Semiconductor structure and method for manufacturing the same

By injecting doping ions into the corner areas of the semiconductor structure to slow down the oxidation rate, and forming trenches and isolation structures during the removal process, the problem of excessively fast oxidation rates in the corner areas of the semiconductor structure is solved, ensuring structural integrity and electrical performance. .

CN114068411BActive Publication Date: 2024-10-01CHANGXIN MEMORY TECH INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010784644.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-06
Publication Date
2024-10-01
Estimated Expiration
2040-08-06

AI Technical Summary

Technical Problem

In the process of manufacturing semiconductor structures, the consumption of film layer materials leads to performance defects such as leakage. Especially during the etching and cleaning of the underlying substrate in the array area and peripheral area, the substrate material is partially consumed, resulting in oxidation in the corner areas. If the speed is too fast, a large chamfer will be formed, which will affect the structural integrity.

Method used

By injecting doping ions, especially nitrogen ions, into the corner areas of the semiconductor structure, the oxidation rate is slowed down, and trenches and isolation structures are formed during the removal process to inhibit oxidation and etching and ensure the integrity of the sidewalls of the corner areas.

Benefits of technology

It effectively slows down the oxidation rate in the corner area, avoids the rapid formation of the oxide layer and the expansion of the chamfer, ensures the structural integrity and electrical performance of the active area, and reduces substrate consumption and performance defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114068411B_ABST
    Figure CN114068411B_ABST
Patent Text Reader

Abstract

The embodiment of the present invention provides a semiconductor structure and a method for manufacturing the same. The method for manufacturing the semiconductor structure includes: providing a substrate, the substrate including an active region and an isolation region located between adjacent active regions, the active region including a corner region adjacent to the isolation region; performing a doping process to inject doping ions into the corner region, the doping ions are used to slow down the oxidation rate of the corner region; after performing the doping process, performing a removal process on the substrate, the removal process can remove the oxidized substrate, and during the removal process, the structure in the isolation region exposes the sidewall of the corner region. The present invention is conducive to maintaining the structural integrity of the corner region of the active region.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to the field of semiconductors, and in particular to a semiconductor structure and a method for manufacturing the same. Background Art

[0002] As the size of semiconductor structures shrinks, the extra consumption of film materials during the manufacturing process of semiconductor structures may lead to major performance defects.

[0003] Specifically, a semiconductor structure usually includes an array area and a peripheral area surrounding the array area. When the underlying substrate of the array area and the peripheral area is subjected to processes such as etching and cleaning, the underlying substrate will be partially consumed or even cause the film layer to fall off. The consumption of substrate material will cause performance defects of the substrate, such as leakage. Summary of the invention

[0004] The embodiment of the present invention provides a semiconductor structure and a method for forming the same, which are beneficial to maintaining the integrity of the corner area of ​​the active region.

[0005] To solve the above problems, an embodiment of the present invention provides a method for manufacturing a semiconductor structure, comprising: providing a substrate, the substrate comprising an active area and an isolation area located between adjacent active areas, the active area comprising a corner area adjacent to the isolation area; performing a doping process to inject doping ions into the corner area, the doping ions are used to slow down the oxidation rate of the corner area; after performing the doping process, performing a removal process on the substrate, the removal process can remove the oxidized substrate, and during the removal process, the structure in the isolation area exposes the side wall of the corner area.

[0006] In addition, the removing process of the substrate includes: performing an etching process on the substrate of the isolation region to form a groove exposing the side wall of the corner region, wherein the groove is used to form an isolation structure.

[0007] In addition, the removal process further includes: after the etching process, performing a first cleaning process on the trench, wherein a cleaning liquid of the first cleaning process contacts the sidewall of the corner region.

[0008] In addition, the isolation area has an isolation structure, the isolation structure has a recessed portion, and the recessed portion exposes the side wall of the corner area; the removal process includes: after the doping process, performing a second cleaning process on the top surface of the active area, and the cleaning liquid of the second cleaning process is in contact with the side wall of the corner area.

[0009] In addition, after the second cleaning process is performed, a deposition process is performed on the active area to form a gate oxide layer covering the top surface of the active area, and the gate oxide layer and the isolation structure expose the side wall of the corner area.

[0010] In addition, the doping ions include nitrogen ions, and the implantation dose of the doping ions is 1e12-1e16 atoms / cm 2 .

[0011] In addition, the process steps for injecting the doped ions include: providing the substrate and a shielding layer located on the substrate, the active area also includes an intermediate area located between adjacent corner areas, the shielding layer covers the top surface of the intermediate area, and the shielding layer is used to shield the injection of the doped ions; performing an ion implantation process on the substrate.

[0012] In addition, the implantation energy range of the ion implantation process is 1 KV to 60 KV.

[0013] In addition, the shielding layer also covers the corner area and exposes the isolation area; and the substrate is subjected to the ion implantation process with an implantation angle.

[0014] In addition, the implantation angle is 5° to 60°. Accordingly, an embodiment of the present invention further provides a semiconductor structure, comprising: a substrate, the substrate comprising an active region and an isolation region located between adjacent active regions, the active region comprising a corner region adjacent to the isolation region, the structure in the isolation region exposing the sidewall of the corner region; the corner region contains doping ions, the doping ions are used to slow down the oxidation rate of the corner region.

[0015] In addition, an isolation structure is provided in the isolation region, the isolation structure has a recessed portion, and the recessed portion exposes the side wall of the corner region.

[0016] In addition, the semiconductor structure further comprises: a gate dielectric layer and an isolation portion, wherein the gate dielectric layer covers the top surface of the active region, and the isolation portion covers the sidewall of the corner region.

[0017] Compared with the prior art, the technical solution provided by the embodiment of the present invention has the following advantages:

[0018] In the above technical solution, the method of injecting doped ions into the corner area is used to slow down the oxidation rate of the corner area, avoid the formation of a thicker oxide layer, and avoid the removal process removing the oxide layer at a faster rate and gradually forming a larger chamfer, thereby ensuring that the corner area of ​​the active area has good structural integrity, and thus ensuring that the active area and the semiconductor structure containing the active area, such as a field effect transistor, have good electrical properties.

[0019] In addition, forming the grooves after the doping process is performed is beneficial to suppressing oxidation of the substrate during the etching process, avoiding etching of a thicker oxide layer by the etching process, and ensuring that the chamfer formed by the etching process is small. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] One or more embodiments are exemplarily described by pictures in the corresponding drawings, and these exemplifications do not constitute limitations on the embodiments. Unless otherwise stated, the pictures in the drawings do not constitute proportional limitations.

[0021] Figures 1 to 5 It is a schematic diagram of the cross-sectional structure corresponding to each step of the method for forming a semiconductor structure;

[0022] Figures 6 to 15 A schematic cross-sectional structure diagram corresponding to each step of the method for forming a semiconductor structure provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0023] refer to Figure 1 A substrate 100 is provided. The substrate 100 includes an active region 101 and an isolation region 102 located between adjacent active regions 101 . The active region 101 includes a corner region adjacent to the isolation region 102 .

[0024] The material of the substrate 100 includes polysilicon. The subsequent removal process for the substrate 100 is mostly performed in an atmospheric environment, and the polysilicon will undergo natural oxidation in an atmospheric environment.

[0025] It should be noted that the dividing line used to divide the active area 101 and the isolation area 102 in the figure is only used for illustration. In fact, the dividing line is not necessarily perpendicular to the surface of the substrate 100, and the dividing line may also have a certain inclination angle, which may be equal to the inclination angle of the groove sidewall formed by subsequent etching.

[0026] refer to Figure 2 , an etching process is performed on the isolation region 102 to form a trench 120, and the trench 120 is used to form an isolation structure.

[0027] During the process of etching to form the trench 120 , the corner area sidewalls of the active area 101 will be exposed, and the exposed corner area sidewalls will be oxidized. The oxide layer formed after oxidation is easier to be removed by the etching process than the substrate 100 material.

[0028] Since the etching process for forming the groove 120 is a continuous process, and the etchant of the etching process will contact the exposed sidewalls of the corner area, the oxide formed by natural oxidation at the sidewalls of the corner area will be etched away in a relatively short time. This causes the substrate 100 at the sidewalls of the corner area to always be exposed to the atmosphere, and the oxide layer formed by oxidation cannot effectively isolate the oxygen in the air. In this way, the sidewalls of the corner area of ​​the substrate 100 will always oxidize at a relatively fast oxidation rate, that is, the oxidation rate when the substrate 100 is in direct contact with the air, thereby causing the substrate 100 to be consumed at a relatively fast rate, and finally forming a relatively large chamfer 103.

[0029] The chamfer 103 has a first width d1 in a direction parallel to the surface of the substrate 100 and a first thickness d2 in a direction perpendicular to the surface of the substrate 100. There is no necessary relationship between the first width d1 and the first thickness d2. The sizes of the first width d1 and the first thickness d2 are related to the etching time of the groove 120 and the oxidation rate of the substrate 100 when it is in direct contact with the air. Specifically, the faster the oxidation rate of the substrate 100 when it is in direct contact with the air, the larger the first width d1 and the first thickness d2.

[0030] refer to Figure 3 After the trench 120 is formed, a first cleaning process is performed on the bottom surface and sidewalls of the trench 120 , and the first cleaning process is used to remove residual etchant and debris of the substrate 100 .

[0031] The cleaning agent of the first cleaning process will contact the substrate 100 at the chamfer 103 and remove the oxide layer formed by natural oxidation, thereby causing further consumption of the substrate 100. Specifically, the first width d1 and the first thickness d2 of the chamfer 103 will be further increased, forming a chamfer 103 with a larger size.

[0032] refer to Figure 4 After the first cleaning process, in the trench 120 (reference Figure 3 ) to form an isolation structure 12.

[0033] The isolation structure 12 generally includes a first isolation layer 121 covering the bottom and side walls of the trench 120, a second isolation layer 122 covering the bottom and side walls of the first isolation layer 121, and a third isolation layer 123 filling the trench 120. The material of the first isolation layer 121 and the third isolation layer 123 is generally silicon oxide, and the material of the second isolation layer 122 is generally silicon nitride, i.e., the commonly used "ONO" isolation structure.

[0034] Since silicon nitride has a high hardness, when etching silicon nitride and silicon oxide, due to the etching selectivity, the first isolation layer 121 is usually over-etched and cannot completely cover the surface of the chamfer 103, that is, the isolation structure 12 will have a recessed portion 124 located at the top of the first isolation layer 121, and the recessed portion 124 will expose at least part of the sidewall of the corner area. In this way, the size of the chamfer 103 will be further enlarged in other subsequent removal processes.

[0035] refer to Figure 5 After the isolation structure 12 is formed, a second cleaning process is performed on the top surface of the active region 101 . The second cleaning process is used to remove impurities on the top surface of the active region 101 .

[0036] The second cleaning process is a pre-step for depositing a gate dielectric layer on the top surface of the active area 101. During the second cleaning process, the cleaning agent will contact the exposed sidewalls of the corner area and etch away the oxide on the sidewalls of the corner area, further enlarging the size of the chamfer 103, thereby making the integrity of the corner area of ​​the active area 101 poor.

[0037] In order to solve the above problems, the present invention provides a semiconductor structure and a manufacturing method thereof, by injecting doped ions into the corner area of ​​the active area, the oxidation rate of the corner area is slowed down, so that the oxide film layer is thinner when the solvent such as the etchant or the cleaning agent of the removal process contacts the side wall of the corner area; since the size of the chamfer is positively correlated with the thickness of the oxide film layer, by inhibiting the oxidation of the corner area, the size of the chamfer can be effectively reduced, which is beneficial to ensure that the corner area of ​​the active area has better structural integrity.

[0038] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the embodiments of the present invention will be described in detail below with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present invention, many technical details are provided to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can be implemented.

[0039] Figures 6 to 14 A schematic cross-sectional structure diagram corresponding to each step of the method for forming a semiconductor structure provided by an embodiment of the present invention.

[0040] refer to Figure 6 , providing a substrate 200 and a mask layer 220 and a shielding film 211 sequentially stacked on the substrate 200 .

[0041] In this embodiment, the substrate 200 includes an active region 201 and an isolation region 202 located between adjacent active regions 201; in a direction perpendicular to the surface of the substrate 200, the orthographic projection of the top surface of the active region 201 coincides with the orthographic projection of the mask layer 220. In this way, the mask layer 220 can be directly used for subsequent trench etching, without the need to form different mask layers for subsequent doping of dopant ions and trench etching, which is beneficial to reducing process steps and shortening the exposure time of the top surface of the substrate 200, thereby reducing the consumption of the substrate 200.

[0042] In this embodiment, the mask layer 220 is a hard mask layer, and the material of the mask layer 220 includes polysilicon; the shielding film 211 is used to form a shielding layer, and the shielding layer plays a role in shielding ion implantation, and the material of the shielding film 211 includes silicon oxide.

[0043] The substrate 200 can be generally divided into an array region and a peripheral region surrounding the array region. In this embodiment, the region where the substrate 200 is located is taken as an example as the peripheral region. The mask layer 220 can be formed together with the polysilicon layer in the array region.

[0044] refer to Figure 7 , the shielding film 211 is etched to form the shielding layer 210 , and the mask layer 220 is removed.

[0045] In this embodiment, the active region 201 includes a corner region 212 adjacent to the isolation region 202 , and the shielding layer 210 covers the top surface of the corner region 212 ; in other embodiments, the shielding layer exposes the top surface of the corner region.

[0046] refer to Figure 8 , and carry out the doping process.

[0047] In this embodiment, ion implantation is performed on the corner region 212 and the top of the isolation region 202 using an ion implantation process with an implantation angle; in other embodiments, ion implantation is performed only on the corner region.

[0048] The type of doping ions is related to the cause of oxidation of the sidewalls of the corner region 212. Specifically, the sidewalls of the corner region 212 may be naturally oxidized, that is, oxidized by oxygen contained in the air in the atmospheric environment, or oxidized by oxidizing components in solvents such as etchants or cleaning agents. Since the oxidizing components in different solvents may be different, the type of doping ions can be adjusted according to the type of solvent used in the subsequent process steps and the length of time the substrate 200 is exposed to the atmospheric environment; in addition, multiple doping ions can be doped simultaneously in the corner region 212 to slow down the oxidation rate of the corner region 212 in different oxidation environments.

[0049] In this embodiment, the doping ions include nitrogen ions, and the implantation dose of the doping ions is 1e12-1e16 atoms / cm 2, for example, 1e13 atoms / cm 2 、1e14atoms / cm 2 or 1e15 atoms / cm 2 If the implantation dose of the doping ions is too small, the effect of slowing down the oxidation rate is not obvious, and a large chamfer will still be formed later; if the implantation dose of the doping ions is too large, the effect of slowing down the oxidation rate is not obvious, and the corner area 212 may be damaged, which is not conducive to the subsequent doping of P-type or N-type doping ions to form a doping area.

[0050] In this embodiment, the implantation energy of the ion implantation process ranges from 1KV to 60KV, such as 20KV, 30KV or 40KV. If the implantation energy is too low, the implantation depth of the doped ions is shallow, which can reduce the consumption of the corner area; if the implantation energy is too high, the substrate 200 may be damaged due to the excessive depth of the implantation range.

[0051] In this embodiment, the implantation angle is 5° to 60°, for example, 20°, 30° or 40°. If the implantation angle is too small, it is easy to cause poor doping effect in the top area of ​​the corner area 212; if the implantation angle is too large, a large implantation energy is required to implant the doping ions to the preset depth, and it is easy to cause unnecessary doping in the middle area between adjacent corner areas 212, which may affect the performance of the semiconductor structure formed subsequently.

[0052] In this embodiment, after the doping process, the substrate 200 is subjected to a removal process, and the removal process can remove the oxidized substrate 200. During the removal process, the structure in the isolation region 202 exposes the sidewall of the corner region 212. The removal process includes an etching process and a cleaning process.

[0053] Specifically, the removal process performed after the doping process may include the following process steps:

[0054] refer to Fig. 9 , for the isolation area 202 (reference Figure 8 ) is subjected to an etching process to form a trench 230 exposing the sidewall of the corner region 212, and the trench 230 is used to form an isolation structure.

[0055] In this embodiment, since the corner region 212 is doped with doped ions, the natural oxidation rate of the side wall of the corner region 212 when exposed and the oxidation rate by the oxidizing components in the etchant are slow. During the entire etching process, the total thickness of the oxide film layer that can be etched and removed by the etchant is thin.

[0056] This helps to avoid film peeling due to excessive consumption of sidewall material in the corner area 212, and to avoid the chamfer 203 being too large due to film peeling or other reasons, that is, to ensure that the second width d3 and the second thickness d4 of the chamfer 203 are small, so that the corner area 212 has better structural integrity, thereby avoiding the risk of leakage caused by structural defects.

[0057] refer to Fig.10 After the etching process, the trench 230 is subjected to a first cleaning process, and the cleaning liquid of the first cleaning process contacts the sidewall of the corner region 212 .

[0058] In this embodiment, since the corner region 212 is doped with doping ions that slow down the doping rate, the doping ions can inhibit the natural oxidation of the substrate 200 from the etching process to the first cleaning process, and inhibit the oxidizing components in the cleaning solution from oxidizing the substrate 200, thereby ensuring that the total thickness of the oxide film layer that can be removed by the first cleaning process is relatively thin. In this way, it is beneficial to inhibit the further consumption of the material of the corner region 212 by the first cleaning process, and ensure that the corner region 212 has good structural integrity.

[0059] refer to Fig.11 , forming an isolation structure 240.

[0060] In this embodiment, the isolation structure 240 is a three-layer stacked structure of silicon oxide layer-silicon nitride layer-silicon oxide layer, and the isolation structure 240 has a recessed portion 241, and the recessed portion 241 exposes the side wall of the corner region 212; in other embodiments, the isolation structure can also be a double-layer stacked structure including a silicon oxide layer and a silicon nitride layer. This article does not limit the structure and material of the isolation structure 240, but only emphasizes that the isolation structure 240 has certain defects, including the presence of a recessed portion 241 that exposes the side wall of the corner region 212.

[0061] It should be noted that, if ion doping is performed on the corner region 212 after the isolation structure 240 is formed to suppress the formation of the chamfer 203 or reduce the size of the chamfer 203, the thickness of the corner region 212 in the direction perpendicular to the surface of the substrate 200 may be only equal to the thickness of the recess 241. In this way, it is beneficial to reduce the number of doping ions to be implanted and shorten the range of ion implantation, so that the ion implantation process causes less damage to the corner region 212, and ensures that the active region 201 has good electrical properties.

[0062] refer to Fig.12 , a second cleaning process is performed on the top surface of the active area 201 , and the cleaning liquid of the second cleaning process contacts the side wall of the corner area 212 .

[0063] In this embodiment, the doped ions can also inhibit the natural oxidation from forming the isolation structure 240 to performing the second cleaning process, as well as inhibiting the natural oxidation of the side walls of the corner area 212 and the oxidation of the cleaning agent during the second cleaning process, further ensuring the structural integrity of the corner area 212.

[0064] refer to Fig.13 , a deposition process is performed on the top surface of the active area 201 to form a gate dielectric layer 250 .

[0065] In this embodiment, the gate dielectric layer 250 only covers the top surface of the active region 201. Since the gate dielectric layer 250 is usually formed by first forming a whole layer of gate dielectric film on the substrate 200 and then patterning and etching the gate dielectric film, when the gate dielectric layer 250 does not cover the side wall of the corner region 212, the etching process will remove the oxide film layer on the side wall of the corner region 212.

[0066] Since the corner region 212 is doped with doping ions that slow down the doping rate, the doping ions can inhibit the natural oxidation of the substrate 200 during the etching process, and inhibit the oxidizing components in the etchant from oxidizing the substrate 200, thereby ensuring that the total thickness of the oxide film layer that can be removed by the etching process is relatively thin. This is conducive to inhibiting the further consumption of the material of the corner region 212 by the etching process, and ensuring that the corner region 212 has good structural integrity.

[0067] In other embodiments, reference Fig.14 The gate dielectric layer 350 also covers the sidewalls of the corner region 212, that is, covers the surface of the chamfer 303. The gate dielectric layer 350 can isolate the corner region 312, which is beneficial to avoid further oxidation of the corner region 312 and avoid further consumption of the material of the corner region 312.

[0068] refer to Fig.15 , forming an isolation portion 260 and a gate 270 .

[0069] In the present embodiment, since the side walls of the corner region 212 are exposed, in order to avoid problems such as the subsequently formed gate 270 contacting the side walls of the corner region 212, an additional isolation portion 260 needs to be formed. The isolation portion 260 covers the side walls of the corner region 212 and serves the purpose of isolating the corner region 212 and the gate 270, which is beneficial to ensure that the transistor composed of the gate 270, the gate dielectric layer 250 and the active area 201 has good electrical properties.

[0070] The material of the isolation portion 260 may be the same as or different from the material of the gate dielectric layer 250 .

[0071] In this embodiment, the method of injecting doped ions into the corner area is used to slow down the oxidation rate of the corner area, avoid the formation of a thicker oxide layer, and avoid the removal process removing the oxide layer at a faster rate to gradually form a larger chamfer, thereby ensuring that the corner area of ​​the active area has good structural integrity, and further ensuring that the active area and the semiconductor structure containing the active area, such as a field effect transistor, have good electrical properties.

[0072] Correspondingly, an embodiment of the present invention further provides a semiconductor structure, which can be manufactured by the above-mentioned semiconductor structure manufacturing method.

[0073] refer to Fig.15 The semiconductor structure includes: a substrate 200, the substrate 200 includes an active area 201 and an isolation area located between adjacent active areas 201, the active area 201 includes a corner area 212 adjacent to the isolation area, and the structure in the isolation area exposes the side wall of the corner area 212; the corner area 212 contains doped ions, and the doped ions are used to slow down the oxidation rate of the corner area 212.

[0074] In this embodiment, the isolation region has an isolation structure 240, and the isolation structure 240 has a recessed portion 241 (see Fig.12 ), the recessed portion 241 exposes the side wall of the corner region 212.

[0075] In this embodiment, the semiconductor structure further includes: a gate dielectric layer 250 and an isolation portion 260, the gate dielectric layer 250 covers the top surface of the active area 201, and the isolation portion 260 covers the side wall of the corner area 212; in other embodiments, the gate dielectric layer covers the top surface of the active area and covers the side wall of the corner area.

[0076] In this embodiment, the corner region has doping ions that can slow down the oxidation rate, which helps to prevent the corner region from being etched and consuming a lot of material during the removal process, thereby ensuring that the corner region has good structural integrity.

[0077] Those skilled in the art will appreciate that the above embodiments are specific examples of the present invention, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present invention. Any person skilled in the art may make changes and modifications without departing from the spirit and scope of the present invention, and therefore the scope of protection of the present invention shall be subject to the scope defined in the claims.

Claims

1. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate, the substrate comprising an active region and an isolation region located between adjacent active regions, the active region comprising a corner region adjacent to the isolation region; Performing a doping process to inject doping ions into the corner region, wherein the doping ions are used to slow down the oxidation rate of the corner region; After the doping process is performed, a removal process is performed on the substrate, wherein the removal process can remove the oxidized substrate, and during the removal process, the structure in the isolation region exposes the side wall of the corner region, wherein the removal process on the substrate includes: performing an etching process on the substrate in the isolation region to form a groove exposing the side wall of the corner region, wherein the groove is used to form an isolation structure; Performing a deposition process on the active area to form a gate dielectric layer that only covers the top surface of the active area, wherein the gate dielectric layer and the isolation structure expose the sidewall of the corner area; An isolation portion is formed to cover the sidewall of the corner region, wherein the material of the isolation portion is different from the material of the gate dielectric layer.

2. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The removal process further includes: after the etching process, performing a first cleaning process on the trench, wherein a cleaning liquid of the first cleaning process contacts the sidewall of the corner region.

3. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The isolation structure has a recessed portion, and the recessed portion exposes the side wall of the corner area; The removal process includes: after the doping process, performing a second cleaning process on the top surface of the active area, wherein a cleaning liquid of the second cleaning process contacts the side wall of the corner area.

4. The method for manufacturing a semiconductor structure according to claim 3, characterized in that: After performing the second cleaning process, the gate dielectric layer is formed.

5. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The doping ions include nitrogen ions, and the implantation dose of the doping ions is 1e12-1e16 atoms / cm 2 .

6. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The process steps for injecting the doped ions include: providing the substrate and a shielding layer located on the substrate, the active area also includes an intermediate area located between adjacent corner areas, the shielding layer covers the top surface of the intermediate area, and the shielding layer is used to shield the injection of the doped ions; performing an ion implantation process on the substrate.

7. The method for manufacturing a semiconductor structure according to claim 6, characterized in that: The implantation energy range of the ion implantation process is 1KV~60KV.

8. The method for manufacturing a semiconductor structure according to claim 6, characterized in that: The shielding layer also covers the corner area and exposes the isolation area; and the ion implantation process with an implantation angle is performed on the substrate.

9. The method for manufacturing a semiconductor structure according to claim 8, characterized in that: The injection angle is 5°~60°.

10. A semiconductor structure manufactured by the method for manufacturing a semiconductor structure according to any one of claims 1 to 9, characterized in that: include: A substrate, the substrate comprising an active region and an isolation region located between adjacent active regions, the active region comprising a corner region adjacent to the isolation region, and a structure in the isolation region exposing a sidewall of the corner region; The corner region contains doping ions, and the doping ions are used to slow down the oxidation rate of the corner region.

11. The semiconductor structure according to claim 10, characterized in that: An isolation structure is provided in the isolation region. The isolation structure has a recessed portion. The recessed portion exposes the side wall of the corner region.

12. The semiconductor structure according to claim 11, characterized in that: Also includes: A gate dielectric layer and an isolation portion, wherein the gate dielectric layer covers the top surface of the active area, and the isolation portion covers the sidewall of the corner area.