Formula and preparation method of blended incense

By using the formulas of agarwood, lavender, mugwort, benzoin, polygonum multiflorum and modified plant powder, combined with high-speed crushing, low-oxygen fermentation and molding processes, the problems of chemical pollution and long preparation time in the production of traditional Chinese medicine fragrance are solved, and safety is achieved , rapid production and the effect of calming the mind and helping sleep.

CN118976068APending Publication Date: 2024-11-19XIAMEN XIANGJITANG INCENSE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411108130.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

During the production process of traditional Chinese medicine fragrance, relatively low-priced smokeless charcoal powder and chemical synthetic fragrances are used on the market, which leads to potential chemical pollutants that harm the human body and are long-term in preparation, making it difficult to meet market demand.

Method used

The formula of agarwood, lavender, mugwort, benzoin, polygonum multiflorum and modified plant powder is prepared by high-speed crushing, low-oxygen fermentation and molding processes combined with low-temperature drying to prepare a safe and fast-produced scented product.

Benefits of technology

It effectively reduces the ash and harmful gas emissions during combustion, improves the fragrance emission efficiency, ensures the safety of the product and market-oriented production capacity, and at the same time realizes the effect of calming the mind and helping sleep.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a formula and a preparation method of blended incense, the blended incense comprises the following components in parts by weight: 50-60 parts of agilawood, 10-15 parts of lavender, 5-8 parts of benzoin, 10-15 parts of folium artemisiae argyi, 5-8 parts of polygonum multiflorum and 15-25 parts of modified plant sticky powder, the polygonum multiflorum is processed by an ancient method, and the modified plant sticky powder is Indonesia nanmu sticky powder subjected to surface oxidation crosslinking treatment. The invention belongs to the technical field of traditional Chinese medicine blended incense formulas and preparation processes, and particularly relates to a blended incense formula and a preparation method. Medicinal materials and incense materials are crushed at a high speed to obtain powder, and modified nanmu sticky powder is used for improving the density and toughness of incense sticks and prolonging the retention time of effective components in the incense stick combustion process; the harm of carbon powder, chemical adhesives and other potential chemical pollutants in the existing joss-stick production industry to the human body is effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of formula and preparation process of traditional Chinese medicine incense, and specifically refers to a formula and preparation method of incense. Background Art

[0002] Traditional Chinese medicine is an important cultural treasure in the inheritance of Chinese civilization, and the use of traditional Chinese medicine and Chinese medicine is widely present in our lives.

[0003] Using Chinese herbal medicine to soothe the mind and help sleep has a long history. The Compendium of Materia Medica and other Chinese medicine books have mentioned the method of using Chinese herbal medicine to calm the mind and spirit, and burning Atractylodes lancea to avoid evil spirits. There is also a folk custom of hanging Atractylodes lancea and mugwort leaves to drive away miasma and remove filth during the Dragon Boat Festival. Among them, the most common methods are Chinese herbal medicine steam fumigation and burning "Chinese medicine incense" fumigation.

[0004] However, in the production process of "Chinese medicine incense", its preparation process is complicated and the preparation time is long, which makes it difficult to meet the market demand. Inferior incense products such as "industrial incense" and "regenerated incense" are mixed in, which not only affects the market order but also affects the health of users. In the production process of "industrial incense", smokeless carbon powder, which is relatively cheap on the market, is used as raw material, and it is scented by mixing with chemical synthetic flavors, etc., and auxiliary materials such as calcium carbonate and magnesium nitrate are added to increase the weight of the product and reduce the smoke of burning cigarettes. The mixed incense raw materials are added with industrial adhesives such as polyacrylamide and cellulose ether to make them into shape. The smoke produced when the incense is burned is complex, containing common formaldehyde, benzene series and polycyclic aromatic hydrocarbons and other air pollutants, which have potential physiological toxicity and are not conducive to long-term use. Summary of the invention

[0005] In order to solve the above-mentioned problems in the current incense stick production industry, such as the use of potential chemical pollutants such as carbon powder and chemical adhesives that are harmful to the human body, and the long preparation time, the present invention provides a formula and preparation method of a mixed incense.

[0006] In order to achieve the above functions, the technical solution adopted by the present invention is as follows: a formula of mixed incense, which consists of 50-60 parts of agarwood, 10-15 parts of lavender, 5-8 parts of benzoin, 10-15 parts of wormwood, 5-8 parts of Polygonum multiflorum, and 15-25 parts of modified plant sticky powder.

[0007] Preferably, the Polygonum multiflorum is processed using traditional methods.

[0008] Preferably, the modified plant adhesive powder is Indonesian nanmu adhesive powder that has been surface oxidized and cross-linked.

[0009] The present invention also discloses a method for preparing a blended fragrance, comprising the following steps:

[0010] (1) Preparation of materials: taking agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder respectively by weight and setting aside;

[0011] (ii) crushing: crushing the reserved agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder at high speed to obtain crushed granules for standby use;

[0012] (iii) pellet stirring: add the crushed pellets obtained in step (ii) into a mixer, set the stirring temperature to 30°C-45°C, and stir at a low speed of 60-240 rpm for 20-30 minutes to obtain premixed pellets for standby use;

[0013] (iv) Granular material bonding: adding the modified plant adhesive powder obtained in step (i) and 3%-5% of the total weight of pure water to the premixed granules, setting the stirring temperature to 55°C-70°C, low speed 60-240 rpm, stirring for 30-45 minutes to obtain a mixed material for standby use;

[0014] (V) Compression molding: adding the mixed pellets obtained in step (IV) into a molding machine, with a pressure of 2-5 MPa, a holding time of 1-10 seconds, a temperature of 45°C-60°C, and demolding to obtain a finished incense product;

[0015] (VI) Low-temperature drying: Place the incense product obtained in step (V) into a drying oven at a temperature of 60-80°C. After drying for 4-6 hours, take it out and air dry it naturally.

[0016] Preferably, after the high-speed crushing in the step (ii), the pellets with a size of 110-135 mesh are screened for use.

[0017] Preferably, the pellets crushed at high speed in the step (ii) are sent to a fermenter for constant temperature and low oxygen natural fermentation, the fermenter temperature is set to 25-30°C, the tank pressure is 0.02-0.05MPa, the oxygen concentration is 1×10-3-4×10-3mmol / L, and the fermentation time is 1-2 months.

[0018] Compared with the prior art, the present invention adopts the above solution to achieve the following beneficial effects:

[0019] 1. The present invention crushes the Chinese medicine raw materials at high speed, selects 110-135 mesh granules for incense making and standby use, and destroys the fiber structure of the Chinese medicine raw materials by high-speed crushing, which is beneficial to bonding and molding during processing, and can also accelerate the emission of aroma and medicinal factors during combustion, and reduce the residual ash after combustion;

[0020] 2. After constant temperature and low oxygen fermentation, the benzaldehyde and unsaturated pyrrolizidine alkaloids widely contained in Chinese medicinal materials can be effectively eliminated through the decomposition of microorganisms, making the Chinese medicine effectively detoxified;

[0021] 3. Through the rational combination of Chinese medicinal materials, commonly used lavender, wormwood, Polygonum multiflorum, benzoin, etc. are selected as the main ingredients for calming the mind and helping sleep, supplemented with aromatic materials with special aromas such as agarwood, which can achieve the effect of calming the mind and helping sleep while achieving the effect of soothing the essence;

[0022] 4. Modified plant adhesive powder is used in the production process. The surface of modified plant adhesive powder has more hydroxyl and carboxyl groups to provide more sticky ends, which can reduce the amount of adhesive powder used. At the same time, it provides stronger adhesion, making the product more resistant to breakage and collision, which is beneficial to the production and transportation of the product. DETAILED DESCRIPTION

[0023] The technical solution of the present invention is described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0024] Example 1

[0025] The invention discloses a formula of incense, which comprises the following components by weight: 50 parts of agarwood, 10 parts of lavender, 5 parts of benzoin, 10 parts of wormwood, 5 parts of polygonum multiflorum and 15 parts of modified plant sticky powder, wherein the polygonum multiflorum is processed by an ancient method, and the modified plant sticky powder is Indonesian nanmu sticky powder subjected to surface oxidation and cross-linking treatment.

[0026] The present invention also discloses a method for preparing a blended fragrance, comprising the following steps:

[0027] (1) Preparation of materials: taking agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder respectively by weight and setting aside;

[0028] (ii) Crushing: The reserved agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder are crushed at high speed to obtain crushed granules, and the granules with a size of 110 mesh are screened for use. The granules after high-speed crushing are sent to a fermentation tank for constant temperature and low oxygen natural fermentation. The fermentation tank temperature is set to 30° C., the tank pressure is 0.05 MPa, the oxygen concentration is 1×10-3 mmol / L, and the fermentation time is 1 month;

[0029] (iii) pellet stirring: add the crushed pellets obtained in step (ii) into a mixer, set the stirring temperature to 30° C., and stir at a low speed of 120 rpm for 20 minutes to obtain premixed pellets for later use;

[0030] (iv) Granular material bonding: Add the modified plant adhesive powder obtained in step (i) and 3% by weight of pure water to the uniformly stirred premixed granules, set the stirring temperature to 45° C., and stir at a low speed of 150 rpm for 30 minutes to obtain a mixed material for standby use;

[0031] (V) Compression molding: Add the mixed pellets obtained in step (IV) into a molding machine, with a pressure of 2 MPa, a holding time of 5 seconds, a temperature of 45°C, and demolding to obtain a finished incense product;

[0032] (VI) Low-temperature drying: Place the blended fragrance product obtained in step (V) in a drying oven at a temperature of 60°C. After drying for 4 hours, take it out and allow it to air dry naturally.

[0033] Example 2

[0034] The invention discloses a formula of incense, which comprises the following components by weight: 60 parts of agarwood, 15 parts of lavender, 8 parts of benzoin, 15 parts of wormwood, 8 parts of polygonum multiflorum and 25 parts of modified plant sticky powder, wherein the polygonum multiflorum is processed by an ancient method, and the modified plant sticky powder is Indonesian nanmu sticky powder subjected to surface oxidation and cross-linking treatment.

[0035] The present invention also discloses a method for preparing a blended fragrance, comprising the following steps:

[0036] (1) Preparation of materials: taking agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder respectively by weight and setting aside;

[0037] (ii) Crushing: The reserved agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder are crushed at high speed to obtain crushed granules, and the granules with a size of 135 mesh are screened for use. The granules after high-speed crushing are sent to a fermentation tank for constant temperature and low oxygen natural fermentation. The fermentation tank temperature is set to 25°C, the tank pressure is 0.02MPa, the oxygen concentration is 4×10-3mmol / L, and the fermentation time is 2 months;

[0038] (iii) pellet stirring: add the crushed pellets obtained in step (ii) into a mixer, set the stirring temperature to 45°C, and stir at a low speed of 240 rpm for 30 minutes to obtain premixed pellets for later use;

[0039] (iv) Granular material bonding: adding the modified plant adhesive powder obtained in step (i) and 5% by weight of pure water to the uniformly stirred premixed granules, setting the stirring temperature to 70° C., stirring at a low speed of 240 rpm for 45 minutes to obtain a mixed material for standby use;

[0040] (V) Compression molding: Add the mixed pellets obtained in step (IV) into a molding machine, with a pressure of 5 MPa, a holding time of 1 second, a temperature of 60° C., and demolding to obtain a finished incense product;

[0041] (VI) Low-temperature drying: The mixed fragrance product obtained in step (V) is placed in a drying oven at a temperature of 80°C. After drying for 6 hours, the product is taken out and air-dried naturally.

[0042] Example 3

[0043] The invention discloses a formula of incense, which comprises the following components by weight: 55 parts of agarwood, 12 parts of lavender, 6 parts of benzoin, 12 parts of wormwood, 6 parts of polygonum multiflorum and 10 parts of modified plant sticky powder, wherein the polygonum multiflorum is processed by an ancient method, and the modified plant sticky powder is Indonesian nanmu sticky powder subjected to surface oxidation and cross-linking treatment.

[0044] The present invention also discloses a method for preparing a blended fragrance, comprising the following steps:

[0045] (1) Preparation of materials: taking agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder respectively by weight and setting aside;

[0046] (ii) Crushing: The reserved agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder are crushed at high speed to obtain crushed granules, and the granules with a size of 120 mesh are screened for use. The granules after high-speed crushing are sent to a fermentation tank for constant temperature and low oxygen natural fermentation. The fermentation tank temperature is set to 27° C., the tank pressure is 0.03 MPa, the oxygen concentration is 3×10-3 mmol / L, and the fermentation time is 1 month;

[0047] (iii) Granule stirring: Add the crushed granules obtained in step (ii) into a mixer, set the stirring temperature to 36° C., and stir at a low speed of 120 rpm for 25 minutes to obtain a premixed granule for later use;

[0048] (iv) Granular material bonding: Add the modified plant adhesive powder obtained in step (i) and 4% by weight of pure water to the premixed granules, set the stirring temperature to 66° C., and stir at a low speed of 60 rpm for 35 minutes to obtain a mixed material for standby use;

[0049] (V) Compression molding: Add the mixed pellets obtained in step (IV) into a molding machine, with a pressure of 3 MPa, a holding time of 10 seconds, a temperature of 55° C., and demolding to obtain a finished incense product;

[0050] (VI) Low-temperature drying: Place the blended fragrance product obtained in step (V) into a drying oven at a temperature of 70°C. After drying for 5 hours, take it out and allow it to air dry naturally.

[0051] The blended flavor products prepared by using Examples 1-3 have clean and simple ingredients, scientific proportions, and balanced nutrition, and meet national food safety standards after testing.

[0052] The present invention and its embodiments are described above, and such description is not restrictive. What is shown in the embodiment is only one of the embodiments of the present invention, and is not actually limited thereto. In short, if ordinary technicians in the field are inspired by it and design embodiments similar to the technical solution without creativity without departing from the purpose of the invention, they should all fall within the protection scope of the present invention.

Claims

1. A formula for a blended fragrance, characterized in that: The formula composition by weight is: 50-60 parts of agarwood, 10-15 parts of lavender, 5-8 parts of benzoin, 10-15 parts of wormwood, 5-8 parts of Polygonum multiflorum and 15-25 parts of modified plant sticky powder.

2. A formula for a blended fragrance according to claim 1, characterized in that: The Polygonum multiflorum is processed through ancient methods.

3. A formula for a blended fragrance according to claim 1, characterized in that: The modified plant adhesive powder is Indonesian nanmu adhesive powder that has been subjected to surface oxidation and cross-linking treatment.

4. A method for preparing a blended fragrance according to any one of claims 1 to 3, characterized in that: The steps include: (1) Preparation of materials: taking agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant sticky powder respectively by weight and setting aside; (ii) crushing: crushing the reserved agarwood, lavender, wormwood, Polygonum multiflorum, benzoin, and modified plant powder at high speed to obtain crushed granules for standby use; (iii) pellet stirring: add the crushed pellets obtained in step (ii) into a mixer, set the stirring temperature to 30°C-45°C, and stir at a low speed of 60-240 rpm for 20-30 minutes to obtain premixed pellets for standby use; (iv) Granular material bonding: adding the modified plant adhesive powder obtained in step (i) and 3%-5% of the total weight of pure water to the premixed granules, setting the stirring temperature to 55°C-70°C, low speed 60-240 rpm, stirring for 30-45 minutes to obtain a mixed material for standby use; (V) Compression molding: Add the mixed pellets obtained in step (IV) into a molding machine, The pressure is 2-5MPa, the holding time is 1-10 seconds, the temperature is 45℃-60℃, demoulding, and the finished product of the mixed fragrance is obtained; (VI) Low-temperature drying: The mixed fragrance product obtained in step (V) is placed in a drying oven at a temperature of 60-80°C. After drying for 4-6 hours, the product is taken out and air-dried naturally.

5. The method for preparing a blended fragrance according to claim 4, characterized in that: In the step (ii), the pellets after high-speed crushing are screened to have a size of 110-135 mesh for later use.

6. The method for preparing a blended fragrance according to claim 4, characterized in that: The pellets crushed at high speed in step (ii) are sent to a fermentation tank for constant temperature and low oxygen natural fermentation. The fermentation tank temperature is set at 25-30°C, the tank pressure is 0.02-0.05MPa, and the oxygen concentration is 1×10 -3 -4×10 -3 mmol / L, the fermentation time is 1-2 months.