Metal complex and organic electroluminescent device

By designing metal complexes with a tridentate ligand-metal-secondary amine structure, the problem of low performance of linear carbene-metal-amine complexes in the existing technology has been solved, and high external quantum properties of organic electroluminescent devices have been achieved. efficiency and long life, and simplifies the preparation process of luminescent materials.

WO2024216750A1PCT designated stage expired Publication Date: 2024-10-24SHENZHEN UNIV
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/104046
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-21
Filing Date
2023-06-29
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing linear carbene-metal-amine complex TADF materials have low performance, resulting in low device lifetime and external quantum efficiency of organic electroluminescent devices.

Method used

Design a metal complex with a tridentate ligand-metal-secondary amine structure. By introducing aryl, heteroaryl and other groups with electron-withdrawing effects into the No. 1 substitution site of carbazole, an intramolecular non-linear structure is formed. Covalent interactions improve the stability of metal complexes and inhibit non-radiative transition processes, thereby improving external quantum efficiency and device lifetime.

Benefits of technology

A higher external quantum efficiency of up to 35.6% and a longer device lifetime of organic electroluminescent devices are achieved, and a simple organic synthesis method is used to prepare metal complexes at low cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023104046_24102024_PF_FP_ABST
    Figure CN2023104046_24102024_PF_FP_ABST
Patent Text Reader

Abstract

Disclosed are a metal complex and an organic electroluminescent device, relating to the technical field of electronic materials. Specifically disclosed is a metal complex having the structure shown below: formula 1. The organic electroluminescent device comprising the metal complex has high external quantum efficiency and long device life.
Need to check novelty before this filing date? Find Prior Art

Description

Metal complex and organic electroluminescent device

[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on April 21, 2023, with application number 202310461167.7 and invention name “A Metal Complex and Organic Electroluminescent Device”, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present application relates to the technical field of electronic materials, and in particular to a metal complex and an organic electroluminescent device. Background Art

[0003] Organic light-emitting diodes (OLEDs) convert electrical energy into light energy. They feature low driving voltage, low energy consumption, flexibility, short response time, and a wide operating temperature range. They hold broad application prospects in industrial lighting, displays for smartphones, and large-screen televisions. Consequently, the emergence of OLEDs has generated significant buzz in both industry and academia, and they are considered the dominant lighting and flat-panel display technology of the future. OLED devices typically consist of two electrodes (anode and cathode) and several organic layers, such as a hole injection layer (HIL), hole and electron transport layers (HELs), and an emitting layer (EML) between the two electrodes. Under external voltage, oppositely charged carriers (holes and electrons) are injected from the anode and cathode, ultimately recombine within the emitting layer to generate photons. The emitting layer significantly determines not only device performance but also its processing methods, making it the most critical component of all OLED components.

[0004] Over the past three decades, luminescent materials have developed rapidly, evolving from traditional fluorescent, phosphorescent, and triplet-triplet annihilation (TTA) materials to the third generation of thermally activated delayed fluorescence (TADF) materials. Based on spin statistics, when an OLED device is excited by an electric field, a 1:3 ratio of singlet and triplet excitons is generated within the light-emitting layer. Varying exciton utilization rates among different luminescent materials can lead to variations in OLED device efficiency. For example, because first-generation fluorescent materials can only utilize singlet excitons, the theoretical internal quantum efficiency (i.e., exciton utilization rate) of fluorescent OLEDs is capped at only 25%, while the external quantum efficiency (the ratio of photons emitted by the light-emitting layer to the injected charge) is only 5%. Second-generation OLED materials utilize phosphorescent complexes containing the extremely rare precious metal iridium. Because they can simultaneously utilize both singlet and triplet excitons, the theoretical internal quantum efficiency of phosphorescent OLEDs can reach 100%. However, the high cost of precious metal phosphorescent materials and the issue of heavy metal contamination have significantly hindered the development of new phosphorescent materials.

[0005] TADF materials can upconvert triplet excitons to singlet excitons through reverse intersystem crossing (RISC), thereby capturing triplet excitons and achieving a theoretical internal quantum efficiency of 100%. Compared to organometallic phosphorescent complexes, organic TADF luminescent materials offer greater freedom in chemical design and exhibit higher long-term stability and sustainability. The potential for high efficiency, wide design diversity, and environmentally friendly properties make TADF materials a promising candidate for third-generation OLED device materials.

[0006] TADF materials can be divided into purely organic materials and metal complex materials. Purely organic TADF materials typically have long emission lifetimes, leading to a significant efficiency roll-off at high device brightness. This long emission lifetime is also considered a key factor in the poor stability of OLED devices.

[0007] However, existing linear carbene-metal-amine complexes have limited ligand options, and their devices suffer from short lifespans and low efficiency, presenting challenges in practical applications. Platinum(II) complexes are widely used in phosphorescent OLED devices, but few have developed Pt(II) complex TADF materials. This is primarily due to the large spin-orbit coupling constant of Pt(II), which results in predominantly phosphorescent emission. On the other hand, some Pd(II) complex OLED devices offer excellent performance, but reports on Pd(II) complex OLED materials, whether phosphorescent or TADF, are scarce. There is an urgent need to design novel Pd(II) complex OLED systems.

[0008] Summary of the Invention

[0009] Therefore, the technical problem to be solved by this application is to overcome the shortcomings of prior art linear carbene-metal-amine complex TADF materials, which have low performance and low device lifespan and external quantum efficiency of the resulting organic electroluminescent devices. Thus, a metal complex and an organic electroluminescent device are provided.

[0010] The scheme adopted in this application is as follows:

[0011] The present application provides a metal complex having the structure shown below:

[0012] wherein M is selected from platinum or palladium, and the oxidation state of M is +2;

[0013] Ring A, Ring B, and Ring C are each independently selected from substituted or unsubstituted C6-C 48 Aromatic ring, substituted or unsubstituted C4-C 48 Heteroaromatic ring; Ring A and Ring B are connected by a single bond or by forming a fused ring; Ring B and Ring C are connected by a single bond or by forming a fused ring; Ring A, Ring B and Ring C are coordinated to the metal M center in the form of a negative monovalent tridentate ligand;

[0014] R 1 -R 7 the same or different, each independently selected from hydrogen, substituted or unsubstituted C1-C 40 Alkyl, substituted or unsubstituted C6-C 48 Aryl, substituted or unsubstituted C3-C 48 heteroaryl;

[0015] Ra is a substituted or unsubstituted C6-C 48 Aryl or substituted or unsubstituted C6-C 48 Heteroaryl.

[0016] Optional, substituted C6-C 48 Aromatic ring, substituted C4-C 48 Heteroaromatic ring, substituted C1-C 40 Alkyl, substituted C6-C 48 Aryl, substituted C3-C 48 The substituents of the heteroaryl group are selected from deuterium, halogen, cyano, C1-C6 alkyl, C3-C 30 Cycloalkyl, C6-C 30 Aryl, C3-C 30 One of the heteroaryl groups.

[0017] In the present application, the oxidation state of M is +2.

[0018] Optional, R 1 、R 3 、R 4 、R 6 , and R 7 is hydrogen, R 2 and R 5 the same or different, independently selected from substituted or unsubstituted C1-C 40 Alkyl, substituted or unsubstituted C6-C 48 Aryl, substituted or unsubstituted C3-C 48 Heteroaryl.

[0019] Optionally, the substituted C1-C 40 Alkyl, substituted C6-C 48 Aryl, substituted C3-C 48 The heteroaryl group is optionally substituted by one or more substituents R b Replace; each R b independently selected from hydrogen, halogen, cyano, C1-C 10 Alkyl, C6-C 30 Aryl.

[0020] Optionally, the C1-C 40Alkyl is selected from methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl;

[0021] The C1-C 10 Alkyl is selected from methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl;

[0022] The C6-C 48 Aryl is selected from phenyl, naphthyl, anthracenyl;

[0023] The C6-C 30 The aryl group is selected from phenyl, naphthyl, anthracenyl.

[0024] Optionally, it is characterized in that

[0025] The tridentate ligand formed by ring A, ring B, and ring C has any of the following structures:

[0026] Optionally, Ra has any of the following structures:

[0027] Optionally, the metal complex has any of the following structures:

[0028] The present application also provides a method for preparing the above-mentioned metal complex, comprising the following steps:

[0029] Step 1: a tridentate ligand reacts with potassium chloroplatinite or palladium dichloride to generate a tridentate ligand M metal chloride E;

[0030] Step 2: Compound A is reacted with pinacol diboronate through a Suzuki coupling reaction to obtain compound aryl borate B, and then compound B is reacted with C through a Suzuki coupling reaction to obtain ligand D;

[0031] Alternatively, compound C is reacted with pinacol borane to obtain compound N, and then compound N is reacted with A through a Suzuki coupling reaction to obtain ligand D;

[0032] Step 3: The ligand D reacts with the tridentate ligand M and the metal chloride E to obtain the metal complex (compound of formula 1).

[0033] The synthesis route of the metal complex described in this application is as follows:

[0034] The present application also provides an organic electroluminescent device, which includes a first electrode, a second electrode, and a light-emitting layer located between the first electrode and the second electrode, and the light-emitting layer includes any one or a combination of at least two of the above-mentioned metal complexes.

[0035] Optionally, the light-emitting layer includes the metal complex and the organic functional material mentioned above, and in terms of mass percentage, the metal complex accounts for 0.01%-100%, and the organic functional material accounts for 0-99.9%.

[0036] It should be noted that the application of the metal complex described in this application is not limited to the device composition, and the film thickness or constituent materials of each layer can be appropriately changed according to the basic physical properties of the specific compound structure of this application.

[0037] The method for preparing the organic device described in this application is a conventional method in the art. Optionally, the preparation of the organic electroluminescent device includes the following steps: using a glass substrate with ITO vapor-deposited thereon as a transparent support substrate, and sequentially vapor-depositing the organic layers and metal electrodes on the ITO film on the transparent support substrate.

[0038] The present application also provides applications of the above-mentioned organic electroluminescent device in electronic devices.

[0039] Beneficial effects of this application:

[0040] The present application provides a metal complex having a structure of Formula 1, which contains a tridentate ligand-metal-secondary amine structure and has good TADF (thermally activated delayed fluorescence) performance. Through the unique molecular structure and transition mode, and the introduction of aromatic, heteroaryl, and other electron-withdrawing groups at the No. 1 substitution site Ra of carbazole, intramolecular non-covalent interactions between Ra and the tridentate ligand can be formed, thereby improving the stability of the metal complex and enhancing the charge transfer process within and between ligands, thereby inhibiting the geometric distortion of the metal complex and further inhibiting the non-radiative transition process, so that the organic electroluminescent device produced has a high external quantum efficiency and a long device life, with an external quantum efficiency of up to 35.6%.

[0041] Furthermore, the tridentate ligand used in the metal complex provided in the present application can be prepared in high yield through simple organic synthesis, and the raw material cost is low, which is of great significance for the mass production process of luminescent materials. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the following is a brief introduction to the drawings required for use in the specific implementation methods or the description of the prior art. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.

[0043] FIG1 is a structural diagram of the organic electroluminescent device in device examples 1-11 of the present application;

[0044] FIG2 is a crystal structure diagram of PtNCN1-12 prepared in Example 3 of the present application;

[0045] FIG3 is a thermogravimetric analysis curve of PtNCN1-12 prepared in Example 3 of the present application;

[0046] FIG4 is an absorption spectrum of PdCCC1-B5 prepared in Example 30 of the present application in toluene solution;

[0047] FIG5 is an absorption spectrum of PdCCC1-5 prepared in Example 28 of the present application in toluene solution;

[0048] FIG6 is an absorption spectrum of PdCCC1-3 prepared in Example 26 of the present application in a toluene solution;

[0049] FIG7 is an emission spectrum of PdCCC1-B5 prepared in Example 30 of the present application in a toluene solution;

[0050] FIG8 is an emission spectrum of PdCCC1-5 prepared in Example 28 of the present application in a toluene solution;

[0051] FIG9 is an emission spectrum of PdCCC1-3 prepared in Example 26 of the present application in a toluene solution;

[0052] FIG10 is an absorption spectrum of PtNCN1-5 prepared in Example 7 of the present application in a toluene solution;

[0053] FIG11 is an absorption spectrum of PtNCN1-3 prepared in Example 8 of the present application in a toluene solution;

[0054] FIG12 is an absorption spectrum of PtNCN1-16 prepared in Example 11 of the present application in a toluene solution;

[0055] FIG13 is an absorption spectrum of PtNCN1-12 prepared in Example 3 of the present application in a toluene solution;

[0056] FIG14 is an absorption spectrum of PtNCN1-20 prepared in Example 21 of the present application in a toluene solution;

[0057] FIG15 is an absorption spectrum of PtNCN1-21 prepared in Example 22 of the present application in a toluene solution;

[0058] FIG16 is an absorption spectrum of PtNCN3-16 prepared in Example 16 of the present application in a toluene solution;

[0059] FIG17 is an absorption spectrum of PtNCN3-22 prepared in Example 23 of the present application in a toluene solution;

[0060] FIG18 is an absorption spectrum of PtNCN3-23 prepared in Example 24 of the present application in a toluene solution;

[0061] FIG19 is an absorption spectrum of PtNCN3-24 prepared in Example 25 of the present application in a toluene solution;

[0062] FIG20 is an emission spectrum of PtNCN1-5 prepared in Example 7 of the present application in a tetrahydrofuran solution;

[0063] FIG21 is an emission spectrum of PtNCN1-3 prepared in Example 8 of the present application in a tetrahydrofuran solution;

[0064] FIG22 is an emission spectrum of PtNCN1-12 prepared in Example 3 of the present application in a toluene solution;

[0065] FIG23 is an emission spectrum of PtNCN1-5 prepared in Example 7 of the present application in a polymethyl methacrylate film;

[0066] FIG24 is an emission spectrum of PtNCN1-3 prepared in Example 8 of the present application in a polymethyl methacrylate film;

[0067] FIG25 is an emission spectrum of PtNCN1-16 prepared in Example 11 of the present application in a polymethyl methacrylate film;

[0068] FIG26 is an emission spectrum of PtNCN1-12 prepared in Example 3 of the present application in a polymethyl methacrylate film;

[0069] FIG27 is an emission spectrum of PtNCN1-20 prepared in Example 21 of the present application in a polymethyl methacrylate film;

[0070] FIG28 is an emission spectrum of PtNCN1-21 prepared in Example 22 of the present application in a polymethyl methacrylate film;

[0071] FIG29 is an emission spectrum of PtNCN3-22 prepared in Example 23 of the present application in a polymethyl methacrylate film;

[0072] FIG30 is an emission spectrum of PtNCN3-23 prepared in Example 24 of the present application in a polymethyl methacrylate film;

[0073] FIG31 is an emission spectrum of PtNCN3-24 prepared in Example 25 of the present application in a polymethyl methacrylate film;

[0074] FIG32 is an emission spectrum of PdCCC1-12 prepared in Example 27 of the present application in a polymethyl methacrylate film;

[0075] FIG33 is an emission spectrum of PdCCC1-3 prepared in Example 26 of the present application in a polymethyl methacrylate film;

[0076] FIG34 is a graph showing the lifetime decay curve of PtNCN1-5 prepared in Example 7 of the present application in a polymethyl methacrylate film;

[0077] FIG35 is a graph showing the lifetime decay curve of PtNCN1-3 prepared in Example 8 of the present application in a polymethyl methacrylate film;

[0078] FIG36 is a graph showing the lifetime decay curve of PtNCN1-16 prepared in Example 11 of the present application in a polymethyl methacrylate film;

[0079] FIG37 is a graph showing the lifetime decay curve of PtNCN1-12 prepared in Example 3 of the present application in a polymethyl methacrylate film;

[0080] FIG38 is a graph showing the lifetime decay curve of PtNCN1-20 prepared in Example 21 of the present application in a polymethyl methacrylate film;

[0081] FIG39 is a lifetime decay curve of PtNCN1-21 prepared in Example 21 of the present application in a polymethyl methacrylate film;

[0082] FIG40 is a graph showing the lifetime decay curve of PtNCN3-16 prepared in Example 16 of the present application in a polymethyl methacrylate film;

[0083] FIG41 is a graph showing the lifetime decay curve of PtNCN3-22 prepared in Example 23 of the present application in a polymethyl methacrylate film;

[0084] FIG42 is a graph showing the lifetime decay curve of PtNCN3-23 prepared in Example 24 of the present application in a polymethyl methacrylate film;

[0085] FIG43 is a lifetime decay curve of PtNCN3-24 prepared in Example 25 of the present application in a polymethyl methacrylate film;

[0086] FIG44 is a graph showing the lifetime decay curve of PdCCC1-12 prepared in Example 27 of the present application in a polymethyl methacrylate film;

[0087] FIG45 is a graph showing the lifetime decay curve of PdCCC1-3 prepared in Example 26 of the present application in a polymethyl methacrylate film;

[0088] FIG46 is an electroluminescence image of device examples 1-4 of the present application based on compound PtNCN1-12;

[0089] FIG47 is a graph showing the electroluminescent quantum efficiency of device examples 1-4 of the present application based on compound PtNCN1-12;

[0090] FIG48 is an electroluminescence image of device examples 5-7 of the present application based on compound PdCCC1-12;

[0091] FIG49 is a graph showing the electroluminescent quantum efficiency of device Examples 5-7 of the present application based on compound PdCCC1-12;

[0092] FIG50 shows the change in brightness over time of device Example 12 of the present application based on compound PdCCC1-12;

[0093] FIG51 is an electroluminescence image of device Examples 8-9 of the present application based on compounds PdCCC1-5;

[0094] FIG52 is a graph showing the electroluminescent quantum efficiency of device Examples 8-9 of the present application based on compounds PdCCC1-5;

[0095] FIG53 is an electroluminescence image of device Examples 10-11 of the present application based on compounds PdCCC1-3;

[0096] FIG54 is a graph showing the electroluminescent quantum efficiency of device Examples 10-11 of the present application based on compounds PdCCC1-3;

[0097] Reference numerals:

[0098] 1- anode layer, 2- hole injection layer, 3- first hole transport layer, 4- second hole transport layer, 5- electron blocking layer, 6- light-emitting layer, 7- first electron transport layer, 8- second electron transport layer, 9- electron injection layer, 10- cathode layer, 100- glass substrate. DETAILED DESCRIPTION

[0099] The following examples are provided to further better understand the present application, but are not limited to the best implementation mode described herein, and do not limit the content and protection scope of the present application. Any product identical or similar to the present application obtained by anyone under the inspiration of the present application or by combining the features of the present application with other prior arts shall fall within the scope of protection of the present application.

[0100] If no specific experimental steps or conditions are specified in the examples, the conventional experimental steps or conditions described in the literature in this field can be used. If the manufacturer of the reagents or instruments is not specified, they are all commercially available conventional reagents.

[0101] The preparation method of the metal complex in this embodiment includes the following steps:

[0102] Step 1: a tridentate ligand reacts with potassium chloroplatinite to generate a tridentate ligand M and a metal chloride E;

[0103] Step 2: Compound A is reacted with pinacol diboronate through a Suzuki coupling reaction to obtain compound aryl borate B, and then compound B is reacted with C through a Suzuki coupling reaction to obtain ligand D;

[0104] Alternatively, compound C is reacted with pinacol borane to obtain compound N, and then compound N is reacted with A through a Suzuki coupling reaction to obtain ligand D;

[0105] Step 3: The ligand D reacts with the tridentate ligand M and the metal chloride E to obtain the metal complex (compound of formula I).

[0106] The synthesis route of the metal complex in this embodiment is as follows:

[0107] Example 1

[0108] This embodiment provides a method for preparing a tridentate ligand intermediate and its tridentate ligand M metal chloride required for the subsequent preparation of a metal complex, as shown below:

[0109] 1) Preparation of tridentate ligand intermediate CNN

[0110] The synthesis path is as follows:

[0111] Phenylboronic acid (244 mg, 2 mmol), 6-bromo-2,2-bipyridine (383 mg, 1.63 mmol) and Na2CO3 (864 mg, 8.15 mmol), tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108 ° C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and distilled under reduced pressure. Purification by column chromatography (eluent: petroleum ether: dichloromethane = 10:1) gave a colorless solid intermediate CNN (yield 98%).

[0112] 2) Preparation of tridentate ligand intermediate NCN1

[0113] The synthesis path is as follows:

[0114] 1,3-Diphenylboronic acid (166 mg, 1 mmol), 1-bromopyridine (258 mg, 1.63 mmol), Na2CO3 (864 mg, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and distilled under reduced pressure. Purification by column chromatography (eluent: petroleum ether: dichloromethane = 10:1) gave a colorless solid intermediate NCN1 (yield 88%). 1 H NMR(400MHz, CDCl3) δ8.71(d,J=4.4Hz,2H),8.64(s,1H),8.05(d,J=7.6Hz,2H),7.81 (d,J=7.5Hz,2H),7.72(t,J=7.6Hz,2H),7.57(t,J=7.8Hz,1H),7.21(t,J=5.6Hz,2H); 13 C NMR (101MHz, CDCl3) δ157.1,149.7,139.9,136.8,129.2,127.5,125.5,122.3,120.7ppm; EI-MS: m / z calcd for C 16 H 12 N2[M] + :232.10;found:232.27.

[0115] 3) Preparation of tridentate ligand intermediate NCN2

[0116] The synthesis path is as follows:

[0117] 2-Pyridineboronic acid (234 mg, 1.9 mmol), monobromide (421 mg, 1.63 mmol) and Na2CO3 (864 mg, 8.15 mmol), tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108 ° C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and distilled under reduced pressure. Purification by column chromatography (eluent: petroleum ether: dichloromethane = 10:1) gave a colorless solid intermediate NCN2 (yield 78%).

[0118] 4) Preparation of tridentate ligand intermediate NCN3

[0119] The synthesis path is as follows:

[0120] 2-(3-Bromobenzene)-pyridine (234 mg, 1 mmol), pyrazole (102 mg, 1.5 mmol) and K2CO3 (830 mg, 6 mmol), 1,2-cyclohexanediamine (46 mg, 0.4 mmol), cuprous iodide (19 mg, 0.1 mmol) were dissolved in 30 ml of DMF, stirred, and slowly heated to 130 ° C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and distilled under reduced pressure. Purification by column chromatography (eluent: petroleum ether: dichloromethane = 2:1) was performed to obtain a colorless solid intermediate NCN3 (yield 88%), 1H NMR (500MHz, CDCl3) δ8.73(d,J=4.6Hz,1H),8.38(t,J=1.9Hz,1H),8.07(d,J=2.4Hz,1H ), 8.03 (s, 1H), 7.93 (d, J = 7.8Hz, 1H), 7.80 (m, 4H), 7.58 (t, J = 7.9Hz, 1H), 7.29 (m, 1H).

[0121] 5) Preparation of tridentate ligand intermediate CCC1

[0122] The synthesis path is as follows:

[0123] 1,3-Diiodobenzene (330 mg, 1 mmol), imidazole (102 mg, 1.5 mmol), K2CO3 (830 mg, 6 mmol), cuprous iodide (19 mg, 0.1 mmol), and L-proline (58 mg, 0.5 mmol) were dissolved in 30 ml of ultra-dry DMSO solution, stirred, and slowly heated to 140°C. The reaction was carried out for 48 h, extracted with dichloromethane and water, and distilled under reduced pressure. Purification by column chromatography (eluent: petroleum ether: dichloromethane = 2:1) gave a colorless solid intermediate 1 (yield 80%).

[0124] Intermediate 1 (210 mg, 1 mmol) and n-butyl bromide (1370 mg, 10 mmol) were dissolved in 30 ml of acetonitrile solution, stirred, and slowly heated to 80°C. The mixture was reacted for 72 h, filtered, and evaporated under reduced pressure to obtain a colorless solid intermediate CCC1 (yield 60%). 1H NMR (300 MHz, CD2Cl2): d 11.56(s,2H),9.04(t,J=2.0Hz,1H),8.91(t,J=1.8Hz,2H),8.24(dd,J=8.3,2.0Hz,2H),7.72(t,J=8.3Hz,1H),7.6 0(t,J=1.8Hz,2H),4.45(t,J=7.3Hz,4H),2.02(tt,J=7.5Hz,4H),1.43(qt,J=7.5Hz,4H),1.00(t,J=7.3Hz,6H).13C NMR(126MHz,CD2Cl2):d 137.0,136.5,133.0,123.4,122.8,122.4,115.5,51.0,32.4,20.1,13.8.

[0125] 6) Preparation of tridentate ligand metal chloride ClPtCNN

[0126] The synthesis path is as follows:

[0127] CNN ligand (232 mg, 1 mmol) and potassium chloroplatinite (415 mg, 1 mmol) were dissolved in 20 mL of glacial acetic acid, stirred, and slowly heated to 120°C. After reacting for 72 hours, the mixture was filtered, washed with water, and dried to obtain a colorless solid intermediate ClPtCNN (yield 65%).

[0128] 7) Preparation of tridentate ligand metal chloride ClPtNCN1

[0129] The synthesis path is as follows:

[0130] NCN1 ligand (232 mg, 1 mmol) and potassium chloroplatinite (415 mg, 1 mmol) were dissolved in 20 mL of glacial acetic acid, stirred, and slowly heated to 120°C. After reacting for 72 hours, the mixture was filtered, washed with water, and dried to obtain a colorless solid intermediate ClPtNCN1 (yield 69%). 1H NMR (300 MHz, DMSO-d6) δ 9.07 (dd, J = 5.5, 0.9 Hz, 2H), 8.17 (td, J = 7.7, 1.6 Hz, 2H), 8.07 (br d, J = 7.6 Hz, 2H), 7.70 (d, J = 7.7 Hz, 2H), 7.52 (ddd, J = 7.4, 5.8, 1.6 Hz, 2H), 7.23 (t, J = 7.7 Hz, 1H); 13C NMR (75MHz, DMSO-d6) δ166.73,161.19,151.41,140.65,140.60,125.09,124.28,123.28,120.62.

[0131] 8) Preparation of tridentate ligand metal chloride ClPtNCN2

[0132] The synthesis path is as follows:

[0133] Dissolve NCN2 ligand (256 mg, 1 mmol) and potassium chloroplatinite (415 mg, 1 mmol) in 20 mL of glacial acetic acid, stir, and slowly heat to 120°C. React for 72 hours, filter, wash with water, and dry to obtain a colorless solid intermediate ClPtNCN2 (yield 75%).

[0134] 9) Preparation of tridentate ligand metal chloride ClPtNCN3

[0135] The synthesis path is as follows:

[0136] NCN3 ligand (221 mg, 1 mmol) and potassium chloroplatinite (415 mg, 1 mmol) were dissolved in 20 mL of glacial acetic acid, stirred, and slowly heated to 120°C. After reacting for 72 hours, the mixture was filtered, washed with water, and dried to obtain a colorless solid intermediate ClPtNCN3 (yield 70%). 1H NMR (500 MHz, CDCl3) δ9.35 (t, J = 10.3 Hz, 1H), 8.07 (dd, J = 10.2, 2.6 Hz, 2H), 7.99 (td, J = 7.8, 1.5 Hz, 1H), 7.73 (d, J = 7.7 Hz, 1H), 7.38 (d, J = 7.7 Hz, 1H), 7.34 (m, 1H), 7.28 (m, 4H), 7.15 (d, J = 7.8 Hz, 1H), 6.68 (m, 1+H).

[0137] 10) Preparation of tridentate ligand metal chloride ClPtCCC1

[0138] The synthesis path is as follows:

[0139] The CCC1 ligand (324 mg, 1 mmol), potassium chloroplatinate (830 mg, 2 mmol), and silver oxide (552 mg, 2.38 mmol) were dissolved in 20 mL of DMSO, shielded from light, stirred, and slowly heated to 156°C. After 72 hours of reaction, the crude product was suspended in dichloromethane and filtered. The filtrate was washed with water, and the organic phase was dried over magnesium sulfate. The organic phase was rotary evaporated, acetonitrile was added, and then rotary evaporated again to obtain the yellow solid intermediate ClPtCCC1 (yield 70%).

[0140] 11) Preparation of tridentate ligand metal chloride ClPdCNN

[0141] The synthesis path is as follows:

[0142] CNN ligand (232 mg, 1 mmol) and palladium dichloride (177 mg, 1 mmol) were dissolved in 20 mL of glacial acetic acid, stirred, and slowly heated to 120°C. After reacting for 72 hours, the mixture was filtered, washed with water, and dried to obtain a colorless solid intermediate ClPdCNN (yield 75%).

[0143] 12) Preparation of tridentate ligand metal chloride ClPdNCN1

[0144] The synthesis path is as follows:

[0145] Dissolve NCN1 ligand (232 mg, 1 mmol) and palladium dichloride (177 mg, 1 mmol) in 20 mL of glacial acetic acid, stir, and slowly heat to 120°C. After reacting for 72 hours, filter, wash with water, and dry to obtain a colorless solid intermediate ClPdNCN1 (yield 69%).

[0146] 13) Preparation of tridentate ligand metal chloride ClPdNCN2

[0147] The synthesis path is as follows:

[0148] Dissolve NCN2 ligand (256 mg, 1 mmol) and palladium dichloride (177 mg, 1 mmol) in 20 mL of glacial acetic acid, stir, and slowly heat to 120°C. After reacting for 72 hours, filter, wash with water, and dry to obtain a colorless solid intermediate ClPdNCN2 (yield 75%).

[0149] 14) Preparation of tridentate ligand metal chloride ClPdNCN3

[0150] The synthesis path is as follows:

[0151] Dissolve NCN3 ligand (221 mg, 1 mmol) and palladium dichloride (177 mg, 1 mmol) in 20 mL of glacial acetic acid, stir, and slowly heat to 120°C. After reacting for 72 hours, filter, wash with water, and dry to obtain a colorless solid intermediate ClPdNCN3 (yield 70%).

[0152] 15) Preparation of tridentate ligand metal chloride ClPdCCC1

[0153] The synthesis path is as follows:

[0154] CCC1 ligand (485 mg, 1 mmol), palladium dichloride (177 mg, 2 mmol), and sodium acetate (320 mg, 4 mmol) were dissolved in 20 mL of DMAc (N,N-dimethylacetamide) and stirred. The temperature was slowly raised to 140°C. After three days of reaction, the crude product was suspended in dichloromethane and filtered. The filtrate was washed with water, and the organic phase was dried over magnesium sulfate. The organic phase was rotary evaporated, acetonitrile was added, and then rotary evaporated again. Finally, the final product was purified by column chromatography (yield 36%), 1H NMR (500MHz, CDCl3) δ7.32 (d, J = 1.9 Hz, 2H), 7.13 (t, J = 7.8 Hz, 1H), 6.91 (d, J = 1.9 Hz, 2H), 6.89 (s, 1H), 6.87 (s, 1H), 4.76 (t, J = 7.4 Hz, 4H), 1.88 (m, 4H), 1.47 (dq, J = 14.9, 7.4 Hz, 4H), 0.96 (t, J = 7.4 Hz, 6H).

[0155] Example 2

[0156] This embodiment provides a method for preparing the intermediate compound required for the subsequent preparation of the metal complex, as shown below:

[0157] 1) Preparation of Intermediate 1

[0158] The synthesis path is as follows:

[0159] The preparation method specifically comprises the following steps:

[0160] 2-(4-Bromophenyl)-4,6-diphenyl-1,3,5-triazine (3 g, 7.73 mmol), pinacol diboron (4.9 g, 19.3 mmol), [1,1'-bis(diphenylphosphino)ferrocene]palladium dichloride (565 mg, 0.773 mmol), and potassium acetate (4.55 g, 46.358 mmol) were dissolved in 100 ml of ultra-dry 1,4-dioxane solvent and refluxed at 108°C for 12 hours. The reaction solution was filtered through diatomaceous earth, and the filtrate was distilled under reduced pressure and purified by column chromatography to obtain a white solid intermediate 1 (yield 95%).

[0161] 2) Preparation of Intermediate 2

[0162] The synthesis path is as follows:

[0163] The preparation method specifically comprises the following steps:

[0164] 2-(4-Bromophenyl)-4,6-diphenyl-1,3,5-pyrimidine (3 g, 7.726 mmol), pinacol diboron (4.9 g, 19.3 mmol), [1,1'-bis(diphenylphosphino)ferrocene]palladium dichloride (565 mg, 0.773 mmol), and potassium acetate (4.55 g, 46.358 mmol) were dissolved in 100 ml of ultra-dry 1,4-dioxane solvent and refluxed at 108°C for 12 hours. The reaction solution was filtered through diatomaceous earth, and the filtrate was distilled under reduced pressure and purified by column chromatography to obtain a white solid intermediate 2 (yield 90%).

[0165] 3) Preparation of Intermediate 3

[0166] The synthesis path is as follows:

[0167] The preparation method specifically comprises the following steps:

[0168] 3,6-di-tert-butyl-9H-carbazole (13.97 g, 50 mmol) was added to 300 ml of chloroform solution, the mixture was cooled to 0°C in an ice bath and stirred, and 30 ml of chloroform solution of NBS (7.079 g, 60 mmol) was added dropwise. The mixture was wrapped with aluminum foil and reacted for 8 h. The solvent was removed by distillation under reduced pressure and purified by dichloromethane / petroleum ether column chromatography to give intermediate 3 as a white solid (yield 90%). 1H NMR (400 MHz, CDCl3): δ 8.06 (d, J = 1.6 Hz, 1H), 8.05 (s, 1H), 8.03 (d, J = 1.4 Hz, 1H), 7.61 (d, J = 1.5 Hz, 1H), 7.52 (dd, J = 8.6, 1.8 Hz, 1H), 7.40 (d, J = 8.5 Hz, 1H), 1.47 (d, J = 3.6 Hz, 18H).

[0169] 4) Preparation of Intermediate 4

[0170] The synthesis path is as follows:

[0171] The preparation method specifically comprises the following steps:

[0172] Intermediate 3 (358 mg, 1 mmol), pinacol borane (0.8 mL, 5 mmol), [bis(triphenylphosphino)] palladium dichloride (70.2 mg, 0.1 mmol), and triethylamine (1.49 mL) were dissolved in 10 ml of ultra-dry 1,4-dioxane solvent and refluxed at 108°C overnight. The reaction solution was filtered through celite, and the filtrate was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) to obtain a white solid intermediate 4 (yield 95%). NMR (400MHz, CDCl3): δ8.96(s,1H),8.22(d,J=2.0Hz,1H),8.08(d,J=1.6Hz,1H),7.89( d, J=2.0Hz, 1H), 7.47 (dd, J=8.5, 1.9Hz, 1H), 7.40 (d, J=8.5Hz, 1H), 1.50-1.41 (m, 30H).

[0173] 5) Preparation of Intermediate 5

[0174] The synthesis path is as follows:

[0175] The preparation method specifically comprises the following steps:

[0176] Intermediate 3 (700 mg, 1.955 mmol), intermediate 1 (708 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) to obtain yellow-green solid intermediate 5 (yield 98%). The product emitted sky blue light under 365 nm ultraviolet light, 1H NMR (500MHz, CDCl3) δ8.98-8.95(m,2H),8.84-8.82(m,4H),8.21(s,1H),8.13(dd,J=5.5Hz,J=1.5Hz,2H),7.94-7 .92(m,2H),7.64-7.58(m,7H),7.50(dd,J=8.5Hz,J=2.0Hz,1H),7.36(d,J=8.5Hz,1H),1.53(s,9H),1.47(s,9H).

[0177] 6) Preparation of Intermediate 6

[0178] The synthesis path is as follows:

[0179] The preparation method specifically comprises the following steps:

[0180] Intermediate 3 (700 mg, 1.955 mmol), intermediate 2 (708 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and distilled under reduced pressure. Purification by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) gave a green solid intermediate 6 (yield 88%). The product emitted sky blue light under a 365 nm UV lamp. 1H NMR (500MHz, CDCl3) δ8.79-8.77(m,2H),8.50-8.48(m,2H),8.35-8.33(m,2H),8.18(s,1H),8.13(t,J=2.5Hz,2H),8.11(s,1 H),7.92-7.91(m,2H),7.62-7.54(m,7H),7.49(dd,J=8.5Hz,J=1.5Hz,1H),7.35(d,J=8.5Hz,1H),1.52(s,9H),1.47(s,9H).

[0181] 7) Preparation of Intermediate 7

[0182] The synthesis path is as follows:

[0183] The preparation method specifically comprises the following steps:

[0184] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-1 (665 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and distilled under reduced pressure. The mixture was purified by column chromatography (eluent: petroleum ether: dichloromethane = 5:1) to give yellow solid intermediate 7 (yield 75%).

[0185] 8) Preparation of Intermediate 8

[0186] The synthesis path is as follows:

[0187] The preparation method specifically comprises the following steps:

[0188] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-2 (300 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water. The extract was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether:dichloromethane = 2:1) to give yellow solid intermediate 8 (yield 60%). 1H NMR (500 MHz, CDCl3) δ 8.46 (m, 1H), 8.36 (d, J = 8.0 Hz 1H),8.23(m,1H),8.18(s,1H),7.84(t,J=2.5Hz,4H),7.62-7.50(m,2H),1.43(s,9H),1.32(s,9H).

[0189] 9) Preparation of Intermediate 9

[0190] The synthesis path is as follows:

[0191] The preparation method specifically comprises the following steps:

[0192] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-3 (340 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether:dichloromethane = 5:1) to give intermediate 9 as a white solid (yield 60%). 1H NMR (500 MHz, CDCl3) δ 9.21 (d, J = 8.5 Hz, 2H), 8.58 (d, J = 8.0 Hz 1H),8.33(m,1H),8.18(s,1H),7.66-7.55(m,2H),1.50(s,9H),1.44(s,9H).

[0193] 10) Preparation of Intermediate 10

[0194] The synthesis path is as follows:

[0195] The preparation method specifically comprises the following steps:

[0196] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-4 (470 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water. The mixture was stirred and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water. The mixture was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether: dichloromethane = 10:1) to give a white product (yield 75%).

[0197] The product obtained in the previous step (970 mg, 2 mmol) and 1,2-phenylenediamine (216 mg, 2 mmol) were then added to a double-necked reaction flask, and 20 mL of n-butanol was injected under a nitrogen atmosphere. The reaction was refluxed at 120°C for 12 hours. After the reaction was completed, the solvent was dried and purified by column chromatography to obtain a dark yellow product 10 (yield 98%). 1H NMR (500 MHz, CDCl3) δ9.53 (d, J = 8.0 Hz, 1H), 9.47-9.45 (m, 1H), 8.86 (d, J = 1.5 Hz, 1H), 8.60-8.58 (m, 1H), 8.42-8.37 (m, 3H), 8.20 (dd, J = 10.0 Hz, J = 1.5 Hz, 2H), 8.06 (dd, J = 8. 5Hz,J=1.5Hz,1H),7.93-7.89(m,2H),7.82-7.78(m,2H),7.69(d,J=2.0Hz,J=1.5Hz,1 H), 7.53 (dd, J = 8.5Hz, J = 2.0Hz, 1H), 7.42 (d, J = 5.5Hz, 1H), 1.59 (s, 10H), 1.51 (s, 9H).

[0198] 11) Preparation of Intermediate 11

[0199] The synthesis path is as follows:

[0200] The preparation method specifically comprises the following steps:

[0201] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-5 (538 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water. The mixture was stirred and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water. The mixture was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether: dichloromethane = 7:1) to give intermediate 11 as a yellow solid (yield 77%). 1H NMR (500MHz, DMSO-d6) δ11.70(s,1H),9.66(d,J=8.0Hz,1H),9.50-9.42(m,2H),8.80(d,J=1.5Hz,1H),8.20(dd,J=10.0Hz,J=1.5Hz, 2H), 8.06 (dd, J=8.5Hz, J=1.5Hz, 2H), 7.91 (m, 2H), 7.53 (dd, J=8.5Hz, J=2.0Hz, 1H), 7.42 (d, J=5.5Hz, 1H), 1.60 (s, 9H), 1.51 (s, 9H).

[0202] 12) Preparation of Intermediate 12

[0203] The synthesis path is as follows:

[0204] The preparation method specifically comprises the following steps:

[0205] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-6 (586 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 15:1) to give yellow solid intermediate 12 (yield 50%). NMR(500MHz, CDCl3)δ9.02(d,J=8.0Hz,1H),8.95(m,1H),8.80(d,J=1.5Hz,1H) ,8.60(m,1H),8.22(m,3H),8.10(dd,J=10.0Hz,J=1.5Hz,2H),7.96(dd,J=8.5H z,J=1.5Hz,1H),7.80(m,2H),7.72(m,2H),7.60(d,J=2.0Hz,J=1.5Hz,1H),7.4 3(dd,J=8.5Hz,J=2.0Hz,1H),7.03(d,J=5.5Hz,1H),1.66(s,9H),1.55(s,9H).

[0206] 13) Preparation of Intermediate 13

[0207] The synthesis path is as follows:

[0208] The preparation method specifically comprises the following steps:

[0209] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-7 (570 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 8:1) to give a light yellow solid intermediate 13 (yield 53%). NMR (500MHz, CDCl3) δ (ppm): 8.71 (dd, J=8.0, 2.0Hz, 2H), 8.38 (s, 1H), 8.17 (dd, J=12.5, 2.0Hz, 2H), 7.74 (t, J=7.8H z,2H),7.67(s,1H),7.60-7.58(m,4H),7.51(dd,J=8.5,2.0Hz,1H),7.46–7.36(m,3H),1.56(s,9H),1.50(s,9H).13C NMR (500MHz, CDCl3) δ (ppm): 160.73, 158.15, 146.84, 143.08, 142.69, 138.21, 135.87, 134.76, 133.85, 124.29, 124.07, 123.97,123.64,123.54,123.10,122.53,118.61,116.64,116.47,113.91,110.42,108.39,35.02,34.90,32.27,32.20.

[0210] 14) Preparation of Intermediate 14

[0211] The synthesis path is as follows:

[0212] The preparation method specifically comprises the following steps:

[0213] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-8 (467 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water. The mixture was stirred and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water. The mixture was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether: dichloromethane = 5:1) to give intermediate 14 as a yellow solid (yield 88%). 1H NMR (500MHz, DMSO-d6) δ10.07 (s, 1H), 9.28 (d, J = 8.5Hz, 2H), 9.00 (d, J = 8.0Hz 2H),8.88(t,J=8.0Hz,1.5Hz1H),8.33(m,4H),8.18(s,1H),7.66-7.55(m,2H),1.50(s,9H),1.44(s,9H).

[0214] 15) Preparation of Intermediate 15

[0215] The synthesis path is as follows:

[0216] The preparation method specifically comprises the following steps:

[0217] Carbazole (8.35 g, 50 mmol) was added to 300 ml of chloroform solution, and the mixture was cooled to 0°C in an ice bath with stirring. 30 ml of chloroform solution containing NBS (7.079 g, 60 mmol) was added dropwise. The mixture was wrapped with aluminum foil and allowed to react for 8 h. The solvent was removed by distillation under reduced pressure, and the mixture was purified by dichloromethane / petroleum ether column chromatography to obtain intermediate 15 as a white solid (yield 90%).

[0218] 16) Preparation of Intermediate 16

[0219] The synthesis path is as follows:

[0220] The preparation method specifically comprises the following steps:

[0221] Intermediate 15 (250 mg, 1 mmol), pinacol borane (0.8 mL, 5 mmol), [bis(triphenylphosphino)]palladium dichloride (70.2 mg, 0.1 mmol), and triethylamine (1.49 mL) were dissolved in 10 ml of ultra-dry 1,4-dioxane solvent and refluxed at 108°C overnight. The reaction solution was filtered through celite, and the filtrate was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether) to obtain intermediate 16 as a white solid (yield 30%).

[0222] 17) Preparation of Intermediate 17

[0223] The synthesis path is as follows:

[0224] The preparation method specifically comprises the following steps:

[0225] Intermediate 15 (500 mg, 1.955 mmol), intermediate 1 (708 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 15:1) to give a light green solid intermediate 17 (yield 78%). NMR (500MHz, CDCl3) δ8.97 (m, 2H), 8.86 (m, 4H), 8.21 (s, 1H), 8.15 (dd, J = 5.5Hz, J = 1.5Hz ,4H),7.92(m,2H),7.60(m,7H),7.40(dd,J=8.5Hz,J=2.0Hz,1H),7.36(d,J=8.5Hz,1H).

[0226] 18) Preparation of Intermediate 18

[0227] The synthesis path is as follows:

[0228] The preparation method specifically comprises the following steps:

[0229] Intermediate 16 (596 mg, 1.955 mmol), intermediate 1-7 (570 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 5:1) to give yellow solid intermediate 18 (yield 67%). NMR (500MHz, CDCl3) δ (ppm): 8.77 (dd, J=8.0, 2.0Hz, 2H), 8.35 (s, 1H), 8.10 (dd, J=12.5, 2.0Hz, 2H),7.67(t,J=7.8Hz,2H),7.66(s,1H),7.52(m,6H),7.41(dd,J=8.5,2.0Hz,1H),7.30(m,3H).

[0230] 19) Preparation of Intermediate 19

[0231] The synthesis path is as follows:

[0232] The preparation method specifically comprises the following steps:

[0233] Carbazole (20 g, 50 mmol) was added to 300 ml of chloroform solution, and the mixture was cooled to 0°C in an ice bath with stirring. 30 ml of chloroform solution containing NBS (7.079 g, 60 mmol) was added dropwise. The mixture was wrapped with aluminum foil and allowed to react for 8 h. The solvent was removed by distillation under reduced pressure, and the mixture was purified by dichloromethane / petroleum ether column chromatography (50:1) to obtain intermediate 19 as a white solid (yield 90%).

[0234] 20) Preparation of Intermediate 20

[0235] The synthesis path is as follows:

[0236] The preparation method specifically comprises the following steps:

[0237] Intermediate 19 (482 mg, 1 mmol), pinacol borane (0.8 mL, 5 mmol), [bis(triphenylphosphino)]palladium dichloride (70.2 mg, 0.1 mmol), and triethylamine (1.49 mL) were dissolved in 10 ml of ultra-dry 1,4-dioxane solvent and refluxed at 108°C overnight. The reaction solution was filtered through celite, and the filtrate was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) to obtain intermediate 20 as a white solid (yield 80%).

[0238] 21) Preparation of Intermediate 21

[0239] The synthesis path is as follows:

[0240] The preparation method specifically comprises the following steps:

[0241] Intermediate 19 (800 mg, 1.955 mmol), intermediate 1 (708 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether:dichloromethane = 15:1) to give a light green solid intermediate 21 (yield 78%). 1H NMR (500 MHz, CDCl3) δ 8.80 (m, 2H), 8.49 (m, 2H), 8.34 (m, 2H), 8.20 (s, 1H), 8.15 (t, J = 2.5 Hz, 2H), 8.11 (s, 1H), 7.92-7.91(m,4H),7.62-7.54(m,7H),7.49(dd,J=8.5Hz,J=1.5Hz,2H),7 .35(d,J=8.5Hz,2H),2.92(s,6H),2.88(s,6H),2.48(s,3H),2.35(s,3H).

[0242] 22) Preparation of Intermediate 22

[0243] The synthesis path is as follows:

[0244] The preparation method specifically comprises the following steps:

[0245] Intermediate 20 (1060 mg, 1.955 mmol), intermediate 1-7 (570 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 5:1) to give yellow solid intermediate 22 (yield 67%). NMR (500MHz, CDCl3) δ (ppm): 8.98 (dd, J = 8.0, 2.0Hz, 2H), 8.55 (s, 1H), 8.37 (dd, J = 12.5, 2.0Hz, 2H), 7.88 (t, J = 7.8Hz, 2H) ,7.80(s,1H),7.66(m,6H),7.58(dd,J=8.5,2.0Hz,1H),7.45(m,5H),2.89(s,6H),2.8.(s,6H),2.40(s,3H),2.29(s,3H).

[0246] 23) Preparation of Intermediate 23

[0247] The synthesis path is as follows:

[0248] The preparation method specifically comprises the following steps:

[0249] Intermediate 3 (700 mg, 1.955 mmol), intermediate 1-9 (199 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) to obtain white solid intermediate 23 (yield 74%). The product emitted sky blue light under a 365 nm ultraviolet lamp. NMR (500MHz, DMSO) δ10.81 (s, 1H, NH), 8.17 (s, 2H), 7.73 (m, 2H), 7.58 (t, J = 7.5Hz, 2H), 7.43 (m, 4H), 1.45 (s, 9H), 1.41 (s, 9H).

[0250] 24) Preparation of Intermediate 24

[0251] The synthesis path is as follows:

[0252] The preparation method specifically comprises the following steps:

[0253] Intermediate 3 (700 mg, 1.955 mmol), intermediate 1-10 (603 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) to obtain white solid intermediate 24 (yield 66%). The product emitted sky blue light under a 365 nm ultraviolet lamp. NMR (500MHz, CDCl3) δ8.23(s,1H),8.19(d,J=7.5Hz,2H),8.14(d,J=2.0Hz,2H),7.94(m,2H),7.76(m,2H),7.58(d,J=2.0Hz,1H),7 .56(d,J=8.0Hz,2H),7.50(dd,J=8.5Hz,J=2.0Hz,1H),7.46(m,2H),7.39(d,J=8.0Hz,1H),7.33(m,2H),1.53(s,9H),1.48(s,9H).

[0254] 25) Preparation of Intermediate 25

[0255] The synthesis path is as follows:

[0256] The preparation method specifically comprises the following steps:

[0257] Intermediate 3 (700 mg, 1.955 mmol), intermediate 1-11 (668 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether: dichloromethane = 20:1) to obtain white solid intermediate 25 (yield 61%). The product emitted sky blue light under a 365 nm ultraviolet lamp, 1H NMR (500MHz, CDCl3) δ8.25(s,1H,NH),8.13(d,J=1.5Hz,2H),7.96(d,J=8.5Hz,2H),7.59(d,J=2.0Hz,1H),7.50(m,5H),7.40(d,J= 8.5Hz, 1H), 7.03 (m, 2H), 6.96 (td, J = 7.5Hz, J = 1.0Hz, 2H), 6.45 (dd, J = 8.5Hz, J = 1.0Hz, 2H), 1.73 (s, 6H), 1.53 (s, 9H), 1.48 (s, 9H).

[0258] 26) Preparation of Intermediate 26

[0259] The synthesis path is as follows:

[0260] The preparation method specifically comprises the following steps:

[0261] Intermediate 3 (700 mg, 1.955 mmol), intermediate 1-12 (630 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water, evaporated under reduced pressure, and purified by column chromatography (eluent: petroleum ether:dichloromethane = 20:1) to obtain white solid intermediate 26 (yield 77%). The product emitted sky blue light under 365 nm ultraviolet light, 1H NMR (400MHz, Acetone) δ10.23(s,1H,NH),8.28(dd,J=10.4Hz,J=2.0Hz,2H),8.08(m,2H),7.64(d,J=1.6Hz,1H),7.57 (m,2H),7.50(dd,J=8.4Hz,J=2.0Hz,1H),7.44(d,J=8.4Hz,1H),6.71(m,6H),6.08(m,2H),1.52(s,9H),1.45(s,9H).

[0262] 27) Preparation of Intermediate 27

[0263] The synthesis path is as follows:

[0264] The preparation method specifically comprises the following steps:

[0265] Intermediate 4 (791 mg, 1.955 mmol), intermediate 1-13 (570 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water, stirred, and slowly heated to 108°C. The reaction was allowed to proceed overnight, extracted with dichloromethane and water, and evaporated under reduced pressure. The mixture was purified by column chromatography (eluent: petroleum ether:dichloromethane = 8:1) to give intermediate 27 as a light yellow solid (yield 53%). 1H NMR (500 MHz, DMSO) δ 10.86 (s, 1H, NH), 8.16 (s, 2H), 7.43 (m, 5H), 7.03 (m, 8H), 1.44 (s, 9H), 1.41 (s, 9H).

[0266] 28) Preparation of Intermediate 28

[0267] The synthesis path is as follows:

[0268] The preparation method specifically comprises the following steps:

[0269] Intermediate 16 (586 mg, 1.955 mmol), intermediate 1-4 (470 mg, 1.63 mmol), K2CO3 (1.126 g, 8.15 mmol), and tetrakis(triphenylphosphine)palladium (95 mg, 0.0815 mmol) were dissolved in 30 ml of ultra-dry tetrahydrofuran solution and 10 ml of deoxygenated water. The mixture was stirred and slowly heated to 108°C. The reaction was allowed to proceed overnight, and the mixture was extracted with dichloromethane and water. The mixture was evaporated under reduced pressure and purified by column chromatography (eluent: petroleum ether: dichloromethane = 10:1) to give a white product (yield 80%).

[0270] The product obtained in the previous step (970 mg, 2 mmol) and 1,2-phenylenediamine (216 mg, 2 mmol) were then added to a double-necked reaction flask. 20 mL of n-butanol was injected under a nitrogen atmosphere and the reaction was refluxed at 120°C for 12 hours. After the reaction was completed, the solvent was dried and purified by column chromatography to obtain a dark yellow product 28 (yield 90%). NMR(600MHz,Chloroform-d)δ9.56(d,J=8.1Hz,1H),9.48–9.44(m,1H),8.87(d, J=1.6Hz,1H),8.63–8.60(m,1H),8.52(s,1H),8.42–8.35(m,2H),8.18(dd,J=7.7 ,5.9Hz,2H),8.07(dd,J=8.2,1.6Hz,1H),7.93–7.86(m,2H),7.84–7.77(m,2H),7 .66(dd,J=7.2,1.1Hz,1H),7.51–7.41(m,3H),7.30(ddd,J=8.0,6.5,1.5Hz,1H).

[0271] Example 3

[0272] This embodiment provides a method for preparing a metal complex PtNCN1-12, and its synthesis path is as follows:

[0273] The preparation method specifically comprises the following steps:

[0274] Intermediate 10 (190 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and reacted at room temperature overnight. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a red powder, which is the metal complex PtNCN1-12 (yield 75%). NMR (400MHz, CDCl3) δ9.18 (dd, J=8.0Hz, J=1.2Hz, 1H), 8.48 (m, 2H), 8.36 (m, 3H), 8.30(m,1H),8.22(s,1H),7.92(m,2H),7.70(m,2H),7.65(d,J=8.8Hz,2H),7.54(m ,2H),7.46(d,J=2.4Hz,1H),7.33(dd,J=8.4Hz,J=2.0Hz,1H),7.15(m,2H),6.94( t,J=5.6Hz,3H),6.35(m,3H),5.97(t,J=7.6Hz,1H),1.60(s,9H),1.52(s,9H).13C NMR (126MHz, CDCl3) δ167.45,166.11,151.80,149.42,148.07,144.81,142.43,142.21,1 42.13,141.69,138.11,137.78,137.58,132.26,131.05,130.16,129.71,129.43,129.37 ,129.18,129.10,127.87,126.95,126.64,126.08,125.68,125.50,124.90,124.44,122.80,121.86,121.68,121.39,118.73,115.34,115.28,114.16,34.69,34.61,32.47,32.39.

[0275] Example 4

[0276] This embodiment provides a method for preparing a metal complex PtNCN2-12, and its synthesis path is as follows:

[0277] The preparation method specifically comprises the following steps:

[0278] Intermediate 10 (190 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN2 (482 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a red powder complex PtNCN2-12 (yield 70%).

[0279] Example 5

[0280] This embodiment provides a method for preparing a metal complex PtNCN3-12, and its synthesis path is as follows:

[0281] The preparation method specifically comprises the following steps:

[0282] Intermediate 10 (190 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN3 (450 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a red powder complex PtNCN3-12 (yield 65%).

[0283] Example 6

[0284] This embodiment provides a method for preparing a metal complex PtCCC1-12, and its synthesis path is as follows:

[0285] The preparation method specifically comprises the following steps:

[0286] Intermediate 10 (190 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtCCC1 (553 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a red powder complex PtCCC1-12 (yield 63%).

[0287] Example 7

[0288] This embodiment provides a method for preparing a metal complex PtNCN1-5, and its synthesis path is as follows:

[0289] The preparation method specifically comprises the following steps:

[0290] Intermediate 6 (200 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and reacted at room temperature overnight. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane: n-hexane = 1:100 to obtain a yellow powder complex PtNCN1-5 (yield 55%), 1H NMR (500MHz, CDCl3) δ8.66 (dd, J=7.7, 1.8Hz, 2H), 8.30 (dd, J=9.7, 1.9Hz, 2H), 8.22 (dd, J=7.8,1.5Hz,2H),7.93(dd,J=12.7,6.6Hz,2H),7.85(td,J=7.8,1.5Hz,2H),7.69(d,J= 8.5Hz,1H),7.60(m,7H),7.52(d,J=7.7Hz,2H),7.45(d,J=8.1Hz,2H),7.33(m,5H),7.05 (d, J=7.7Hz, 2H), 6.94 (t, J=6.6Hz, 2H), 6.64 (t, J=7.7Hz, 1H), 1.54 (s, 9H), 1.49 (s, 9H).

[0291] Example 8

[0292] This embodiment provides a method for preparing a metal complex PtNCN1-3, and its synthesis path is as follows:

[0293] The preparation method specifically comprises the following steps:

[0294] Intermediate 5 (201 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange powder complex PtNCN1-3 (yield 75%). 1H NMR (500MHz, CDCl3) δ8.70(dd,J=8.2,1.3Hz,4H),8.30(dd,J=8.6,1.9Hz,2H),7.88(m,6H),7.65(m,7H),7.48(d,J=7.7Hz,2H),7.33(dd,J=8.6,2.0H z,2H),7.31(d,J=2.0Hz,2H),7.26(m,1H),6.94(ddd,J=7.2,5.7,1.3Hz,2 H), 6.88 (d, J = 7.7Hz, 2H), 6.48 (t, J = 7.6Hz, 1H), 1.54 (s, 9H), 1.49 (s, 9H).

[0295] Example 9

[0296] This embodiment provides a method for preparing a metal complex PtNCN1-1, and its synthesis path is as follows:

[0297] The preparation method specifically comprises the following steps:

[0298] Intermediate 8 (130 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a yellow-green powder complex PtNCN1-1 (yield 71%).

[0299] Example 10

[0300] This embodiment provides a method for preparing a metal complex PtNCN1-7, and its synthesis path is as follows:

[0301] The preparation method specifically comprises the following steps:

[0302] Intermediate 9 (165 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange powder complex PtNCN1-7 (yield 63%).

[0303] Example 11

[0304] This embodiment provides a method for preparing a metal complex PtNCN1-16, and its synthesis path is as follows:

[0305] The preparation method specifically comprises the following steps:

[0306] Intermediate 7 (206 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a red powder complex PtNCN1-16 (yield 80%).

[0307] Example 12

[0308] This embodiment provides a method for preparing a metal complex PtNCN1-A8, and its synthesis path is as follows:

[0309] The preparation method specifically comprises the following steps:

[0310] Intermediate 22 (230 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a yellow powder complex PtNCN1-A8 (yield 70%).

[0311] Example 13

[0312] This embodiment provides a method for preparing a metal complex PtCNN1-18, and its synthesis path is as follows:

[0313] The preparation method specifically comprises the following steps:

[0314] Intermediate 11 (180 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtCNN (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure and washed with cold n-pentane to obtain a red powder complex PtCNN1-5 (yield 75%).

[0315] Example 14

[0316] This embodiment provides a method for preparing a metal complex PtNCN1-14, and its synthesis path is as follows:

[0317] The preparation method specifically comprises the following steps:

[0318] Intermediate 12 (190 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN1-14 (yield 67%).

[0319] Example 15

[0320] This embodiment provides a method for preparing a metal complex PtNCN1-17, and its synthesis path is as follows:

[0321] The preparation method specifically comprises the following steps:

[0322] Intermediate 13 (186 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a yellow-green powder complex PtNCN1-17 (yield 63%).

[0323] Example 16

[0324] This embodiment provides a method for preparing a metal complex PtNCN3-16, and its synthesis path is as follows:

[0325] The preparation method specifically comprises the following steps:

[0326] Intermediate 7 (206 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN3 (154 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN3-16 (yield 61%).

[0327] Example 17

[0328] This embodiment provides a method for preparing a metal complex PtNCN1-B2, and its synthesis path is as follows:

[0329] The preparation method specifically comprises the following steps:

[0330] Intermediate 17 (165 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN1-B2 (yield 70%).

[0331] Example 18

[0332] This embodiment provides a method for preparing a metal complex PtNCN1-B8, and its synthesis path is as follows:

[0333] The preparation method specifically comprises the following steps:

[0334] Intermediate 18 (150 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized from dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN1-B8 (yield 60%).

[0335] Example 19

[0336] This embodiment provides a method for preparing a metal complex PtNCN1-A2, and its synthesis path is as follows:

[0337] The preparation method specifically comprises the following steps:

[0338] Intermediate 21 (242 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN1-A2 (yield 70%).

[0339] Example 20

[0340] This embodiment provides a method for preparing a metal complex PtNCN1-19, and its synthesis path is as follows:

[0341] The preparation method specifically comprises the following steps:

[0342] Take tert-butylcarbazole (95 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol), dissolve them in 20 ml of ultra-dry tetrahydrofuran solution, stir at room temperature for 1 h, then add the intermediate ClPtNCN1 (157 mg, 0.3413 mmol), react at room temperature overnight, filter the reaction solution with diatomaceous earth, distill the filtrate under reduced pressure, wash with cold n-pentane, and then recrystallize with dichloromethane: n-hexane = 1:100 to obtain a yellow-green powder complex PtNCN1-19 (yield 63%), 1H NMR (600MHz, CDCl3) δ8.30(d,J=1.8Hz,2H),8.10(dd,J=5.7,0.9Hz,2H),7.89(td,J=7.8,1.6Hz,2H),7.77(d,J=7.9 Hz, 2H), 7.70 (d, J = 8.5Hz, 2H), 7.61 (d, J = 7.7Hz, 2H), 7.35 (m, 4H), 6.96 (ddd, J = 7.3, 5.7, 1.4Hz, 2H), 1.60 (s, 18H).

[0343] Example 21

[0344] This embodiment provides a method for preparing a metal complex PtNCN1-20, and its synthesis path is as follows:

[0345] The preparation method specifically comprises the following steps:

[0346] Intermediate 23 (120 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN1-20 (yield 53%). 1H NMR (400MHz, CDCl3) δ8.30(s,2H),7.97(d,J=5.4Hz,2H),7.84(td,J=7.9,1.3Hz,2H),7.70(d,J=8.5Hz,2H),7.62(d,J=7.7Hz,2H),7.45(d,J=7 .7Hz,2H),7.32(dd,J=8.5,1.9Hz,2H),7.25(m,2H),7.21(d,J=7.8Hz,1H),6.90(dd,J=9.5,3.5Hz,2H),6.59(m,3H),1.53(s,9H),1.51(s,9H).

[0347] Example 22

[0348] This embodiment provides a preparation method of a metal complex PtNCN1-21, and its synthesis path is as follows:

[0349] The preparation method specifically comprises the following steps:

[0350] Intermediate 24 (177 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN1-21 (yield 66%). 1H NMR (400MHz, CDCl3) δ8.34(dd,J=14.2,1.8Hz,2H),8.16(d,J=5.7Hz,2H),8.05(dd,J=6.2,2.3Hz,2H),7.83(m,2H),7.71(d,J=8.5Hz,1H),7.65(dd,J=7. 7,6.0Hz,4H),7.51(d,J=7.7Hz,2H),7.36(d,J=2.0Hz,1H),7.32(dd,J=8.7, 2.1Hz,2H),7.22(m,4),6.98(m,4H),6.83(m,2H),1.58(s,9H),1.51(s,9H).

[0351] Example 23

[0352] This embodiment provides a method for preparing a metal complex PtNCN3-22, and its synthesis path is as follows:

[0353] The preparation method specifically comprises the following steps:

[0354] Intermediate 25 (192 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN3-22 (yield 76%).

[0355] Example 24

[0356] This embodiment provides a method for preparing a metal complex PtNCN3-23, and its synthesis path is as follows:

[0357] The preparation method specifically comprises the following steps:

[0358] Intermediate 26 (192 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN3-23 (yield 73%).

[0359] Example 25

[0360] This embodiment provides a method for preparing a metal complex PtNCN3-24, and its synthesis path is as follows:

[0361] The preparation method specifically comprises the following steps:

[0362] Intermediate 27 (188 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 ml of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPtNCN1 (157 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized from dichloromethane:n-hexane = 1:100 to obtain an orange-red powder complex PtNCN3-24 (yield 80%).

[0363] Example 26

[0364] This embodiment provides a method for preparing a metal complex PdCCC1-3, and its synthesis path is as follows:

[0365] The preparation method specifically comprises the following steps:

[0366] Intermediate 10 (200 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 mL of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPdCCC1 (160 mg, 0.3413 mmol) was added and reacted at room temperature overnight. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange powder complex PdCCC1-3 (yield 70%). 1H NMR (600 MHz, CDCl3)δ8.75(d,J=8.1Hz,4H),8.21(s,1H),8.15(s,1H),8.02(d,J=7.9Hz,2H),7 .67(m,6H),7.57(d,J=8.4Hz,1H),7.43(d,J=7.9Hz,2H),7.31(s,1H),7.28(m,2H) ,6.79(s,2H),6.38(m,1H),6.31(d,J=7.8Hz,2H),3.31(m,2H),3.10(m,2H),1.55( s,9H),1.48(s,9H),1.18(m,4H),0.52(m,2H),0.44(t,J=7.1Hz,6H),0.26(m,2H).

[0367] Example 27

[0368] This embodiment provides a method for preparing a metal complex PdCCC1-12, and its synthesis path is as follows:

[0369] The preparation method specifically comprises the following steps:

[0370] Intermediate 10 (190 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 mL of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPdCCC1 (160 mg, 0.3413 mmol) was added and reacted at room temperature overnight. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain a red powder complex PdCCC1-12 (yield 63%). NMR (400MHz, CDCl3) δ9.17 (dd, J=8.0, J=1.0Hz, 1H), 8.62 (d, J=8.0Hz, 1H), 8.53 (s, 1H), 8.35-8.31 (m, 1H) ,8.29-8.25(m,1H),8.23(s,1H),8.14(d,J=1.7Hz,1H),7.87(dq,J=6.7,J=3.3Hz,2H),7.69(d,J=8.1Hz,1 H),7.55(t,J=7.2Hz,1H),7.33(m,4H),7.11-7.0(m,1H),6.72(s,2H),6.62(d,J=1.6Hz,2H),5.83(t,J=7. 8Hz,1H),5.67(d,J=7.7Hz,2H),3.29-3.15(m,4H),1.55(s,9H),1.45(s,9H),1.18(s,4H),0.39(m,6H).13C NMR (126MHz, CDCl3) δ145.10,142.68,142.40,142.07,141.67,132.31,130 .82,130.08,129.53,129.46,129.33,129.27,129.16,129.03,127.24,126. 39,125.76,124.25,123.12,122.08,119.50,118.56,114.54,113.86,108.02,107.89,106.43,49.35,33.95,32.18,32.06,19.19,13.90,13.84,13.54.

[0371] Example 28

[0372] This embodiment provides a method for preparing a metal complex PdCCC1-5, and its synthesis path is as follows:

[0373] The preparation method specifically comprises the following steps:

[0374] Intermediate 10 (200 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 mL of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPdCCC1 (160 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized from dichloromethane:n-hexane = 1:100 to obtain an orange powder complex PdCCC1-5 (yield 72%).

[0375] Example 29

[0376] This embodiment provides a method for preparing a metal complex PdCCC1-17, and its synthesis path is as follows:

[0377] The preparation method specifically comprises the following steps:

[0378] Intermediate 13 (186 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 mL of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPdCCC1 (160 mg, 0.3413 mmol) was added and reacted at room temperature overnight. The reaction solution was filtered through celite, and the filtrate was distilled under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange powder complex PdCCC1-17 (yield 72%). NMR(600MHz,Chloroform-d)δ8.51(dd,J=7.7,1.7Hz,2H),8.20(d,J=2.0Hz,1H),8.12(d, J=2.0Hz,1H),7.62(ddd,J=8.4,6.9,1.6Hz,2H),7.51(d,J=8.5Hz,1H),7.33–7.31(m,2H) ,7.23(dd,J=8.5,1.9Hz,1H),7.19(d,J=7.9Hz,2H),7.05(s,2H),6.79(d,J=1.8Hz,2H),6 .72(d,J=1.8Hz,2H),6.29(t,J=7.8Hz,1H),5.83(d,J=7.8Hz,2H),3.31–3.25(m,2H),3.19 –3.13(m,2H),1.52(s,9H),1.44(s,9H),1.23–1.13(m,4H),0.50–0.44(m,2H),0.38(t,J=7.2Hz,6H),0.24–0.17(m,2H).

[0379] Example 30

[0380] This embodiment provides a method for preparing a metal complex PdCCC1-B5, and its synthesis path is as follows:

[0381] The preparation method specifically comprises the following steps:

[0382] Intermediate 28 (152 mg, 0.3413 mmol) and potassium tert-butoxide (46 mg, 0.409 mmol) were dissolved in 20 mL of ultra-dry tetrahydrofuran solution and stirred at room temperature for 1 h. Then, intermediate ClPdCCC1 (160 mg, 0.3413 mmol) was added and the reaction was allowed to proceed overnight at room temperature. The reaction solution was filtered through celite, and the filtrate was evaporated under reduced pressure, washed with cold n-pentane, and then recrystallized with dichloromethane:n-hexane = 1:100 to obtain an orange powder complex PdCCC1-B5 (yield 76%). NMR(600MHz,Chloroform-d)δ9.17(d,J=8.0Hz,1H),8.64(d,J=8.0Hz,1H),8.51(s,1H),8.34(dd,J=6.0,3.8Hz,1H),8.26(d, J=3.6Hz,2H),8.18(d,J=7.8Hz,1H),7.88(dd,J=6.4,3.4Hz,2H),7.66(d,J=8.1Hz,1H),7.61(d,J=8.1Hz,1H),7.56(t,J=7.4H z,1H),7.40–7.33(m,3H),7.19(t,J=7.2Hz,1H),7.16–7.12(m,1H),7.01–6.96(m,1H),6.72(s,2H),6.64(s,2H),5.86(t,J=7. 7Hz,1H),5.67(s,2H),3.22(s,4H),1.16(s,4H),0.47(dq,J=14.4,7.7,7.1Hz,2H),0.35(s,6H),0.26(dt,J=12.8,7.1Hz,2H).

[0383] Device Example 1

[0384] This embodiment provides an organic electroluminescent device, as shown in FIG1 , comprising an anode layer 1, a hole injection layer 2, a first hole transport layer 3, a second hole transport layer 4, an electron blocking layer 5, a light-emitting layer 6, a first electron transport layer 7, a second electron transport layer 8, an electron injection layer 9, and a cathode layer 10, which are sequentially arranged on a glass substrate 100 from bottom to top;

[0385] The materials used to manufacture the organic electroluminescent device are as follows:

[0386] The anode layer 1 is made of ITO, i.e., indium tin oxide; the hole injection layer 2 is made of 1,2-hexaazatriphenylene (HAT-CN); the first hole transport layer 3 is made of 4,4'-cyclohexylbis[N,N-bis(4-methylphenyl)aniline] (TAPC); the second hole transport layer 4 is made of tris(4-carbazolyl-9-ylphenyl)amine (TCTA); the electron blocking layer 5 is made of 3,3'-bis(9H-carbazol-9-yl)-1,1'-biphenyl; 3,3'-bis(9H-carbazol-9-yl)-1,1'-biphenyl (mCBP); the light-emitting layer 6 is formed by co-doping a host material and a guest material, wherein the host material is 5-(3-(4,6-diphenyl-1,3,5-triazin-2-yl)phenyl)- 7,7-dimethyl-5,7-dihydroindeno[2,1-b]carbazole (DMIC-TRZ), the guest material is the metal complex X of the present application, wherein X is PtNCN1-12, and the doping amount of the guest material accounts for 1% of the total mass of the host material and the guest material; the material of the first electron transport layer 7 is: 2,4,6-tris[3-(diphenylphosphinoyl)phenyl]-1,3,5-triazole (PO-T2T); the material of the second electron transport layer 8 is (1-(4-(10-([1,1'-biphenyl]-4-yl)anthracene-9-yl)phenyl)-2-ethyl-1H-benzo[d]-imidazole) (ANT-BIZ); the material of the electron injection layer 9 is Liq (8-hydroxyquinoline lithium); the material of the cathode layer 10 is metal Al material.

[0387] The device structure is ITO / hole injection layer (HAT-CN) (5 nm thick) / first hole transport layer (TAPC) (40 nm thick) / second hole transport layer (TCTA) (10 nm thick) / electron blocking layer (mCBP) (10 nm thick) / luminescent layer (DMIC-TRZ:X) (40 nm thick) / first electron transport layer (PO-T2T) (20 nm thick) / second electron transport layer (ANT-BIZ) (30 nm thick) / electron injection layer (Liq) (1.2 nm thick) / Al (100 nm thick). Where X is PtNCN1-12.

[0388] Device Example 2

[0389] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the doping amount of the guest material PtNCN1-12 in the light-emitting layer accounts for 3% of the total mass of the host material and the guest material.

[0390] Device Example 3

[0391] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the doping amount of the guest material PtNCN1-12 in the light-emitting layer accounts for 5% of the total mass of the host material and the guest material.

[0392] Device Example 4

[0393] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the doping amount of the guest material PtNCN1-12 in the light-emitting layer accounts for 10% of the total mass of the host material and the guest material.

[0394] Device Example 5

[0395] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-12, and the doping amount of PdCCC1-12 accounts for 1% of the total mass of the host material and the guest material.

[0396] Device Example 6

[0397] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-12, and the doping amount of PdCCC1-12 accounts for 3% of the total mass of the host material and the guest material.

[0398] Device Example 7

[0399] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-12, and the doping amount of PdCCC1-12 accounts for 5% of the total mass of the host material and the guest material.

[0400] Device Example 8

[0401] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-5, and the doping amount of PdCCC1-5 accounts for 1% of the total mass of the host material and the guest material.

[0402] Device Example 9

[0403] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-5, and the doping amount of PdCCC1-5 accounts for 3% of the total mass of the host material and the guest material.

[0404] Device Example 10

[0405] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-3, and the doping amount of PdCCC1-3 accounts for 1% of the total mass of the host material and the guest material.

[0406] Device Example 11

[0407] This embodiment provides an organic electroluminescent device, which differs from the organic electroluminescent device provided in Device Example 1 in that the guest material X in the light-emitting layer is PdCCC1-3, and the doping amount of PdCCC1-3 accounts for 3% of the total mass of the host material and the guest material.

[0408] Device Example 12

[0409] This embodiment provides an organic electroluminescent device, comprising an anode layer, a hole injection layer, a hole transport layer, an electron blocking layer, a light-emitting layer, an electron transport layer, an electron injection layer, and a cathode layer, which are sequentially arranged on a glass substrate from bottom to top;

[0410] The materials used to manufacture the organic electroluminescent device are as follows:

[0411] The anode layer is made of ITO material, that is, indium tin oxide material; the hole injection layer material is 1,2-hexaazatriphenylene (HAT-CN); the hole transport layer material is N4,N4,N4',N4'-tetrakis(4-biphenyl)-biphenyl-4,4'-diamine (TBBD); the electron blocking layer material is N-([1,1'-biphenyl]-2-yl)-N-(9,9-dimethyl-9H-fluorene-2-yl)-9,9'-spirobi[fluorene]-2-amine (o-SFAF); the light-emitting layer is formed by co-doping the host material and the guest material, wherein the host material is 5-(3-(4,6-diphenyl- The invention discloses a novel nanostructured ...

[0412] The device structure is ITO / hole injection layer (HAT-CN) (thickness of 5nm) / hole transport layer (TBBD) (thickness of 30nm) / electron blocking layer (o-SFAF) (thickness of 15nm) / light-emitting layer (DMIC-TRZ:PdCCC1-12) (thickness of 45nm) / electron transport layer (ANT-BIZ) (thickness of 40nm) / electron injection layer (Liq) (thickness of 2nm) / Al (thickness of 100nm).

[0413] Testing and characterization of metal complexes:

[0414] The metal complex PtNCN1-12 was analyzed by H-NMR spectroscopy, and its crystal structure is shown in FIG2 . The thermal stability of the metal complex PtNCN1-12 was analyzed, and FIG3 is a thermogravimetric analysis curve of PtNCN1-12.

[0415] The absorption spectrum and emission spectrum of the metal complex solution of the present application were tested, wherein the solution was a toluene solution or a tetrahydrofuran solution, the concentration of the metal complex in the toluene solution was 1×10-5mol L-1, and the concentration of the metal complex in the tetrahydrofuran solution was 1×10-5mol L-1. L-1; Figure 4 is an absorption spectrum of PdCCC1-B5 in toluene solution; Figure 5 is an absorption spectrum of PdCCC1-5 in toluene solution; Figure 6 is an absorption spectrum of PdCCC1-3 in toluene solution; Figure 7 is an emission spectrum of PdCCC1-B5 in toluene solution; Figure 8 is an emission spectrum of PdCCC1-5 in toluene solution; Figure 9 is an emission spectrum of PdCCC1-3 in toluene solution; Figure 10 is an absorption spectrum of PtNCN1-5 in toluene solution; Figure 11 is an absorption spectrum of PtNCN1-3 in toluene solution; Figure 12 is an absorption spectrum of PtNCN1-16 in toluene solution; Figure 13 is an absorption spectrum of PtNCN1-12 in toluene solution Figure 14 is the absorption spectrum of PtNCN1-20 in toluene solution; Figure 15 is the absorption spectrum of PtNCN1-21 in toluene solution; Figure 16 is the absorption spectrum of PtNCN3-16 in toluene solution; Figure 17 is the absorption spectrum of PtNCN3-22 in toluene solution; Figure 18 is the absorption spectrum of PtNCN3-23 in toluene solution; Figure 19 is the absorption spectrum of PtNCN3-24 in toluene solution; Figure 20 is the emission spectrum of PtNCN1-5 in tetrahydrofuran solution; Figure 21 is the emission spectrum of PtNCN1-3 in tetrahydrofuran solution; Figure 22 is the emission spectrum of PtNCN1-12 in toluene solution.

[0416] The emission spectra and lifetime of the metal complexes of the present application were tested in polymethyl methacrylate films, with the metal complexes being incorporated into the polymethyl methacrylate films at a concentration of 5 wt%. Figure 23 shows the emission spectra of PtNCN1-5 in polymethyl methacrylate films; Figure 24 shows the emission spectra of PtNCN1-3 in polymethyl methacrylate films; Figure 25 shows the emission spectra of PtNCN1-16 in polymethyl methacrylate films; Figure 26 shows the emission spectra of PtNCN1-12 in polymethyl methacrylate films; Figure 27 shows the emission spectra of PtNCN1-20 in polymethyl methacrylate films; and Figure 28 shows the emission spectra of PtNCN1-21 in polymethyl methacrylate films. Figure 29 is an emission spectrum of PtNCN3-22 in polymethyl methacrylate film; Figure 30 is an emission spectrum of PtNCN3-23 in polymethyl methacrylate film; Figure 31 is an emission spectrum of PtNCN3-24 in polymethyl methacrylate film; Figure 32 is an emission spectrum of PdCCC1-12 in polymethyl methacrylate film; Figure 33 is an emission spectrum of PdCCC1-3 in polymethyl methacrylate film; Figure 34 is a lifetime decay curve of PtNCN1-5 in polymethyl methacrylate film Figure 35 is a lifetime decay curve of PtNCN1-3 in polymethyl methacrylate film; Figure 36 is a lifetime decay curve of PtNCN1-16 in polymethyl methacrylate film; Figure 37 is a lifetime decay curve of PtNCN1-12 in polymethyl methacrylate film; Figure 38 is a lifetime decay curve of PtNCN1-20 in polymethyl methacrylate film; Figure 39 is a lifetime decay curve of PtNCN1-21 in polymethyl methacrylate film; Figure 40 is a lifetime decay curve of PtNCN3-16 in polymethyl methacrylate film Figure 41 is a lifetime decay curve diagram of PtNCN3-22 in polymethyl methacrylate film; Figure 42 is a lifetime decay curve diagram of PtNCN3-23 in polymethyl methacrylate film; Figure 43 is a lifetime decay curve diagram of PtNCN3-24 in polymethyl methacrylate film; Figure 44 is a lifetime decay curve diagram of PdCCC1-12 in polymethyl methacrylate film; Figure 45 is a lifetime decay curve diagram of PdCCC1-3 in polymethyl methacrylate film.

[0417] Test Example 1

[0418] The organic electroluminescent devices provided in device embodiments 1-4 were tested, and PtNCN-12 was selected as the guest material. The current-brightness-voltage characteristics of the devices were measured by a Keithley source measurement system (Keithley 2400 Sourcemeter, Keithley 2000 Currentmeter) with a calibrated silicon photodiode. All tests were completed in room temperature atmosphere. The test results are shown in Table 1 and Figures 46-47, where Figure 46 is an electroluminescence graph of device embodiments 1-4 of the present application based on the compound PtNCN1-12, and Figure 47 is an electroluminescence quantum efficiency graph of device embodiments 1-4 of the present application based on the compound PtNCN1-12.

[0419] Table 1 Device performance test results [a] Maximum brightness; [b] Current efficiency; [c] Lumen efficiency; [d] External quantum efficiency; [e] CIE coordinates (1000 cd m -2 )

[0420] As shown in Figures 46-47, the present application uses PtNCN1-12 as the guest material and prepares a doped luminescent OLED with a doping concentration of 1%. The maximum luminous brightness can reach 136834 cd m-2, the maximum current efficiency is 61.2 cd A-1, the maximum lumen efficiency is 60.7 lm W-1, the maximum external quantum efficiency is as high as 35.6%, and the CIE coordinates are (0.58, 0.42) at a brightness of 1000 cd m-2.

[0421] Test Example 2

[0422] The organic electroluminescent devices provided in device embodiments 5-7 were tested, and PdCCC1-12 was selected as the guest material. The current-brightness-voltage characteristics of the devices were measured by a Keithley source measurement system (Keithley 2400 Sourcemeter, Keithley 2000 Currentmeter) with a calibrated silicon photodiode. All tests were completed in room temperature atmosphere. The test results are shown in Table 2 and Figures 48-49, where Figure 48 is an electroluminescence graph of device embodiment 5-7 of the present application based on compound PdCCC1-12, and Figure 49 is an electroluminescence quantum efficiency graph of device embodiment 5-7 of the present application based on compound PdCCC1-12.

[0423] Table 2 Device performance test results [a] Maximum brightness; [b] Current efficiency; [c] Lumen efficiency; [d] External quantum efficiency; [e] CIE coordinates (1000 cd m -2 )

[0424] As shown in Figures 48-49, the doped luminescent OLED prepared in this application using PdCCC1-12 as the guest material and a doping concentration of 1% has a maximum luminous brightness of 92000 cd m-2, a maximum current efficiency of 29.6 cd A-1, a maximum lumen efficiency of 27.5 lm W-1, and a maximum external quantum efficiency of up to 30.1%. The CIE coordinates are (0.63, 0.37) at a brightness of 1000 cd m-2.

[0425] Test Example 3

[0426] The stability test of the organic electroluminescent device provided in Device Example 12 was conducted. PdCCC1-12 was selected as the guest material. The device was encapsulated with a glass cover using a UV-curable adhesive in a nitrogen-filled glove box. The device was then removed from the glove box and the luminance of the operating device was measured at a constant current density using an OLED lifetime test system (FS-MP64, Suzhou FSTAR Scientific Instrument Co., Ltd., China). All tests were performed in ambient air. As shown in FIG50 , the doped luminescent OLED prepared in this application using PdCCC1-12 as the guest material and a doping concentration of 1% had an LT95 (LT95 is defined as the time it takes for the luminance to decay by 5%) of 232 hours at an initial luminance of 1000 cd m-2, and an LT90 (LT90 is defined as the time it takes for the luminance to decay by 50%) of 1000 hours at an initial luminance of 1000 cd m-2.

[0427] Test Example 4

[0428] The organic electroluminescent devices provided in device embodiments 8-9 were tested, and PdCCC1-5 was selected as the guest material. The current-brightness-voltage characteristics of the devices were measured by a Keithley source measurement system (Keithley 2400 Sourcemeter, Keithley 2000 Currentmeter) with a calibrated silicon photodiode. All tests were completed in room temperature atmosphere. The test results are shown in Table 3 and Figures 51-52. Figure 51 is an electroluminescence graph of device embodiments 8-9 of the present application based on compound PdCCC1-5, and Figure 52 is an electroluminescence quantum efficiency graph of device embodiments 8-9 of the present application based on compound PdCCC1-5.

[0429] Table 3 Device performance test results [a] Maximum brightness; [b] Current efficiency; [c] Lumen efficiency; [d] External quantum efficiency; [e] CIE coordinates (1000 cd m -2 )

[0430] As shown in Figures 51-52, the present application uses PdCCC1-5 as the guest material and prepares a doped luminescent OLED with a doping concentration of 1%. The maximum luminous brightness can reach 40550 cd m-2, the maximum current efficiency is 65.8 cd A-1, the maximum lumen efficiency is 73.8 lm W-1, the maximum external quantum efficiency is as high as 21.5%, and the CIE coordinates are (0.42, 0.53) at a brightness of 1000 cd m-2.

[0431] Test Example 5

[0432] The organic electroluminescent devices provided in device embodiments 10-11 were tested, and PdCCC1-3 was selected as the guest material. The current-brightness-voltage characteristics of the devices were measured by a Keithley source measurement system (Keithley 2400 Sourcemeter, Keithley 2000 Currentmeter) with a calibrated silicon photodiode. All tests were completed in the atmosphere at room temperature. The test results are shown in Table 4 and Figures 53-54. Figure 53 is an electroluminescence graph of device embodiments 10-11 of the present application based on compound PdCCC1-3, and Figure 54 is an electroluminescence quantum efficiency graph of device embodiments 10-11 of the present application based on compound PdCCC1-3.

[0433] Table 4 Device performance test results [a] Maximum brightness; [b] Current efficiency; [c] Lumen efficiency; [d] External quantum efficiency; [e] CIE coordinates (1000 cd m -2 )

[0434] As shown in Figures 53-54, the present application uses PdCCC1-3 as the guest material and prepares a doped luminescent OLED with a doping concentration of 1%. The maximum luminous brightness can reach 150300 cd m-2, the maximum current efficiency is 79.1 cd A-1, the maximum lumen efficiency is 76.4 lm W-1, the maximum external quantum efficiency is as high as 28.8%, and the CIE coordinates are (0.49, 0.50) at a brightness of 1000 cd m-2.

[0435] In summary, the "V"-shaped molecular structure comprising a tridentate ligand-metal-secondary amine-acceptor described in this application exhibits excellent TADF performance. Through a unique molecular design, the additional acceptor unit introduced onto the metal ligand creates multiple excited states, thereby weakening the charge transfer from the metal to the complex during molecular excitation transitions and enhancing the charge transfer process within and between ligands. The excited-state properties of the metal complex described in this application effectively suppress structural distortion of the excited state, thereby inhibiting non-radiative transitions. This results in an organic electroluminescent device with an external quantum efficiency of up to 35.6% and a long device lifetime.

[0436] Obviously, the above embodiments are merely examples for clarity of explanation and are not intended to limit the implementation methods. Those skilled in the art will readily appreciate that other variations or modifications based on the above descriptions are possible. It is not necessary and impossible to enumerate all implementation methods here. Obvious variations or modifications arising therefrom remain within the scope of protection of this application.

Claims

1. A metal complex, characterized in that Has the following structure: Wherein, M is selected from platinum or palladium; Ring A, Ring B, and Ring C are each independently selected from substituted or unsubstituted C6-C 48 Aromatic ring, substituted or unsubstituted C4-C 48 Heteroaromatic ring; Ring A and Ring B are connected by a single bond or by forming a condensed ring; Ring B and Ring C are connected by a single bond or by forming a condensed ring; Ring A, Ring B and Ring C are coordinated with the metal M center in the form of a negative monovalent tridentate ligand; R 1 -R 7 are the same or different, each independently selected from hydrogen, substituted or unsubstituted C1-C 40 Alkyl, substituted or unsubstituted C6-C 48 Aryl, substituted or unsubstituted C3-C 48 heteroaryl; Ra is a substituted or unsubstituted C6-C 48 Aryl or substituted or unsubstituted C6-C 48 Heteroaryl.

2. The metal complex according to claim 1, characterized in that R 1 , R 3 , R 4 , R 6 , and R 7 is hydrogen, R 2 and R 5 are the same or different, independently selected from substituted or unsubstituted C1-C 40 Alkyl, substituted or unsubstituted C6-C 48 Aryl, substituted or unsubstituted C3-C 48 Heteroaryl.

3. The metal complex according to claim 1 or 2, characterized in that The substituted C1-C 40 Alkyl, substituted C6-C 48 Aryl, substituted C3-C 48 The heteroaryl group is optionally substituted by one or more substituents R b Replace; each R b independently selected from hydrogen, halogen, cyano, C1-C 10 Alkyl, C6-C 30 Aryl.

4. The metal complex according to claim 3, characterized in that The C1-C 40 The alkyl group is selected from methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl; The C1-C 10 The alkyl group is selected from methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, sec-butyl, tert-butyl; The C6-C 48 Aryl is selected from phenyl, naphthyl, anthracenyl; The C6-C 30 The aryl group is selected from phenyl, naphthyl, anthracenyl.

5. The metal complex according to claim 1 or 2, characterized in that The tridentate ligand formed by ring A, ring B and ring C has any of the following structures:

6. The metal complex according to claim 1 or 2, characterized in that Ra has any of the following structures:

7. The metal complex according to claim 1 or 2, characterized in that The metal complex has any of the following structures:

8. An organic electroluminescent device, characterized in that: The organic electroluminescent device comprises a first electrode, a second electrode and a light-emitting layer located between the first electrode and the second electrode, and the light-emitting layer comprises any one or a combination of at least two of the metal complexes according to any one of claims 1 to 7.

9. The organic electroluminescent device according to claim 8, characterized in that: The light-emitting layer comprises the metal complex according to any one of claims 1 to 7 and an organic functional material, wherein, by mass percentage, the metal complex accounts for 0.01% to 100%, and the organic functional material accounts for 0 to 99.9%.

10. Use of the organic electroluminescent device according to claim 8 or 9 in electronic equipment.

Citation Information

Patent Citations

  • Metal complex, luminescent solid, organic EL element, and organic EL display

    CN101018796A

  • Photo-responsive light emitting material and application thereof

    CN110699069A

  • Metal complex and organic electroluminescent device

    CN115700250A

  • Platinum complexes

    EP2873711A1

  • Organometallic compound, organic light-emitting device including the organometallic compound, and diagnosis composition including the organometallic compound

    EP3130595A1