IGBT device and manufacturing method thereof

By adopting specific trench structures and material configurations in IGBT devices, the problem of difficult to take into account in the prior art is solved, and high-performance IGBT devices are realized, suitable for high-voltage and high-frequency applications.

CN118712218BActive Publication Date: 2024-11-12SHENZHEN GUANYU SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411210616.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-12
Estimated Expiration
2044-08-30

AI Technical Summary

Technical Problem

Existing IGBT devices are difficult to simultaneously improve shutdown speed and stable voltage tolerance, limiting their application in high-performance power electronic systems.

Method used

An IGBT device structure is adopted, including epitaxially growing an N+ type buffer layer, an N-type drift well layer, an N+ type etching relieving layer and a P-type body well layer on a semiconductor substrate, and several gate trenches and emissions are provided therein. The electrode trench is controlled by the configuration of P-pillar and gate filler with a speed difference epitaxial growth, so as to enhance the internal electric field and PN junction barrier of the P-type body well layer, and improve the opening and closing. speed while maintaining stable voltage tolerance.

Benefits of technology

It achieves the improvement of the on-off speed and shutdown speed of IGBT devices while maintaining stable voltage tolerance, enhancing the performance and stability of the device, and is suitable for high-voltage, high-current and high-frequency application scenarios.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118712218B_ABST
    Figure CN118712218B_ABST
Patent Text Reader

Abstract

The invention relates to an IGBT device and a manufacturing method thereof. The device has a gate groove and an emitter groove, and includes a semiconductor substrate, an IGBT device working layer region grown by covering epitaxial growth, a P column of a PNP tube grown by differential speed epitaxial growth in the emitter groove, and a gate filling body grown in the gate groove; the P column protrudes upward from an N+ type source layer, and based on the groove width setting of the same etching process, the emitter groove can be shallow and does not penetrate the P type body well layer, the gate oxide layer does not cover the inner groove bottom of the emitter groove, and the P column is arranged on the P type body well layer and protrudes upward from the N+ type source layer. The key step among steps S1 to S7 of the manufacturing method is S5, which adopts differential speed epitaxial growth of the P column of the PNP tube and simultaneously grows the gate filling body. The semiconductor substrate based on a specific layer, the groove structure of different designs, and the optimized gate and emitter configuration can ensure that the device opening speed and the closing speed are improved, and the voltage bearing capacity of the device is stabilized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor devices, and in particular to an IGBT device and a manufacturing method thereof, wherein IGBT refers to an insulated gate bipolar transistor (Insulated Gate Bipolar Transistor). Background Art

[0002] The main application of IGBT devices is in power electronic conversion systems that require high performance, such as motor control, power conversion, and renewable energy systems. As a core component in the field of power electronics, IGBT devices are used in various power conversion and control systems. The traditional IGBT manufacturing process usually forms a P+ body well by ion diffusion in the N-type drift well formed by ion diffusion, and increases the N-type ion concentration of the N-type drift well to increase the turn-off speed, but it often leads to an unstable decrease in the voltage tolerance of the IGBT device; if the N-type ion concentration of the N-type drift well is reduced or the thickness of the N-type drift well is increased, the voltage tolerance of the IGBT device can be improved, but the turn-off speed is reduced in the opposite direction. In addition, when P+ ions are injected into the N-type drift well to form the P-well region, it is necessary to ensure that the doping concentration of P+ is higher than that of the N-type drift well. The doping concentration of the P+ body well usually needs to be 5 to 10 times that of the N-type drift well, so that the original doping of the N-type drift well can be compensated to effectively form a P-type well region that can establish an N-type conductive channel. Therefore, in the traditional IGBT structure, the configuration and optimization of the region often cannot meet the requirements of high-speed switching and high voltage tolerance at the same time.

[0003] IGBT devices are mainly divided into planar gate structures and trench gate structures. Regarding IGBT devices with planar gate structures, semiconductor power devices also include metal oxide field effect transistors (MOSFETs), and the channel between the source and drain of the MOSFET is a surface; for example, the invention patent publication number CN101478000A discloses an improved sawtooth electric field drift region structure for power semiconductor devices, and the semiconductor power device further includes a plurality of rows of horizontal columnar thin layers with alternating conductive forms on the drift region of the semiconductor substrate, and the thickness of each thin layer ensures that the thin layer can be broken down when the semiconductor power device is turned on. In a specific embodiment, the thickness of the thin layer satisfies the charge balance formula: q*ND*WN=q*NA*WP and the breakdown condition WP<2*WD*[ND / (NA+ND), where ND and WN represent the doping concentration and thickness of the N-type layer, and NA and WP represent the doping concentration and thickness of the P-type layer; WD represents the depletion width; q represents the electron charge, which can offset each other. The device achieves a near ideal rectangular electric field distribution and sawtooth-like edges (ridges) at the breakdown voltage. In the related art, the common defect of the planar gate structure IGBT device is that the number of MOSFET transistors that can be configured on a surface is limited. This is because the surface channel occupies the surface space of the chip. Usually, a patterned P-body well region is formed on the N-type drift well layer, and an N+ type source region is formed in the P-body well region. The emitter metal is arranged on the N+ type source region. The portion of the P-body well region between the N+ type source region and the surface region of the N-type drift well layer is covered with a gate oxide layer, and a gate metal is arranged above the gate oxide layer in this region. A plurality of layers of alternating P-type horizontal columns and N-type horizontal columns (in series) are arranged below the N-type drift well layer to generate a horizontal electric field in the epitaxial growth layer. However, with the miniaturization of semiconductor devices, how to arrange more parallel MOSFET transistors under the limited chip surface size is a continuous development technology trend. In addition, the voltage tolerance of the IGBT device depends on the N concentration of the N-type drift well layer. Although the reduction of the N concentration will increase the voltage tolerance, it will reduce the turn-off speed. On the contrary, when the N concentration increases, increasing the number of thin layers of alternating P-type horizontal columns and N-type horizontal columns to compensate for the voltage tolerance will also weaken the turn-off speed of the IGBT device. This is because the multi-layer PN alternating structure increases the carrier transmission path inside the device, thereby increasing the delay time during the switching process, and the increase in voltage resistance also increases the capacitance effect inside the device.

[0004] Regarding the IGBT device with a trench gate structure, the channel between the source and drain of the MOSFET is vertical, so as to arrange a larger number of parallel MOSFET transistors; for example, the invention patent publication number CN108538912A discloses a trench step gate IGBT chip, including a substrate and a trench gate located in the surface of the substrate, the gate oxide layer of the trench gate is composed of different gate oxide thicknesses, and the gate oxide thickness of the real gate gate oxide layer located above is less than the gate oxide thickness of the real gate gate oxide layer located below. Therefore, the effective channel working area of ​​the trench step gate IGBT chip adopts a relatively thin gate oxide layer, and a relatively thick gate oxide layer is adopted at the bottom of the trench. The trench gate structure can improve the chip density, reduce the conduction loss and enhance the gate's control ability over the switch. In the related technology, the channel is located in the P-well region on both sides of the trench. If the gate trench passes through the P-well region, the N-well region (equivalent to the N-type drift well layer) and reaches the N-type substrate, that is, the trench gate divides the N-type drift well layer into multiple drift well cells and is affected by the electric field on the trench side, when the collector and the emitter are turned on, the N-type drift well layer loses the function of the equivalent PNP tube in the IGBT chip, and the device characteristics are more inclined to MOSFET chips, so it is only suitable for medium and low voltage chip applications. In addition, the gate oxide thickness of the gate oxide layer on both sides of the trench must be thin on the upper side and thick on the lower side, and the thickness change connection point must be controlled to be located between the upper P-well region (channel formation layer) and the lower N-well region (N-type drift well layer), which is difficult to manufacture.

[0005] In the current IGBT devices, the manufacturing of the grooves of the MOSFET transistors has the problem of unstable electrical performance due to the impact on other components in the chip. In addition, for example, in the semiconductor devices and manufacturing methods disclosed in the invention patent publications CN1430793A and CN106252396A, the gate grooves in the trench gate structure IGBT devices are deep enough to penetrate the P-type body well layer formed by the channel until it extends to the N-type drift well layer, and even penetrate the N-type drift well layer. This is the inherent thinking in this field, but it does not take into account the impact of the MOSFET gate on other electrical components of the chip and the etching defects of the deep gate grooves. Therefore, while the current technical solutions improve the turn-off speed of the IGBT device, it is often difficult to stabilize its voltage tolerance, which limits the application of IGBT devices in high-performance scenarios. Summary of the invention

[0006] The main purpose of the present invention is to provide an IGBT device, the main improvement of which is to solve the problem of increasing the turn-off speed of the IGBT device but failing to stabilize the voltage tolerance of the device in an architecture that integrates multiple parallel trench MOSFET transistors in the IGBT device.

[0007] The second main purpose of the present invention is to provide a method for manufacturing an IGBT device, which can prepare an IGBT device with a new architecture and take into account both improving the shutdown speed and stabilizing the voltage tolerance of the device.

[0008] The main purpose of the present invention is achieved through the following technical solutions:

[0009] An IGBT device is provided, comprising:

[0010] A semiconductor substrate having a P-type implantation layer;

[0011] The IGBT device working layer region is epitaxially grown on the P-type injection layer of the semiconductor substrate; wherein the IGBT device working layer region includes an N+ type buffer layer, an N-type drift well layer, an N+ type etching relief layer, a P-type body well layer and an N+ type source region layer sequentially located on the P-type injection layer; wherein the N+ type etching relief layer is disposed between the P-type body well layer and the N-type drift well layer, and a plurality of gate trenches and an emitter trench between two adjacent gate trenches are simultaneously opened in the IGBT device working layer region; according to the difference in trench opening pattern and trench width, the emitter trench is relatively enclosed in the gate trench and is not connected, the gate trench penetrates the N+ type source region layer and the P-type body well layer and stops at the N+ type etching relief layer, and the emitter trench penetrates the N+ type source region layer and stops at the P-type body well layer or the N+ type etching relief layer;

[0012] A gate oxide layer, covering the inner sidewall and the bottom of the gate trench;

[0013] A P column and a gate filling body grown by speed differential epitaxy, wherein the P column is arranged on the inner groove bottom of the emitter groove and connected to the P-type body well layer, the gate filling body is arranged in the gate groove, and the P column protrudes upward from the N+ type source layer relative to the gate filling body;

[0014] An interlayer film is formed on the gate filling body to isolate the gate filling body from the P column;

[0015] The emitter metal layer is disposed on the N+ type source region layer, the interlayer film and the P column. The emitter metal layer connects the N+ type source region layer and the P column at individual locations.

[0016] By adopting the above-mentioned structural technical solution, utilizing the configuration relationship between the P column and the gate filling body grown by differential speed epitaxial growth and the N+ type etching relief layer interposed between the P type body well layer and the N type drift well layer, the gate trench can stop at the N+ type etching relief layer, and the emitter trench can stop at the P type body well layer or the N+ type etching relief layer, depending on the groove opening pattern and the groove width difference, the depth of the emitter trench is precisely controlled not to be greater than the depth of the gate trench, so that the P column arranged on the inner groove bottom of the emitter trench can be connected to the P type body well layer, and the P column protrudes upward from the N+ type source region layer relative to the gate filling body to increase the combination with the emitter metal layer, the P column can improve the internal electric field of the P type body well layer, and combined with the N+ type etching relief layer, the PN junction barrier in contact with the P type body well layer can be enhanced (the depletion layer becomes thicker), and there is a high impedance between the N+ type etching relief layer and the P type body well layer. Combined with the gate filler of differential epitaxial growth (single crystal growth rate is slower than P column) and the N-type drift well layer is part of the epitaxial structure layer and the N-type concentration is increased from N-type, the excess carriers are quickly eliminated, and the turn-on and turn-off speeds of the IGBT are improved. Therefore, the PN junction internal resistance when the channel is closed can be increased, and a low on-state voltage drop and high current density can be maintained in the on state, so as to achieve stable voltage tolerance while improving the turn-on and turn-off speeds.

[0017] In a preferred example, the present invention can be further configured as follows: the semiconductor substrate includes a collector single crystal layer located below the P-type injection layer, and the IGBT device also includes: a collector metal, which is covered and arranged on the back side of the semiconductor substrate to connect the collector single crystal layer.

[0018] By adopting the above-mentioned preferred technical features, the collector metal is used to connect the collector single crystal layer to establish the bottom surface structure of the IGBT device, thereby realizing the connection between the collector of the IGBT device and the external circuit, so as to improve the electrical performance and reliability of the IGBT device and make the device have better stability and durability in harsh environments such as high voltage and high current.

[0019] In a preferred example, the present invention may be further configured as follows: the top surface of the gate filling body is relatively recessed from the upper surface of the N+ type source region layer, so as to facilitate the patterning of the gate oxide layer before the interlayer film is deposited.

[0020] By adopting the above-mentioned preferred technical features, by making the top surface of the gate filling body relatively recessed in relation to the upper surface of the N+ type source layer, the additional anti-etching mask formation step is reduced during the gate oxide patterning process before the interlayer film deposition, or / and the recessing of the gate filling body can prevent cross-contamination of areas that do not need to be covered during the interlayer film deposition process. When an error occurs between the pattern of the interlayer film and the gate groove, the top surface of the gate filling body is still covered with a portion of the interlayer film, which can expand and improve the performance of the IGBT device and the accuracy requirements of the interlayer film patterning during the manufacturing process, and prevent the reduction of leakage between the gate and the emitter.

[0021] In a preferred example, the present invention may be further configured as follows: the width of the emitter trench is greater than the width of the gate trench, so as to reduce the depth of the emitter trench.

[0022] By adopting the above preferred technical features, the width and depth of the emitter trench are optimized to reduce the conduction loss and improve the performance of the IGBT device. In the IGBT design, by adjusting the width of the emitter trench to be greater than the width of the gate trench, the depth of the emitter trench is effectively reduced when the gate trench reaches a satisfactory depth in the same trench etching process. The depth of the gate trench stops at the N+ type etching relief layer. During etching, the N-type ions in the N+ type etching relief layer are monitored in the etching chamber and their concentration increases sharply, which can serve as an etching stop signal. There are three reasons for reducing conduction loss. First, as the width of the emitter trench increases, the effective width of the conductive channel increases accordingly, which helps to reduce the impedance of the current in the conductive channel of the P-type body well layer on the trench side. At the same time, the P-type body well layer and the N+ type etching relief layer increase in the opposite direction, thereby reducing conduction loss. Second, the wider emitter trench is beneficial to increase the carrier concentration and optimize the carrier distribution of the P-type body well layer when the device is turned on, thereby improving the conductivity modulation efficiency and further reducing conduction loss. Third, the vertical trench structure can eliminate the JFET effect, that is, eliminate the impedance in the horizontal current path, thereby reducing the overall voltage drop and conduction loss.

[0023] In a preferred example, the present invention can be further configured as follows: based on the width of the emitter trench being greater than the width of the gate trench, the emitter trench only penetrates the N+ type source region layer and ends at the P type body well layer, the gate oxide layer also includes an isolation oxide layer covering the side walls of the emitter trench, and the isolation oxide layer does not cover the inner bottom of the emitter trench.

[0024] By adopting the above-mentioned preferred technical features and optimizing the structure of the emitter trench and the configuration of the isolation oxide layer as above, the conduction loss of the channel can be reduced, the current density can be increased, the electron injection efficiency of the P-type body well layer can be optimized, the heat loss can be reduced, the voltage resistance performance can be enhanced, and the process steps can be reduced. It is suitable for IGBT devices in high voltage, high current and high frequency application scenarios.

[0025] In a preferred example, the present invention can be further configured as follows: the P column protrudes from the N+ type source layer, and the inner bottom of the emitter trench exposes the P type body well layer, so that the P column is directly connected to the P type body well layer; the gate trench and the emitter trench have a concave arc surface on the inner side wall of the P type body well layer.

[0026] By adopting the above preferred technical features, the bottom of the P column is directly connected to the P-type body well layer, eliminating the oxide layer isolation at the bottom of the groove, making the current conduction path more direct and reducing the on-resistance; the top of the P column protrudes to increase the bonding area with the emitter. This improves the electrical performance and reliability of the IGBT device, simplifies the IGBT device manufacturing process, and improves the overall efficiency of the system.

[0027] In a preferred example, the present invention can be further configured as follows: the depth of the emitter trench stops at the N+ type etching relief layer, and a P-type column bottom junction is formed below the inner bottom of the emitter trench so that the P column is indirectly connected to the P-type body well layer.

[0028] By adopting the above-mentioned preferred technical features, the formation of the P-type column bottom junction is utilized to effectively block the direct contact between the P column and the N-type drift well layer. When the IGBT is turned on, the unnecessary hole carriers injected by the P column into the N-type drift well layer are reduced, and the P-type column bottom junction more accurately controls the distribution of minority carriers in the N-type drift well layer, thereby optimizing the conductivity modulation effect. When the IGBT is turned off, the P column does not directly contact the N-type drift well layer, and the formation of the P-type column bottom junction can effectively avoid the punch-through phenomenon caused under high voltage, thereby enhancing the stability of the IGBT device under high voltage environment.

[0029] In a preferred example, the present invention can be further configured as follows: a P-type gate bottom junction is formed below the inner bottom of the gate trench to pattern the N+ type etching mitigation layer.

[0030] By adopting the above-mentioned preferred technical features, through the formation of a P-type gate bottom junction, on the one hand, the conductivity on both sides of the bottom of the gate trench is effectively enhanced to ensure that the current is evenly distributed at the bottom of the gate trench, thereby improving the conductivity stability of the entire IGBT device when it is turned on, and helping to shorten the opening and closing time of the IGBT device. In other words, it helps to reduce the local dynamic loss of the IGBT device during the switching process, reduce the current tailing phenomenon during the switching transient process, and improve the switching efficiency of the device. On the other hand, it helps to homogenize the electric field distribution of the N-type drift well layer in the IGBT device, avoid early breakdown caused by excessive local electric field, increase the breakdown voltage, and enhance the voltage resistance of the IGBT device.

[0031] The second main purpose of the present invention is achieved by the following technical solution: a method for manufacturing an IGBT device is proposed, which can be used to prepare an IGBT device with the above possible technical feature combination, comprising:

[0032] S1, providing a semiconductor substrate having a P-type injection layer;

[0033] S2, a blanket epitaxially grown IGBT device working layer region is on the P-type injection layer of the semiconductor substrate; wherein the IGBT device working layer region includes an N+ type buffer layer, an N-type drift well layer, an N+ type etching relief layer, a P-type body well layer, and an N+ type source region layer formed by epitaxial growth or ion diffusion on the P-type body well layer; wherein the N+ type etching relief layer is disposed between the P-type body well layer and the N-type drift well layer;

[0034] S3, simultaneously opening a plurality of gate trenches and an emitter trench between two adjacent gate trenches in the working layer area of ​​the IGBT device; according to the difference in trench opening pattern and trench width, the emitter trench is relatively enclosed in the gate trench and is not connected, the gate trench penetrates the N+ type source region layer and the P type body well layer and stops at the N+ type etching relief layer, and the emitter trench penetrates the N+ type source region layer and stops at the P type body well layer or the N+ type etching relief layer;

[0035] S4, forming a gate oxide layer on the N+ type source layer, the gate oxide layer also covering the inner sidewalls and the inner groove bottom of the gate groove and the emitter groove; after step S4, comprising: S41, removing the portion of the gate oxide layer at the inner groove bottom of the emitter groove to expose the P type body well layer;

[0036] S5, setting a P column on the inner groove bottom of the emitter groove, and setting a gate filling body in the gate groove; the P column protrudes upward and penetrates the N+ type source region layer, and the top surface of the gate filling body is relatively recessed in the upper surface of the N+ type source region layer; wherein step S5 comprises: S51, differential speed epitaxial growth of the P column of the PNP tube on the inner groove bottom of the emitter groove and simultaneously growing the gate filling body in the gate groove, the P column connecting the P type body well layer, and a P+ connection layer is also formed on the gate oxide layer on the N+ type source region layer, integrally connecting the P column and the gate filling body; S52, based on the portion of the gate oxide layer formed on the N+ type source region layer as the bottom mask, selectively etching and removing the P+ connection layer to separate the gate filling body from the P column; S53, using the gate filling body and the P column as masks, etching and removing the portion of the gate oxide layer formed on the N+ type source region layer;

[0037] S6, forming an interlayer film on the gate filling body to isolate the gate filling body from the P column;

[0038] S7, disposing an emitter metal layer on the N+ type source region layer, the interlayer film and the P column, wherein the emitter metal layer connects the N+ type source region layer and the P column at individual locations.

[0039] By adopting the above method and technical solution, the step S51 of growing the P column of the PNP tube on the bottom of the inner groove of the emitter groove by speed differential epitaxy and growing the gate filling body in the gate groove at the same time is conducive to forming an interlayer film with good isolation effect in step S6, avoiding the short circuit between the P column and the gate filling body. In addition, the step S52 of removing the P+ connection layer by selective etching effectively separates the gate filling body from the P column, further improving the reliability and stability of the IGBT device.

[0040] In a preferred example, the present invention can be further configured as follows:

[0041] In step S1, the semiconductor substrate includes a collector single crystal layer located below the P-type injection layer; the manufacturing method of the IGBT device further includes: S8, coveringly arranging a collector metal on the back side of the semiconductor substrate to connect the collector single crystal layer;

[0042] In step S6 , the interlayer film is patterned to correspond to the trench opening of the gate trench.

[0043] By adopting the preferred technical scheme of the above method, a collector single crystal layer is provided through step S1, and the collector single crystal layer is included under the P-type injection layer in the semiconductor substrate, which is helpful to form a stable collector contact in the subsequent steps and optimize the electrical performance of the IGBT device; the existence of the collector single crystal layer can optimize the current distribution, reduce the local current over-density phenomenon, and improve the short-circuit capability and stability of the device; through the etching back process of the gate filling body in step S51, the top surface of the gate filling body is relatively recessed in the upper surface of the N+ type source layer, which helps to reduce the parasitic capacitance between the gate and the emitter and improve the switching speed and efficiency of the device; through the interlayer film patterning in step S6, the patterning of the interlayer film corresponds to the groove opening of the gate groove, and an effective isolation structure is formed in the IGBT device to prevent unnecessary coupling between the gate and the emitter and improve the anti-interference ability of the device; through the collector metal covering ground setting in step S8 to connect the collector single crystal layer, a good back-side contact can be provided, the contact resistance can be reduced, and the current injection efficiency can be improved. The setting of collector metal also helps to improve the thermal management of IGBT devices. The metal layer can act as a heat diffusion layer to help heat conduct from the inside of the chip to the outside faster, thereby improving the thermal stability of the device.

[0044] In a preferred example, the present invention can be further configured as follows:

[0045] In step S3, according to the same etching process of the groove opening pattern, the width of the emitter groove is greater than the width of the gate groove, and the depth of the emitter groove is less than the depth of the gate groove, so that the inner bottom of the emitter groove does not extend to the N+ type etching relaxation layer; in step S41, the inner bottom of the emitter groove exposes the P-type body well layer; in step S5, the P column is directly connected to the P-type body well layer.

[0046] By adopting the preferred technical scheme of the above method, in step S3, the width of the emitter groove is greater than the width of the gate groove, and its depth is less than the depth of the gate groove, so that the inner bottom of the emitter groove does not extend to the N+ type etching relaxation layer, thereby ensuring effective isolation between the emitter groove and the gate groove during the manufacturing process and reducing the risk of short circuit; in step S41, by removing part of the gate oxide layer at the bottom of the inner groove of the emitter groove, the P-type body well layer is exposed. This step helps to achieve direct connection between the P column and the P-type body well layer in the subsequent step S5, reduce the recombination loss of electrons and holes inside the device, and thus improve the overall performance of the IGBT device.

[0047] Alternatively, the present invention can be further configured as follows in a preferred example:

[0048] In step S3, the depth of the emitter trench stops at the N+ type etching relaxation layer; after step S4, it also includes: S42, forming a P-type column bottom junction below the inner groove bottom of the emitter trench; in step S5, the P column is indirectly connected to the P-type body well layer; the gate trench and the emitter trench have a concave arc surface on the inner side wall of the P-type body well layer;

[0049] After step S4, the method further includes: S43, forming a P-type gate bottom junction below the inner groove bottom of the gate groove, wherein the P-type gate bottom junction is used to pattern the N+ type etching relaxation layer.

[0050] By adopting the preferred technical scheme of the above method, in the manufacturing process of the IGBT device, the formation step S42 of the P-type column bottom junction and the formation step S43 of the P-type gate bottom junction are introduced. The P-type column bottom junction effectively avoids partial over-etching of the emitter trench, which causes the upper P column of the PNP tube to be unable to connect to the P-type body well layer of the MOSFET transistor; the P-type gate bottom junction patterns the N+ type etching relaxation layer, effectively improving the gate bottom electric field, which is beneficial to the stable operation of the IGBT device under high current and high temperature conditions.

[0051] In summary, the present invention includes at least one of the following technical effects that contribute to the prior art:

[0052] 1. Compared with the existing technology, the traditional trench gate structure IGBT device structure cannot meet the requirements of high-speed switching and stable voltage tolerance at the same time, which limits its application in high-performance power electronic systems. This technical solution uses a unique trench structure design to achieve the improvement of the turn-on and turn-off speeds of the trench gate structure IGBT device while maintaining the stable voltage tolerance of the IGBT device.

[0053] 2. By using an emitter trench with a width greater than that of the gate trench and an N+ type etching mitigation layer disposed between the P-type body well layer and the N-type drift well layer, the same process can be used to prevent the gate oxide layer from covering the bottom of the emitter trench, and to unify the depth of multiple gate trenches so that they do not penetrate into the N-type drift well layer. The N-type drift well layer has a stable internal resistance due to its complete epitaxial growth thickness that is not penetrated by the gate trench, and the IGBT device can withstand voltage fluctuations more stably when operating at high voltage and high frequency. In a preferred example, the N-type drift well layer is formed under the P-column and directly connected to the P-type body well layer, or / and the P-type body well layer forms a P-type gate bottom junction under the insufficiently etched gate trench, further improving the performance and stability of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0054] Figure 1 A partial cross-sectional schematic diagram of an IGBT device in a first embodiment of the present invention is shown;

[0055] Figure 2 A partial top view schematically shows that the emitter trench of the IGBT device is relatively enclosed in the gate trench and is not connected in the first embodiment of the present invention;

[0056] Figure 3 A block flow chart of a method for manufacturing an IGBT device according to an embodiment of the present invention is shown;

[0057] Figure 4 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Schematic diagram of components of step S1;

[0058] Figure 5 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Schematic diagram of components of step S2;

[0059] Figure 6 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Schematic diagram of components of step S3;

[0060] Figure 7 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Schematic diagram of components of step S4;

[0061] Figure 8 The corresponding embodiment of the present invention is shown in FIG. Figure 3Schematic diagram of components of step S41 after step S4;

[0062] Fig. 9 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Component diagram of step S51 in step S5;

[0063] Fig.10 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Component diagram of step S52 in step S5;

[0064] Fig.11 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Component diagram of step S53 in step S5;

[0065] Fig.12 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Schematic diagram of components of step S6;

[0066] Fig.13 The corresponding embodiment of the present invention is shown in FIG. Figure 3 Component diagram of step S7;

[0067] Fig.14 A partial cross-sectional schematic diagram of an IGBT device according to a second embodiment of the present invention is shown.

[0068] Reference numerals:

[0069] 10. semiconductor substrate; 11. P-type injection layer; 12. collector single crystal layer;

[0070] 20. IGBT device working layer area; 21. N+ type buffer layer; 22. N type drift well layer;

[0071] 23. N+ type etching relaxation layer; 24. P type body well layer; 25. N+ type source region layer;

[0072] 30. Gate trench; 31. Gate filling body; 32. P-type gate bottom junction; 33. P+ connection layer;

[0073] 40. emitter trench; 41. P column; 42. P-type column bottom junction;

[0074] 50. gate oxide layer; 51. isolation oxide layer;

[0075] 60. Interlayer film; 70. Emitter metal layer; 80. Collector metal. DETAILED DESCRIPTION

[0076] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments for understanding the inventive concept of the present invention, and cannot represent all the embodiments, nor are they interpreted as the only embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field on the premise of understanding the inventive concept of the present invention are within the scope of protection of the present invention.

[0077] It should be noted that if there are directional indications (such as up, down, left, right, front, back, etc.) involved in the embodiments of the present invention, the directional indications are only used to explain the relative position relationship, movement, etc. between the components in a certain specific posture. If the specific posture changes, the directional indications will also change accordingly. In order to facilitate the understanding of the technical solution of the present invention, an IGBT device and a manufacturing method thereof of the present invention are further described and explained in detail below, but they are not limited to the protection scope of the present invention.

[0078] The drawings only illustrate the common parts of multiple embodiments, and the parts with differences or distinctions are described in text or presented in comparison with the drawings. Therefore, based on the industrial characteristics and technical essence, technicians familiar with the field should correctly and reasonably understand and judge whether the individual technical features described below or any combination of them can represent the same embodiment, or whether multiple technical features with mutually exclusive technical essences can only represent different variant embodiments respectively. Embodiments with too similar drawings will not be drawn repeatedly.

[0079] The "overlay epitaxial growth" mentioned in the article refers to epitaxial growth on a plane. The film layer formed is a semiconductor single crystal structure. The epitaxial growth structure on the single crystal substrate has a different crystal orientation from the epitaxial growth structure on the insulating layer. The film layer structure is similar to the external extension of the original crystal. The difference between "N+ type" and "N type" in semiconductor conductivity type is that the N-type doping concentration of pentavalent elements doped in N+ type semiconductor is higher and the conductivity is also better. The pentavalent element is usually phosphorus (P) or arsenic (As). With electrons as carriers, the Fermi level of N+ type semiconductor is closer to the conduction band; usually the doping concentration of N-type semiconductor is 10 14 ~10 16 / cm³, while the doping concentration of N+ semiconductors can be as high as 10 18 ~10 21 Pieces / cm³.

[0080] The "speed differential epitaxial growth" mentioned in the article refers to two patterned epitaxial growths at different epitaxial growth rates; usually, the epitaxial growth structure on the insulating layer has a slower epitaxial growth rate than the epitaxial growth structure on the single crystal substrate. For example, the epitaxial growth rate of the gate filler 31 is slower than the epitaxial growth rate of the P column 41, and the crystal orientations of the two are generally different, which can produce different etching selectivity ratios (not 1:1).

[0081] Reference Figure 1 and Figure 2 The first embodiment of the present invention discloses an IGBT device having a gate trench 30 and an emitter trench 40 between two adjacent gate trenches 30. The IGBT device includes: a semiconductor substrate 10 having a P-type injection layer 11, an IGBT device working layer region 20 epitaxially grown on the semiconductor substrate 10, a gate oxide layer 50 covering the gate trench 30, a P column 41 epitaxially grown in the emitter trench 40 at a differential speed and a gate filling body 31 epitaxially grown in the gate trench 30, an interlayer film 60 formed on the gate filling body 31, and an emitter metal layer 70 arranged on the IGBT device working layer region 20. The P column 41 is used to connect the P-type body well layer 24 and the emitter metal layer 70 in the working layer area 20 of the IGBT device. The gate filler 31 and the P column 41 are formed together in the same epitaxial process but have different epitaxial growth rates. The epitaxial growth rate of the P column 41 is greater than the epitaxial growth rate of the gate filler 31, so the epitaxial growth length of the P column 41 is greater than the epitaxial growth length of the gate filler 31. The P column 41 can protrude from the working layer area 20 of the IGBT device. The depth of the emitter trench 40 should be less than or equal to the depth of the gate trench 30. In the first embodiment, the depth of the emitter trench 40 is less than the depth of the gate trench 30.

[0082] The P-type injection layer 11 of the semiconductor substrate 10 serves as the lower P end of the equivalent PNP tube in the IGBT device circuit, and is used to connect to the collector (C) of the IGBT circuit. The material of the semiconductor substrate 10 can be silicon or silicon carbide. The IGBT device working layer region 20 is epitaxially grown on the P-type injection layer 11 of the semiconductor substrate 10. Among them, the IGBT device working layer region 20 includes an N+ type buffer layer 21, an N-type drift well layer 22, an N+ type etching relief layer 23, a P-type body well layer 24 and an N+ type source region layer 25, which are sequentially located on the P-type injection layer 11. Through the conductivity modulation effect, the N+ type buffer layer 21 mainly plays the role of reducing the conduction voltage drop and improving the device efficiency. Based on the thickness and doping concentration of the N-type drift well layer 22, the N-type drift well layer 22 mainly plays the role of withstanding high voltage and reducing power consumption. The gate trench 30 will not penetrate into the N-type drift well layer 22 to weaken its performance. The thickness of the N-type drift well layer 22 remains consistent to stabilize the high voltage resistance, provide a longitudinal high impedance region to support high voltage operation and optimize the switching characteristics of the IGBT device. Therefore, the N-type drift well layer 22 can be determined to be N-type or N-type during the epitaxial growth stage. The thickness of the N-type drift well layer 22 is not affected by the trench and can determine the N-pole characteristics of the PNP tube.

[0083] Among them, the N+ type etching mitigation layer 23 is disposed between the P type body well layer 24 and the N type drift well layer 22. The N+ type etching mitigation layer 23 mainly plays the role of mitigating the etching depth of the gate trench 30. When the depth of the gate trench 30 is etched to the N+ type etching mitigation layer 23 during the etching process with a high etching selectivity ratio for the P type body well layer 24, the etching rate will be slowed down, and a large number of N type ions will appear in the etching chamber and can be detected to stop etching. Therefore, the depth of multiple gate trenches 30 can be effectively controlled to stop at the N+ type etching mitigation layer 23, and the N type drift well layer 22 can remain intact.

[0084] The P-type body well layer 24 is disposed between the N+ type etching relief layer 23 and the N+ type source layer 25. The P-type body well layer 24 mainly plays the role of providing a longitudinal channel of the MOSFET, and the channel is located on both sides of the gate trench 30, connecting the N+ type etching relief layer 23 and the N+ type source layer 25. The doping degree and thickness of the P-type body well layer 24 will directly affect the switching rate of the IGBT device. The epitaxially grown P-type body well layer 24 has a consistent thickness. Compared with the P-type body well junction formed by traditional ion implantation, the P-type body well layer 24 has better stability. The P-type ions of the P-type body well layer 24 will not be implanted into the N-type drift well layer 22, so it will not affect the withstand voltage impedance characteristics of the N-type drift well layer 22. The function of the N+ type source layer 25 is to provide electrons to realize the conduction control of the IGBT device.

[0085] The plurality of gate trenches 30 in the working layer region 20 of the IGBT device and the emitter trench 40 between two adjacent gate trenches 30 are formed simultaneously. Figure 2 The emitter trench 40 is relatively enclosed in the gate trench 30 and is not connected, and the gate trenches 30 adjacent to each other on both sides of the emitter trench 40 are connected to each other (specifically, as shown in Figure 2 As shown). The gate trench 30 penetrates the N+ type source layer 25 and the P type body well layer 24 and stops at the N+ type etching relief layer 23, and the emitter trench 40 penetrates the N+ type source layer 25 and stops at the P type body well layer 24 or the N+ type etching relief layer 23. In the first embodiment, the emitter trench 40 stops at the P type body well layer 24, that is, the depth of the emitter trench 40 is less than the depth of the gate trench 30. When the width of the emitter trench 40 is greater than the width of the gate trench 30, in the same etching process, the depth of the emitter trench 40 can be less than the depth of the gate trench 30. The gate oxide layer 50 specifically covers the inner sidewall and the inner groove bottom of the gate trench 30. Since the width of the emitter trench 40 is greater than the width of the gate trench 30, the gate oxide layer 50 is easily removed at the bottom of the emitter trench 40.

[0086] The P column 41 and the gate filler 31 are epitaxially grown at different speeds. The P column 41 is arranged on the bottom of the inner groove of the emitter trench 40 and is connected to the P-type body well layer 24. The gate filler 31 is arranged in the gate trench 30. Under the isolation of the gate oxide layer 50, the gate filler 31 is not connected to the P-type body well layer 24. Moreover, the P column 41 protrudes upward from the N+ type source layer 25 relative to the gate filler 31. The gate filler 31 is epitaxially grown based on the insulating material of the gate oxide layer 50, and the P column 41 is epitaxially grown based on the semiconductor material of the P-type body well layer 24. The gate filler 31 and the P column 41 have different crystal orientations and different epitaxial growth rates. The epitaxial growth rate of the P column 41 starting from the bottom of the emitter trench 40 is approximately several times the epitaxial growth rate of the gate filler 31 starting from the bottom of the gate trench 30. The epitaxial growth method includes hydrogen reduction method or direct thermal decomposition method. The P column 41 and the gate filler 31 have the same single crystal semiconductor material, and adopt homoepitaxial technology or heteroepitaxial technology, wherein heteroepitaxial technology means that the semiconductor material of the semiconductor substrate 10 is different from the semiconductor material epitaxially grown by the P column 41 and the gate filler 31, for example, silicon carbide is epitaxially grown on a silicon substrate to form the P column and the gate filler. The type of the P column 41 is P type, P+ type or a combination. In a specific structure, the bottom of the P column 41 is P type and the top can be P+ type. The gate filler 31 can be doped with pentavalent elements (P type elements) to make it have better conductivity.

[0087] The interlayer film 60 is used to isolate the gate filler 31 from the P column 41. The interlayer film 60 covers the top surface of the gate filler 31 and is connected to the gate oxide layer 50. The emitter metal layer 70 is specifically disposed on the N+ type source layer 25, the interlayer film 60 and the P column 41. The emitter metal layer 70 connects the N+ type source layer 25 and the P column 41 at individual locations.

[0088] The implementation principle of this basic embodiment is to utilize the configuration relationship between the P column 41 and the gate filling body 31 grown by differential speed epitaxial growth and the N+ type etch relief layer 23 disposed between the P type body well layer 24 and the N type drift well layer 22. According to the design of the groove opening pattern and the groove width difference, the depth of the emitter groove 40 can not exceed the depth of the N+ type etch relief layer 23. The emitter groove 40 stops at the P type body well layer 24 or the N+ type etch relief layer 23. The depth of the emitter groove 40 is precisely controlled so that the P column 41 disposed on the inner groove bottom of the emitter groove 40 can be connected to the P type body well layer 24, and the P column 41 protrudes upward from the N+ type source layer 25 relative to the gate filling body 31, so as to increase the bonding strength between the P column 41 and the emitter metal layer 70 and reduce the metal diffusion to the P type body well layer 24. On the one hand, the P-column 41 connected to the emitter metal layer 70 can improve and uniformly stabilize the internal electric field of the P-type body well layer 24. The characteristic combination of the P-type body well layer 24 with changed internal electric field and the N+ type etching relief layer 23 can enhance the PN junction barrier in contact with the P-type body well layer 24 (the depletion layer becomes thicker). The depletion layer at the interface between the P-type body well layer 24 with changed internal electric field and the N+ type source layer 25 will not become thinner, and the interface between the N+ type etching relief layer 23 and the P-type body well layer 24 exhibits high impedance. On the other hand, since the gate filler 31 (the single crystal growth rate of the gate filler 31 is slower than that of the P column 41) grown by differential epitaxy and the N-type drift well layer 22 are part of the epitaxial structure layer and the N-type concentration is increased from that of the N-type, and the N+ type buffer layer 21 and the N+ type etching relaxation layer 23 are interposed, the excess carriers (electrons in the embodiment) in the N-type drift well layer 22 can be quickly eliminated, and the turn-on and turn-off speeds of the IGBT can be improved. Therefore, the PN junction internal resistance when the channel is closed (channel cut-off state) can be improved, and a low on-state voltage drop and high current density can be maintained in the on state, so as to achieve stable voltage tolerance while improving the turn-on and turn-off speeds.

[0089] For a better example, see Figure 1 , the semiconductor substrate 10 includes a collector single crystal layer 12 located below the P-type injection layer 11, for example, a P+ type and close to the conduction band, and the IGBT device also includes: a collector metal 80, which is arranged on the back of the semiconductor substrate 10 in a covering manner to connect the collector single crystal layer 12. The collector metal 80 is connected to the collector single crystal layer 12 to establish the bottom surface structure of the IGBT device, thereby realizing the connection between the collector of the IGBT device and the external circuit, so as to improve the electrical performance and reliability of the IGBT device, so that the device has better stability and durability in harsh environments such as high voltage and high current. The IGBT device circuit is well known and will not be described here.

[0090] In a preferred example, the width of the emitter trench 40 is specifically greater than the width of the gate trench 30, and can be greater than the width of the gate trench 30 by 1.5 to several times, so as to reduce the depth of the emitter trench 40, reduce conduction loss, and improve the performance of the IGBT device. In the IGBT design, by adjusting the width of the emitter trench 40 to be greater than the width of the gate trench 30, the depth of the emitter trench 40 is effectively reduced when the gate trench 30 reaches a sufficient depth in the same trench etching process. The depth of the gate trench 30 stops at the N+ type etching mitigation layer 23. During etching, the N-type ions in the N+ type etching mitigation layer 23 are monitored in the etching chamber and their concentration increases sharply, which can serve as an etching stop signal. There are three reasons for reducing conduction loss. First, the width of the emitter trench 40 increases, and the effective width of the conductive channel increases accordingly, which helps to reduce the impedance of the current in the conductive channel of the P-type body well layer 24 on the groove side. At the same time, the P-type body well layer 24 and the N+ type etching relaxation layer 23 increase in the opposite direction, thereby reducing conduction loss; second, the wider emitter trench 40 is beneficial to increase the carrier concentration of the P-type body well layer 24 and optimize the carrier distribution when the device is turned on, thereby improving the conductivity modulation efficiency and further reducing the conduction loss; third, the vertical trench structure can eliminate the JFET effect, that is, eliminate the impedance in the horizontal current path, thereby reducing the overall voltage drop and conduction loss.

[0091] In this embodiment, based on the fact that the width of the emitter trench 40 is greater than the width of the gate trench 30, the emitter trench 40 only penetrates the N+ type source layer 25 and stops at the P type body well layer 24, and the gate oxide layer 50 also includes an isolation oxide layer 51 covering the sidewalls of the emitter trench 40, and the isolation oxide layer 51 does not cover the inner groove bottom of the emitter trench 40. By optimizing the structure of the emitter trench 40 and the configuration of the isolation oxide layer 51 as above, the conduction loss of the channel can be reduced, the current density can be increased, the electron injection efficiency of the P type body well layer 24 can be optimized, the heat loss can be reduced, the withstand voltage performance can be enhanced, and the process steps can be reduced, which is suitable for the application scenarios of IGBT devices in high voltage, high current and high frequency.

[0092] In a preferred example, the top surface of the gate filler 31 is relatively recessed from the upper surface of the N+ source layer 25, so as to facilitate the patterning of the gate oxide layer 50 before the interlayer film 60 is deposited. The top surface of the gate filler 31 is located between the upper and lower surfaces of the N+ source layer 25. When the top surface of the gate filler 31 is recessed, the surface gate oxide layer will be exposed. Under selective etching, this also means that the epitaxial growth layer formed on the N+ source layer 25 at the same time as the gate filler 31 is etched away, and the N-type ions in the etching chamber will be significantly reduced (as the first etching stop signal). The P column 41 is etched at a lower etching rate based on different crystal orientations and can be retained to protrude from the N+ source layer 25. The convex shape of the P column 41 and the concave shape of the gate filler 31 realize the patterning of the gate oxide layer 50. During the etching process of the gate oxide layer 50, when the portion of the gate oxide layer 50 on the N+ type source layer 25 is etched away, the oxide ions in the etching chamber will be significantly reduced (serving as a second etching stop signal). Therefore, the formation of the gate filler 31 and the P column 41 is patterning without a mask, and the patterning of the gate oxide layer 50 is also patterning without an additional mask, corresponding to process steps S52 and S53, respectively.

[0093] Therefore, the top surface of the gate filler 31 is relatively recessed from the upper surface of the N+ type source region layer 25, and the additional anti-etching mask formation setting can be reduced in the process of patterning the gate oxide layer 50 before the deposition of the interlayer film 60 (corresponding to step S53), or / and, the recess of the gate filler 31 can prevent the components of the gate filler 31 from causing cross contamination to the area on the surface of the N+ type source region layer that does not need to be covered during the deposition of the interlayer film 60, and the interlayer film 60 can be better connected to the patterned gate oxide layer 50. When there is an error between the pattern of the interlayer film 60 and the gate trench 30, the top surface of the gate filler 31 is still covered with a part of the interlayer film 60, which can expand and improve the performance of the IGBT device and the precision requirements of the patterning of the interlayer film 60 during the manufacturing process, and prevent the leakage between the gate and the emitter from being reduced.

[0094] In a preferred example, the P column 41 protrudes from the N+ type source layer 25, and the inner groove bottom of the emitter groove 40 exposes the P type body well layer 24, which is conducive to the top surface of the P column 41 being exposed and easier to connect with the emitter, and the bottom of the P column 41 is directly connected to the P type body well layer 24, so that a relatively high epitaxial growth rate and a crystal orientation with a lower selective etching ratio (compared to the gate filler 31) are obtained, so the gate filler 31 and the P column 41 can be made in the same step but have different forms. The bottom of the P column 41 is directly connected to the P type body well layer 24, eliminating the oxide layer isolation at the bottom of the groove, making the current conduction path more direct and reducing the on-resistance; the top of the P column 41 protrudes to increase the bonding area with the emitter. This improves the electrical performance and reliability of the IGBT device, simplifies the IGBT device manufacturing process, and improves the overall efficiency of the system.

[0095] See also Figure 3 The present invention also provides a method for manufacturing an IGBT device, which is used to prepare the aforementioned IGBT device. The manufacturing method includes steps S1 to S8, wherein steps S1 to S7 are necessary steps, and are referred to in conjunction with Figures 4 to 12 The details are as follows.

[0096] Step S1 See Figure 4 A semiconductor substrate 10 having a P-type injection layer 11 is provided. The semiconductor substrate 10 is in the form of a wafer. The P-type injection layer 11 can be used as the lower P-pole of the PNP tube of the IGBT device circuit.

[0097] Step S2 See Figure 5 , an IGBT device working layer region 20 is epitaxially grown on the P-type injection layer 11 of the semiconductor substrate 10; wherein the IGBT device working layer region 20 includes an N+ type buffer layer 21, an N-type drift well layer 22, an N+ type etching relief layer 23, a P-type body well layer 24, and an N+ type source region layer 25 formed by epitaxial growth or ion diffusion on the P-type body well layer 24, which are epitaxially grown in sequence on the P-type injection layer 11; wherein the N+ type etching relief layer 23 is interposed between the P-type body well layer 24 and the N-type drift well layer 22. After this step, the combination of the IGBT device working layer region 20 and the semiconductor substrate 10 constitutes an epitaxial wafer.

[0098] Step S3 See Figure 6, a plurality of gate trenches 30 and an emitter trench 40 between two adjacent gate trenches 30 are simultaneously provided in the IGBT device working layer region 20; according to the trench opening pattern and the trench width difference, the emitter trench 40 is relatively enclosed in the gate trench 30 and is not connected, the gate trench 30 penetrates the N+ type source region layer 25 and the P type body well layer 24 and stops at the N+ type etching relief layer 23, and the emitter trench 40 penetrates the N+ type source region layer 25 and stops at the P type body well layer 24 or the N+ type etching relief layer 23. When the depth of the gate trench 30 stops at the N+ type etching relief layer 23, the N type ions of the N+ type etching relief layer 23 will be released and detected, which can be used as an etching stop signal. In this embodiment, since the emitter trench 40 is relatively wide and the depth of the emitter trench 40 is relatively shallow, the inner groove bottom of the emitter trench 40 stops at the P-type body well layer 24. More specifically, the semiconductor etching technology of step S3 has etching selectivity, and the etching selectivity ratio of the P-type body well layer 24 is higher than that of the N+ type etching relief layer 23, that is, the etching rate of the P-type body well layer 24 is higher than that of the N+ type etching relief layer 23. The gate trench 30 and the emitter trench 40 have a concave arc surface on the inner side wall of the P-type body well layer 24, similar to the open groove of the cross section of a bottle. The curved inner sidewall of the gate groove 30 is beneficial to suppressing the lateral extension of the vertical ion implantation, and the curved inner sidewall of the emitter groove 40 is beneficial to suppressing the lateral epitaxial growth based on the insulating material. The vertical epitaxial growth rate based on the semiconductor material of the inner bottom of the emitter groove 40 on the P-type body well layer 24 is not restricted.

[0099] Step S4 see Figure 7 , forming a gate oxide layer 50 on the N+ type source layer 25, and the gate oxide layer 50 can be formed by thermal oxidation, chemical vapor deposition or a combination of methods. The gate oxide layer 50 also covers the inner sidewall and inner groove bottom of the gate trench 30 and the inner sidewall and inner groove bottom of the emitter trench 40. After step S4, the manufacturing method further includes step S41, referring to Figure 8 The gate oxide layer 50 at the bottom of the emitter trench 40 may be removed by patterned vertical plasma etching or other known methods to expose the P-type body well layer 24 at the bottom of the emitter trench 40 .

[0100] Step S5 see Fig. 9 , Fig.10 and Fig.11, a P column 41 is arranged on the inner bottom of the emitter trench 40 by using a differential speed epitaxial growth method, and a gate filler 31 is arranged in the gate trench 30; the P column 41 protrudes upward and penetrates the N+ type source region layer 25, and the top surface of the gate filler 31 is relatively recessed in the upper surface of the N+ type source region layer 25. Wherein, step S5 includes steps S51, S52 and S53 as described later.

[0101] Step S51: Fig. 9 The P column 41 of the PNP tube is grown on the bottom of the inner groove of the emitter groove 40 by speed differential epitaxial growth, and the gate filling body 31 is grown in the gate groove 30 at the same time. The P column 41 is connected to the P-type body well layer 24. A P+ connection layer 33 is also formed on the gate oxide layer 50 on the N+ type source layer 25. The P+ connection layer 33 integrally connects the P column 41 and the gate filling body 31. The epitaxial growth rate of the P+ connection layer 33 is slightly greater than the epitaxial growth rate of the gate filling body 31, but significantly less than the epitaxial growth rate of the P column 41.

[0102] Step S52: Fig.10 , based on the portion of the gate oxide layer 50 formed on the N+ type source region layer 25 as the bottom mask, the P+ connection layer 33 is removed by semiconductor selective etching to separate the gate filler 31 and the P column 41. Based on the different single crystal orientations, the selective etching rate of the P column 41 is the lowest, which is lower than the selective etching rates of the gate filler 31 and the P+ connection layer 33. When the P+ connection layer 33 is etched away, the gate oxide layer 50 on the N+ type source region layer 25 blocks the P-type semiconductor from being further etched, and the concentration of P-type ions in the etching chamber will be greatly reduced. The sudden decrease in the P concentration can be used as an etching stop signal in step S52, and no photolithography mask is required.

[0103] Step S53: Fig.11 , using the gate filler 31 and the P column 41 as natural masks, the portion of the gate oxide layer 50 formed on the N+ type source layer 25 is removed by an oxide etching method. The etching technology of step S53 does not etch the gate filler 31 and the P column 41, and the gate oxide layer 50 blocked by the gate filler 31 and the P column 41 is retained. Therefore, it is worth noting that the separation patterning of the P column 41 and the gate filler 31 in step S52 and the surface exposure patterning of the gate oxide layer 50 in step S53 do not require photolithography and development operations, which can significantly save semiconductor manufacturing costs.

[0104] Step S6 See Fig.12An interlayer film 60 is formed on the gate filler 31 to isolate the gate filler 31 from the P column 41. The interlayer film 60 connects the ends of the gate oxide layer 50 on both sides of the gate trench 30 opening.

[0105] Step S7 See Fig.13 An emitter metal layer 70 is disposed on the N+ type source region layer 25, the interlayer film 60 and the P column 41, and the emitter metal layer 70 connects the N+ type source region layer 25 and the P column 41 at individual locations.

[0106] The implementation principle of the method of this embodiment is described below. The step S51 of growing the P column 41 of the PNP tube on the inner groove bottom of the emitter groove 40 and growing the gate filling body 31 in the gate groove 30 simultaneously by speed differential epitaxy is conducive to forming an interlayer film 60 with good isolation effect in step S6, avoiding the short circuit between the P column 41 and the gate filling body 31. In addition, the step S52 of removing the P+ connection layer 33 by selective etching effectively separates the gate filling body 31 from the P column 41, further improving the reliability and stability of the IGBT device.

[0107] In a preferred example, in step S1, refer to Figure 4 The semiconductor substrate 10 includes a collector single crystal layer 12 located below the P-type injection layer 11. The manufacturing method of the IGBT device further includes step S8, referring to Figure 1 , a collector metal 80 is provided on the back of the semiconductor substrate 10 to cover and connect the collector single crystal layer 12. In a preferred example, in step S6, refer to Fig.12 The patterning of the interlayer film 60 corresponds to the groove opening of the gate trench 30; the interlayer film 60 is formed using a photolithography mask.

[0108] In the preferred technical solution of the above method, the collector single crystal layer 12 is provided through step S1, and the collector single crystal layer 12 is included in the semiconductor substrate 10 below the P-type injection layer 11, which is helpful to form a stable collector contact in the subsequent steps and optimize the electrical performance of the IGBT device; the existence of the collector single crystal layer 12 can optimize the current distribution, reduce the local current over-density phenomenon, and improve the short-circuit capability and stability of the device; the gate filling body 31 is etched back through the etching process in step S51 so that the top surface of the gate filling body 31 is relatively recessed in the N+ type source layer 25. The upper surface of the collector electrode 12 is provided, which helps to reduce the parasitic capacitance between the gate and the emitter, and improve the switching speed and efficiency of the device; through the interlayer film 60 patterning in step S6, the patterning of the interlayer film 60 corresponds to the slot opening of the gate trench 30, and an effective isolation structure is formed in the IGBT device to prevent unnecessary coupling between the gate and the emitter, and improve the anti-interference ability of the device; through the collector metal 80 covering the ground in step S8 to connect the collector single crystal layer 12, a good back side contact can be provided, the contact resistance can be reduced, and the injection efficiency of the current can be improved. The setting of the collector metal 80 also helps to improve the thermal management of the IGBT device. The metal layer can serve as a heat diffusion layer to help heat transfer from the inside of the chip to the outside faster, and improve the thermal stability of the device.

[0109] In a preferred example, in step S3, refer to Figure 6 According to the same etching process of the groove opening pattern, the width of the emitter groove 40 is greater than the width of the gate groove 30, and the depth of the emitter groove 40 is less than the depth of the gate groove 30, so that the inner groove bottom of the emitter groove 40 does not extend to the N+ type etching relief layer 23. In step S3, the width of the emitter groove 40 is greater than the width of the gate groove 30, and its depth is less than the depth of the gate groove 30, so that the inner groove bottom of the emitter groove 40 does not extend to the N+ type etching relief layer 23, so that the effective isolation between the emitter groove 40 and the gate groove 30 can be ensured during the manufacturing process, reducing the risk of short circuit.

[0110] In a preferred example, in step S41, refer to Figure 8 , the inner bottom of the emitter trench 40 exposes the P-type body well layer 24. In step S41, by removing part of the gate oxide layer 50 at the inner bottom of the emitter trench 40, the P-type body well layer 24 is exposed. This step helps to achieve direct connection between the P column 41 and the P-type body well layer 24 in the subsequent step S5, reducing the recombination loss of electrons and holes inside the device, thereby improving the overall performance of the IGBT device. In a preferred example, in step S5, refer to Fig.10 The P column 41 can be directly connected to the P-type body well layer 24, and the setting of the P-type column bottom junction can be omitted to stably maintain the N-pole performance in the PNP tube circuit (corresponding to the N-type drift well layer 22).

[0111] Reference Fig.14 The second embodiment of the present invention discloses another IGBT device, whose basic structure and manufacturing process are substantially the same as those of the first embodiment. The IGBT device comprises a semiconductor substrate 10 having a P-type injection layer 11, an IGBT device working layer region 20 epitaxially grown on the semiconductor substrate 10, a gate oxide layer 50 covering the inner sidewall and the bottom of the gate trench 30, a P column 41 and a gate filling body 31 grown by differential speed epitaxy, an interlayer film 60 formed on the gate filling body 31, and an emitter metal layer 70 disposed thereon. The IGBT device working layer region 20 includes an N+ type buffer layer 21, an N type drift well layer 22, an N+ type etching relief layer 23, a P type body well layer 24 and an N+ type source region layer 25 which are sequentially located on the P type injection layer 11; wherein the N+ type etching relief layer 23 is disposed between the P type body well layer 24 and the N type drift well layer 22, and a plurality of gate trenches 30 are simultaneously opened in the IGBT device working layer region 20 and a plurality of gate trenches 30 are disposed between adjacent gate trenches 30. An emitter trench 40 between two gate trenches 30; according to the difference in trench opening pattern and trench width, the emitter trench 40 is relatively enclosed in the gate trench 30 and is not connected. The gate trench 30 penetrates the N+ type source layer 25 and the P type body well layer 24 and stops at the N+ type etching relief layer 23. The emitter trench 40 penetrates the N+ type source layer 25 and can stop at the P type body well layer 24 or the N+ type etching relief layer 23. The P column 41 is arranged on the inner groove bottom of the emitter trench 40 and is connected to the P type body well layer 24. The gate filling body 41 is arranged in the gate trench 30. The P column 41 protrudes upward from the N+ type source layer 25 relative to the gate filling body 31. The emitter metal layer 70 is disposed on the N+ type source region layer 25 , the interlayer film 60 , and the P column 41 . The emitter metal layer 70 connects the N+ type source region layer 25 and the P column 41 at individual locations.

[0112] See also Fig.14 In the second embodiment, the depth of the gate trench 30 may stop at the N+ type etch mitigation layer 23, and the emitter trench 40 may penetrate the N+ type source layer 25 and also stop at the N+ type etch mitigation layer 23. The P-type column bottom junction 42 may be used to connect the P-column 41 and the P-type body well layer 24.

[0113] Specifically, when the depth of the emitter trench 40 stops at the N+ type etching mitigation layer 23, a P-type column bottom junction 42 is formed below the inner groove bottom of the emitter trench 40, so that the P column 41 is indirectly connected to the P-type body well layer 24. The formation of the P-type column bottom junction 42 effectively blocks the direct contact between the P column 41 and the N-type drift well layer 22. When the IGBT is turned on, the unnecessary hole carriers injected by the P column 41 into the N-type drift well layer 22 are reduced, and the P-type column bottom junction 42 more accurately controls the distribution of minority carriers in the N-type drift well layer 22, thereby optimizing the conductivity modulation effect. When the IGBT is turned off, the P column 41 does not directly contact the N-type drift well layer 22, and the formation of the P-type column bottom junction 42 can effectively avoid the punch-through phenomenon under high voltage, thereby enhancing the stability of the IGBT device under high voltage environment. In addition, the emitter trench 40 having a concave arc surface on the inner side wall of the P-type body well layer 24 is also conducive to the formation of a P-type column bottom junction 42 below the inner bottom of the emitter trench 40, reducing the lateral implantation of P-type ions on the inner side wall of the concave arc surface during the formation process of the P-type column bottom junction 42.

[0114] In a preferred example, a P-type gate bottom junction 32 is formed below the inner groove bottom of the gate trench 30 to pattern the N+ type etching mitigation layer 23. Through the formation of the P-type gate bottom junction 32, on the one hand, the conductivity of the bottom of the gate trench 30 is effectively enhanced, ensuring that the current is evenly distributed in the N-type drift well layer 22 at the bottom of the gate trench 30, thereby improving the conductivity stability of the entire IGBT device when it is turned on, and helping to shorten the opening and closing time of the IGBT device. That is, it helps to reduce the local dynamic loss of the IGBT device during the switching process, reduce the current tailing phenomenon during the switching transient process, and improve the device switching efficiency. On the other hand, it helps to evenly distribute the electric field of the N-type drift well layer 22 in the IGBT device, avoid early breakdown caused by excessive local electric field, improve the breakdown voltage, and enhance the withstand voltage capability of the IGBT device. In addition, the concave arc surface of the gate trench 30 on the inner side wall of the P-type body well layer 24 is conducive to the formation of a P-type gate bottom junction 32 below the inner bottom of the gate trench 30, reducing the lateral implantation of P-type ions on the inner side wall of the concave arc surface during the formation process of the P-type gate bottom junction 32.

[0115] In the manufacturing method of the second embodiment, there is Figure 3The same basic manufacturing steps as shown. In addition, in step S3, the depth of the emitter trench 40 stops at the N+ type etching relief layer 23. After step S4, it also includes: step S42, forming a P-type column bottom junction 42 below the inner bottom of the emitter trench 40. In step S5, the P column 41 is indirectly connected to the P-type body well layer 24. After step S4, it also includes: step S43, forming a P-type gate bottom junction 32 below the inner bottom of the gate trench 30, and the P-type gate bottom junction 32 is used to pattern the N+ type etching relief layer 23. Step S42 and step S43 can be implemented individually, or they can be implemented together in the same ion implantation process. In the manufacturing process of IGBT devices, the step S42 for forming the P-type column bottom junction 42 is introduced to effectively avoid the P-column 41 above the PNP tube of the partially over-etched emitter trench 40 from being unable to connect to the P-type body well layer 24 of the MOSFET transistor. The step S43 for forming the P-type gate bottom junction 32 is introduced to pattern the N+ type etching mitigation layer 23, effectively enhancing the conductivity on both sides of the bottom of the gate trench and facilitating the uniform electric field distribution of the N-type drift well layer 22. The formation of the P-type column bottom junction 42 and the P-type gate bottom junction 32 does not require simultaneous setting; in a variation example, only the P-type gate bottom junction 32 may be set without the P-type column bottom junction 42, as shown in FIG. Figure 1 In the structure shown, an additional layer is added at the bottom of the gate trench 30. Fig.14 The P-type gate bottom junction 32 shown is used to pattern the N+ type etching relaxation layer 23. The P-type column bottom junction 42 has two functions: one is to serve as a relay connection between the P-type body well layer 24 and the P column 41, and the other is to adjust the N-pole performance of the equivalent PNP tube in the IGBT device circuit (the position corresponds to the N-type drift well layer 22).

[0116] The embodiments of this specific implementation method are all preferred embodiments for facilitating the understanding or implementation of the technical solutions of the present invention, and are not intended to limit the protection scope of the present invention. All equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. An IGBT device, characterized in that: include: A semiconductor substrate having a P-type implantation layer; The IGBT device working layer region is epitaxially grown on the P-type injection layer of the semiconductor substrate; wherein the IGBT device working layer region includes an N+ type buffer layer, an N-type drift well layer, an N+ type etching relief layer, a P-type body well layer and an N+ type source region layer sequentially located on the P-type injection layer; wherein the N+ type etching relief layer is disposed between the P-type body well layer and the N-type drift well layer, and the IGBT device working layer region is simultaneously provided with a plurality of gate trenches and an emitter trench between two adjacent gate trenches; according to the difference in the trench opening pattern and the trench width, the emitter trench is relatively enclosed in the gate trench and is not connected, the gate trench penetrates the N+ type source region layer and the P-type body well layer and stops at the N+ type etching relief layer, and the emitter trench penetrates the N+ type source region layer and stops at the P-type body well layer or the N+ type etching relief layer; wherein the width of the emitter trench is greater than the width of the gate trench; A gate oxide layer, covering the inner sidewall and the bottom of the gate trench; A P column and a gate filling body grown by speed differential epitaxy, wherein the P column is arranged on the inner groove bottom of the emitter groove and connected to the P-type body well layer, the gate filling body is arranged in the gate groove, and the P column protrudes upward from the N+ type source layer relative to the gate filling body; An interlayer film is formed on the gate filling body to isolate the gate filling body from the P column; The emitter metal layer is disposed on the N+ type source region layer, the interlayer film and the P column. The emitter metal layer connects the N+ type source region layer and the P column at individual locations.

2. The IGBT device according to claim 1, characterized in that: The semiconductor substrate comprises a collector single crystal layer located below the P-type injection layer, and the IGBT device further comprises: a collector metal which is arranged on the back side of the semiconductor substrate in a covering manner to connect the collector single crystal layer.

3. The IGBT device according to claim 1, characterized in that: The top surface of the gate filling body is relatively recessed from the upper surface of the N+ type source region layer, so as to facilitate the patterning of the gate oxide layer before the interlayer film is deposited.

4. The IGBT device according to claim 1, characterized in that: Based on the fact that the width of the emitter trench is greater than the width of the gate trench, the emitter trench only penetrates the N+ type source layer and ends at the P type body well layer, and the gate oxide layer also includes an isolation oxide layer covering the side walls of the emitter trench, and the isolation oxide layer does not cover the inner bottom of the emitter trench.

5. The IGBT device according to claim 4, characterized in that: The P column protrudes from the N+ type source layer, and the inner groove bottom of the emitter trench exposes the P type body well layer, so that the P column is directly connected to the P type body well layer.

6. The IGBT device according to claim 1, characterized in that: The depth of the emitter trench stops at the N+ type etching relief layer, and a P-type column bottom junction is formed below the inner bottom of the emitter trench so that the P column is indirectly connected to the P-type body well layer; the gate trench and the emitter trench have a concave arc surface on the inner side wall of the P-type body well layer.

7. The IGBT device according to any one of claims 1 to 6, characterized in that: A P-type gate bottom junction is formed below the inner bottom of the gate trench to pattern the N+ type etching relaxation layer.

8. A method for manufacturing an IGBT device, characterized in that: include: S1, providing a semiconductor substrate having a P-type injection layer; S2, a blanket epitaxially grown IGBT device working layer region is on the P-type injection layer of the semiconductor substrate; wherein the IGBT device working layer region includes an N+ type buffer layer, an N-type drift well layer, an N+ type etching relief layer, a P-type body well layer, and an N+ type source region layer formed by epitaxial growth or ion diffusion on the P-type body well layer; wherein the N+ type etching relief layer is disposed between the P-type body well layer and the N-type drift well layer; S3, simultaneously opening a plurality of gate trenches and an emitter trench between two adjacent gate trenches in the working layer area of ​​the IGBT device; according to the trench opening pattern and the difference in trench width, the emitter trench is relatively enclosed in the gate trench and is not connected, the gate trench penetrates the N+ type source region layer and the P type body well layer and stops at the N+ type etching relief layer, and the emitter trench penetrates the N+ type source region layer and stops at the P type body well layer or the N+ type etching relief layer; in step S3, according to the same etching process of the trench opening pattern, the width of the emitter trench is greater than the width of the gate trench; S4, forming a gate oxide layer on the N+ type source layer, the gate oxide layer also covering the inner sidewalls and the inner groove bottom of the gate groove and the emitter groove; after step S4, comprising: S41, removing the portion of the gate oxide layer at the inner groove bottom of the emitter groove to expose the P type body well layer; S5, setting a P column on the inner groove bottom of the emitter groove, and setting a gate filling body in the gate groove; the P column protrudes upward and penetrates the N+ type source region layer, and the top surface of the gate filling body is relatively recessed in the upper surface of the N+ type source region layer; wherein step S5 comprises: S51, differential speed epitaxial growth of the P column of the PNP tube on the inner groove bottom of the emitter groove and simultaneously growing the gate filling body in the gate groove, the P column connecting the P type body well layer, and a P+ connection layer is also formed on the gate oxide layer on the N+ type source region layer, integrally connecting the P column and the gate filling body; S52, based on the portion of the gate oxide layer formed on the N+ type source region layer as the bottom mask, selectively etching and removing the P+ connection layer to separate the gate filling body from the P column; S53, using the gate filling body and the P column as masks, etching and removing the portion of the gate oxide layer formed on the N+ type source region layer; S6, forming an interlayer film on the gate filling body to isolate the gate filling body from the P column; S7, disposing an emitter metal layer on the N+ type source region layer, the interlayer film and the P column, wherein the emitter metal layer connects the N+ type source region layer and the P column at individual locations.

9. The method for manufacturing an IGBT device according to claim 8, characterized in that: In step S1, the semiconductor substrate includes a collector single crystal layer located below the P-type injection layer; the manufacturing method of the IGBT device further includes: S8, coveringly arranging a collector metal on the back side of the semiconductor substrate to connect the collector single crystal layer; In step S6 , the interlayer film is patterned to correspond to the trench opening of the gate trench.

10. The method for manufacturing an IGBT device according to claim 9, characterized in that: In step S3, the depth of the emitter trench is less than the depth of the gate trench, so that the inner bottom of the emitter trench does not extend to the N+ type etching relaxation layer; in step S41, the inner bottom of the emitter trench exposes the P-type body well layer; in step S5, the P column is directly connected to the P-type body well layer; the gate trench and the emitter trench have a concave arc surface on the inner side wall of the P-type body well layer.

11. The method for manufacturing an IGBT device according to claim 9, characterized in that: In step S3, the depth of the emitter trench stops at the N+ type etching mitigation layer; after step S4, it also includes: S42, forming a P-type column bottom junction below the inner groove bottom of the emitter trench; in step S5, the P column is indirectly connected to the P-type body well layer; After step S4, the method further includes: S43, forming a P-type gate bottom junction below the inner groove bottom of the gate groove, wherein the P-type gate bottom junction is used to pattern the N+ type etching relaxation layer.