Sealing method of photovoltaic module
By using the combination technology of a three-dimensional mesh structure formed by cross-linking reaction in the photovoltaic module, the problem of poor sealing of the photovoltaic module is solved, and the lower water vapor transmittance and higher packaging stability are achieved, and the The service life of the components and improves power generation efficiency.
Patent Information
- Application Number
- CN202411189285.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-05
AI Technical Summary
The sealing properties of existing photovoltaic modules are poor, resulting in water vapor penetration, affecting the service life of the module and power generation efficiency.
Linear molecular structure cross-linking reaction is used to form a three-dimensional network structure encapsulation film, and a high-flow and high adhesion melt sealing tape is used during the lamination and packaging process, combining the thermosetting film and the thermoplastic sealing tape to form Highly dense and highly adhesive sealing layer to prevent water vapor penetration.
It significantly reduces the water vapor transmission rate, extends the reliable performance of photovoltaic cells, improves the sealing and service life of the components, enhances the power generation efficiency, and improves the stability and process matching of the packaging.
Smart Images

Figure CN118899356A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of photovoltaic cell power generation, and in particular to a sealing method for a photovoltaic component. Background Art
[0002] With the development of photovoltaic technology, the power and conversion efficiency of photovoltaic cells are getting higher and higher. Since high-power and high-conversion-efficiency cells are more sensitive to environmental factors such as water vapor, especially the current TOPCon and HJT battery processes have higher and higher requirements for the water vapor packaging of components, high-sealing component packaging methods are very important now and in the future.
[0003] Currently, mainstream manufacturers generally use butyl rubber for packaging. Although butyl rubber has a very low water vapor permeability, the bonding performance of butyl rubber is poor and its compatibility with the packaging materials of photovoltaic modules is poor. During the 20-30-year service life of photovoltaic modules, there is a risk of delamination between butyl rubber and the photovoltaic substrate, which can easily cause water vapor to penetrate into the module from the interlayer of the packaging material. Summary of the invention
[0004] The purpose of the present invention is to provide a sealing packaging method for photovoltaic modules, so as to solve the problem that the poor sealing of photovoltaic modules leads to water vapor penetration and module failure. The present invention can make photovoltaic modules reach a lower water vapor permeability, reduce the water vapor entering the module through the surroundings and corroding the photovoltaic cells, extend the reliability of the photovoltaic cells, and bring more power generation gain. In order to solve the above technical problems, the present invention provides a sealing method for photovoltaic modules, and its working principle and manufacturing method are as follows:
[0005] A method for sealing a photovoltaic module, characterized in that the sealing method comprises: when the module is laminated and packaged, the packaging film of the module, that is, the first layer packaging film and the second layer packaging film, undergo a cross-linking reaction of a linear molecular structure to form a three-dimensional network structure; as the lamination packaging temperature increases, the sealing tape melts and is in a molten state with high fluidity and high adhesion, and can be well integrated into the three-dimensional network structure to form good compactness; at the same time, when the module is operated outdoors at high temperature, the sealing tape is in a molten and highly adhesive state under the action of high temperature, thereby preventing water vapor from penetrating from between material layers into the interior of the module, and further improving the sealing of the module; the method steps are specifically as follows:
[0006] Step 1: Lay the first substrate (i.e. Figure 1 The substrate 1);
[0007] Step 2, laying the first layer of packaging film; laying the first layer of packaging film horizontally and centrally on the surface of the first substrate, the first layer of packaging film has the function of providing high light transmittance and adhesion, the first layer of packaging film is a thermosetting film of EVA / EPE / POE for photovoltaics, the thickness is 0.4-0.6mm, and the transmittance setting range is 91-93%;
[0008] Step 3: Laying photovoltaic cell strings; placing the photovoltaic cell strings in series or parallel horizontally and centrally on the surface of the first layer of packaging film, the photovoltaic cell strings provide the main power generation for the photovoltaic module, the cells include PERC, TOPCon, HJT photovoltaic cells, and can also be used for the sealing of other photovoltaic cells; the size of the first layer of packaging film is 3 to 5 mm larger than the photovoltaic cell string;
[0009] Step 4, laying the second layer of packaging film: laying the second layer of packaging film horizontally and centrally on the photovoltaic cell string group, the size of the second layer of packaging film is consistent with the size of the first layer of packaging film, and the four sides are aligned with the first layer of packaging film; the second layer of packaging film is used to provide adhesion, and the second layer of packaging film is a thermosetting film including EVA / EPE / POE for photovoltaic use, with a thickness of 0.4-0.6mm and a transmittance setting range of 91-93%;
[0010] Step 5: Press and pre-fix the sealing tape: tear off the separation film with a sealing tape adhesive layer on one side of the sealing tape, and press and pre-fix them on the packaging film respectively, the two layers of packaging film are 10 to 15 mm away from the first substrate, the edges of the two layers of packaging film are pasted with sealing tape, and the sealing tape is pasted on the first substrate, that is, on the surface of the first substrate around the edges of the first layer of packaging film and the second layer of packaging film, and the outer edge is 10 to 15 mm away from the outer edge of the glass; the function of the sealing tape is to block the infiltration of water vapor;
[0011] Step 6: Laying the packaging adhesive tape: Cut the upper and lower layers of packaging adhesive tape with the same width as the sealing tape to the edge of the glass, that is, lay the first adhesive tape and the second adhesive tape around the edge of the glass; laying the packaging adhesive tape serves to provide adhesion and sealing for the first substrate and the second substrate, and prevents the base material of the sealing tape from flowing out of the glass;
[0012] Step 7: Lay the second substrate (i.e. Figure 1 Substrate 2): The second substrate is laid on the uppermost layer, and the second substrate is used for protection. The second substrate is made of 0 water-permeable and highly permeable tempered or semi-tempered photovoltaic glass with a thickness of 1.6 to 3.2 mm;
[0013] Step 8: After the laying is completed, a sealing method of the photovoltaic module is completed through lamination and assembly processes to prepare a sealing component of the photovoltaic module.
[0014] Furthermore, in the step 1, the substrate is made of 0 water-transmittance and highly transparent tempered or semi-tempered photovoltaic glass, with a thickness of 1.6 to 3.2 mm and a light transmittance setting range of 92 to 94%. The substrate mainly provides light transmission and protection.
[0015] Furthermore, the first layer of packaging film and the second layer of packaging film (2) are made of the same material or different materials.
[0016] Furthermore, the sealing tape is made of a thermoplastic material. The function of the sealing tape is to increase the compactness of the packaging film during the component lamination process and to be in a molten state when the component is operated outdoors at high temperature, so as to better block the lamination penetration of water vapor; the sealing tape is made of EVA / POE or other thermoplastic material, with a melting temperature of 60 to 100°C, and is solid at room temperature (25°C), and has a square or rectangular or circular or other shape; the thickness of the sealing tape is 1 to 2 mm thicker than the two layers of packaging film, or the thickness is set according to the thickness of the packaging film.
[0017] Furthermore, the thickness of the adhesive layer of the sealing tape is 0.01 to 0.05 mm; the separation membrane of the sealing tape has the function of providing a quick separation effect and can provide a quick separation effect when bonding, including PET material, with a thickness range of 0.1 to 0.3 mm.
[0018] Furthermore, the packaging adhesive tape comprises a thermosetting adhesive film of EVA / EPE / POE for photovoltaics; the thickness and material combination of the packaging adhesive tape are consistent with those of the first layer of packaging film and the second layer of packaging film.
[0019] Furthermore, the sealing assembly prepared by the sealing method is: a first substrate, wherein the first substrate is the bottom layer, and the upper end of the first substrate is sequentially a first layer of packaging film, a battery string group, and a second layer of packaging film; the edges around the first layer of packaging film, the battery string group, and the second layer of packaging film are sealing tapes, and the adhesive layer of the sealing tape is located at the bottom of the sealing tape and above the first layer of the substrate; the left side of the sealing tape is a packaging adhesive tape, namely a first adhesive tape and a second adhesive tape; wherein the first adhesive tape is located above the first substrate, and the second adhesive tape is located above the first adhesive tape); the topmost layer is the second layer of the substrate.
[0020] Compared with the existing solutions, the beneficial effects of the present invention are:
[0021] 1. Compared with the conventional component packaging method, the present invention uses a sealing tape with a low melt index. The molten state during the lamination process can fully fill the gaps in the three-dimensional network structure of the packaging film, greatly increasing the density of the packaging film and reducing the water vapor transmission rate. At the same time, when the component is operated outdoors at high temperature, the sealing tape is in a molten state, which can effectively prevent water vapor from penetrating from the material layers into the interior of the component. It can well extend the service life of the component, thereby bringing more power generation benefits;
[0022] 2. The sealing tape uses the same base material as the packaging film, and has better bonding performance. Compared with the risk of delamination of butyl rubber, the sealing tape of this invention has better reliability. At the same time, at the process end, the process stability and matching of the same base material are better. Compared with other methods, the packaging yield of the components is higher.
[0023] 3. The sealing tape base material is made of thermoplastic sealing material, which is solid at room temperature, making the operation simpler and more convenient. The pressure-sensitive adhesive surface is provided with a release film. During the bonding pre-fixation process, compared with other sealing methods using butyl adhesive, this method has higher separation and bonding efficiency;
[0024] 4. The sealing tape of this method can be the same transparent color as the packaging film, or other colorful colors (red or yellow, etc.) can be selected to make the appearance design of the component more diverse and more beautiful. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 A schematic diagram of a sealing method for a photovoltaic module of the present invention;
[0026] Figure 2 A method flow chart of a sealing method for a photovoltaic module of the present invention;
[0027] Figure 3 A schematic diagram of the structure of a sealing component prepared by a sealing method of a photovoltaic component of the present invention;
[0028] Figure 4 A schematic plan view of a sealing component prepared by a sealing method for a photovoltaic component of the present invention;
[0029] 1-second substrate, 2-second packaging film layer, 3-photovoltaic cell string group, 4-first packaging film layer, 5-sealing tape, 6-sealing tape adhesive layer, 7-second adhesive tape, 8-first adhesive tape, 9-first substrate. DETAILED DESCRIPTION
[0030] In order to make the purpose, technical solution and effect of the present invention clearer and more specific, the present invention is further described in detail by enumerating examples below. It should be noted that the specific implementation described here is only used to explain the present invention and is not used to limit the present invention.
[0031] like Figures 1-2 As shown: The present invention provides a sealing method for a photovoltaic module, and the sealing principle is as follows Figure 1 As shown, when the components are laminated and packaged, the packaging film of the components is cross-linked from a linear molecular structure to a three-dimensional network structure. As the temperature of the laminated package increases, the sealing tape melts into a molten state with high fluidity and high adhesion, and can be well integrated into the three-dimensional network structure to form a good density. At the same time, when the components are operated outdoors at high temperatures, the sealing tape is in a molten and highly adhesive state under the action of high temperature, preventing water vapor from penetrating from the material layers into the interior of the component, further improving the sealing of the component. The details of its production method are as follows:
[0032] Step 1: Laying the first substrate 9: The main function of this substrate is to provide light transmission and protection. Usually, tempered or semi-tempered photovoltaic glass with zero water permeability and high light transmittance is used. The thickness is usually 1.6-3.2mm, and the transmittance setting range is 92-94%.
[0033] Step 2: Lay the first layer of packaging film 4: Lay the first layer of packaging film 4 horizontally and centrally on the surface of the first substrate 9. The dimensions of the first layer of packaging film 4 are 3 to 5 mm larger than the photovoltaic cell string group 3. The function of this layer of packaging film is to provide high light transmittance and adhesion. Usually, thermosetting films such as EVA / EPE / POE for photovoltaics are used, but not limited to. The thickness is usually 0.4 to 0.6 mm, and the transmittance setting range is 91 to 93%.
[0034] Step 3: Laying photovoltaic cell strings 3: Place the series or parallel cell strings horizontally and centrally on the surface of the first layer of packaging film 4. The photovoltaic cell strings 3 mainly provide the main power generation for the photovoltaic module. The cells include but are not limited to PERC, TOPCon, HJT and other photovoltaic cells.
[0035] Step 4: Lay the second layer of packaging film 2: The second layer of packaging film 2 is horizontally centered on the photovoltaic cell string group 3. The size of the second layer of packaging film 2 is consistent with that of the first layer of packaging film 4, and the four sides are aligned with the first layer of packaging film 4. The function of the second layer of packaging film 2 is to provide adhesion. It is usually made of, but not limited to, thermosetting films such as EVA / EPE / POE for photovoltaics. The thickness is usually 0.4-0.6mm, and the transmittance is set in the range of 91-93%. It can be made of the same material as the first layer of film, or it can be made of a different material from the first layer of packaging film 4.
[0036] Step 5: Press and pre-fix the sealing tape 5: Tear off the separation film with the sealing tape adhesive layer 6 on one side of the sealing tape 5 substrate, and press and pre-fix them on the packaging film. The two layers of packaging film are 10 to 15 mm away from the first substrate 9. The edges of the two layers of packaging film are pasted with sealing tape. The sealing tape 5 is pasted on the first substrate 9, that is, on the surface of the first substrate 9 around the edges of the first layer of packaging film 4 and the second layer of packaging film 2, and the outer edge is 10 to 15 mm away from the outer edge of the glass; the function of the sealing tape 5 is to block the infiltration of water vapor. Among them:
[0037] The sealing tape 5 is made of thermoplastic material, and its main function is to increase the density of the packaging film during the component lamination process and to be in a molten state when the component is operated outdoors at high temperature, so as to better block the lamination penetration of water vapor. Including but not limited to EVA / POE or other equivalent materials, the melting temperature is usually set to 60-100°C, and it is solid at room temperature (25°C). The shape can usually be set to square or rectangular, but not limited to circular or other shapes. The thickness can be designed according to the thickness of the packaging film, which is usually 1-2mm thicker than the two layers of packaging film.
[0038] The sealing tape adhesive layer 6 is a UV-resistant and aging-resistant pressure-sensitive adhesive layer, which has adhesion properties at room temperature and can play a good role in pre-adhesion. The thickness is usually set to 0.01-0.05 mm.
[0039] Separation layer of the sealing tape: The function of this layer is to provide a quick separation effect, and it can provide a quick separation effect when bonding, including but not limited to PET material, with a thickness range of 0.1 to 0.3 mm.
[0040] Step 6: Laying the packaging adhesive tape: Cut the upper and lower layers of packaging adhesive tape (6-sealing tape adhesive layer, 7-first adhesive tape) with the same width as the sealing tape to the edge of the glass and lay them around the edges of the glass. The main function of this step is to provide adhesion and sealing for the first substrate 9 and the second substrate 1, and prevent the base material of the sealing tape from flowing out of the glass. Usually, thermosetting adhesive films such as EVA / EPE / POE for photovoltaics are used, but not limited to them. The thickness and material are consistent with the first layer of packaging film 4 and the second layer of packaging film 2.
[0041] Step 7: Laying the second substrate 1: The second substrate 1 is mainly used for protection, and usually adopts 0 water-permeable and high-transmittance tempered or semi-tempered photovoltaic glass, and the thickness is usually 1.6-3.2mm.
[0042] Step 8: After laying is completed, a sealing method for photovoltaic modules is completed through lamination, assembly and other processes.
[0043] The sealing component prepared by the above method is as follows Figures 3-4As shown, the sealing component prepared by the sealing method is: a first substrate 9, wherein the first substrate 9 is the bottom layer, and the upper end of the first substrate 9 is sequentially provided with a first packaging film 4, a battery string group 3, and a second packaging film 2; the edges of the first packaging film 4, the battery string group 3, and the second packaging film 2 are sealed with a sealing tape 5, and the adhesive layer 6 of the sealing tape is located at the bottom of the sealing tape 5 and above the first substrate 9; the left side of the sealing tape is a packaging adhesive tape, namely a first adhesive tape 8 and a second adhesive tape 7; wherein the first adhesive tape 8 is located above the first substrate 9, and the second adhesive tape 7 is located above the first adhesive tape 8); the topmost layer is the second substrate 1.
[0044] The above description is only a preferred embodiment of the present invention. It should be pointed out that a person skilled in the art can make several improvements without departing from the principle of the present invention, and these improvements should also be regarded as within the protection scope of the present invention.
Claims
1. A method for sealing a photovoltaic module, characterized in that: The sealing method is: Step 1: laying a first substrate (9); Step 2, laying a first layer of packaging film (4); laying the first layer of packaging film (4) horizontally and centrally on the surface of the first substrate (9); the first layer of packaging film (4) has the function of providing high light transmittance and adhesion; the first layer of packaging film (4) is a thermosetting film of EVA / EPE / POE for photovoltaics, has a thickness of 0.4 to 0.6 mm, and a light transmittance setting range of 91 to 93%; Step 3: Laying a photovoltaic cell string group (3); placing the photovoltaic cell string group (3) connected in series or in parallel horizontally and centrally on the surface of the first layer of packaging film (4); the photovoltaic cell string group (3) provides a power generation body for the photovoltaic module, and the cells include PERC, TOPCon, and HJT photovoltaic cells; the size of the first layer of packaging film (4) is 3 to 5 mm larger than the photovoltaic cell string group (3); Step 4, laying the second layer of packaging film (2): laying the second layer of packaging film (2) horizontally and centrally on the photovoltaic cell string group (3), the size of the second layer of packaging film (2) is consistent with the size of the first layer of packaging film (4), and the four sides are aligned with the first layer of packaging film (4); the function of the second layer of packaging film (2) is to provide adhesion, the second layer of packaging film (2) adopts a thermosetting film including EVA / EPE / POE for photovoltaics, the thickness is 0.4-0.6mm, and the transmittance setting range is 91-93%; Step 5: Press and pre-fix the sealing tape (5): tear off the separation film provided with the sealing tape adhesive layer (6) on one side of the sealing tape (5), and press and pre-fix them on the packaging films respectively, the two layers of packaging films are 10 to 15 mm away from the first substrate (9), the edges of the two layers of packaging films are pasted with the sealing tape, and the sealing tape (5) is pasted on the first substrate (9), that is, on the surface of the first substrate (9) around the edges of the first layer of packaging film (4) and the second layer of packaging film (2), and the outer edge is 10 to 15 mm away from the outer edge of the glass; The sealing tape (5) is used to prevent water vapor from penetrating. Step 6: Laying the sealing adhesive tape: cutting two layers of sealing adhesive tape with the same width as the sealing tape (5) to the edge of the glass, that is, laying the first adhesive tape (8) and the second adhesive tape (7) around the edge of the glass; Step 7: Laying the second substrate (1): The second substrate (1) is laid at the uppermost layer. The second substrate (1) serves as a protective layer. The second substrate (1) is made of 0 water-permeable and high-permeability tempered or semi-tempered photovoltaic glass with a thickness of 1.6 to 3.2 mm. Step 8: After the laying is completed, a sealing method of the photovoltaic module is completed through lamination and assembly processes to prepare a sealing component of the photovoltaic module.
2. A method for sealing a photovoltaic module according to claim 1, characterized in that: When the components are laminated and packaged, the packaging films of the components, i.e., the first layer packaging film (4) and the second layer packaging film (2), undergo a cross-linking reaction of a linear molecular structure to form a three-dimensional network structure. As the temperature of the laminated packaging increases, the sealing tape (5) melts into a molten state with high fluidity and high adhesion, and can be well integrated into the three-dimensional network structure to form a good density. At the same time, when the components are operated outdoors at high temperature, the sealing tape (5) is in a molten and highly adhesive state under the action of high temperature, thereby preventing water vapor from penetrating from between material layers into the interior of the component, thereby further improving the sealing of the component.
3. A method for sealing a photovoltaic module according to claim 1, characterized in that: In the step 1, the substrate is made of tempered or semi-tempered photovoltaic glass with zero water transmittance and high light transmittance, with a thickness of 1.6 to 3.2 mm and a light transmittance setting range of 92 to 94%.
4. A method for sealing a photovoltaic module according to claim 1, characterized in that: The first layer of packaging adhesive film (4) and the second layer of packaging adhesive film (2) are made of the same material or different materials.
5. A method for sealing a photovoltaic module according to claim 1, characterized in that: The sealing tape (5) is made of thermoplastic material. The function of the sealing tape (5) is to increase the compactness of the packaging film during the component lamination process and to better block the lamination penetration of water vapor when the component is in a molten state when operating outdoors at high temperature.
6. A method for sealing a photovoltaic module according to claim 5, characterized in that: The sealing tape (5) is made of EVA / POE or other thermoplastic material, has a melting temperature of 60-100°C, is solid at room temperature (25°C), and has a square, rectangular, circular or other shape; the thickness of the sealing tape (5) is 1-2 mm thicker than the two layers of packaging film, or the thickness is set according to the thickness of the packaging film.
7. A method for sealing a photovoltaic module according to claim 1, characterized in that: The thickness of the adhesive layer of the sealing tape is 0.01-0.05 mm; the separation film of the sealing tape (5) has the function of providing a quick separation effect and can provide a quick separation effect when bonding, including PET material, with a thickness range of 0.1-0.3 mm.
8. A method for sealing a photovoltaic module according to claim 1, characterized in that: The packaging adhesive tape comprises a thermosetting adhesive film of EVA / EPE / POE for photovoltaics; the thickness and material combination of the packaging adhesive tape are consistent with those of the first layer of packaging film (4) and the second layer of packaging film (2).
9. A method for sealing a photovoltaic module according to any one of claims 1 to 6, characterized in that: A sealing component prepared by the sealing method.
10. A method for sealing a photovoltaic module according to claim 9, characterized in that: The sealing component comprises: a first substrate (9), wherein the first substrate (9) is the bottom layer, and the upper end of the first substrate (9) is sequentially provided with a first layer of packaging film (4), a battery string group (3), and a second layer of packaging film (2); the edges around the first layer of packaging film (4), the battery string group (3), and the second layer of packaging film (2) are sealing tapes (5), and the adhesive layer (6) of the sealing tape is located at the bottom of the sealing tape (5) and above the first layer of substrate (9); the left side of the sealing tape is a packaging adhesive tape, namely a first adhesive tape (8) and a second adhesive tape (7); wherein the first adhesive tape (8) is located above the first substrate (9), and the second adhesive tape (7) is located above the first adhesive tape (8); and the topmost layer is the second layer of substrate (1).
Citation Information
Cited By
Low-water-permeability packaging method suitable for offshore photovoltaic module
CN120980998A