Semiconductor structure and method for forming semiconductor structure

By designing an isolation structure higher than the substrate surface and a gate structure spanning the nanostructure in the fork nanosheet structure, the problem of poor performance of the fork nanosheet is solved, and better channel control and driving current are achieved , expands the miniaturability of the device.

CN113809175BActive Publication Date: 2024-11-22SEMICON MFG INT (SHANGHAI) CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010538103.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-06-12
Publication Date
2024-11-22
Estimated Expiration
2040-06-12

AI Technical Summary

Technical Problem

The performance of fork nanosheets needs to be improved, especially in terms of channel control and driving current. The existing processes limit the spacing between NMOS and PMOS devices, resulting in poor performance.

Method used

Design a semiconductor structure, including a substrate, a base nanowire, a first and second nanostructures, and an isolated structure, with an opening between the first and second nanostructures, the bottom plane of the isolation structure is higher than the substrate surface, and the gate The structure spans the isolation structure, the first and second nanostructures, and forms the underlying nanowires through dry etching process to reduce the volume of the isolation structure and improve the stress distortion problem.

Benefits of technology

By reducing the height of the isolation structure and reducing stress offsets, the performance of the semiconductor structure is improved, the channel control capability and driving current are improved, and the miniaturization of the device is expanded.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113809175B_ABST
    Figure CN113809175B_ABST
Patent Text Reader

Abstract

A semiconductor structure and a method for forming the semiconductor structure, the structure comprising: a substrate; a bottom layer nanowire located on the substrate; a first nanostructure and a second nanostructure located on the bottom layer nanowire, a first opening being provided between the first nanostructure and the second nanostructure, the bottom plane of the first opening being higher than the surface of the substrate; an isolation structure located in the first opening; and a gate structure located on the substrate, the gate structure spanning the isolation structure, the first nanostructure and the second nanostructure. The performance of the semiconductor structure is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the semiconductor structure. Background Art

[0002] FinFET transistor architecture is the main force in today's semiconductor industry. However, with the continuous miniaturization of devices, when the channel length is small to a certain value, the FinFET structure cannot provide sufficient electrostatic control and sufficient drive current. Therefore, the Nanosheet structure, namely the gate-all-around technology (GAA), is introduced. Compared with the FinFET, the surrounding gate characteristic of the Nanosheet provides excellent channel control capabilities. At the same time, the excellent distribution of the channel in three dimensions optimizes the effective drive current per unit area.

[0003] As the journey towards smaller track heights continues, further reductions in cell height will require smaller spacing between NMOS and PMOS devices within a standard cell. However, for FinFETs and nanosheets, the process limits the spacing between these NMOS and PMOS devices. To expand the scalability of these devices, an innovative architecture is proposed, called a forksheet device. Forksheets can be considered a natural extension of nanosheets. Compared to nanosheets, the channel of forksheets is controlled by a forked gate structure, which is achieved by introducing a "dielectric wall" between NMOS and PMOS devices before gate patterning. The wall physically isolates the NMOS gate trench from the PMOS gate trench, thereby significantly reducing the spacing between NMOS and PMOS, making forksheets have better area and performance scalability.

[0004] However, the performance of fork-shaped nanosheets needs to be improved. Summary of the invention

[0005] The technical problem solved by the present invention is to provide a semiconductor structure and a method for forming the semiconductor structure, so as to improve the performance of fork-shaped nanosheets.

[0006] To solve the above technical problems, the technical solution of the present invention provides a semiconductor structure, including: a substrate; an underlying nanowire located on the substrate; a first nanostructure and a second nanostructure located on the underlying nanowire, wherein a first opening is provided between the first nanostructure and the second nanostructure, and a bottom plane of the first opening is higher than the surface of the substrate; an isolation structure located in the first opening; and a gate structure located on the substrate, wherein the gate structure spans the isolation structure, the first nanostructure and the second nanostructure.

[0007] Optionally, the first nanostructure includes: a plurality of first nanowires separated from each other along a direction perpendicular to the substrate surface, with a first groove between adjacent first nanowires; the second nanostructure includes: a plurality of second nanowires separated from each other along a direction perpendicular to the substrate surface, with a second groove between adjacent second nanowires; the gate structure is also located in the first groove and the second groove.

[0008] Optionally, the method further includes: a dielectric layer located between the bottom nanowire and the gate structure, wherein the dielectric layer is also located on the sidewall of the bottom nanowire.

[0009] Optionally, a bottom plane of the isolation structure is lower than a bottom plane of the gate structure.

[0010] Optionally, a bottom plane of the isolation structure is lower than a top plane of the bottom nanowires.

[0011] Optionally, the height of the bottom plane of the isolation structure below the top plane of the bottom nanowires ranges from 0 nanometers to 50 nanometers.

[0012] Optionally, a bottom plane of the isolation structure is higher than a bottom plane of the dielectric layer.

[0013] Optionally, the etching selectivity ratio of the material of the isolation structure and the material of the dielectric layer is different.

[0014] Optionally, the thickness of the bottom layer nanowires ranges from 0 nanometers to 150 nanometers.

[0015] Correspondingly, the technical solution of the present invention also provides a method for forming a semiconductor structure, including: providing a substrate; forming an initial bottom layer nanowire and an initial first nanostructure and an initial second nanostructure located on the initial bottom layer nanowire on the substrate, wherein a first opening is provided between the initial first nanostructure and the initial second nanostructure, and a bottom plane of the first opening is higher than the surface of the substrate; forming an isolation structure in the first opening; after forming the isolation structure, etching the initial bottom layer nanowire using the initial first nanostructure, the initial second nanostructure and the isolation structure as masks until the substrate surface is exposed to form a bottom layer nanowire.

[0016] Optionally, the process of etching the initial bottom layer nanowires includes a dry etching process.

[0017] Optionally, the initial first nanostructure includes: a plurality of first sacrificial layers and first nanowires located between adjacent first sacrificial layers; a first bottom sacrificial layer located between the initial bottom nanowires and the first sacrificial layer; the initial second nanostructure includes: a plurality of second sacrificial layers and second nanowires located between adjacent second sacrificial layers; and a second bottom sacrificial layer located between the initial bottom nanowires and the second sacrificial layer.

[0018] Optionally, the method for forming the initial underlying nanowires, the initial first nanostructure and the initial second nanostructure includes: forming an underlying nanowire material layer on a substrate; forming a stacked material structure on the underlying nanowire material layer, the stacked material structure including an underlying sacrificial material layer, a plurality of sacrificial material layers located on the underlying sacrificial material layer, and a nanowire material layer located between adjacent sacrificial material layers; forming a mask structure on the stacked material structure, the mask structure exposing a portion of the surface of the stacked material structure; using the mask structure as a mask, removing a portion of the stacked material structure and a portion of the underlying nanowire material layer, forming a first opening in the stacked material structure and the underlying nanowire material layer, and forming the initial first nanostructure and the initial second nanostructure.

[0019] Optionally, the bottom plane of the isolation structure is lower than the bottom plane of the first sacrificial layer adjacent to the first bottom sacrificial layer; the bottom plane of the isolation structure is lower than the bottom plane of the second sacrificial layer adjacent to the second bottom sacrificial layer.

[0020] Optionally, a bottom plane of the isolation structure is lower than a top plane of the initial bottom nanowires.

[0021] Optionally, the height of the bottom plane of the isolation structure below the top plane of the bottom nanowires ranges from 0 nanometers to 50 nanometers.

[0022] Optionally, the bottom plane of the isolation structure is higher than the bottom plane of the first bottom sacrificial layer; the bottom plane of the isolation structure is higher than the bottom plane of the second bottom sacrificial layer.

[0023] Optionally, the process of forming the mask structure includes a self-aligned multi-patterning technique.

[0024] Optionally, the process of removing part of the stacked material structure and part of the bottom nanowire material layer includes a dry etching process.

[0025] Optionally, after forming the bottom nanowire, it also includes: removing the first bottom sacrificial layer and the second bottom sacrificial layer, forming a second opening between the bottom nanowire and the first sacrificial layer, forming a third opening between the bottom nanowire and the second sacrificial layer, the second opening and the third opening exposing a portion of the side wall surface of the isolation structure; forming a dielectric layer in the second opening and the third opening, the dielectric layer is also located on the side wall of the bottom nanowire.

[0026] Optionally, after forming the dielectric layer, it also includes: forming a dummy gate structure on the dielectric layer, the dummy gate structure spanning the isolation structure, the initial first nanostructure and the initial second nanostructure; after forming the dummy gate structure, forming a dielectric layer on the substrate, the dielectric layer being located on the sidewall of the dummy gate structure; removing the dummy gate structure to form an initial gate opening in the dielectric layer; removing the first sacrificial layer and the second sacrificial layer exposed by the initial gate opening, forming a gate opening in the dielectric layer, and forming the first nanostructure and the second nanostructure; forming a gate structure in the gate opening.

[0027] Optionally, the method for forming an isolation structure in the first opening includes: forming an isolation material layer in the first opening and on the surfaces of the initial first nanostructure and the initial second nanostructure; removing the isolation material layer on the surfaces of the initial first nanostructure and the initial second nanostructure to form an isolation structure in the first opening.

[0028] Optionally, the process of forming the isolation material layer includes an atomic layer deposition process.

[0029] Optionally, the process of removing the isolation material layer on the surface of the initial first nanostructure and the initial second nanostructure includes a wet etching process.

[0030] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0031] In the semiconductor structure in the technical solution of the present invention, the bottom plane of the isolation structure is higher than the substrate surface, so that the height of the isolation structure is reduced, and the volume of the isolation structure located between the first nanostructure and the second nanostructure is reduced. When the gate structure and the dielectric layer located on the side wall of the gate structure are subsequently formed, the stress imbalance caused by the different thermal expansion coefficients between the isolation structure and the dielectric layer located on both sides of the first nanostructure and the second nanostructure is improved, thereby improving the bending deformation of the first nanostructure and the second nanostructure, thereby improving the performance of the semiconductor structure.

[0032] The method for forming a semiconductor structure in the technical solution of the present invention forms an initial bottom layer nanowire and an initial first nanostructure and an initial second nanostructure on the initial bottom layer nanowire on a substrate, wherein a first opening is provided between the initial first nanostructure and the initial second nanostructure, and the bottom plane of the first opening is higher than the substrate surface, and then an isolation structure is formed in the first opening, and the bottom plane of the isolation structure is higher than the substrate surface. In the semiconductor structure formed by the method, the bottom plane of the isolation structure is higher than the substrate surface, so that the height of the isolation structure is reduced, and the volume of the isolation structure between the first nanostructure and the second nanostructure is reduced. When the gate structure and the dielectric layer on the sidewall of the gate structure are subsequently formed, the stress imbalance caused by the different thermal expansion coefficients between the isolation structure and the dielectric layer on both sides of the first nanostructure and the second nanostructure is improved, thereby improving the bending deformation of the first nanostructure and the second nanostructure, and thus improving the performance of the semiconductor structure.

[0033] Furthermore, the process of forming a mask structure on the stacked material structure includes a self-aligned multiple patterning technology, so that the initial first nanostructure, the initial second nanostructure and the first opening can be formed through a mask process, thereby saving production costs and improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 and Figure 2 is a schematic cross-sectional structural diagram of a semiconductor structure forming process in one embodiment;

[0035] Figures 3 to 8 It is a schematic cross-sectional structure diagram of the semiconductor structure forming process in an embodiment of the present invention. DETAILED DESCRIPTION

[0036] As described in the background art, the performance of the existing fork-shaped nanosheets needs to be improved. Now, an analysis and explanation will be given in conjunction with specific embodiments.

[0037] Figure 1 and Figure 2 It is a schematic cross-sectional structure diagram of a semiconductor structure forming process in one embodiment.

[0038] Please refer to Figure 1, including: a substrate 100; an isolation structure 109 located on the substrate 100; an initial first nanostructure and an initial second nanostructure located on both sides of the isolation structure 109, the initial first nanostructure including a first bottom nanowire 101, a first bottom sacrificial layer 105 located on the first bottom nanowire 101, a plurality of first sacrificial layers 107 located on the first bottom sacrificial layer 105 and a first nanowire 103 located between adjacent first sacrificial layers 107, the initial second nanostructure including a second bottom nanowire 102, a second bottom sacrificial layer 106 located on the second bottom nanowire 102, a plurality of second sacrificial layers 108 located on the second bottom sacrificial layer 106 and a second nanowire 104 located between adjacent second sacrificial layers 108.

[0039] Please refer to Figure 2 , remove the first bottom sacrificial layer 105 and the second bottom sacrificial layer 106, form a first dielectric layer 110 between the first bottom sacrificial layer 105 and the first bottom nanowire 101 and between the second bottom sacrificial layer 106 and the second bottom nanowire 102, and form a second dielectric layer 111 on the sidewalls of the first bottom nanowire 101 and the second bottom nanowire 102. The first dielectric layer 110 and the second dielectric layer 111 are formed simultaneously.

[0040] During the formation of the semiconductor structure, the first dielectric layer 110 is used to electrically isolate the subsequently formed gate structure from the substrate 100. During the formation of the first dielectric layer 110, the isolation structure 109 is first formed, and then the first bottom sacrificial layer 105 and the second bottom sacrificial layer 106 are removed to form the first dielectric layer 110, and then a gate structure (not shown) spanning the initial first nanostructure, the initial second nanostructure and the isolation structure 109 is formed on the first dielectric layer 110, and then a dielectric layer (not shown) is formed on the sidewall of the gate structure, wherein the gate structure only covers a portion of the isolation structure 109 surface, and the dielectric layer is also located on the sidewall surface of the initial first nanostructure portion and the sidewall surface of the initial second nanostructure portion.

[0041] However, the material of the isolation structure 109 is different from that of the dielectric layer, and thus the thermal expansion coefficients of the isolation structure 109 and the dielectric layer are different. After annealing, the volume changes of the isolation structure 109 and the dielectric layer on both sides of the initial first nanostructure are different, and the volume changes of the isolation structure 109 and the dielectric layer on both sides of the initial second nanostructure are also different, resulting in unbalanced stress on both sides of the initial first nanostructure and the initial second nanostructure, thereby causing the initial first nanostructure and the initial second nanostructure to bend and deform, affecting the performance of the semiconductor structure.

[0042] In another embodiment, the isolation structure is formed simultaneously with the first dielectric layer. The method for forming the first dielectric layer includes: forming a stacked material structure on a substrate, the stacked material structure including a bottom nanowire material layer, a bottom sacrificial material layer located on the bottom nanowire material layer, a plurality of sacrificial material layers located on the bottom sacrificial material layer, and a nanowire material layer located between the sacrificial material layers; forming a first mask layer on the stacked material structure, and forming an initial stacked structure using a self-aligned multiple patterning technique; then forming a dielectric layer on the sidewall of the initial stacked structure; forming a second mask layer on the dielectric layer and the initial stacked structure, the second mask layer exposing a portion of the surface of the initial stacked structure; etching the initial stacked structure using the second mask layer as a mask, forming a first opening in the initial stacked structure, the first opening exposing the bottom nanowire material layer, forming the initial first nanostructure and the initial second nanostructure; removing the first bottom sacrificial layer and the second bottom sacrificial layer exposed by the first opening, and forming a second opening between the first sacrificial layer and the first bottom nanowire and between the second sacrificial layer and the second bottom nanowire; then forming an isolation structure in the first opening, and forming a dielectric layer in the second opening.

[0043] Although the semiconductor structure solves the problem of uneven stress on both sides of the initial first nanostructure and the initial second nanostructure, in the process of forming the semiconductor structure, after forming the first mask layer, the self-aligned multiple patterning technology is used to form the initial stacking structure, and the second mask layer is formed on the initial stacking structure to form the first opening, the initial first nanostructure and the initial second nanostructure. The method needs to use two mask patterns, which makes the process flow more complicated and also causes a waste of production costs.

[0044] In order to solve the above problems, the technical solution of the present invention provides a semiconductor structure and a method for forming the semiconductor structure, wherein an initial bottom layer nanowire and an initial first nanostructure and an initial second nanostructure located on the initial bottom layer nanowire are formed on a substrate, wherein a first opening is provided between the initial first nanostructure and the initial second nanostructure, wherein the bottom plane of the first opening is higher than the substrate surface, and then an isolation structure is formed in the first opening, wherein the bottom plane of the isolation structure is higher than the substrate surface. In the semiconductor structure formed by the method, the bottom plane of the isolation structure is higher than the substrate surface, thereby reducing the height of the isolation structure, and reducing the volume of the isolation structure located between the first nanostructure and the second nanostructure. When the gate structure and the dielectric layer located on the sidewall of the gate structure are subsequently formed, the stress misalignment caused by the different thermal expansion coefficients between the isolation structure and the dielectric layer located on both sides of the first nanostructure and the second nanostructure is improved, thereby improving the bending deformation of the first nanostructure and the second nanostructure, and further improving the performance of the semiconductor structure.

[0045] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0046] Figures 3 to 8 It is a schematic cross-sectional structure diagram of the semiconductor structure forming process in an embodiment of the present invention.

[0047] Please refer to Figure 3 , providing a substrate 200.

[0048] In this embodiment, the material of the substrate 200 is silicon.

[0049] In other embodiments, the substrate material includes silicon carbide, silicon germanium, a multinary semiconductor material composed of group III-V elements, silicon on insulator (SOI) or germanium on insulator (GOI). Among them, the multinary semiconductor material composed of group III-V elements includes InP, GaAs, GaP, InAs, InSb, InGaAs or InGaAsP.

[0050] Please refer to Figure 4 An initial bottom layer nanowire 201 and an initial first nanostructure and an initial second nanostructure located on the initial bottom layer nanowire 201 are formed on a substrate 200 , wherein a first opening 208 is provided between the initial first nanostructure and the initial second nanostructure, and a bottom plane of the first opening 208 is higher than the surface of the substrate 200 .

[0051] The initial first nanostructure includes: a plurality of first sacrificial layers 203 and first nanowires 202 located between adjacent first sacrificial layers 203 ; and a first bottom sacrificial layer 204 located between the initial bottom nanowires 201 and the first sacrificial layers 203 .

[0052] The initial second nanostructure includes: a plurality of second sacrificial layers 206 and second nanowires 205 located between adjacent second sacrificial layers 206 ; and a second bottom sacrificial layer 207 located between the initial bottom nanowires 201 and the second sacrificial layers 206 .

[0053] The method for forming the initial underlying nanowire 201, the initial first nanostructure and the initial second nanostructure includes: forming an underlying nanowire material layer (not shown) on the substrate 200; forming a stacked material structure on the underlying nanowire material layer, the stacked material structure including an underlying sacrificial material layer (not shown), a plurality of sacrificial material layers (not shown) located on the underlying sacrificial material layer, and a nanowire material layer (not shown) located between adjacent sacrificial material layers; forming a mask structure (not shown) on the stacked material structure, the mask structure exposing a portion of the surface of the stacked material structure; using the mask structure as a mask, removing a portion of the stacked material structure and a portion of the underlying nanowire material layer, forming a first opening 208 in the stacked material structure and in the underlying nanowire material layer, and forming the initial first nanostructure and the initial second nanostructure.

[0054] The material of the sacrificial material layer includes silicon or first silicon germanium; the material of the nanowire material layer includes silicon or first silicon germanium; the material of the bottom sacrificial material layer includes silicon, first silicon germanium or second silicon germanium.

[0055] The first silicon germanium material and the second silicon germanium material are materials having different germanium contents in atomic percentage.

[0056] The materials of the sacrificial material layer, the nanowire material layer and the bottom sacrificial material layer are different from each other, so that when the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 are subsequently removed, the removal process causes less damage to the first nanowire 202, the second nanowire 205, the first sacrificial layer 203 and the second sacrificial layer 206; when the first sacrificial layer 203 and the second sacrificial layer 206 are removed, the first nanowire 202 and the second nanowire 205 are less damaged.

[0057] In this embodiment, the material of the sacrificial material layer includes first silicon germanium; the material of the nanowire material layer includes silicon; and the material of the bottom sacrificial material layer includes second silicon germanium.

[0058] In this embodiment, the atomic percentage of germanium in the first silicon germanium material is 25%; the atomic percentage of germanium in the second silicon germanium material is 75%, so that the second silicon germanium material has a larger etching selectivity ratio with the first silicon germanium material, and when the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 are subsequently removed, the removal process causes less damage to the first nanowire 202 and the second nanowire 205.

[0059] In this embodiment, the material of the initial bottom layer of nanowires 201 is the same as the material of the nanowire material layer.

[0060] In this embodiment, the process of forming the mask structure includes a self-aligned multi-patterning technology, so that the initial first nanostructure, the initial second nanostructure and the first opening 208 can be formed by one mask process, thereby saving production costs and improving production efficiency.

[0061] In other embodiments, the process of forming the mask structure can be other pattern forming techniques.

[0062] In this embodiment, the process of removing part of the stacked material structure and part of the underlying nanowire material layer includes a dry etching process, and the dry etching process can form an initial first nanostructure, an initial second nanostructure and a first opening 208 with good and straight sidewall morphology, so that the formed initial first nanostructure, the initial second nanostructure and the first opening 208 have good dimensional accuracy, which is beneficial to improving the uniformity of the device size.

[0063] In this embodiment, the thickness of the initial bottom layer nanowires 201 ranges from 0 nanometers to 150 nanometers.

[0064] The initial bottom nanowire 201 has the thickness range, and after a dielectric layer is subsequently formed between the bottom nanowire and the first sacrificial layer, between the bottom nanowire and the second sacrificial layer, and on the sidewalls of the bottom nanowire, a gate structure is formed on the dielectric layer. The thickness of the initial bottom nanowire 201 can ensure that the dielectric layer has sufficient thickness to electrically isolate the gate structure from the substrate 200, avoiding the situation where the gate structure is too close to the substrate 200 to generate a large parasitic capacitance, thereby improving the performance of the semiconductor structure.

[0065] The bottom plane of the first opening 208 is lower than the bottom plane of the first sacrificial layer 203 adjacent to the first bottom sacrificial layer 204; the bottom plane of the first opening 208 is lower than the bottom plane of the second sacrificial layer 206 adjacent to the second bottom sacrificial layer 207. Thus, when an isolation structure is subsequently formed in the first opening 208, the isolation structure can completely electrically isolate the first nanostructure from the second nanostructure.

[0066] In this embodiment, the bottom plane of the first opening 208 is lower than the top plane of the initial bottom nanowire 201. Therefore, when the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 are removed later, the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 can be removed completely.

[0067] In this embodiment, the height of the first opening 208 from the top of the initial bottom nanowire 201 ranges from 0 nanometers to 50 nanometers.

[0068] The height range allows the bottom plane of the isolation structure to be higher than the substrate surface after the isolation structure is subsequently formed in the first opening 208, while the bottom plane of the isolation structure can be slightly lower than the surface of the initial underlying nanowire 201, so that the isolation structure can have a smaller height while completely electrically isolating the first nanostructure and the second nanostructure formed subsequently.

[0069] In other embodiments, the bottom plane of the first opening is higher than the bottom plane of the first bottom sacrificial layer; the bottom plane of the first opening is higher than the bottom plane of the second bottom sacrificial layer. Thus, the isolation structure can have a smaller height while completely electrically isolating the first nanostructure and the second nanostructure formed subsequently.

[0070] Please refer to Figure 5 , an isolation structure 209 is formed in the first opening 208 , and a bottom plane of the isolation structure 209 is higher than the surface of the substrate 200 .

[0071] In this embodiment, the bottom plane of the isolation structure 209 is lower than the top plane of the initial bottom nanowire 201. The bottom plane of the isolation structure 209 is higher than the surface of the substrate 200, and the bottom plane of the isolation structure 209 is slightly lower than the surface of the initial bottom nanowire 201, so that the isolation structure 209 can have a smaller height under the condition of completely electrically isolating the first nanostructure and the second nanostructure formed subsequently, so that the height of the isolation structure 209 is reduced, and the volume of the isolation structure 209 located between the first nanostructure and the second nanostructure is reduced. When the gate structure and the dielectric layer located on the sidewall of the gate structure are subsequently formed, the stress imbalance caused by the different thermal expansion coefficients between the isolation structure and the dielectric layer located on both sides of the first nanostructure and the second nanostructure is improved, thereby improving the bending deformation of the first nanostructure and the second nanostructure, thereby improving the performance of the semiconductor structure.

[0072] The height of the bottom plane of the isolation structure 209 below the top plane of the bottom nanowire 201 is in the range of 0 nanometers to 50 nanometers.

[0073] The method for forming an isolation structure 209 in the first opening 208 includes: forming an isolation material layer (not shown) in the first opening 208 and on the surfaces of the initial first nanostructure and the initial second nanostructure; removing the isolation material layer on the surfaces of the initial first nanostructure and the initial second nanostructure to form an isolation structure 209 in the first opening 208.

[0074] The process of forming the isolation material layer includes an atomic layer deposition process or a chemical vapor deposition process.

[0075] The process of removing the isolation material layer on the surface of the initial first nanostructure and the initial second nanostructure includes a wet etching process or an isotropic dry etching process.

[0076] The material of the isolation structure 209 includes a dielectric material, and the dielectric material includes a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. In this embodiment, the material of the isolation structure 209 includes silicon nitride.

[0077] In other embodiments, the bottom plane of the isolation structure is higher than the bottom plane of the first bottom sacrificial layer; the bottom plane of the isolation structure is higher than the bottom plane of the second bottom sacrificial layer.

[0078] Please refer to Figure 6 After forming the isolation structure 209 , the initial bottom layer nanowire 201 is etched using the initial first nanostructure, the initial second nanostructure and the isolation structure 209 as masks until the surface of the substrate 200 is exposed to form a bottom layer nanowire 210 .

[0079] In this embodiment, the process of etching the initial bottom nanowire 201 includes a dry etching process, and the dry etching process can form a bottom nanowire 210 with good sidewall morphology and high dimensional accuracy.

[0080] Please refer to Figure 7 After forming the bottom nanowire 210, the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 are removed, a second opening (not shown) is formed between the bottom nanowire 210 and the first sacrificial layer 203, and a third opening (not shown) is formed between the bottom nanowire 210 and the second sacrificial layer 206, wherein the second opening and the third opening expose a portion of the side wall surface of the isolation structure 209.

[0081] The process of removing the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 includes a wet etching process, a dry etching process or a reactive cyclic etching process (Certas).

[0082] The wet etching process, dry etching process or reactive cycle etching process has a large etching selectivity for the first nanowire 202, the second nanowire 205, the first sacrificial layer 203 and the second sacrificial layer 206, so that the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 can be removed cleanly while causing less damage to the first nanowire 202, the second nanowire 205, the first sacrificial layer 203 and the second sacrificial layer 206.

[0083] In this embodiment, the process of removing the first bottom sacrificial layer 204 and the second bottom sacrificial layer 207 includes a dry etching process, and the etching gas of the dry etching process includes a mixed gas of fluorine-containing gas, oxygen, argon and helium.

[0084] In other embodiments, the first bottom sacrificial layer and the second bottom sacrificial layer can be removed first, and then the initial bottom nanowires are etched using the initial first nanostructure, the initial second nanostructure and the isolation structure as masks to form the bottom nanowires.

[0085] Please continue to refer to Figure 7 A dielectric layer 211 is formed in the second opening and the third opening, and the dielectric layer 211 is also located on the sidewalls of the bottom nanowire 210 .

[0086] The method for forming the dielectric layer 211 includes: forming a dielectric material layer (not shown) in the second opening, in the third opening, on the substrate 200, on the initial first nanostructure, on the initial second nanostructure and on the isolation structure, wherein the dielectric material layer fills the second opening and the third opening; flattening the dielectric material layer until the top surface of the initial first nanostructure and the top surface of the initial second nanostructure are exposed to form an initial dielectric layer (not shown); and etching back the initial dielectric layer until the side wall surface of the first sacrificial layer 203 and the side wall surface of the second sacrificial layer 206 are exposed to form the dielectric layer 211.

[0087] The material of the dielectric layer 211 and the material of the isolation structure 209 have different etching selectivities, so that when the initial dielectric layer is etched back, the etching process causes less damage to the isolation structure 209 .

[0088] The material of the dielectric layer 211 includes a dielectric material, and the dielectric material includes one or more combinations of dielectric materials such as silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbide, silicon carbide nitride, and silicon oxycarbon nitride. The process of forming the dielectric material layer includes a chemical vapor deposition process, an atomic layer deposition process, or a thermal treatment process.

[0089] In this embodiment, the material of the dielectric layer 211 includes silicon oxide; the process of forming the dielectric material layer includes an atomic layer deposition process, and the atomic layer deposition process is easy to form a dielectric layer 211 with a dense structure in the second opening and the third opening.

[0090] Please refer to Figure 8After forming the dielectric layer 211, a dummy gate structure (not shown) is formed on the dielectric layer 211, and the dummy gate structure spans the isolation structure 209, the initial first nanostructure and the initial second nanostructure; after forming the dummy gate structure, a dielectric layer (not shown) is formed on the substrate 200, and the dielectric layer is located on the sidewall of the dummy gate structure; the dummy gate structure is removed to form an initial gate opening (not shown) in the dielectric layer; the first sacrificial layer 203 and the second sacrificial layer 206 exposed by the initial gate opening are removed, a gate opening (not shown) is formed in the dielectric layer, and the first nanostructure and the second nanostructure are formed; a gate structure 213 is formed in the gate opening.

[0091] The material of the dielectric layer includes a dielectric material, and the dielectric material includes one or more combinations of dielectric materials such as silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. In this embodiment, the material of the dielectric layer includes silicon oxide.

[0092] The gate structure 213 includes: a gate dielectric layer (not shown) and a gate layer (not shown) located on the gate dielectric layer. In this embodiment, the gate structure 213 further includes a work function layer (not shown), and the work function layer is located between the gate dielectric layer and the gate layer.

[0093] The material of the gate dielectric layer includes a high dielectric constant material, the dielectric constant of the high dielectric constant material is greater than 3.9, and the high dielectric constant material includes aluminum oxide or hafnium oxide; the material of the gate layer includes a metal, and the metal includes tungsten; the material of the work function layer includes an N-type work function material or a P-type work function material, the N-type work function material includes titanium aluminum, and the P-type work function material includes titanium nitride or tantalum nitride.

[0094] Accordingly, the embodiment of the present invention further provides a semiconductor structure, please continue to refer to Figure 8 ,include:

[0095] Substrate 200;

[0096] bottom layer of nanowires 210 located on substrate 200;

[0097] A first nanostructure and a second nanostructure located on the bottom nanowire 201, wherein a first opening (not shown) is provided between the first nanostructure and the second nanostructure, and a bottom plane of the first opening is higher than the surface of the substrate 200;

[0098] an isolation structure 209 located in the first opening;

[0099] A gate structure 213 is located on the substrate 200 , and the gate structure 213 spans the isolation structure 209 , the first nanostructure, and the second nanostructure.

[0100] In this embodiment, the first nanostructure includes: a plurality of first nanowires 202 separated from each other along a direction perpendicular to the surface of the substrate 200, with a first groove (not shown) between adjacent first nanowires 202; the second nanostructure includes: a plurality of second nanowires 205 separated from each other along a direction perpendicular to the surface of the substrate 200, with a second groove (not shown) between adjacent second nanowires 205; the gate structure 213 is also located in the first groove and the second groove.

[0101] In this embodiment, the structure further includes: a dielectric layer 211 located between the bottom nanowire 210 and the gate structure 213 , and the dielectric layer 211 is also located on the sidewall of the bottom nanowire 210 .

[0102] In this embodiment, a bottom plane of the isolation structure 209 is lower than a bottom plane of the gate structure 213 .

[0103] In this embodiment, the bottom plane of the isolation structure 209 is lower than the top plane of the bottom nanowire 210 .

[0104] In this embodiment, the height of the bottom plane of the isolation structure 209 below the top plane of the bottom nanowire 210 is in the range of 0 nanometers to 50 nanometers.

[0105] In other embodiments, a bottom plane of the isolation structure is higher than a bottom plane of the dielectric layer.

[0106] In this embodiment, it further includes: a dielectric layer (not shown) located on the substrate 200 , and the dielectric layer is located on the sidewall of the gate structure 213 .

[0107] In this embodiment, the etching selectivity ratios of the material of the isolation structure 209 and the material of the dielectric layer 211 are different.

[0108] In this embodiment, the material of the isolation structure 209 includes a dielectric material, and the dielectric material includes one or more combinations of dielectric materials such as silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon carbon nitride oxynitride.

[0109] In this embodiment, the thickness of the bottom layer nanowires 210 ranges from 0 nanometers to 150 nanometers.

[0110] In the semiconductor structure, the bottom plane of the isolation structure 209 is higher than the surface of the substrate 200, so that the height of the isolation structure 209 is reduced, and the volume of the isolation structure 209 located between the first nanostructure and the second nanostructure is reduced. Therefore, when the gate structure 213 and the dielectric layer located on the side wall of the gate structure 213 continue to be formed, the stress imbalance caused by the different thermal expansion coefficients between the isolation structure 209 and the dielectric layer located on both sides of the first nanostructure and the second nanostructure is improved, thereby improving the bending deformation of the first nanostructure and the second nanostructure, thereby improving the performance of the semiconductor structure.

[0111] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A semiconductor structure, It is characterized in that include: substrate; a bottom layer of nanowires located on a substrate; A first nanostructure and a second nanostructure are located on the bottom nanowire, wherein a first opening is provided between the first nanostructure and the second nanostructure, and a bottom plane of the first opening is higher than a surface of the substrate; an isolation structure located within the first opening; a gate structure located on the substrate, the gate structure spanning the isolation structure, the first nanostructure and the second nanostructure; A dielectric layer is located between the bottom nanowire and the gate structure, and the dielectric layer is also located on the sidewall of the bottom nanowire.

2. The semiconductor structure according to claim 1, It is characterized in that The first nanostructure includes: a plurality of first nanowires separated from each other along a direction perpendicular to the substrate surface, with a first groove between adjacent first nanowires; the second nanostructure includes: a plurality of second nanowires separated from each other along a direction perpendicular to the substrate surface, with a second groove between adjacent second nanowires; the gate structure is also located in the first groove and the second groove.

3. The semiconductor structure according to claim 1, It is characterized in that A bottom plane of the isolation structure is lower than a bottom plane of the gate structure.

4. The semiconductor structure according to claim 1, It is characterized in that The bottom plane of the isolation structure is lower than the top plane of the bottom nanowires.

5. The semiconductor structure according to claim 4, It is characterized in that The height of the bottom plane of the isolation structure below the top plane of the bottom nanowires ranges from 0 nanometers to 50 nanometers.

6. The semiconductor structure according to claim 1, It is characterized in that A bottom plane of the isolation structure is higher than a bottom plane of the dielectric layer.

7. The semiconductor structure according to claim 1, It is characterized in that The material of the isolation structure and the material of the dielectric layer have different etching selectivities when etching back the dielectric layer material.

8. The semiconductor structure according to claim 1, It is characterized in that The thickness of the bottom nanowires ranges from 0 nanometers to 150 nanometers.

9. A method for forming a semiconductor structure, It is characterized in that include: providing a substrate; Forming an initial bottom layer nanowire and an initial first nanostructure and an initial second nanostructure on the initial bottom layer nanowire on a substrate, wherein a first opening is provided between the initial first nanostructure and the initial second nanostructure, and a bottom plane of the first opening is higher than a surface of the substrate; forming an isolation structure in the first opening; After the isolation structure is formed, the initial bottom layer nanowires are etched using the initial first nanostructure, the initial second nanostructure and the isolation structure as masks until the substrate surface is exposed, thereby forming bottom layer nanowires.

10. The method for forming a semiconductor structure according to claim 9, It is characterized in that The process of etching the initial bottom layer nanowires includes a dry etching process.

11. The method for forming a semiconductor structure according to claim 9, It is characterized in that The initial first nanostructure comprises: a plurality of first sacrificial layers and first nanowires located between adjacent first sacrificial layers; a first bottom sacrificial layer located between the initial bottom nanowires and the first sacrificial layer; the initial second nanostructure comprises: a plurality of second sacrificial layers and second nanowires located between adjacent second sacrificial layers; A second bottom sacrificial layer is positioned between the initial bottom nanowires and the second sacrificial layer.

12. The method for forming a semiconductor structure according to claim 11, It is characterized in that The method for forming the initial underlying nanowires, the initial first nanostructure and the initial second nanostructure includes: forming an underlying nanowire material layer on a substrate; forming a stacked material structure on the underlying nanowire material layer, the stacked material structure including an underlying sacrificial material layer, a plurality of sacrificial material layers located on the underlying sacrificial material layer, and a nanowire material layer located between adjacent sacrificial material layers; forming a mask structure on the stacked material structure, the mask structure exposing a portion of the surface of the stacked material structure; using the mask structure as a mask, removing a portion of the stacked material structure and a portion of the underlying nanowire material layer, forming a first opening in the stacked material structure and the underlying nanowire material layer, and forming the initial first nanostructure and the initial second nanostructure.

13. The method for forming a semiconductor structure according to claim 12, It is characterized in that The bottom plane of the isolation structure is lower than the bottom plane of the first sacrificial layer adjacent to the first bottom sacrificial layer; the bottom plane of the isolation structure is lower than the bottom plane of the second sacrificial layer adjacent to the second bottom sacrificial layer.

14. The method for forming a semiconductor structure according to claim 13, It is characterized in that The bottom plane of the isolation structure is lower than the top plane of the initial bottom layer of nanowires.

15. The method for forming a semiconductor structure according to claim 14, It is characterized in that The height of the bottom plane of the isolation structure below the top plane of the bottom nanowires ranges from 0 nanometers to 50 nanometers.

16. The method for forming a semiconductor structure according to claim 13, It is characterized in that The bottom plane of the isolation structure is higher than the bottom plane of the first bottom sacrificial layer; the bottom plane of the isolation structure is higher than the bottom plane of the second bottom sacrificial layer.

17. The method for forming a semiconductor structure according to claim 12, It is characterized in that The process of forming the mask structure includes a self-aligned multi-patterning technique.

18. The method for forming a semiconductor structure according to claim 12, It is characterized in that The process of removing part of the stacked material structure and part of the underlying nanowire material layer includes a dry etching process.

19. The method for forming a semiconductor structure according to claim 11, It is characterized in that After forming the bottom nanowire, it also includes: removing the first bottom sacrificial layer and the second bottom sacrificial layer, forming a second opening between the bottom nanowire and the first sacrificial layer, forming a third opening between the bottom nanowire and the second sacrificial layer, the second opening and the third opening exposing part of the side wall surface of the isolation structure; forming a dielectric layer in the second opening and the third opening, the dielectric layer is also located on the side wall of the bottom nanowire.

20. The method for forming a semiconductor structure according to claim 19, It is characterized in that After forming the dielectric layer, it also includes: forming a dummy gate structure on the dielectric layer, the dummy gate structure spanning the isolation structure, the initial first nanostructure and the initial second nanostructure; after forming the dummy gate structure, forming a dielectric layer on the substrate, the dielectric layer being located on the sidewall of the dummy gate structure; removing the dummy gate structure to form an initial gate opening in the dielectric layer; removing the first sacrificial layer and the second sacrificial layer exposed by the initial gate opening, forming a gate opening in the dielectric layer, and forming the first nanostructure and the second nanostructure; forming a gate structure in the gate opening.

21. The method for forming a semiconductor structure according to claim 9, It is characterized in that The method for forming an isolation structure in a first opening includes: forming an isolation material layer in the first opening and on the surfaces of an initial first nanostructure and an initial second nanostructure; removing the isolation material layer on the surfaces of the initial first nanostructure and the initial second nanostructure to form an isolation structure in the first opening.

22. The method for forming a semiconductor structure according to claim 21, It is characterized in that The process of forming the isolation material layer includes an atomic layer deposition process.

23. The method for forming a semiconductor structure according to claim 21, It is characterized in that The process of removing the isolation material layer on the surface of the initial first nanostructure and the initial second nanostructure includes a wet etching process.