Multicolor micro-display chip and preparation method thereof

By designing a combination of multi-color master pixels and driver wafers in micro-display chips, the problem of brightness attenuation of red pixels in micro-display chips is solved and the color display effect is improved.

CN118870909APending Publication Date: 2024-10-29NUOSHI TECH (SUZHOU) CO LTD
View PDF 0 Cites 5 Cited by

Patent Information

Application Number
CN202411013387.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

In the field of micro-displays, the reduction in chip size of micro-display chips has resulted in serious attenuation of the brightness of red pixels, making it difficult to achieve a specific brightness ratio and unable to achieve ideal color display effects.

Method used

Design a multi-color microdisplay chip, including a mother pixel and a driver wafer. The mother pixel is composed of at least four sub-pixels, at least two of which have different light colors, and the number of sub-pixels with red light color is not less than that of the mother pixel. 50% of all sub-pixels in the chip are electrically connected to the driving wafer and stacked in sequence along the Z direction to ensure that the number of red sub-pixels is sufficient to control red light attenuation.

Benefits of technology

Effectively increasing the number of red sub-pixels, ensuring that the brightness ratio of red light in the parent pixel is within a specific range, thereby achieving ideal color display effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118870909A_ABST
    Figure CN118870909A_ABST
Patent Text Reader

Abstract

The invention relates to a multicolor micro-display chip and a preparation method thereof, the chip comprises a mother pixel, a driving wafer and at least two pixel layers, the mother pixel comprises at least four sub-pixels, at least two sub-pixels in the mother pixel have different light emitting colors, the sub-pixels have red light emitting colors, and the sub-pixels have red light emitting colors. The number of the sub-pixels of which the light emitting color is red is not less than 50% of the number of all the sub-pixels in the mother pixel; the sub-pixels are electrically connected with the driving wafer; all the pixel layers are sequentially stacked on the driving wafer in the Z direction, at least one sub-pixel is arranged in each pixel layer, the sub-pixels in the same pixel layer have the same light emitting color, and the sub-pixels in the two adjacent pixel layers have different light emitting colors. The invention also discloses a preparation method of the micro-display chip. The number of the red sub-pixels is effectively increased, so that attenuation of red light in the mother pixels can be effectively controlled, and the ideal color display effect is guaranteed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a multi-color micro display chip and a preparation method thereof. Background Art

[0002] In the field of LED, color display is mainly produced by combining RGB sub-pixels to form a mother pixel and combining light in different proportions. In theory, all colors on the spectrum can be produced by matching the three primary colors of red R, green G, and blue B. Our sense of color for objects is determined on the one hand by the physical stimulation of external objects to the human eye, and on the other hand by the visual characteristics of the human eye in processing stimulation. However, the final calibration of color must conform to the visual laws of the human eye. The human retina has two types of photoreceptor cells, namely cones and rods. Rods are used to perceive light intensity and mainly work in dim light environments. Cones are used to perceive color and mainly work in strong light environments. Cones are divided into three types: blue cones, green cones, and red cones. In order to enable the human eye retina to better perceive the corresponding colors, when the LED display screen is used for light distribution, the brightness of the three primary colors of red, green and blue or two primary colors needs to reach a specific ratio. For example, you can choose three primary color pixels with a brightness ratio of 3 (red): 6 (green): 1 (blue) or 2 (red): 7 (green): 1 (blue) to achieve white light synthesis. At this time, you can generally choose a color pixel layout mode such as RGB, RGGB or RGBW.

[0003] However, in the field of micro-display, such as Micro-LED display, the chip size is greatly reduced compared to conventional LED chips. As the size decreases, the brightness of the red pixel decays more seriously. According to the conventional color pixel layout method, it is difficult to achieve a specific brightness ratio, thereby failing to achieve the ideal color display effect and failing to meet production and use requirements. Summary of the invention

[0004] Therefore, the technical problem to be solved by the present invention is to overcome the defect of poor color display effect of the micro display chip in the prior art.

[0005] In order to solve the above technical problems, the present invention provides a multi-color micro display chip, comprising:

[0006] A mother pixel, wherein the mother pixel includes at least four sub-pixels, at least two of the sub-pixels in the mother pixel have different light emitting colors, and the mother pixel has a sub-pixel with a light emitting color of red, and the number of sub-pixels with a light emitting color of red is not less than 50% of the number of all sub-pixels in the mother pixel;

[0007] A driving wafer, the sub-pixels are all electrically connected to the driving wafer;

[0008] At least two pixel layers, all of the pixel layers are stacked in sequence along the Z direction on the driving wafer, all of the sub-pixels of the mother pixel are respectively arranged in the corresponding pixel layers, at least one sub-pixel is arranged in each pixel layer, the light emitting color of each sub-pixel in the same pixel layer is the same, and the light emitting colors of the sub-pixels in two adjacent pixel layers are different.

[0009] In one embodiment of the present invention, the projections of all sub-pixels in the mother pixel on the driving wafer do not overlap.

[0010] In one embodiment of the present invention, the sub-pixel is in a trapezoidal or cylindrical shape.

[0011] In one embodiment of the present invention, an anode contact and a cathode contact are provided on the driving wafer, each of the pixel layers includes an insulating body, the sub-pixels in the pixel layer are encapsulated inside the insulating body, a bonding metal part is provided on the side of each sub-pixel close to the driving wafer, the bonding metal part is electrically connected to the corresponding anode contact, the outside of each sub-pixel is encapsulated with an insulating passivation layer, the bonding metal part is located inside the insulating passivation layer, the upper portion of the insulating passivation layer has an opening, the outside of the insulating passivation layer is encapsulated with a common cathode layer, the sub-pixels are electrically connected to the common cathode layer through the opening, and the common cathode layer is used to be electrically connected to the cathode contact.

[0012] In one embodiment of the present invention, the sub-pixels each include a P-type semiconductor layer, an active layer and an N-type semiconductor layer arranged in sequence along the Z direction, the bonding metal part is provided on one side of the P-type semiconductor layer close to the driving wafer, and the N-type semiconductor layer is electrically connected to the common cathode layer through the opening.

[0013] In one embodiment of the present invention, the bonding metal of the sub-pixel in the upper pixel layer is electrically connected to the corresponding anode contact by an anode connection passing through the underlying pixel layer.

[0014] In one embodiment of the present invention, an anode hole corresponding to the anode connector is opened on the interface of two adjacent pixel layers, the anode hole is filled with the anode connector, the top surface of the anode connector filled in the anode hole is lower than the interface to form a recessed portion, and the bonding metal part of the sub-pixel in the pixel layer is embedded in the recessed portion of the corresponding anode hole of the adjacent pixel layer below to be in electrical contact with the anode connector; or,

[0015] The top surface of the anode connector filled in the anode hole is higher than the interface to form a convex portion, and the bonding metal member of the sub-pixel in the pixel layer is embedded with the convex portion of the corresponding anode connector of the adjacent pixel layer below.

[0016] In one embodiment of the present invention, at least three pixel layers are included, and the bonding metal parts of the sub-pixels in the third and above pixel layers are electrically connected to corresponding anode contacts by multiple anode connectors connected sequentially along the Z direction below, and each anode connector connected sequentially along the Z direction is located in a different pixel layer, and two adjacent anode connectors among the anode connectors connected sequentially along the Z direction are in direct contact with each other, or a conductive metal part is provided between two adjacent anode connectors.

[0017] In one embodiment of the present invention, a cathode hole is opened on the interface of two adjacent pixel layers, and the cathode hole is filled with a cathode connector, and the cathode connectors are electrically connected to the cathode contacts, and the common cathode layers in the upper pixel layer are electrically connected to the cathode contacts through the cathode connectors and cathode contacts in the lower pixel layer.

[0018] In one embodiment of the present invention, the interface between two adjacent pixel layers is also covered with the insulating passivation layer, the upper portion of the insulating passivation layer at the interface is also covered with the common cathode layer, and a metal grid layer is disposed on the upper portion of the common cathode layer.

[0019] In one embodiment of the present invention, light emitted from a sub-pixel in a lower pixel layer is emitted through a first notch in an upper pixel layer, the first notch is opened on the metal grid layer, and the length of the first notch in the X direction is greater than the top surface length of the sub-pixel corresponding to the lower layer, wherein the X direction is perpendicular to the Z direction.

[0020] In one embodiment of the present invention, light emitted from a sub-pixel in a lower pixel layer is emitted sequentially through a second notch and a first notch in an upper pixel layer, the second notch is opened on a common cathode layer, and a length of the second notch in the X direction is greater than a top surface length of the sub-pixel corresponding to the lower layer.

[0021] In one embodiment of the present invention, the anode connector located in the bottom pixel layer passes through an auxiliary pixel and is electrically connected to the corresponding anode contact on the driving wafer; the auxiliary pixel is located in the bottom pixel layer and between two adjacent sub-pixels in the X direction, wherein the X direction is perpendicular to the Z direction.

[0022] In one embodiment of the present invention, at least one lens is connected to the upper portion of the pixel layer at the top layer, and the lens corresponds to the mother pixel one-to-one, or each lens corresponds to the sub-pixel one-to-one.

[0023] The present invention also discloses a method for preparing a multi-color micro-display chip, comprising:

[0024] Step M1, preparing a driver wafer;

[0025] Step M2, stacking at least two pixel layers in sequence along the Z direction on the driving wafer, so that all sub-pixels in the mother pixel are respectively arranged in the corresponding pixel layers, at least one sub-pixel is arranged in each pixel layer, the light output color of each sub-pixel in the same pixel layer is the same, the light output colors of the sub-pixels in two adjacent pixel layers are different, and the sub-pixels are all electrically connected to the driving wafer, so that the driving wafer can be used to drive the sub-pixels to emit light.

[0026] In one embodiment of the present invention, in the above-mentioned preparation method, an anode contact and a cathode contact are prepared on the driving wafer; and when preparing the pixel layer, the sub-pixels in the pixel layer are all encapsulated inside the insulating body, and a bonding metal part is arranged on the side of each sub-pixel close to the driving wafer, so that the bonding metal part is electrically connected to the corresponding anode contact, and the outside of each sub-pixel is encapsulated by an insulating passivation layer, and the bonding metal part is located inside the insulating passivation layer, and the upper part of the insulating passivation layer has an opening, and the outside of the insulating passivation layer is encapsulated by a common cathode layer, and the sub-pixels are electrically connected to the common cathode layer through the opening, and the common cathode layer is used to be electrically connected to the cathode contact.

[0027] In one embodiment of the present invention, when preparing pixel layers other than the top layer, anode holes are opened on the insulating body and anode connectors are filled in the anode holes, so that the bonding metal parts of the sub-pixels in the pixel layer are electrically connected to the corresponding anode contacts by the anode connectors passing through the underlying pixel layer.

[0028] In one embodiment of the present invention, during preparation, the anode hole needs to be opened on the interface between two adjacent pixel layers, and the top surface of the anode connector filled in the anode hole is lower than the interface to form a recessed portion, and the bonding metal part of the sub-pixel in the pixel layer is embedded in the recessed portion of the corresponding anode hole of the adjacent pixel layer below to be in electrical contact with the anode connector; or,

[0029] The top surface of the anode connector filled in the anode hole is higher than the interface to form a convex portion, and the bonding metal member of the sub-pixel in the pixel layer is embedded with the convex portion of the corresponding anode connector of the adjacent pixel layer below.

[0030] In one embodiment of the present invention, auxiliary pixels are also prepared when the underlying pixel layer is prepared, so that the anode connector in the underlying pixel layer corresponds to the auxiliary pixel, the auxiliary pixel is located in the underlying pixel layer and between two adjacent sub-pixels in the X direction, the X direction is perpendicular to the Z direction, and the anode connector in the underlying pixel layer passes through the corresponding auxiliary pixel and is electrically connected to the corresponding anode contact on the driving wafer.

[0031] In one embodiment of the present invention, after step M2, at least one lens is further connected to the upper part of the pixel layer located at the top layer, so that the lens corresponds to the mother pixel one-to-one, or each lens corresponds to the sub-pixel one-to-one.

[0032] The above technical solution of the present invention has the following advantages compared with the prior art:

[0033] The multi-color micro-display chip and the preparation method thereof of the present invention effectively increase the number of red sub-pixels, thereby effectively controlling the attenuation of red light in the mother pixel, thereby ensuring an ideal color display effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to make the contents of the present invention more clearly understood, the present invention is further described in detail below based on specific embodiments of the present invention in conjunction with the accompanying drawings.

[0035] Figure 1 It is a brightness curve diagram of a multi-color micro display chip of the present invention;

[0036] Figure 2 This is a schematic diagram of the first pixel distribution of the multi-color micro display chip of the present invention;

[0037] Figure 3 is a second pixel distribution schematic diagram of the multi-color micro display chip of the present invention;

[0038] Figure 4 Schematic diagram of the comparison between trapezoidal sub-pixels and hemispherical sub-pixels;

[0039] Figure 5 1 is an overall structural diagram of the multi-color micro display chip of the present invention (top view);

[0040] Figure 6 yes Figure 5 A partial enlarged view of the middle A;

[0041] Figure 7 is a diagram showing the internal structure of a first mother pixel of the present invention;

[0042] Figure 8 yes Figure 7 Schematic diagram of the layout of the middle and bottom pixel layers;

[0043] Fig. 9 is a diagram showing the internal structure of a second mother pixel of the present invention;

[0044] Fig.10 is a diagram showing the internal structure of a third mother pixel of the present invention;

[0045] Fig.11 yes Fig.10 Schematic diagram of the layout of the middle and bottom pixel layers;

[0046] Fig.12 is a diagram showing the internal structure of a fourth mother pixel of the present invention;

[0047] Fig.13 yes Fig.12 A partial enlarged view of the middle Q;

[0048] Fig.14 is a diagram showing the internal structure of a fifth mother pixel of the present invention;

[0049] Fig.15 yes Fig.14 A partial enlarged view of the S in the middle;

[0050] Fig.16 is a diagram showing the internal structure of a sixth mother pixel of the present invention;

[0051] Fig.17 is a third pixel distribution schematic diagram of the present invention;

[0052] Fig.18 is a diagram showing the internal structure of a seventh mother pixel of the present invention;

[0053] Fig.19 yes Fig.18 Flow chart for the preparation of the structure shown;

[0054] Fig. 20 is a diagram showing the internal structure of an eighth mother pixel of the present invention;

[0055] Fig.21 is a partial preparation flow chart of the chip of the present invention;

[0056] Fig. 22 yes Figure 7 Flow chart for the preparation of the structure shown;

[0057] Description of the Figures in the Specification:

[0058] 10. Mother pixel;

[0059] 20, sub-pixel; 201, P-type ohmic contact layer; 202, P-type semiconductor layer; 203, active layer; 204, N-type semiconductor layer; 205, N-type ohmic contact layer;

[0060] 30, pixel layer; 301, insulating body; 302, bonding layer; 3021, bonding metal part; 3022, conductive metal part; 303, insulating passivation layer; 3031, opening; 304, common cathode layer; 3041, second notch; 3042, auxiliary hole; 305, metal grid layer; 3051, first notch; 306, anode hole; 3061, recessed part; 307, anode connector; 3071, raised part; 308, cathode hole; 309, cathode connector;

[0061] 40. Interface;

[0062] 50, driving wafer; 501, anode contact; 502, cathode contact;

[0063] 60. compound semiconductor; 601. substrate; 70. pixel array region; 80. peripheral common cathode region;

[0064] 90. Auxiliary pixel; 100. Lens. DETAILED DESCRIPTION

[0065] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.

[0066] In the description of the present invention, it should be understood that the terms "vertical", "upper", "lower", "top", "side", "inner", "outer", etc., indicating the orientation or positional relationship are based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.

[0067] See also Figure 1-Figure 22 , this embodiment discloses a multi-color micro display chip, including a mother pixel 10, a driving wafer 50 and at least two pixel layers 30;

[0068] The mother pixel 10 includes at least four sub-pixels 20, at least two sub-pixels 20 in the mother pixel 10 have different light emitting colors, and at least two sub-pixels 20 have red light emitting colors, and the number of sub-pixels with red light emitting colors is not less than 50% of the total number of sub-pixels in the mother pixel 10;

[0069] The sub-pixels 20 are all electrically connected to the driving wafer 50, and the driving wafer 50 has a driving circuit to control the sub-pixels 20 to emit light by using the driving circuit; the driving wafer 50 can be a CMOS driving wafer;

[0070] At least two pixel layers 30 are provided, and all pixel layers 30 are stacked in sequence along the Z direction on the driving wafer 50. All sub-pixels 20 of the mother pixel 10 are respectively provided in the corresponding pixel layers 30. At least one sub-pixel 20 is provided in each pixel layer 30. The light emitting color of each sub-pixel 20 in the same pixel layer 30 is the same, and the light emitting colors of the sub-pixels 20 in two adjacent pixel layers 30 are different.

[0071] Furthermore, the number of sub-pixels with red light emission color may be 50% to 90% of the total number of sub-pixels in the mother pixel 10 ; specifically, it may be 60%, 65%, 70%, 75%, 85%, etc.

[0072] It should be noted that the specific pixel layer in which the sub-pixels of different colors are located can be selected as needed and is not limited here;

[0073] In the above structure, by making the mother pixel include at least four sub-pixels and making the number of sub-pixels that produce red light color greater than or equal to 50% of the total number of sub-pixels in the mother pixel, the number of red sub-pixels is effectively increased, so that the attenuation of red light in the mother pixel can be effectively controlled, so that the brightness ratio of various colors can be maintained at a specific ratio, thereby achieving an ideal color display effect.

[0074] Among them, the sub-pixels 20 all include a P-type semiconductor layer 202, an active layer 203 and an N-type semiconductor layer 204 arranged in sequence along the Z direction, wherein the active layer 203 is used to emit light, the P-type semiconductor layer 202 is arranged close to the driving wafer 50, and a P-type ohmic contact layer 201 is also arranged on the side of the P-type semiconductor layer 202 close to the driving wafer 50, the P-type semiconductor layer 202 is used to be connected to the anode of the driving wafer 50 to achieve anode connection, and the N-type semiconductor layer 204 is used to be connected to the cathode of the driving wafer 50 to achieve cathode connection.

[0075] It should be noted that, for the convenience of description, the micro display chip in the present invention has a Z direction, an X direction and a Y direction, and the three directions are perpendicular to each other, wherein the Z direction is generally the direction away from the driving wafer, and the "up" and "down" in the present invention are relative in the Z direction, and similarly, "top", "bottom" or "high" and "low" are also relative in the Z direction. The top pixel layer refers to the topmost pixel layer, and the bottom pixel layer refers to the bottommost pixel layer, wherein the bottom pixel layer is also referred to as the first pixel layer, and the pixel layers stacked sequentially above are the second layer, the third layer, and so on.

[0076] The following will be combined Figure 1-Figure 22 , the structure of the multi-color micro display chip of this embodiment is further described in detail.

[0077] Embodiment 1

[0078] See also Figure 1-Figure 6 , this embodiment discloses a multi-color micro display chip, including a mother pixel 10, a driving wafer 50 and three pixel layers 30;

[0079] The mother pixel 10 includes at least four sub-pixels 20, at least two sub-pixels 20 in the mother pixel 10 have different light emitting colors, and at least two sub-pixels 20 have red light emitting colors, and the number of sub-pixels with red light emitting colors is not less than 50% of the total number of sub-pixels in the mother pixel 10;

[0080] The sub-pixels 20 are all electrically connected to the driving wafer 50 so as to utilize the driving wafer 50 to control the sub-pixels 20 to emit light;

[0081] The three pixel layers 30 are stacked in sequence along the Z direction, and all the sub-pixels 20 of the mother pixel 10 are respectively arranged in the corresponding pixel layers 30. At least one sub-pixel 20 is arranged in each pixel layer 30. The light output color of each sub-pixel 20 in the same pixel layer 30 is the same, and the light output colors of the sub-pixels 20 in two adjacent pixel layers 30 are different.

[0082] For ease of description, the sub-pixel 20 with a red light-emitting color is referred to as a red sub-pixel, the sub-pixel 20 with a green light-emitting color is referred to as a green sub-pixel, and the sub-pixel 20 with a blue light-emitting color is referred to as a blue sub-pixel;

[0083] The above-mentioned mother pixel has three sub-pixels with different light emitting colors, namely red sub-pixel R, green sub-pixel G and blue sub-pixel B. The above-mentioned three sub-pixels are respectively located in different pixel layers. The red sub-pixels can be arranged in the first pixel layer (bottom pixel layer), the green sub-pixels can be arranged in the second pixel layer, and the blue sub-pixels can be arranged in the third pixel layer (top pixel layer). In actual working conditions, the specific pixel layer where the sub-pixels of different colors are located can be selected as needed, and no limitation is made here;

[0084] For example, Figure 2 and Figure 3 As shown, the mother pixel 10 includes four sub-pixels 20, and the four sub-pixels 20 include a red sub-pixel R, a green sub-pixel G, and a blue sub-pixel B. The red sub-pixel R is used to emit red light, the green sub-pixel G is used to emit green light, and the blue sub-pixel B is used to emit blue light. The micro display chip includes a plurality of mother pixels 10, and the four sub-pixels 20 in each mother pixel 10 can be arranged according to Figure 2 The arrangement is in the RGRB manner shown in the figure, with one green sub-pixel G and one blue sub-pixel B, and two red sub-pixels R arranged diagonally, or in the manner of Figure 3The arrangement is in the RRGB manner shown in the figure, with one green sub-pixel G and one blue sub-pixel B, and two red sub-pixels R, arranged in a row in the Y direction; if the combination of four sub-pixels still cannot meet the light distribution requirements of red light, the surrounding red sub-pixels can continue to be used for light distribution, for example Figure 2 In the figure, the mother pixel at the lower right corner can call a red sub-pixel in the upper mother pixel for light distribution, or Figure 3 In the figure, the mother pixel located in the lower left corner can call the two red sub-pixels in the mother pixel on the right for light distribution.

[0085] Figure 1 is the brightness curve of the mother pixel 10, Figure 1 In the figure, "G" represents the brightness curve of the green sub-pixel, "B" represents the brightness curve of the blue sub-pixel, "R75%" represents the brightness curve of all red sub-pixels that account for 75% of the mother pixel, "R50%" represents the brightness curve of all red sub-pixels that account for 50% of the mother pixel, and "R25%" represents the brightness curve of all red sub-pixels that account for 25% of the mother pixel. Figure 1 It can be seen from the brightness curve shown that when the number of red sub-pixels in the mother pixel is 50% or 75%, compared to 25%, its brightness curve moves upward and the overall brightness increases, thereby effectively controlling the attenuation of red light and being more conducive to ensuring the stability of light distribution, thereby achieving an ideal color display effect.

[0086] It can be understood that the number of sub-pixels 20 in the mother pixel 10 can be greater than four, and the specific number is not limited here.

[0087] Furthermore, the projections of all sub-pixels 20 in the mother pixel 10 on the driving wafer 50 do not overlap, so as to minimize the optical crosstalk between the sub-pixels 20 or the color noise caused by photoexcitation, thereby more accurately controlling the light combining effect.

[0088] Figure 5 is a top view of a micro display chip. Each micro display chip includes a plurality of mother pixels 10 arranged in an array to form a pixel array area 70, and a peripheral common cathode area 80 is provided on the periphery. Figure 6 yes Figure 5 The partial enlarged image at A in the middle shows the common cathode area of ​​a mother pixel and its surrounding parts. Figure 7 yes Figure 6 A cross-sectional view of the structure at the a1-a2 path; a cross-sectional view of the subsequent mother pixel, such as Figure 8-Figure 16 , Fig.18 , Fig. 20 etc. are also cross-sectional views at the path;

[0089] In one embodiment, if Figure 7As shown, the sub-pixel 20 is trapezoidal or cylindrical. Compared with the pixels of hemispherical structure or hemispherical structure, the trapezoidal or cylindrical sub-pixel can effectively increase the pixel light-emitting area, thereby increasing the light-emitting intensity; the sub-pixel 20 generally has an active layer 203 to emit light, Figure 4 It can be seen that, when the bottom size of the sub-pixel is the same, the area of ​​the active layer 203 in the trapezoidal sub-pixel (the entire shaded portion) is larger than the area of ​​the active layer in the hemispherical sub-pixel (the shaded portion inside the hemispherical shape), thereby effectively increasing the luminous intensity. Similarly, the cylindrical sub-pixel can also increase the area of ​​the active layer compared to the hemispherical sub-pixel, thereby effectively increasing the luminous intensity.

[0090] Further, the inclination angle θ of the side wall of the sub-pixel 20 relative to the driving wafer 50 is 45° to 135°; it can be understood that the side wall of the sub-pixel 20 here refers to the wall surface located between the top surface and the bottom surface of the sub-pixel 20;

[0091] The above-mentioned tilt angle can reduce total reflection and is more conducive to light extraction. Exceeding this range will reduce the light extraction efficiency. In addition, due to limited horizontal space, a certain amount of space needs to be reserved for subsequent processes. If the tilt angle is too small, the bottom surface of the pixel occupies too much horizontal space, which will increase the difficulty of pixel spacing arrangement.

[0092] Preferably, the inclination angle θ of the side wall of the sub-pixel 20 relative to the driving wafer 50 is 75° to 105°, which has the best light extraction efficiency and the best pixel pitch design.

[0093] In one embodiment, an anode contact 501 and a cathode contact 502 are provided on the driving wafer 50, each pixel layer 30 includes an insulating body 301, and the sub-pixels 20 in the pixel layer 30 are all covered inside the insulating body 301, and a bonding metal part 3021 is provided on a side of each sub-pixel 20 close to the driving wafer 50, that is, each sub-pixel 20 has a bonding metal part 3021, and the bonding metal part 3021 is electrically connected to the corresponding anode contact 501;

[0094] The outside of each sub-pixel 20 is covered with an insulating passivation layer 303, the bonding metal part 3021 is located inside the insulating passivation layer 303, the upper part of the insulating passivation layer 303 has an opening 3031, the outside of the insulating passivation layer 303 is covered with a common cathode layer 304, the sub-pixel 20 is electrically connected to the common cathode layer 304 through the opening 3031, and the common cathode layer 304 is used to be electrically connected to the cathode contact 502.

[0095] It can be understood that the sub-pixel 20 includes a P-type ohmic contact layer 201, a P-type semiconductor layer 202, an active layer 203 and an N-type semiconductor layer 204 which are sequentially arranged upward along the Z direction. The P-type semiconductor layer 202 is provided with a bonding metal part 3021 on one side close to the driving wafer 50. The P-type ohmic contact layer 201 is arranged between the P-type semiconductor layer 202 and the bonding metal part 3021, so that the P-type semiconductor layer 202 and the bonding metal part 3021 are in ohmic contact, so that the P-type semiconductor layer 202 is finally electrically connected to the corresponding anode contact 501 through the bonding metal part 3021, and the N-type semiconductor layer is exposed at the above-mentioned opening 3031, and the exposed part is electrically connected to the common cathode layer 304. The insulating passivation layer 303 is used to insulate and isolate the N-type semiconductor layer 204 and the P-type semiconductor layer 202 in the sub-pixel 20 to avoid short circuit.

[0096] The bonding metal parts 3021 may correspond to the anode contacts 501 one by one, or multiple anode contacts 501 may correspond to one bonding metal part 3021 .

[0097] In some embodiments, Fig. 22 As shown in stage d, the height D of the sub-pixel 20 in the Z direction is 0.3um to 5um; preferably, D is 0.3um to 1.5um; wherein the height of the sub-pixel 20 is the distance between its P-type semiconductor layer 202 and N-type semiconductor layer 204 (including the thickness of the P-type semiconductor layer 202 to the N-type semiconductor layer 204 itself).

[0098] In some embodiments, the P-type ohmic contact layer 201 has a thickness of 10 nm to 300 nm, and its material may be a transparent conductive film such as indium tin oxide (ITO), indium zinc oxide (IZO), indium gallium zinc oxide (IGZO), or a metal alloy film such as AuBe, AnZn, etc.

[0099] In some embodiments, the thickness d1 of the insulating passivation layer 303 is 30 nm to 500 nm to better ensure the insulating and passivation capabilities.

[0100] In some embodiments, the thickness d2 of the common cathode layer 304 is 50 nm to 500 nm, so as to maximize its transmittance while ensuring the current expansion capability. The thicker the common cathode layer 304 is, the better the current expansion, but the lower the transmittance, which will cause greater light loss and increase the processing difficulty. If the thickness is too thin, it will affect the metal current expansion capability.

[0101] In one embodiment, the bonding metal part 3021 carried by the sub-pixel 20 in the upper pixel layer 30 is electrically connected to the corresponding anode contact 501 by the anode connector 307 passing through the lower pixel layer 30, and the other pixel layers 30 except the top layer are provided with an anode hole 306 corresponding to the anode connector 307, and the anode hole 306 is filled with an anode metal material to form the anode connector 307, so as to realize the anode connection between the upper sub-pixel 20 and the driving wafer 50 through the anode connector 307.

[0102] It can be understood that the sub-pixels in the bottom pixel layer can be directly connected to the corresponding anode contacts through the bonding metal parts.

[0103] In one embodiment, the length of the top end (in the X direction) of the anode hole 306 is greater than the length of the bottom end.

[0104] In one embodiment, if Figure 8 As shown, the angle φ between the inner wall of the anode hole 306 and the top surface of the driving wafer 50 is 90° to 120°.

[0105] Furthermore, the anode hole 306 may be in a trapezoidal shape or a Y-shape.

[0106] In some embodiments, Figure 8 As shown, in the Z direction, the spacing H between the top surface of the insulating body 301 of each pixel layer 30 and the common cathode layer 304 at the top of the sub-pixel of this layer is not less than 100 nm to prevent interlayer leakage caused by insulation abnormality.

[0107] In one embodiment, an anode hole 306 corresponding to the anode connector 307 is opened on the interface 40 of two adjacent pixel layers, and the anode hole 306 is filled with the anode connector 307. Figure 7-Figure 9 As shown, the top surface of the anode connector 307 filled in the anode hole 306 is lower than the interface 40 to form a recessed portion 3061, and the bonding metal member 3021 of the sub-pixel 20 in the pixel layer is embedded in the recessed portion 3061 of the corresponding anode hole 306 of the adjacent pixel layer below and is in electrical contact with the anode connector 307;

[0108] Or, if Figure 10-11As shown, the top surface of the anode connector 307 filled in the anode hole 306 is higher than the interface 40 to form a protrusion 3071, and the bonding metal part 3021 of the sub-pixel 20 in the pixel layer is embedded with the protrusion 3071 of the corresponding anode connector 307 of the adjacent pixel layer below. This embedding method can avoid the formation of bonding voids between the bonding metal part 3021 and the anode connector 307, which will lead to poor electrical transmission. The above-mentioned convex-concave embedding method can effectively avoid the above-mentioned problems and ensure excellent electrical transmission effects. At the same time, it also effectively increases the connection stability and connection strength between the bonding metal part 3021 and the anode connector 307.

[0109] Further, such as Figure 8 As shown, the height h1 of the recessed portion 3061 is 10 nm to 300 nm. Fig.11 As shown, the height h2 of the protrusion 3071 is 10nm to 300nm to better avoid bonding voids and ensure electrical transmission effect. The above height should not be too large, which will easily increase the process difficulty. If the height is too small, the electrical transmission effect cannot be better guaranteed.

[0110] In one embodiment, the micro display core includes three pixel layers 30, the bottom pixel layer is also referred to as the first pixel layer, and the pixel layers stacked sequentially thereon are sequentially the second layer, the third layer, and so on, then the bonding metal parts 3021 of the sub-pixels in the third and above pixel layers can be electrically connected to the corresponding anode contacts 501 by the multiple anode connectors 307 sequentially connected along the Z direction below, and the respective anode connectors 307 sequentially connected along the Z direction are respectively located in different pixel layers 30;

[0111] Among them, Fig.16 As shown, two adjacent anode connectors 307 along the Z direction are in direct contact with each other. This method does not retain the bonding metal parts and other components between the two adjacent anode connectors. This method is more conducive to avoiding the phenomenon of poor electrical transmission caused by bonding voids.

[0112] Or, if Fig.14 As shown, a conductive metal part 3022 may also be provided between two anode connectors 307 adjacent to each other in the Z direction. This method retains the bonding metal parts of the two anode connectors 307 as the conductive metal part 3022, and the processing technology is simpler.

[0113] In one embodiment, the length of the top of the anode connector 307 in the X direction is greater than the length of the bottom, that is, it presents a structure that is wide at the top and narrow at the bottom. When the bottom length is the same, this shape of structure can obtain a thicker anode connector compared to the structure that is narrow at the top and wide at the bottom, thereby enhancing the electrical transmission capacity of the anode.

[0114] In one embodiment, cathode holes 308 are provided in pixel layers 30 other than the top layer, cathode holes 308 are filled with cathode connectors 309, cathode connectors 309 are electrically connected to cathode contacts 502, and common cathode layers 304 in the upper pixel layers are electrically connected to cathode contacts 502 via cathode connectors 309 in the lower pixel layers.

[0115] It can be understood that, in the specific arrangement, the common cathode layer 304 of the pixel layer of the third layer is electrically connected to the cathode contact 502 through the cathode connectors 309 in the second layer and the first layer in turn, the common cathode layer 304 of the pixel layer of the second layer is electrically connected to the cathode contact 502 through the cathode connector 309 in the first layer in turn, and the common cathode layer 304 of the pixel layer of the first layer can be directly electrically connected to the cathode contact 502; or, the cathode connector 309 of the second layer can be directly connected to the cathode contact 502, in which case, the common cathode layer 304 of the pixel layer of the third layer can also be directly electrically connected to the cathode contact 502 through the cathode connector 309 in the second layer. That is, the common cathode layer 304 in each pixel layer can be electrically connected to the cathode contact 502 through multiple cathode connectors 309 in the lower pixel layer in turn, and can also be directly electrically connected to the cathode contact 502 through the pixel layer of the adjacent layer below.

[0116] Furthermore, a cathode hole 308 is also opened on the interface 40 between two adjacent pixel layers 30, and the top surface of the cathode connector 309 filled in the cathode hole 308 is lower than the interface 40 to form a recessed portion, or the top surface of the cathode connector 309 filled in the cathode hole 308 is higher than the interface 40 to form a raised portion, which is similar to the setting method of the anode connector 307 and will not be repeated here.

[0117] In one embodiment, if Fig.12 and Fig.14 As shown, the interface 40 between two adjacent pixel layers 30 is also covered by the insulating passivation layer 303 , the upper part of the insulating passivation layer 303 at the interface is covered by the common cathode layer 304 , and a metal grid layer 305 is provided on the upper part of the common cathode layer 304 to achieve the effect of cathode current enhancement through the metal grid layer 305 .

[0118] Furthermore, the metal grid layer 305 can be made of one or more materials selected from the group consisting of Cr, Pt, Ti, Au, Al, Cu, TiN and TaN.

[0119] In one embodiment, the thickness d3 of the metal grid layer 305 is 100nm to 5000nm, which is relatively thin. This increases the distance between the metal grid layer 305 and the upper bonding metal part 3021, so that there is enough space between the metal grid layer 305 and the upper bonding metal part 3021 to fill the insulating body 301, thereby effectively avoiding the risk of short circuit between the metal grid layer 305 and the upper bonding metal part 3021, thereby improving insulation and increasing safety.

[0120] In one embodiment, if Figure 12-13 As shown, the light emitted from the sub-pixel 20 in the lower pixel layer is emitted through the first notch 3051 in the upper pixel layer. The first notch 3051 is opened on the metal grid layer 305. The length L1 of the first notch 3051 in the X direction is greater than the top surface length L2 of the sub-pixel 20 corresponding to the lower layer, so that the light emitted from the sub-pixel 20 in the lower layer can be emitted through the first notch 3051 to the greatest extent, thereby improving the light extraction efficiency of the pixel.

[0121] It is understandable that the “corresponding sub-pixel” here refers to the sub-pixel 20 through which the incident light passes through the first notch 3051. If the sizes of all sub-pixels in this layer are the same, then the length L1 of the first notch 3051 in the X direction is greater than the top surface length L2 of each sub-pixel in this layer.

[0122] The above method opens a first gap 3051 on the metal grid layer 305 at the interface 40 between two adjacent pixel layers 30, that is, removes the metal grid material in the first gap 3051, so as to reduce the shielding of the metal grid in the original gap on the light emitted by the bottom sub-pixel, so that the light emitted by the sub-pixel in the lower pixel layer does not need to be emitted through the metal grid layer 305, thereby reducing light loss and making the bottom sub-pixel have higher light extraction efficiency.

[0123] In the above method, a notch may be provided only on the metal grid layer 305 , but not on the common cathode layer 304 .

[0124] The number of the first openings 3051 may be determined according to the number of the lower layer sub-pixels 20 .

[0125] In addition, a large gap may be opened in the metal grid layer 305 of the top pixel layer, so that the length of the large gap in the X direction is greater than the sum of the top surface lengths of all sub-pixels in the two layers below through which the light is emitted.

[0126] The metal grid layer 305 in each pixel layer 30 is a whole, and the first notch 3051 is equivalent to a hole opened on the metal grid layer 305 .

[0127] In one embodiment, if Figure 14-15 As shown, the light emitted from the sub-pixel 20 in the lower pixel layer is emitted after passing through the second notch 3041 and the first notch 3051 in the upper pixel layer in sequence. The second notch 3041 is opened on the common cathode layer 304, and the length L3 of the second notch 3041 in the X direction is greater than the top surface length L2 of the corresponding sub-pixel in the lower layer.

[0128] It can be understood that the "corresponding sub-pixels" here refer to the sub-pixels 20 through which the incident light passes through the second notch 3041 and the first notch 3051 in sequence. If the sizes of all sub-pixels in this layer are the same, then the length of the second notch 3041 in the X direction is greater than the top surface length of each sub-pixel in this layer.

[0129] The above method opens a second notch 3041 on the common cathode layer 304 at the interface 40 between two adjacent pixel layers 30, that is, removes the common cathode material in the second notch 3041, so that the light emitted by the sub-pixel 20 in the lower pixel layer 30 does not need to be emitted through the common cathode, further reducing light loss and allowing the bottom sub-pixel to have a higher light extraction efficiency.

[0130] The number of the second notches 3041 may be determined according to the number of the lower layer sub-pixels 20 , and the second notches 3041 and the first notches 3051 may correspond one to one.

[0131] The common cathode layer 304 in each pixel layer 30 is a whole, and the second notch 3041 is equivalent to a hole opened on the common cathode layer 304 .

[0132] The anode connector 307 in the bottom pixel layer 30 can be arranged in the following two ways:

[0133] In one embodiment, a separate space is reserved between two adjacent sub-pixels 20 in the X direction in the bottom pixel layer to provide an anode connector 307, wherein the X direction is perpendicular to the Z direction;

[0134] In another method, the original sub-pixel 20 is retained as an auxiliary pixel 90 between two adjacent sub-pixels 20 in the X direction in the bottom pixel layer, so that the anode connector 307 in the bottom pixel layer passes through an auxiliary pixel 90 and is electrically connected to the corresponding anode contact 501 on the driving wafer 50. This method can avoid re-preparing the bottom pixel layer and can directly use the original single-layer monochrome product, that is, the second layer and above pixel layers can be directly superimposed on the original single-layer product for use. The preparation method is faster and can reduce the cost of preparing the bottom pixel layer separately.

[0135] It should be noted that after the auxiliary pixel 90 is penetrated by the anode connector 307 , the auxiliary pixel 90 cannot emit light normally and is only used as a connector.

[0136] It can be understood that the anode connector 307 needs to pass through the common cathode layer 304 outside the auxiliary pixel 90 and the insulating passivation layer 303 in sequence and then be electrically connected to the anode contact 501 of the driving wafer 50. In order to prevent the anode connector 307 from contacting the common cathode layer 304 outside the auxiliary pixel 90, an auxiliary hole 3042 is provided on the common cathode layer 304 for the anode connector 307 to pass through. Fig.19 In the middle stage a, the length L4 of the auxiliary hole 3042 in the X direction is greater than the length L5 of the opening 3031 of the insulating passivation layer 303 at the top of the auxiliary pixel 90 .

[0137] In one embodiment, at least one lens 100 is connected to the upper part of the pixel layer at the top layer. The lenses 100 can be arranged in the following two ways: one is that the lenses 100 correspond to the mother pixels 10 one by one, and the other is that each lens 100 corresponds to the sub-pixel 20 one by one. This method can better collimate the outgoing light of each sub-pixel 20 and further reduce the light interference in the mother pixel;

[0138] This embodiment also discloses a method for preparing a micro display chip, comprising:

[0139] Step M1, preparing a driving wafer 50;

[0140] Step M2, stacking three pixel layers 30 in sequence along the Z direction on the driving wafer 50, so that all sub-pixels 20 in the mother pixel 10 are respectively arranged in the corresponding pixel layers 30, at least one sub-pixel 20 is arranged in each pixel layer 30, the light output color of each sub-pixel 20 in the same pixel layer is the same, the light output colors of the sub-pixels 20 in two adjacent pixel layers are different, and the sub-pixels 20 are all electrically connected to the driving wafer 50, so that the driving wafer 50 can be used to drive the sub-pixels 20 to emit light.

[0141] In one of the embodiments, when preparing the driving wafer 50, an anode contact 501 and a cathode contact 502 need to be prepared on the driving wafer 50; and when preparing the pixel layer 30, the sub-pixels 20 in the pixel layer 30 are all enclosed inside the insulating body 301, and a bonding metal part 3021 is arranged on the side of each sub-pixel 20 close to the driving wafer 50, so that the bonding metal part 3021 is electrically connected to the corresponding anode contact 501, and the outside of each sub-pixel 20 is enclosed by an insulating passivation layer 303, and the bonding metal part 3021 is located inside the insulating passivation layer 303, and the upper part of the insulating passivation layer 303 has an opening 3031, and the outside of the insulating passivation layer 303 is enclosed by a common cathode layer 304, and the sub-pixels 20 are electrically connected to the common cathode layer 304 through the opening 3031, and the common cathode layer 304 is used to be electrically connected to the cathode contact 502.

[0142] During the specific preparation, step M2 includes:

[0143] Step M21, bonding a compound semiconductor 60 onto the driver wafer 50;

[0144] like Fig.21 As shown, the compound semiconductor 60 includes a P-type ohmic contact layer 201, a P-type semiconductor layer 202, an active layer 203, an N-type semiconductor layer 204 and a substrate 601 which are sequentially arranged away from the driving wafer. After the compound semiconductor 60 is bonded to the driving wafer 50, the substrate 601 needs to be removed to expose the N-type semiconductor layer 204. After removing the substrate 601, an N-type ohmic contact layer 205 may be further arranged on the N-type semiconductor layer 204.

[0145] Furthermore, the thickness of the N-type ohmic contact layer 205 is in the range of 10 nm to 300 nm, and its material can be a transparent conductive film such as indium tin oxide (ITO), indium zinc oxide (IZO), indium gallium zinc oxide (IGZO), or a metal alloy film such as gold germanium alloy (AuGe), gold nickel alloy (AuNi), etc.

[0146] Preferably, the thickness of the N-type ohmic contact layer 205 is 10 nm to 100 nm, so as to ensure ohmic contact and also have a higher transmittance, thereby reducing light loss.

[0147] The compound semiconductor 60 may be bonded to the driving wafer 50 via the bonding layer 302 , and the bonding alignment accuracy may be 10 to 500 um.

[0148] Step M22: patterning and etching the compound semiconductor 60 to obtain at least one sub-pixel 20, so that the sub-pixel 20 is electrically connected to the corresponding anode contact 501 through the bonding layer 302; the bonding layer 302 includes a plurality of bonding metal parts 3021, so that each sub-pixel 20 corresponds to a bonding metal part 3021, and the sub-pixel 20 is electrically connected to the corresponding anode contact 501 through the corresponding bonding metal part 3021;

[0149] Wherein, each bonding metal member 3021 is obtained by etching the bonding layer 302; the anode contact 501 here corresponds to the sub-pixel 20 one by one, or multiple anode contacts 501 correspond to one sub-pixel 20; step M23, depositing an insulating passivation layer 303 outside the sub-pixel 20, and setting an opening 3031 on the upper part of the insulating passivation layer 303 to expose the N-type semiconductor layer 204 or the N-type ohmic contact layer 205 of the sub-pixel 20;

[0150] Step M24, depositing a common cathode layer 304 outside the insulating passivation layer 303, so that the sub-pixel 20 is electrically connected to the common cathode layer 304 through the opening 3031, and the common cathode layer 304 is used to be electrically connected to the cathode contact 502, see Fig. 22 Middle d stage;

[0151] That is, the N-type semiconductor layer 204 of the sub-pixel 20 is electrically connected to the cathode contact 502 through the common cathode layer 304 to achieve cathode connection;

[0152] Among them, only one cathode contact 502 may be provided on the driving wafer 50 , or the number of cathode contacts 502 may be determined according to needs.

[0153] Step M25: Fill the insulating body 301 outside the common cathode layer 304 so that all sub-pixels 20 are located inside the insulating body 301, thereby obtaining a pixel layer 30. Fig. 22 Middle e stage;

[0154] It can be understood that the insulating passivation layer 303 and the common cathode layer 304 outside the sub-pixel 20 are also located inside the insulating body 301 .

[0155] Step M26: Bond another compound semiconductor 60 to the top of the previous pixel layer through the bonding layer 302, and perform steps M22 to M25 to obtain the next pixel layer. Fig. 22 Middle f stage;

[0156] Step M27: Repeat step M26 until all pixel layers 30 are prepared. Fig. 22 Middle g stage;

[0157] The light emitting colors of each sub-pixel in the same pixel layer are the same, and the light emitting colors of the sub-pixels in two adjacent pixel layers are different.

[0158] It is understandable that the bonding metal part 3021 between adjacent anode connectors in the Z direction can be directly used as the conductive metal part 3022. It is understandable that, since the light emission colors of the sub-pixels in two adjacent pixel layers are different, the materials of the compound semiconductor 60 used in the preparation of the two adjacent pixel layers are also different, so that the light emission colors of the compound semiconductor 60 used are different; when each pixel layer 30 is prepared, the light emission color of the selected compound semiconductor 60 is determined according to the actual situation. If it is necessary to prepare a sub-pixel with a red light emission color, a compound semiconductor with a red light emission color is selected.

[0159] The compound semiconductor 60 uses inorganic compound materials, such as the compound semiconductor corresponding to the blue light pixel layer uses InGaN material, the compound semiconductor corresponding to the green light pixel layer uses InGaN material, and the compound semiconductor corresponding to the red light pixel layer uses InGaN or AlGaInP material.

[0160] In practical applications, the film layers of compound semiconductors will be more complicated, or there will be cross-use of materials. The typical compound semiconductor structure mainly includes a P-type semiconductor layer, an N-type semiconductor layer, an active layer (MQW active quantum well) sandwiched between the two, and other functional layers. For the materials of each film layer of red light compound semiconductors, please refer to Table 1, and for the materials of each film layer of green and blue light compound semiconductors, please refer to Table 2;

[0161] Table 1 Material table of each film layer of compound semiconductor (R)

[0162] Layer Name Material Material Material Material Material Material P-type semiconductor layer GaP GaAs GaAs GaN GaN GaN MQW Active Quantum Well AlGaInP AlGaInP AlGaAs InGaN InGaN InGaN N-type semiconductor layer GaAs AlGaAs GaAs GaN GaN GaN Substrate GaAs GaAs GaAs GaN Si Sapphire

[0163] Table 2 Material table of each film layer of compound semiconductor (G / B)

[0164] Layer Name Material Material Material P-type semiconductor layer GaN GaN GaN MQW Active Quantum Well InGaN InGaN InGaN N-type semiconductor layer GaN GaN GaN Substrate GaN Si Sapphire

[0165] In one embodiment, the insulating passivation layer 303 may be made of one or more of aluminum oxide, silicon dioxide, and silicon nitride.

[0166] In one embodiment, the insulating body 301 may be made of one or more of silicon oxide, silicon nitride, silicon carbide (SiC), silicon carbon nitride (SiCN), phosphate glass (PSG) and borophosphosilicate glass (BPSG).

[0167] In one embodiment, the common cathode layer 304 includes one or more of indium tin oxide (ITO), indium zinc oxide (IZO), Al-doped zinc oxide (AZO), Al-doped indium tin oxide, Ag-doped indium tin oxide, and Au-doped indium tin oxide;

[0168] In one embodiment, the metal grid layer 305 can be made of one or more materials selected from the group consisting of Cr, Pt, Ti, Au, Al, Cu, TiN and TaN.

[0169] In one embodiment, the material of the anode connector 307 can be one or more of aluminum, copper, and tungsten.

[0170] Furthermore, the material of the cathode connector 309 can be the same as that of the anode connector, that is, a conductive material.

[0171] In one embodiment, the material of the bonding metal part 3021 can be one of Al, Au, and Cu, or a stacked structure of Ni, Au, Cu, etc. and Sn, or a bonding stack of Au, In, Ge, or a bonding stack of Au and Si.

[0172] Furthermore, the bonding metal part 3021 may adopt the following structure: Cr2nm / Pt50nm / T i 10nm / Pt50nm / Au100nm / Sn150nm / Au50nm, wherein Cr is an adhesion layer and Pt / T i / Pt is a barrier layer.

[0173] Further, after all pixel layers are prepared in step M2, refer to Fig. 22 In the middle h stage, a dielectric layer is deposited on the top pixel layer, and the dielectric layer is patterned and etched to form a lens 100, so that the lens 100 corresponds to the mother pixel 10 one by one, that is, one mother pixel 10 corresponds to one lens 100; or, each lens 100 corresponds to the sub-pixel 20 one by one, that is, each sub-pixel 20 corresponds to a lens 100 separately, so as to better collimate the output light of each sub-pixel 20 and further reduce the light interference in the mother pixel;

[0174] In one embodiment, when preparing pixel layers other than the top layer, an anode hole 306 is opened on the insulating body 301, and an anode metal material is filled in the anode hole 306 to form an anode connector 307, so that the bonding metal part 3021 of the sub-pixel 20 in the pixel layer 30 is electrically connected to the corresponding anode contact 501 by the anode connector 307 passing through the pixel layer 30 below.

[0175] After the insulating body 301 is prepared, CMP planarization may be performed first, and then patterned dry etching may be performed on the insulating body 301 to prepare the anode hole 306 .

[0176] Furthermore, when the anode connector 307 is specifically prepared, an anode hole 306 is firstly opened on the interface 40 of two adjacent pixel layers, and then an anode metal material is filled in the anode hole 306 to form the anode connector 307, and finally the top surface of the anode connector 307 filled in the anode hole 306 is lower than the interface 40 to form a recessed portion 3061; or,

[0177] Anode metal material is filled in anode hole 306 to form anode connector 307 , so that the top surface of anode connector 307 filled in anode hole 306 is higher than interface 40 to form a protrusion 3071 .

[0178] In some embodiments, auxiliary pixels 90 are also prepared when the underlying pixel layer is prepared, so that the anode connector 307 in the underlying pixel layer corresponds to the auxiliary pixel 90, and a through anode hole 306 is prepared in the auxiliary pixel 90, and an anode metal material is filled in the anode hole 306 to form the anode connector 307, so that the anode connector 307 located in the underlying pixel layer passes through the corresponding auxiliary pixel 90 and is electrically connected to the corresponding anode contact 501 on the driving wafer 50.

[0179] Through this embodiment, a chip structure with three pixel layers 30 can be prepared, and the light output color of each pixel layer 30 is different. The three pixel layers 30 can be configured as a layer where the red sub-pixel is located, a layer where the green sub-pixel is located, and a layer where the blue sub-pixel is located, respectively, to achieve a three-primary color configuration.

[0180] In one embodiment, pixel structures corresponding to multiple micro display chips can be arranged on each driving wafer 50, and each micro display chip can correspond to an independent bonding layer 302. That is, before preparing the pixels of the micro display chip, multiple non-continuous independent bonding layers 302 can be prepared on the driving wafer 50, so that the bonding layer at this time corresponds one-to-one to the subsequent micro display chip. In the subsequent preparation process of the micro display chip, the bonding layer can be further etched to form multiple bonding metal parts 3021.

[0181] An insulating dielectric layer may be filled between the discontinuous bonding layers 302; the discontinuous bonding layers may achieve better improvement in bonding warpage and utilize metal cost control; in each microdisplay chip, the four sides of the bonding layer 302 are further expanded than the peripheral common cathode region 80, and the expanded width is at least 50um, and further, the expanded width is between 50um and 500um.

[0182] It is understandable that, if necessary, more pixel layers can be stacked on the basis of the above three pixel layers.

[0183] Embodiment 2

[0184] like Figure 17-Figure 20 As shown, the main difference between this embodiment and the first embodiment is that the multi-color micro display chip of this embodiment includes a mother pixel 10, a driving wafer 50 and two pixel layers 30 to achieve a dual-color configuration:

[0185] The mother pixel 10 includes at least four sub-pixels 20, at least two sub-pixels 20 in the mother pixel 10 have different light emitting colors, and at least two sub-pixels 20 have red light emitting colors, and the number of sub-pixels with red light emitting colors is not less than 50% of the total number of sub-pixels in the mother pixel 10;

[0186] The sub-pixels 20 are all electrically connected to the driving wafer 50 so as to utilize the driving wafer 50 to control the sub-pixels 20 to emit light;

[0187] Two pixel layers 30 are stacked in sequence along the Z direction, and all sub-pixels 20 of the mother pixel 10 are respectively arranged in the corresponding pixel layers 30. At least one sub-pixel 20 is arranged in each pixel layer 30. The light output color of each sub-pixel 20 in the same pixel layer 30 is the same, and the light output colors of the sub-pixels 20 in two adjacent pixel layers 30 are different.

[0188] The mother pixel 10 has two sub-pixels 20 with different light emitting colors, namely a red sub-pixel R and a green sub-pixel. The two sub-pixels 20 are respectively located in different pixel layers 30. The red sub-pixels can be arranged in the first pixel layer (bottom pixel layer), and the green sub-pixels can be arranged in the second pixel layer. In actual working conditions, the specific pixel layer where the sub-pixels of different colors are located can be selected as needed, and is not limited here;

[0189] Specifically, the mother pixel 10 includes four sub-pixels 20. The four sub-pixels 20 in each mother pixel 10 can be Fig.17 The arrangement is in the RGRR manner shown in the figure, with three red sub-pixels R and one green sub-pixel G. The specific arrangement can be as follows Fig.18 As shown, three red sub-pixels are arranged in the first pixel layer, and one green sub-pixel is arranged in the second pixel layer; Fig. 20 As shown, one green sub-pixel is arranged in the first pixel layer, and three red sub-pixels are arranged in the second pixel layer.

[0190] Furthermore, the projections of all sub-pixels 20 in the mother pixel 10 on the driving wafer 50 do not overlap, so as to avoid light crosstalk between sub-pixels or color noise caused by photoexcitation to the greatest extent, thereby more accurately controlling the light combining effect.

[0191] In one of the embodiments, the cathode connector 309 in the bottom pixel layer can also pass through an auxiliary pixel 90 and then be electrically connected to the corresponding cathode contact 502 on the driving wafer 50. This method can avoid re-preparing the bottom pixel layer and can directly use the original single-layer monochrome product, that is, the second layer and above pixel layers can be directly superimposed on the original single-layer product for use. The preparation method is faster and can reduce the cost of preparing the bottom pixel layer separately. It can be understood that the cathode connector 309 in the first embodiment can also adopt this setting method of passing through the bottom auxiliary pixel 90, which will not be repeated here.

[0192] In this embodiment, the colors of the sub-pixels in the two pixel layers may be red sub-pixels and blue sub-pixels, or red sub-pixels and other color sub-pixels, which can be selected according to actual needs.

[0193] The preparation method of the micro display chip in this embodiment can be found in Fig.19 The preparation method is basically the same as that of the first embodiment, except that the number of pixel layers stacked is two, and the specific preparation method will not be repeated here.

[0194] The micro display chip and its preparation method of the above-mentioned embodiments effectively increase the number of red sub-pixels, thereby effectively controlling the attenuation of red light in the mother pixel, so that the brightness ratio of various colors can be maintained at a specific ratio, thereby ensuring an ideal color display effect.

[0195] All of the above optional technical solutions can be combined in any way to form optional embodiments of the present invention, that is, any multiple embodiments can be combined to meet the needs of different application scenarios. They are all within the protection scope of this application and will not be described one by one here.

[0196] It should be noted that the above embodiments are merely examples for the purpose of clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

Claims

1. A multi-color micro display chip, characterized in that: include, A mother pixel, wherein the mother pixel includes at least four sub-pixels, at least two of the sub-pixels in the mother pixel have different light emitting colors, and the mother pixel has a sub-pixel with a light emitting color of red, and the number of sub-pixels with a light emitting color of red is not less than 50% of the number of all sub-pixels in the mother pixel; A driving wafer, the sub-pixels are all electrically connected to the driving wafer; At least two pixel layers, all of the pixel layers are stacked in sequence along the Z direction on the driving wafer, all of the sub-pixels of the mother pixel are respectively arranged in the corresponding pixel layers, at least one sub-pixel is arranged in each pixel layer, the light emitting color of each sub-pixel in the same pixel layer is the same, and the light emitting colors of the sub-pixels in two adjacent pixel layers are different.

2. The multi-color micro display chip according to claim 1, characterized in that: The projections of all sub-pixels in the mother pixel on the driving wafer do not overlap.

3. The multi-color micro display chip according to claim 1, characterized in that: The sub-pixel is in a trapezoidal or cylindrical shape.

4. The multi-color micro display chip according to claim 1, characterized in that: An anode contact and a cathode contact are provided on the driving wafer, each of the pixel layers includes an insulating body, the sub-pixels in the pixel layer are all enclosed inside the insulating body, a bonding metal part is provided on the side of each sub-pixel close to the driving wafer, the bonding metal part is electrically connected to the corresponding anode contact, the outside of each sub-pixel is enclosed by an insulating passivation layer, the bonding metal part is located inside the insulating passivation layer, the upper part of the insulating passivation layer has an opening, the outside of the insulating passivation layer is enclosed by a common cathode layer, the sub-pixels are electrically connected to the common cathode layer through the opening, and the common cathode layer is used to be electrically connected to the cathode contact.

5. The multi-color micro display chip according to claim 4, characterized in that: The sub-pixels all include a P-type semiconductor layer, an active layer and an N-type semiconductor layer arranged in sequence along the Z direction, the bonding metal part is arranged on one side of the P-type semiconductor layer close to the driving wafer, and the N-type semiconductor layer is electrically connected to the common cathode layer through the opening.

6. The multi-color micro display chip according to claim 4, characterized in that: The bonding metal members of the sub-pixels in the upper pixel layer are electrically connected to corresponding anode contacts by anode connectors that pass through the lower pixel layer.

7. The multi-color micro display chip according to claim 6, characterized in that: An anode hole corresponding to the anode connector is opened on the interface of two adjacent pixel layers, the anode hole is filled with the anode connector, the top surface of the anode connector filled in the anode hole is lower than the interface to form a recessed portion, and the bonding metal part of the sub-pixel in the pixel layer is embedded in the recessed portion of the corresponding anode hole of the adjacent pixel layer below to be in electrical contact with the anode connector; or, The top surface of the anode connector filled in the anode hole is higher than the interface to form a convex portion, and the bonding metal member of the sub-pixel in the pixel layer is embedded with the convex portion of the corresponding anode connector of the adjacent pixel layer below.

8. The multi-color micro display chip according to claim 7, characterized in that: The present invention comprises at least three pixel layers, wherein the bonding metal parts of the sub-pixels in the third pixel layer and above are electrically connected to the corresponding anode contacts by a plurality of anode connectors connected sequentially along the Z direction below, and each anode connector connected sequentially along the Z direction is respectively located in a different pixel layer, and two adjacent anode connectors among the anode connectors connected sequentially along the Z direction are in direct contact with each other, or a conductive metal part is provided between two adjacent anode connectors.

9. The multi-color micro display chip according to claim 4, characterized in that: A cathode hole is opened on the interface of two adjacent pixel layers, and the cathode hole is filled with a cathode connector, which is electrically connected to the cathode contact. The common cathode layer in the upper pixel layer is electrically connected to the cathode contact through the cathode connector in the lower pixel layer.

10. The multi-color micro display chip according to claim 4, characterized in that: The interface between two adjacent pixel layers is also covered with the insulating passivation layer, the upper part of the insulating passivation layer at the interface is also covered with the common cathode layer, and the upper part of the common cathode layer is provided with a metal grid layer.

11. The multi-color micro display chip according to claim 10, characterized in that: The light emitted by the sub-pixel in the lower pixel layer is emitted through the first notch in the upper pixel layer, the first notch is opened on the metal grid layer, the length of the first notch in the X direction is greater than the top surface length of the sub-pixel corresponding to the lower layer, wherein the X direction is perpendicular to the Z direction.

12. The multi-color micro display chip according to claim 11, characterized in that: The light emitted from the sub-pixel in the lower pixel layer is emitted after passing through the second notch and the first notch in the upper pixel layer in sequence. The second notch is opened on the common cathode layer, and the length of the second notch in the X direction is greater than the top surface length of the sub-pixel corresponding to the lower layer.

13. The multi-color micro display chip according to claim 6, characterized in that: The anode connector in the bottom pixel layer passes through an auxiliary pixel and is electrically connected to a corresponding anode contact on the driving wafer; the auxiliary pixel is located in the bottom pixel layer and between two adjacent sub-pixels in the X direction, wherein the X direction is perpendicular to the Z direction.

14. The multi-color micro display chip according to claim 1, characterized in that: At least one lens is connected to the upper part of the pixel layer located at the top layer, and the lens corresponds to the mother pixel one-to-one, or each lens corresponds to the sub-pixel one-to-one.

15. The method for preparing a multi-color micro display chip according to any one of claims 1 to 14, characterized in that: include, Step M1, preparing a driver wafer; Step M2, stacking at least two pixel layers in sequence along the Z direction on the driving wafer, so that all sub-pixels in the mother pixel are respectively arranged in the corresponding pixel layers, at least one sub-pixel is arranged in each pixel layer, the light output color of each sub-pixel in the same pixel layer is the same, the light output colors of the sub-pixels in two adjacent pixel layers are different, and the sub-pixels are all electrically connected to the driving wafer, so that the driving wafer can be used to drive the sub-pixels to emit light.

16. The preparation method according to claim 15, characterized in that: Anode contacts and cathode contacts are prepared on the driving wafer; and when preparing the pixel layer, the sub-pixels in the pixel layer are all enclosed inside the insulating body, a bonding metal part is arranged on the side of each sub-pixel close to the driving wafer, so that the bonding metal part is electrically connected to the corresponding anode contact, the outside of each sub-pixel is enclosed by an insulating passivation layer, the bonding metal part is located inside the insulating passivation layer, the upper part of the insulating passivation layer has an opening, the outside of the insulating passivation layer is enclosed by a common cathode layer, the sub-pixels are electrically connected to the common cathode layer through the opening, and the common cathode layer is used to be electrically connected to the cathode contact.

17. The preparation method according to claim 16, characterized in that: When preparing other pixel layers except the top layer, anode holes are opened on the insulating body and anode connectors are filled in the anode holes, so that the bonding metal parts of the sub-pixels in the pixel layer are electrically connected to the corresponding anode contacts through the anode connectors passing through the pixel layer below.

18. The preparation method according to claim 17, characterized in that: The anode hole is opened at the interface between two adjacent pixel layers, and the top surface of the anode connector filled in the anode hole is lower than the interface to form a recessed portion, and the bonding metal part of the sub-pixel in the pixel layer is embedded in the recessed portion of the corresponding anode hole of the adjacent pixel layer below to be in electrical contact with the anode connector; or, The top surface of the anode connector filled in the anode hole is higher than the interface to form a convex portion, and the bonding metal member of the sub-pixel in the pixel layer is embedded with the convex portion of the corresponding anode connector of the adjacent pixel layer below.

19. The preparation method according to claim 17, characterized in that: Auxiliary pixels are also prepared when the bottom pixel layer is prepared, so that the anode connector in the bottom pixel layer corresponds to the auxiliary pixel, the auxiliary pixel is located in the bottom pixel layer and between two adjacent sub-pixels in the X direction, the X direction is perpendicular to the Z direction, and the anode connector in the bottom pixel layer passes through the corresponding auxiliary pixel and is electrically connected to the corresponding anode contact on the driving wafer.

20. The preparation method according to claim 15, characterized in that: After step M2, at least one lens is further connected to the upper portion of the pixel layer located at the top layer, so that the lens corresponds to the mother pixel one-to-one, or each lens corresponds to the sub-pixel one-to-one.

Citation Information

Cited By

  • Micro-display device and preparation method

    CN121548176A

  • Multi-color micro-display chip and manufacturing method therefor

    WO2026020867A1

  • Multilayer micro-display chip and method for manufacturing same

    WO2026020868A1

  • Polychrome micro-LED pixel with non-coaxial stacking LED structure

    WO2026103079A1

  • Stacked display unit and manufacturing method therefor

    WO2026130318A1