Laser-electric spark-grinding composite super-hard micro cutter preparation method
Through the laser-electric spark-grinding composite process, combined with laser and electric spark processing, the problem of difficult efficiency and quality in the manufacturing of ultra-hard micro tools is solved, and high-quality and efficient preparation of tools with a diameter of less than 2mm and a large length-to-diameter ratio is achieved. , improves the shape accuracy and surface quality of the tool.
Patent Information
- Application Number
- CN202411116999.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-05
AI Technical Summary
When manufacturing ultra-hard micro tools, the prior art is difficult to ensure high efficiency and high quality, especially in tool processing with a diameter of less than 2mm and a large aspect ratio, there are problems such as tool wear, poor surface quality and low shape accuracy.
Using laser-electric spark-grinding composite technology, ultra-hard micro tools are prepared by combining laser cutting, electric spark perforation, vacuum brazing, laser diameter reduction, spiral slot electric spark preformation and CNC tool grinding. Leave micron-scale processing allowance to reduce grinding time and wheel wear, and remove heat-affected layers to improve surface quality.
It realizes high-efficiency forming processing, reduces precision grinding time, improves tool surface quality and shape accuracy, breaks through the processing limits of traditional processes, and obtains high-quality ultra-hard micro tools.
Smart Images

Figure CN118893432A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of tool manufacturing, and in particular to a method for preparing a laser-electric spark-grinding composite superhard micro tool. Background Art
[0002] With the development of advanced manufacturing technology, industrial products are gradually becoming miniaturized. The demand for tiny precision parts in high-end manufacturing fields such as aerospace, automobiles, precision instruments and 3C industries is growing. These tiny parts are mostly made of typical difficult-to-process materials such as high-temperature alloys, titanium alloys, cemented carbides, silicon carbide ceramics, etc., which are very likely to cause tool wear and failure during the processing process, thereby affecting the processing quality and efficiency of the parts. Superhard tool materials such as polycrystalline diamond (PCD) and polycrystalline cubic boron nitride (PCBN) have become advanced materials for manufacturing high-performance micro-tools due to their advantages such as ultra-high hardness, wear resistance, small thermal deformation, and high thermal conductivity.
[0003] The excellent performance of superhard tool materials directly affects their machinability, which brings difficulties to their manufacturing process. Superhard tool manufacturing processes such as laser processing and electrospark machining have the advantages of high processing efficiency and small processing deformation, but the surface and cutting edge quality of the tool after processing are poor and there is a heat-affected layer. When high-quality tool surface integrity is required, grinding is still better than other tool manufacturing processes, but the grinding wheel wears quickly when sharpening superhard material micro-tools, which seriously affects the shape accuracy, dimensional consistency and manufacturing efficiency of the tool. Therefore, when manufacturing superhard micro-tools, it is necessary to reasonably select the manufacturing process method according to different preparation processes to ensure that the superhard micro-tools have both high manufacturing efficiency and stable manufacturing quality. Summary of the invention
[0004] The purpose of the present invention is to provide a laser-electric spark-grinding composite superhard micro-tool preparation method to solve the problems existing in the above-mentioned prior art, and to achieve high-quality and high-efficiency preparation of superhard micro-tools with a diameter of less than 2 mm and a large aspect ratio.
[0005] To achieve the above object, the present invention provides the following solutions:
[0006] The present invention provides a method for preparing a superhard micro-tool by laser-electric spark-grinding composite, comprising the following steps:
[0007] S1: Preparation of superhard tool bar blank: A cylindrical sample with a diameter of 0.8-2 mm is cut from a superhard material composite sheet by laser cutting. Then, a blind hole is machined in the center of the end face of the carbide tool handle by an electric spark puncher. The cylindrical sample is inserted into the blind hole, and the gap between the two is filled with brazing solder. The cylindrical sample is welded to the carbide tool handle by vacuum brazing.
[0008] S2: Laser diameter reduction of superhard tool bars: Combined with laser roughing and finishing processes, the cylindrical surface of superhard tool bars is reduced. During the processing, a picosecond pulse laser with a wavelength of 1064nm is used, the laser power is 2 to 25W, and the laser scanning speed is 100-2000mm / s;
[0009] S3: Spiral groove EDM preforming processing: The spiral groove is processed on the cylindrical surface of the superhard tool bar by micro-EDM milling method, so as to realize the preforming processing of the spiral groove of the superhard micro tool and obtain the preformed spiral groove superhard micro tool; in the micro-EDM process of the spiral groove, a cylindrical electrode of cemented carbide material is used, the electrode diameter is 0.1-0.3mm, the peak current is 5-12A, and the peak voltage is 100-150V;
[0010] S4: Precision grinding of superhard micro tools: The surface of the preformed spiral groove superhard micro tool obtained in step S3 is precisely ground by a CNC tool grinder, such as the cylindrical surface, spiral groove, front tool face, back tool face, end edge, side edge and other structures of the tool, and the metamorphic layer left on the surface of the tool bar by laser processing and electrospark processing is quantitatively removed to form the tool edge. During the grinding process, the grinding wheel linear speed is 1200-1500m / min, the grinding feed speed is 5-100mm / min, and the grinding depth is 0.5-2μm, and finally a superhard micro tool is obtained.
[0011] Preferably, in step S1, the superhard material composite sheet includes a PCD composite sheet and a PCBN composite sheet.
[0012] Compared with the prior art, the present invention has achieved the following technical effects:
[0013] (1) The method for preparing superhard micro tools provided by the present invention can pre-form the cylindrical surface and spiral groove of the superhard micro tools through laser processing and micro-electrodischarge machining, so as to realize the high-efficiency forming processing of superhard micro tools, and at the same time only reserve micron-level processing allowance for subsequent precision grinding process, which greatly reduces the processing time and grinding wheel wear of the precision grinding process, thereby improving the overall manufacturing efficiency of superhard micro tools.
[0014] (2) The method for preparing super-hard micro-tools provided by the present invention, due to the thermal effect during laser processing and micro-EDM, a metamorphic layer will be produced on the surface of the tool. The strength and hardness of the metamorphic layer are much lower than that of the super-hard tool material matrix and rich in surface defects, so its grindability is increased. In the subsequent grinding process to remove the metamorphic layer, the grinding force is reduced, the grinding process is more stable, and the defects such as micro-cracks and micro-pits on the surface of the tool after grinding are reduced, so the surface quality and edge quality of the tool are greatly improved. In addition, as the diameter of the super-hard micro-tool decreases and the aspect ratio increases, the rigidity and strength of the tip part further deteriorate, and it is easy to deform or even break under the action of the grinding force. Compared with the traditional grinding method for manufacturing super-hard micro-tools, the method for preparing super-hard micro-tools provided by the present invention reduces the grinding force, improves the shape accuracy of the super-hard micro-tools, breaks through the processing limits of the tool diameter and aspect ratio, and thus obtains high-quality super-hard micro-tools. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0016] Figure 1 Schematic diagram of the structure of the PCBN superhard micro-drilling tool to be prepared in an embodiment of the present invention;
[0017] Figure 2 The figure is a flow chart of the method for preparing a super-hard micro-tool by laser-electric spark-grinding composite in an embodiment of the present invention.
[0018] In the figure: 1-PCBN composite sheet, 2-cylindrical sample, 3-carbide tool handle, 4-solder, 5-cylindrical electrode, 6-grinding wheel, 7-thin copper tube electrode. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0020] The purpose of the present invention is to provide a laser-electric spark-grinding composite superhard micro-tool preparation method to solve the problems existing in the prior art and to achieve high-quality and high-efficiency preparation of superhard micro-tools with a diameter of less than 2 mm and a large aspect ratio.
[0021] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0022] The tool to be prepared in this embodiment is a PCBN superhard micro-drilling tool, such as Figure 1 As shown, the tool diameter D1 = 0.4 mm, the spiral groove length L1 = 1.6 mm, the helix angle β = 30°, the PCBN layer thickness L2 = 0.8 mm, the tool handle diameter D2 = 3 mm, and the overall tool length L3 = 50 mm.
[0023] like Figure 2 As shown, the above-mentioned PCBN superhard micro-drilling tool is made by the laser-electric spark-grinding composite superhard micro-tool preparation method provided by the present invention, and the specific production steps are as follows:
[0024] Step 1: Preparation of superhard tool bar blank: A cylindrical sample 2 is cut from a PCBN composite sheet 1 by laser cutting. The PCBN composite sheet 1 is a DBW85 composite sheet produced by Element Six. The diameter of the cylindrical sample 2 is 1.5 mm. Then, a fine copper tube electrode 7 in an electrospark puncher is used to machine a tiny blind hole with a diameter of 1.7 mm in the center of the end face of the carbide tool handle 3. The cylindrical sample 2 is inserted into the tiny blind hole, and the gap between the two is filled with brazing solder 4. The superhard material cylindrical sample 2 and the carbide tool handle 3 are welded together by vacuum brazing. The vacuum degree during the welding process is 3×10 -4 Pa, welding temperature is 780℃, holding time is 30min;
[0025] Step 2: Laser diameter reduction processing of superhard tool bar: Combine laser rough processing and fine processing to reduce the cylindrical surface of the superhard tool bar (cylindrical sample 2) to a suitable diameter size. Picosecond pulse laser is used in the processing process. The laser rough processing process parameters are laser power 20W and laser scanning speed 400mm / s. The diameter of the PCBN superhard tool bar is reduced to 0.42mm by laser diameter reduction processing, and a metamorphic layer with a thickness of about 5μm is left on the cylindrical surface of the tool bar.
[0026] Step 3: Pre-forming spiral groove electrospark machining: adopting micro-electrospark milling machining method, using a 0.25mm diameter cemented carbide cylindrical electrode 5, two symmetrically distributed spiral grooves with a groove width of 0.3mm, a groove depth of 0.15mm, and a spiral angle of 30° are machined on the cylindrical surface of a PCBN rod with a diameter of 0.42mm to obtain a pre-formed spiral groove PCBN super-hard micro-tool. The peak current during the machining process is 6A, and the peak voltage is 120V. After machining, a metamorphic layer with a thickness of about 3μm is generated on the surface of the spiral groove of the PCBN super-hard micro-tool;
[0027] Step 4: Precision grinding of superhard micro tools: The cylindrical surface, spiral groove, back face, blade back and other structural features of the preformed spiral groove PCBN superhard micro tool obtained in step 3 are precisely ground by a CNC tool grinder, and the heat-affected layer left on the surface of the tool bar by laser processing and electrospark processing is accurately removed to form a micro-drill cutting edge. The specific grinding process is a grinding wheel linear speed of 1400m / min, a grinding depth of 1μm, and a feed speed of 10mm / min, and finally a PCBN superhard micro drill with a diameter of 0.4mm is precisely ground.
[0028] The present invention uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only used to help understand the method and core ideas of the present invention. At the same time, for those skilled in the art, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A method for preparing a superhard micro-tool by laser-electric spark-grinding composite, characterized in that: The following steps are involved: S1: Preparation of superhard tool bar blank: A cylindrical sample with a diameter of 0.8-2 mm is cut from a superhard material composite sheet by laser cutting. Then, a blind hole is machined in the center of the end face of the carbide tool handle by an electric spark puncher. The cylindrical sample is inserted into the blind hole, and the gap between the two is filled with brazing solder. The cylindrical sample is welded to the carbide tool handle by vacuum brazing. S2: Laser diameter reduction of superhard tool bars: Combined with laser roughing and finishing processes, the cylindrical surface of superhard tool bars is reduced. During the processing, a picosecond pulse laser with a wavelength of 1064nm is used, the laser power is 2 to 25W, and the laser scanning speed is 100-2000mm / s; S3: Spiral groove EDM preforming processing: The spiral groove is processed on the cylindrical surface of the superhard tool bar by micro-EDM milling method, so as to realize the preforming processing of the spiral groove of the superhard micro tool and obtain the preformed spiral groove superhard micro tool; in the micro-EDM process of the spiral groove, a cylindrical electrode of cemented carbide material is used, the electrode diameter is 0.1-0.3mm, the peak current is 5-12A, and the peak voltage is 100-150V; S4: Precision grinding of superhard micro tools: The surface of the preformed spiral groove superhard micro tool obtained in step S3 is precisely ground by a CNC tool grinder to quantitatively remove the metamorphic layer left on the surface of the tool bar by laser processing and electrospark processing and form a tool edge. During the grinding process, the grinding wheel linear speed is 1200-1500m / min, the grinding feed speed is 5-100mm / min, and the grinding depth is 0.5-2μm, and finally a superhard micro tool is obtained.
2. The method for preparing a superhard micro-tool by laser-electric spark-grinding composite according to claim 1, characterized in that: In step S1, the superhard material composite sheet includes a PCD composite sheet and a PCBN composite sheet.
Citation Information
Patent Citations
Method for manufacturing metal ceramic micro milling cutter and milling cutter
CN106825713A
Integrated PCBN round rod-shaped cutting tool and manufacturing method thereof
CN107738077A
Micro-small-diameter milling and grinding composite PCD ball-end milling cutter and blade grinding method thereof
CN111113168A
Micro milling and grinding composite PCD end mill and preparation method thereof
CN112719825A
Super-hard cutter bar with large length-diameter ratio and micro-diameter and preparation method of super-hard cutter bar
CN115365775A