Application of AuNCs-dmSiO2 composite material in detection of organophosphorus pesticide on oxygen and phosphorus

Through the combination of AuNCs@dmSiO2 composite material with Cu2+ quenching effect and acetylcholinesterase reaction, a simple and fast fluorescence detection method was developed, which solved the problem of complex existing technology and insufficient fluorescence intensity of gold nanoclusters, and realized the use of organic phosphorus pesticides Efficient and portable detection of paraoxyphosphorus.

CN118961667AActive Publication Date: 2024-11-15NANOZYME LABORATORY IN ZHONGYUAN

Patent Information

Application Number
CN202411177642.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-15
Estimated Expiration
2044-08-26

AI Technical Summary

Technical Problem

The existing organic phosphorus pesticide detection technology is complex, expensive and not suitable for agricultural field applications. Traditional methods require advanced equipment and professional operation, and the low quantum yield of gold nanoclusters limits its wide application.

Method used

Using AuNCs@dmSiO2 composite material, a simple, simple, Fast fluorescence detection method, loading on cotton swabs to achieve portable detection.

Benefits of technology

High selectivity and quantitative detection of organophosphorus pesticide para-oxyphosphorus is achieved, with a detection limit of 0.032 ng/mL, overcoming the disadvantage of weak fluorescence intensity of gold nanoclusters and providing a portable and simple field detection technology.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118961667A_ABST
    Figure CN118961667A_ABST
Patent Text Reader

Abstract

The invention discloses application of an AuNCs-dmSiO2 composite material in detection of oxygen and phosphorus in organophosphorus pesticide, and belongs to the technical field of fluorescence sensing. Mesoporous silica spheres are combined with AuNCs, an AuNCs-dmSiO2 fluorescent composite material with better fluorescent property is prepared through a space confinement effect, based on a quenching effect of Cu < 2 + > on the fluorescent composite probe, a reaction product thiocholine of acetylcholin esterase and a substrate acetylthiocholine (ATCh) is combined with Cu < 2 + >, so that fluorescence of the probe is recovered, and the fluorescence of the probe is recovered. And the organophosphorus pesticide can inactivate acetylcholin esterase to cause quenching of a fluorescence system, so that the AuNCs-dmSiO2 composite material is used for fluorescence detection of the organophosphorus pesticide on oxygen and phosphorus.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of fluorescence sensing, and specifically relates to the application of AuNCs@dmSiO2 composite materials in the detection of organophosphorus pesticide paraoxon. Background Art

[0002] Organophosphorus pesticides (OPs) are widely used in agriculture to control pests and increase crop yields. However, as public concern about food safety increases, the issue of OP residues has attracted widespread attention. These residues enter the human body through ingestion, skin contact, and inhalation, and may affect the nervous, endocrine, and immune systems, manifesting as symptoms of headache, nausea, vomiting, and even potentially fatal poisoning. In addition, long-term exposure to OPs may increase the risk of cancer, reproductive system abnormalities, and neurological diseases. Therefore, accurate detection of OPs is essential to maintaining food safety and public health.

[0003] Traditional techniques, such as chromatography and mass spectrometry, have been used for the detection of organophosphorus pesticide residues. However, these traditional techniques not only require expensive equipment and complex operating procedures, are time-consuming, and require skilled operators, which limits their field application in agricultural environments. Therefore, it is necessary to establish efficient organophosphorus pesticide detection methods.

[0004] In recent years, fluorescence has emerged as a new detection technology and has shown unique advantages in the detection of organophosphorus pesticide residues. They have the advantages of high sensitivity, rapid response, simple operation and real-time monitoring, and therefore have broad application prospects and important practical significance in the detection of organophosphorus pesticides. The development of high-performance fluorescent probes is essential to improve the efficiency of sensors. Gold nanoclusters (AuNCs) have attracted widespread attention due to their attractive physicochemical properties, including strong photoluminescence, non-toxicity, high water solubility and excellent biocompatibility, but the low quantum yield of AuNCs is the main obstacle to their widespread application. Summary of the invention

[0005] The present invention aims to provide an application of AuNCs@dmSiO2 composite material in the detection of organophosphorus pesticide paraoxon.

[0006] Based on the above purpose, the present invention adopts the following technical solutions: Application of AuNCs@dmSiO2 composite materials (mesoporous silica spheres loaded with gold nanoclusters) in the detection of organophosphorus pesticide paraoxon.

[0007] The application method comprises the following steps: a. Mix the test solution containing the organophosphorus pesticide paraoxon, acetylcholinesterase, acetylthiocholine and a portion of Tris-HCl buffer solution, incubate, and then add Cu2+ solution and another part of Tris-HCl buffer solution to obtain a mixed solution; b. Adding the AuNCs@dmSiO2 composite material aqueous solution to the mixed solution in step a, mixing to obtain a test solution, and performing fluorescence spectrum detection on the test solution; Alternatively, the carrier loaded with the AuNCs@dmSiO2 composite material is placed in the mixed solution of step a, immersed, taken out, and the carrier is analyzed.

[0008] In step b, the carrier is a cotton swab. The cotton swab loaded with the AuNCs@dmSiO2 composite material is immersed in the mixed solution of step a. The cotton swab is photographed under ultraviolet light, the color RGB value of the image is identified, and the paraoxon concentration is determined by calculating the color signal ratio R / (G+B).

[0009] In step a, the concentration of the Tris-HCl buffer solution is 17-25 mM, the pH value is 5-10, the concentration of acetylcholinesterase is 0.8-1.5 U / mL, the concentration of acetylthiocholine is 0.7-1.5 mM, and the concentration of Cu 2+ The concentration of the solution is 0.05-0.15 mM; in step b, the concentration of the AuNCs@dmSiO2 composite material aqueous solution is 1.0-1.5 mg / mL, Tris-HCl buffer solution, acetylcholinesterase, acetylthiocholine, Cu 2+ The volume ratio of the solution and the AuNCs@dmSiO2 composite material aqueous solution is (360-465): (10-15): (15-25): (50-80): (450-650); the incubation conditions are: the incubation temperature is 30-40 °C, and the incubation time is 30-50 min; the AuNCs@dmSiO2 composite material aqueous solution is prepared by dispersing the AuNCs@dmSiO2 composite material in water.

[0010] The preparation method of the AuNCs@dmSiO2 composite material comprises the following steps: 1) Preparation of AuNCs solution: Mix glutathione aqueous solution and chloroauric acid aqueous solution, heat and stir, dialysis purification, freeze-dry, and disperse the obtained solid in water to obtain AuNCs solution; 2) Preparation of dmSiO2 dispersion: triethanolamine, hexadecyltrimethylammonium bromide, sodium salicylate and water are mixed, heated and stirred, ethyl orthosilicate is added, heated and stirred for reaction, cooled, precipitates are collected, washed and purified, the precipitates are dispersed in an organic solvent, ammonia water and (3-aminopropyl)triethoxysilane are added, stirred for reaction, the products are collected, washed and freeze-dried to obtain mesoporous silica spheres, and the mesoporous silica spheres are dispersed in water to obtain dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: The AuNCs solution in step 1) and the dmSiO2 dispersion in step 2) were mixed, and freeze-dried to obtain the AuNCs@dmSiO2 composite material (mesoporous silica spheres loaded with gold nanocluster material).

[0011] In step 1), the molar ratio of glutathione in the glutathione aqueous solution to chloroauric acid in the chloroauric acid aqueous solution is (1-3):2; the heating and stirring conditions are: temperature of 65-75°C, stirring speed of 500-800 rpm, and time of 20-30 h.

[0012] In step 2), the amount ratio of triethanolamine, hexadecyltrimethylammonium bromide, sodium salicylate, tetraethyl orthosilicate, ammonia water and (3-aminopropyl)triethoxysilane is (60-80) mg: (360-400) mg: (140-180) mg: (3-5) mL: (2-4) mL: (0.5-1.5) mL; at a stirring speed of 500-800 rpm, triethanolamine, hexadecyltrimethylammonium bromide, sodium salicylate and water are mixed, stirred at 80-90 ° C for 1-2 h, tetraethyl orthosilicate is added, stirred at 70-85 ° C for 2-3 h, cooled, and the precipitate is collected. After washing and purification, the precipitate is dispersed in an organic solvent, and ammonia water and (3-aminopropyl)triethoxysilane are added at a stirring speed of 500-800 rpm, and stirred for 10-15 h; the organic solvent is ethanol.

[0013] In step 3), the mass ratio of dmSiO2 in the dmSiO2 dispersion and AuNCs in the AuNCs solution is (1-5):1, and the mixing conditions are: temperature of 20-35 °C and time of 10-20 min; the particle size of the AuNCs@dmSiO2 composite material is 250-300 nm.

[0014] The preparation method of the cotton swab loaded with the AuNCs@dmSiO2 composite material is as follows: placing the cotton swab in a solution containing the AuNCs@dmSiO2 composite material and gelatin, soaking for 10-15 minutes, taking out, and freeze-drying; in the solution, the concentration of the AuNCs@dmSiO2 composite material is 1.0-1.5 mg / mL, and the concentration of the gelatin is 4.0-7.0 mg / mL.

[0015] In step b, a cotton swab loaded with AuNCs@dmSiO2 composite material is placed in the mixed solution of step a, each cotton swab is loaded with 0.50-0.75 mg AuNCs@dmSiO2 composite material, and 1 cotton swab can be used for 500 μL of the mixed solution; in step a, the concentration of Tris-HCl buffer solution is 17-25 mM, the pH value is 5-10, the concentration of acetylcholinesterase is 0.8-1.5 U / mL, the concentration of acetylthiocholine is 0.7-1.5 mM, and the concentration of Cu is 1. 2+ The concentration of the solution is 0.05-0.15 mM, Tris-HCl buffer solution, acetylcholinesterase, acetylthiocholine, Cu 2+ The volume ratio of the solution is (360-465): (10-15): (15-25): (50-80); incubation conditions: incubation temperature is 30-40 °C, and incubation time is 30-50 min.

[0016] Compared with the prior art, the present invention has the following beneficial effects: 1) In the present invention, mesoporous silica spheres are combined with AuNCs to prepare AuNCs@dmSiO2 fluorescent composite materials with better fluorescence properties through spatial confinement effect. 2+ The quenching effect of the fluorescent composite probe is that the reaction product of acetylcholinesterase and substrate acetylthiocholine (ATCh) binds to Cu 2+ The probe fluorescence is restored, and organophosphorus pesticides can inactivate acetylcholinesterase, resulting in quenching of the fluorescence system. The sensing mechanism is as follows Fig.13 As shown, therefore, the AuNCs@dmSiO2 composite material was used for the fluorescence detection of the organophosphorus pesticide paraoxon; 2) The present invention prepares gold nanoclusters (AuNCs) and pomegranate-shaped mesoporous silica spheres (dmSiO2) with the best fluorescence emission, and then mixes the dmSiO2 dispersion and the AuNCs solution. Based on electrostatic interaction, the confinement effect of dmSiO2 is used to enhance the fluorescence of the gold nanoclusters, thereby effectively overcoming the disadvantage of weak fluorescence intensity of AuNCs and preparing AuNCs@dmSiO2 composite materials with the best fluorescence intensity. The preparation method is simple, rapid and pollution-free. 3) The AuNCs@dmSiO2 composite material of the present invention is applied to the fluorescence detection method of the organophosphorus pesticide paraoxon, which has simple and fast steps and can achieve highly selective and specific quantitative detection of organophosphorus pesticides with a detection limit of 0.032 ng / mL; 4) The present invention prepares a portable detection cotton swab by loading the AuNCs@dmSiO2 composite material on a cotton swab to detect the organophosphorus pesticide paraoxon, providing a promising portable technology for the qualitative identification and quantitative detection of the organophosphorus pesticide paraoxon on site. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the technical solution of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without paying creative work.

[0018] Figure 1 This is a fluorescence emission spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 1; Figure 2 This is a fluorescence emission spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 2; Figure 3 This is a fluorescence emission spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 3; Figure 4 This is a fluorescence emission spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 4; Figure 5 This is a fluorescence emission spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 5; Figure 6 The fluorescence emission spectra of the gold nanoclusters, mesoporous silica spheres and mesoporous silica spheres loaded with gold nanoclusters prepared in Example 5; Figure 7 This is a SEM spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 5; Figure 8 This is the TEM spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 5; Fig. 9 The AuNCs solution (gold nanoclusters) and AuNCs@dmSiO2 composite material (mesoporous silica spheres loaded with gold nanoclusters) prepared in Example 5 were used to measure the Cu 2+ Sensing test results, where 9A and 9B are the result graphs of the AuNCs solution (gold nanoclusters) prepared in Example 5, 9A is a fluorescence spectrum graph, Fig. 9 B is Cu 2+ The concentration is the horizontal axis, and the fluorescence intensity ratio signal (F / F0) is the vertical axis fitting straight line; 9C and 9D are the result graphs of the AuNCs@dmSiO2 composite material prepared in Example 5, 9C is the fluorescence spectrum, and 9D is the Cu2+ The concentration is the horizontal axis, and the fluorescence intensity ratio signal (F / F0) is the vertical axis fitting straight line; Fig.10 10A is a fluorescence spectrum of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 5 detecting different concentrations of paraoxon, 10B is a fitted straight line with the concentration of paraoxon as the abscissa and the fluorescence intensity ratio signal (F / F0) as the ordinate, where F and F0 represent the fluorescence intensity when paraoxon is present and absent in the detection system, respectively; Fig.11 The selectivity test results of the mesoporous silica sphere-loaded gold nanocluster material prepared in Example 5 for detecting organophosphorus pesticides; Fig.12 middle, Fig.12 A is a schematic diagram of the preparation process of cotton swabs loaded with AuNCs@dmSiO2 composite materials. Fig.12 B is a photo of a cotton swab containing different concentrations of the organophosphorus pesticide paraoxon taken under ultraviolet light. Fig.12 C is the fitting curve between the color signal ratio (R / (G+B)) and the paraoxon concentration; Fig.13 The sensing mechanism of the AuNCs@dmSiO2 composite material of the present invention. DETAILED DESCRIPTION

[0019] In order to make the purpose, technical scheme and advantages of the present invention clearer, the technical scheme of the present invention is described in detail below, but the following embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other implementation methods obtained by those skilled in the art without making creative work belong to the scope of protection of the present invention.

[0020] Example 1 The preparation method of the AuNCs@dmSiO2 composite material comprises the following steps: 1) Preparation of AuNCs solution: glutathione and chloroauric acid were dissolved in water respectively to prepare 50 mM glutathione aqueous solution and 5 mM chloroauric acid aqueous solution. 0.6 mL glutathione aqueous solution and 4.0 mL chloroauric acid aqueous solution were mixed. The mixture was stirred at 65 °C and 600 rpm for 20 h. After that, the mixture was dialyzed and freeze-dried. The obtained solid was dispersed in water to obtain 1 mg / mL AuNCs solution. 2) Preparation of dmSiO2 dispersion: Mix 68 mg of triethanolamine, 380 mg of hexadecyltrimethylammonium bromide, and 168 mg of sodium salicylate with 25 mL of water at a stirring speed of 500 rpm, stir at 80 °C for 1 h, add 4 mL of tetraethyl orthosilicate, stir at 70 °C for 2 h, cool to room temperature, collect the precipitate by centrifugation, wash three times with ethanol (analytical grade, the same below), disperse the precipitate in a mixture of 50 mL of methanol (analytical grade, the same below) and 3 mL of hydrochloric acid (mass concentration 38%, the same below), reflux at 60 °C for 6 h, disperse the purified precipitate in 100 mL of ethanol, add 2.5 mL of ammonia water (mass concentration 26%, the same below) and 1 mL of (3-aminopropyl)triethoxysilane (APTES, analytical grade, the same below) at a stirring speed of 800 rpm, and stir at room temperature for 12 h, collect the product, wash it 3 times with ethanol, then wash it 3 times with deionized water, freeze-dry it for 12 h to obtain mesoporous silica spheres, disperse the mesoporous silica spheres in water to obtain 2 mg / mL dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: Mix 2 mL of AuNCs solution (1 mg / mL) prepared in step 1) and 1 mL of dmSiO2 dispersion (2 mg / mL) prepared in step 2), stir for 10 min at 25°C, and freeze-dry to obtain AuNCs@dmSiO2 composite material.

[0021] A certain amount of AuNCs@dmSiO2 was dispersed in water to obtain a AuNCs@dmSiO2 aqueous solution with a concentration of 0.4 mg / mL. Its fluorescence spectrum is shown in the figure below. Figure 1 shown.

[0022] Example 2 The difference from Example 1 is that in step 2), the mesoporous silica spheres are dispersed in water to prepare a 4 mg / mL dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: Mix 2 mL of AuNCs solution (1 mg / mL) from step 1) and 1 mL of dmSiO2 dispersion (4 mg / mL) from step 2), stir for 10 min at 25 °C, and freeze-dry to obtain AuNCs@dmSiO2 composite material.

[0023] A certain amount of AuNCs@dmSiO2 was dispersed in water to obtain a AuNCs@dmSiO2 aqueous solution with a concentration of 0.6 mg / mL. Its fluorescence spectrum is shown in the figure below. Figure 2 shown.

[0024] Example 3 The difference from Example 1 is that in step 2), the mesoporous silica spheres are dispersed in water to prepare a 6 mg / mL dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: Mix 2 mL of AuNCs solution (1 mg / mL) from step 1) and 1 mL of dmSiO2 dispersion (6 mg / mL) from step 2), stir for 10 min at 25 °C, and freeze-dry to obtain AuNCs@dmSiO2 composite material.

[0025] A certain amount of AuNCs@dmSiO2 was dispersed in water to obtain a AuNCs@dmSiO2 aqueous solution with a concentration of 0.8 mg / mL. Its fluorescence spectrum is shown in the figure below. Figure 3 shown.

[0026] Example 4 The difference from Example 1 is that in step 2), the mesoporous silica spheres are dispersed in water to prepare a 8 mg / mL dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: Mix 2 mL of AuNCs solution (1 mg / mL) from step 1) and 1 mL of dmSiO2 dispersion (8 mg / mL) from step 2), stir for 10 min at 25 °C, and freeze-dry to obtain AuNCs@dmSiO2 composite material.

[0027] A certain amount of AuNCs@dmSiO2 was dispersed in water to obtain a 1.0 mg / mL AuNCs@dmSiO2 aqueous solution. Its fluorescence spectrum is shown in the figure below. Figure 4 shown.

[0028] Example 5 The difference from Example 1 is that in step 2), the mesoporous silica spheres are dispersed in water to prepare a 10 mg / mL dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: Mix 2 mL of AuNCs solution (1 mg / mL) prepared in step 1) and 1 mL of dmSiO2 dispersion (10 mg / mL) prepared in step 2), stir for 10 min at 25°C, and freeze-dry to obtain AuNCs@dmSiO2 composite material.

[0029] A certain amount of AuNCs@dmSiO2 composite material was dispersed in water to obtain a AuNCs@dmSiO2 aqueous solution with a concentration of 1.2 mg / mL. Its fluorescence spectrum is shown in the figure below. Figure 5 shown.

[0030] Depend on Figure 1-5It is known that, under the same mass of AuNCs, the fluorescence intensity of the AuNCs@dmSiO2 composite material prepared in Example 5 is the highest.

[0031] The AuNCs solution and dmSiO2 dispersion prepared in Example 5 were subjected to fluorescence analysis. The fluorescence spectra of the AuNCs solution, dmSiO2 dispersion and AuNCs@dmSiO2 aqueous solution prepared in Example 5 are shown in FIG. Figure 6 shown.

[0032] from Figure 6 It can be seen that dmSiO2 has no fluorescence. Before and after dmSiO2 loading, the fluorescence of AuNCs is enhanced by 2.6 times, and the fluorescence emission peak is blue-shifted by 6 nm from 604 nm to 598 nm.

[0033] The SEM image of the AuNCs@dmSiO2 composite material (mesoporous silica spheres loaded with gold nanocluster material) prepared in Example 5 is shown in FIG. Figure 7 As shown in the TEM image Figure 8 shown.

[0034] from Figure 7 It can be seen that the mesoporous silica sphere-loaded gold nanocluster material of the present invention has a pomegranate-shaped morphology and a uniform size, with a particle diameter of 250-300 nm.

[0035] from Figure 8 It can be seen that the mesoporous silica sphere-loaded gold nanocluster material has radial pore channels, which is more conducive to the enrichment of the substrate and improves the detection sensitivity.

[0036] Example 6 The preparation method of the AuNCs@dmSiO2 composite material comprises the following steps: 1) Preparation of AuNCs solution: glutathione and chloroauric acid were dissolved in water respectively to prepare 50 mM glutathione aqueous solution and 5 mM chloroauric acid aqueous solution, 0.4 mL glutathione aqueous solution and 4.0 mL chloroauric acid aqueous solution were mixed, stirred at 65 °C and 500 rpm for 28 h, dialyzed and purified, freeze-dried, and the obtained solid was dispersed in water to obtain AuNCs solution; 2) Preparation of dmSiO2 dispersion: Mix 75 mg of triethanolamine, 360 mg of hexadecyltrimethylammonium bromide, and 180 mg of sodium salicylate with 30 mL of water at a stirring speed of 700 rpm, stir at 90 °C for 2 h, add 3 mL of tetraethyl orthosilicate, stir at 85 °C for 3 h, cool to room temperature, collect the precipitate by centrifugation, wash three times with ethanol, disperse the precipitate in a mixture of 55 mL of methanol and 4 mL of hydrochloric acid, and reflux at 60 °C for 5 h, disperse the purified precipitate in 110 mL of ethanol, add 3 mL of ammonia water and 1.5 mL of (3-aminopropyl)triethoxysilane (APTES) at a stirring speed of 800 rpm, stir at room temperature for 15 h, collect the product, wash the product three times with ethanol, then wash it three times with deionized water, and freeze-dry it for 12 h, obtain mesoporous silica spheres, disperse the mesoporous silica spheres (dmSiO2) in water to obtain a dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: The AuNCs solution in step 1) and the dmSiO2 dispersion in step 2) were mixed at a mass ratio of dmSiO2 to AuNCs of 2:1, stirred at 25°C for 10 min, and freeze-dried to obtain the AuNCs@dmSiO2 composite material.

[0037] A certain amount of AuNCs@dmSiO2 was dispersed in water to obtain an AuNCs@dmSiO2 aqueous solution.

[0038] Example 7 The preparation method of the AuNCs@dmSiO2 composite material comprises the following steps: 1) Preparation of AuNCs solution: glutathione and chloroauric acid were dissolved in water respectively to prepare 50 mM glutathione aqueous solution and 5 mM chloroauric acid aqueous solution, 0.2 mL glutathione aqueous solution and 4.0 mL chloroauric acid aqueous solution were mixed, stirred at 85 °C and 800 rpm for 30 h, dialyzed and freeze-dried, and the obtained solid was dispersed in water to obtain AuNCs solution; 2) Preparation of dmSiO2 dispersion: 80 mg of triethanolamine, 400 mg of hexadecyltrimethylammonium bromide, 180 mg of sodium salicylate and 35 mL of water were mixed at a stirring speed of 600 rpm, stirred at 80 °C for 2 h, 5 mL of tetraethyl orthosilicate was added, stirred at 70 °C for 3 h, cooled to room temperature, centrifuged to collect the precipitate, washed with ethanol three times, dispersed the precipitate in a mixture of 60 mL of methanol and 5 mL of hydrochloric acid, and refluxed at 60 °C for 6 h, dispersed the purified precipitate in 120 mL of ethanol, added 4 mL of ammonia water and 0.5 mL of (3-aminopropyl)triethoxysilane (APTES) at a stirring speed of 800 rpm, stirred at room temperature for 15 h, collected the product, washed the product with ethanol three times, washed it with deionized water three times, and freeze-dried it for 12 h. h, obtaining mesoporous silica spheres, dispersing the mesoporous silica spheres in water to obtain a dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: The AuNCs solution in step 1) and the dmSiO2 dispersion in step 2) were mixed at a mass ratio of dmSiO2 to AuNCs of 5:1, stirred at 25°C for 20 min, and freeze-dried to obtain the AuNCs@dmSiO2 composite material.

[0039] A certain amount of AuNCs@dmSiO2 was dispersed in water to obtain an AuNCs@dmSiO2 aqueous solution.

[0040] Example 8 The preparation method of cotton swabs loaded with AuNCs@dmSiO2 composite materials is as follows: a medical cotton swab is placed in a solution containing the AuNCs@dmSiO2 composite material prepared in the above Example 5 and gelatin, soaked for 10 min, taken out, and freeze-dried to obtain; in the solution, the concentration of the AuNCs@dmSiO2 composite material is 1.2 mg / mL, and the concentration of gelatin is 5.0 mg / mL, and each cotton swab is loaded with 0.60 mg of the AuNCs@dmSiO2 composite material.

[0041] Example 9 Sensitivity Detection Test Similarly, 60 μL of different concentrations of Cu 2+ The solution was mixed with 340 μL Tris-HCl buffer solution (pH 6.0, 20 mM), 500 μL AuNCs solution (0.2 mg / mL, prepared by diluting the AuNCs solution in Example 5) and 100 μL H2O to obtain a mixed solution with an excitation wavelength of 405 nm, an emission wavelength of 604 nm, an excitation light source slit of 10 nm, and an emission light source slit of 5 nm. Fluorescence detection was performed using a 1 cm × 1 cm cuvette. The fluorescence spectrum is shown in Figure 9A. Fig. 9 B is Cu 2+ The concentration is the horizontal axis and the fluorescence intensity ratio signal (F / F0) is the vertical axis for fitting the straight line.

[0042] 60 μL of Cu 2+ The solution was mixed with 340 μL Tris-HCl buffer solution (pH 6.0, 20 mM), 500 μL AuNCs@dmSiO2 aqueous solution (1.2 mg / mL, prepared by dispersing the AuNCs@dmSiO2 composite material of Example 5 in water) and 100 μL H2O to obtain a mixed solution with an excitation wavelength of 405 nm, an emission wavelength of 598 nm, an excitation light source slit of 10 nm, and an emission light source slit of 5 nm. Fluorescence detection was performed using a 1 cm × 1 cm cuvette. The fluorescence spectrum is shown in Figure 9C. Fig. 9 D is Cu 2+ The concentration is the horizontal axis and the fluorescence intensity ratio signal (F / F0) is the vertical axis for fitting the straight line.

[0043] Fig. 9 Cu in A, 9B, 9C, 9D 2+ The concentration is the Cu 2+ final concentration.

[0044] Fig. 9 A shows that as Cu 2+ With the increase of concentration, the fluorescence of AuNCs gradually decreased; Fig. 9 B can be seen that this method has a great 2+ The detectable range is 0.1-3.0 μM, and the linear equation is F / F0=1.004-0.147[Cu 2+ ], ng / mL, and the detection limit was 35 nM.

[0045] Fig. 9 C shows that as Cu 2+ With the increase of concentration, the fluorescence intensity of AuNCs@dmSiO2 gradually decreased; Fig. 9 D can be seen that this method has a great 2+ The detectable range is 0.005-3.0 μM, and the linear equation is F0 / F=0.983-0.191[Cu 2+ ], ng / mL, with a detection limit of 2.8 nM. The Cu 2+The detection limit is as low as 1 / 10 of the detection line using AuNCs as probes. This indicates that the porous structure of the carrier material dmSiO2 can provide a larger surface area, increase the contact area between the probe and the target substance, and make the probe more sensitive to the target substance. In addition, the dmSiO2 matrix with abundant pores can be used as a high-performance adsorbent to effectively adsorb and enrich the target substance, promote the diffusion and transport of the target substance, and thus improve the response sensitivity of the analyte.

[0046] Example 10 Detection test of organophosphorus pesticide paraoxon The application of AuNCs@dmSiO2 composite material in the detection of organophosphorus pesticide paraoxon includes the following steps: a. 40 μL of the test solution containing different concentrations of the organophosphorus pesticide paraoxon was mixed with 12 μL of acetylcholinesterase (1.0 U / mL), 20 μL of acetylthiocholine (1.0 mM) and 28 μL of Tris-HCl buffer solution (pH 7.4, 20 mM), incubated at 37°C for 40 min, and then 60 μL of Cu 2+ solution (0.1 mM), 340 μL Tris-HCl buffer solution (pH 6.0, 20 mM) to obtain a mixed solution; b. Add 500 μL of the AuNCs@dmSiO2 composite material aqueous solution (1.2 mg / mL) of Example 5 to the mixed solution in step a, mix, and obtain a test solution. The excitation wavelength is 405 nm, the emission wavelength is 598 nm, the excitation light source slit is 10 nm, and the emission light source slit is 5 nm. Use a 1 cm×1 cm cuvette to perform fluorescence spectrum detection on the test solution. The fluorescence spectrum is shown in Figure 10A. Fig.10 B is a fitted straight line with paraoxon concentration as the horizontal axis and fluorescence intensity ratio signal (F / F0) as the vertical axis. The final concentration of paraoxon in each test solution is 0 ng / mL, 0.05 ng / mL, 0.1 ng / mL, 0.5 ng / mL, 1 ng / mL, 2 ng / mL, 4 ng / mL, 6 ng / mL, 8 ng / mL, 10 ng / mL, 15 ng / mL, 20 ng / mL, 25 ng / mL, 30 ng / mL, 40 ng / mL, and 50 ng / mL.

[0047] Fig.10 A shows that with the increase of paraoxon concentration, the fluorescence of AuNCs@dmSiO2 gradually decreases; Fig.10As can be seen from B, this method can detect paraoxon in the range of 0.05-25 ng / mL, the linear equation is F0 / F=1.061+0.046[paraoxon], ng / mL, and the detection limit is 0.032 ng / mL, thereby achieving sensitive detection of paraoxon.

[0048] Example 11 Selectivity test of the system method for organophosphorus pesticides 40 μL of other pesticides (propynylamine, chlorpyrifos, imidacloprid, bifenthrin, cypermethrin) (0.625 μg / mL), 40 μL of ions (Na + Mg 2+ , K + , Cl - 、NO3 - 、SO4 2- ,I - ) (1.25 mM), 40 μL of amino acids (serine, methionine, aspartic acid, proline, glycine, valine, tyrosine) (1.25 mM), 40 μL of other biomolecules (creatinine, cholesterol, urea, glucose, sucrose, galactose) (1.25 mM) were mixed with 12 μL of acetylcholinesterase (1.0 U / mL), 20 μL of acetylthiocholine (1.0 mM), and 28 μL of Tris-HCl buffer solution (pH 7.4, 20 mM), and incubated at 37°C for 40 min. Then, 60 μL of Cu 2+ (0.1 mM), 340 μL Tris-HCl buffer solution (pH 6.0, 20 mM) and 500 μL AuNCs@dmSiO2 aqueous solution (1.2 mg / mL) of Example 5 were added, and fluorescence detection was performed on each test solution. The fluorescence spectrum is shown in Fig.11 shown.

[0049] Fig.11 It can be seen that the fluorescence intensity is significantly reduced only in the presence of the organophosphorus pesticide paraoxon, and there is no obvious change in the presence of other types of substances, which shows that the sensing system has a high selectivity for organophosphorus pesticides.

[0050] Example 12 Cotton swabs loaded with AuNCs@dmSiO2 composite materials were used in the detection test of organophosphorus pesticide paraoxon at different concentrations The application method is as follows: a. 40 μL of the test solution containing different concentrations of the organophosphorus pesticide paraoxon was mixed with 12 μL of acetylcholinesterase (1.0 U / mL), 20 μL of acetylthiocholine (1.0 mM) and 28 μL of Tris-HCl buffer solution (pH 7.4, 20 mM), incubated at 37 °C for 40 min, and then 60 μL of Cu 2+ Solution (0.1 mM), 340 μL Tris-HCl buffer solution (pH 6.0, 20 mM), prepared into 8 mixed solutions containing different concentrations of paraoxon; in each mixed solution, the final concentration of paraoxon was 0 ng / mL, 2 ng / mL, 6 ng / mL, 10 ng / mL, 20 ng / mL, 40 ng / mL, 50 ng / mL, 70 ng / mL; b. Eight cotton swabs loaded with the AuNCs@dmSiO2 composite material of Example 5 in Example 8 were respectively immersed in the eight portions of the mixed solution of step a, and the cotton swabs were photographed under a 365 nm ultraviolet lamp. The color RGB value of the image was identified using the color recognition program (ColorCollection) in the smartphone, and the paraoxon concentration was determined by calculating the color signal ratio R / (G+B).

[0051] The process diagram is as follows Fig.12 As shown in A, the test results are Fig.12 As shown in B, Fig.12 C is the fitted straight line between the color signal ratio (R / (G+B)) and the paraoxon concentration. Fig.12 In B, from left to right and from top to bottom, the final concentrations of paraoxon in the mixed solution corresponding to the cotton swabs are 0 ng / mL, 2 ng / mL, 6 ng / mL, 10 ng / mL, 20 ng / mL, 40 ng / mL, 50 ng / mL, and 70 ng / mL.

[0052] Fig.12 B shows that the detection cotton swab has obvious fluorescence dimming visible fluorescence change under 365 nm ultraviolet light; Fig.12 C shows that the detection range of this method for paraoxon is 2-70 ng / mL, the linear equation is R / (G+B) = 0.656-0.00401[paraoxon], ng / mL, and the detection limit is 0.65 ng / mL, which provides a portable and simple method for the detection of organophosphorus pesticide paraoxon.

Claims

1. Application of AuNCs@dmSiO2 composite materials in the detection of organophosphorus pesticide paraoxon.

2. The use according to claim 1, characterized in that The application method comprises the following steps: a. Mix the test solution containing the organophosphorus pesticide paraoxon, acetylcholinesterase, acetylthiocholine and a portion of Tris-HCl buffer solution, incubate, and then add Cu 2+ solution and another part of Tris-HCl buffer solution to obtain a mixed solution; b. Adding the AuNCs@dmSiO2 composite material aqueous solution to the mixed solution in step a, mixing to obtain a test solution, and performing fluorescence spectrum detection on the test solution; Alternatively, the carrier loaded with the AuNCs@dmSiO2 composite material is placed in the mixed solution of step a, immersed, taken out, and the carrier is analyzed.

3. The use according to claim 2, characterized in that In step b, the carrier is a cotton swab. The cotton swab loaded with the AuNCs@dmSiO2 composite material is immersed in the mixed solution of step a. The cotton swab is photographed under ultraviolet light, the color RGB value of the image is identified, and the paraoxon concentration is determined by calculating the color signal ratio R / (G+B).

4. The use according to claim 2, characterized in that In step a, the concentration of the Tris-HCl buffer solution is 17-25 mM, the pH value is 5-10, the concentration of acetylcholinesterase is 0.8-1.5 U / mL, the concentration of acetylthiocholine is 0.7-1.5 mM, and the concentration of Cu 2+ The concentration of the solution is 0.05-0.15 mM; in step b, the concentration of the AuNCs@dmSiO2 composite material aqueous solution is 1.0-1.5 mg / mL, Tris-HCl buffer solution, acetylcholinesterase, acetylthiocholine, Cu 2+ The volume ratio of the solution and the AuNCs@dmSiO2 composite material aqueous solution is (360-465): (10-15): (15-25): (50-80): (450-650); the incubation conditions are: the incubation temperature is 30-40 °C, and the incubation time is 30-50 min; the AuNCs@dmSiO2 composite material aqueous solution is prepared by dispersing the AuNCs@dmSiO2 composite material in water.

5. The use according to any one of claims 1 to 4, characterized in that: The preparation method of the AuNCs@dmSiO2 composite material comprises the following steps: 1) Preparation of AuNCs solution: Mix glutathione aqueous solution and chloroauric acid aqueous solution, heat and stir, dialysis purification, freeze-dry, and disperse the obtained solid in water to obtain AuNCs solution; 2) Preparation of dmSiO2 dispersion: triethanolamine, hexadecyltrimethylammonium bromide, sodium salicylate and water are mixed, heated and stirred, ethyl orthosilicate is added, heated and stirred for reaction, cooled, precipitates are collected, washed and purified, the precipitates are dispersed in an organic solvent, ammonia water and (3-aminopropyl)triethoxysilane are added, stirred for reaction, the products are collected, washed and freeze-dried to obtain mesoporous silica spheres, and the mesoporous silica spheres are dispersed in water to obtain dmSiO2 dispersion; 3) Preparation of AuNCs@dmSiO2 composite material: The AuNCs solution in step 1) and the dmSiO2 dispersion in step 2) were mixed, and freeze-dried to obtain the AuNCs@dmSiO2 composite material.

6. The use according to claim 5, characterized in that In step 1), the molar ratio of glutathione in the glutathione aqueous solution to chloroauric acid in the chloroauric acid aqueous solution is (1-3):2; the heating and stirring conditions are: temperature of 65-75°C, stirring speed of 500-800 rpm, and time of 20-30 h.

7. The use according to claim 5, characterized in that In step 2), the amount ratio of triethanolamine, hexadecyltrimethylammonium bromide, sodium salicylate, ethyl orthosilicate, ammonia water and (3-aminopropyl)triethoxysilane is (60-80) mg: (360-400) mg: (140-180) mg: (3-5) mL: (2-4) mL: (0.5-1.5) mL; at a stirring speed of 500-800 rpm, triethanolamine, hexadecyltrimethylammonium bromide, sodium salicylate and water are mixed, stirred at 80-90 ° C for 1-2 h, ethyl orthosilicate is added, stirred at 70-85 ° C for 2-3 h, cooled, and the precipitate is collected. After washing and purification, the precipitate is dispersed in an organic solvent, and ammonia water and (3-aminopropyl)triethoxysilane are added at a stirring speed of 500-800 rpm, and stirred for 10-15 h.

8. The use according to claim 5, characterized in that In step 3), the mass ratio of dmSiO2 in the dmSiO2 dispersion and AuNCs in the AuNCs solution is (1-5):1, and the mixing conditions are: temperature of 20-35 °C and time of 10-20 min; The particle size of AuNCs@dmSiO2 composite materials is 250-300 nm.

9. The use according to claim 3, characterized in that The preparation method of the cotton swab loaded with the AuNCs@dmSiO2 composite material is as follows: placing the cotton swab in a solution containing the AuNCs@dmSiO2 composite material and gelatin, soaking for 10-15 min, taking out, and freeze-drying; in the solution, the concentration of the AuNCs@dmSiO2 composite material is 1.0-1.5 mg / mL, and the concentration of gelatin is 4.0-7.0 mg / mL.

10. The use according to claim 9, characterized in that In step b, a cotton swab loaded with AuNCs@dmSiO2 composite material is placed in the mixed solution of step a, and each cotton swab is loaded with 0.50-0.75 mg of AuNCs@dmSiO2 composite material.

Citation Information

Patent Citations

  • Intelligent silicon dioxide nano pesticide for preventing and treating pine tree wilt

    CN114027297A

  • Mesoporous silicon drug loading system, preparation method and mesoporous silicon loaded drug

    CN114767871A

  • Quantum dot sensor array based on dendritic mesoporous nanoparticles, preparation method of quantum dot sensor array and application of quantum dot sensor array in water sample detection

    CN115541546A

  • Nanometer pesticide preparation with dendritic mesoporous silica as carrier and preparation method and application thereof

    CN115968871A

  • Preparation method of pitaya type colorimetric microsphere probe and application of pitaya type colorimetric microsphere probe in hypersensitive instant detection of aflatoxin B1

    CN117451987A

Cited By

  • Colorimetric / fluorescent bimodal analysis method for detecting paraoxon methyl pesticide based on Ca-APTA-CeO2 nano enzyme