Semiconductor chip mounting method using conductive paste
The semiconductor chip mounting method addresses the issue of surface uniformity and heat resistance by using a conductive paste with silver powder, applying initial low-pressure pressing to flatten the paste and subsequent high-pressure sintering, resulting in improved uniformity and chip bonding with enhanced yield and conductivity.
Patent Information
- Application Number
- PCT/KR2024/095745
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-17
- Filing Date
- 2024-04-16
- Publication Date
- 2024-10-24
AI Technical Summary
Conventional solder is not suitable for bonding semiconductor chips operating at high temperatures due to its limited heat resistance, and the surface uniformity of conductive paste on heat dissipation substrates is compromised by bubbles and fine wrinkles, leading to uneven pressure distribution and potential chip damage during sintering.
A semiconductor chip mounting method using a conductive paste with silver powder and a binder, where the dried paste is pressed under a first condition with lower pressure, temperature, and shorter time to flatten the surface, followed by sintering under a second condition with higher pressure and temperature to form a joint, utilizing a buffering material to prevent damage.
Improves surface uniformity, ensures even force distribution during sintering, prevents chip damage, and enhances mass production yield by creating a joint with high shear strength and excellent electrical conductivity.
Smart Images

Figure KR2024095745_24102024_PF_FP_ABST
Abstract
Description
Semiconductor chip mounting method using conductive paste
[0001] The present invention relates to a semiconductor chip mounting method using conductive paste, and more particularly, to a semiconductor chip mounting method using conductive paste that can improve the surface uniformity of conductive paste that has been applied to a heat dissipation substrate and then dried.
[0002] Semiconductor chips using SiC and other materials have the ability to operate at temperatures exceeding 300°C. When operating semiconductor chips at such high temperatures, conventional solders, with a heat-resistant temperature of approximately 150°C, are unsuitable as bonding materials. Therefore, the use of conductive pastes containing metal particles with excellent heat resistance and electrical conductivity dispersed in a solvent is being considered.
[0003] Conductive paste is applied to the heatsink substrate and then dried before mounting the semiconductor chip. During this drying process, the conductive paste can create bubbles and fine wrinkles on the surface, creating an uneven surface.
[0004] In this way, when a semiconductor chip is placed on the surface of a non-uniform conductive paste and a pressure sintering process is performed, there is a problem in that the semiconductor chip is destroyed because the force applied during the pressure is not transmitted evenly.
[0005] The matters described in the background art above are intended to help understand the background of the invention and may include matters that are not publicly disclosed prior art.
[0006] The present invention was invented to improve the above-mentioned problem, and the problem to be solved by the present invention is to provide a semiconductor chip mounting method using a conductive paste that can improve the surface uniformity of the conductive paste dried on a heat dissipation substrate.
[0007] The method for mounting a semiconductor chip using a conductive paste of the present invention for solving the above-described technical problem is a method for mounting a semiconductor chip on a heat dissipation substrate using a conductive paste, the method including the steps of: applying a conductive paste on a heat dissipation substrate; drying the applied conductive paste; pressing the dried conductive paste under a first pressurizing condition; placing a semiconductor chip on the conductive paste after the pressing; and pressing the conductive paste and the semiconductor chip under a second pressurizing condition to form a joint in which the conductive paste is sintered.
[0008] Here, the pressure of the first pressurizing condition may be lower than the pressure of the second pressurizing condition, the temperature of the first pressurizing condition may be lower than the temperature of the second pressurizing condition, and the time of the first pressurizing condition may be shorter than the time of the second pressurizing condition.
[0009] The pressure of the first pressurizing condition may be in the range of 1 MPa or more and 3 MPa or less, the temperature of the first pressurizing condition may be in the range of 100°C or more and 200°C or less, and the time of the first pressurizing condition may be in the range of 1 second or more and 3 seconds or less.
[0010] The pressure of the second pressurizing condition may be in the range of 10 MPa or more and 15 MPa or less, the temperature of the second pressurizing condition may be in the range of 230°C or more and 300°C or less, and the time of the second pressurizing condition may be in the range of 2 minutes or more and 5 minutes or less.
[0011] The step of pressurizing the dried conductive paste under the first pressurizing condition can pressurize the entire upper surface of the heat sink substrate including the conductive paste.
[0012] The step of pressurizing the dried conductive paste under the first pressurizing condition may include the step of placing a heat dissipating substrate including the dried conductive paste in a lower region of a buffer substrate located at the lower portion of the press, and the step of moving the press downward to pressurize the buffer substrate so that it comes into contact with the entire upper surface of the heat dissipating substrate.
[0013] In the step of placing in the lower region of the buffer substrate, the buffer substrate may be an aluminum substrate or a Teflon film.
[0014] The step of forming a sintered joint of the conductive paste may include the step of placing a heat sink substrate having a semiconductor chip disposed on the conductive paste in a lower region of a buffer substrate located at the lower portion of a press, and the step of moving the press downward to pressurize the buffer substrate so that it comes into contact with the upper surface of the semiconductor chip.
[0015] In the step of applying a conductive paste on a heat sink substrate, the conductive paste includes silver (Ag) powder and a binder, and the silver powder includes a first silver particle group, a second silver particle group, a third silver particle group, and a fourth silver particle group, and the first silver particle group, the second silver particle group, and the third silver particle group are flake-shaped particle groups having different average particle diameters (D50) and different average aspect ratio ranges, and the fourth silver particle group may be a spherical particle group.
[0016] The average particle diameter (D50) of the first silver particle group is in the range of 0.3 ㎛ or more and 0.5 ㎛ or less, the average particle diameter (D50) of the second silver particle group is in the range of 0.7 ㎛ or more and 0.9 ㎛ or less, the average particle diameter (D50) of the third silver particle group is in the range of 1.2 ㎛ or more and 1.8 ㎛ or less, and the average particle diameter (D50) of the fourth silver particle group may be in the range of 0.2 ㎛ or more and 0.4 ㎛ or less.
[0017] The first group of particles may have an average aspect ratio of 2 to 3, the second group of particles may have an average aspect ratio of 3 to 5, and the third group of particles may have an average aspect ratio of 4 to 6.
[0018] The first silver particle group may be included in an amount of 10 wt% to 20 wt% based on the total weight of the silver powder, the second silver particle group may be included in an amount of 25 wt% to 30 wt% based on the total weight of the silver powder, the third silver particle group may be included in an amount of 30 wt% to 35 wt% based on the total weight of the silver powder, and the fourth silver particle group may be included in an amount of 25 wt% to 35 wt% based on the total weight of the silver powder.
[0019] The silver powder may be included in an amount of 75 wt% or more and 90 wt% or less based on the total weight, and the binder may be included in an amount of 0.5 wt% or more and 1.5 wt% or less based on the weight of the silver powder.
[0020] The conductive paste further includes a solvent, at least one of alcohol and acetate, and the solvent may be included in an amount of 5 wt% to 20 wt% relative to the weight of the silver powder.
[0021] The conductive paste further includes an additive, at least one of an organic acid and an organic base, and the additive may be included in a range of 0.2 wt% to 1 wt% relative to the weight of the silver powder.
[0022] According to the semiconductor chip mounting method using the conductive paste of the present invention, by additionally performing a step of pressing the dried conductive paste under a first pressing condition before placing the semiconductor chip on the dried conductive paste, a portion of the outer surface of the conductive paste does not protrude, and fine wrinkles or surface bubbles on the surface are reduced, thereby improving flatness.
[0023] Furthermore, according to the semiconductor chip mounting method using the conductive paste of the present invention, even when the dried conductive paste is pressed under low pressure, low temperature, and short time compared to the pressure sintering process for forming a joint, surface uniformity can be significantly improved, and the force applied to the semiconductor chip laminated on the conductive paste during the pressure sintering process can be evenly distributed. This can prevent the phenomenon of the semiconductor chip breaking and causing defects, and improve the mass production yield.
[0024] In addition, according to the semiconductor chip mounting method using the conductive paste of the present invention, a buffering material that buffers the pressing force of the press applied to the heat dissipation substrate is placed between the press and the heat dissipation substrate, thereby preventing damage to the conductive paste that may occur when the press makes direct contact.
[0025] In addition, according to the semiconductor chip mounting method using the conductive paste of the present invention, a joint having high shear strength can be manufactured even under low pressure conditions, since the silver powder included in the conductive paste is in the form of flakes and includes first to third silver particle groups having different average particle diameters and different average aspect ratio ranges, and a fourth silver particle group having a spherical shape.
[0026] Fig. 1 is a cross-sectional view showing a semiconductor chip assembly according to an embodiment of the present invention.
[0027] Figure 2 is a plan view showing the state of drying conductive paste and positioning a semiconductor chip on the conductive paste.
[0028] Figure 3 is a photograph showing the surface of a conductive paste that has undergone a drying process.
[0029] Figure 4 is a photograph showing the surface of a conductive paste when a pressing process is performed on the dried conductive paste under the first pressing condition.
[0030] FIG. 5 is a flowchart illustrating a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention.
[0031] FIG. 6 is a drawing schematically illustrating a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention.
[0032] FIG. 7 is a drawing schematically illustrating a pressurizing process using a buffer substrate in a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention.
[0033] Hereinafter, a preferred embodiment of the present invention will be described in detail with reference to the attached drawings.
[0034] These examples are provided to more fully illustrate the present invention to those skilled in the art. The following examples may be modified in various ways, and the scope of the present invention is not limited to the examples described below. Rather, these examples are provided to further faithfully and completely convey the spirit of the present invention.
[0035] The terms used herein are used to describe specific embodiments and are not intended to limit the present invention. Furthermore, the singular forms used herein may include the plural forms, unless the context clearly dictates otherwise.
[0036] In the description of the embodiments, when each layer (film), region, pattern or structure is described as being formed "on" or "under" the substrate, each layer (film), region, pad or pattern, "on" and "under" include both being formed "directly" or "indirectly" through another layer. In addition, the reference for above or below each layer is, in principle, based on the drawing.
[0037] The drawings are intended solely to facilitate understanding of the invention and should not be construed as limiting the scope of the invention. Furthermore, relative thicknesses, lengths, and sizes in the drawings may be exaggerated for convenience and clarity of explanation.
[0038] Fig. 1 is a cross-sectional view showing a semiconductor chip assembly according to an embodiment of the present invention.
[0039] Referring to FIG. 1, a semiconductor chip assembly (1) according to an embodiment of the present invention may be configured to include a heat dissipation substrate (100), a conductive paste (200), and a semiconductor chip (300). Here, the conductive paste (200) is applied on the heat dissipation substrate (100), and is interposed between the heat dissipation substrate (100) and the semiconductor chip (300) to bond the heat dissipation substrate (100) and the semiconductor chip (300) by sintering. At this time, the conductive paste (200) may be configured to include silver (Ag) powder and a binder. The conductive paste (200) may use Au powder, but it is preferable to use Ag powder in terms of cost.
[0040] The heat dissipation substrate (100) may be configured to include a ceramic substrate (110) and a metal layer (120) bonded to the upper and lower portions of the ceramic substrate (110), respectively. The ceramic substrate (110) may be configured to include any one of alumina (Al2O3), AlN, SiN, and Si3N4, and the metal layer (120) may be configured in the form of an aluminum foil or a copper foil and may be brazed to both sides of the ceramic substrate (110). This heat dissipation substrate (100) may dissipate heat generated from a semiconductor chip (300) to the outside, thereby preventing the semiconductor chip (300) from overheating. The semiconductor chip (300) may be a power semiconductor chip such as a Si chip, a SiC chip, or a GaN chip.
[0041] In order to bond a semiconductor chip (300) to a heat dissipation substrate (100), sintering is performed while pressing the semiconductor chip (300) toward the heat dissipation substrate (100). However, prior to this pressure sintering process, a process of drying the conductive paste (200) must be performed. Specifically, as shown in FIG. 2, a conductive paste (200) is applied to a bonding target area on the surface of the heat dissipation substrate (100), dried, and a semiconductor chip (300) is placed on the dried conductive paste (200) to perform the pressure sintering process.
[0042] If a semiconductor chip (300) is placed on the conductive paste (200) while the conductive paste (200) is not dried and then a pressure sintering process is performed, it is difficult to form a sintered joint (1) because the pressure is not properly applied in the paste state. Therefore, the drying process can be said to be an essential process for bonding the semiconductor chip (300).
[0043] The drying of the conductive paste (200) is generally carried out at a temperature of 130℃ for about 20 minutes. As shown in FIG. 3, the surface of the dried conductive paste (200) frequently has a portion of the outer periphery protruding, or fine wrinkles or surface bubbles forming. Here, the size of the surface bubbles was found to be 10 mm x 10 mm. If the surface uniformity of the dried conductive paste (200) is low as described above, there is a problem in that the force is not evenly transmitted when the semiconductor chip (300) is pressed in the pressure sintering process, resulting in the breakage of the semiconductor chip (300). Since the thickness of the semiconductor chip (300) is thin, on the order of several tens of micrometers, if the surface of the dried conductive paste (200) is not uniform, the force applied to the semiconductor chip (300) laminated on the conductive paste (200) is not evenly distributed but is concentrated on a part, which may cause the semiconductor chip (300) to break.
[0044] In order to solve these problems, there are methods such as changing the material composition of the conductive paste (200) to flatten the dried conductive paste (200) or setting the printing conditions for mass production more precisely during the drying process, but these methods have the problem of incurring a lot of costs. Therefore, the semiconductor chip mounting method using the conductive paste according to an embodiment of the present invention is characterized by additionally performing a step of pressurizing the dried conductive paste (200) under a first pressurizing condition before positioning the semiconductor chip (300) on the dried conductive paste (200). At this time, the pressure of the first pressurizing condition is in the range of 1 MPa or more and 3 MPa or less. In addition, the temperature under the first pressurizing condition is in the range of 100°C or more and 200°C or less, preferably 130°C or more and 180°C or less, and more preferably around 150°C. The temperature of the press for pressurization may also be in the range of 100°C to 200°C, preferably in the range of 130°C to 180°C, and more preferably around 150°C. The time for which pressurization is performed under the first pressurization condition is in the range of 1 second to 3 seconds.
[0045] Meanwhile, after positioning the semiconductor chip (300), the conductive paste (200) and the semiconductor chip (300) are pressed under a second pressurizing condition in a pressurizing sintering process to form a bond (1) in which the conductive paste (200) is sintered. At this time, the pressure of the second pressurizing condition may be in the range of 10 MPa to 15 MPa. The temperature under the second pressurizing condition is in the range of 230°C to 300°C, and the optimal temperature is 250°C. In addition, the temperature of the press for pressing under the second pressurizing condition is also in the range of 230°C to 300°C, and the optimal temperature is 250°C. The time for which pressing under the second pressurizing condition is performed is in the range of 2 minutes to 5 minutes.
[0046] In this way, the first pressing condition when pressing the conductive paste (200) before positioning the semiconductor chip (300) on the dried conductive paste (200) and the second pressing condition when pressing to form the sintered joint (1) after positioning the semiconductor chip (300) on the pressed conductive paste (200) are different in terms of pressure, temperature, and time. That is, the pressure, temperature, and time of the first pressing condition may have smaller values compared to the pressure, temperature, and time of the second pressing condition. Specifically, the pressure of the first pressing condition is in the range of 1 MPa to 3 MPa, and the pressure of the second pressing condition is in the range of 10 MPa to 15 MPa, so the pressure of the first pressing condition is lower than the pressure of the second pressing condition. In addition, since the temperature of the first pressurization condition is in the range of 100°C to 200°C and the temperature of the second pressurization condition is in the range of 230°C to 300°C, the temperature of the first pressurization condition is lower than the temperature of the second pressurization condition. In addition, since the time of the first pressurization condition is in the range of 1 second to 3 seconds and the time of the second pressurization condition is in the range of 2 minutes to 5 minutes, the time of the first pressurization condition is shorter than the time of the second pressurization condition.
[0047] Figure 4 is a photograph showing the surface of a conductive paste when a pressing process is performed on the dried conductive paste under the first pressing condition.
[0048] As illustrated in FIG. 4, when the pressing process is performed under the first pressing condition, the surface of the dried conductive paste (200) shows that the size of the conductive paste (200) does not change, some of the outer edges do not protrude, and the number of fine wrinkles and surface bubbles is reduced, resulting in a significant improvement in flatness. In this way, it can be seen that the process of pressing the dried conductive paste (200) before positioning the semiconductor chip (300) can significantly improve the surface uniformity of the dried conductive paste (200) even when pressing is performed at a lower pressure, at a lower temperature, and for a shorter time compared to the pressing sintering process for forming the bond (1). As the surface uniformity of the dried conductive paste (200) is improved, the force applied to the semiconductor chip (300) stacked on the conductive paste (200) during the pressing sintering process can be evenly distributed. This can prevent the semiconductor chip (300) from breaking and causing defects, and can improve the mass production yield.
[0049] Meanwhile, although not illustrated in detail, the conductive paste (200) that acts as a conductive adhesive for bonding the semiconductor chip (300) to the heat dissipation substrate (100) is configured to include silver (Ag) powder and a binder, and the silver powder may be in the form of a combination of flake-shaped particles and spherical particles. Preferably, the silver powder includes a first silver particle group, a second silver particle group, a third silver particle group, and a fourth silver particle group, wherein the first to third silver particle groups may be formed of flake-shaped particles, and the fourth silver particle group may be formed of spherical particles. The method for producing the silver powder is not particularly limited, and may be produced by, for example, a reduction method, a pulverization method, an electrolytic method, an atomization method, a heat treatment method, or a combination thereof. The flake-shaped silver particles may be produced by, for example, crushing spherical or granular silver particles using a ball mill or the like.
[0050] The average particle diameter of the first to fourth silver particle groups adopts the value of the median diameter (D50). The average particle diameter (D50) refers to the particle diameter at the point where the volume accumulation of the cumulative curve in the cumulative particle size distribution according to the particle size distribution system becomes 50%. The average particle diameter (D50) of the first silver particle group may be in the range of 0.3 ㎛ to 0.5 ㎛ and may have an average aspect ratio of 2 to 3. The average particle diameter (D50) of the second silver particle group may be in the range of 0.7 ㎛ to 0.9 ㎛ and may have an average aspect ratio of 3 to 5. The average particle diameter (D50) of the third silver particle group may be in the range of 1.2 ㎛ to 1.8 ㎛ and may have an average aspect ratio of 4 to 6. In this way, the first silver particle group, the second silver particle group, and the third silver particle group may be flake-shaped particle groups each having different average particle diameters (D50) and average aspect ratios. In addition, the average particle diameter (D50) of the fourth silver particle group, which is spherical, may be in the range of 0.2 μm to 0.4 μm.
[0051] In this way, the silver powder of the conductive paste is composed of first to fourth silver particle groups and has a relatively wide particle size distribution. Therefore, when the silver powder is precipitated on the substrate surface, relatively small particles are interposed between large particles, so that the gaps between the particles become small and dense, and as a result, voids are small, high shear strength can be achieved, and a conductive path is well formed due to surface contact between the particles, so that excellent electrical conductivity can be exhibited. In addition, the conductive paste is useful as a bonding material for a semiconductor chip (300) because it can be used at high temperatures (e.g., 300°C or higher), which was difficult with conventional bonding materials.
[0052] In the conductive paste, the silver powder preferably includes a first silver particle group in an amount of 10 wt% to 20 wt% based on the total weight of the silver powder, a second silver particle group in an amount of 25 wt% to 30 wt%, a third silver particle group in an amount of 30 wt% to 35 wt%, and a fourth silver particle group in an amount of 25 wt% to 35 wt%. When each of the first to fourth silver particle groups in the silver powder is included within the above range, the effect of forming a dense aggregate with small gaps between the silver particles during sintering of the conductive paste is enhanced.
[0053] The silver powder may be included in an amount ranging from 75 wt% to 90 wt% based on the total weight of the conductive paste. If the silver powder is less than 75 wt% of the total weight, it is difficult to secure electrical conductivity, and if it exceeds 90 wt%, there is a problem of difficulty in adhesion due to the relative insufficient content of solvent and binder.
[0054] The binder ensures excellent bonding strength of the conductive paste and uniform application of the silver powder. The binder controls the spreadability of the paste, thereby controlling the coating thickness. An acrylic polymer may be used as the binder. For example, acrylate, polyethylene glycol, etc. may be used as the binder. The binder may be included in an amount of 0.5 wt% to 1.5 wt% relative to the weight of the silver powder. If the binder is less than 0.5 wt% relative to the weight of the silver powder, uniform distribution of the silver powder is difficult, and if it exceeds 1.5 wt%, conductivity is difficult to ensure.
[0055] The conductive paste may contain a solvent. The solvent controls the viscosity of the binder to provide flowability. The solvent may be an alcohol-based solvent, an acetate-based solvent, etc. For example, alcohol-based solvents such as terpineol, isopropyl alcohol, ethyl hexanediol, 1-hexanol, 1-octanol, etc. may be used, and acetate-based solvents such as butyl carbitol acetate may be used. The solvent is preferably included in an amount of 5 wt% to 20 wt% based on the weight of the silver powder. If the solvent is included in an amount of less than 5 wt% based on the weight of the silver powder, uniform dispersion of the paste may be difficult, and if it exceeds 20 wt%, it may be difficult to secure adhesive strength due to a relative insufficient binder content.
[0056] The conductive paste may include additives. Examples of the additives include organic acids and organic bases. For example, ascorbic acid, formic acid, and tartaric acid may be used as additives. These organic additives readily decompose or volatilize when the conductive paste is applied to the bonding surface and heated, thereby exposing the surfaces of highly active portions of the first to fourth silver particle groups, thereby facilitating a sintering reaction between the first to fourth silver particle groups. In addition, the organic additive may have a reducing ability to reduce an oxide film on the bonding surface. The additive may be included in an amount of 0.2 wt% to 1 wt% relative to the weight of the silver powder. If the additive is included in excess of the above range, organic substances may remain in the bonding layer and decompose over time, thereby generating voids in the bonding layer. Therefore, it is preferable that the additive be included in an amount of 0.2 wt% to 1 wt%, based on 100 wt% of the total amount of the first to fourth silver particle groups.
[0057] Hereinafter, with reference to FIGS. 5 to 7, a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention will be described.
[0058] FIG. 5 is a flowchart illustrating a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention, FIG. 6 is a drawing for schematically explaining a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention, and FIG. 7 is a drawing for schematically explaining a pressurizing process using a buffer material in a semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention.
[0059] A semiconductor chip mounting method using a conductive paste according to an embodiment of the present invention may be configured to include a step (S10) of applying a conductive paste (200) on a heat dissipation substrate (100), a step (S20) of drying the applied conductive paste (200), a step (S30) of pressing the dried conductive paste (200) under a first pressing condition, a step (S40) of placing a semiconductor chip (300) on the conductive paste (200) after pressing, and a step (S50) of pressing the conductive paste (200) and the semiconductor chip (300) under a second pressing condition to form a joint (1) in which the conductive paste (200) is sintered.
[0060] In the step (S10) of applying conductive paste (200) on the heat dissipation substrate (100), the conductive paste (200) can be formed on the surface of the metal layer (120) of the heat dissipation substrate (100) by applying a printing method such as a metal mask method, screen printing, stencil printing, or jetting.
[0061] The step (S20) of drying the applied conductive paste (200) can dry the conductive paste (200) applied on the heat dissipation substrate (100) at a temperature of 130°C for about 20 minutes.
[0062] The step (S30) of pressurizing the dried conductive paste (200) under the first pressurizing condition can pressurize the entire upper surface of the heat dissipation substrate (100) including the conductive paste (200). As illustrated in FIG. 6, the portion that the press contacts is not only the conductive paste (200) but also the entire upper surface of the heat dissipation substrate (100) including the conductive paste, so that the pressing force by the press (400) can be uniformly applied to the entire upper surface of the heat dissipation substrate (100).
[0063] In the step (S30) of pressurizing the dried conductive paste (200) under a first pressurizing condition, the pressure of the first pressurizing condition is in the range of 1 MPa or more and 3 MPa or less. In addition, the temperature under the first pressurizing condition is in the range of 100°C or more and 200°C or less, preferably in the range of 130°C or more and 180°C or less, and more preferably is around 150°C. The temperature of the press for pressurizing may also be in the range of 100°C or more and 200°C or less, preferably in the range of 130°C or more and 180°C or less, and more preferably is around 150°C. The time for which pressurization is performed under the first pressurizing condition is in the range of 1 second or more and 3 seconds or less. The pressure, temperature, and time under the first pressurizing condition have smaller values than the pressure, temperature, and time under the second pressurizing condition in the pressure sintering process for bonding the semiconductor chip (300). The purpose of the pressurizing process according to the first pressurizing condition is to improve the surface uniformity of the dried conductive paste (200), and even if the pressurizing process is performed at a lower pressure, lower temperature, and shorter time than the pressurizing sintering process for forming the joint (1), the surface uniformity of the dried conductive paste (200) is greatly improved, so that the force applied to the semiconductor chip (300) in the subsequent process can be evenly distributed, and thereby the phenomenon of the semiconductor chip (300) being broken and defective can be prevented, and the mass production yield can be improved.
[0064] Meanwhile, as illustrated in FIG. 7, the step (S30) of pressurizing the dried conductive paste (200) under the first pressurizing condition may be configured to include the step (S31) of placing the heat dissipation substrate (100) including the dried conductive paste (200) in the lower region of the buffer substrate (500) located at the lower portion of the press (400), and the step (S32) of moving the press (400) downward to pressurize the buffer substrate (500) so that it comes into contact with the entire upper surface of the heat dissipation substrate (100).
[0065] In the step (S31) of arranging the buffer material (500) in the lower region, the buffer material (500) may be arranged at a lower portion spaced apart from the bottom of the press (400) by a certain distance. At this time, the buffer material (500) may be arranged spaced apart from the upper surface of the heat dissipation substrate (100) by a certain distance. The buffer material (500) may be arranged in a horizontal direction perpendicular to the pressing direction (vertical direction) of the press (400) so that both ends may be supported by support means that are not shown. Accordingly, the buffer material (500) may be arranged in the region between the press (400) and the heat dissipation substrate (100). In addition, the buffer material (500) may be arranged on the upper surface of the heat dissipation substrate (100) before pressing so as to cover the entire upper surface of the heat dissipation substrate (100).
[0066] The buffering substrate (500) may be an aluminum substrate or a Teflon film, and may have the function of buffering the pressing force of the press (400) applied to the heat dissipation substrate (100). That is, the buffering substrate (500) may serve as a buffering medium that prevents the press (400) from making direct contact with the dried conductive paste (200) when the press (400) moves downward and presses the heat dissipation substrate (100) including the dried conductive paste (200). Accordingly, damage to the dried conductive paste (200) that may occur due to direct contact between the press (400) and the heat dissipation substrate (100) may be prevented.
[0067] The step (S32) of pressing the buffer material (500) so that it comes into contact with the entire upper surface of the heat dissipation substrate (100) is such that as the press (400) moves downward, the buffer material (500) moves downward together with the press (400) so that it comes into contact with the entire upper surface of the heat dissipation substrate (100) including the dried conductive paste (200), and at this time, as the conductive paste (200) is pressed by the pressing force of the press (400), the flatness of the surface of the conductive paste (200) can be greatly improved.
[0068] The step (S40) of placing a semiconductor chip (300) on a conductive paste (200) after pressurization is to place the semiconductor chip (300) on a portion of the conductive paste (200) that has been applied to the upper surface of the metal layer (120) of the heat dissipation substrate (100) and then dried and pressed.
[0069] The step (S50) of forming a sintered joint (1) with conductive paste (200) can be performed by pressing the conductive paste (200) and the semiconductor chip (300) according to the pressure, temperature, and time of the second pressing condition to bond the semiconductor chip (300) onto the conductive paste (200) on the heat dissipation substrate (100). Here, the pressure of the second pressing condition may be in the range of 10 MPa to 15 MPa. The temperature in the second pressing condition is in the range of 230°C to 300°C, and the optimal temperature is 250°C. In addition, the temperature of the press for pressing in the second pressing condition is also in the range of 230°C to 300°C, and the optimal temperature is 250°C. The time for performing pressing in the second pressing condition is in the range of 2 minutes to 5 minutes. As this pressure sintering process progresses, the conductive paste (200) including silver (Ag) powder interposed between the semiconductor chip (300) and the heat dissipation substrate (100) is sintered and hardened, thereby forming a bond between the semiconductor chip (300) and the heat dissipation substrate (100).
[0070] Meanwhile, although not illustrated, in the step (S50) of forming a sintered joint (1) with conductive paste (200), the buffer substrate (500) illustrated in FIG. 7 may be placed between the press (400) for pressing and the semiconductor chip (300). That is, the heat dissipation substrate (100) on which the semiconductor chip (300) is placed on the conductive paste (200) may be placed in the lower region of the buffer substrate (500) located below the press (400). In this state, when the press (400) moves downward, the buffer substrate (500) moves downward together with the press (400) and comes into contact with the upper surface of the semiconductor chip (300), and as the semiconductor chip (300) is pressed downward by the pressing force of the press (400), the conductive paste (200) interposed between the semiconductor chip (300) and the heat dissipation substrate (100) may be sintered and hardened. In this way, when a pressure sintering process is performed by placing a buffer material (500) between a press (400) and a semiconductor chip (300), the buffer material (500) acts as a buffer medium, thereby preventing damage to the semiconductor chip (300) that may occur due to direct contact between the press (400) and the semiconductor chip (300).
[0071] As described above, according to the semiconductor chip mounting method using the conductive paste according to the embodiment of the present invention, by additionally performing a step of pressing the dried conductive paste under a first pressing condition before placing the semiconductor chip on the dried conductive paste, a portion of the outer surface of the conductive paste does not protrude, and the number of fine wrinkles or surface bubbles on the surface is reduced, thereby improving flatness, and the force applied to the semiconductor chip stacked on the conductive paste during the pressure sintering process can be evenly distributed. As a result, the phenomenon of the semiconductor chip breaking and causing defects can be prevented, and the mass production yield can be improved.
[0072] The above description is merely an illustrative illustration of the technical idea of the present invention, and those skilled in the art will appreciate that various modifications and variations can be made without departing from the essential characteristics of the present invention. Therefore, the embodiments disclosed in the present invention are intended to illustrate rather than limit the technical idea of the present invention, and the scope of the technical idea of the present invention is not limited by these embodiments. The scope of protection of the present invention should be interpreted by the following claims, and all technical ideas within a scope equivalent thereto should be interpreted as being included in the scope of the rights of the present invention.
Claims
1. A method for mounting a semiconductor chip on a heat dissipation substrate using conductive paste, A step of applying conductive paste on a heat sink substrate; A step of drying the applied conductive paste; A step of pressurizing the dried conductive paste under a first pressurizing condition; A step of placing the semiconductor chip on the conductive paste after pressurization; and A semiconductor chip mounting method using a conductive paste, comprising a step of pressing the conductive paste and the semiconductor chip under a second pressurizing condition to form a sintered joint of the conductive paste.
2. In paragraph 1, The pressure of the above first pressurizing condition is lower than the pressure of the above second pressurizing condition, The temperature of the first pressurizing condition is lower than the temperature of the second pressurizing condition, A semiconductor chip mounting method using a conductive paste in which the time of the first pressurizing condition is shorter than the time of the second pressurizing condition.
3. In paragraph 2, The pressure of the above first pressurizing condition is in the range of 1 MPa or more and 3 MPa or less, The temperature of the above first pressurizing condition is in the range of 100℃ or more and 200℃ or less, A semiconductor chip mounting method using a conductive paste, wherein the time of the first pressurizing condition is in the range of 1 second or more and 3 seconds or less.
4. In paragraph 2, The pressure of the above second pressurizing condition is in the range of 10 MPa or more and 15 MPa or less, The temperature of the above second pressurization condition is in the range of 230℃ or more and 300℃ or less, A semiconductor chip mounting method using a conductive paste, wherein the time of the second pressurizing condition is in the range of 2 minutes or more and 5 minutes or less.
5. In paragraph 1, The step of pressurizing the above dried conductive paste under the first pressurizing condition is: A semiconductor chip mounting method using a conductive paste that pressurizes the entire upper surface of the heat dissipation substrate including the conductive paste.
6. In paragraph 1, The step of pressurizing the above dried conductive paste under the first pressurizing condition is: A step of placing the heat sink substrate including the dried conductive paste in the lower area of the buffer substrate located at the lower part of the press; and A method for mounting a semiconductor chip using a conductive paste, comprising the step of moving the press downward to pressurize the buffer material so that it comes into contact with the entire upper surface of the heat dissipation substrate.
7. In paragraph 6, In the step of placing it in the lower area of the above buffer material, The above buffer material is a semiconductor chip mounting method using conductive paste, which is an aluminum substrate or a Teflon film.
8. In paragraph 1, The step of forming a sintered joint by the conductive paste is as follows: A step of placing the heat dissipation substrate on which the semiconductor chip is placed on the conductive paste in the lower region of the buffer substrate located at the lower part of the press; and A semiconductor chip mounting method using a conductive paste, comprising a step of moving the press downward to pressurize the buffer material so that it comes into contact with the upper surface of the semiconductor chip.
9. In paragraph 1, In the step of applying conductive paste on the above heat sink substrate, The above conductive paste contains silver (Ag) powder and a binder, The above silver powder includes a first silver particle group, a second silver particle group, a third silver particle group, and a fourth silver particle group, The first silver particle group, the second silver particle group, and the third silver particle group are flake-shaped particle groups having different average particle diameters (D50) and different average aspect ratio ranges. The above fourth particle group is a method for mounting a semiconductor chip using a conductive paste that is a spherical particle group.
10. In paragraph 9, The average particle diameter (D50) of the above first particle group is in the range of 0.3㎛ or more and 0.5㎛ or less, The average particle diameter (D50) of the above second silver particle group is in the range of 0.7㎛ or more and 0.9㎛ or less, The average particle diameter (D50) of the above third particle group is in the range of 1.2㎛ to 1.8㎛, A semiconductor chip mounting method using a conductive paste in which the average particle diameter (D50) of the fourth silver particle group is in the range of 0.2 ㎛ to 0.4 ㎛.
11. In paragraph 9, The above first particle group has an average aspect ratio of 2 to 3, The above second particle group has an average aspect ratio of 3 to 5, The third particle group is a semiconductor chip mounting method using a conductive paste having an average aspect ratio of 4 to 6.
12. In paragraph 9, The above first silver particle group is included in a range of 10 wt% to 20 wt% based on the total weight of the silver powder, The above second silver particle group is included in a range of 25 wt% to 30 wt% based on the total weight of the silver powder, The above third silver particle group is included in a range of 30 wt% to 35 wt% based on the total weight of the silver powder, A semiconductor chip mounting method using a conductive paste in which the fourth silver particle group is included in a range of 25 wt% to 35 wt% based on the total weight of the silver powder.
13. In paragraph 9, The above silver powder is included in a range of 75% by weight or more and 90% by weight or less based on the total weight, A method for mounting a semiconductor chip using a conductive paste in which the binder is included in an amount of 0.5 wt% to 1.5 wt% relative to the weight of the silver powder.
14. In paragraph 9, The conductive paste further comprises a solvent of at least one of alcohol and acetate, A method for mounting a semiconductor chip using a conductive paste in which the solvent is included in an amount of 5 wt% to 20 wt% relative to the weight of the silver powder.
15. In paragraph 9, The conductive paste further comprises an additive of at least one of an organic acid and an organic base, A method for mounting a semiconductor chip using a conductive paste in which the additive is included in an amount of 0.2 wt% to 1 wt% relative to the weight of the silver powder.
Citation Information
Patent Citations
Method for flattening bump and method for manufacturing mounting substrate
JP2002289732A
Printed wiring board, manufacturing method thereof, and semiconductor device
JP2002305376A
Semiconductor module mounting method
JP2013012693A
Electronic component, connection body, method of manufacturing connection body, method of manufacturing electronic component, and buffer material
JP2016058718A
Low-firing silver conductor
KR1020140099215A