Para-aramid fiber continuous production device and control method
By improving the continuous production device and control method of para-aramid fiber, the problem of discontinuous polymerization and spinning processes is solved, the dissolution and washing efficiency is improved, the continuous production of para-aramid fiber is realized, and the production cost is reduced. Material accumulation impact.
Patent Information
- Application Number
- PCT/CN2024/094833
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-30
- Filing Date
- 2024-05-23
- Publication Date
- 2024-12-05
AI Technical Summary
The polymerization and spinning processes in the existing para-aramid fiber production process are discontinuous, resulting in unstable polymer materials, low washing efficiency, serious pollution, and material accumulation affects spinning quality and production costs.
A continuous production device for para-aramid is designed, including an improved para-phenylenediamine dissolution device and a washing device, adopting two-stage continuous dissolution and organic liquid washing, combining the controller to monitor and adjust the feed volume in real time to achieve polymerization and Linkage control of spinning.
The dissolution efficiency and washing efficiency of para-aramid resin are improved, the continuous production of polymerization and spinning is realized, material accumulation is reduced, and product quality and production efficiency are improved.
Smart Images

Figure CN2024094833_05122024_PF_FP_ABST
Abstract
Description
A continuous production device and control method for para-aramid fiber Technical Field
[0001] The present invention relates to a para-aramid fiber production process, in particular to a para-aramid fiber continuous production device and a control method. Background Art
[0002] Para-aramid fiber, also known as poly(p-phenylene terephthalamide) fiber (hereinafter referred to as PPTA fiber), has excellent physical and chemical properties such as high strength, high modulus, high temperature resistance, acid and alkali resistance, and light weight. It is widely used in military fields such as aerospace and civilian fields. It is also widely used as a reinforcing material in composite materials.
[0003] The production process of para-aramid fiber includes polymerization, spinning, and recycling, with polymerization and spinning being the key processes for the synthesis of para-aramid fiber. The main principle of the polymerization process is to use terephthaloyl chloride (TPC) and para-phenylenediamine (PPD) as raw materials under low temperature conditions in a polar solvent system of N-methylpyrrolidone (NMP) to carry out a polymerization reaction to produce PPTA resin. The main principle of the spinning process is to dissolve the PPTA resin in concentrated sulfuric acid to form a PPTA / concentrated sulfuric acid liquid crystal slurry at a high temperature (80-90°C). Under the action of relatively high shear force, the liquid crystal slurry is sprayed out at high speed using a dry jet method. After water washing, drying, and subsequent heat treatment, para-aramid fiber is obtained.
[0004] At present, the production process of para-aramid generally adopts the intermittent polymerization and intermittent spinning method, that is, the polymerization and spinning are not continuous. The polymerized product needs to be temporarily stored in a storage tank and then spun and the polymerized product is taken out of the storage tank for spinning.
[0005] However, in the process of implementing the existing technical solutions, the inventors of this application discovered that the above technology has at least the following technical problems:
[0006] 1. Continuity of polymerization.
[0007] The polymerization reaction involves the low-temperature polycondensation of the monomers terephthaloyl chloride (TPC) and p-phenylenediamine (PPD) in a complex system of N-methylpyrrolidone (NMP) and calcium chloride as a cosolvent. This process takes place in a polymerization reactor and is a continuous process. However, the mixing of PPD with the solvent system (NMP and calcium chloride) is a batch process, not a continuous one. Generally, a mixture of PPD and the solvent system is prepared in batches before polymerization and then reconstituted after use. This has the disadvantage of making the polymer unstable. Because PPD is a highly reactive monomer, the storage time after mixing with the solvent system can affect the quality of the PPD entering the polymerization system, and thus the quality of the resulting PPTA resin.
[0008] Next is polymer cleaning. After PPTA polymerization is complete, it needs to be thoroughly separated from other components, such as the solvent. Countercurrent washing is a commonly used method. Its advantages are simplicity and ease of operation. However, its disadvantages include low washing efficiency, severe pollution, and low efficiency in recovering NMP from the washing liquid. This low washing efficiency directly impacts the material supply for subsequent spinning production.
[0009] 2. Continuity of polymerization and spinning.
[0010] In addition to the problems of the polymerization process itself mentioned above, the characteristics of the spinning process also lead to the inability to produce polymerization and spinning continuously for the following reasons:
[0011] To improve production efficiency in para-aramid spinning, multiple spinning stations (typically 10-30) are typically installed on the spinning manifold for simultaneous spinning. However, when multiple spinning stations operate simultaneously, proper spinning cannot be guaranteed. Frequently, a malfunctioning spinning station will shut down, requiring cleaning and maintenance before restarting. This results in an uncertain material level at the spinning head, necessitating real-time adjustments to the polymer material level. Failure to do so can disrupt the entire polymer spinning system.
[0012] The current production method uses isolated production, meaning that polymerization is carried out solely without regard to spinning demand. The polymerized material is first stored in an intermediate silo. During spinning, the material is drawn from the intermediate silo for spinning, without any connection to the polymerization process. This method offers the advantage of simplicity. However, its disadvantage is that, to ensure both spinning production and a buffer for polymerization output, the intermediate silo must be relatively large, leading to material accumulation. This accumulation of material absorbs moisture and degrades, affecting spinning quality. Furthermore, material accumulation can lead to material mixing. Generally, the quality of the polymerized material varies, and entering the intermediate silo can result in high-quality and low-quality materials being mixed. Finally, material accumulation consumes capital, increasing production costs. Summary of the Invention
[0013] The object of the present invention is to provide a continuous production device and control method for para-aramid fiber to solve the problems raised in the above background technology.
[0014] The invention provides a p-aramid continuous production device, comprising a polymerization component for polymerizing p-phenylenediamine and terephthaloyl chloride into a p-aramid resin.
[0015] The spinning assembly is used to dissolve the para-aramid resin and spray it into para-aramid fibers.
[0016] The buffer tank is used to connect the polymerization component and the spinning component and to buffer the polymer material.
[0017] The controller is used to control the operating speed of each component. According to the control method set in the present invention, the controller monitors the data of the sensors in the polymerization component and the spinning component in real time, and controls the feed amount and the operation of the equipment.
[0018] The polymerization assembly includes: a p-phenylenediamine dissolving device, a terephthaloyl chloride feeding device, a polymerization reactor and a washing device. The outlets of the p-phenylenediamine dissolving device and the terephthaloyl chloride feeding device are connected to the inlet of the polymerization reactor, the outlet of the polymerization reactor is connected to the inlet of the washing device, and the outlet of the washing device is connected to the buffer tank.
[0019] The p-phenylenediamine dissolving device includes: a first mixer and a second mixer, the outlet of the first mixer is connected to the inlet of the second mixer, the p-phenylenediamine enters the first mixer after being metered by a first feeder, the solvent system is controlled and metered by a first regulating valve and a first flowmeter, and then split by a diversion device, a part of which enters the first mixer for mixing, and the remaining part enters the second mixer. The material entering the first mixer in the diversion device accounts for 70%-80% of the input.
[0020] The p-phenylenediamine dissolving device provided by the present invention adopts a two-stage continuous dissolution. The first mixer is a room temperature mixer to improve the dissolution efficiency, and the second mixer is a low-temperature mixer to quickly reduce the mixed liquid to the temperature required for the polymerization reaction while minimizing the precipitation of the solute caused by the low temperature.
[0021] The terephthaloyl chloride feeding device is provided with a second flow meter, and the feeding amount of terephthaloyl chloride is controlled by a third regulating valve.
[0022] The washing device includes a crusher, the inlet of which is connected to the outlet of the polymerization reactor and the chloroform pipeline respectively. The polymer material and chloroform are mixed and crushed in the crusher and then pass through a first filter, a first drying device, a water washer, a second filter and a second drying device in sequence. The second drying device is connected to the inlet of the buffer tank.
[0023] The spinning assembly includes a second blanking machine, the feed port of the second blanking machine is connected to the outlet of the buffer tank, and the outlet of the second blanking machine is connected to the dissolver. The spinning assembly also includes a third flow meter and a second regulating valve. The concentrated sulfuric acid enters the dissolver after being regulated by the second regulating valve and measured by the third flow meter. The discharge end of the dissolver is connected to the third filter, pump, pressure sensor in sequence, and finally enters the spinning box.
[0024] A method for controlling continuous production of para-aramid fiber, comprising the following steps:
[0025] Step S1, prefabricating control system parameters, determining the number K of spinning positions installed on the spinning manifold, the unit spinning flow array Q[q1,q2,q3,q4,q5], the polymerization time constant T0, and the buffer tank capacity;
[0026] Step S2: The system pre-judges whether nozzle blockage occurs in the current spinning production, calculates the number of actual spinning positions L, and sets the feeding parameters for spinning and polymerization to L*Q[q1,q2,q3,q4,q5];
[0027] Step S3, flow adjustment system, the system adjusts the feed amount of polymerization and spinning according to the actual number of spinning positions L calculated in step S2.
[0028] In step S1, the unit spinning flow array Q[q1,q2,q3,q4,q5] is the material flow required for normal spinning at one spinning position, corresponding to the feed amount in polymerization production and spinning production, where:
[0029] q1, feed flow rate of phthaloyl chloride in polymerization production;
[0030] q2, feed flow rate of p-phenylenediamine in polymerization production;
[0031] q3, feed flow rate of the solvent system in polymerization production;
[0032] q4, feed flow rate of para-aramid resin in spinning production;
[0033] q5, feed flow rate of para-aramid resin in spinning production.
[0034] In the present invention, the capacity V of the buffer tank should satisfy: V>K*q4*T 0 If the capacity of the buffer tank is set too large, it will cause material accumulation and affect the quality of the raw materials. The optimal capacity range of the buffer tank in the present invention is: 1.5*K*q4*T0≤V≤2*K*q4*T 0 At the same time, the present invention provides a warning value for the capacity of the buffer tank, the material lower limit alarm V min =0.5*K*q4*T 0 , and material upper limit alarm Vmax =K*q4*T 0 .
[0035] The polymerization time constant T0 in step S1 is the time required from the start of the material being put into the polymerization assembly to the end of the polymerization and the time when the material leaves the polymerization assembly.
[0036] Step S2 includes:
[0037] Step S201, obtaining the speed value of the pump;
[0038] Step S202, determining the current speed gear N according to the pump speed value obtained in step S201;
[0039] Step S203, the number of spinning positions L in step S2 is subtracted from the pump speed gear N to obtain the number of currently faulty spinning positions M;
[0040] Step S204, assigning the pump speed gear N to the number of spinning positions L;
[0041] The present invention provides a method for determining the pump speed gear N. In order to ensure the stability of spinning at the rear end of the spinning box, the pump and pressure sensor at the front end of the spinning box adopt PID control to ensure the stability of the input pressure. When the spinning position on the spinning box is blocked, the pump speed will decrease under the condition of unchanged pressure. By recording the number of blockages at the spinning position and the corresponding pump speed value, the pump speed gear can be determined.
[0042] Step S3 includes:
[0043] Step S301, obtaining the current number M of faulty spinning positions obtained in step S203;
[0044] Step S302, determining whether the current number M of faulty spinning positions is equal to 0, if M=0, executing step S303, otherwise executing step S304;
[0045] Step S303: If the number of spinning positions does not change, the material is unloaded according to the unloading parameters set in step S2;
[0046] Step S304: if the number of spinning positions changes, execute step S305;
[0047] Step S305, initialize timer T, set T=T0, and start the timer;
[0048] Step S306 , the system adjusts the polymerization feed amount to (LM) units and the spinning feed amount to L units;
[0049] Step S307, determine whether the timer T has expired, if so, execute step S308, otherwise, continue to execute step S306;
[0050] Step S308, the system adjusts the polymerization feed amount to L units, and the spinning feed amount remains at L units;
[0051] Compared with the prior art, the present invention has the following beneficial effects:
[0052] 1. The present invention improves the p-phenylenediamine dissolving device in the polymerization production of p-aramid resin. The improved device can realize continuous dissolution of p-phenylenediamine, thereby improving dissolution efficiency and dissolution quality.
[0053] 2. The present invention improves the washing device in the polymerization production of para-aramid resin, abandons the traditional water washing process, and adopts a combination of organic liquid washing and water washing to improve the washing efficiency;
[0054] 3. The continuous control method disclosed in the technology of the present invention takes the spinning position as the control target and control unit, divides the control flow of polymerization and spinning according to the spinning position, and combines system prejudgment to achieve control of polymerization output, thereby realizing linkage control of polymerization and spinning. BRIEF DESCRIPTION OF THE DRAWINGS
[0055] FIG1 is a schematic structural diagram of a continuous production device for para-aramid fibers according to the present invention;
[0056] FIG2 is a general flow chart of the control method of the present invention;
[0057] FIG3 is a flow chart of the prediction system of the present invention;
[0058] FIG4 is a flow chart of the flow regulation system of the present invention;
[0059] FIG5 is a block diagram of a control system according to the present invention;
[0060] The meaning of each number in the figure is:
[0061] 1. Polymerization component; 2. Buffer tank; 3. Spinning component; 4. Controller;
[0062] 101, first feeder; 102, first flowmeter; 103, flow splitter; 104, first mixer; 105, second mixer; 105a, refrigerant inlet; 105b, refrigerant outlet; 106, second flowmeter; 107, polymerization reactor; 180, crusher; 109, first filter; 110, first drying device; 111, washing machine; 112, second filter; 113, second drying device; 114, first regulating valve; 115, third regulating valve.
[0063] 301. Second feeder; 302. Third flowmeter; 303. Dissolver; 304. Third filter; 305. Pump; 306. Pressure sensor; 307. Spinning manifold; 308. Second regulating valve. DETAILED DESCRIPTION
[0064] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the embodiments described are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.
[0065] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like to indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention. Example 1
[0066] This embodiment provides a para-aramid continuous production device, comprising: a polymerization component 1 for polymerizing para-phenylenediamine and terephthaloyl chloride into para-aramid resin.
[0067] The spinning assembly 3 is used to dissolve the para-aramid resin and spray it into para-aramid fibers.
[0068] The buffer tank 2 is used to connect the polymerization component 1 and the spinning component 3 and to buffer the polymer material.
[0069] The controller 4 is used to control the operating speed of each component. According to the control method set in the present invention, the controller 4 monitors the data of the sensors in the polymerization component 1 and the spinning component 3 in real time, and controls the feed amount and the operation of the equipment.
[0070] In this embodiment, a buffer tank 2 is introduced to connect the polymerization assembly 1 and the spinning assembly 3 into a whole, thereby ensuring the continuity of production at the equipment level. Example 2
[0071] In addition to the contents of the previous embodiment, this embodiment further provides a polymerization assembly 1 comprising: a p-phenylenediamine dissolving device, a terephthaloyl chloride feeding device, a polymerization reactor 107, and a washing device. The outlets of the p-phenylenediamine dissolving device and the terephthaloyl chloride feeding device are connected to the inlet of the polymerization reactor 107, the outlet of the polymerization reactor 107 is connected to the inlet of the washing device, and the outlet of the washing device is connected to the buffer tank 2. The polymerized material is directly transported to the buffer tank 2. Example 3
[0072] In addition to the contents of the previous embodiment, this embodiment further provides a p-phenylenediamine dissolving device, which includes: a first mixer 104 and a second mixer 105, wherein the outlet of the first mixer 104 is connected to the inlet of the second mixer 105, and the p-phenylenediamine enters the first mixer 104 after being metered by the first feeder 101, and the solvent system is metered by the first regulating valve 114 and the first flowmeter 102 and then diverted by the diverter 103, with a portion entering the first mixer 104 for mixing, and the remaining portion entering the second mixer 105, and the material entering the first mixer 104 from the diverter 103 accounts for 70%-80% of the input.
[0073] In the p-phenylenediamine dissolving device provided by the present invention, a two-stage continuous dissolution is adopted. The first mixer 104 is a room temperature mixer to improve the dissolution efficiency, and the second mixer 105 is a low-temperature mixer to quickly reduce the mixed liquid to the temperature required for the polymerization reaction while minimizing the precipitation of the solute caused by the low temperature. Example 4
[0074] In addition to the contents of the previous embodiment, this embodiment further provides a terephthaloyl chloride feeding device, which is provided with a second flow meter 106 , and the feeding amount of terephthaloyl chloride is controlled by a third regulating valve 115 .
[0075] In this embodiment, the feed rate of terephthaloyl chloride is controlled by PID. The controller 4 controls the opening of the third regulating valve 115 by collecting data from the second flow meter 106 to ensure that terephthaloyl chloride enters the polymerization reactor 107 according to the flow rate set by the system. Example 5
[0076] In addition to the contents of the previous embodiment, this embodiment further provides a washing device, which includes a crusher 108. The inlet of the crusher 108 is connected to the outlet of the polymerization reactor 107 and the chloroform pipeline respectively. The polymer material and chloroform are mixed and crushed in the crusher 108 and then pass through the first filter 109, the first drying device 110, the water washer 111, the second filter 112 and the second drying device 113 in sequence. The second drying device 113 is connected to the inlet of the buffer tank 2.
[0077] This embodiment provides a PPTA resin washing device. To ensure production continuity and avoid the time-consuming impact of traditional washing methods that affect subsequent feeding, the present invention adopts a two-step washing method. The first step is to wash with chloroform. The NMP in the PPTA polymer will quickly dissolve in the chloroform to form a mixture of NMP and chloroform. The washed material is then dried at low temperature, taking advantage of the volatility of chloroform. The NMP-chloroform mixture and the chloroform volatilized during the drying process are then fed into a recovery process for separation of NMP and chloroform. The second step is to wash with deionized water to dissolve the calcium chloride in the polymer into the water, followed by filtration and drying. Example 6
[0078] In addition to the contents of the previous embodiment, this embodiment further provides a spinning assembly 3, which includes a second feeder 301, the feed port of the second feeder 301 is connected to the outlet of the buffer tank 2, and the outlet of the second feeder 301 is connected to the dissolver 303. The spinning assembly 3 also includes a third flowmeter 302 and a second regulating valve 308. The concentrated sulfuric acid enters the dissolver 303 after being regulated by the second regulating valve 308 and measured by the third flowmeter 302. The discharge end of the dissolver 303 is connected in sequence to the third filter 304, the pump 305, and the pressure sensor 306, and finally enters the spinning box 307.
[0079] In this embodiment, a spinning assembly is provided, in which, in order to ensure the stability of the flow entering the spinning manifold 307, a pump 305 and a pressure sensor 306 are installed on the pipeline between the third filter 304 and the spinning manifold 307. PID control is adopted, and the controller 4 controls the speed of the pump 305 by collecting the pressure value of the pressure sensor 306. In this example, the pump 305 preferably uses a metering pump or a gear pump, which has a low speed and high flow accuracy. Example 7
[0080] This embodiment provides a method for controlling continuous production of para-aramid fiber, which uses the aforementioned continuous production device for para-aramid fiber, and includes the following steps:
[0081] Step S1, prefabricate control system parameters, determine the number K of spinning positions installed on the spinning manifold 307 and the unit spinning flow array Q[q1,q2,q3,q4,q5], polymerization time constant T0, and buffer tank capacity;
[0082] Step S2: The system pre-judges whether nozzle blockage occurs in the current spinning production, calculates the number of actual spinning positions L, and sets the feeding parameters for spinning and polymerization to L*Q[q1,q2,q3,q4,q5];
[0083] Step S3, flow adjustment system, the system adjusts the feed amount of polymerization and spinning according to the actual number of spinning positions L calculated in step S2.
[0084] In step S1, the unit spinning flow array Q[q1,q2,q3,q4,q5] is the material flow required for normal spinning at one spinning position, corresponding to the feed amount in polymerization production and spinning production, where:
[0085] q1, feed flow rate of phthaloyl chloride in polymerization production;
[0086] q2, feed flow rate of p-phenylenediamine in polymerization production;
[0087] q3, feed flow rate of the solvent system in polymerization production;
[0088] q4, feed flow rate of para-aramid resin in spinning production;
[0089] q5, feed flow rate of para-aramid resin in spinning production.
[0090] In the present invention, the capacity V of the buffer tank should satisfy: V>K*q4*T 0 If the capacity of the buffer tank is set too large, it will cause material accumulation and affect the quality of the raw materials. The optimal capacity range of the buffer tank in the present invention is: 1.5*K*q4*T0≤V≤2*K*q4*T 0 At the same time, the present invention provides a warning value for the capacity of the buffer tank, the material lower limit alarm V min =0.5*K*q4*T 0 , and material upper limit alarm V max =K*q4*T 0 .
[0091] The polymerization time constant T0 in step S1 is the time required from the start of the material being put into the polymerization component 1 to the end of the polymerization and the time when the material leaves the polymerization component 1. Example 8
[0092] In addition to the content of the previous embodiment, this embodiment further provides a system prejudgment method, wherein step S2 includes:
[0093] Step S201, obtaining the rotation speed value of the pump 305;
[0094] Step S202, determining the current speed gear N according to the speed value of the pump 305 obtained in step S201;
[0095] Step S203, the number of spinning positions L in step S2 is subtracted from the speed gear N of the pump 305 to obtain the number M of currently faulty spinning positions;
[0096] Step S204, assigning the speed gear N of the pump 305 to the number L of spinning positions;
[0097] In the present invention, a method for determining the speed gear N of the pump 305 is provided. In order to ensure the stability of spinning at the rear end of the spinning manifold, the pump 305 and the pressure sensor 306 at the front end of the spinning manifold adopt PID control to ensure the stability of the input pressure. When the spinning position on the spinning manifold is blocked, the speed of the pump 305 will decrease while the pressure remains unchanged. By recording the number of blockages at the spinning position and the corresponding pump 305 speed value, the speed gear of the pump 305 can be determined. Example 9
[0098] In addition to the content of the previous embodiment, this embodiment further provides a flow adjustment method, wherein step S3 includes:
[0099] Step S301, obtaining the current number M of faulty spinning positions obtained in step S203;
[0100] Step S302, determining whether the current number M of faulty spinning positions is equal to 0, if M=0, executing step S303, otherwise executing step S304;
[0101] Step S303: If the number of spinning positions does not change, the material is unloaded according to the unloading parameters set in step S2;
[0102] Step S304: if the number of spinning positions changes, execute step S305;
[0103] Step S305, initialize timer T, set T=T0, and start the timer;
[0104] Step S306 , the system adjusts the polymerization feed amount to (LM) units and the spinning feed amount to L units;
[0105] Step S307, determine whether the timer T has expired, if so, execute step S308, otherwise, continue to execute step S306;
[0106] Step S308, the system adjusts the polymerization feed amount to L units, and the spinning feed amount remains at L units;
[0107] In the present invention, when a spinning station is clogged, the system determines the number of spinning stations based on the pre-judgment result in step S2 and promptly adjusts the polymerization and spinning feed rates based on the number of spinning stations. However, due to the time delay of polymerization production, some material will accumulate in the buffer tank, and the capacity of the buffer tank needs to be designed to be as small as possible. In order to reduce the capacity of the buffer tank, precise control is required. This solution adopts an overshoot control scheme. When the number of spinning stations changes, the polymerization is over-adjusted within a polymerization time constant T0 period. After the T0 period ends, the feed rate is restored to the actual number of spinning stations.
[0108] It is worth noting that in this embodiment, the current number M of faulty spinning positions can be a positive value or a negative value, corresponding to two different situations, namely, when M>0, a fault occurs in the spinning position, and the number of faulty spinning positions is |M|; when M<0, it means that a number of |M| spinning positions have been repaired and restored to normal use.
[0109] Specifically, regardless of whether a failure occurs at the spinning position or the spinning position returns to normal, the technical solution provided in this embodiment can accurately determine and automatically adjust the flow rate to ensure continuous production of the entire device.
[0110] The above shows and describes the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are merely preferred examples of the present invention and are not intended to limit the present invention. Various changes and improvements may be made to the present invention without departing from the spirit and scope of the present invention, and such changes and improvements fall within the scope of the present invention. The scope of protection claimed in the present invention is defined by the appended claims and their equivalents.
Claims
1. A device for continuous production of para-aramid fiber, comprising: A polymerization component (1) for polymerizing p-phenylenediamine and terephthaloyl chloride into a p-aramid resin; A spinning assembly (3) for dissolving the para-aramid resin and spraying it into para-aramid fibers; It is characterized by further comprising: The polymerization component (1) comprises a p-phenylenediamine dissolving device, a polymerization reactor (107) and a washing device; a buffer tank (2) is used to connect the polymerization component (1) and the spinning component (3) and to buffer the polymer material to a certain extent; A controller (4) for controlling the operating speed of each component; The p-phenylenediamine dissolving device comprises: a first mixer (104) and a second mixer (105), wherein the outlet of the first mixer (104) is connected to the inlet of the second mixer (105), and the p-phenylenediamine enters the first mixer (104) after being metered by a first feeder (101), and the solvent system is metered by a first regulating valve (114) and a first flow meter (102) and then divided by a flow dividing device (103), a part of which enters the first mixer (104) for mixing, and the remaining part enters the second mixer (105), and the material in the flow dividing device (103) entering the first mixer (104) accounts for 70%-80% of the input; The washing device comprises a crusher (108), the inlet of the crusher (108) is respectively connected to the outlet of the polymerization reactor (107) and the chloroform pipeline; the polymer material and chloroform are mixed and crushed in the crusher (108) and then sequentially pass through a first filter (109), a first drying device (110), a washing machine (111), a second filter (112) and a second drying device (113); the second drying device (113) is connected to the inlet of the buffer tank (2).
2. The continuous production device of para-aramid fiber according to claim 1, characterized in that: The polymerization assembly (1) further comprises: a terephthaloyl chloride feeding device, wherein the outlets of the p-phenylenediamine dissolving device and the terephthaloyl chloride feeding device are connected to the inlet of the polymerization reactor (107), the outlet of the polymerization reactor (107) is connected to the inlet of the washing device, and the outlet of the washing device is connected to the buffer tank (2).
3. The continuous production device of para-aramid fiber according to claim 2, characterized in that: The terephthaloyl chloride feeding device is provided with a second flow meter (106).
4. The continuous production device of para-aramid fiber according to claim 1, characterized in that: The spinning assembly (3) comprises a second feeder (301), the feed port of the second feeder (301) is connected to the outlet of the buffer tank (2), the outlet of the second feeder (301) is connected to the dissolver (303), the spinning assembly (3) further comprises a third flow meter (302) and a second regulating valve (308), the concentrated sulfuric acid enters the dissolver (303) after being regulated by the second regulating valve (308) and measured by the third flow meter (302), the discharge end of the dissolver (303) is connected in sequence to a third filter (304), a pump (305), a pressure sensor (306), and finally enters a spinning box (307).
5. A method for controlling the continuous production of para-aramid fiber, using the para-aramid continuous production device according to claim 4, the method comprising the following steps: Step S1, prefabricate control system parameters, determine the number of spinning positions K installed on the spinning manifold (307) and the unit spinning flow array Q[q1, q2, q3, q4, q5], the polymerization time constant T0, and the buffer tank capacity; Step S2, the system pre-judges whether the nozzle is blocked in the current spinning production, calculates the number of current actual spinning positions L, and sets the feeding parameters of spinning and polymerization to L*Q[q1,q2,q3,q4,q5]; Step S3, flow adjustment system, the system adjusts the feed amount of polymerization and spinning according to the actual number of spinning positions L calculated in step S2; The unit spinning flow array Q[q1, q2, q3, q4, q5] in step S1 is the material flow required for normal spinning at one spinning position, corresponding to the feed amount in polymerization production and spinning production, wherein: q1, feed flow rate of phthaloyl chloride in polymerization production; q2, feed flow rate of p-phenylenediamine in polymerization production; q3, feed flow rate of solvent system in polymerization production; q4, feed flow rate of para-aramid resin in spinning production; q5, feed flow rate of para-aramid resin in spinning production; The polymerization time constant T0 in step S1 is the time required from the time when the material is put into the polymerization component (1) to the time when the polymerization is completed and the material leaves the polymerization component (1).
6. The method for controlling continuous production of para-aramid fiber according to claim 5, characterized in that: The step S2 comprises: Step S201, obtaining the rotation speed value of the pump (305); Step S202, determining the current speed gear N according to the speed value of the pump (305) obtained in step S201; Step S203, the number of spinning positions L in step S2 minus the speed gear N of the pump (305) to obtain the number of currently faulty spinning positions M; Step S204, assigning the speed gear N of the pump (305) to the number L of spinning positions.
7. The method for controlling continuous production of para-aramid fiber according to claim 5, characterized in that: The step S3 comprises: Step S301, obtaining the current number M of faulty spinning positions obtained in step S203; Step S302, determining whether the current number M of faulty spinning positions is equal to 0, if M=0, executing step S303, otherwise executing step S304; Step S303: the number of spinning positions does not change, and the material is unloaded according to the unloading parameter settings set in step S2; Step S304, the number of spinning positions changes, and step S305 is executed; Step S305, initialize timer T, set T=T0, and start the timer; Step S306, the system adjusts the polymerization feed amount to (LM) units and the spinning feed amount to L units; Step S307, determine whether the timer T has ended, if the timer T has ended, execute step S308, otherwise continue to execute step S306; Step S308, the system adjusts the polymerization feed amount to L units, and the spinning feed amount remains at L units.
Citation Information
Patent Citations
Spandex microfilament and spinning method thereof
CN101469455A
Poly-p-phenylene terephthamide (PPTA) polymer washing and solvent recovery method
CN102634011A
High-concentration continuous and stable polymerization method and system for poly-p-phenylene terephthamide
CN108623803A
Melt direct spinning functional masterbatch single part uniform quantitative injection method
CN109056082A
PPTA spinning flow control system and method
CN110241465A