pores (PO). As an example, FIGS. 2a to 2j illustrate an anodic oxide film (AL) having a structure in which the barrier layer (BL) seals one end of the pores (PO).
[0059] Then, referring to Fig. 2a, an anodic oxide film (AL) is formed on the seed layer (SD), and a first photoresist layer (PR1) is formed on the anodic oxide film (AL). The first photoresist layer (PR1) is formed continuously on one surface of the anodic oxide film (AL).
[0060] Then, referring to FIG. 2b, a step of patterning the first photoresist layer (PR1) to form a first patterning region (PN1) is performed.
[0061] The first photoresist layer (PR1) is patterned through an exposure and development process. As a result, a discontinuous first photoresist layer (PR1) is formed on one surface of the anodic oxide film (AL) by a first patterning region (PN1).
[0062] Then, referring to Fig. 2c, a step of etching the anodic oxide film (AL) to form an etched portion (EC) is performed.
[0063] Specifically, a process of forming an etched portion (EC) by etching the anodic oxide film (AL) exposed by the first patterning area (PN1) using an etching solution is performed.
[0064] After forming the etching section (EC), an unpatterned first photoresist layer (PR1) and an anodic oxide film (AL) corresponding to the first photoresist layer (PR1) exist on the seed layer (SD).
[0065] On the width direction (±x direction) side of the anodic oxide film (AL) located under the unpatterned first photoresist layer (PR1), a micro trench (NT) is formed by etching the anodic oxide film (AL) at a position corresponding to the first patterning region (PN1).
[0066] Then, referring to FIG. 2d, a step of performing metal plating using a seed layer (SD) to provide a metal portion (MP) in the etched portion (EC) is performed.
[0067] The metal portion (MP) is composed of at least one of rhodium (Rd), platinum (Pt), iridium (Ir), palladium (Pd), nickel (Ni), manganese (Mn), tungsten (W), phosphorus (Ph) or an alloy thereof, or a palladium-cobalt (PdCo) alloy, a palladium-nickel (PdNi) alloy or a nickel-phosphorus (NiPh) alloy, a nickel-manganese (NiMn), a nickel-cobalt (NiCo) or a nickel-tungsten (NiW) alloy, copper (Cu), silver (Ag), gold (Au) or an alloy thereof. However, the metal constituting the metal portion (MP) is not limited thereto, and any metal that can improve the physical, chemical and / or electrical properties of the metal structure (MS1) of the first embodiment is included.
[0068] The metal part (MP) may be provided in an etching part (EC) and may be provided in a form of continuous connection, surrounding the anodic oxide film (AL) at a position corresponding to the unpatterned first photoresist layer (PR1).
[0069] Then, referring to FIG. 2e, a step of removing the unpatterned first photoresist layer (PR1) is performed.
[0070] With the first photoresist layer (PR1) completely removed, a metal portion (MP) is formed in a form that surrounds and is continuously connected to a plurality of anodic oxide films (AL). In other words, a plurality of anodic oxide films (AL) are formed on the inside of the metal portion (MP) with a distance therebetween. In Fig. 2e, as an example, three anodic oxide films (AL) are formed on the inside of the metal portion (MP) in the width direction (±x direction) with a distance therebetween. On the seed layer (SD), a metal portion (MP) and a plurality of anodic oxide films (AL) formed on the inside of the metal portion (MP) and surrounded by the metal portion (MP) are formed.
[0071] Once the metal plating process is completed, a planarization process can be performed. The planarization process removes any metal protruding from the upper surface of the anodic oxide film (AL) through a chemical mechanical polishing (CMP) process. The method for manufacturing the metal structure (MS1) of the first embodiment preferably includes performing the metal plating process and the step of removing the unpatterned first photoresist layer (PR1), followed by the planarization process.
[0072] Then, referring to FIG. 2f, a step of continuously forming a second photoresist layer (PR2) on one surface (upper surface) of the metal portion (MP) and the anodic oxide film (AL) in the thickness direction (±z direction) is performed.
[0073] Then, referring to FIG. 2g, a step of forming a second patterning region (PN2) by patterning a second photoresist layer (PR2) at a position corresponding to at least one of the plurality of anodic oxide films (AL) provided on the inner side of the metal part (MP) is performed.
[0074] In FIG. 2g, as an example, a second photoresist layer (PR2) at a position corresponding to the first anodic oxide film (AL1) provided at the far left in the width direction (±x direction) is patterned to form a second patterning region (PN2).
[0075] Then, referring to FIG. 2h, a step of forming a first through hole (PH1) by etching the first anodic oxide film (AL1) exposed by the second patterning region (PN2) is performed.
[0076] The first through-hole (PH1) is formed by etching the first anodic oxide film (AL1) having a micro-trench (NT) on the side in the width direction (±x direction). Therefore, the first through-hole (PH1) is formed on the inner side of the metal part (MP) that is in direct contact with the first anodic oxide film (AL1) and surrounds the first anodic oxide film (AL1) along the circumferential direction. Since the first through-hole (PH1) is formed at a location where the first anodic oxide film (AL1) having the micro-trench (NT) on the side is etched, the micro-trench (NT) is formed on the inner wall (IW) in the same shape as the micro-trench (NT) of the first anodic oxide film (AL1).
[0077] More specifically, the first anodic oxide film (AL1) at a position corresponding to the second patterning area (PN2) is etched using an etching solution. As a result, the seed layer (SD) at a position corresponding to the second patterning area (PN2) is exposed, and a first through hole (PH1) having a micro-trench (NT) of the same shape as the micro-trench (NT) provided on the side surface of the first anodic oxide film (AL1) is formed on the inner wall (IW).
[0078] Then, referring to FIG. 2i, a step of forming an insulating film (FL) on the inner wall (IW) of the first through hole (PH1) is performed.
[0079] The insulating film (FL) can be formed in the form of parylene by depositing parylene through chemical vapor deposition (CVD).
[0080] Alternatively, the insulating film (FL) may be formed by a deposition method in which a cycle of adsorbing a precursor gas, supplying a reactant gas, and forming a monoatomic layer through chemical substitution of the precursor gas and the reactant gas is repeatedly performed, such that a single monoatomic layer having a thin thickness is formed each time the cycle is performed. In this case, the insulating film (FL) may include at least one of an aluminum oxide layer, an yttrium oxide layer, a hafnium oxide layer, a silicon oxide layer, an erbium oxide layer, a zirconium oxide layer, a fluoride layer, a transition metal layer, a titanium nitride layer, a tantalum nitride layer, and a zirconium nitride layer, depending on the composition of the precursor gas and the reactant gas.
[0081] The method of forming an insulating film (FL) is not limited to this, and includes all methods of forming a thin film by depositing an insulating material on a surface.
[0082] Specifically, an insulating material is deposited on the surface of a second photoresist layer (PR2) including a through-hole having the same cross-sectional shape as the first through-hole (PH1) in at least a portion of the first through-hole (PH1). The through-hole is in communication with the first through-hole (PH1). The insulating material is deposited on the exposed surface of the second photoresist layer (PR2), and at a position where the through-hole and the first through-hole (PH1) are provided, the insulating material is deposited on a side surface of the second photoresist layer (PR2) forming the through-hole and an inner wall (IW) of the first through-hole (PH1), and is deposited on one surface of the seed layer (SD) exposed by the first through-hole (PH1).
[0083] In other words, an insulating material is deposited on a surface including a side surface of the second photoresist layer (PR2) forming the penetration portion and an exposed upper surface of the unpatterned second photoresist layer (PR2), an inner wall (IW) of the first through-hole (PH1), and at least a portion of a surface of the seed layer (SD) exposed by the first through-hole (PH1), so that an insulating film (FL) is continuously formed on the surface of the second photoresist layer (PR2), the inner wall (IW) of the first through-hole (PH1), and at least one surface of the exposed seed layer (SD). As a result, a first through-hole (PH1) including an insulating film (FL) is provided.
[0084] Then, referring to FIG. 2j, in the step of forming the second patterning region (PN2), a step of removing the second photoresist layer (PR2) and the insulating film (FL) formed on the surface thereof at positions corresponding to the plurality of anodic oxide films (AL) that are not exposed by the unpatterned second photoresist layer (PR2) is performed.
[0085] Referring to Fig. 2j, a first anodic oxide film (AL1) is provided with a metal portion (MP) therebetween, and a second anodic oxide film (AL2) and a third anodic oxide film (AL3) are provided at a distance in the width direction (±x direction). A step of removing the second photoresist layer (PR2) and the insulating film (FL) formed on the surface thereof at positions corresponding to each of the second and third anodic oxide films (AL2, AL3) is performed.
[0086] The second photoresist layer (PR2) at a corresponding position corresponding to the anodic oxide film (AL) and the insulating film (FL) formed on its surface can be selectively removed using a laser irradiation method. The method for removing the second photoresist layer (PR2) and the insulating film (FL) can be any method for removing a photosensitive material and an insulating material.
[0087] The second photoresist layer (PR2) at a position corresponding to the anodic oxide film (AL) and the insulating film (FL) formed on its surface can preferably be removed simultaneously. Alternatively, the insulating film (FL) exposed to the outside can be removed first, and then the second photoresist layer (PR2) at a position corresponding to the removed insulating film (FL) can be removed sequentially, thereby removing the insulating film (FL) and the second photoresist layer (PR2).
[0088] By removing the second photoresist layer (PR2) corresponding to the anodic oxide film (AL) and the insulating film (FL) formed on its surface, the anodic oxide film (AL) is exposed. In Fig. 2j, two anodic oxide films (AL) are exposed.
[0089] Then, referring to FIG. 2k, a step of etching the exposed anodic oxide film (AL) to form a second through hole (PH2) is performed. In FIG. 2k, the exposed second anodic oxide film (AL2) and the third anodic oxide film (AL3) are each etched to form one second through hole (PH2) at a location where the second anodic oxide film (AL2) was present, and one second through hole (PH2) is formed at a location where the third anodic oxide film (AL3) was present. In other words, the second and third anodic oxide films (AL2, AL3) are each etched to form two second through holes (PH2).
[0090] The second through hole (PH2) is formed after the step of forming an insulating film (FL) on the inner wall (IW) of the first through hole (PH1), and thus does not have an insulating film (FL) on its inner wall. Accordingly, the second through hole (PH2) is formed without an insulating film (FL). However, since the second through hole (PH2) is also formed at a location where the anodic oxide film (AL) has been removed, the inner wall has a micro-trench (NT) of the same shape due to the micro-trench (NT) on the side of the anodic oxide film (AL).
[0091] Then, referring to FIG. 2l, a step of removing the second photoresist layer (PR2) provided on one surface of the metal part (MP) and the insulating film (FL) formed on the surface is performed.
[0092] The second photoresist layer (PR2) provided on one side of the metal part (MP) and the insulating film (FL) on the surface thereof can be removed by a laser irradiation method and a method of removing a photosensitive material and an insulating material, or a chemical-mechanical polishing (CMP) method.
[0093] Afterwards, when the seed layer (SD) and the insulating film (FL) formed on a part of the seed layer (SD) are removed, the metal structure (MS1) of the first embodiment is manufactured.
[0094] Figure 4 is a drawing showing a first modified example of the metal structure (MS1) of the first embodiment.
[0095] The first variation example differs from the first embodiment in that the body (BD) is composed of multiple metal layers (MT) laminated together. Since the remaining components are identical, the following description will focus on the characteristic components, and descriptions of identical or similar components will be omitted as much as possible.
[0096] A first modified example includes a body (BD) formed by stacking a plurality of metal layers (MT) of the same material, and an insulating film (FL) formed along a micro-trench of the through hole (PH) on the inner wall of the through hole (PH) of the body (BD).
[0097] In Fig. 4, as an example, three metal layers (MT) are laminated in the thickness direction (±z direction) to form a body (BD). The number of laminated metal layers (MT) is not limited thereto, and the body (BD) may be formed by laminating at least two or more layers.
[0098] Each metal layer (MT) can be composed of a metal material of the same type.
[0099] Specifically, the metal layer (MT) may be composed of at least one of rhodium (Rd), platinum (Pt), iridium (Ir), palladium (Pd), nickel (Ni), manganese (Mn), tungsten (W), phosphorus (Ph), or an alloy thereof, or a palladium-cobalt (PdCo) alloy, a palladium-nickel (PdNi) alloy, a nickel-phosphorus (NiPh) alloy, a nickel-manganese (NiMn), a nickel-cobalt (NiCo), or a nickel-tungsten (NiW) alloy.
[0100] Alternatively, the metal layer (MT) may be composed of at least one of copper (Cu), silver (Ag), gold (Au), or an alloy thereof.
[0101] Each metal layer (MT) includes a plurality of holes (HO) penetrating the metal layer (MT) from above and below.
[0102] The holes (HO) of each metal layer (MT) are formed at positions corresponding to each other in the thickness direction (±z direction). Accordingly, when multiple metal layers (MT) are laminated in the thickness direction (±z direction), the holes (HO) of each metal layer (MT) are connected to each other.
[0103] The metal layer (MT) can be manufactured by the manufacturing method of the metal structure (MS1) of the first embodiment. Accordingly, a micro-trench (NT) exists on the inner wall of the hole (HO) of the metal layer (MT).
[0104] An insulating film (FL) is provided on the inner wall of at least one hole (HO) among a plurality of holes (HO) of a metal layer (MT). Accordingly, the metal layer (MT) has a first hole (HO1) provided with an insulating film (FL) and a second hole (HO2) not provided with an insulating film (FL).
[0105] Each metal layer (MT) is positioned so that the first holes (HO1) provided with an insulating film (FL) correspond to each other when stacked in the thickness direction (±z direction), and the second holes (HO2) not provided with an insulating film (FL) correspond to each other.
[0106] The first variation example has a first through hole (PH1) provided with an insulating film (FL) by having first holes (HO1) of each metal layer (MT) positioned correspondingly and communicating with each other. In addition, the first through hole (PH2) of each metal layer (MT) has a second through hole (PH2) not provided with an insulating film (FL) by having second holes (HO2) of each metal layer (MT) positioned correspondingly and communicating with each other.
[0107] Each metal layer (MT) can be bonded by a bonding layer having an opening corresponding to the hole (HO) of each metal layer (MT) between the metal layers (MT), but is not limited thereto. The metal layers (MT) can be bonded by a bonding method. The method of bonding between the metal layers (MT) includes all methods of bonding metal materials.
[0108] The first variation example can further improve the durability of the body (BD) by forming the body (BD) by stacking multiple metal layers (MT).
[0109] Figure 5a is a diagram showing a second-first variation example of the metal structure (MS1) of the first embodiment.
[0110] The second variation example differs from the first embodiment in that the body (BD) is composed of multiple metal layers (MT) laminated together. Aside from this, the remaining components are identical. Therefore, the following description will focus on the characteristic components, and descriptions of identical or similar components will be omitted as much as possible.
[0111] The second-first variation example includes a body (BD) formed by stacking multiple metal layers (MT) of different materials, and an insulating film (FL) formed along a micro-trench (NT) of a through hole (PH) on an inner wall (IW) of a through hole (PH) of the body (BD).
[0112] In Fig. 5a, as an example, three metal layers (MT) are laminated in the thickness direction (±z direction) to form a body (BD). The number of laminated metal layers (MT) is not limited thereto, and the body (BD) may be formed by laminating at least two or more layers.
[0113] The multiple metal layers (MT) may be composed of different metal materials.
[0114] Specifically, at least one of the plurality of metal layers (MT) may be configured to include at least one of rhodium (Rd), platinum (Pt), iridium (Ir), palladium (Pd), nickel (Ni), manganese (Mn), tungsten (W), phosphorus (Ph) or an alloy thereof, or a palladium-cobalt (PdCo) alloy, a palladium-nickel (PdNi) alloy, a nickel-phosphorus (NiPh) alloy, a nickel-manganese (NiMn), a nickel-cobalt (NiCo), or a nickel-tungsten (NiW) alloy.
[0115] The remaining one of the plurality of metal layers (MT) may be composed of at least one of copper (Cu), silver (Ag), gold (Au) or an alloy thereof.
[0116] A second variation example is, as an example, a first metal layer (MT1) provided at the uppermost portion in the thickness direction (±z direction) and a third metal layer (MT3) provided at the lowermost portion are composed of at least one of rhodium (Rd), platinum (Pt), iridium (Ir), palladium (Pd), nickel (Ni), manganese (Mn), tungsten (W), phosphorus (Ph), or an alloy thereof, or a palladium-cobalt (PdCo) alloy, a palladium-nickel (PdNi) alloy, a nickel-phosphorus (NiPh) alloy, a nickel-manganese (NiMn), a nickel-cobalt (NiCo), or a nickel-tungsten (NiW) alloy.
[0117] Since the first and third metal layers (MT) are metal layers (MT1 and MT3) exposed to the outside, it is preferable that they be composed of metals with excellent durability and rigidity. Accordingly, in the second variation example, the first and third metal layers (MT) are composed of metal materials with relatively excellent rigidity.
[0118] The second metal layer (MT2) is provided between the first and third metal layers (MT1 and MT3). In other words, the second metal layer (MT2) is not exposed to the outside by the first and third metal layers (MT1 and MT3) but is interposed between the first and third metal layers (MT1 and MT3). In the second-first variation example, the second metal layer (MT2) is formed of a metal having relatively high electrical conductivity. Specifically, the second metal layer (MT2) is formed of at least one of copper (Cu), silver (Ag), gold (Au), or an alloy thereof.
[0119] Each of the first to third metal layers (MT1, MT2, MT3) includes a plurality of holes (HO) penetrating the upper and lower metal layers (MT1, MT2, MT3).
[0120] The holes (HO) of each metal layer (MT1, MT2, MT3) are formed at positions corresponding to each other in the thickness direction (±z direction). Accordingly, when multiple metal layers (MT1, MT2, MT3) are laminated in the thickness direction (±z direction), the holes (HO) of each metal layer (MT) are connected to each other.
[0121] A metal layer (MT) including first to third metal layers (MT1, MT2, MT3) can be manufactured by the manufacturing method of the metal structure (MS1) of the first embodiment. Accordingly, a micro-trench (NT) exists in the inner wall of the hole (HO) of the metal layer (MT1, MT2, MT3).
[0122] An insulating film (FL) is provided on the inner wall of at least one hole (HO) among the plurality of holes (HO) of each of the first to third metal layers (MT1, MT2, MT3). Accordingly, the metal layers (MT1, MT2, MT3) have a first hole (HO1) provided with an insulating film (FL) and a second hole (HO2) not provided with an insulating film (FL).
[0123] When the first to third metal layers (MT1, MT2, MT3) are laminated in the thickness direction (±z direction), the first holes (HO1) provided with an insulating film (FL) are positioned so as to correspond to each other, and the second holes (HO2) not provided with an insulating film (FL) are positioned so as to correspond to each other.
[0124] The second variation example has a first through hole (PH1) provided with an insulating film (FL) by having the first holes (HO1) of the first to third metal layers (MT1, MT2, MT3) positioned correspondingly and communicating with each other. In addition, the second through hole (PH2) not provided with an insulating film (FL) is provided by having the second holes (HO2) of the respective metal layers (MT1, MT2, MT3) positioned correspondingly and communicating with each other.
[0125] The first to third metal layers (MT1, MT2, MT3) can be bonded by a bonding layer having an opening corresponding to the hole (HO) of each metal layer (MT1, MT2, MT3) between each metal layer (MT1, MT2, MT3), but is not limited thereto. The first to third metal layers (MT1, MT2, MT3) can be bonded by a method of bonding metal materials of different materials. The method of bonding between the metal layers (MT1, MT2, MT3) of different materials includes all methods of bonding metal materials of different materials.
[0126] Figure 5b is a diagram showing a second-second variation example of the metal structure (MS1) of the first embodiment.
[0127] The second variation example differs from the second variation example in that the body (BD) is formed by laminating at least one metal layer (MT) and at least one anodic oxide layer (MT2'). Since the remaining components are identical, the following description will focus on the characteristic components, and descriptions of identical or similar components will be omitted as much as possible.
[0128] A second-2 variation example includes a body (BD) formed by stacking at least one metal layer (MT) and at least one anodic oxide layer (MT2'), and an insulating film (FL) formed along a micro-trench (NT) of a through hole (PH) on an inner wall (IW) of the through hole (PH) of the body (BD).
[0129] In Fig. 5b, as an example, two metal layers (MT1, MT3) are provided at the uppermost and lowermost positions in the thickness direction (±z direction), and an anodic oxide layer (MT2') is provided between the metal layers (MT1, MT3), so that a body (BD) is formed of three heterogeneous layers. The number of metal layers (MT1, MT3) and the number of anodic oxide layers (MT2') constituting the body (BD) are not limited thereto, and the body (BD) may be formed as a heterogeneous material laminated structure in which at least one metal layer (MT) and at least one anodic oxide layer (MT2) are laminated.
[0130] The multiple metal layers (MT) may be composed of metal materials of different or similar materials. The second variation example of Fig. 5b illustrates that the metal layers (MT1, MT3) are composed of metal materials of the same type.
[0131] The second-2nd variation example, as an example, includes an anodic oxide layer (MT2') between the first metal layer (MT1) provided at the topmost portion in the thickness direction (±z direction) and the third metal layer (MT3) provided at the bottommost portion.
[0132] The anodic oxide layer (MT2') can be manufactured relatively simply compared to the metal layer (MT) by performing the steps of preparing an anodic oxide layer (AL), forming a first photoresist layer (PR1) on one surface of the anodic oxide layer (AL) to form a first patterning area (PN1), and then etching the anodic oxide layer (AL) through the first patterning area (PN1) to form a through hole (AO).
[0133] A plurality of through holes (AO) are provided by separately etching the anodic oxide film (AL) so that the through holes have a diameter larger than the diameter of the pores (PO) of the anodic oxide film (AL). The diameter of the through holes (AO) is the same as the diameter of the holes (HO) of the metal layer (MT).
[0134] The second variation example has the same number of holes (HO) in the metal layer (MT) and the same number of holes (AO) in the anodic oxide layer (MT2'). As an example, Fig. 5b shows that the metal layer (MT) has three holes (HO) and the anodic oxide layer (MT2') also has three holes (AO). The number of holes (HO) in the metal layer (MT) and the holes (AO) in the anodic oxide layer (MT2') is not limited thereto.
[0135] In the second variation example, the through hole (AO) of the anodic oxide layer (MT2') is positioned to correspond to the hole (HO) of the metal layer (MT) so that the through hole (AO) of the anodic oxide layer (MT2') and the hole (HO) of the metal layer (MT) are connected to each other. Accordingly, the second variation example has a through hole (PH) by connecting the through hole (AO) of the anodic oxide layer (MT2') and the hole (HO) of the metal layer (MT).
[0136] The inner wall of the through hole (AO) and the hole (HO) of the metal layer (MT) is provided with a micro trench (NT).
[0137] Since the anodic oxide layer (MT2') has insulating properties, the step of providing a separate insulating film (FL) on the inner wall of the through hole (AO) can be omitted. As an example, the second-2 variation example of Fig. 5b is illustrated in which the insulating film (FL) is not provided on the inner wall of the through hole (AO).
[0138] The method of bonding between the anodic oxide layer (MT2') and the metal layer (MT) may be a method of bonding through a bonding layer including a bonding film and an adhesive, and includes all methods of bonding dissimilar materials such as a metal and an anodic oxide layer (AL).
[0139] The second-second variation example has an anodic oxide layer (MT2') between the first and third metal layers (MT1, MT2), so that it can be manufactured more efficiently and more advantageously in terms of manufacturing cost compared to having all of the multiple layers constituting the body (BD) as metal layers (MT).
[0140] In addition, when using the 2nd-2nd variation example as a guide plate, a body (BD) is formed by stacking a metal layer (MT) and an anodic oxide layer (MT2'), so that sufficient thickness can be secured to function as a guide plate.
[0141] In addition, the anodic oxide film (AL) has a smaller coefficient of thermal expansion than the metal. Therefore, the second-second variation example can minimize the change in the position of the through hole (PH) depending on the temperature in the laminated structure of the metal layer (MT) and the anodic oxide film layer (MT2').
[0142] In the second-2nd variation example, as an example, the anodic oxide layer (MT2') is provided between the first and third metal layers (MT1, MT3) so as to be unexposed by the metal layers (MT1, MT3), but the position at which the anodic oxide layer (MT2') is provided is not limited to this. The anodic oxide layer (MT2') may be provided at the uppermost part in the thickness direction (±z direction) of the body (BD), or may be provided at the lowermost part.
[0143] Alternatively, the anodic oxide layer (MT2') may be provided at the uppermost and lowermost portions of the body (BD) in the thickness direction (±z direction). In this case, the body (BD) may be formed with a structure in which the anodic oxide layer (MT2') is provided at the uppermost and lower portions of the body (BD) in the thickness direction (±z direction), and at least one metal layer (MT) is provided between the anodic oxide layers (MT2').
[0144] Figure 5c is a diagram showing a second-third variation example of the metal structure (MS1) of the first embodiment.
[0145] The second-third variation example differs from the second-first variation example in that the body (BD) is formed by laminating at least one metal layer (MT) and at least one ceramic layer (CR), or by laminating at least one metal layer (MT) and at least one polymer layer (PM). Since the remaining components are the same, the following description will focus on the characteristic components, and descriptions of identical or similar components will be omitted as much as possible.
[0146] The body (BD) of the second-third variant is formed by laminating at least one metal layer (MT) and at least one ceramic layer (CR). Here, an insulating film (FL) is provided on the inner wall of at least one hole (HO) among the plurality of holes (HO) of the metal layer (MT). Accordingly, the metal layer (MT) has a first hole (HO1) provided with an insulating film (FL) and a second hole (HO2) not provided with an insulating film (FL).
[0147] As an example, FIG. 5c illustrates a body (BD) having a structure in which two metal layers (MT1, MT3) are provided at the uppermost and lowermost positions in the thickness direction (±z direction), and a ceramic layer (CR) is provided between the metal layers (MT1, MT3), thereby forming a body (BD) having a three-layered structure of different materials. The number of metal layers (MT1, MT3) and the number of ceramic layers (CR) constituting the body (BD) are not limited thereto, and the body (BD) may be formed as a layered structure of different materials by stacking at least one metal layer (MT) and at least one ceramic layer (CR).
[0148] As an example of the 2nd-3rd variant, a ceramic layer (CR) may be provided between the first metal layer (MT1) provided at the topmost portion in the thickness direction (±z direction) and the third metal layer (MT3) provided at the bottommost portion.
[0149] The ceramic layer (CR) can be manufactured relatively simply compared to the metal layer (MT) by forming holes (CO) by any method that penetrates the ceramic material from top to bottom.
[0150] The second-third variation example has the same number of holes (HO) in the metal layer (MT) and the same number of holes (CO) in the ceramic layer (CR). As an example, Fig. 5c shows that the metal layer (MT) has three holes (HO) and the ceramic layer (CR) also has three holes (CO). The number of holes (HO) in the metal layer (MT) and the holes (AO) in the ceramic layer (CR) is not limited thereto.
[0151] In the second-third variation example, the hole (CO) of the ceramic layer (CR) is positioned to correspond to the hole (HO) of the metal layer (MT) so that the hole (CO) of the ceramic layer (CR) and the hole (HO) of the metal layer (MT) are connected. Accordingly, the second-third variation example has a through hole (PH) by connecting the hole (CO) of the ceramic layer (CR) and the hole (HO) of the metal layer (MT).
[0152] The inner wall of the hole (HO) of the metal layer (MT) is provided with a micro-trench (NT).
[0153] Since the ceramic layer (CR) has insulating properties, the step of providing a separate insulating film (FL) on the inner wall of the hole (CO) of the ceramic layer (CR) can be omitted. As an example, the second-third variation example of Fig. 5c is illustrated in which the insulating film (FL) is not provided on the inner wall of the hole (CO) of the ceramic layer (CR).
[0154] The method of bonding between the ceramic layer (CR) and the metal layer (MT) may be a method of bonding through a bonding layer including a bonding film and an adhesive, and includes all methods of bonding different materials of the metal layer (CT) and the ceramic layer (CR).
[0155] In contrast, the 2nd-3rd variant example may include, as an example, a polymer layer (PM) between the first metal layer (MT1) provided at the topmost position in the thickness direction (±z direction) and the third metal layer (MT3) provided at the bottommost position.
[0156] The polymer layer (PM) can be manufactured relatively simply compared to the metal layer (MT) by providing holes (MO) through any method that penetrates the polymer material from top to bottom to form holes.
[0157] The second-third variation example has the same number of holes (HO) in the metal layer (MT) and the same number of holes (MO) in the polymer layer (PM). As an example, Fig. 5c illustrates that the metal layer (MT) has three holes (HO) and the polymer layer (PM) also has three holes (MO). The number of holes (HO) in the metal layer (MT) and the holes (MO) in the polymer layer (PM) is not limited thereto.
[0158] The second-third variation example positions the hole (MO) of the polymer layer (PM) to correspond to the hole (HO) of the metal layer (MT) so that the hole (MO) of the polymer layer (PM) and the hole (HO) of the metal layer (MT) are in communication. Accordingly, the second-third variation example has a through hole (PH) by connecting the hole (MO) of the polymer layer (PM) and the hole (HO) of the metal layer (MT).
[0159] The inner wall of the hole (HO) of the metal layer (MT) is provided with a micro-trench (NT).
[0160] Since the polymer layer (PM) has insulating properties, the step of providing a separate insulating film (FL) on the inner wall of the hole (MO) of the polymer layer (PM) can be omitted. As an example, the second-third variation example of Fig. 5c is illustrated in which the insulating film (FL) is not provided on the inner wall of the hole (MO) of the polymer layer (PM).
[0161] The method of bonding between the polymer layer (PM) and the metal layer (MT) may be a method of bonding through a bonding layer including a bonding film and an adhesive, and includes all methods of bonding different materials of the metal layer (CT) and the polymer layer (PM).
[0162] Figure 6 is a plan view of a metal structure (MS2) of the second embodiment.
[0163] The metal structure (MS2) of the second embodiment differs from the metal structure (MS1) of the first embodiment in that at least a portion of the body (BD) is composed of an anodic oxide film (AL) material, and the remaining portion is composed of a metal (M) material, such that the anodic oxide film (AL) functions as an insulating film (FL). Since the remaining components are the same, the following description will focus on the characteristic components, and descriptions of identical or similar components will be omitted as much as possible.
[0164] The metal structure (MS2) of the second embodiment includes a body (BD) having a plurality of through holes (PH'), and at least a portion of the body (BD) is made of an anodic oxide film (AL) material, and the remaining portion is made of a metal (M) material.
[0165] The metal structure (MS2) of the second embodiment has an anodic oxide film portion (AP) made of an anodic oxide film (AL) material and a metal portion (MP) made of a metal (M) material, and at least one through hole (PH').
[0166] In Fig. 6, it is shown that four through holes (PH') are provided in the anodic oxide film portion (AP) and four through holes (PH') are provided in the metal portion (MP).
[0167] The anodic oxide film portion (AP) is provided on the inner side of the metal portion (MP) in the width direction (±x direction).
[0168] A through hole (PH') provided in an anodic oxide film portion (AP) composed of an anodic oxide film (AL) material and a metal portion (MP) composed of a metal (M) material has a plurality of micro-trenches (NT) on its inner wall (IW).
[0169] The anodic oxide film portion (AP) has micro-trench (NT) not only on the inner wall (IW) of the through hole (PH') but also at the interface with the metal portion (MP). Therefore, the anodic oxide film portion (AP) can be bonded to the metal portion (MP) with high bonding strength, thereby minimizing the problem of delamination.
[0170] The metal structure (MS2) of the second embodiment uses an anodic oxide film (AL) having insulating properties so that the inner wall (IW) of the through hole (PH') formed in the anodic oxide film portion (AP) is composed of an insulating material. Accordingly, the metal structure (MS2) of the second embodiment may not separately include the insulating film (FL) of the first embodiment on the inner wall (IW) of the through hole (PH').
[0171] The metal structure (MS2) of the second embodiment, when used as a guide plate (GP), has improved frequency characteristics in high-frequency characteristic inspection.
[0172] When the metal structure (MS2) of the second embodiment is used as a guide plate (GP), an electrically conductive contact pin (EP) is inserted into a through hole (PH'). At this time, the electrically conductive contact pin (EP) includes a signal pin (SG) for transmitting an input / output signal, a ground pin (GR) for transmitting a ground signal, and a power pin (PW) for transmitting a power signal.
[0173] The signal pin (SG) is inserted into a through hole (PH') formed in the anodic oxide film portion (AP). The inner wall (IW) of the through hole (PH') formed in the anodic oxide film portion (AP) is composed of an anodic oxide film (AL) material, and thus has insulating properties even without a separate insulating film (FL).
[0174] Meanwhile, the ground pin (GR) or power pin can be installed by being inserted into a through hole (PH') formed in the metal part (MP).
[0175] Many electrically conductive contact pins (EP), which are intended to carry not only power signals but also ground signals, introduce noise into the operational signals, which are input / output signals, which limits the performance of the probe card (PC) as a whole, especially the frequency performance.
[0176] However, according to the present invention, the ground pin (GR) and the power pin (PW) are electrically connected to the metal part (MP), so that noise is not generated in the operating signal of the signal pin (SG), thereby improving the high-frequency characteristic inspection performance.
[0177] The metal structure (MS2) of the second embodiment comprises a body (BD) including an anodic oxide film portion (AP) and a metal portion (MP), and has a plurality of through holes (PH') by forming through holes (PH') in each of the anodic oxide film portion (AP) and the metal portion (MP). Accordingly, the metal structure (MS2) of the second embodiment may not have a separate insulating film (FL) in the through holes (PH').
[0178] Figures 7a to 7i are flowcharts of a method for manufacturing a metal structure (MS2) of a second embodiment. In Figures 7a to 7i, as an example, one through hole (PH') is shown to be formed in each of the anodic oxide film portion (AP) and the metal portion (MP).
[0179] In the method for manufacturing the metal structure (MS2) of the second embodiment, a detailed description of the steps performed in the same manner as the method for manufacturing the metal structure (MS1) of the first embodiment is omitted, and the description focuses on the characteristic components.
[0180] A method for manufacturing a metal structure (MS2) of the second embodiment includes a step of preparing an anodic oxide film (AL), a step of etching the anodic oxide film (AL) to form an etched portion (EC), a step of forming a first through hole (PH1') in the anodic oxide film (AL), and a step of forming a second through hole (PH2') in the metal portion (MP).
[0181] First, the step of preparing the anodic oxide film (AL) is performed.
[0182] Then, referring to FIG. 7a, a step of providing an anodic oxide film (AL) on a seed layer (SD) and providing a first photoresist layer (PR1) on one surface of the anodic oxide film (AL) is performed.
[0183] Then, referring to FIG. 7b, a step of patterning the first photoresist layer (PR1) at a position corresponding to the first region (FD1) of the anodic oxide film (AL) to form a first patterning region (PN1) is performed.
[0184] Accordingly, the anodic oxide film (AL) is divided into a first region (FD1) including a first patterning region (PN1) and a second region (FD2) not including the first patterning region (PN1).
[0185] Then, referring to FIG. 7c, a step of forming an etched portion (EC) by etching the anodic oxide film (AL) exposed by the first patterning region (PN1) corresponding to the first patterning region (PN1) is performed.
[0186] Then, referring to FIG. 7d, a step of performing metal plating using a seed layer (SD) to provide a metal portion (MP) in the etched portion (EC) is performed. The metal portion (MP) is formed by growing a metal (M) on a portion where the anodic oxide film (AL) is etched. Accordingly, a micro-trench (NT) is formed on the side surface of the metal portion (MP) by the anodic oxide film (AL). The micro-trench (NT) on the side surface of the metal portion (MP) forms a large surface area on the side surface of the metal portion (MP), thereby improving the bonding strength between the anodic oxide film (AL) of the second region (FD2) and the metal portion (MP) of the first region (FD1).
[0187] Then, referring to FIG. 7e, a step of removing the first photoresist layer (PR1) of the first region (FD1) and the first photoresist layer (PR1) of the second region (FD2) is performed.
[0188] In the first region (FD1), the remaining first photoresist layer (PR1) that is not patterned among the first photoresist layers (PR1) existing in the first region (FD1) by the first patterning region (PN1) remains.
[0189] In the second region (FD2), a first photoresist layer (PR1) exists covering one surface of the anodic oxide film (AL) located in the second region (FD2) as no patterning is performed.
[0190] Accordingly, a step of removing both the first photoresist layer (PR1) of the first region (FD1) and the first photoresist layer (PR1) of the second region (FD2) is performed.
[0191] Then, referring to FIG. 7f, a step of forming a second photoresist layer (PR2) is performed to continuously cover one surface of the anodic oxide film (AL) and metal portion (MP) included in the first region (FD1) and the anodic oxide film (AL) included in the second region (FD2).
[0192] At this time, the anodic oxide film (AL) included in the first region (FD1) may be located on the inner side in the width direction (±x direction) of the metal portion (MP).
[0193] Then, referring to FIG. 7g, a step of forming a second patterning region (PN2) by patterning a second photoresist layer (PR2) at a position corresponding to the anodic oxide film (AL) of the first region (FD1), and forming a second patterning region (PN2) by patterning a second photoresist layer (PR2) at a position corresponding to at least a portion of the anodic oxide film (AL) of the second region (FD2) is performed.
[0194] Accordingly, a second patterning region (PN2) is formed in the first region (FD1) and the second region (FD2).
[0195] Then, referring to FIG. 7h, a step of etching the anodic oxide film (AL) exposed by the second patterning region (PN2) is performed.
[0196] Specifically, the anodic oxide film (AL) exposed by the second patterning region (PN2) of the first region (FD1) is etched and removed. As a result, a second through hole (PH2') is formed in the metal portion (MP). Since the second through hole (PH2') is formed by etching the anodic oxide film (AL) provided on the inner side of the metal portion (MP) in the width direction (±x direction), a micro trench (NT) is provided in the inner wall (IW). The first region (FD1) including the metal portion (MP) in which the second through hole (PH2') is formed corresponds to the metal portion (MP) of the metal structure (MS2) of the second embodiment. Therefore, the second through hole (PH2') illustrated in FIGS. 7A to 7I corresponds to the through hole (PH') formed in the metal portion (MP) illustrated in FIG. 6.
[0197] In addition, the anodic oxide film (AL) exposed by the second patterning region (PN2) of the second region (FD2) is etched and removed. As a result, a first through hole (PH1') is formed in the anodic oxide film (AL) of the second region (FD2). The second region (FD2) including the anodic oxide film (AL) in which the first through hole (PH1') is formed corresponds to the anodic oxide film portion (AP) of the metal structure (MS2) of the second embodiment. Therefore, the first through hole (PH1') illustrated in FIGS. 7h and 7i corresponds to the through hole (PH') formed in the anodic oxide film portion (AP) illustrated in FIG. 6.
[0198] The first through hole (PH1') is formed by etching at least a portion of the anodic oxide film (AL), and thus has a micro-trench (NT) provided in its inner wall (IW). The inner wall (IW) of the first through hole (PH1') is made of an anodic oxide film (AL) material and has insulating properties.
[0199] The first and second through holes (PH1, PH2) are preferably formed, regardless of the order, in the same step of forming the through hole (PH') through the second patterning region (PN2).
[0200] Then, referring to Fig. 7i, a step of removing the remaining second photoresist layer (PR2) remaining on one side of the metal portion (MP) and one side of the anodic oxide film (AL) and having a discontinuous shape by the first and second through holes (PH1, PH2) and a step of removing the seed layer (SD) are performed. Through this, the manufacturing of the metal structure (MS2) of the second embodiment is completed.
[0201] Figure 8 is a schematic diagram of a probe card (specifically, a vertical type probe card), which is an example of a test device (TD).
[0202] The probe card (PC) has at least one of the metal structures (MS1) of the first embodiment, the first modified example, the second-1 modified example and the metal structures (MS2) of the second embodiment as a guide plate (GP).
[0203] In Fig. 8, the probe card (PC) is illustrated as having a first modified example as a guide plate (GP). Hereinafter, the symbols of the first through-hole (PH1) provided with an insulating film (FL) of the guide plate (GP) and the second through-hole (PH2) not provided with an insulating film (FL) are assigned the same symbols as the first and second through-holes (PH1, PH2) of the first modified example.
[0204] A probe card (PC) inspects a pattern of a wafer (W) by means of electrically conductive contact pins (EP) that directly contact the wafer (W) through an electrical path provided in the order of a circuit board (CB'), an interposer (IP), a space transducer (ST) and a probe head (PH). The electrically conductive contact pins (EP) come into contact with electrode pads (WP) of the wafer (W) to perform wafer (W) pattern inspection.
[0205] The probe head (PH) supports an electrically conductive contact pin (EP) and serves to prevent electrical short-circuiting due to contact between adjacent probes. The probe head (PH) includes at least one guide plate (GP) and supports an electrically conductive contact pin (EP) installed in a through hole (PH) of the guide plate (GP). In this case, the electrically conductive contact pin (EP) may be a probe pin.
[0206] Referring to Fig. 8, the guide plate (GP) includes a first guide plate (GP1) and a second guide plate (GP2). Accordingly, the probe card (PC) has two guide plates (GP1, GP2). In Fig. 8, each of the first and second guide plates (GP1, GP2) is illustrated as being provided as a first variation example.
[0207] The guide plate (GP) is composed of a body (BD) made of metal, and the ground pin (GR) and power pin (PW) are electrically connected to the body (BD) made of metal, thereby preventing signal interference or noise generation to the signal pin (GR).
[0208] The first guide plate (GP1) is provided in the first settling area (SF1) formed on the first plate (P1).
[0209] The second guide plate (GP2) is mounted on the second mounting area (SF2) of the second plate (P2) which is inverted upside down from the first plate (P1) on the lower portion of the first plate (P1).
[0210] The first and second plates (P1, P2) are coupled in a state where their positions are misaligned with respect to each other in the width direction (±x direction). Accordingly, the first and second guide plates (GP1, GP2) are provided in a state where their positions are misaligned with respect to each other in the width direction. As a result, the electrically conductive contact pins (EP) installed in the through holes (PH) of the first and second guide plates (GP1, GP2) are provided in a form where the middle portion located at the distance between the first and second guide plates (GP1, GP2) is elastically deformed.
[0211] The first guide plate (GP1) and the second guide plate (GP2) each include a body (BD) made of a metal material including a plurality of through holes (PH) having micro-trench (NT) formed on the inner wall thereof, and an insulating film (FL) formed along the micro-trench (NT) on the inner wall (IW) of the through holes (PH).
[0212] The electrically conductive contact pins (EP) installed through the through holes (PH) of the first guide plate (GP1) and the second guide plate (GP2) include a signal pin, a ground pin, and a power pin.
[0213] Since the signal pin (SG) has the function of transmitting input / output signals, it must be insulated from the guide plates (GP1, GP2) while inserted into the through hole (PH). Therefore, the signal pin (SG) is inserted into the first through hole (PH1) having an insulating film (FL) provided on its inner wall (IW).
[0214] An insulating film (FL) is provided along a micro-trench (NT) provided on the inner wall (IW) of the first through-hole (PH1). Accordingly, even if a signal pin (SG) inserted into the first through-hole (PH1) comes into contact with the inner wall (IW) of the first through-hole (PH1), it is not electrically connected.
[0215] Meanwhile, the ground pin (GR) and the power pin (PW) are inserted into the second through-hole (PH2') that is not provided with an insulating film (FL). The ground pin (GR) transmits a ground signal, and the power pin (PW) transmits a power signal. Therefore, the ground pin (GR) and the power pin (PW) are inserted into the second through-hole (PH2') that is not provided with an insulating film (FL) so that they come into contact with the inner wall (IW) of the through-hole (PH) made of a metal material while sliding inside the through-hole (PH) and are electrically connected.
[0216] In this way, the guide plate (GP) maintains an insulating state through an insulating film (FL) at the position where the signal pin (SG) is inserted, and at the position where the ground pin (GR) and power pin (PW) are inserted, it is grounded by making contact with the ground pin (GR) and power pin (PW) through a metal material.
[0217] The guide plate (GP) has a micro-trench (NT) formed on the inner wall (IW) of the through hole (PH) to form a large surface area, and an insulating film (FL) formed along the micro-trench (NT). Therefore, the guide plate (GP) has a structure in which the bonding strength between the insulating film (FL) and the body (BD) is high. Accordingly, even if the electrically conductive contact pin (EP) slides on the inner wall (IW) of the through hole (PH) and comes into contact with the insulating film (FL), the insulating film (FL) is not easily peeled off from the body (BD) due to friction with the electrically conductive contact pin (EP).
[0218] Figure 9 is a schematic diagram of a test socket (TS), which is an example of a test device (TD).
[0219] The test socket (TS) has at least one of the metal structures (MS1) of the first embodiment, the first modified example, the second-first modified example and the metal structures (MS2) of the second embodiment as a guide plate (GP).
[0220] In Fig. 9, the probe card (PC) is illustrated as having a first modified example as a guide plate (GP). Hereinafter, the symbols of the first through-hole (PH1) provided with an insulating film (FL) of the guide plate (GP) and the second through-hole (PH2') not provided with an insulating film (FL) are assigned the same symbols as the first and second through-holes (PH1, PH2) of the first modified example.
[0221] A test socket (TS) includes a guide plate (GP1) having electrically conductive contact pins (EP) installed thereon, an insert (IS) for accommodating a semiconductor package (PG), and a pusher (PS) for pressing the semiconductor package (PG). A plurality of electrically conductive contact pins (EP) are installed on the guide plate (GP). The electrically conductive contact pins (EP) are preferably provided as socket pins.
[0222] An insert (IS) accommodates a semiconductor package (PG) so that testing of the semiconductor package (PG) can be performed in a stable state. An insert film (IF) having holes provided to guide the connection terminal (CN) of the semiconductor package (PG) is installed at the bottom of the insert (IS). The insert film (IF) is provided between the semiconductor package (PG) and an electrically conductive contact pin (EP). When inspecting the semiconductor package (PG), the insert film (IF) guides the accurate contact position by ensuring that the connection terminal (CN) of the semiconductor package (PG) is inserted into the hole provided in the insert film (IF).
[0223] The pusher (PS) pressurizes the semiconductor package (PG) seated in the receiving portion of the insert (IS) with a constant pressure. The semiconductor package (PG) is pressed by the pusher (PS) and electrically connected to the pad (PD) of the circuit board (CB) through the electrically conductive contact pin (EP) installed on the guide plate (GP).
[0224] A guide plate (GP) includes a body (BD) having a plurality of through holes (PH) having micro-trench (NT) in an inner wall (IW), and an insulating film (FL) provided along the micro-trench (NT) in the inner wall (IW) of the through holes (PH).
[0225] The test socket (TS) performs a process of electrically connecting a semiconductor package (PG) to a pad (PD) of a circuit board (CB) through an electrically conductive contact pin (EP) installed on a guide plate (GP) by pressing the semiconductor package (PG) with a pusher (PS).
[0226] At this time, the guide plate (GP) is made of a body (BD) made of metal material and has improved frequency characteristics in high-frequency characteristic inspection.
[0227] Many electrically conductive contact pins (EP), which are intended to carry not only power signals but also ground signals, introduce noise into the operational signals, which are input / output signals, which limits the performance of the test socket (TS) as a whole, especially the frequency performance.
[0228] However, according to the present invention, the ground pin (GR) and the power pin (PW) are inserted into the second through hole (PH2) in which the insulating film (FL) is not formed and are electrically connected to the metal part (MP), so that noise is not generated in the operation signal of the signal pin (SG) inserted into the first through hole (PH1) in which the insulating film (FL) is formed, thereby improving the inspection performance of high-frequency characteristics.
[0229] Meanwhile, the metal structure (MS1) of the first embodiment and its modified examples (the first and second modified examples) and the metal structure (MS2) of the second embodiment may be provided not only as a guide plate (GP) provided in an inspection device (TD) but also as a mask in a process using a mask in a semiconductor or display process.
[0230] As described above, the present invention has been described with reference to preferred embodiments thereof, but it will be apparent to those skilled in the art that various modifications or variations may be made to the present invention without departing from the spirit and scope of the present invention as set forth in the following claims.
[0231] [Explanation of symbols]
[0232] MS: Metal structures
[0233] BD: Body
[0234] PH: Through hole
[0235] FL: insulating film
[0236] NT: Microtrench
Claims
1. A body made of a metal material having a plurality of through holes and a plurality of micro-trenches having a width and depth formed on the inner wall of the through holes; and A metal structure comprising an insulating film formed to extend in the thickness direction of the body along the micro-trench and formed in the circumferential direction of the through hole.
2. In paragraph 1, A metal structure, wherein the plurality of through holes include a first through hole provided with the insulating film and a second through hole not provided with the insulating film.
3. In paragraph 1, The above body is a metal structure formed by laminating multiple metal layers of the same material.
4. In paragraph 1, The above body is a metal structure formed by laminating multiple metal layers of different materials.
5. In paragraph 1, The above metal structure is a guide plate.
6. A body having a plurality of through holes; At least a portion of the above body is made of an anodic oxide material, and the remaining portion is made of a metal material, A metal structure in which a through hole provided in the above anodic oxide film material and the above metal material has a width and depth on its inner wall and is formed to extend in the thickness direction of the body, and has a plurality of micro trenches formed in the circumferential direction of the through hole.
7. A guide plate including a body made of a metal material having a plurality of through holes and a plurality of micro-trenches having a width and depth formed on the inner wall of the through holes, and an insulating film formed to extend in the thickness direction of the body along the micro-trenches and formed in the circumferential direction of the through holes; and An inspection device comprising an electrically conductive contact pin inserted into the above through hole.
8. In paragraph 7, A test device, wherein the electrically conductive contact pin includes at least one of a signal pin and a ground pin.
9. In paragraph 8, The above guide plate is an inspection device having the insulating film on the inner wall of the through hole into which the signal pin is inserted.
10. Step for preparing the anode oxide film; A step of forming an etched portion by etching the above anodic oxide film; A step of forming a first through hole by etching the above anodic oxide film; and A method for manufacturing a metal structure, comprising: forming an insulating film on the inner wall of the first through hole.
11. Step for preparing the anode oxide film; A step of forming an etched portion by etching the above anodic oxide film; A step of forming a first through hole in an anodic oxide film; and A method for manufacturing a metal structure, comprising: forming a second through hole in a metal part.
Citation Information
Patent Citations
Socket for semiconductor integrated circuit
JP2009145165A
Inspection socket
JP2009156710A
Wiring board and method for manufacturing wiring board
JP2011014612A
Method and device of arbitrating multi-cores
KR1020230046884A
Nozzle assembly and substrate processing apparatus including the same
KR1020240070070A