A technology for steel strands and waste products, which is applied in the field of changing the length of waste products in the process of steel strand joints, can solve the problems of waste of materials, damage, etc., and achieve the effects of reducing production costs and improving utilization rates
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0014] The method for changing the length of steel strand joint process waste product of the present invention, it comprises the following steps:
[0015] a. After the production of the last batch of steel strands is completed, some steel wires are left on the I-shaped wheel 1;
[0016] b. Put the next batch of steel wire full I-shaped wheels to be produced on the shelf and connect with the remaining steel wires of the previous batch through the splicing machine;
[0017] c. Open the equipment, make the joint pass through the ply crimping groove 2 until it reaches the exit of the first tension wheel 3, and stop; the process parameters are: the speed of the take-up wheel 6 is 50-60 meters per minute, and the intermediate frequency heating furnace 4 The temperature is 380°C, the first tension wheel 3 and the second tension wheel 5 rotate asynchronously to form a tension of 10N;
[0018] d. Turn on the equipment again, so that the joint passes through the intermediate frequency ...