Step cross beam island staggered film high-overload pressure sensor chip and preparation method thereof

By using the stepped cross-beam archipelago dislocated membrane structure and back cavity design in the pressure sensor, the problem of insufficient overload capability of traditional pressure sensors in harsh environments is solved, bidirectional high overload and high sensitivity are achieved, and the process is simple and easy to produce.

CN118706299APending Publication Date: 2024-09-27DALIAN UNIV OF TECH
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410767217.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-14
Publication Date
2024-09-27

AI Technical Summary

Technical Problem

Existing pressure sensors are prone to high overload conditions in harsh environments. The traditional structural design results in insufficient overload capability. Moreover, the existing anti-overload device has the problem of being large in size and can only withstand one-way or instantaneous overload.

Method used

Using a stepped cross beam island dislocation film structure, a closed cavity is formed between the silicon wafer substrate and the glass substrate, and a stepped cross beam and back cavity structure are provided on the front and back of the film, combined with a varistor strip and a Wheatstone bridge. Achieve stress concentration and bidirectional high overload capability.

Benefits of technology

The overload capacity and sensitivity of the pressure sensor are significantly improved, and bidirectional high overload is achieved. The process is simple, easy to be mass produced, and the performance is stable and reliable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118706299A
    Figure CN118706299A
Patent Text Reader

Abstract

The invention discloses a stepped cross beam island staggered film high-overload pressure sensor chip and a preparation method thereof, and belongs to the technical field of pressure sensors. Comprising a glass substrate and a silicon wafer substrate, the outer edge of the silicon wafer substrate is supported above the glass substrate, the middle of the silicon wafer substrate is of a hollow structure, and a closed cavity is formed between the glass substrate and the silicon wafer substrate; a diaphragm pressure sensing structure is arranged on the top wall surface of the closed cavity; the diaphragm pressure sensing structure is divided into a stepped cross beam group island structure layer, a thin film layer and a back cavity structure layer. The stepped cross-shaped beam group island structure layer is composed of four stepped cross-shaped beams distributed in the middle of the edge of the vertical thin film layer and a group island composed of square islands evenly distributed above the thin film. The back cavity structure layer is composed of short beams, long beams, islands and group islands. The short beam corresponds to the stepped cross beam and is short in length, and dislocation is formed to improve the overload capacity of the sensor. The sensor chip provided by the invention is reasonable in structure and has the characteristic of bidirectional high overload, the dynamic performance and the overall linearity of the sensor are improved, and the overload capacity is remarkably enhanced; the manufacturing method is simple, and batch production is easy.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of pressure sensors and relates to a stepped cross-beam archipelago dislocation film high overload pressure sensor chip and a preparation method thereof. Background Art

[0002] Since Smith discovered the piezoresistive effect in semiconductors in the 1950s, piezoresistive pressure sensors have received widespread attention. Silicon has been proven to be one of the best materials for manufacturing pressure sensors. Piezoresistive pressure sensors are widely used in pressure measurement, pressure monitoring and pressure control in many fields such as the automotive industry, aerospace, biomedicine, industrial robots, ship systems, and industrial testing due to their compact structure, easy integration, good performance, high reliability, and low cost. When pressure sensors are used in harsh environments such as aerospace, petrochemicals, and marine science, due to the fluidity and volatility of the measured medium, the pressure often exceeds the measurement range of the pressure sensor, and even a severe overload of "water hammer" may occur, which requires the pressure sensor to have a strong overload capacity.

[0003] A large number of studies have confirmed that the performance of the sensor can be significantly improved by designing the sensitive diaphragm structure of the pressure sensor. Invention patent CN 111504526 B discloses a piezoresistive pressure sensor chip with a stress concentration structure and a preparation method thereof. The invention uses the principle of stress mutation to concentrate stress in the gap of the peninsula island of the silicon cup cavity through the peninsula island structure, stress concentration groove and stress adjustment groove, which significantly improves the sensitivity and linearity of the sensor. The overload breakage of the pressure sensor is closely related to the distribution and value of the maximum stress. The ideal maximum stress point should be located in the varistor area. The maximum stress distribution of the sensitive diaphragm structure of the above invention is located at the stress concentration point on the back of the silicon cup cavity, resulting in its overload capacity being very limited. At present, most sensor structures are similar to this invention. By designing different structures to increase the stress in the varistor area, the sensitivity of the sensor is improved, but the maximum stress point is still distributed in the middle of the edge of the film at the top of the silicon pressure sensor cavity. The above maximum stress distribution causes the stress value of the maximum stress point to increase rapidly when the external pressure increases. When the maximum stress value reaches the fracture strength of silicon, the pressure sensor will break and fail. Therefore, scholars have proposed some other measures to improve the overload capacity of pressure sensors.

[0004] Invention patent CN 112345157 A discloses a pressure sensor that is resistant to high overloads. Based on the corresponding fluid mechanics principles, the invention adds a pressure buffer structure in the pressure-conducting hole, and adds a flow channel of appropriate length to the pressure buffer structure to buffer the overload pressure, thereby suppressing transient overload pressure and improving the overload capacity of the pressure sensor. The existence of the pressure buffer mechanism of the invention increases the overall size of the pressure sensor, and can only detect unidirectional pressure, and cannot achieve bidirectional overload resistance. At the same time, limited by the length of the flow channel in the buffer structure, the invention can only suppress transient overload pressure. When subjected to continuous overload pressure, the buffer structure of the invention will not work, and the sensor will still break and fail.

[0005] Invention patent CN 116399484 A discloses a high overload pressure sensor and its preparation method. The invention proposes a three-layer structure of a silicon cup, a silicon boss and glass. The silicon boss plays a limiting role and is located inside the silicon cup cavity. Together with the silicon cup, it is bonded to the glass substrate. When subjected to overload pressure, the film of the silicon cup will deform and contact with the silicon boss, thereby resisting external pressure and improving the overload capacity of the pressure sensor. However, the production of the silicon boss requires adding multiple processes such as bonding, low-pressure chemical vapor deposition, photolithography, reactive ion etching and wet etching, which is relatively cumbersome, and the dimensional accuracy requirements of the silicon boss and the silicon cup cavity are also high. At the same time, the three-layer structure of the silicon cup, silicon boss and glass determines that it can only withstand overload pressure from top to bottom and cannot achieve bidirectional overload resistance.

[0006] In summary, there are still some problems in the existing methods for improving the overload capacity of pressure sensors. On the one hand, the structural design of the existing pressure sensor is to simply increase the stress of the piezoresistive area by making some stress concentration structures. Although the sensitivity of the sensor is greatly improved, the overload capacity has not been improved, and even the phenomenon of high sensitivity and extremely poor overload capacity of the sensor may occur. On the other hand, some anti-overload devices, such as pressure buffer structures, membrane box devices, etc., although they improve the overload capacity of the sensor to a certain extent, also have many disadvantages: they can only resist instantaneous overload, the device is too large relative to the pressure sensor, and can only achieve unidirectional overload resistance. In addition, some scholars have proposed stop structures such as silicon bosses, but they are difficult to implement due to complex processes and extremely high dimensional accuracy. Therefore, it is difficult to achieve bidirectional high overload of pressure sensors with simple silicon structure designs in existing processes. Based on existing research and technology, the present invention proposes a stepped cross beam island dislocation membrane high overload pressure sensor chip and a preparation method thereof, which realizes bidirectional high overload of pressure sensors based on a simple silicon piezoresistive pressure sensor process and a silicon body structure design concept. Summary of the invention

[0007] In order to solve the difficulty of improving the overload capacity and overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a stepped cross-beam island dislocation membrane high overload pressure sensor chip and a preparation method thereof. The pressure sensor chip has the advantages of bidirectional high overload and is based on the silicon body structure design, the manufacturing method is simple, the performance is stable and reliable, and it is easy to mass produce.

[0008] To achieve the above object, the technical solution adopted by the present invention is as follows:

[0009] A step cross beam archipelago dislocation membrane high overload pressure sensor chip, the pressure sensor chip comprises a silicon wafer substrate 1 and a glass substrate 8 anodically bonded to the silicon wafer substrate 1, the outer edge of the glass substrate 8 is supported below the silicon wafer substrate 1, the middle of the silicon wafer substrate 1 is a hollow structure, so that a closed cavity is formed between the two; the top wall of the closed cavity is provided with a diaphragm pressure sensing structure, and the diaphragm pressure sensing structure is divided into a step cross beam archipelago structure layer, a thin film layer and a back cavity structure layer. Specifically:

[0010] The step cross beam island structure layer is composed of four step cross beams 2 distributed in the middle of the edge of the vertical film layer and an island 6 composed of square islands evenly distributed above the film. The step cross beam island structure layer has the advantages of good linearity and high overload capacity; the step cross beam 2 is composed of a first step beam 2-1, a second step beam 2-2, a third step beam 2-3 and a fourth step beam 2-4, the outer end of each step beam is located in the middle of the edge of the film layer, and the other end extends to the center, and the four step beams do not touch, and the first varistor strip 3-1, the second varistor strip 3-2, the third varistor strip 3-3 and the fourth varistor strip 3-4 are respectively arranged at the center of the step of the step cross beam 2; the island 6 is composed of a first island 6-1, a second island 6-2, a third island 6-3 and a fourth island 6-4, each island contains seven islands, and the first island 6-1, the second island 6-2, the third island 6-3 and the fourth island 6-4 are evenly distributed on the front of the film 7.

[0011] The back cavity structure layer is composed of short beams 9, long beams 10, islands 11 and archipelagos 12. The bottom surface of the back cavity structure layer is the back side of the film 7. The short beams 9 correspond to the step cross beams 2, but are slightly shorter in length to form a misalignment, which further improves the overload capacity of the pressure sensor chip. Specifically, the short beams 9 are composed of a first short beam 9-1, a second short beam 9-2, a third short beam 9-3 and a fourth short beam 9-4, which are arranged in the direction of the symmetric axis on the back side of the film 7. The first short beam 9-1, the second short beam 9-2, the third short beam 9-3 and the fourth short beam 9-4 are connected to the side wall of the back cavity, in the same direction as the step cross beam 2, but opposite to each other. It is slightly shorter than the length of the step cross beam by 100 to 200 μm, forming a spatial position dislocation; the long beam 10 is composed of a first long beam 10-1, a second long beam 10-2, a third long beam 10-3 and a fourth long beam 10-4, and the four long beams are respectively located in the middle of the four short beams and the isolated island 11 and are 300 μm to 500 μm away from the short beams and the isolated island; the isolated island 11 is arranged at the center of the back side of the film 7; the archipelago 12 is composed of a first archipelago 12-1, a second archipelago 12-2, a third archipelago 12-3 and a fourth archipelago 12-4, which are evenly distributed on the back side of the film 7 and correspond to the front archipelago 6.

[0012] The thin film layer is composed of a thin film 7, which is formed by etching a stepped cross beam island structure layer on the front side and a back cavity structure layer on the back side of a silicon wafer substrate 1.

[0013] The first varistor strip 3-1, the second varistor strip 3-2, the third varistor strip 3-3 and the fourth varistor strip 3-4 are connected by metal leads 4 and pads 5 to form a Wheatstone bridge. Further, the Wheatstone bridge is specifically as follows: the first varistor strip 3-1 is connected to the first pad 5-1 and the second pad 5-2 through the first metal lead 4-1 and the second metal lead 4-2 respectively; the second varistor strip 3-2 is connected to the second pad 5-2 and the third pad 5-3 through the third metal lead 4-3 and the fourth metal lead 4-4 respectively; the third varistor strip 3-3 is connected to the fourth pad 5-4 and the fifth pad 5-5 through the fifth metal lead 4-5 and the sixth metal lead 4-6 respectively; The fourth varistor strip 3-4 is connected to the fifth pad 5-5 and the first pad 5-1 through the seventh metal lead 4-7 and the eighth metal lead 4-8 respectively; the five pads are all squares with a side length of 300μm to 500μm, among which the first pad 5-1, the second pad 5-2, the third pad 5-3 and the fifth pad 5-5 are located at the four corners of the edge of the film 7, and the center of the pad is 300μm to 500μm away from the edge, and the fourth pad 5-4 is located on the left side of the third pad 5-3, at a distance of 700μm to 1000μm.

[0014] Furthermore, the steps of the step cross beam 2 on the front of the film 7 are all rounded, with a radius of 50 μm to 100 μm, and the varistor is arranged on the symmetry axis of the step cross beam 2. The step cross beam 2 is a two-stage step structure with a large outer end size.

[0015] Furthermore, the step cross beams 2 and the islands 6 on the front side of the film 7 have the same thickness, which is 100% to 200% of the film thickness of the film 7 .

[0016] Furthermore, the widths of the step cross beam 2, the short beam 9, the long beam 10 and the island 11 are equal, and are all 200 μm to 300 μm.

[0017] Furthermore, all islands in the first archipelago 6-1, the second archipelago 6-2, the third archipelago 6-3 and the fourth archipelago 6-4 on the front side of the film 7 and all corresponding islands on the back side are squares with equal side lengths of 200 μm to 300 μm.

[0018] Furthermore, the short beam 9 on the back of the film 7 is 50 μm to 150 μm away from the bonding surface between the silicon wafer and the glass, and the long beam 10, the island 11 and the archipelago 12 have the same thickness and are 50 μm to 100 μm away from the bonding surface.

[0019] Furthermore, a through hole 13 is provided in the middle of the glass substrate 8 , and the hole diameter is 0.5 mm to 1 mm. The through hole 13 is used to transmit the external pressure to the back side of the film 7 .

[0020] Furthermore, the Wheatstone bridge is a semi-open-loop Wheatstone bridge, and the open loop of the semi-open-loop Wheatstone bridge is used to connect to an external resistor.

[0021] A method for preparing a stepped cross beam archipelago dislocation film high overload pressure sensor chip comprises the following steps:

[0022] Step 1: Use an N-type 100-crystal double-sided polished silicon wafer and perform standard RCA cleaning;

[0023] Step 2: photolithography is performed on the front side of the cleaned silicon wafer 1 using a varistor mask, and then light boron ion doping is performed by ion implantation to form a first varistor strip 3-1, a second varistor strip 3-2, a third varistor strip 3-3, and a fourth varistor strip 3-4, respectively, and then annealing is performed;

[0024] Step 3, photolithography is performed on the front side of the product obtained in step 2 using an ohmic contact mask, heavy boron ion doping is performed by ion implantation to form an ohmic contact region 14, and then annealing is performed;

[0025] Step 4: deposit a silicon nitride layer 15 on the front side of the product obtained in step 3 by using a plasma enhanced chemical vapor deposition process, and etch a contact hole 16 by using an ICP technique;

[0026] Step 5, photolithography is performed on the front side of the product obtained in step 4 using a metal lead mask, followed by magnetron sputtering and stripping to form metal leads 4 and pads 5, and then high-temperature alloying treatment is performed;

[0027] Step 6, photolithography the front side of the product obtained in step 5, using ICP technology to etch out the front stepped cross beam 9 and the islands 6: the stepped cross beam 2 includes the first stepped beam 2-1, the second stepped beam 2-2, the third stepped beam 2-3 and the fourth stepped beam 2-4, and the front islands 6 include the first islands 6-1, the second islands 6-2, the third islands 6-3 and the fourth islands 6-4;

[0028] Step 7, using a back cavity etching mask to perform photolithography on the back side of the product obtained in step 6, and using ICP technology to etch and form short beams 9, long beams 10, islands 11 and archipelagos 12 of the back cavity: the short beams 9 include the first short beams 9-1, the second short beams 9-2, the third short beams 9-3 and the fourth short beams 9-4, the long beams 10 include the first long beams 10-1, the second long beams 10-2, the third long beams 10-3 and the fourth long beams 10-4, and the archipelagos 12 of the back cavity include the first archipelagos 12-1, the second archipelagos 12-2, the third archipelagos 12-3 and the fourth archipelagos 12-4;

[0029] Step 8, photolithography is performed on the back of the product obtained in step 7, and the thickness of the long beam 10, the island 11 and the archipelago 12 is reduced by using ICP technology;

[0030] Step 9, performing laser drilling on the BF33 glass substrate 8 to form a through hole 13;

[0031] Step 10: Anodically bond the silicon wafer substrate 1 manufactured in step 8 to the glass substrate 8 processed in step 9 to obtain a high overload pressure sensor chip.

[0032] Furthermore, after the completion of step 2 and step 3, the silicon wafer is annealed to make the impurity doping concentration of the varistor strip 3 and the ohmic contact region 14 more uniform.

[0033] Compared with the prior art, the present invention has at least the following beneficial technical effects:

[0034] 1) The sensor chip proposed in the present invention has a reasonable structure and has the characteristics of bidirectional high overload, which is conducive to mass production.

[0035] 2) The present invention improves on the traditional square film structure. According to the stress distribution of the traditional film structure under pressure, it can be seen that the maximum stress distribution is not concentrated, and the stress value is small, which cannot meet the requirements of high sensitivity. In order to improve the above shortcomings, a stepped cross beam is added to the front of the film and a short beam is added to the back to concentrate the stress at the steps of the stepped cross beam. At the same time, the varistor is set here, which solves the problem of unconcentrated stress value and small stress value in the traditional film structure. At the same time, the beam structure increases the stiffness of the film structure to a certain extent, thereby improving the linearity and natural frequency. The increase in the natural frequency improves the dynamic performance of the sensor.

[0036] 3) In order to further optimize the stress distribution and size of the film and make the stress concentration effect more obvious, an island structure is set on the front and back of the film. The island structure makes the film more sensitive to stress and better concentrates it at the steps of the step cross beam, while significantly improving the overall linearity.

[0037] 4) In order to improve the overload capacity of the pressure sensor, the steps of the stepped cross beam on the front side of the film are staggered with the short beam boundary on the back side of the film to form a staggered film. At the same time, the thickness of the cross beam and the film thickness are adjusted to concentrate the maximum stress at the varistor on the front side of the film, thereby solving the problem that the maximum stress of the traditional film structure is concentrated at the midpoint of the cavity boundary on the back side, which is easy to reach the fracture strength and thus cause the silicon film to break and fail. At the same time, a rounded transition is set at the steps of the stepped cross beam to evenly distribute the stress concentration on the surface along the width direction of the steps of the stepped cross beam, so that the varistor is subjected to more uniform force, thereby improving the performance of the pressure sensor and significantly enhancing the overload capacity.

[0038] 5) The Wheatstone bridge designed in the present invention is a semi-open-loop Wheatstone bridge, and the open-loop portion can be used to connect to an external resistor, thereby compensating for the inconsistency of the resistance of the four varistor strips caused by process errors.

[0039] 6) The method for preparing the pressure sensor chip described in the present invention mainly realizes bidirectional high overload through bulk silicon technology, the process is mature and stable, the manufacturing method is simple, and it is easy to mass produce. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 It is an axonometric schematic diagram of the present invention;

[0041] Figure 2 This is a perspective view of the back glass of the present invention;

[0042] Figure 3 for Figure 2 Schematic cross-sectional view at the AA section;

[0043] Figure 4 A schematic diagram of a Wheatstone bridge formed by connecting varistor strips of the present invention;

[0044] Figure 5-1 This is a schematic diagram of the distribution of the first varistor strips of the present invention;

[0045] Figure 5-2 This is a schematic diagram of the distribution of the second varistor strips of the present invention;

[0046] Figure 6 It is a schematic diagram of stress distribution of the present invention and a flat membrane with the same size and the same range under pressure;

[0047] Figure 7 It is a schematic diagram of the manufacturing process of the present invention.

[0048] In the figure: 1 silicon wafer substrate; 2 step beam; 3 varistor strip; 4 metal lead; 5 pad; 6 islands; 7 film; 8 glass substrate; 9 short beam; 10 long beam; 11 islands; 12 islands;

[0049] 2-1 first step beam; 2-2 second step beam; 2-3 third step beam; 2-4 fourth step beam;

[0050] 3-1 first varistor strip; 3-2 first varistor strip; 3-3 first varistor strip; 3-4 first varistor strip;

[0051] 4-1 first metal lead; 4-2 second metal lead; 4-3 third metal lead; 4-4 fourth metal lead; 4-5 fifth metal lead; 4-6 sixth metal lead; 4-7 seventh metal lead; 4-8 eighth metal lead;

[0052] 5-1 first pad; 5-2 second pad; 5-3 third pad; 5-4 fourth pad; 5-5 fifth pad;

[0053] 6-1 First Islands; 6-2 Second Islands; 6-3 Third Islands; 6-4 Fourth Islands;

[0054] 9-1 the first short beam; 9-2 the second short beam; 9-3 the third short beam; 9-4 the fourth short beam;

[0055] 10-1 the first long beam; 10-2 the second long beam; 10-3 the third long beam; 10-4 the fourth long beam;

[0056] 12-1 First Islands; 12-2 Second Islands; 12-3 Third Islands; 12-4 Fourth Islands; DETAILED DESCRIPTION

[0057] In order to make the purpose and technical solution of the present invention clearer and easier to understand. The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. The specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of this application.

[0058] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, which are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, the meaning of "multiple" is two or more. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0059] Reference Figure 1 , a step cross beam island dislocation membrane high overload pressure sensor chip, the sensor chip is structurally divided into a step cross beam island film structure layer and a back cavity structure layer.

[0060] Reference Figure 1 The stepped cross beam island membrane structure includes: a square membrane 7, a first stepped beam 2-1, a second stepped beam 2-2, a third stepped beam 2-3, a fourth stepped beam 2-4 located inside the membrane 7 and arranged in sequence along the center of the membrane 7, and a first island 6-1, a second island 6-2, a third island 6-3 and a fourth island 6-4 evenly distributed in four regions of the membrane 7. The thickness of the first stepped beam to the fourth stepped beam and the first island to the fourth island is 100% to 200% of the thickness of the membrane 7.

[0061] The step cross beam is composed of four step beams, the steps of the step beams are smoothly connected by fillets and form a stress concentration area, the stress concentration area of ​​the first step beam is provided with a first varistor strip 3-1, the stress concentration area of ​​the second step beam is provided with a second varistor strip 3-2, the stress concentration area of ​​the third step beam is provided with a third varistor strip 3-3, and the stress concentration area of ​​the fourth step beam is provided with a fourth varistor strip 3-4. The effective length of all varistor strips is along the crystal direction with the largest piezoresistance coefficient, and the metal lead connects the first to fourth varistor strips to form a semi-open-loop Wheatstone full bridge, and the Wheatstone full bridge is connected to five pads arranged on the substrate 1 to realize the input and output of electrical signals.

[0062] Reference Figure 1 and Figure 4 , the first metal lead 4-1 connects the first end of the first varistor strip 3-1 to the first pad 5-1, and the second metal lead 4-2 connects the second end of the first varistor strip 3-1 to the second pad 5-2; the third metal lead 4-3 connects the first end of the second varistor strip 3-2 to the second pad 5-2, and the fourth metal lead 4-4 connects the second end of the second varistor strip 3-2 to the third pad 5-3; the fifth metal lead 4-5 connects the first end of the third varistor strip 3-3 to the fourth pad 5-4, and the sixth metal lead 4-6 connects the second end of the third varistor strip 3-3 to the fifth pad 5-5; the seventh metal lead 4-7 connects the first end of the fourth varistor strip 3-4 to the fifth pad 5-5, and the eighth metal lead 4-8 connects the second end of the fourth varistor strip 3-4 to the first pad 5-1. The third pad 5 - 3 and the fourth pad 5 - 4 are set as open loops, and are used to connect to external resistors to compensate for the inconsistency of resistance of the four varistor strips caused by process errors.

[0063] Reference Figure 2The back cavity structure mainly includes: the first short beam 9-1, the second short beam 9-2, the third short beam 9-3, the fourth short beam 9-4, the first long beam 10-1, the second long beam 10-2, the third long beam 10-3 and the fourth long beam 10-4, which are connected to the substrate 1 and uniformly distributed in the middle of the boundary of the film 7 and have equal width. The central axis of the first short beam 9-1, the first long beam 10-1, the third long beam 10-3 and the third short beam 9-3 are reciprocated; the central axis of the second short beam 9-2, the second long beam 10-2, the fourth long beam 10-4 and the fourth short beam 9-4 coincides; there is a gap of 300μm to 400μm between the first short beam 9-1 and the first long beam 10-1, between the second short beam 9-2 and the second long beam 10-2, between the third short beam 9-3 and the third long beam 10-3, and between the fourth short beam 9-4 and the fourth long beam 10-4. The gap can further concentrate the stress. An island 11 is provided in the middle of the back cavity film 7, and a gap of 200 μm to 300 μm is provided between the island 11 and the first to fourth long beams. The widths of the first to fourth short beams, the first to fourth long beams and the island 11 are equal, all of which are 150 μm to 200 μm. On the surface of the back cavity film 7, corresponding to the four front archipelagos, the first archipelagos 12-1, the second archipelagos 12-2, the third archipelagos 12-3 and the fourth archipelagos 12-4 are provided, and their widths are the same as those of the four front archipelagos, all of which are 200 μm to 300 μm.

[0064] Reference Figure 3 The back of the substrate 1 is combined with the glass substrate 8 by vacuum bonding. The heights of the first islands 12-1, the second islands 12-2, the third islands 12-3, the fourth islands 12-4, the first long beam 10-1, the second long beam 10-2, the third long beam 10-3, the fourth long beam 10-4 and the isolated island 11 in the back cavity of the substrate 1 are the same, which is determined by the displacement of the sensor diaphragm at the maximum stress, ensuring that the first to fourth long beams and the isolated island 11 do not interfere with the glass substrate 8, and the differential pressure measurement is realized through the through hole 13.

[0065] Reference Figure 5-1 and Figure 5-2 , the first varistor strip 3-1 is located in the middle of the step of the first step beam 2-1; the second varistor strip 3-2 is located in the middle of the step of the second step beam 2-2; the third varistor strip 3-3 has the same structure and layout as the first varistor strip 3-1, and is located in the middle of the step of the third step beam 2-3; the fourth varistor strip 3-4 has the same structure and layout as the second varistor strip 3-2, and is located in the middle of the step of the fourth step beam 2-4. All four varistors are of four-fold structure, with the same initial resistance value, and their effective length directions are all along the crystal direction with the largest piezoresistance coefficient.

[0066] As a preferred embodiment of the present invention, the film 7 is a square film, and the first step beam 2-1, the second step beam 2-2, the third step beam 2-3, and the fourth step beam 2-4 distributed perpendicular to the midpoint of the edge of the film are all stepped from large to small, and the length, width and height of the four are the same, and together form a step cross beam.

[0067] The working principle of the present invention is:

[0068] When the sensor chip is subjected to different pressures from top to bottom, the film begins to deform under the action of the differential pressure. The step cross beam on the film and the short beam and long beam of the back cavity cause the stress to be concentrated at the step of the step cross beam and the gap between the short beam and the long beam. The spatial misalignment of the step and the gap causes the maximum stress to be concentrated at the step cross beam, which not only increases the resistance change of the first to fourth varistor strips and improves the sensitivity of the sensor, but also makes the stress increase less drastic than that of the traditional flat film, thereby improving the overload capacity of the sensor. Figure 6 As shown, compared with the flat membrane of the same size and the same range, the maximum stress of the sensor chip of the present invention is smaller, and a stronger overload capacity can be achieved. At the same time, the islands on the film and the islands and islands in the back cavity increase the support and mass of the structure, thereby increasing the rigidity of the structure and improving the linearity of the sensor. Therefore, the sensor chip of the present invention has the advantages of strong bidirectional overload capacity, high sensitivity and good linearity.

[0069] The preparation method of the sensor chip of the present invention is as follows:

[0070] Reference Figure 7 As shown, the present invention provides a method for preparing a stepped cross beam archipelago dislocation membrane high overload pressure sensor chip, comprising the following steps:

[0071] Step 1: Use an N-type (100) double-sided polished silicon wafer and perform standard RCA cleaning;

[0072] Step 2: photolithography is performed on the front side of the cleaned silicon wafer 1 using a varistor mask, and then light boron ion doping is performed by ion implantation to form a first varistor strip 3-1, a second varistor strip 3-2, a third varistor strip 3-3, and a fourth varistor strip 3-4, respectively, and then annealing is performed to make the impurity doping concentration of the varistor region more uniform;

[0073] Step 3, photolithography is performed on the front side of the product obtained in step 2 using an ohmic contact mask, and heavy boron ion doping is performed by ion implantation to form an ohmic contact region 14, and then annealing is performed to make the impurity doping concentration of the ohmic contact region 14 more uniform;

[0074] Step 4: deposit a silicon nitride layer 15 on the front side of the product obtained in step 3 by using a plasma enhanced chemical vapor deposition process, and etch a contact hole 16 by using an ICP technique;

[0075] Step 5, photolithography is performed on the front side of the product obtained in step 4 using a metal lead mask, followed by magnetron sputtering and stripping to form metal leads 4 and pads 5, and then high-temperature alloying treatment is performed;

[0076] Step 6, photolithography the front side of the product obtained in step 5, using ICP technology to etch out the front stepped cross beam 2 and the archipelago 6: the stepped cross beam 2 includes the first stepped beam 2-1, the second stepped beam 2-2, the third stepped beam 2-3 and the fourth stepped beam 2-4, the front archipelago 6 includes the first archipelago 6-1, the second archipelago 6-2, the third archipelago 6-3 and the fourth archipelago 6-4, and the thickness of the first stepped beam to the fourth stepped beam and the first archipelago to the fourth archipelago is 100% to 200% of the thickness of the film 7;

[0077] Step 7, using the back cavity etching mask to perform photolithography on the back side of the product obtained in step 6, and using ICP technology to etch and form short beams 9, long beams 10, islands 11 and archipelagos 12 of the back cavity: the short beams 9 include the first short beams 9-1, the second short beams 9-2, the third short beams 9-3 and the fourth short beams 9-4, the long beams 10 include the first long beams 10-1, the second long beams 10-2, the third long beams 10-3 and the fourth long beams 10-4, the archipelagos 12 of the back cavity include the first archipelagos 12-1, the second archipelagos 12-2, the third archipelagos 12-3 and the fourth archipelagos 12-4, and the short beams are 50μm to 150μm away from the bottom surface of the back cavity;

[0078] Step 1: Photolithography the back of the product obtained in step 7, using ICP technology to reduce the thickness of the long beam 10, the island 11 and the archipelago 12, so that the thickness of the long beam 10, the island 11 and the archipelago 12 is equal and the distance from the bottom surface of the back cavity is 50 μm to 100 μm;

[0079] Step 9, laser drilling is performed on the glass substrate 8 to form a through hole 13 with a diameter of 0.5 mm to 1 mm;

[0080] Step 10: Anodic bonding is performed on the silicon substrate 1 manufactured in step 8 and the glass substrate 8 processed in step 9 to obtain a high overload pressure sensor chip.

[0081] The pressure sensor produced by this embodiment has a measuring range of 100kPa, and an overload capacity of more than 6 times the full scale. Compared with the MPM288 piezoresistive OEM pressure sensitive element produced by Mike Sensor Co., Ltd., with a measuring range of 0 to 100kPa and an overload capacity of 1.5 times the full scale, the overload capacity of the present invention is increased by more than 4 times. Compared with the QBE2003-P1 pressure sensor of Siemens of Germany, with a measuring range of 0 to 100kPa and an overload capacity of 2.5 times the full scale, the overload capacity of the present invention is increased by more than 2.4 times. Compared with the 7000 series products of Merit Sensor of the United States, with a measuring range of 15psi (103kPa) and an overload capacity of 3 times the full scale, the overload capacity of the present invention is increased by more than 2 times. It can be seen that the use of the method of the present invention can significantly improve the overload capacity of the pressure sensor.

[0082] The above is only one embodiment of the present invention, not all or the only embodiment. Any equivalent changes made by ordinary technicians in this field in the face of the technical solution of the present invention after reading the specification of the present invention are covered by the claims of the present invention.

Claims

1. A stepped cross beam island dislocation film high overload pressure sensor chip, characterized in that: The pressure sensor chip comprises a silicon wafer substrate (1) and a glass substrate (8) anodically bonded to the silicon wafer substrate (1); the outer edge of the glass substrate (8) is supported below the silicon wafer substrate (1); the middle of the silicon wafer substrate (1) is a hollow structure, so that a closed cavity is formed between the two; a diaphragm pressure-sensing structure is provided on the top wall of the closed cavity, and the diaphragm pressure-sensing structure is divided into a stepped cross-beam island structure layer, a thin film layer and a back cavity structure layer.

2. The step cross beam island dislocation film high overload pressure sensor chip according to claim 1, characterized in that: The step cross beam archipelago structure layer is composed of four step cross beams (2) distributed in the middle of the edge of the vertical film layer and an archipelago (6) composed of square islands evenly distributed above the film; four varistor strips are respectively arranged at the center of the steps of the step cross beam (2), and the four varistor strips are connected by metal leads (4) and pads (5) to form a Wheatstone bridge; The back cavity structure layer is composed of short beams (9), long beams (10), isolated islands (11) and archipelagos (12); the bottom surface of the back cavity structure layer is the back surface of the film (7); the short beams (9) correspond to the stepped cross beams (2), but are short in length to form a misalignment, thereby improving the overload capacity of the pressure sensor chip; The thin film layer is composed of a thin film (7), and the thin film (7) is formed by etching a stepped cross beam island structure layer on the front side and a back cavity structure layer on the back side of a silicon wafer substrate (1).

3. The step cross beam island dislocation film high overload pressure sensor chip according to claim 2, characterized in that: In the stepped cross beam archipelago structure layer: the stepped cross beam (2) is composed of a first stepped beam (2-1), a second stepped beam (2-2), a third stepped beam (2-3) and a fourth stepped beam (2-4); the outer end of each stepped beam is located in the middle of the edge of the film layer, and the other end extends toward the center, and the four stepped beams are not in contact; a first varistor strip (3-1), a second varistor strip (3-2), a third varistor strip (3-3) and a fourth varistor strip (3-4) are respectively arranged at the center of the step of the stepped cross beam (2); the archipelago (6) is composed of a first archipelago (6-1), a second archipelago (6-2), a third archipelago (6-3) and a fourth archipelago (6-4); each archipelago contains seven islands; the first archipelago (6-1), the second archipelago (6-2), the third archipelago (6-3) and the fourth archipelago (6-4) are uniformly distributed on the front of the film (7); In the back cavity structure layer: the short beam (9) is composed of a first short beam (9-1), a second short beam (9-2), a third short beam (9-3) and a fourth short beam (9-4), and is arranged in the direction of the symmetric axis of the back side of the film (7); the first short beam (9-1), the second short beam (9-2), the third short beam (9-3) and the fourth short beam (9-4) are connected to the side wall of the back cavity, and have the same direction as the step cross beam (2), but are slightly shorter than the step cross beam by 100 to 200 μm, forming a spatial position dislocation; the long beam (10) is composed of the first long beam The four long beams are respectively located between the four short beams and the isolated island (11) and are 300 μm to 500 μm away from the short beams and the isolated island; the isolated island (11) is arranged at the center of the back side of the film (7); the archipelago (12) is composed of the first archipelago (12-1), the second archipelago (12-2), the third archipelago (12-3) and the fourth archipelago (12-4), which are evenly distributed on the back side of the film (7) and correspond to the front archipelago (6); The Wheatstone bridge is specifically: the first varistor strip (3-1), the second varistor strip (3-2), the third varistor strip (3-3) and the fourth varistor strip (3-4) are connected by metal leads (4) and pads (5) to form a Wheatstone bridge; the first varistor strip (3-1) is connected to the first pad (5-1) and the second pad (5-2) by the first metal lead (4-1) and the second metal lead (4-2); the second varistor strip (3-2) is connected to the first pad (5-1) and the second pad (5-2) by the first metal lead (4-1) and the second metal lead (4-2) respectively; The third metal lead (4-3) and the fourth metal lead (4-4) are connected to the second pad (5-2) and the third pad (5-3); the third varistor strip (3-3) is connected to the fourth pad (5-4) and the fifth pad (5-5) through the fifth metal lead (4-5) and the sixth metal lead (4-6); the fourth varistor strip (3-4) is connected to the fifth pad (5-5) and the first pad (5-1) through the seventh metal lead (4-7) and the eighth metal lead (4-8).

4. The step cross beam island dislocation film high overload pressure sensor chip according to claim 3, characterized in that: The Wheatstone bridge is a semi-open loop Wheatstone bridge, and the open loop of the Wheatstone bridge is used to connect to an external resistor.

5. The step cross beam island dislocation film high overload pressure sensor chip according to claim 3, characterized in that: The five pads are all squares with a side length of 300 μm to 500 μm, wherein the first pad (5-1), the second pad (5-2), the third pad (5-3) and the fifth pad (5-5) are located at the four corners of the edge of the film (7), and the center of the pad is 300 μm to 500 μm away from the edge, and the fourth pad (5-4) is located on the left side of the third pad (5-3) at a distance of 700 μm to 1000 μm; The step cross beam (2) on the front side of the film (7) is a two-stage step structure, and fillets are arranged at the steps, with a fillet radius of 50 μm to 100 μm, and the varistor is arranged on the symmetry axis of the step cross beam (2); The step cross beam (2) and islands (6) on the front side of the film (7) have the same thickness, which is 100% to 200% of the film thickness of the film (7); the step cross beam (2), short beam (9), long beam (10) and islands (11) have the same width, which is 200 μm to 300 μm.

6. The step cross beam island dislocation film high overload pressure sensor chip according to claim 3, characterized in that: All islands in the first archipelago (6-1), the second archipelago (6-2), the third archipelago (6-3) and the fourth archipelago (6-4) on the front side of the film (7) and all corresponding islands on the back side are square, with equal side lengths of 200 μm to 300 μm; The short beam (9) on the back of the film (7) is 50 μm to 150 μm away from the bonding surface between the silicon wafer and the glass, and the long beam (10), the island (11) and the archipelago (12) have the same thickness and are 50 μm to 100 μm away from the bonding surface.

7. The step cross beam island dislocation film high overload pressure sensor chip according to claim 1, characterized in that: A through hole (13) is provided in the middle of the glass substrate (8), with a hole diameter of 0.5 mm to 1 mm. The through hole (13) is used to transmit external pressure to the back of the film (7).

8. A method for preparing a high overload pressure sensor chip with a stepped cross beam archipelago dislocation film as described in any one of claims 1 to 7, characterized in that: The following steps are involved: Step 1: Use an N-type 100 crystal double-sided polished silicon wafer for cleaning; Step 2: photolithography is performed on the front side of the cleaned silicon wafer (1) using a varistor mask, and then light boron ion doping is performed by ion implantation to form a first varistor strip (3-1), a second varistor strip (3-2), a third varistor strip (3-3), and a fourth varistor strip (3-4); Step 3, photolithography is performed on the front side of the product obtained in step 2 using an ohmic contact mask, and heavy boron ion doping is performed by ion implantation to form an ohmic contact region (14); Step 4: depositing a silicon nitride layer (15) on the front side of the product obtained in step 3 by using a plasma enhanced chemical vapor deposition process, and etching contact holes (16) by using an ICP technique; Step 5, photolithography is performed on the front side of the product obtained in step 4 using a metal lead mask, magnetron sputtering is performed and peeling is performed to form metal leads (4) and pads (5), and high temperature alloying treatment is performed; Step 6: Photolithography the front side of the product obtained in step 5, using ICP technology to etch out the front stepped cross beams (9) and islands (6); Step 7: Use a back cavity etching mask to perform photolithography on the back side of the product obtained in step 6, and use ICP technology to etch and form short beams (9), long beams (10), isolated islands (11) and archipelagos (12) of the back cavity; Step 8, photolithography the back of the product obtained in step 7, using ICP technology to reduce the thickness of the long beam (10), the island (11) and the archipelago (12); Step 9, performing laser drilling on the BF33 glass substrate (8) to form a through hole (13); Step 10: Anodically bond the silicon wafer substrate (1) produced in step 8 to the glass substrate (8) processed in step (9) to obtain a high overload pressure sensor chip.

9. The method for preparing the stepped cross beam island dislocation film high overload pressure sensor chip according to claim 8, characterized in that: After the step 2 is completed, the silicon wafer is annealed to make the impurity doping concentration of the varistor strip (3) more uniform.

10. The method for preparing the stepped cross beam island dislocation film high overload pressure sensor chip according to claim 8, characterized in that: After the step 3 is completed, the silicon wafer is annealed to make the impurity doping concentration of the ohmic contact region (14) more uniform.

Citation Information

Cited By

  • Micro electric field sensing device based on electrostatic force and piezoresistive effect coupling

    CN119246976A

  • Inverted MEMS three-dimensional force sensor and decoupling method thereof