Method for testing viscosity of sticky mat
By cleaning the test board and cutting the multi-layer adhesive tape spline, and continuously peeling the peeling force data using the press roller rolling and test machine, the problem that the dust pad detection in the prior art cannot provide a better peeling force range. Accurate evaluation of viscosity of the sticky dust pad and improvement of product matching.
Patent Information
- Application Number
- CN202411038306.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-15
AI Technical Summary
The existing dust pad detection method cannot provide an excellent peeling force range, resulting in the product being easily peeled and replaced when the adhesion force is sufficient, and cannot meet the needs of different application environments.
By cleaning the test board and cutting the multi-layer adhesive tape spline, rolling it with a press roller, then leaving it to stand, combine with the test machine to continuously peel and record the peeling curve and peeling force data, and repeatedly obtain multiple sets of data to divide the easy peeling, It is easier to peel, more difficult to peel and difficult to peel range, and is used to evaluate the viscosity of the sticky dust pad.
Accurate evaluation of the viscosity of the sticky dust pad is achieved, and a variety of peeling force evaluation ranges are provided to help select suitable sticky dust pad products and improve product matching.
Smart Images

Figure CN118961574A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of sticky mats, and more specifically to a method for testing the viscosity of a sticky mat. Background Art
[0002] Sticky mats, also known as sticky floor glue, are mainly suitable for being placed at the entrance of clean spaces and in buffer zones. They can effectively remove dust from soles and wheels, minimizing the impact of dust on the quality of the clean environment, thereby achieving a simple dust removal effect and solving the problem that other floor mats cannot completely remove dust and cannot ensure that dust does not spread.
[0003] The closest technology to the existing technology is the announcement number: CN111909631B, a bactericidal emulsion pressure-sensitive adhesive, a sticky mat and a preparation method thereof, which discloses a bactericidal emulsion pressure-sensitive adhesive, a sticky mat and a preparation method thereof. In parts by weight, the bactericidal emulsion pressure-sensitive adhesive comprises at least 900-1100 parts of acrylate monomers, 0.2-2 parts of molecular weight regulators, 10-80 parts of surfactants, 0.01-0.05 parts of initiators, and 1200-1400 parts of deionized water; the surfactant comprises a quaternary ammonium salt surfactant.
[0004] This method can only detect the peeling force of a single layer of sticky mat, and when peeling the sticky mat, the layers are often peeled off, which cannot provide a better peeling force range, making the product easy to peel off and replace when the adhesion is sufficient.
[0005] In view of this, the present invention provides a method for testing the viscosity of a sticky mat which is easy to test and has high test accuracy. Summary of the invention
[0006] In view of this, in order to solve the problem that the existing sticky pad detection method cannot provide a better peeling force range, the present invention proposes a method for testing the viscosity of a sticky pad, comprising the following steps:
[0007] Step 1: Clean the test board until the working surface of the board is free of dust, residual glue and other debris;
[0008] Step 2, cutting a sample strip, wherein the sample strip includes multiple layers of adhesive tape, and adjacent adhesive tapes are stacked and connected;
[0009] Step 3: Peel off the sample strips obtained in step 2, bond the sample strips to the cleaned test plate, use a roller to roll the sample strips several times until there are no bubbles at the bonding point between the sample strips and the test plate, and let it stand for 20-40 minutes to avoid deformation of the adhesive layer after rolling. Test after the adhesive layer returns to normal;
[0010] Step 4: Fold the free end of the sample processed in step 3 by 180°, and peel off the joint about 25mm from the test plate. Clamp the free end of the sample and the test plate on the upper and lower clamps respectively. The testing machine peels continuously, and an automatic recorder draws the peeling curve and peeling force data.
[0011] Step 5, repeat steps 1 to 4 multiple times to obtain multiple sets of peeling force data, and compare the multiple sets of peeling force data with the peeling force set value. When the peeling force data is 2-4N / 45mm, it is in the easy peeling range; when the peeling force data is less than 2N / 45mm, it is in the easier peeling range; when the peeling force data is 4-6N / 45mm, it is in the difficult peeling range; when the peeling force data is greater than 6N / 45mm, it is in the difficult peeling range.
[0012] Furthermore, step one is to clean the test board with a wiping material dipped in a detergent, and wipe it dry with a clean absorbent gauze until there is no dust on the working surface of the board, and repeat three times until there is no residual glue and other debris on the working surface of the test board. After cleaning, the working surface of the board must not be touched by hands or other objects.
[0013] Furthermore, the cleaning agent is one of cyclohexane, gasoline, ethanol, isopropanol, and toluene, and the scrubbing material is one of absorbent gauze, bleaching cloth, and non-woven fabric.
[0014] In some embodiments, step three specifically includes peeling off the sample strip after sampling in step two, bonding the sample strip to the cleaned test plate, placing a polyester film about 200 mm long and 40 mm wide under the other end of the test plate, and using a pressure roller to roll the sample strip three times until there are no bubbles at the bonding point between the sample strip and the test plate and let it stand for 20-40 minutes.
[0015] Furthermore, in step three, the sample strips sampled in step two are peeled off, and the outer 3-5 layers of adhesive tape are torn off, and it is ensured that there are still 3-5 layers of adhesive tape on the sample strips after tearing off. Removing the outer layer of adhesive tape makes the detection more accurate, and the sample strips are bonded to the cleaned test plate. A polyester film about 200 mm long and 40 mm wide is placed under the other end of the test plate. The sample strips are rolled three times with a pressure roller and left to stand for 20-40 minutes, so that there are no bubbles at the bonding between the sample strips and the test plate.
[0016] Furthermore, in step 4, the descending speed of the testing machine is 300 mm / min±10 mm / min.
[0017] In some embodiments, in step 2, the sample strip has a width of 45 mm ± 1 mm and a length of 200 mm. The wider the width of the adhesive tape, the easier it is to perform the unwinding force test.
[0018] In some embodiments, the test plate needs to be polished before step 1. The surface of the test plate is polished with water-resistant sandpaper with a particle size of P280, first in the horizontal direction and then in the vertical direction. When the test plate has been used multiple times or has not been used for a long time, it should be polished before use.
[0019] In some embodiments, the test plate is made of SUS304 steel.
[0020] Furthermore, the test plate has a length of 125 mm ± 1 mm, a width of 50 mm ± 1 mm, and a thickness of 1.5-2.0 mm.
[0021] Beneficial effects of the present invention: The present invention proposes a method for testing the viscosity of a sticky mat, which is used to evaluate the peeling force between the tape layer and the sticky plate in the existing test specimen by testing the force between the tape layers in the test specimen, and to provide a variety of peeling force evaluation ranges. When the peeling force data is 2-4N / 45mm, it is an easy peeling range; when the peeling force data is less than 2N / 45mm, it is an easier peeling range; when the peeling force data is 4-6N / 45mm, it is a harder peeling range; when the peeling force data is greater than 6N / 45mm, it is a harder peeling range. The viscosity of the sticky mat can be selected according to the range to improve product matching. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 FIG. 1 is a diagram showing the test steps of the method for testing the viscosity of a sticky mat of the present invention. DETAILED DESCRIPTION
[0023] The following examples are described to assist the understanding of the present application, and the examples are not and should not be interpreted in any way as limiting the scope of protection of the present application.
[0024] In the following description, those skilled in the art will recognize that throughout this discussion, components may be described as separate functional units (which may include sub-units), but those skilled in the art will recognize that various components or portions thereof may be divided into separate components or may be integrated together (including within a single system or component).
[0025] At the same time, the connections between components or systems are not intended to be limited to direct connections, rather, the data between these components may be modified, reformatted, or otherwise changed by intermediate components. In addition, additional or fewer connections may be used. It should also be noted that the terms "coupled," "connected," or "input" should be understood to include direct connections, indirect connections through one or more intermediate devices, and wireless connections.
[0026] Embodiment 1:
[0027] like Figure 1As shown in FIG. 1 , it is a test step diagram of a method for testing the viscosity of a sticky mat of the present invention. The present invention provides a method for testing the viscosity of a sticky mat, comprising the following steps:
[0028] Step 1: Clean the test board until the working surface of the board is free of dust, residual glue and other debris;
[0029] Step 2, cutting a sample strip, wherein the sample strip includes multiple layers of adhesive tape, and adjacent adhesive tapes are stacked and connected;
[0030] Step 3: Peel off the sample strips obtained in step 2, bond the sample strips to the cleaned test plate, use a roller to roll the sample strips several times until there are no bubbles at the bonding point between the sample strips and the test plate, and let it stand for 20-40 minutes to avoid deformation of the adhesive layer after rolling. Test after the adhesive layer returns to normal;
[0031] Step 4: Fold the free end of the sample processed in step 3 by 180°, and peel off the joint about 25mm from the test plate, and clamp the free end of the sample and the test plate on the upper and lower clamps respectively. The test machine peels continuously, and an automatic recorder draws the peeling curve and peeling force data;
[0032] Step 5, repeat steps 1 to 4 multiple times to obtain multiple sets of peeling force data, and compare the multiple sets of peeling force data with the peeling force set value. When the peeling force data is 2-4N / 45mm, it is in the easy peeling range; when the peeling force data is less than 2N / 45mm, it is in the easier peeling range; when the peeling force data is 4-6N / 45mm, it is in the difficult peeling range; when the peeling force data is greater than 6N / 45mm, it is in the difficult peeling range.
[0033] Experimental process:
[0034] 1-10 groups of samples were taken, and the samples were artificially peeled and divided into group A, group B, group C, and group D of human sensory perception. Group A was the easy-to-peel group, group B was the relatively easy-to-peel group, group C was the relatively difficult-to-peel group, and group D was the difficult-to-peel group.
[0035] The test plate is 125mm ± 1mm in length, 50mm ± 1mm in width, and 1.5-2.0mm in thickness. The test plate is made of SUS304 steel.
[0036] Pretreatment: Before step 1, the test board needs to be polished. The surface of the test board is polished horizontally and then vertically with water-resistant sandpaper with a particle size of P280. When the test board has been used many times or has not been used for a long time, it should be polished before use; Step 1: Clean the test board with wiping material dipped in ethanol, and wipe it with a clean degreased gauze until there is no dust on the working surface of the board. Repeat three times until there is no residual glue and other debris on the working surface of the test board. After cleaning, do not touch the working surface of the board with your hands or other objects; Step 2: Cut a sample with a width of 45mm and a length of 200mm. The sample includes multiple layers of adhesive tape, and adjacent adhesive tapes are stacked and connected; Step 3: Tear off the outer 3-5 layers of adhesive tape, and ensure that there are still 3-5 layers of adhesive tape on the sample after tearing. Removing the outer tape makes the test more accurate. Bond the sample to the cleaned test board, place a polyester film about 200mm long and 40mm wide under the other end of the test board, and use a pressure roller to perform three-way pressure on the sample. Roll and let stand for 20-40 minutes to make sure that there are no bubbles at the bonding point between the sample and the test plate, and to avoid deformation of the adhesive layer after rolling. Test after the adhesive layer recovers to normal; Step 4, fold the free end of the sample processed in Step 3 by 180°, and peel off the bonding position about 25mm from the test plate, and clamp the free end of the sample and the test plate on the upper and lower clamps respectively. The test machine continuously peels, and the descending speed of the test machine is 300mm / min±10mm / min, and an automatic recorder draws the peeling curve and peeling force data. Step 5, repeat steps 1 to 4 for multiple times to obtain multiple sets of peeling force data, see Table 1, compare the multiple sets of peeling force data with the peeling force set value, when the peeling force data is 2-4N / 45mm, it is in the easy peeling range; when the peeling force data is less than 2N / 45mm, it is in the relatively easy peeling range; when the peeling force data is 4-6N / 45mm, it is in the relatively difficult peeling range; when the peeling force data is greater than 6N / 45mm, it is in the difficult peeling range.
[0037] Table 1
[0038] Spline sequence Test 1 Test 2 Test 3 Mean Human senses 1 3.42 3.59 3.46 3.49 A 2 8.24 7.96 8.04 8.08 D 3 5.86 5.82 5.71 5.80 C 4 1.17 1.19 1.32 1.23 B 5 2.87 2.69 2.38 2.65 A 6 3.21 2.97 3.09 3.09 A 7 1.32 1.58 1.63 1.51 B 8 5.55 5.41 5.63 5.53 C 9 4.23 4.56 4.37 4.39 C 10 7.25 7.47 7.62 7.45 D
[0039] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A method for testing the viscosity of a sticky mat, characterized in that , including the following steps, Step 1: Clean the test board until the working surface of the board is free of dust, residual glue and other debris; Step 2, cutting a sample strip, wherein the sample strip includes multiple layers of adhesive tape, and adjacent adhesive tapes are stacked and connected; Step 3: Peel off the sample strips obtained in step 2, bond the sample strips to the cleaned test plate, and use a roller to roll the sample strips several times until there are no bubbles at the bonding point between the sample strips and the test plate and let it stand for 20-40 minutes to avoid deformation of the adhesive layer after rolling. Test after the adhesive layer returns to normal; Step 4: Fold the free end of the sample processed in step 3 by 180°, and peel off the joint about 25mm from the test plate. Clamp the free end of the sample and the test plate on the upper and lower clamps respectively. The testing machine peels continuously, and an automatic recorder draws the peeling curve and peeling force data. Step 5, repeat steps 1 to 4 multiple times to obtain multiple sets of peeling force data, and compare the multiple sets of peeling force data with the peeling force set value. When the peeling force data is 2-4N / 45mm, it is in the easy peeling range; when the peeling force data is less than 2N / 45mm, it is in the easier peeling range; when the peeling force data is 4-6N / 45mm, it is in the difficult peeling range; when the peeling force data is greater than 6N / 45mm, it is in the difficult peeling range.
2. The method for testing the viscosity of a sticky mat as claimed in claim 1, wherein: Step 1 is to clean the test board with a wiping material dipped in a detergent, and then wipe it with a clean absorbent gauze until there is no dust on the working surface of the board. Repeat this process three times until there is no residual glue or other debris on the working surface of the test board. After cleaning, do not touch the working surface of the board with your hands or other objects.
3. The method for testing the viscosity of a sticky mat as claimed in claim 2, wherein: The cleaning agent is one of cyclohexane, gasoline, ethanol, isopropanol and toluene, and the scrubbing material is one of absorbent gauze, bleaching cloth and non-woven fabric.
4. The method for testing the viscosity of a sticky mat as claimed in claim 1, wherein: Step three is specifically, step three is specifically, peeling off the sample strip after sampling in step two, bonding the sample strip to the cleaned test plate, placing a polyester film about 200 mm long and 40 mm wide under the other end of the test plate, using a pressure roller to roll the sample strip three times until there are no bubbles at the bonding point between the sample strip and the test plate and let it stand for 20-40 minutes.
5. The method for testing the viscosity of a sticky mat as claimed in claim 4, characterized in that: In step three, peel off the sample strips sampled in step two, tear off the outer 3-5 layers of adhesive tape, and ensure that there are still 3-5 layers of adhesive tape on the sample strips after tearing off. Removing the outer layer of tape makes the test more accurate. Bond the sample strips to the cleaned test plate, place a polyester film about 200 mm long and 40 mm wide under the other end of the test plate, use a pressure roller to roll the sample strips three times and let it stand for 20-40 minutes to ensure that there are no bubbles at the bonding between the sample strips and the test plate.
6. The method for testing the viscosity of a sticky mat as claimed in claim 1, wherein: In step 4, the descending speed of the testing machine is 300 mm / min±10 mm / min.
7. The method for testing the viscosity of a sticky mat as claimed in claim 1, wherein: In step 2, the sample strip has a width of 45 mm ± 1 mm and a length of 200 mm. The wider the width of the adhesive tape, the easier it is to perform the unwinding force test.
8. The method for testing the viscosity of a sticky mat as claimed in claim 1, wherein: Before step 1, the test board needs to be polished. Use water-resistant sandpaper with a particle size of P280 on the surface of the test board. First polish it horizontally and then polish it vertically. When the test board has been used many times or has not been used for a long time, it should be polished before use.
9. The method for testing the viscosity of a sticky mat as claimed in claim 1, wherein: The test plate is made of SUS304 steel.
10. The method for testing the viscosity of a sticky pad as claimed in claim 1, wherein: The test plate has a length of 125 mm ± 1 mm, a width of 50 mm ± 1 mm, and a thickness of 1.5-2.0 mm.
Citation Information
Patent Citations
A bactericidal emulsion pressure-sensitive adhesive, a dust-repellent mat, and its preparation method
CN111909631B