The wiring board laminate with embedded ceramic members and a metal film-free region addresses the lamination and cost challenges of ceramic circuit boards, achieving efficient heat dissipation and reduced cracking, thereby improving thermal conductivity and structural robustness.

WO2024247133A1PCT designated stage expired Publication Date: 2024-12-05YAMATO KOGYO CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/020180
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-30
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Ceramic circuit boards with high thermal conductivity substrates face challenges in lamination and cost due to the use of expensive, single-piece ceramics, which also increases the risk of cracking from thermal expansion differences.

Method used

A wiring board laminate with embedded highly thermally conductive ceramic members in openings of a wiring board, using a metal film-free region for improved adhesion and reduced thermal stress, and a thermosetting resin for bonding, allowing for easier lamination and cost reduction.

Benefits of technology

The solution enables effective heat dissipation and reduced cracking risks while maintaining thermal conductivity, allowing for the use of ceramic materials in a more cost-effective and structurally robust manner.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023020180_05122024_PF_FP_ABST
    Figure JP2023020180_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides a wiring board laminate with which a wiring board can be easily configured to have a laminated structure and the wiring board can be prevented from becoming expensive. The wiring board laminate 10 comprises a wiring board WB having an opening 19a, an embedding member 14 embedded in the opening 19a of the wiring board WB, a curing material 17 which has a thermosetting resin, which is arranged between the embedding member 14 and an inner peripheral surface of the opening 19a, and which is bonded to the wiring board WB, and a wiring layer 23 formed on surfaces of the wiring board WB, the embedding member 14, and the curing material 17, and is characterized in that the embedding member 14 has a ceramic body 13 and has metal films 15 formed on both surfaces of the ceramic body 13.
Need to check novelty before this filing date? Find Prior Art

Description

Wiring board laminate and method for manufacturing wiring board laminate

[0001] The present invention relates to a wiring board laminate and a method for manufacturing the wiring board laminate.

[0002] 2. Description of the Related Art Wiring board laminates that dissipate heat from the rear surface of wiring boards are known in order to suitably cool heat-generating components such as LEDs and electronic components such as QFNs (Quad For Non-Lead Packages) mounted on wiring boards.

[0003] In recent years, ceramic circuit boards using ceramics with high thermal conductivity, such as aluminum nitride (AlN), as substrate materials have become known for use on wiring substrates (see, for example, Patent Document 1). By using ceramics with high thermal conductivity as substrate materials, high heat dissipation and heat resistance can be achieved.

[0004] Patent No. 3690944

[0005] However, the ceramic circuit board (wiring board laminate) described in Patent Document 1 has the problem that it is difficult to laminate the substrates because ceramics is used for the entire substrate, and also has the problem that the substrate is expensive because relatively expensive ceramics is used for the entire substrate.

[0006] The present invention has been made to solve these problems, and has an object to provide a wiring board laminate that allows easy stacking of substrates and prevents the substrates from becoming expensive, and also to provide a method for manufacturing such a wiring board laminate.

[0007] [1] The wiring board laminate of the present invention comprises a wiring board having an opening, an embedding member embedded in the opening of the wiring board, a curing material containing a thermosetting resin and disposed between the embedding member and the inner peripheral surface of the opening and bonded to the wiring board, and a wiring layer formed on the surfaces of the wiring board, the embedding member, and the thermosetting resin, wherein the embedding member has a ceramic body and a metal film formed on both surfaces of the ceramic body.

[0008] The wiring board laminate of the present invention comprises a wiring board having an opening and a filling member filled in the opening of the wiring board, and the filling member has a ceramic body, so that high heat dissipation and heat resistance can be achieved by using ceramics with high thermal conductivity as the substrate material. Furthermore, because a wiring board is used, it is possible to laminate in the wiring board area while achieving high heat dissipation and heat resistance by using ceramics as the substrate material. Furthermore, it is possible to reduce costs compared to a ceramic circuit board in which the entire substrate is made of ceramics.

[0009] Furthermore, the wiring board laminate of the present invention comprises a wiring board having an opening and an embedded member embedded in the opening of the wiring board, and the embedded member has a ceramic body. Therefore, by using an individualized ceramic body rather than a single ceramic substrate and using the other area as a wiring board, the possibility of cracks occurring is reduced compared to when a single ceramic substrate is used.

[0010] [2] In the wiring board laminate of the present invention, it is preferable that at least one surface of the outer edge of the embedded member has a metal film-free region where the metal film is not formed, and that the hardening material is also arranged between the ceramic body and the wiring layer in the metal film-free region.

[0011] According to the wiring board laminate of the present invention, at least one surface of the outer edge of the embedded member has a metal film-free region where no metal film is formed, and the hardening material is also disposed between the ceramic body and the wiring layer in the metal film-free region, thereby improving the adhesion between the ceramic and the wiring layer, which are relatively difficult to adhere to each other.

[0012] However, if no metal film-free area is formed and a metal film is formed to cover the entire ceramic body, there is a risk of cracks occurring in the corners of the ceramic body due to the difference in thermal expansion coefficient between the metal film and the ceramic body.However, according to the wiring board laminate of the present invention, the outer edge of the embedded member has a metal film-free area where no metal film is formed, and the hardening material is also placed between the ceramic body and the wiring layer in the metal film-free area.Therefore, there is no metal film on the outer edge of the embedded member, and it is possible to prevent cracks from occurring in the corners of the ceramic body due to the difference in thermal expansion coefficient between the metal film and the ceramic body.

[0013] [3] In the wiring board laminate of the present invention, it is preferable that the ceramic body has metal film-free regions on both sides of the outer edge thereof, and that the hardening material is also disposed between the ceramic body and the wiring layer in both metal film-free regions of the ceramic body.

[0014] According to the wiring board laminate of the present invention, the ceramic body has areas where no metal film is formed on both sides, and the hardening material is also arranged between the ceramic body and the wiring layer in the areas where no metal film is formed. This makes it possible to improve the adhesion between the ceramic and the wiring layer, which are relatively difficult to adhere to on both sides of the ceramic body, and more reliably prevents cracks from occurring in the corners of the ceramic body.

[0015] [4] In the wiring board laminate of the present invention, it is preferable that the metal film non-formation region is formed over the entire outer edge portion so as to surround the metal film in plan view.

[0016] According to the wiring board laminate of the present invention, the metal film non-forming area is formed over the entire outer edge portion so as to surround the metal film, making it less likely that cracks will occur locally in part of the outer edge portion of the ceramic body, making it even more unlikely that cracks will occur in the ceramic body.

[0017] [5] In the wiring board laminate of the present invention, the metal film is preferably formed on the surface of the ceramic body by direct plating.

[0018] According to the wiring board laminate of the present invention, the metal film is formed on the surface of the ceramic body by direct plating, so that the ceramic body and the metal film can be bonded with high adhesion. Furthermore, since there is no need to place a bonding material between the ceramic body and the metal film to improve adhesion, it is possible to prevent the bonding material from reducing heat dissipation.

[0019] [6] In the wiring board laminate of the present invention, it is preferable that a metal layer is disposed on the surface of the wiring board, and that the wiring layer, metal layer, and metal film constitute circuit wiring.

[0020] According to the wiring board laminate of the present invention, a metal layer is disposed on the surface of the wiring board, and the circuit wiring is formed by the wiring layer, the metal layer, and the metal film, so that a variety of wiring structures can be formed even in the vertical direction.

[0021] [7] In the wiring board laminate of the present invention, the metal layer is preferably a metal plating film formed on the surface of the wiring board by plating.

[0022] According to the wiring board laminate of the present invention, the metal layer is a metal plating film formed on the surface of the wiring board by plating, and therefore has high adhesion to the wiring layer of the wiring board, making it easier to form a laminate board with a complex structure.

[0023] [8] In the wiring board laminate of the present invention, the embedding member is preferably rectangular in plan view.

[0024] In the wiring board laminate of the present invention, the embedding member has a rectangular shape in plan view, which makes it easy to process and align with the opening. Furthermore, when electronic elements are placed on the embedding member via the wiring layer, heat can be dissipated evenly from the electronic elements, many of which have a rectangular shape, preventing localized thermal stress and making it even more difficult for cracks to occur.

[0025] [9] A method for manufacturing a wiring board laminate of the present invention is a method for manufacturing a wiring board laminate according to any one of [1] to [3] above, the method comprising: obtaining a laminate including a wiring board or wiring board material having an opening, a filling member located inside the opening, and a cured product of a filler sheet or coating layer integrated with the wiring board or wiring board material and containing a thermosetting resin, the laminate having a thermosetting resin filled between the inner surface of the opening of the wiring board or wiring board material and the filling member; and grinding the cured product of the filler sheet or coating layer so that the thickness of the laminate after grinding is uniform, and removing the cured product.

[0026] According to the method for manufacturing a wiring board laminate of the present invention, a laminate structure is used in which a filling member is placed in an opening of a wiring board or wiring board material and a thermosetting resin is filled into the opening (by heating and pressurizing). Therefore, complicated processes are not required when placing the filling member, and filling members of various shapes can be accommodated. Furthermore, the cured material, such as a filling sheet, is ground so that the thickness of the laminate after grinding is consistent, and the cured material is removed. Therefore, the thermosetting resin filled into the opening is not integrated with the cured material, such as the filling sheet, and fracture or chipping of the filled thermosetting resin is less likely to occur when the cured material is peeled off. This improves the reliability of the filling member filling structure and the surface smoothness.

[0027]

[10] The method for manufacturing a wiring board laminate of the present invention preferably includes the steps of: preparing a laminate material including the wiring board or the wiring board material, the embedding member, and the filler sheet; integrating the laminate material by heating and pressurizing to obtain the laminate; and grinding the cured material of the filling sheet so that the thickness of the laminate after grinding is constant, thereby removing the cured material of the filling sheet.

[0028] According to the method for manufacturing a wiring board laminate of the present invention, a filling member is placed in an opening in a wiring board or wiring board material, and the thermosetting resin contained in a filling sheet is filled into the opening by heating and pressurizing, thereby enabling a laminate to be obtained by a dry process. In this case, complicated steps are not required when placing the filling member, and filling members of various shapes can be accommodated. Furthermore, the cured filling sheet is ground so that the thickness of the laminate after grinding is consistent, and the cured filling sheet is removed. This prevents the thermosetting resin filled into the opening from becoming integrated with the cured filling sheet, making it less likely to break or chip. This improves the reliability of the filling member filling structure and the surface smoothness.

[0029]

[11] In the method for producing a wiring board laminate of the present invention, the laminate is a laminate in which a resin film having an opening at a position corresponding to the opening in the wiring board or the wiring board material is attached to the wiring board or the wiring board material, and when removing the filler sheet or the cured product of the coating layer, the thickness of the laminate after grinding is set to a thickness that removes a portion of the resin film, and the method preferably further includes the steps of peeling off the remaining portion of the resin film from the laminate and removing the cured product of the thermosetting resin that covers the embedded member of the laminate.

[0030] According to the method for manufacturing a wiring board laminate of the present invention, by adhering a resin film to the wiring board or wiring board material, the thermosetting resin is less likely to adhere to the surface of the wiring board, etc., during filling. Furthermore, since the resin film is interposed between the cured material, such as the filling sheet, and the wiring board, etc., and the cured material is ground to a thickness that allows a portion of the resin film to be removed, the cured material can be more reliably removed. Furthermore, when the remaining portion of the resin film is peeled off from the laminate, the height of the thermosetting resin located in the openings in the resin film is reduced, making it easier to remove the convex thermosetting resin.

[0031] FIG. 1 is a cross-sectional view showing a wiring board laminate 10 according to embodiment 1. FIG. 2 is a view shown to explain an embedding member 14 in embodiment 1. FIG. 3 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 1. FIG. 4 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 1. FIG. 5 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 1. FIG. 6 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 2. FIG. 7 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 3. FIG. 8 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 3. FIG. 9 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to embodiment 3. FIG. 10 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to modification 1. FIG. 11 is a cross-sectional view shown to explain a method for manufacturing a wiring board laminate according to modification 2.

[0032] Hereinafter, a wiring board laminate and a method for manufacturing the wiring board laminate according to an embodiment of the present invention will be described with reference to the drawings. Note that the drawings described below are schematic diagrams that do not strictly reflect the actual structure, dimensions, vertical and horizontal scales, etc.

[0033] [Embodiment 1] 1. Configuration of a wiring board laminate 10 according to embodiment 1 Fig. 1 is a cross-sectional view showing a wiring board laminate 10 according to embodiment 1. Fig. 2 is a diagram shown to explain an embedding member 14 in embodiment 1. Fig. 2(a) is a cross-sectional view showing the embedding member 14, Fig. 2(b) is a perspective view showing the embedding member 14, and Fig. 2(c) is a diagram showing a ceramic wafer 100 on which the embedding member 14 is formed.

[0034] 1, the wiring board laminate 10 according to the first embodiment includes a wiring board WB, an embedding member 14, a curing material 17, and a wiring layer 23. The wiring layer 23 is formed on both sides of the wiring board laminate 10. The wiring layer 23 on the upper surface has a patterned wiring formed thereon, and the wiring layer 23 on the lower surface is formed over the entire surface and can be connected to a heat sink (not shown).

[0035] Therefore, in the wiring board laminate 10, if an electrical element (semiconductor chip, LED, reactor, etc.) is placed on the wiring layer 23 on the embedded member 14, the heat generated from the electrical element is transmitted to a heat sink (not shown) via the embedded member and the wiring layer 23 on the underside, and the heat can be dissipated from the heat sink to the outside.

[0036] The wiring board WB is a double-sided metal-clad laminate in which metal layers 20 are disposed on both sides of an insulating layer 19. The wiring board WB can be, for example, a glass epoxy substrate, but may also be a substrate made of an appropriate material described below. In the wiring board WB, a patterned metal layer is formed on one side (the upper surface in FIG. 1 ) of the insulating layer 19, but a non-wired metal layer may also be used. Furthermore, although a single-layer wiring board is used in the first embodiment for ease of explanation, a laminated wiring board may also be used.

[0037] The material of the insulating layer 19 preferably contains a thermosetting resin, and is preferably a prepreg containing a thermosetting resin and reinforcing fibers. The thermosetting resin may be any material that hardens when heated and has the heat resistance required for a wiring board. Specific examples of the thermosetting resin include various thermosetting resins such as epoxy resin, phenol resin, and polyimide resin.

[0038] The prepreg may be any material that contains a thermosetting resin, cures when heated, etc., and has the heat resistance required for a wiring board. Specific examples include composites of various thermosetting resins, such as epoxy resin, phenolic resin, and polyimide resin, with reinforcing fibers, such as glass fiber, ceramic fiber, aramid fiber, and paper.

[0039] Any metal may be used for the metal layer 20, such as copper, copper alloy, aluminum, stainless steel, nickel, iron, and other alloys. Among these, copper and aluminum are preferred from the viewpoint of thermal conductivity and electrical conductivity.

[0040] The wiring board WB has openings 18 in portions corresponding to the positions where the embedding members 14 are to be disposed. The wiring board WB usually has a plurality of openings 18. The openings 18 can be formed using a drill, a punch, a router, or the like. It is preferable that the size of the openings 18 be slightly larger than the ceramic body 13 of the embedding member 14.

[0041] The opening 18 has a rectangular shape, but any shape can be adopted, such as a circle, an oval, a square, or a shape that corresponds to the outer shape of the embedded member 14. Even in the case of a square or complex shape, the opening 18 can be formed into a complex shape by using a router or the like.

[0042] The embedding member 14 is embedded in the opening 18 of the wiring board WB. The ceramic body 13 has a substantially rectangular parallelepiped shape, and the embedding member 14 has a rectangular shape (substantially rectangular shape) in plan view (see FIGS. 2(a) and 2(b)), but can have any appropriate shape corresponding to the opening 18, such as a circle, an ellipse, a square, or other shapes. If the lateral size of the embedding member 14 is too large, it will be prone to falling off after filling, and if it is too small, it will be difficult to place, so the widest part should preferably be 0.1 to 20 mm.

[0043] The embedding member 14 has a ceramic body 13 and a metal film 15 formed on both surfaces of the ceramic body 13 (see FIGS. 2(a) and 2(b)). The thickness of the metal film 15 of the embedding member 14 is the same as the thickness of the metal layer 20 of the wiring board WB.

[0044] Both surfaces of the outer edge of the embedding member 14 have metal film-free regions E where the metal film 15 is not formed. That is, on both surfaces of the embedding member 14, the ceramic body 13 is exposed around the entire outer edge.

[0045] The embedded member 14 can be formed by forming a metal film on both sides of a flat ceramic substrate by direct plating, etching the metal film to a predetermined width along the dicing lines to form metal film-free areas E, and then cutting the substrate along the dicing lines to separate the substrate (see Figure 2 (c) for the ceramic substrate before cutting).

[0046] The ceramic body 13 is made of aluminum nitride (AlN), but alumina (Al 2 O 3 ) and other ceramic materials can be used.

[0047] The metal film 15 is formed on the surface of the ceramic body 13 by direct plating. Any metal may be used for the metal film 15, such as copper, copper alloy, aluminum, stainless steel, nickel, iron, or other alloys. Among these, copper and aluminum are preferred from the viewpoint of thermal conductivity and electrical conductivity.

[0048] The hardening material 17 contains a thermosetting resin and is disposed between the filling member 14 and the inner peripheral surface of the opening 18, and is bonded to the wiring board WB. The hardening material 17 is also disposed between the ceramic body 13 and the wiring layer 23 in the metal film non-forming region E.

[0049] The resin constituting the curing material 17 preferably has excellent adhesive strength with the embedding member 14 and does not impair voltage resistance characteristics. Furthermore, it is preferable that the resin deforms when heated and pressurized, hardens when heated, and has the heat resistance required for a wiring substrate. Examples of such resins include epoxy resins, phenolic resins, polyimide resins, and various engineering plastics, which can be used alone or in combination. Of these, epoxy resins are preferred because of their excellent bonding strength between metals. Among epoxy resins, bisphenol A epoxy resins, bisphenol F epoxy resins, hydrogenated bisphenol A epoxy resins, hydrogenated bisphenol F epoxy resins, triblock polymers having bisphenol A epoxy resin structures at both ends, and triblock polymers having bisphenol F epoxy resin structures at both ends are particularly preferred, as they have high fluidity and excellent compatibility with metal oxides and metal nitrides.

[0050] The wiring layer 23 is formed on both sides of the wiring board laminate 10, and is formed on the surfaces of the wiring board WB, the embedding member 14, and the curing material 17. The wiring layer 23 is a metal plating layer formed by metal plating the surfaces of the wiring board WB, the embedding member 14, and the curing material 17. The wiring layer 23 forms a wiring pattern together with the metal film 15 of the embedding member 14, and also forms a wiring pattern together with the metal layer 20 of the wiring board WB.

[0051] By placing electronic elements on the pattern wiring (particularly on the pattern wiring on the embedded member 14), heat generated from the electronic elements can be dissipated to the back side via the upper wiring layer 23, the embedded member 14 and the lower wiring layer 23, and can be dissipated to the outside via heat dissipation fins (not shown) connected to the surface of the back wiring layer 23.

[0052] 2. Manufacturing Method of Wiring Board Laminate According to Embodiment 1 Next, a method of manufacturing a wiring board laminate for manufacturing the wiring board laminate 10 will be described. Figures 3 to 5 are cross-sectional views shown to explain the manufacturing method of the wiring board laminate according to embodiment 1. Figures 3(a) to 3(e), 4(a) to 4(d), and 5(a) to 5(e) are diagrams showing the respective steps.

[0053] In this embodiment, first, as shown in FIGS. 3(a) and 3(b), a double-sided metal-clad laminate is used as the wiring board material WB', and a resin film 21 (filler sheet) is laminated on the wiring board material WB'.

[0054] The double-sided metal-clad laminate, which is the wiring board material WB', is formed by bonding a cured insulating layer 19' to a metal layer 20' on both sides. However, a material having a semi-cured insulating layer 19' may also be used and cured at any stage. It is also possible to use two single-sided metal-clad laminates, each having a semi-cured insulating layer 19' bonded to a metal layer 20', stacked with the insulating layers 19' facing each other. Furthermore, two metal plates (metal layers 20') may be stacked on both sides of the semi-cured insulating layer 19'. The wiring board WB may also have a patterned metal layer 20 on the surface of the insulating layer 19. The material for the semi-cured insulating layer 19' is preferably a material containing a thermosetting resin, and preferably a prepreg containing a thermosetting resin and reinforcing fibers.

[0055] The resin film 21 may simply be placed on the wiring board material WB' as shown in Figure 3 (b), but it is preferable to attach it to the wiring board WB or the wiring board material WB' from the viewpoint of preventing misalignment and preventing the hardener 17 from adhering to the surface of the wiring board WB or the wiring board material WB'.

[0056] The resin film 21 is preferably a resin film, and any of polyesters such as polyethylene terephthalate, polyolefins such as polyethylene and polypropylene, and polyamides can be used. However, from the viewpoint of heat resistance, polyesters such as polyethylene terephthalate are preferred. When attaching the resin film 21, it is preferable to provide an adhesive layer on the resin film 21. Examples of adhesives that can be used include rubber-based adhesives, acrylic-based adhesives, and silicone-based adhesives. Instead of providing an adhesive layer on the resin film 21, it is also possible to form an adhesive layer by separately applying it to the wiring board WB or the wiring board material WB'.

[0057] Next, as shown in FIG. 3( c), openings 18 are formed in the wiring board material WB′ in portions corresponding to the filling members 14. The wiring board material WB′ usually has a plurality of openings 18. The openings 18 can be formed using a drill, a punch, a router, or the like. It is preferable that the size of the openings 18 is slightly larger than the top surface of the filling members 14.

[0058] 3(d), a support film 22 is attached to the lower surface of the wiring board material WB'. The support film 22 can be the same as the resin film 21, and preferably has a similar adhesive layer.

[0059] Next, as shown in FIG. 3( e ), the wiring board material WB′ is placed on the support table 1 .

[0060] Next, as shown in FIG. 4A, a filling member 14 is placed inside the opening 18 of the wiring board material WB'. In this embodiment, a filling member 14 having the same thickness as the wiring board material WB' is used. Any filling member that can be placed inside the opening 18 of the wiring board material WB' is sufficient. If the filling member 14 has a thickness smaller than the thickness of the wiring board material WB', the upper surface of the filling member 14 can be exposed by removing the curing material 17 covering the upper surface of the filling member 14, as necessary.

[0061] The embedding member 14 can be placed by using a mounting device for surface-mounting micro-components on a wiring board, or by using embedding members 14 that have been previously formed on a support by etching or the like at the positions of the openings and then stacking and placing them on the wiring board WB or wiring board material WB', as will be described later.However, a preferred method is to place the embedding member 14 inside the openings by applying vibration.As such a device, a commercially available transfer device used for surface-mounting micro-components on a wiring board can be used.

[0062] As a method of applying vibration, similar to the transport of micro-components by a vibrating feeder, a method may be used in which the wiring board material WB' is vibrated while the filling material 14 is transported on the surface of the wiring board material WB' and continuously placed inside the openings. Alternatively, a batch method may be used in which a large number of filling materials 14 are supplied onto the upper surface of the wiring board material WB', and after vibration is applied to the wiring board material WB' and / or the filling materials 14, the filling materials 14 present outside the openings may be removed.

[0063] The frequency and amplitude of the vibration can be set appropriately depending on the size of the embedded member 14, but for example, the frequency is preferably 100 to 10,000 Hz and the amplitude is preferably 10 μm to 1,000 μm. A generator of such minute vibrations can be configured, for example, by a vibrator using an electromagnet and iron piece, or an electroacoustic transducer such as a piezoelectric transducer or a ferrite vibrator.

[0064] As shown in Figure 4(a), a method using a mounting device or the like is preferable for placing the embedded member 14 evenly inside the opening 18 (preferably in the central position), but even in the vibration application method, the embedded member 14 can be placed evenly inside the opening by, for example, placing a jig on the upper side of the wiring board WB or wiring board material WB' that has a smaller opening that opens at or near the central position of the opening.

[0065] Next, as shown in FIG. 4(b), a filling sheet 16' containing a hardening material 17 is laminated and arranged on the wiring board material WB' and the filling member 14 on the support table 1 to form a laminate material LM containing these.

[0066] The filling sheet 16' may be any material containing the curing material 17, and may be a sheet made of a thermosetting resin, but is preferably a prepreg containing the curing material 17 and reinforcing fibers. The resin constituting the filling sheet 16' is preferably one that has excellent adhesive strength with the embedding member 14 and does not impair voltage resistance characteristics, etc. Examples of such resins include epoxy resin, phenolic resin, polyimide resin, and various engineering plastics, which can be used alone or in combination of two or more. Of these, epoxy resin is preferred because of its excellent bonding strength between metals. Furthermore, the filling sheet 16' is preferably made of a material with high thermal conductivity, such as a resin containing a thermally conductive filler.

[0067] Any material may be used as the hardening material 17 as long as it deforms when heated and pressurized, hardens due to heat, etc., and has the heat resistance required for a wiring board. Specific examples of the hardening material 17 include various thermosetting resins such as epoxy resin, phenol resin, and polyimide resin.

[0068] The prepreg may be any material that deforms when heated and pressurized, solidifies when heated, etc., and has the heat resistance required for a wiring board. Specific examples include composites of various thermosetting resins such as epoxy resin, phenolic resin, and polyimide resin with reinforcing fibers such as glass fiber, ceramic fiber, aramid fiber, and paper.

[0069] 4(c), an example is shown that includes a step of integrating the laminate material LM by heating and pressurizing to obtain a laminate LB in which the hardening material 17 is filled between the inner surface of the opening of the wiring board material WB' and the filling member 14. In the example shown, this allows the formation of a laminate LB in which the height of the filling member 14 is the same as the surface of the wiring board WB or the wiring board material WB'.

[0070] 4(c) and 4(d), the filling sheet 16' becomes a thinner hardened material 16 by heating and pressurizing, and the hardening material 17 is filled between the inner surface of the opening 18 of the wiring board WB or wiring board material WB' and the embedding member 14, and the hardening material 17 of the filling sheet 16' covers the upper surface of the embedding member 14. The hardening material 17 is also disposed between the ceramic body 13 and the wiring layer 23 in the metal film non-forming region E where no metal film is formed.

[0071] The heating and pressing can be performed by placing the laminate material LM on a support table 1 and hot-pressing it with a press plate 2 or the like. The hot-pressing method can be performed using a heating and pressing device (thermal laminator, heating press) or the like, and the atmosphere can be made vacuum (vacuum laminator, etc.) to prevent air from being mixed in. In particular, when the support film 22 is attached to the underside, it is preferable to perform the heating and pressing in a reduced pressure atmosphere, as there is no escape route for the air inside the opening. Conditions such as heating temperature and pressure can be set appropriately depending on the material and thickness of the filling sheet 16', but a pressure of 0.5 to 30 MPa is preferred.

[0072] Next, as shown in Fig. 5(a), the cured product 16 of the coating layer is ground so that the thickness of the laminate LB after grinding is constant, and the cured product 16 is removed. In this embodiment, an example is shown in which the thickness of the laminate LB after grinding is set to a thickness that removes a portion of the resin film 21 when removing the cured product 16. As a result, the entire cured product 16 is removed, and also a portion of the resin film 21 is removed. Of course, only the entire cured product 16 may be removed, or both the cured product 16 and the entire resin film 21 may be removed.

[0073] A commercially available movable-table belt sander can be used as a device for grinding the laminate LB to a uniform thickness. In Fig. 5(a), the grinding belt supported on the surface of a rotating roll is shown by a virtual line. In reality, however, the grinding belt has a larger radius of curvature than the object to be ground, and the grinding belt, which moves together with the roll, is spaced apart from the moving table 3. By passing the laminate LB through this space, the laminate LB can be ground to a uniform thickness.

[0074] 5B, the remaining portion 21b of the resin film 21 is peeled off from the laminate LB, leaving the curing material 17 covering the embedding member 14, and forming a protrusion A made of the curing material 17.

[0075] 5(c), there is a step of removing the protruding portions A of the curing material 17 that covers the embedded member 14 of the laminate LB. This allows the upper surface of the laminate LB to be flattened. In the first embodiment, the resin film 21 is removed prior to removing the protruding portions A, but the resin film 21 can also be removed simultaneously with removing the protruding portions A.

[0076] The method of removing the convex portion A is preferably a grinding or polishing method, and examples thereof include a method using a grinding device having hard rotary blades in which multiple hard blades made of diamond or the like are arranged in the radial direction of a rotating plate, and a method using a sander, belt sander, grinder, surface grinding machine, hard abrasive grain molded product, etc.

[0077] Next, a step of peeling at least the support film 22 (lower surface side) from the laminate LB is carried out. When peeling the support film 22, it is preferable to set the adhesive strength between the embedding member 14 and the support film 22 to be smaller than the adhesive strength between the embedding member 14 and the curing material 17. With such adhesive strength, the support film 22 can be easily peeled off.

[0078] Next, as shown in Fig. 5(d), the exposed embedded member 14 and the metal layer 20' are metal-plated to form a metal-plated layer 23' (on both sides). Examples of metal species for the metal plating include copper, silver, and Ni. Examples of methods for forming the metal-plated layer 23' include a combination of electroless plating and electroplating.

[0079] 5( e), the metal plating layer 23′ and the metal layer 20′ are patterned to form the wiring layer 23. For example, an etching resist is used to etch the metal plating layer 23′ and the metal layer 20′ in a predetermined pattern, thereby forming the patterned wiring layer 23. The metal film 15 may also be etched.

[0080] In this manner, the wiring board laminate 10 can be manufactured.

[0081] 3. Effects of the wiring board laminate 10 and the method for manufacturing the wiring board laminate according to embodiment 1 The wiring board laminate 10 according to embodiment 1 includes a wiring board WB having an opening 18 and an embedding member 14 embedded in the opening 18 of the wiring board WB. The embedding member 14 has a ceramic body 13, and therefore high heat dissipation and heat resistance can be achieved by using ceramics with high thermal conductivity as the substrate material. Furthermore, because the wiring board WB is used, it is possible to laminate in the area of ​​the wiring board WB while achieving high heat dissipation and heat resistance by using ceramics as the substrate material. Furthermore, costs can be reduced compared to the case of a ceramic circuit board in which the entire substrate is made of ceramic.

[0082] Furthermore, the wiring board laminate 10 according to embodiment 1 includes a wiring board WB having an opening 18 and an embedded member 14 embedded in the opening 18 of the wiring board WB, and the embedded member 14 has a ceramic body 13. Therefore, by using an individualized ceramic body 13 rather than a single ceramic substrate and using the other region as a wiring board, the possibility of cracks occurring can be reduced compared to when a single ceramic substrate is used.

[0083] According to the wiring board laminate 10 of embodiment 1, the outer edge of the embedded member 14 has a metal film non-forming region E where the metal film 15 is not formed, and the hardening material 17 is also arranged between the ceramic body 13 and the wiring layer 23 in the metal film non-forming region E, thereby improving the adhesion between the ceramic body 13 made of ceramic, which is relatively difficult to adhere to, and the wiring layer 23 made of metal.

[0084] According to the wiring board laminate 10 of embodiment 1, the ceramic body 13 has metal film non-forming areas E on both sides thereof, and the hardening material 17 is also arranged between the ceramic body 13 and the wiring layer 23 in the metal film non-forming areas E. This makes it possible to improve the adhesion between the ceramic body 13 and the wiring layer 23, which are relatively difficult to adhere to on both sides of the ceramic body 13, and more reliably prevents cracks from occurring in the corners of the ceramic body 13.

[0085] According to the wiring board laminate 10 of embodiment 1, the metal film non-forming area E is formed over the entire outer edge so as to surround the metal film 15, so that local cracks are less likely to occur in part of the outer edge of the ceramic body 13, making it even more difficult for cracks to occur in the ceramic body 13.

[0086] According to the wiring board laminate 10 of the first embodiment, the metal film 15 is formed on the surface of the ceramic body 13 by direct plating, and therefore the ceramic body 13 and the metal film 15 can be bonded with high adhesion. Furthermore, since it is not necessary to dispose a bonding material between the ceramic body 13 and the metal film 15 to improve adhesion, it is possible to prevent the bonding material from reducing heat dissipation.

[0087] According to the wiring board laminate 10 of embodiment 1, a wiring layer 23 is arranged on the surface of the wiring board WB, and the circuit wiring is formed by the wiring layer 23, the metal layer 20, and the metal film 15, making it possible to form a wiring pattern with a complex configuration.

[0088] According to the wiring board laminate 10 of embodiment 1, the wiring layer 23 is a metal plating film formed on the surface of the wiring board WB by plating, so that the adhesion between the wiring board WB and the wiring layer 23 is high, making it easier to construct a laminate board with a complex structure.

[0089] In the wiring board laminate 10 according to the first embodiment, the embedding member 14 has a rectangular shape in plan view, which allows for easy processing and alignment with the opening. Furthermore, when electronic elements are disposed on the embedding member 14 via the wiring layer 23, heat can be dissipated evenly from the electronic elements, many of which have a rectangular shape, preventing localized increases in thermal stress and making it even more difficult for cracks to occur.

[0090] According to the method for manufacturing a wiring board laminate of the first embodiment, a laminate structure is used in which a filling member 14 is placed in an opening of a wiring board WB or wiring board material WB' and a thermosetting resin is filled into the opening by heating and pressurizing. Therefore, complicated processes are not required when placing the filling member 14, and filling members of various shapes can be accommodated. Furthermore, the cured material, such as the filling sheet 16', is ground so that the thickness of the laminate after grinding is consistent, and the cured material is removed. Therefore, the thermosetting resin filled inside the opening 18 is not integrated with the cured material, such as the filling sheet, and fracture or chipping of the filled thermosetting resin is less likely to occur when the cured material is peeled off. This improves the reliability of the filling member filling structure and the surface smoothness.

[0091] According to the method for manufacturing a wiring board laminate according to the first embodiment, a filling member 14 is placed in the opening 18 of the wiring board WB or wiring board material WB', and the thermosetting resin contained in the filling sheet 16' can be filled into the opening (by heating and pressurizing), thereby enabling the laminate to be obtained by a dry process. This eliminates the need for complicated steps when placing the filling member, and can accommodate filling members of various shapes. Furthermore, the cured filling sheet is ground to remove the cured filling sheet so that the thickness of the laminate after grinding is consistent. This prevents the thermosetting resin filling the opening from becoming integrated with the cured filling sheet, reducing the risk of breakage or chipping of the filled thermosetting resin. This improves the reliability of the filling member's filling structure and surface smoothness.

[0092] According to the method for manufacturing a wiring board laminate of embodiment 1, by adhering a resin film to the wiring board WB or wiring board material WB', the thermosetting resin is less likely to adhere to the surface of the wiring board or the like during filling. Furthermore, since the resin film is interposed between the cured material, such as the filling sheet, and the wiring board or the like, and the cured material is ground to a thickness that allows a portion of the resin film to be removed, the cured material can be more reliably removed. Furthermore, when the remaining portion of the resin film is peeled off from the laminate, the height of the thermosetting resin located in the openings in the resin film is reduced, making it easier to remove the convex thermosetting resin.

[0093] 6A to 6C are cross-sectional views illustrating a method for manufacturing a wiring substrate laminate according to embodiment 2. The method for manufacturing a wiring substrate laminate according to embodiment 2 basically includes the same steps as the method for manufacturing a wiring substrate laminate according to embodiment 1, but differs from the method for manufacturing a wiring substrate laminate according to embodiment 1 in that support film 22 is not used.

[0094] In embodiment 2, as shown in FIG. 6(a), the wiring board material WB′ is placed on a support 1 such as a mirror plate, and an embedding member 14 is placed inside the opening of the wiring board material WB′ (see FIG. 6(b)).

[0095] Next, a filling sheet containing the hardening material 17 is placed on top and heated and pressurized (see FIG. 6( c)). This integrates the components to obtain a laminate LB in which the hardening material 17 is filled between the inner surface of the opening 18 of the wiring board WB or wiring board material WB' and the filling member 14. During this process, the hardening material 17 may adhere to the periphery of the opening on the underside of the wiring board WB or wiring board material WB', but the adhered hardening material 17 can be removed by polishing or chemical treatment.

[0096] The subsequent steps are the same as those in the method for manufacturing a wiring board laminate according to the first embodiment, except for the step of removing the support film, and therefore a description thereof will be omitted.

[0097] As described above, the method for manufacturing a wiring board laminate according to the second embodiment differs from the method for manufacturing a wiring board laminate according to the first embodiment in that it does not use a support film 22. However, as with the method for manufacturing a wiring board laminate according to the first embodiment, a laminate structure is used in which a filling member is placed in an opening of a wiring board or wiring board material and a thermosetting resin is filled into the opening by heating and pressurizing. This eliminates the need for complicated steps when placing the filling member, and can accommodate filling members of various shapes. Furthermore, since the cured material, such as a filling sheet, is ground so that the thickness of the laminate after grinding is consistent, the cured material is removed. Therefore, the thermosetting resin filled into the opening is not integrated with the cured material, such as the filling sheet. Therefore, the thermosetting resin is less likely to break or chip when the cured material is peeled off. This improves the reliability of the filling member filling structure and the surface smoothness.

[0098] The method for manufacturing a wiring board laminate according to embodiment 2 has the same steps as the method for manufacturing a wiring board laminate according to embodiment 1 except that it does not use support film 22, and therefore has the corresponding effects of the method for manufacturing a wiring board laminate according to embodiment 1.

[0099] 7A to 7E are cross-sectional views illustrating a method for manufacturing a wiring board laminate according to a third embodiment. The method for manufacturing a wiring board laminate according to the third embodiment basically includes the same steps as the method for manufacturing a wiring board laminate according to the first embodiment, but differs from the method for manufacturing a wiring board laminate according to the first embodiment in that resin film 21 is not used.

[0100] In the third embodiment, a laminate material LM is prepared (see FIG. 7( a)), which includes a wiring board material WB' having an opening 18 and no resin film 21 attached thereto, a filling member 14 positioned inside the opening, and a filler sheet 16' laminated on the wiring board material WB' and containing a curing material 17 (see FIG. 7( b)). In this embodiment, a support film 22 is attached to the underside of the wiring board material WB'.

[0101] Next, in the same manner as in the previous embodiment, the laminate material LM is integrated by heating and pressurizing to obtain a laminate LB in which the hardening material 17 is filled between the inner surface of the opening 18 of the wiring board material WB' and the filling member 14. This makes it possible to form a laminate LB in which the height of the filling member 14 is the same as the surface of the wiring board material WB'.

[0102] 7(d), the cured material 16 of the filling sheet 16' is then ground so that the thickness of the laminate LB after grinding is constant, and the cured material 16 of the filling sheet 16' is removed. In this embodiment, when removing the cured material 16 of the filling sheet 16', the thickness of the laminate LB after grinding is set to a thickness that removes all or almost all of the cured material 16. As a result, all or almost all of the cured material 16 is removed.

[0103] Next, the support film 22 is removed. The subsequent steps are the same as those in the method for manufacturing the wiring board laminate according to embodiment 1, and therefore, a description thereof will be omitted. In this manner, the wiring board laminate 10 according to embodiment 3 can be manufactured (see FIG. 7( e)).

[0104] As described above, the method for manufacturing a wiring board laminate according to the third embodiment differs from the method for manufacturing a wiring board laminate according to the first embodiment in that it does not use resin film 21. However, as with the method for manufacturing a wiring board laminate according to the first embodiment, a laminate structure is used in which a filling member is placed in an opening of a wiring board or wiring board material and a thermosetting resin is filled into the opening by heating and pressurizing. This eliminates the need for complicated steps when placing the filling member, and can accommodate filling members of various shapes. Furthermore, since the cured material, such as a filling sheet, is ground so that the thickness of the laminate after grinding is consistent, the cured material is removed. Therefore, the thermosetting resin filled into the opening is not integrated with the cured material, such as the filling sheet. Therefore, breakage or chipping of the filled thermosetting resin is less likely to occur when the cured material is peeled off. This improves the reliability of the filling member filling structure and the surface smoothness.

[0105] The method for manufacturing a wiring board laminate according to embodiment 3 has the same steps as the method for manufacturing a wiring board laminate according to embodiment 1 except that resin film 21 is not used, and therefore has the corresponding effects among the effects of the method for manufacturing a wiring board laminate according to embodiment 1.

[0106] 8A and 8B are cross-sectional views illustrating a method for manufacturing a wiring substrate laminate according to embodiment 4. The method for manufacturing a wiring substrate laminate according to embodiment 4 basically includes the same steps as the method for manufacturing a wiring substrate laminate according to embodiment 1, but differs from the method for manufacturing a wiring substrate laminate according to embodiment 1 in that embedding member 14 is disposed on support film 22 before disposing wiring substrate material WB.

[0107] In embodiment 4, as shown in Figure 8(a), before placing the wiring board material WB', the embedding member 14 is placed on the support film 22, and then the wiring board material WB is placed on the support film 22 while aligning it with the embedding member 14, and the filling sheet 16' is placed on the wiring board material WB and the embedding member 14.

[0108] The subsequent steps are the same as those in the method for manufacturing the wiring board laminate according to the first embodiment, and therefore a description thereof will be omitted.

[0109] As described above, the method for manufacturing a wiring board laminate according to the fourth embodiment differs from the method for manufacturing a wiring board laminate according to the first embodiment in that the embedding member 14 is placed on the support film 22 before the wiring board material WB is placed. However, as with the method for manufacturing a wiring board laminate according to the first embodiment, a laminate structure is used in which an embedding member is placed in an opening of a wiring board or wiring board material and a thermosetting resin is filled into the opening by heating and pressurizing. This eliminates the need for complicated steps when placing the embedding member, and can accommodate embedding members of various shapes. Furthermore, since the cured material, such as a filling sheet, is ground so that the thickness of the laminate after grinding is consistent, the cured material is removed. Therefore, the thermosetting resin filled into the opening is not integrated with the cured material, such as the filling sheet. This reduces the risk of breakage or chipping of the filled thermosetting resin when the cured material is peeled off. This improves the reliability of the embedding member filling structure and the surface smoothness.

[0110] The method for manufacturing a wiring board laminate according to embodiment 4 has the same steps as the method for manufacturing a wiring board laminate according to embodiment 1, except that the embedding member 14 is placed on the support film 22 before the wiring board material WB is placed, and therefore has the corresponding effects among the effects of the method for manufacturing a wiring board laminate according to embodiment 1.

[0111] 9A to 9E are cross-sectional views illustrating a method for manufacturing a wiring board laminate according to a fifth embodiment. The method for manufacturing a wiring board laminate according to the fifth embodiment basically includes the same steps as the method for manufacturing a wiring board laminate according to the first embodiment. However, the method differs from the method for manufacturing a wiring board laminate according to the first embodiment in that a wiring board WB having wiring patterns 20 and an insulating layer 19 as metal layers is used instead of the wiring board material WB.

[0112] 9(a), a lamination material LM including a support film 22 on which embedding members 14 are formed, a wiring board WB having a plurality of openings 18 in portions corresponding to the embedding members 14, and a filler sheet 16′ including a curing material 17 is laminated so that the embedding members 14 are located inside each of the openings 18. At this time, the upper surface of the wiring board WB is preferably covered with a resin film 21, and it is more preferable that the resin film 21 has a plurality of openings 21a in portions corresponding to the embedding members 14.

[0113] 9(b), a process is carried out in which the laminate material LM is integrated by heating and pressurizing to obtain a laminate LB in which the hardening material 17 is filled between the inner surface of the opening 18 of the wiring board WB and the filling member 14. This makes it possible to form a laminate LB in which the height of the filling member 14 is the same as or slightly lower than the top surface of the wiring board WB. This process can be carried out in the same manner as in the previous embodiment.

[0114] 9(c), similar to the previous embodiment, the cured material 16 of the filling sheet 16' is ground so that the thickness of the laminate LB after grinding is constant, and a process for removing the cured material 16 of the filling sheet 16' is performed. In this embodiment, an example is shown in which, when removing the cured material 16 of the filling sheet 16', the thickness of the laminate LB after grinding is set to a thickness that removes a portion of the resin film 21. As a result, the entire cured material 16 is removed, and a portion of the resin film 21 is also removed. Of course, it is also possible to remove only the entire cured material 16.

[0115] 9(d) and 9(e), the resin film 21 on the upper surface is peeled off, and the thermosetting resin (protrusions A) covering the upper surface of the embedding member 14 is removed. If the upper surface of the embedding member 14 is higher than the upper surface of the wiring board WB, it is possible to remove the embedding member 14 by that amount, if necessary.

[0116] This makes it possible to obtain a wiring board having an insulating layer 19, an embedding member 14 embedded in the insulating layer 19, and a wiring layer (wiring pattern 20), in which the insulating layer 19 contains a cured product 16 of the filling sheet 16', and the periphery of the embedding member 14 is bonded to the insulating layer 19 by a curing material 17 that is different from the resin component of the insulating layer 19.

[0117] When using a double-sided wiring board as in the illustrated example, it is preferable to have an interlayer connection structure such as plated through holes, metal bumps, filled vias, or plated vias.

[0118] As described above, the method for manufacturing a wiring board laminate according to the fifth embodiment differs from the method for manufacturing a wiring board laminate according to the first embodiment in that a wiring board WB having a wiring pattern 20 and an insulating layer 19 is used instead of a wiring board material WB. However, as with the method for manufacturing a wiring board laminate according to the first embodiment, a laminate structure is used in which a filling member is placed in an opening of a wiring board or wiring board material and a thermosetting resin is filled into the opening by heating and pressurizing. This eliminates the need for complicated processes when placing the filling member, and can accommodate filling members of various shapes. Furthermore, since the cured material, such as a filling sheet, is ground so that the thickness of the laminate after grinding is consistent, the cured material is removed. Therefore, the thermosetting resin filled into the opening is not integrated with the cured material, such as the filling sheet. Therefore, breakage or chipping of the filled thermosetting resin is less likely to occur when the cured material is peeled off. This improves the reliability of the filling member filling structure and the surface smoothness.

[0119] The method for manufacturing a wiring board laminate according to embodiment 5 has the same steps as the method for manufacturing a wiring board laminate according to embodiment 1, except that it uses a wiring board WB having a wiring pattern 20 and an insulating layer 19 instead of a wiring board material WB, and therefore has the corresponding effects among the effects of the method for manufacturing a wiring board laminate according to embodiment 1.

[0120] Although the present invention has been described above based on the above embodiment, the present invention is not limited to the above embodiment and can be embodied in various forms without departing from the spirit of the present invention, and for example, the following modifications are also possible.

[0121] (1) The number, material, shape, position, size, etc. of the components described in each of the above embodiments are examples and can be changed within the scope that does not impair the effects of the present invention.

[0122] (2) In each of the above embodiments (including the above and following modified examples; the same applies hereinafter), the wiring board laminate has an insulated front and rear surfaces, but the present invention is not limited to this. A wiring board laminate may also be used in which the front and rear surfaces are electrically connected. In this case, a wiring board laminate in which the front and rear surfaces are electrically connected can be obtained by forming through holes in the openings of the wiring board material WB and plating the inner surfaces of the through holes to form plated through holes (wiring board overall according to modified example 1; see FIGS. 10(a) to 10(c)).

[0123] (3) In the above embodiments, the metal layer 20 has a single-layer structure, but the present invention is not limited to this. A multilayer wiring board having two or more metal layers may also be used.

[0124] (4) In the above embodiments, an example of forming a laminate LB using a filling sheet 16' containing a curing material 17 was described, but the present invention is not limited thereto. As shown in FIG. 11( a), a laminate LB is formed using a coating material containing a curing material 17, in which a cured product 16 of a coating layer having a recess 17a above an embedding member 14 is integrated with a wiring board material WB' (see FIG. 11( a)). The cured product 16 of the coating layer is ground so that the thickness of the laminate LB after grinding is uniform. In performing the step of removing the cured product 16, a peripheral portion 17b of the cured product 16 of the coating layer and a portion of the thickness of the resin film 21 are removed (see FIG. 11( b)). The remaining portion 21b of the resin film 21 is peeled off from the laminate LB (see FIG. 11( c)). The cured product 16 of the coating layer on the upper surface of the embedding member 14 may be removed by polishing, such as buffing or sandblasting (see FIG. 11( d)).

[0125] (5) In the above embodiments, the wiring board laminate is manufactured using the wiring board material WB′ in which metal layers are formed on both surfaces of the ceramic body 13, but the present invention is not limited to this. The wiring board laminate may also be manufactured using a wiring board material in which a metal layer is formed on one surface of the ceramic body 13.

[0126] (6) In the above embodiments, the ceramic body has a metal film-free region on both sides of the outer edge thereof, but the present invention is not limited to this. The ceramic body may have a metal film-free region on only one side of the outer edge thereof, and the metal film-free region may be filled with a hardening agent, or the ceramic body may have a metal film-free region on only a portion of the outer edge thereof, and the metal film-free region may be filled with a hardening agent.

[0127] (7) In the above embodiments, the thickness of the metal film 15 of the embedding member 14 is the same as the thickness of the metal layer 20 of the wiring board WB, but the present invention is not limited to this. The thickness of the metal film 15 of the embedding member 14 may be different from the thickness of the metal layer 20 of the wiring board WB. If the thickness of the metal film 15 of the embedding member 14 is thinner than the thickness of the metal layer 20 of the wiring board WB, the thermal resistance when heat generated by the electronic element is transferred to the back side through the embedding member 14 is reduced, thereby making it easier to transfer the heat generated by the electronic element to the outside. Furthermore, if the thickness of the metal film 15 of the embedding member 14 is thicker than the thickness of the metal layer 20 of the wiring board WB, the stress of the ceramic body 13 and the stress of the metal film 15 can be adjusted.

[0128] 10... wiring board laminate, 13... ceramic body, 14... embedded member, 15... metal film, 17... hardening material, 19... insulating layer, 20... metal layer, 19a... opening, 23... wiring layer, E... metal film non-forming region, WB... wiring board

Claims

1. A wiring board laminate comprising: a wiring board having an opening; a filling member filled in the opening of the wiring board; a hardening material including a thermosetting resin, disposed between the filling member and an inner peripheral surface of the opening and adhered to the wiring board; and a wiring layer formed on surfaces of the wiring board, the filling member and the thermosetting resin, wherein the filling member has a ceramic body and a metal film formed on both surfaces of the ceramic body.

2. The wiring board laminate described in claim 1, characterized in that at least one surface of the outer edge of the embedded member has a metal film-free area where the metal film is not formed, and the hardening material is also disposed between the ceramic body and the wiring layer in the metal film-free area.

3. The wiring board laminate described in claim 2, characterized in that the embedded member has a non-metal film area on both sides of the outer edge thereof, and the hardening material is also disposed between the ceramic body and the wiring layer in both of the non-metal film areas of the ceramic body.

4. A wiring board laminate according to any one of claims 1 to 3, characterized in that, in a plan view, the metal film non-forming area is formed over the entire outer edge portion so as to surround the metal film.

5. The wiring board laminate according to any one of claims 1 to 3, wherein the metal film is formed on the surface of the ceramic body by direct plating.

6. A wiring board laminate according to any one of claims 1 to 3, characterized in that a metal layer is disposed on the surface of the wiring board, and the wiring layer, the metal layer and the metal film constitute circuit wiring.

7. The wiring board laminate according to claim 6, wherein the metal layer is a metal plating film formed on the surface of the wiring board by plating.

8. The wiring board laminate according to any one of claims 1 to 3, characterized in that the opening is rectangular, and the filling member is rectangular in plan view.

9. A method for producing a wiring board laminate according to any one of claims 1 to 3, comprising the steps of: obtaining a laminate comprising a wiring board or wiring board material having an opening, a filling member located inside the opening, and a hardened product of a filling sheet or coating layer integrated with the wiring board or wiring board material and containing a thermosetting resin, the laminate being filled with thermosetting resin between the inner surface of the opening of the wiring board or wiring board material and the filling member; and grinding the hardened product of the filling sheet or coating layer so that the thickness of the laminate after grinding is constant, thereby removing the hardened product.

10. A method for manufacturing a wiring board laminate as described in claim 9, characterized in that it comprises the steps of: preparing a laminate material including the wiring board or the wiring board material, the embedding member, and the filling sheet; integrating the laminate material by heating and pressurizing to obtain the laminate; and grinding the hardened material of the filling sheet so that the thickness of the laminate after grinding is constant, thereby removing the hardened material of the filling sheet.

11. The method for manufacturing a wiring board laminate according to claim 9 or 10, characterized in that the laminate is a laminate in which a resin film having an opening at a position corresponding to the opening of the wiring board or wiring board material is attached to the wiring board or wiring board material, and when removing the filling sheet or the cured product of the coating layer, the thickness of the laminate after grinding is set to a thickness that removes a portion of the resin film, and further includes a step of peeling off the remaining portion of the resin film from the laminate, and a step of removing the cured product of the thermosetting resin covering the embedded member of the laminate.

Citation Information

Patent Citations

  • Circuit board including ceramic inlay

    JP2015103809A

  • Method for manufacturing wiring board or wiring board material

    JP7274809B1

  • Multilayer printed circuit board and manufacturing method therefor

    WO2011102561A1