Preparation method of tantalum nitride-based heterojunction
By optimizing the heterojunction of the unit cell structure of tantalum nitride and tantalum nitride, the problem of insufficient charge transfer characteristics in PEC equipment is solved, and its performance in photoelectrocatalysis is improved.
Patent Information
- Application Number
- CN202411032947.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
AI Technical Summary
No suitable materials have been found in the prior art to form a type II heterojunction photoanode material with tantalum nitride, which limits the large-scale promotion and use of tantalum nitride in PEC equipment.
By optimizing the unit cell structure of tantalum nitride and tantalum nitride, static self-consistent and non-consistent calculations are performed, a heterojunction of tantalum nitride nitride is formed, the spacing and locations of the layers are tested, and the structure is optimized to improve Its energy band arrangement and charge transport characteristics.
The charge transfer characteristics of tantalum nitride-based materials have been improved, the photoelectrocatalytic performance has been improved, and new research ideas have been provided for the application of tantalum nitride in PEC equipment.
Smart Images

Figure CN118957661A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of heterojunction preparation, and in particular to a method for preparing a tantalum nitride-based heterojunction. Background Art
[0002] The production of hydrogen and oxygen by sunlight-driven photoelectrochemical (PEC) water splitting can effectively utilize solar energy and alleviate the energy crisis. For commercial implementation of PEC devices, we need low-cost, non-toxic materials that can achieve more than 10% solar-to-hydrogen (STH) conversion efficiency. Among the various candidate materials studied, tantalum nitride (Ta3N5) stands out for its good direct band gap (~2.1eV), suitable band edge alignment, and abundant earth reserves. However, due to the fast carrier recombination (<10ps) of Ta3N5, it leads to a high onset potential (0.8-1.1V) relative to the hydrogen electrode, which in turn limits its large-scale promotion and use. Therefore, it is very necessary to develop an effective strategy to improve the charge transport properties of Ta3N5, but it is a major challenge.
[0003] A common strategy is to separate the photogenerated charges by building an electric field in the depletion region of the heterojunction, thereby improving the charge transport properties.
[0004] After searching, the Chinese patent with the announcement number CN113293404A discloses a heterojunction photoanode material and its preparation method and application, which proposes a technical solution to achieve efficient separation of photogenerated charges by preparing a heterojunction photoanode material with interface lattice matching;
[0005] The Chinese patent with the announcement number CN115613037A discloses a Ni2P / TiO2S-type heterojunction photoanode material and its application, which proposes a technical solution to achieve the purpose of slowing down corrosion by combining nanoparticle Ni2P and TiO2 nanotube array to construct an S-type heterojunction;
[0006] However, although the staggered (Type II) heterojunction between two semiconductors can usually generate a built-in electric field at its interface, thereby effectively separating the charges, and coupling the two semiconductors to form a heterojunction can make up for the shortcomings of a single component and produce a synergistic effect, a suitable material has not yet been found to combine with tantalum nitride to form a Type II heterojunction. Therefore, it is a challenge to find a material with a correctly arranged energy band position to construct a Type II heterojunction photoanode material with tantalum nitride. Summary of the invention
[0007] The purpose of the present invention is to solve the defects in the prior art and to propose a method for preparing a tantalum nitride-based heterojunction.
[0008] In order to achieve the above object, the present invention adopts the following technical solutions:
[0009] A method for preparing a tantalum nitride-based heterojunction comprises the following steps:
[0010] Step S1: Optimizing the unit cell structure of tantalum oxynitride and tantalum nitride;
[0011] Step S2: Perform static self-consistent and non-self-consistent calculations to obtain energy and band structure data of the stable model;
[0012] Step S3: cutting the tantalum oxynitride and tantalum nitride, wherein the crystal direction of the cut surface is a direction;
[0013] Step S4: combining tantalum oxynitride and tantalum nitride to form a heterojunction, and testing the interlayer spacing and positions;
[0014] Step S5: Structural optimization of the heterojunction model with tested interlayer spacing and sites;
[0015] Step S6: Perform self-consistent calculations to obtain the energy of the stable model, and then perform differential charge density, partial charge density and energy band arrangement analysis.
[0016] Furthermore, in step S1, the calculation method is specifically as follows:
[0017] The plane wave function basis vector cutoff energy is set to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10-5 eV, the force on each atomic force does not exceed 0.01 GPa, the Brillouin zone K point density is 0.04, the interaction between the valence electrons and the ion core is described by the pseudopotential generated by the projected augmented wave (PAW) method, the exchange correlation functional between electrons is described by GGA-PBE, and the Hubbard U treatment method is used for the transition metal Ta atom, and the U value of Ta is determined to be set to 6.47;
[0018] Optimizing the unit cell structure of tantalum oxynitride and tantalum nitride comprises the following steps:
[0019] The lattice and atomic positions of the tantalum nitride unit cell are optimized, wherein the lattice constant of the optimized tantalum nitride unit cell is The angle between the lattices is α = β = γ = 90°;
[0020] The lattice and atomic positions of the tantalum oxynitride unit cell are optimized, wherein the lattice constant of the optimized tantalum oxynitride unit cell is The angles between the lattices are α=γ=90° and β=99.77°.
[0021] Furthermore, step S2 is specifically as follows:
[0022] By setting the plane wave function basis vector cutoff energy to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10-5 eV, ion step is 1, broadening is 0.05, and Brillouin zone K-point density is 0.03 to calculate the 1s energy level of nitrogen atoms at the edge of the unit cell and then the core energy level position;
[0023] In addition, the band structure was obtained by changing the K point in the Brillouin zone to a high symmetry point for non-self-consistent calculations.
[0024] Furthermore, step S3 is specifically as follows:
[0025] Tantalum oxynitride and tantalum nitride were sectioned along the crystal direction. The surface of tantalum oxynitride contained 6 tantalum atomic layers with a thickness of Its lattice constant is The angle between the lattices is 90°;
[0026] The surface of tantalum nitride contains 7 layers of carbon atoms with a thickness of Its lattice constant is The angle between the lattices is 90°.
[0027] Furthermore, step S4 is specifically as follows:
[0028] The tantalum oxynitride surface and the tantalum nitride surface in step S3 are merged along the vertical direction of the Z axis to form a tantalum oxynitride-tantalum nitride heterojunction model, wherein the lattice mismatch calculation formula between the two is:
[0029] Lattice mismatch μ = |x1-x2| / x2×100%
[0030] In the formula, x1 is the lattice constant of the epitaxial layer, and x2 is the lattice constant of the substrate layer, wherein the epitaxial layer and the substrate layer are tantalum nitride and tantalum oxynitride, respectively.
[0031] Further, in step S4, the interlayer spacing between the nearest neighboring atomic layers of tantalum oxynitride and tantalum nitride is tested, specifically:
[0032] By moving in the vertical Z-axis direction, the distance between the two nearest neighboring atomic layers is adjusted, respectively from Move to The interval is Finally, the initial layer spacing is determined to be
[0033] On the basis of determining the interlayer distance, the initial optimized site is determined by moving left and right between the two, and the final initial optimized site is the second site.
[0034] Furthermore, step S5 is specifically as follows:
[0035] The optimization method uses the calculation method proposed in step S1, and further fixes two layers of tantalum atoms in the bottom layer of tantalum oxynitride as the substrate layer;
[0036] After optimization, the top oxygen atoms of tantalum oxynitride move upward to form chemical bonds with tantalum atoms in tantalum nitride;
[0037] The nitrogen atoms in tantalum nitride move downward and form chemical bonds with the tantalum atoms in tantalum oxynitride.
[0038] Furthermore, step S6 is specifically as follows:
[0039] By setting the plane wave function basis vector cutoff energy to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10 -5 The electronic state density of the heterojunction model was calculated using the ion step of 1, the broadening of 0.05, and the Brillouin zone K-point density of 0.03. The core energy level was aligned by reading the 1s energy level of the nitrogen atom far away from the interface.
[0040] Compared with the prior art, the present invention has the following beneficial effects:
[0041] By cutting tantalum oxynitride and tantalum nitride, a heterojunction is formed by combining tantalum nitride (100) direction with tantalum oxynitride (100) direction, and studying their electronic properties and energy band arrangement, the charge transfer characteristics of Ta3N5-based materials can be improved. Not only can a lattice-matched heterostructure be obtained, but its charge transfer efficiency can also be improved, thereby promoting the improvement of PEC performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention.
[0043] Figure 1 It is a schematic diagram of the implementation process of the method for preparing a tantalum nitride-based heterojunction in an embodiment of the present invention;
[0044] Figure 2 The unit cell structure diagram and energy band structure diagram of tantalum nitride and tantalum oxynitride in the embodiment of the present invention are shown in FIG. Figure 2 middle:
[0045] Figure 2 (a) is the crystal cell structure diagram of tantalum nitride. Figure 2 (b) is the crystal cell structure diagram of tantalum oxynitride. Figure 2 (c) is the energy band structure diagram of tantalum nitride. Figure 2 (d) is the energy band structure diagram of tantalum oxynitride;
[0046] Figure 3 Figure 2 is a surface and heterojunction diagram of tantalum nitride and tantalum oxynitride in an embodiment of the present invention. Figure 3 middle:
[0047] Figure 3 (a) Placement and Figure 3 (b) are the crystal structures of tantalum nitride (100) and tantalum oxynitride (100) respectively; Figure 3 (c) is a diagram of the unoptimized tantalum nitride (100)-tantalum oxynitride (100) heterostructure; Figure 3 (d) is the optimized tantalum nitride (100)-tantalum oxynitride (100) heterostructure diagram;
[0048] Figure 4 The interlayer spacing and site test diagram of the heterojunction structure in the embodiment of the present invention is shown in FIG. Figure 4 middle:
[0049] Figure 4 (a) is the heterojunction layer spacing test diagram, Figure 4 (b) is the heterojunction site test image;
[0050] Figure 5 is a diagram of the electronic state density, partial charge density, differential charge density, surface average charge density and energy band arrangement of the heterojunction in the embodiment of the present invention. Figure 5 middle:
[0051] Figure 5 (a) Figure 5 (b) are the electronic state density and the corresponding partial charge density diagram of the heterojunction; Figure 5 (c) is the differential charge density diagram of the heterojunction; Figure 5 (d) is the area integral differential charge density corresponding to the heterojunction differential charge density; Figure 5 (e) is the energy band arrangement diagram of the heterojunction. DETAILED DESCRIPTION
[0052] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0053] In this application, a type II heterojunction photoanode is constructed by combining tantalum oxynitride (TaON) with tantalum nitride (Ta3N5), thereby improving the charge transfer characteristics of Ta3N5-based materials. This not only obtains a lattice-matched heterostructure, but also improves its charge transfer efficiency, thereby promoting the improvement of PEC performance, thereby providing new research ideas for the development of photoelectrocatalysis.
[0054] Reference Figure 1-5 , a method for preparing a tantalum nitride-based heterojunction comprises the following steps:
[0055] Step S1: Optimizing the unit cell structure of tantalum oxynitride and tantalum nitride;
[0056] Step S2: Perform static self-consistent and non-self-consistent calculations to obtain data such as energy and band structure of the stable model;
[0057] Step S3: cutting the tantalum oxynitride and tantalum nitride, wherein the crystal orientation of the cut surface is (100);
[0058] Step S4: combining the tantalum oxynitride (100) with the tantalum nitride (100) to form a heterojunction, and testing the interlayer spacing and positions;
[0059] Step S5: Structural optimization of the heterojunction model with tested interlayer spacing and sites;
[0060] Step S6: Perform self-consistent calculations to obtain the energy of the stable model, and then perform differential charge density, partial charge density, and energy band arrangement analysis.
[0061] Step S1 is specifically as follows:
[0062] The calculation method is to set the plane wave function basis vector cutoff energy to 520eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process to 1.0×10-5eV, the force on each atomic force does not exceed 0.01Gpa, the Brillouin zone K point density is 0.04, and the interaction between the valence electrons and the ion real is described by the pseudopotential generated by the projected augmented wave (PAW) method. The exchange correlation functional between electrons is described by GGA-PBE. The Hubbard U (DFT+U) treatment method is used for the transition metal Ta atom, and the U value of Ta is determined to be set to 6.47.
[0063] The lattice and atomic positions of the Ta3N5 unit cell are optimized, and the lattice constant of the optimized Ta3N5 unit cell is The angle between the lattices is α = β = γ = 90°, and the unit cell structure is shown in the figure Figure 2 (a)
[0064] The lattice and atomic positions of the TaON unit cell are optimized, where the lattice constant of the optimized TaON unit cell is The angles between the lattices are α = γ = 90°, β = 99.77°, and the unit cell structure is shown in the figure Figure 2 (b)
[0065] Step S2 is specifically as follows:
[0066] By setting the plane wave function basis vector cutoff energy to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10 -5eV, ion step is 1, broadening is 0.05, and Brillouin zone K point density is 0.03 to calculate the 1s energy level of nitrogen atoms at the edge of the unit cell, and then the core energy level position; further, by changing the Brillouin zone K point to a high symmetry point for non-self-consistent calculation, the band structure is obtained. The band structure diagrams of tantalum nitride and tantalum oxynitride are shown as follows: Figure 2 (c) and Figure 2 (d) shows that the calculated band gaps of the two are 2.12 and 2.61 eV respectively;
[0067] Step S3 is specifically as follows:
[0068] Tantalum oxynitride and tantalum nitride were sectioned along the (100) crystal direction. The surface of tantalum oxynitride (100) contains 6 tantalum atomic layers with a thickness of Its lattice constant is The angle between the lattices is 90°; the surface of tantalum nitride (100) contains 7 layers of carbon atoms with a thickness of Its lattice constant is The angle between the lattices is 90°. The structural diagrams of the two are as follows Figure 3 As shown in (a) and (b);
[0069] Step S4 is specifically as follows:
[0070] The above-mentioned tantalum oxynitride (100) surface and tantalum nitride (100) surface are merged along the vertical direction of the Z axis to form a TaON (100)-Ta3N5 (100) heterojunction model, as shown in Figure 3 (c) is shown. The calculation formula of the lattice mismatch between the two is:
[0071] Lattice mismatch μ = |x1-x2| / x2×100%
[0072] Where x1 is the lattice constant of the epitaxial layer, and x2 is the lattice constant of the substrate layer. Here, the epitaxial layer and the substrate layer are tantalum nitride and tantalum oxynitride, respectively. After calculation, the lattice mismatch of the heterojunction along the a and b directions is 1.45% and 0.95%, respectively, which is lower than the standard threshold of 5%, indicating that when forming the heterojunction, both need only generate a small lattice strain.
[0073] Furthermore, the interlayer spacing between the nearest neighboring atomic layers of tantalum oxynitride and tantalum nitride was tested. Specifically, the distance between the nearest neighboring atomic layers of the two was adjusted by moving in the vertical Z-axis direction, respectively. Move to The interval is like Figure 4 As shown in (a), the initial interlayer spacing is finally determined to be Further, on the basis of determining the interlayer spacing, the initial optimized position is determined by moving left and right between the two, such as Figure 4 As shown in (b), the final initial optimized site is the second site;
[0074] Step S5 is specifically as follows:
[0075] The optimization method follows the calculation method proposed in step S1, and further fixes the two layers of tantalum atoms in the bottom layer of tantalum oxynitride as the substrate layer. The structure diagram of the optimized TaON (100)-Ta3N5 (100) heterojunction model is shown in the figure Figure 3 After optimization, the top oxygen atoms of tantalum oxynitride move upward and form chemical bonds with the tantalum atoms in tantalum nitride; the nitrogen atoms in tantalum nitride move downward and form chemical bonds with the tantalum atoms in tantalum oxynitride, and the interlayer distance between the two is reduced to The above results show that the two form a stable chemical contact, which further proves that the constructed heterojunction model has high stability;
[0076] Step S6 is specifically as follows:
[0077] By setting the plane wave function basis vector cutoff energy to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10 -5 The electronic state density of the heterojunction model was calculated using the ion step of 1, the broadening of 0.05, and the Brillouin zone K-point density of 0.03. The core energy level was aligned by reading the 1s energy level of the nitrogen atom far away from the interface.
[0078] The differential charge density is calculated by ρ=AB-AB, where AB, A, and B are the overall charge density of the heterojunction, the charge density of tantalum nitride (100), and the charge density of tantalum oxynitride (100), respectively; further, the surface integral differential charge density is obtained by integrating the differential charge density along the Z axis; and the work function and electrostatic potential are obtained by averaging the electrostatic potential along the Z direction in the heterojunction plane. The specific analysis is as follows:
[0079] like Figure 5 As shown in the electronic state density and partial charge density of (a) and (b), after the heterojunction is formed, the top of the valence band of the heterostructure is mainly dominated by tantalum nitride, and the bottom of the conduction band is mainly dominated by tantalum oxynitride. There is an interface state in the band gap. Figure 5 The partial charge density in (b) shows that the interface state originates from the top surface of tantalum nitride;
[0080] like Figure 5 As shown in (c) and (d), after the heterojunction is formed, more charge gain and loss will occur in the tantalum nitride-tantalum oxynitride interface layer, and this part of the charge is concentrated on the nitrogen atoms. Figure 5The surface integral differential charge density diagram (d) shows that the oxygen and tantalum atoms at the interface between tantalum nitride and tantalum oxynitride lose their charges and transfer the charges to the nitrogen atoms at the interface.
[0081] like Figure 5 As shown in (e), when tantalum nitride and tantalum oxynitride form a heterojunction, the Fermi levels of the two are aligned, thus forming a type II heterojunction. Among them, electrons can be transferred from tantalum nitride to tantalum oxynitride, and holes are transferred from tantalum oxynitride to tantalum nitride. This structure shows that the construction of tantalum nitride-tantalum oxynitride heterojunction can effectively separate the electron-hole pairs of tantalum nitride, thereby improving its charge transfer efficiency.
[0082] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for preparing a tantalum nitride-based heterojunction, characterized in that: The following steps are involved: Step S1: Optimizing the unit cell structure of tantalum oxynitride and tantalum nitride; Step S2: Perform static self-consistent and non-self-consistent calculations to obtain energy and band structure data of the stable model; Step S3: cutting the tantalum oxynitride and tantalum nitride, wherein the crystal direction of the cut surface is a direction; Step S4: combining tantalum oxynitride and tantalum nitride to form a heterojunction, and testing the interlayer spacing and positions; Step S5: Structural optimization of the heterojunction model with tested interlayer spacing and sites; Step S6: Perform self-consistent calculations to obtain the energy of the stable model, and then perform differential charge density, partial charge density and energy band arrangement analysis.
2. The method for preparing a tantalum nitride-based heterojunction according to claim 1, characterized in that: In step S1, the calculation method is specifically as follows: The plane wave function basis vector cutoff energy is set to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10-5 eV, the force on each atomic force does not exceed 0.01 GPa, the Brillouin zone K point density is 0.04, the interaction between the valence electrons and the ion core is described by the pseudopotential generated by the projected augmented wave (PAW) method, the exchange correlation functional between electrons is described by GGA-PBE, and the Hubbard U treatment method is used for the transition metal Ta atom, and the U value of Ta is determined to be set to 6.47; Optimizing the unit cell structure of tantalum oxynitride and tantalum nitride comprises the following steps: The lattice and atomic positions of the tantalum nitride unit cell are optimized, wherein the lattice constant of the optimized tantalum nitride unit cell is The angle between the lattices is α = β = γ = 90°; The lattice and atomic positions of the tantalum oxynitride unit cell are optimized, wherein the lattice constant of the optimized tantalum oxynitride unit cell is The angles between the lattices are α=γ=90° and β=99.77°.
3. The method for preparing a tantalum nitride-based heterojunction according to claim 2, characterized in that: Step S2 is specifically as follows: By setting the plane wave function basis vector cutoff energy to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10 -5 eV, ion step is 1, broadening is 0.05, and Brillouin zone K-point density is 0.03 to calculate the 1s energy level of nitrogen atoms at the edge of the unit cell and then the core energy level position; In addition, the band structure was obtained by changing the K point in the Brillouin zone to a high symmetry point for non-self-consistent calculations.
4. The method for preparing a tantalum nitride-based heterojunction according to claim 3, characterized in that: Step S3 is specifically as follows: Tantalum oxynitride and tantalum nitride were sectioned along the crystal direction. The surface of tantalum oxynitride contained 6 tantalum atomic layers with a thickness of Its lattice constant is The angle between the lattices is 90°; The surface of tantalum nitride contains 7 layers of carbon atoms with a thickness of Its lattice constant is The angle between the lattices is 90°.
5. The method for preparing a tantalum nitride-based heterojunction according to claim 4, characterized in that: Step S4 is specifically as follows: The tantalum oxynitride surface and the tantalum nitride surface in step S3 are merged along the vertical direction of the Z axis to form a tantalum oxynitride-tantalum nitride heterojunction model, wherein the lattice mismatch calculation formula between the two is: Lattice mismatch μ = |x1-x2| / x2×100% In the formula, x1 is the lattice constant of the epitaxial layer, and x2 is the lattice constant of the substrate layer, wherein the epitaxial layer and the substrate layer are tantalum nitride and tantalum oxynitride, respectively.
6. The method for preparing a tantalum nitride-based heterojunction according to claim 5, characterized in that: In step S4, the interlayer spacing between the nearest atomic layers of tantalum oxynitride and tantalum nitride is tested, specifically: By moving in the vertical Z-axis direction, the distance between the two nearest neighboring atomic layers is adjusted, respectively from Move to The interval is Finally, the initial layer spacing is determined to be On the basis of determining the interlayer distance, the initial optimized site is determined by moving left and right between the two, and the final initial optimized site is the second site.
7. The method for preparing a tantalum nitride-based heterojunction according to claim 6, characterized in that: Step S5 is specifically as follows: The optimization method uses the calculation method proposed in step S1, and further fixes two layers of tantalum atoms in the bottom layer of tantalum oxynitride as the substrate layer; After optimization, the top oxygen atoms of tantalum oxynitride move upward to form chemical bonds with tantalum atoms in tantalum nitride; The nitrogen atoms in tantalum nitride move downward and form chemical bonds with the tantalum atoms in tantalum oxynitride.
8. The method for preparing a tantalum nitride-based heterojunction according to claim 7, characterized in that: Step S6 is specifically as follows: By setting the plane wave function basis vector cutoff energy to 520 eV, the convergence accuracy of the generalized gradient approximation correlation function GGA iteration process is set to 1.0×10 -5 The electronic state density of the heterojunction model was calculated using the ion step of 1, the broadening of 0.05, and the Brillouin zone K-point density of 0.
03. The core energy level was aligned by reading the 1s energy level of the nitrogen atom far away from the interface.